Power storage cell

By varying the thickness of electrode composite material layers in the electrode body to reduce stress, the design addresses cracking issues, ensuring stability and longevity in power storage cells.

JP2024169885AInactive Publication Date: 2024-12-06TOYOTA JIDOSHA KK
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023086722
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-26
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The electrode composite material layers in wound lithium secondary batteries are prone to cracking due to small winding radii, particularly at the center, leading to peeling and other issues.

Method used

The electrode body is designed with a varying thickness distribution, where the electrode composite material layers are thinner towards the starting end and thicker towards the terminal end, maintaining a constant ratio, to reduce stress and prevent cracking.

Benefits of technology

This design effectively suppresses the occurrence of cracks in the electrode composite material layers, even under repeated charge and discharge cycles, thereby enhancing the stability and longevity of the power storage cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024169885000001_ABST
    Figure 2024169885000001_ABST
Patent Text Reader

Abstract

To provide a power storage cell in which occurrence of cracks and the like in an electrode mixture layer is restrained.SOLUTION: A power storage cell includes an electrode body 10 in which a sheet body is wound so as to surround the periphery of a winding axis, and a housing case in which the electrode body 10 is housed. The electrode body 10 includes a start end portion and a terminal portion located on the opposite side to the start end portion in a winding direction. The sheet body includes an electrode sheet and a separator. The electrode sheet includes a current collector and an electrode mixture layer 45 formed on the current collector. The electrode sheet includes a first portion W0 located at one-turn portion from the start end portion and a second portion WE located to be closer to the terminal portion side than the first portion W0. The thickness of the electrode mixture layer 45 located at the first portion W0 is smaller than the thickness of the electrode mixture layer 45 located at the second portion WE.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an energy storage cell. [Background technology]

[0002] Japanese Patent No. 4805545 (Patent Document 1) discloses a lithium secondary battery having a wound internal electrode assembly in which a positive electrode metal foil body and a negative electrode metal foil body are arranged with a separator interposed therebetween. The internal electrode assembly is formed by winding a positive electrode sheet, a separator, and a negative electrode sheet.

[0003] The positive electrode sheet includes a positive electrode current collector and a positive electrode mixture layer formed on the positive electrode current collector, and the negative electrode sheet includes a negative electrode current collector and a negative electrode mixture layer formed on the negative electrode current collector. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 4805545 Summary of the Invention [Problem to be solved by the invention]

[0005] The electrode assembly of the lithium secondary battery configured as described above is formed by winding each sheet.

[0006] For example, the winding radius is small at the winding center of the electrode body. As a result, the winding radius of the positive electrode mixture layer of the positive electrode sheet is also small at the winding center, and the positive electrode mixture layer peels off or cracks occur in the positive electrode mixture layer. The same problem occurs in the negative electrode mixture layer of the negative electrode sheet.

[0007] The present disclosure has been made in consideration of the above-mentioned problems, and has an object to provide an electricity storage cell in which the occurrence of cracks and the like in an electrode mixture layer is suppressed. [Means for solving the problem]

[0008] The energy storage cell comprises an electrode body in which a sheet body is wound so as to surround a winding axis, and a storage case in which the electrode body is housed, the electrode body including a starting end in the winding direction and a terminal end located opposite the starting end, the sheet body including an electrode sheet and a separator, the electrode sheet including a current collector plate and an electrode composite layer formed on the current collector plate, the electrode sheet including a first portion located one turn from the starting end and a second portion located closer to the terminal end than the first portion, and the thickness of the electrode composite layer located in the first portion is thinner than the thickness of the electrode composite layer located in the second portion.

[0009] The electrode sheet includes a positive electrode sheet and a negative electrode sheet. The positive electrode sheet includes a positive electrode current collector and a positive electrode composite layer formed on the positive electrode current collector. The negative electrode sheet includes a negative electrode current collector and a negative electrode composite layer formed on the negative electrode current collector. At least one of the positive electrode composite layer and the negative electrode composite layer has a first portion having a thickness smaller than a second portion.

[0010] The positive electrode mixture layer is formed so as to become thinner from the terminal end to the starting end, and the negative electrode mixture layer is formed so as to become thinner from the terminal end to the starting end. From the terminal end to the starting end, the ratio of the thickness of the positive electrode mixture layer to the thickness of the negative electrode mixture layer is constant. At the same position in the winding direction, the thickness of the negative electrode mixture layer is thicker than the thickness of the positive electrode mixture layer. The thickness of the electrode mixture layer located in the first portion is the average thickness of the electrode mixture layer located in the first portion, and the thickness of the electrode mixture layer located in the second portion is the average thickness of the electrode mixture layer located in the second portion. Effect of the Invention

[0011] According to the energy storage cell according to the present disclosure, the occurrence of cracks and the like in the electrode mixture layer can be suppressed. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a cross-sectional view showing a storage cell 1 according to the present embodiment. [Diagram 2]FIG. 2 is a perspective view showing a schematic view of an electrode body 10. [Diagram 3] FIG. 2 is a plan view showing a positive electrode sheet 22. [Figure 4] FIG. 2 is a plan view showing a negative electrode sheet 24. [Diagram 5] FIG. 2 is a development view showing a state in which the sheet body 20 is developed and the individual sheets are arranged. [Figure 6] 2 is a cross-sectional view showing a positive electrode sheet 22, a negative electrode sheet 24, a separator 21, and a separator 23. FIG. [Figure 7] 2 is a cross-sectional view showing a negative electrode sheet 24A, a separator 23, a positive electrode sheet 22A, and a separator 21 of a storage cell 1A. [Figure 8] 1 is a cross-sectional view showing a negative electrode sheet 24B, a separator 23, a positive electrode sheet 22B, and a separator 21 of a storage cell 1B. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the drawings. In the drawings, the same or corresponding parts are denoted by the same reference characters, and the description thereof will not be repeated.

[0014] 1 is a cross-sectional view showing an energy storage cell 1 according to the present embodiment. The energy storage cell 1 includes a cylindrical electrode body 10 formed so as to surround a winding axis O, a case 11, a positive electrode current collecting member 12, a negative electrode current collecting member 13, insulating members 14 and 15, and a positive electrode terminal 16.

[0015] 1 and the like, "Z" indicates the direction in which the winding axis O extends. "Z1" indicates one direction of the Z direction. "Z2" indicates the other direction of the Z direction. "R" indicates the radial direction of the electrode body 10.

[0016] The case 11 includes a top plate 17, a bottom plate 18, and a peripheral wall 19. The case 11 is formed of a metal material. The top plate 17 is located at one end of the case 11, and the bottom plate 18 is located at the other end of the case 11. The peripheral wall 19 is disposed between the top plate 17 and the bottom plate 18.

[0017] A through hole 7 is formed in the top plate 17. The insulating member 14 is disposed on the outer surface of the top plate 17, and a through hole is formed in the insulating member 14.

[0018] The insulating member 15 includes a top plate portion 2 and a peripheral wall 3 provided on the outer periphery of the top plate portion 2. The top plate portion 2 is disposed on the inner surface of a top plate 17. The peripheral wall 3 is disposed on the inner periphery of a peripheral wall 19. The top plate 17 has a through hole formed therein.

[0019] The positive electrode terminal 16 includes a flat plate 50 and a shaft 51. The flat plate 50 is disposed on the insulating member 14. The shaft 51 is connected to the flat plate 50 and is formed so as to extend in the Z2 direction. The shaft 51 is inserted into the case 11 through a through hole formed in the insulating member 14, the through hole 7, and a through hole formed in the insulating member 15.

[0020] The positive current collecting member 12 is disposed on the Z2 direction side with respect to the insulating member 15. The positive current collecting member 12 is formed in a plate shape, and the lower end of the shaft 51 is welded to the upper surface of the positive current collecting member 12. The positive current collecting member 12 is formed of, for example, aluminum.

[0021] The negative electrode current collecting member 13 is disposed on the inner surface of the bottom plate 18. The negative electrode current collecting member 13 is formed in a plate shape and is made of a metal material such as copper.

[0022] The electrode body 10 is disposed within the case 11 between a positive electrode current collecting member 12 and a negative electrode current collecting member 13 .

[0023] The electrode body 10 includes an end 5 located on the Z1 direction side, and a positive electrode current collecting member 12 is disposed at the end 5. The electrode body 10 includes an end 6 located on the Z2 direction side, and a negative electrode current collecting member 13 is disposed at the end 6. The electrode body 10 is formed in a hollow shape, and a hollow portion 43 is formed. The hollow portion 43 is formed at a position passing through the winding axis O.

[0024] 2 is a perspective view that shows a schematic view of the electrode body 10. The electrode body 10 includes a sheet body 20 that is formed so as to surround the periphery of the winding axis O. Note that "D" is the direction in which the sheet body 20 extends in the electrode body 10 in a wound state.

[0025] The sheet body 20 is formed long in the winding direction D of the electrode body 10. The sheet body 20 includes a separator 21, a positive electrode sheet 22, a separator 23, and a negative electrode sheet 24.

[0026] 3 is a plan view showing the positive electrode sheet 22. The positive electrode sheet 22 shown in FIG. 3 is in a state in which it has been unwound from the electrode body 10 and is unfolded. The positive electrode sheet 22 includes a long side 30, a long side 31, and short sides 32 and 33. The long sides 30 and 31 extend in the L1 direction in which the positive electrode current collector plate 25 extends. The L1 direction corresponds to the winding direction D in the wound electrode body 10. In the wound state, the long side 30 is located at the end 5 of the electrode body 10, and the long side 31 is located at the end 6 of the electrode body 10 in the wound state.

[0027] Positive electrode sheet 22 includes a positive electrode current collector 25 and a positive electrode mixture layer 26. Positive electrode current collector 25 is formed of a metal material such as aluminum or an aluminum alloy.

[0028] The positive electrode mixture layer 26 includes a positive electrode active material, a binder, etc. The positive electrode active material includes, for example, LiCoO2, LiNo2, LiMn2O4, etc. The thickness of the positive electrode mixture layer 26 is, for example, not less than 0.1 μm and not more than 1000 μm.

[0029] The positive electrode current collector 25 includes a coated portion 27 on which the positive electrode mixture layer 26 is formed, and an uncoated portion 28 on which the positive electrode mixture layer 26 is not formed. The positive electrode mixture layer 26 is formed from the short side 33 to the short side 32. The positive electrode mixture layer 26 is formed on both the front and back sides of the positive electrode current collector 25, but the positive electrode mixture layer 26 may be formed on one side. The uncoated portion 28 is formed on the long side 30. The uncoated portion 28 includes a plurality of positive electrode metal pieces 29 arranged in the L1 direction.

[0030] FIG. 4 is a plan view showing the negative electrode sheet 24. The negative electrode sheet 24 shown in FIG. 4 is in a state in which it has been unwound from the electrode body 10 and spread out. The negative electrode sheet 24 includes a negative electrode current collector 34 and a negative electrode mixture layer 35. The negative electrode sheet 24 includes a long side 36, a long side 37, and short sides 38 and 39. The long sides 36 and 37 extend in the L2 direction in which the negative electrode sheet 24 extends. The long side 36 is located at the end 5 of the electrode body 10 in the wound state, and the long side 37 is located at the end 6 of the electrode body 10 in the wound state.

[0031] Negative electrode mixture layer 35 is formed from short side 39 to short side 38. Negative electrode mixture layer 35 includes a negative electrode active material, a binder, and the like. The negative electrode active material is graphite, for example. Negative electrode mixture layer 35 has a thickness of, for example, 0.1 μm or more and 1000 μm or less.

[0032] The negative electrode current collector 34 includes a metal material such as copper. The negative electrode current collector 34 includes a coated portion 40 on which the negative electrode composite layer 35 is formed, and an uncoated portion 41 on which the negative electrode composite layer 35 is not formed. The uncoated portion 41 is formed on the long side 37. The uncoated portion 41 includes a plurality of negative electrode metal pieces 42 arranged in the L2 direction.

[0033] 5 is a development view showing the state in which the sheet body 20 is developed and the individual sheets are arranged. The sheet body 20 is formed by overlapping the separator 23 on the negative electrode sheet 24, the positive electrode sheet 22 on the separator 23, and the separator 21 on the positive electrode sheet 22. The positions of the negative electrode sheet 24 and the positive electrode sheet 22 may be interchanged.

[0034] Separator 21 and separator 23 are formed to be long. Separator 21 includes long sides 70 and 71 and short sides 72 and 73. Separator 23 includes long sides 75 and 76 and short sides 77 and 78.

[0035] 5, the electrode body 10 includes an electrode mixture layer 45, which includes a positive electrode mixture layer 26 and a negative electrode mixture layer 35. "S" indicates a starting end S of the electrode mixture layer 45 that is located on the winding axis O side. "E" indicates an ending end E of the electrode mixture layer 45 that is located on the opposite side to the starting end S.

[0036] In the example shown in FIG. 5, the short side 33 and the short side 39 are located at the starting end S. The short side 32 and the short side 38 are located at the terminal end E. The short side 33 and the short side 39 may be shifted in the winding direction D. In this case, in the wound state, the side closer to the winding axis O becomes the starting end S. Similarly, when the short side 32 and the short side 38 are shifted in the winding direction D, the side farther from the winding axis O becomes the terminal end E. In the example shown in FIG. 5, the short sides 73 and 78 of the separators 21 and 23 are also located at the starting end S, and the short sides 72 and 73 are also located at the terminal end E. On the other hand, the separators 21 and 23 may be formed longer in the winding direction D than the positive electrode sheet 22 and the negative electrode sheet 24.

[0037] 6 is a cross-sectional view showing positive electrode sheet 22, negative electrode sheet 24, separator 21, and separator 23. Positive electrode current collector 25 includes main surface 80 and main surface 81. Positive electrode mixture layer 26 includes one-sided positive electrode mixture layer 82 formed on main surface 80, and one-sided positive electrode mixture layer 83 formed on main surface 81.

[0038] Here, thickness Th26 of positive electrode mixture layer 26 is the sum of thickness Th82 of one-side positive electrode mixture layer 82 and thickness Th83 of one-side positive electrode mixture layer 83. The thickness is measured in a direction perpendicular to main surfaces 80, 81.

[0039] Negative current collector 34 includes main surface 84 and main surface 85. Negative mixture layer 35 includes one-sided negative mixture layer 86 formed on main surface 84 and one-sided negative mixture layer 87 formed on main surface 85.

[0040] Thickness Th35 of negative electrode mixture layer 35 is the sum of thickness Th86 of one-side negative electrode mixture layer 86 and thickness Th87 of one-side negative electrode mixture layer 87.

[0041] "W0" is a one-turn portion W0 indicating a portion of the electrode mixture layer 45 from the starting end S to one turn. "WE" indicates a portion WE of the electrode mixture layer 45 located on the terminal end E side of the one-turn portion W0.

[0042] The first portion W1 is a portion of the positive electrode mixture layer 26 that is located at the one-turn portion W0. The second portion W2 is a portion of the negative electrode mixture layer 35 that is located at the one-turn portion W0.

[0043] The thickness of electrode mixture layer 45 is the sum of thickness Th26 of positive electrode mixture layer 26 and thickness Th35 of negative electrode mixture layer 35.

[0044] The thickness of the electrode mixture layer 45 located at the one-turn portion W0 is smaller than the thickness of the electrode mixture layer 45 located at the portion WE.

[0045] The electrode body 10 is formed so as to surround the periphery of the winding axis O from the starting end S. Therefore, in the electrode body 10 in a wound state, the radius of curvature Rs of the one-turn portion W0 is smaller than the radius of curvature Re of the portion WE.

[0046] Therefore, there is a risk that cracks may occur in the electrode mixture layer 45 at the one-turn portion W0. On the other hand, in the energy storage cell 1 according to the present embodiment, the thickness of the electrode mixture layer 45 located at the one-turn portion W0 is thinner than the thickness of the electrode mixture layer 45 located at the portion WE, so that the occurrence of cracks and the like in the electrode mixture layer 45 is suppressed.

[0047] Positive electrode mixture layer 26 is formed so as to have a thickness Th26 that decreases from terminal end E toward starting end S. Thicknesses Th82, Th83 are also formed so as to decrease from terminal end E toward starting end S.

[0048] The radius of curvature Rs of the one-turn portion W0 becomes smaller toward the starting end S. Therefore, by forming the thickness Th26 to become thinner from the terminal end E toward the starting end S, the occurrence of cracks and the like in the positive electrode mixture layer 26 and the one-side positive electrode mixture layers 82, 83 is suppressed.

[0049] The thickness Th35 of the negative electrode mixture layer 35 is formed to become thinner from the terminal end E toward the starting end S. The thicknesses Th86 and Th87 are also formed to become thinner from the terminal end E toward the starting end S. For this reason, the occurrence of cracks and the like is suppressed in the negative electrode mixture layer 35 and the one-side negative electrode mixture layers 86 and 87 as well.

[0050] The ratio of the thickness Th26 to the thickness Th35 is constant from the terminal end E to the starting end S. Here, "constant" means that the difference in the ratio is, for example, 0.1 or less. This makes it possible to suppress lithium deposition even if the energy storage cell 1 is repeatedly charged and discharged.

[0051] At the same position in the winding direction D, the thickness Th35 of the negative electrode mixture layer 35 is formed to be greater than the thickness Th26 of the positive electrode mixture layer 26. This makes it possible to effectively suppress the occurrence of lithium precipitation.

[0052] In the above embodiment, both the positive electrode mixture layer 26 and the negative electrode mixture layer 35 are formed to be thin in the one-turn portion W0, but at least one of the positive electrode mixture layer 26 and the negative electrode mixture layer 35 may be thinned. For example, only the positive electrode mixture layer 26 may be thinned to reduce the thickness of the electrode mixture layer 45 in the one-turn portion W0. (Variation 1) The energy storage cell 1A according to the first modification will be described with reference to Fig. 7. Fig. 7 is a cross-sectional view showing the negative electrode sheet 24A, separator 23, positive electrode sheet 22A, and separator 21 of the energy storage cell 1A.

[0053] The electrode mixture layer 45A includes a positive electrode mixture layer 26A and a negative electrode mixture layer 35A. The electrode mixture layer 45A is formed so that the thickness of the portion located at the one-turn portion W0 is thinner than the thickness of the portion located at the portion WE.

[0054] As a result, in electrode body 10A in a wound state, the occurrence of cracks or the like in positive electrode mixture layer 26A and negative electrode mixture layer 35A is suppressed in one-turn portion W0.

[0055] A thickness Th260 of positive electrode mixture layer 26A located in one-turn portion W0 is constant. A thickness Th350 of negative electrode mixture layer 35A located in one-turn portion W0 is also constant.

[0056] A thickness Th26e of positive electrode mixture layer 26A located in portion WE is constant, and a thickness Th35e of negative electrode mixture layer 35A located in portion WE is also constant.

[0057] Furthermore, thickness Th260 is thinner than thickness Th26e, and thickness Th350 is thinner than Th35e. This makes it possible to suppress the occurrence of cracks or the like in one-turn portion W0 in both positive electrode mixture layer 26A and negative electrode mixture layer 35A. (Variation 2) An energy storage cell 1B according to Modification 2 will be described with reference to Fig. 8. Fig. 8 is a cross-sectional view showing a negative electrode sheet 24B, a separator 23, a positive electrode sheet 22B, and a separator 21 of the energy storage cell 1B.

[0058] The energy storage cell 1B includes positive electrode tabs 90, 91 and negative electrode tabs 92, 93. The positive electrode tabs 90, 91 are provided on a positive electrode sheet 22B.

[0059] One-side positive electrode mixture layer 82 of positive electrode sheet 22B has exposed portions 95 and 96. One-side positive electrode mixture layer 82 is not formed in exposed portions 95 and 96, and part of main surface 80 is exposed.

[0060] One-side negative electrode mixture layer 86 of negative electrode sheet 24B has exposed portions 97 and 98. One-side negative electrode mixture layer 86 is not formed in exposed portions 97 and 98, and main surface 84 is exposed. Positive electrode tabs 90 and 91 are connected to main surface 80 located at exposed portions 95 and 96, and negative electrode tabs 92 and 93 are connected to main surface 84 located at exposed portions 97 and 98.

[0061] In the example shown in this storage cell 1B, a portion where the composite layer is thin is formed in the portion WE, but the average thickness of the electrode composite layer 45B located in the first portion W1 is thinner than the average thickness of the electrode composite layer 45B located in the portion WE.

[0062] Therefore, in the power storage cell 1B as well, the occurrence of cracks or the like in the electrode mixture layer 45B at the one-turn portion W0 can be suppressed.

[0063] The embodiments disclosed herein should be considered as illustrative and not restrictive in all respects. The present disclosure is defined by the scope of claims, and it is intended to include all modifications within the scope and meaning equivalent to the claims. [Explanation of symbols]

[0064] 1,1A,1B storage cell, 2 top plate portion, 3,19 peripheral wall, 5,6 end portion, 7 through hole, 10,10A electrode body, 11 case, 12 positive electrode current collector, 13 negative electrode current collector, 14,15 insulating member, 16 positive electrode terminal, 17 top plate, 18 bottom plate, 20 sheet body, 21,23 separator, 22,22A,22B positive electrode sheet, 24,24A,24B negative electrode sheet, 25 positive electrode current collector, 26,26A,82,83 positive electrode mixture layer, 27,40 coated portion, 28,41 uncoated portion, 29 positive electrode metal piece, 30,31,36,37,70,71,75,76 Long side, 32,33,38,39,72,73,77,78 Short side, 34 Negative current collector, 35,35A,86,87 Negative composite layer, 42 Negative metal piece, 43 Hollow portion, 45,45A,45B Electrode composite layer, 50 Flat plate, 51 Axis, 80,81,84,85 Main surface, 90,91 Positive tab, 92,93 Negative tab, 95,96,97,98 Exposed portion, D Winding direction, E End portion, O Winding axis, Re,Rs Radius of curvature, S Starting end, Th26,Th26e,Th35,Th35e,Th82,Th83,Th86,Th87,Th260,Th350 Thickness, W0 One turn part, W1 first part, W2 second part, WE part.

Claims

1. an electrode body in which the sheet body is wound so as to surround a winding axis; A housing case in which the electrode body is housed; Equipped with The sheet body includes an electrode sheet and a separator, The electrode sheet includes a current collector plate and an electrode mixture layer formed on the current collector plate, the electrode mixture layer includes a starting end in a winding direction, a terminal end located opposite to the starting end, a first portion located one turn from the starting end, and a second portion located closer to the terminal end than the first portion, A storage cell, wherein a thickness of the electrode mixture layer located in the first portion is thinner than a thickness of the electrode mixture layer located in the second portion.

2. The electrode sheet includes a positive electrode sheet and a negative electrode sheet, The positive electrode sheet includes a positive electrode current collector and a positive electrode mixture layer formed on the positive electrode current collector, the negative electrode sheet includes a negative electrode current collector and a negative electrode mixture layer formed on the negative electrode current collector, The energy storage cell according to claim 1 , wherein in at least one of the positive electrode mixture layer and the negative electrode mixture layer, the first portion has a thickness smaller than a thickness of the second portion.

3. The positive electrode mixture layer is formed so as to become thinner from the terminal end portion toward the starting end portion, The energy storage cell according to claim 2 , wherein the negative electrode mixture layer is formed so as to become thinner from the terminal end portion toward the starting end portion.

4. The energy storage cell according to claim 3 , wherein a ratio of a thickness of the positive electrode mixture layer to a thickness of the negative electrode mixture layer is constant from the terminal end portion to the starting end portion.

5. The energy storage cell according to claim 2 , wherein the negative electrode mixture layer has a thickness greater than a thickness of the positive electrode mixture layer at the same position in the winding direction.

6. a thickness of the electrode mixture layer located in the first portion is an average thickness of the electrode mixture layer located in the first portion, The energy storage cell according to claim 1 , wherein a thickness of the electrode mixture layer located in the second portion is an average thickness of the electrode mixture layer located in the second portion.

Citation Information

Patent Citations

  • Pole piece and battery pole group

    CN218602472U

  • Nonaqueous secondary battery

    JP2011138729A

  • Positive electrode for secondary battery, and secondary battery

    WO2024225018A1

  • JP1973005545B1