Crystallized glass, heavy metal recovery material, soil modifier, crystallized glass manufacturing method, and heavy metal recovery method
Crystallized glass with magnetic crystals effectively recovers heavy metals and reforms contaminated soil, providing a simple and efficient solution to agricultural soil contamination issues.
Patent Information
- Application Number
- JP2023086984
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-26
- Publication Date
- 2024-12-06
AI Technical Summary
Conventional agriculture faces challenges with soil contamination from heavy metals and organic substances, particularly due to the use of phosphorus raw materials with high heavy metal content, leading to potential health risks and disease concerns, and existing recovery methods are not efficient or cost-effective.
Development of crystallized glass containing 20-80% magnetic crystals, primarily Fe2O3, which can be used as a heavy metal recovery material and soil reforming material, utilizing a simple method involving a melting and crystallization process to adsorb and recover heavy metals effectively.
The crystallized glass efficiently recovers heavy metals and reforms soil by adsorbing them using magnetic crystals, facilitating easy collection with a magnet, thus addressing contamination issues and promoting sustainable agricultural practices.
Smart Images

Figure 2024170046000001 
Figure 2024170046000002
Abstract
Description
[Technical field]
[0001] The present invention relates to crystallized glass, a heavy metal recovery material, a soil improver, a method for producing crystallized glass, and a method for recovering heavy metals. [Background technology]
[0002] There are concerns that food supply will not be able to keep up with the growing food demand caused by the global population growth. Vertical farming and urban farming mainly produce leafy vegetables, and they do not have the production volume or variety to meet the nutritional needs of the world's population. Therefore, it can be said that we will have no choice but to respond to future population growth and expanding food demand with existing conventional agriculture.
[0003] Problems faced by conventional agriculture include contamination of agricultural soil with heavy metals and certain organic matter. For example, contaminants can be introduced from agricultural fertilizers such as phosphorus. Phosphorus is an important nutritional component that is one of the three major nutrients for agricultural crops, and it is expected that phosphorus raw materials with relatively high heavy metal contents will have to be used to meet the demand from various industries. In addition, although various countries have been researching and developing methods to recover phosphorus from sewage sludge, etc., there is a problem that such recycled phosphorus also has a large amount of residual heavy metals. Therefore, regardless of the phosphorus source used, it is expected that heavy metals will accumulate in agricultural soil, and as a result, there are concerns about an increase in the amount of heavy metals accumulating in the human body and an increased risk of various diseases such as kidney damage.
[0004] Against this background, methods for recovering heavy metals from phosphorus sources and agricultural soils are being investigated (e.g., Reference 1). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2012-188492 A Summary of the Invention [Problem to be solved by the invention]
[0006] Although the cited document 1 considers a sheet-shaped recovery material, it does not consider the recovery method of the sheet-shaped recovery material itself. In order to meet the global need for heavy metal recovery, a heavy metal recovery method that takes into account the cost of the entire recovery process is required.
[0007] In view of the above, an object of the present invention is to provide crystallized glass capable of recovering heavy metals and the like in a simple manner, a heavy metal recovery material, a soil improver, a method for producing crystallized glass, and a method for recovering heavy metals. [Means for solving the problem]
[0008] The following describes various aspects of providing crystallized glass, a heavy metal recovery material, a soil improver, a method for producing crystallized glass, and a method for recovering heavy metals that solve the above problems.
[0009] The crystallized glass of aspect 1 is characterized by containing, by mass %, 20 to 80% of Fe2O3 and including magnetic crystals.
[0010] The crystallized glass of embodiment 2 is preferably the same as that of embodiment 1, containing, by mass%, SiO20-80%, Al2O30-80%, B2O30-80%, P2O50-80%, Li2O0-50%, Na2O0-50%, K2O0-50%, MgO0-50%, CaO0-50%, SrO0-50%, BaO0-50%, ZnO0-50%, ZrO20-50%, HfO20-50%, TiO20-50%, SnO20-50%, V2O50-50%, NiO0-80%, Cr2O30-80%, and MoO30-80%.
[0011] The crystallized glass of the embodiment 3 preferably contains, by mass %, 20% or more of SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3 in the embodiment 1 or 2. Here, "SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3" means the total content of SnO2, Fe2O3, V2O5, NiO, Cr2O3 and MoO3.
[0012] The crystallized glass of Aspect 4 is preferably such that, in mass %, K2O / (Li2O+Na2O+K2O) is 0.01 to 0.99 in any one of Aspects 1 to 3. Here, "K2O / (Li2O+Na2O+K2O)" means the value obtained by dividing the content of K2O by the total content of Li2O, Na2O, and K2O.
[0013] The crystallized glass of embodiment 5 is preferably such that the mass % ratio (SiO2+P2O5) / (SiO2+Al2O3+P2O5) is 0.01 to 0.99 in any one of embodiments 1 to 4. Here, "(SiO2+P2O5) / (SiO2+Al2O3+P2O5)" means the value obtained by dividing the total content of SiO2 and P2O5 by the total content of SiO2, Al2O3, and P2O5.
[0014] The crystallized glass of embodiment 6, in any one of embodiment 1 to embodiment 5, preferably has a mass % ratio of SiO2 / (B2O3+P2O5+ZrO2+HfO2+TiO2+SnO2) of 0.1 to 10000. Here, "SiO2 / (B2O3+P2O5+ZrO2+HfO2+TiO2+SnO2)" means the value obtained by dividing the content of SiO2 by the total content of B2O3, P2O5, ZrO2, HfO2, TiO2 and SnO2.
[0015] The crystallized glass of embodiment 7, in any one of embodiments 1 to 6, preferably has a mass % ratio of SiO2 / (MgO+CaO+SrO+BaO+ZnO) of 0.1 to 10000. Here, "SiO2 / (MgO+CaO+SrO+BaO+ZnO)" means the value obtained by dividing the content of SiO2 by the total content of MgO, CaO, SrO, BaO, and ZnO.
[0016] The crystallized glass of embodiment 8, in any one of embodiments 1 to 7, preferably has a mass % ratio of SiO2 / (SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3) of 0.01 to 10. Here, "SiO2 / (SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3)" means the value obtained by dividing the content of SiO2 by the total content of SnO2, Fe2O3, V2O5, NiO, Cr2O3, and MoO3.
[0017] The crystallized glass of Example 9, in any one of Examples 1 to 8, preferably contains, by mass%, more than 30% MoO.
[0018] The crystallized glass of embodiment 10, in any one of embodiments 1 to 9, preferably contains, by mass %, 100 ppm or less of Pt.
[0019] The crystallized glass of embodiment 11, in any one of embodiments 1 to 10, preferably contains, by mass %, 100 ppm or less of Rh.
[0020] The crystallized glass of embodiment 12 is any one of embodiment 1 to embodiment 11, in which the β-OH value of the original glass before crystallization is preferably more than 0 and 2 / mm.
[0021] The crystallized glass of embodiment 13, in any one of embodiments 1 to 12, preferably has an absolute value of Seebeck coefficient of 0.000001 V / K or more at any one temperature point between 25°C and 400°C.
[0022] The crystallized glass of embodiment 14, in any one of embodiments 1 to 13, preferably has a thermoelectric conversion index ZT of 0.00001 or more at any one temperature point between 25°C and 400°C.
[0023] The crystallized glass of embodiment 15 is any one of embodiment 1 to embodiment 14, wherein the carrier mobility is 0.0001 cm 2 It is preferable that the value is equal to or larger than / Vs.
[0024] The crystallized glass of the sixteenth embodiment is preferably used as a heavy metal recovery material in any one of the first to fifteenth embodiments.
[0025] A heavy metal recovery material according to a seventeenth aspect is characterized in that it contains, by mass %, 20 to 80% of Fe2O3 and is made of crystallized glass containing magnetic crystals.
[0026] The soil conditioner of aspect 18 is characterized in that it contains, by mass %, 20 to 80% of Fe2O3 and is made of crystallized glass containing magnetic crystals.
[0027] The method for producing crystallized glass of embodiment 19 is a method for producing crystallized glass of any one of embodiments 1 to 16, and is characterized in that it includes a melting step of melting a mixture of glass raw materials and Fe2O3 raw materials, and a crystallization step of forming the molten glass into a predetermined shape to obtain crystallized glass.
[0028] A method for recovering heavy metals according to a twentieth aspect of the present invention is characterized by comprising an adsorption step of adsorbing heavy metals to crystallized glass containing magnetic crystals, and a recovery step of recovering the crystallized glass after the heavy metals have been adsorbed thereto by a magnet.
[0029] The method for recovering heavy metals in embodiment 21 is preferably the same as in embodiment 20, in which heavy metals are recovered from soil. Effect of the Invention
[0030] According to the present invention, it is possible to provide crystallized glass capable of recovering heavy metals and the like in a simple manner, a heavy metal recovery material, a soil improver, a method for producing crystallized glass, and a method for recovering heavy metals. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] Hereinafter, the embodiments of the present invention will be described in detail. However, the present invention is not limited to the following embodiments. In addition, in the following description of the content of each component, "%" means "mass %" unless otherwise specified.
[0032] <Glass-ceramics> The crystallized glass of the present invention is characterized by containing, by mass%, 20-80% Fe2O3 and containing magnetic crystals. More specifically, the crystallized glass further contains, by mass%, 0-80% SiO2, 0-80% Al2O3, 0-80% B2O3, 50-80% P2O, 0-50% Li2O, 0-50% Na2O, 0-50% K2O, 0-50% MgO, 0-50% CaO, 0-50% SrO, 0-50% BaO, 0-50% ZnO, 0-50% ZrO20-50%, 0-50% HfO20-50%, 0-50% TiO2, 0-50% SnO20-50%, 50-50% V2O, 0-80% NiO, 0-80% Cr2O3, and 0-80% MoO3. The inclusion of Fe2O3 allows the glass to adsorb heavy metals, and the inclusion of magnetic crystals allows the glass to be easily recovered using a magnet when used as a heavy metal recovery material.
[0033] Fe2O3 is a component that has the ability to adsorb heavy metals. It is also a component that can form magnetic crystals. The content of Fe2O3 is 20 to 80%. More specifically, the lower limit of the content of Fe2O3 is preferably 20% or more, 21% or more, 23% or more, and particularly 25% or more, and the upper limit of the content of Fe2O3 is preferably 80% or less, 70% or less, 60% or less, and particularly 55% or less. If the content of Fe2O3 is too low, it becomes difficult to include magnetic crystals in the crystallized glass. If the content of Fe2O3 is too high, the viscosity of the glass melt decreases, making it difficult to mold it into a desired shape. In addition, when used in agricultural soil, Fe ions are easily eluted, which results in a decrease in the fertility of the soil.
[0034] Here, the magnetic crystal means a crystal having properties such as superferromagnetism, ferromagnetism, paramagnetism, and ferrimagnetism. More specifically, the magnetic crystal is preferably a ferrite crystal. Ferrite crystals include magnetite (Fe3O4), maghemite (γ-Fe2O3), manganese zinc ferrite, nickel zinc ferrite, copper zinc ferrite, (Fe2O3)10.6667[γ-Fe2O3], and Na 0.75 Ca 0.25 It is preferable to contain one of Fe(SiO6). The crystallized glass of the present invention may contain crystals other than the crystals exemplified above, as long as the desired characteristics are obtained. For example, it may contain gahnite, willemite (zinc silicate), Al2SiO5 (aluminum silicate), zirconia, zirconia titanate, tin-containing zirconia-based oxide, titania, aluminotitanate, β-quartz solid solution, α-quartz, β-quartz, β-spodumene solid solution, spodumene, zircon, cordierite other than α-cordierite, enstatite, mica, nepheline, anorthite, lithium disilicate, lithium metasilicate, wollastonite, diopsite, cristobalite, tridymite, feldspar, spinel-based crystals, metal colloids, etc. These crystals may be contained only one type, or two or more types.
[0035] SiO2 forms the skeleton of glass and can be a constituent of crystals in crystallized glass. It is also a component that improves the chemical durability of glass. It is also a component that reduces the thermal expansion coefficient and makes it easier to obtain crystallized glass with excellent thermal shock resistance. The content of SiO2 is preferably 0 to 80%. More specifically, the lower limit of the content of SiO2 is preferably 0% or more, 1% or more, 5% or more, 10% or more, 20% or more, 25% or more, and particularly 29% or more, and the upper limit of the content of SiO2 is preferably 80% or less, 75% or less, 70% or less, 65% or less, and particularly 60% or less. If the content of SiO2 is too high, the meltability of glass is likely to decrease. In addition, the viscosity of the glass melt increases, making it difficult to clarify and mold the glass. In addition, the time required for crystallization increases, and productivity is likely to decrease.
[0036] Al2O3 forms the skeleton of the glass and can be a constituent of the crystals in the crystallized glass. It also contributes to the viscosity of the glass melt and is a component that easily improves the formability. The content of Al2O3 is preferably 0 to 80%. More specifically, the lower limit of the content of Al2O3 is preferably 0% or more, particularly 1% or more, and the upper limit of the content of Al2O3 is preferably 80% or less, 70% or less, 60% or less, 50% or less, 40% or less, 30% or less, 20% or less, particularly 15% or less. If the content of Al2O3 is too high, the chemical durability of the crystallized glass is likely to decrease.
[0037] B2O3 is a component that reduces the viscosity of glass and improves the melting and moldability of glass. It can also be a constituent of crystals in crystallized glass. The content of B2O3 is preferably 0 to 80%. More specifically, the lower limit of the content of B2O3 is preferably 0% or more, 1% or more, and particularly 2% or more, and the upper limit of the content of B2O3 is preferably 80% or less, 70% or less, 60% or less, 50% or less, 40% or less, 30% or less, 20% or less, and particularly 10% or less. If the content of B2O3 is too high, the amount of evaporation of B2O3 during melting increases, which increases the environmental load, and the chemical durability of the crystallized glass is likely to decrease. Note that B2O3 may not be substantially contained. However, since B2O3 is easily mixed in as an impurity, if it is attempted to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, B2O3 may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more. In this specification, the term "substantially free" means that the substance is not intentionally contained as a raw material, and objectively refers to a content of less than 0.1%.
[0038] P2O5 is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a component of crystals in crystallized glass. The content of P2O5 is preferably 0 to 80%. More specifically, the lower limit of the content of P2O5 is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of P2O5 is preferably 80% or less, 70% or less, 60% or less, 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of P2O5 is too high, the amount of evaporation of P2O5 during melting increases, which increases the environmental load, and the chemical durability of the crystallized glass tends to decrease. It is not necessary to substantially contain P2O5. However, since P2O5 is easily mixed in as an impurity, if it is attempted to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, P2O5 may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0039] Li2O is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a component of crystals in crystallized glass. The content of Li2O is preferably 0 to 50%. More specifically, the lower limit of the content of Li2O is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of Li2O is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of Li2O is too high, the amount of evaporation of Li2O during melting increases, which increases the environmental load, and the chemical durability of the crystallized glass is likely to decrease. Li2O may not be substantially contained. However, since Li2O is easily mixed in as an impurity, if it is attempted to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, Li2O may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0040] Na2O is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a constituent of crystals in crystallized glass. The content of Na2O is preferably 0 to 50%. More specifically, the lower limit of the content of Na2O is preferably 0% or more, 0.1% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of Na2O is preferably 50% or less, 40% or less, 30% or less, 20% or less, 15% or less, and particularly 11% or less. If the content of Na2O is too high, the amount of evaporation of Na2O during melting increases, which increases the environmental load, and the chemical durability of the crystallized glass is likely to decrease. Note that Na2O may not be substantially contained. However, since Na2O is easily mixed in as an impurity, if it is attempted to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, Na2O may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0041] K2O is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a constituent of crystals in crystallized glass. The content of K2O is preferably 0 to 50%. More specifically, the lower limit of the content of K2O is preferably 0% or more, 0.1% or more, 0.5 or more, and particularly 1% or more, and the upper limit of the content of K2O is preferably 50% or less, 40% or less, 30% or less, 20% or less, 15% or less, 10% or less, 5% or less, and particularly 3% or less. If the content of K2O is too high, the amount of evaporation of K2O during melting increases, which increases the environmental load, and the chemical durability of the crystallized glass is likely to decrease. It is not necessary to substantially contain K2O. However, since K2O is easily mixed in as an impurity, if it is attempted to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, K2O may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0042] MgO is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a component of crystals in crystallized glass. The content of MgO is preferably 0 to 50%. More specifically, the lower limit of the content of MgO is preferably 0% or more, 0.1% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of MgO is preferably 50% or less, 40% or less, 30% or less, 20% or less, 15% or less, 10% or less, 5% or less, and particularly 4% or less. If the content of MgO is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain MgO. However, since MgO is easily mixed in as an impurity, if MgO is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, MgO may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0043] CaO is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a component of crystals in crystallized glass. The content of CaO is preferably 0 to 50%. More specifically, the lower limit of the CaO content is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the CaO content is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the CaO content is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain CaO. However, since CaO is easily mixed in as an impurity, if CaO is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, CaO may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0044] SrO is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a component of crystals in crystallized glass. The content of SrO is preferably 0 to 50%. More specifically, the lower limit of the content of SrO is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of SrO is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of SrO is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain SrO. However, since SrO is easily mixed in as an impurity, if SrO is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, SrO may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0045] BaO is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a component of crystals in crystallized glass. The content of BaO is preferably 0 to 50%. More specifically, the lower limit of the content of BaO is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of BaO is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of BaO is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain BaO. However, since BaO is easily mixed in as an impurity, if BaO is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, BaO may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0046] ZnO is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a component of crystals in crystallized glass. The content of ZnO is preferably 0 to 50%. More specifically, the lower limit of the content of ZnO is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of ZnO is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of ZnO is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain ZnO. However, since ZnO is easily mixed in as an impurity, if ZnO is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, ZnO may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0047] ZrO2 is a component that can promote crystallization and can increase the chemical durability of crystallized glass. In some cases, it can be a constituent of crystals in crystallized glass. The content of ZrO2 is preferably 0 to 50%. More specifically, the lower limit of the content of ZrO2 is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of ZrO2 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of ZrO2 is too high, unintended crystals (devitrified particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain ZrO2. However, since ZrO2 is easily mixed in as an impurity, if ZrO2 is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, ZrO2 may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0048] HfO2 is a component that can promote crystallization and can improve the Young's modulus of crystallized glass. In some cases, it can be a constituent of crystals in crystallized glass. The content of HfO2 is preferably 0 to 50%. More specifically, the lower limit of the content of HfO2 is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of HfO2 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of HfO2 is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain HfO2. However, since HfO2 is easily mixed in as an impurity, if HfO2 is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, HfO2 may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0049] TiO2 is a component that can promote crystallization. In some cases, it can be a constituent of crystals in crystallized glass. The content of TiO2 is preferably 0 to 50%. More specifically, the lower limit of the content of TiO2 is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of TiO2 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of TiO2 is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain TiO2. However, if TiO2 is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, TiO2 may be contained at 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0050] At high temperatures, SnO2 undergoes the reaction SnO2 → SnO + 1 / 2O2, releasing O2 gas into the molten glass. This reaction is known as the fining mechanism of SnO2, and the O2 gas released during the reaction has a "defoaming effect" of enlarging tiny bubbles present in the molten glass and releasing them outside the glass system, as well as a "stirring effect" of mixing the molten glass. Furthermore, SnO2 is a component that can promote crystallization and can improve the Young's modulus of crystallized glass. In some cases, it can also be a component of the crystals in the crystallized glass. The content of SnO2 is preferably 0 to 50%. More specifically, the lower limit of the content of SnO2 is preferably 0% or more, 0.5% or more, and particularly preferably 1% or more, and the upper limit of the content of SnO2 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly preferably 5% or less. If the SnO2 content is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, making the crystallized glass and the original glass before crystallization more likely to break. It is not necessary to substantially contain SnO2. However, since SnO2 is easily mixed in as an impurity, if SnO2 is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, SnO2 may be contained in an amount of 0.0001% or more, 0.0003% or more, and especially 0.0005% or more.
[0051] V2O5 is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a constituent of crystals in crystallized glass. The content of V2O5 is preferably 0 to 50%. More specifically, the lower limit of the content of V2O5 is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of V2O5 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of V2O5 is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain V2O5. However, since V2O5 is easily mixed in as an impurity, if V2O5 is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, V2O5 may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0052] NiO is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a constituent of crystals in crystallized glass. In addition, in a reduced state, it can form an alloy with other metal elements and improve the magnetic property and strength of crystallized glass. Examples of the alloy include nickel-chromium alloy, nickel-copper alloy, and nickel-iron alloy. The content of NiO is preferably 0 to 50%. More specifically, the lower limit of the content of NiO is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of NiO is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of NiO is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain NiO. However, since NiO is easily mixed in as an impurity, if NiO is to be completely removed, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, NiO may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0053] Cr2O3 is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a constituent of crystals in crystallized glass. In addition, in a reduced state, it can form an alloy with other metal elements and improve the magnetic properties and strength of crystallized glass. Examples of alloys include nickel-chromium-molybdenum steel, chromium-molybdenum steel, and nichrome. The content of Cr2O3 is preferably 0 to 50%. More specifically, the lower limit of the content of Cr2O3 is preferably 0% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of Cr2O3 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of Cr2O3 is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain Cr2O3. However, since Cr2O3 is easily mixed in as an impurity, if one tries to completely remove Cr2O3, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, Cr2O3 may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0054] MoO3 is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a constituent of crystals in crystallized glass. In addition, in a reduced state, it can form an alloy with other metal elements to improve the magnetism and strength of crystallized glass. Examples of alloys include binary molybdenum alloys, nickel chromium molybdenum steel, chromium molybdenum steel, and nichrome. The content of MoO3 is preferably 0 to 50%. More specifically, the lower limit of the content of MoO3 is preferably 0% or more, more than 0%, 0.1% or more, 0.2% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of MoO3 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of MoO3 is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain MoO3. However, since MoO3 is easily mixed in as an impurity, if one tries to completely remove MoO3, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, MoO3 may be contained in an amount of 0.0001% or more, 0.0003% or more, and particularly 0.0005% or more.
[0055] The crystallized glass of the present invention may further contain the following components.
[0056] MnO2 is a component that reduces the viscosity of glass and improves the melting and moldability of glass. In some cases, it can be a constituent of crystals in crystallized glass. In addition, in a reduced state, it can form an alloy with other metal elements and improve the magnetism and strength of crystallized glass. Examples of alloys include ferromanganese. The content of MnO2 is preferably 0 to 50%. More specifically, the lower limit of the content of MnO2 is preferably 0% or more, 0.1% or more, 0.5% or more, and particularly 1% or more, and the upper limit of the content of MnO2 is preferably 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, and particularly 5% or less. If the content of MnO2 is too high, unintended crystals (devitrification particles) are likely to precipitate during melting and molding, and the crystallized glass or the original glass before crystallization is likely to be damaged. It is not necessary to substantially contain MnO2. However, since MnO2 is easily mixed in as an impurity, if one tries to completely remove MnO2, the raw material becomes expensive and the manufacturing cost tends to increase. Therefore, it is preferable that MnO2 is 0.0001% or more, 0.0003% or more, and especially 0.0005% or more.
[0057] Sb2O3, As2O3, and SO3 may be added as fining agents, and their contents may be 0.0001% or more, 0.0003% or more, particularly 0.0005% or more, and 1% or less, particularly 0.8% or less. From an environmental standpoint, the contents of Sb2O3 and As2O3 are preferably 0.5% or less, 0.2% or less, particularly less than 0.1%, respectively.
[0058] Cl, F, Y2O3, La2O3, WO3, Ta2O5, Nd2O3, Nb2O5, and RfO2 may be contained in a total amount of up to 30% as long as the desired characteristics are obtained. However, since the raw materials for the above components are expensive and tend to increase the manufacturing cost, it is preferable not to contain them unless there are special circumstances.
[0059] Pt is a component that can promote crystallization, but since it is a precious metal, from the viewpoint of cost reduction, its content is preferably 100 ppm or less, 50 ppm or less, 20 ppm or less, 10 ppm or less, 9 ppm or less, 8 ppm or less, 7 ppm or less, 6 ppm or less, 5 ppm or less, 4 ppm or less, 3 ppm or less, 2 ppm or less, 1.6 ppm or less, 1.4 ppm or less, 1.2 ppm or less, 1 ppm or less, 0.9 ppm or less, 0.8 ppm or less, 0.7 ppm or less, 0.6 ppm or less, 0.5 ppm or less, 0.45 ppm or less, 0.40 ppm or less, 0.35 ppm or less, and particularly 0.30 ppm or less. Note that Pt may be mixed in from the melting equipment, and if Pt is to be completely removed, the manufacturing cost may increase. Therefore, as long as the crystallized glass of the present invention can obtain desired characteristics, the lower limit of the Pt content is preferably 0.0001 ppm or more, 0.001 ppm or more, 0.005 ppm or more, 0.01 ppm or more, 0.02 ppm or more, 0.03 ppm or more, 0.04 ppm or more, 0.05 ppm or more, 0.06 ppm or more, and particularly 0.07 ppm or more. When Pt is made to function as a crystallization promoter, Pt may be used alone or may be combined with other components. When Pt is used as a crystallization promoter, the form of Pt is not particularly important. For example, the form of Pt may be colloidal or metal crystal.
[0060] Rh is a component that can promote crystallization, but since it is a precious metal, from the viewpoint of cost reduction, its content is preferably 100 ppm or less, 50 ppm or less, 20 ppm or less, 10 ppm or less, 9 ppm or less, 8 ppm or less, 7 ppm or less, 6 ppm or less, 5 ppm or less, 4 ppm or less, 3 ppm or less, 2 ppm or less, 1.6 ppm or less, 1.4 ppm or less, 1.2 ppm or less, 1 ppm or less, 0.9 ppm or less, 0.8 ppm or less, 0.7 ppm or less, 0.6 ppm or less, 0.5 ppm or less, 0.45 ppm or less, 0.40 ppm or less, 0.35 ppm or less, and particularly 0.30 ppm or less. Note that Rh may be mixed in from the melting equipment, and if Rh is to be completely removed, the manufacturing cost may increase. Therefore, the lower limit of the content of Rh is preferably 0.0001 ppm or more, 0.001 ppm or more, 0.005 ppm or more, 0.01 ppm or more, 0.02 ppm or more, 0.03 ppm or more, 0.04 ppm or more, 0.05 ppm or more, 0.06 ppm or more, and particularly 0.07 ppm or more. When Rh is made to function as a crystallization promoter, Rh may be used alone or may be combined with other components. When Rh is used as a crystallization promoter, the form of Rh is not particularly important. For example, the form of Rh may be colloidal or metal crystal.
[0061] The crystallized glass of the present invention may contain trace components such as H2, CO2, CO, H2O, He, Ne, Ar, and N2 up to less than 0.1% each, so long as the desired properties are obtained.
[0062] As, Sb, Ag, Au, Pd, Ir, V, Cr, Sc, Ce, Pr, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Ac, Th, Pa, and U tend to increase the raw material cost and the manufacturing cost when intentionally added. Therefore, the content of the above components is preferably 10% or less, 5% or less, 3% or less, 1% or less, 0.5% or less, 0.3% or less, 0.1% or less, 500 ppm or less, 300 ppm or less, 100 ppm or less, and particularly 10 ppm or less. On the other hand, when glass containing Ag, Au, etc. is irradiated with light or heat treated, aggregates of these components are formed, and crystallization can be promoted from the starting point. In addition, Pd, etc. have various catalytic effects, and by containing them, it is possible to impart unique functions to the crystallized glass. In view of these circumstances, when the purpose is to promote crystallization or to impart other functions, the above components may be contained in an amount of 0.1% or more, 0.2% or more, and particularly 0.5% or more.
[0063] From the viewpoint of improving the meltability and moldability of glass, it is preferable to control the total amount of SnO2, Fe2O3, V2O5, NiO, Cr2O3, and MoO3. More specifically, in the crystallized glass of the present invention, SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3 is preferably 20% or more, 21% or more, 23% or more, 25% or more, and particularly preferably 30% or more. The upper limit is not particularly limited, but may be 90% or less, 80% or less, 70% or less, 60% or less, and particularly 55% or less.
[0064] Li2O, Na2O, and K2O are components that reduce the viscosity of glass and improve the melting and moldability of glass. Here, when the content of K cations increases, the Young's modulus and rigidity modulus of the crystallized glass tend to decrease, and the crystallized glass tends to break during processing. On the other hand, the raw material of K2O is cheaper than Li2O. In addition, when K2O is contained together with Li2O and Na2O, the diffusion of Li cations and Na cations in the remaining glass of the crystallized glass is less likely to occur, and as a result, the chemical durability of the crystallized glass may be improved. In order to manufacture efficiently and inexpensively and prevent unintended breakage and deterioration of chemical durability, it is preferable to control K2O / (Li2O+Na2O+K2O). More specifically, the mass % ratio of K2O / (Li2O+Na2O+K2O) is preferably 0.01 to 0.99, 0.01 to 0.95, 0.01 to 0.90, 0.01 to 0.85, or 0.01 to 0.80, and particularly preferably 0.01 to 0.75.
[0065] By the way, when the crystallized glass is used as a soil conditioner described later, the remaining glass portion may be scratched when blended with soil, and the scratch may cause breakage. In general, in glass having many open spaces (also called voids or free volume) in the glass network, energy is consumed by structural changes in the open spaces, so scratches are unlikely to progress. From the viewpoint of providing such open spaces in the glass network, it is preferable that the crystallized glass contains SiO2 and / or P2O5. On the other hand, the higher the hardness of the glass, the less likely it is to be scratched, so from the viewpoint of reducing the open spaces in the glass network, it is preferable that the crystallized glass contains Al2O3. That is, it is preferable to control (SiO2+P2O5) / (SiO2+Al2O3+P2O5) in the crystallized glass of the present invention from the viewpoint of making it difficult to be scratched and difficult to break even if the remaining glass is scratched. More specifically, the mass % ratio (SiO2+P2O5) / (SiO2+Al2O3+P2O5) is preferably 0.01 to 0.99, 0.1 to 0.99, 0.2 to 0.99, 0.3 to 0.99, 0.4 to 0.99, 0.5 to 0.99, 0.6 to 0.99, and particularly preferably 0.7 to 0.99.
[0066] However, when crystals precipitate from the raw glass, the distribution of components in the raw glass may become biased. Hereinafter, the state in which the bias occurs is referred to as a phase separation state. By controlling this phase separation state, crystallization can be promoted efficiently. For example, the phase separation state is likely to be divided into a region rich in SiO2, which is the main glass skeleton, and a region rich in components other than SiO2. In particular, glass containing B2O3, P2O5, ZrO2, HfO2, TiO2, and SnO2 is prone to phase separation, so from the viewpoint of efficiently promoting crystallization, it is preferable to control SiO2 / (B2O3+P2O5+ZrO2+HfO2+TiO2+SnO2). More specifically, the mass % ratio of SiO2 / (B2O3+P2O5+ZrO2+HfO2+TiO2+SnO2) is preferably 0.1 to 10,000, 0.1 to 8,000, 0.1 to 6,000, 0.1 to 5,000, 0.2 to 5,000, and particularly preferably 0.2 to 4,000.
[0067] From the viewpoint of stable melting and forming of glass, it is preferable to control SiO2 / (MgO+CaO+SrO+BaO+ZnO). More specifically, SiO2 / (MgO+CaO+SrO+BaO+ZnO) of the crystallized glass of the present invention is preferably 0.1-10000, 0.1-8500, 0.1-5000, 0.1-3000, 0.1-1000, 0.5-1000, and particularly preferably 1-100.
[0068] From the viewpoint of suppressing the deterioration of the crystallized glass and the elution of the constituent components, it is preferable to control SiO2 / (SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3). More specifically, the crystallized glass of the present invention preferably has SiO2 / (SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3) of 0.01-10, 0.1-8, 0.3-5, and particularly 0.5-3.
[0069] In the crystallized glass of the present invention, the β-OH value of the raw glass before crystallization is preferably more than 0 to 2 / mm. More specifically, the lower limit of the β-OH value is preferably more than 0, 0.01 / mm or more, 0.02 / mm or more, 0.03 / mm or more, 0.04 / mm or more, 0.05 / mm or more, 0.06 / mm or more, 0.07 / mm or more, 0.08 / mm or more, 0.09 / mm or more, and particularly 0.1 / mm or more. In addition, the upper limit of the β-OH value is preferably 2 / mm or less, 1.5 / mm or less, 1.4 / mm or less, and particularly 1.3 / mm or less. When the β-OH value is within the above range, the quality of the glass is unlikely to deteriorate. That is, when the β-OH value is too small, the amount of water vapor generated when melting the glass batch is reduced. Therefore, the stirring action of the glass batch due to the generation of water vapor is reduced, making it difficult to promote the initial reaction, and the manufacturing load is likely to increase. If the β-OH value is too large, bubbles are likely to occur at the interface between the molten glass and metal members such as Pt or refractory members, which may result in unintended voids in the crystallized glass and a decrease in strength. In addition, the linear thermal expansion coefficient of the crystallized glass increases, which may deteriorate the heat resistance and thermal shock resistance, making it unsuitable for use at high temperatures.
[0070] The crystallized glass of the present invention has an absolute value of Seebeck coefficient of 0.000001V / K or more, 0.000005V / K or more, 0.00001V / K or more, 0.00002V / K or more, 0.00003V / K or more, 0.00004V / K or more, 0.00005V / K or more, particularly 0.00006V / K or more at any one or more temperature points of 25°C to 400°C. For example, it is preferable that the absolute value of the Seebeck coefficient satisfies the above value at 25°C, 100°C, 200°C or 400°C. By the absolute value of the Seebeck coefficient satisfying the above value, the thermoelectric conversion index ZT can be increased, and the thermoelectric conversion efficiency can be increased. In addition, when thermoelectric conversion occurs at 25°C to 400°C, it becomes possible to generate electricity in various places such as the ocean, rivers, mountainous areas, desert areas, residential areas, and space. Furthermore, it is possible to generate electricity by utilizing body heat, exhaust heat from automobiles and electronic devices, etc. There is no particular upper limit to the absolute value of the Seebeck coefficient, but it may be, for example, 0.0001 V / K or less.
[0071] The crystallized glass of the present invention preferably has a thermoelectric conversion index ZT of 0.00001 or more, 0.00005 or more, 0.0001 or more, particularly 0.0002 or more at any one or more temperature points between 25°C and 400°C. For example, it is preferable that the thermoelectric conversion index ZT satisfies the above value at 400°C. The crystallized glass having the thermoelectric conversion index ZT satisfies the above value is suitable as a thermoelectric conversion material. The upper limit of the thermoelectric conversion index ZT is not particularly limited, but may be, for example, 0.01 or less, particularly 0.001 or less. The thermoelectric conversion index ZT is expressed by the following formula.
[0072] ZT=S 2 ×σ / κ Here, S is the Seebeck coefficient [V / K], σ is the electrical conductivity [S / m], and κ is the thermal conductivity [W / m K].
[0073] The crystallized glass of the present invention has a carrier mobility of 0.0001 cm 2 / Vs or more, 0.001cm 2 / Vs or more, 0.01cm 2 / Vs or more, especially 0.1 cm 2 / Vs or more. Glass-ceramics with carrier mobility that satisfies the above value are useful for producing semiconductor members with higher performance. The upper limit of carrier mobility is not particularly limited, but is, for example, 1 cm 2 / Vs or less.
[0074] The crystallized glass of the present invention has a thermal expansion coefficient of 200×10 -7 / ℃ or less, 180×10 -7 / ℃ or less, 150×10 -7 / ℃ or less, 120×10 -7 / ℃ or less, 100×10 -7 / ℃ or less, especially 98×10 -7 The lower limit of the thermal expansion coefficient is preferably, but not limited to, for example, 50×10 -7 / °C or more. The thermal expansion coefficient at 30 to 380°C may be 200×10 -7 / ℃ or less, 180×10 -7 / ℃ or less, 150×10 -7 / ℃ or less, 120×10 -7 / ℃ or less, 100×10 -7 / ℃ or less, especially 98×10 -7 The lower limit of the thermal expansion coefficient is preferably, but not limited to, for example, 50×10 -7 / °C or more.
[0075] The glass-ceramics of the present invention are treated as a substitute for the softening point, with the glass transition temperature Tg being the temperature at which the gradient of the thermal expansion curve of the glass before crystallization changes. The glass transition temperature Tg is preferably 450°C or higher, 460°C or higher, 470°C or higher, 480°C or higher, 490°C or higher, 500°C or higher, 510°C or higher, and particularly 520°C or higher in the state of the glass before crystallization. If the glass transition temperature Tg is too low, the glass will flow too much during crystallization, making it difficult to mold into a desired shape. The upper limit of the glass transition temperature Tg may be, for example, 700°C or lower. In addition, the yield point Tf is preferably 900°C or lower, 850°C or lower, 800°C or lower, and particularly 780°C or lower. If the yield temperature of the glass-ceramics exceeds 900°C, it becomes difficult to soften by reheating, and the accuracy of softening processing such as bending processing is likely to decrease. The lower limit of the yield point Tf may be, for example, 500°C or higher, 520°C or higher, and particularly preferably more than 520°C.
[0076] The crystallized glass of the present invention has a density of 2.4 to 4 g / cm3 after crystallization. 3 , 2.5~3.8g / cm 3 , 2.6~3.6g / cm 3 , especially 2.7 to 3.5 g / cm 3 It is preferable that the density of the crystallized glass is too low, the density of the crystallized glass is too low for the soil particles, and it is difficult to mix uniformly into the soil. On the other hand, if the density of the crystallized glass is too high, the weight per unit area becomes large, and it becomes difficult to handle. The density of the crystallized glass is also an index for judging whether the glass is sufficiently crystallized. Specifically, the greater the density difference between the original glass and the crystallized glass, the more the crystallization has progressed.
[0077] The crystallized glass of the present invention preferably has a crystallinity of 1% or more, 5% or more, 10% or more, 20% or more, particularly 25% or more. If the crystallinity is too low, the mechanical strength tends to decrease. The upper limit of the crystallinity is not particularly limited, but may be, for example, 80% or less, 70% or less, particularly 60% or less. Here, the "crystallinity" can be evaluated by a powder method using an X-ray diffractometer (Rigaku RINT-2100). For example, after calculating the area of the halo corresponding to the mass of the amorphous material and the area of the peak corresponding to the mass of the crystal, it can be obtained by the formula [peak area] x 100 / [peak area + halo area] (%).
[0078] The crystal grain size of the crystallized glass of the present invention is preferably 1000nm or less, 800nm or less, 500nm or less, 400nm or less, 300nm or less, particularly 200nm or less. This makes it easier to lower the thermal expansion coefficient of the crystallized glass. The crystal grain size can be evaluated using, for example, analysis software installed in an X-ray diffractometer (Rigaku's fully automatic multipurpose horizontal X-ray diffractometer Smart Lab).
[0079] The Young's modulus of the crystallized glass of the present invention is preferably 60 to 120 GPa, 70 to 110 GPa, 75 to 110 GPa, or 75 to 100 GPa, particularly preferably 75 to 95 GPa. If the Young's modulus is too low or too high, the mechanical strength of the crystallized glass is likely to decrease.
[0080] The crystallized glass of the present invention preferably has a modulus of rigidity of 25 to 40 GPa, 28 to 40 GPa, particularly preferably 30 to 40 GPa. If the modulus of rigidity is too low or too high, the mechanical strength of the crystallized glass is likely to decrease.
[0081] The crystallized glass of the present invention preferably has a Poisson's ratio of 0.35 or less, 0.32 or less, 0.3 or less, 0.28 or less, 0.26 or less, and particularly preferably 0.25 or less.If the Poisson's ratio is too large, the mechanical strength of the crystallized glass is easily reduced.The lower limit of the Poisson's ratio is not particularly limited, but may be, for example, 0.15 or more.
[0082] The crystallized glass of the present invention has an electric resistance of 100,000 Ω·m or less, preferably 10,000 Ω·m or less, 5,000 Ω·m or less, 1000 Ω·m or less, 500 Ω·m or less, 100 Ω·m or less, 50 Ω·m or less, 10 Ω·m or less, 5 Ω·m or less, 4 Ω·m or less, and particularly preferably Ω·m or less. Because of its low electric resistance, the crystallized glass of the present invention can be suitably used as a material for thermoelectric conversion members, semiconductor members, communication members, etc., in addition to being used as a heavy metal recovery material for adsorbing and recovering heavy metals and the like and as a soil improver.
[0083] The crystallized glass of the present invention preferably has carrier type of ion, electron, hole, or combination thereof.In particular, when the crystallized glass of the present invention is used as a material for thermoelectric conversion, semiconductor, communication, building, chemical reaction, heat-resistant, space, medical, etc., it is preferably has carrier type of electron, hole, or combination thereof, which are easily increased in electrical conductivity.
[0084] The crystallized glass of the present invention has a Hall coefficient of 0.0001 cm 3 / C or more, 0.0005cm 3 / C or more, 0.001cm 3 / C or more, 0.005cm 3 / C or more, 0.01cm 3 / C or more, 0.05cm 3 / C or more, 0.1cm 3 / C or more, especially 0.5cm 3 / C or more. This makes it easier to use the crystallized glass of the present invention as a material for thermoelectric conversion members, semiconductor members, communication members, building members, chemical reaction members, heat-resistant members, space members, medical members, etc.
[0085] The crystallized glass of the present invention has a carrier concentration of 1×10 15 / cm 3 , 5×10 15 / cm 3 , 1×10 16 / cm 3 , 5×10 16 / cm3 , 1×10 17 / cm 3 , 5×10 17 / cm 3 , especially 1×10 18 / cm 3 It is preferable that the sheet carrier concentration is 1×10 15 / cm 2 , 5×10 15 / cm 2 , 1×10 16 / cm 2 , 5×10 16 / cm 2 , especially 1×10 17 / cm 2 By doing so, the crystallized glass of the present invention can be easily used as a material for thermoelectric conversion members, semiconductor members, communication members, building members, chemical reaction members, heat-resistant members, space members, medical members, etc.
[0086] The crystallized glass of the present invention has a saturation magnetization of 0.5 emμ / cm 3 More than 1<em>μ / cm 3 More than 5<em>μ / cm 3 More than 10emμ / cm 3 More than 15emμ / cm 3 More than 20emμ / cm 3 More than 25emμ / cm 3 More than 30emμ / cm 3 Above, 35emμ / cm 3 Above 40emμ / cm 3 By doing so, after the crystallized glass of the present invention is dispersed in soil or the like, the crystallized glass of the present invention can be easily collected with a magnet or the like.
[0087] The crystallized glass of the present invention has a liquidus temperature of 1540°C or less, 1535°C or less, 1530°C or less, 1525°C or less, 1520°C or less, 1515°C or less, 1510°C or less, 1505°C or less, 1500°C or less, 1495°C or less, 1490°C or less, 1485°C or less, 1480°C or less, 1475°C or less, 1470°C or less, 1465°C or less, 1460°C or less, 1455°C or less, 1450°C or less, 1445°C or less, 1440°C or less, 1435°C or less, 1430°C or less, 1425°C or less, 1420°C or less, 1415°C or less, and particularly 1410°C or less. If the liquidus temperature is too high, it is likely to devitrify during production. Furthermore, if the liquidus temperature is 1480°C or lower, production by a roll method or the like becomes easy, if it is 1450°C or lower, production by a casting method or the like becomes easy, and if it is 1410°C or lower, production by a fusion method or the like becomes easy, so these are preferable.
[0088] The crystallized glass of the present invention has a liquidus viscosity (logarithm of viscosity corresponding to liquidus temperature) of 1.70 or more, 1.75 or more, 1.80 or more, 1.85 or more, 1.90 or more, 1.95 or more, 2.00 or more, 2.05 or more, 2.10 or more, 2.15 or more, 2.20 or more, 2.25 or more, 2.30 or more, 2.35 or more, 2.40 or more, 2.45 or more, 2.50 or more, 2.55 or more, 2.60 or more , 2.65 or more, 2.70 or more, 2.75 or more, 2.80 or more, 2.85 or more, 2.90 or more, 2.95 or more, 3.00 or more, 3.05 or more, 3.10 or more, 3.15 or more, 3.20 or more, 3.25 or more, 3.30 or more, 3.35 or more, 3.40 or more, 3.45 or more, 3.50 or more, 3.55 or more, 3.60 or more, 3.65 or more, and particularly 3.70 or more are preferable. If the liquidus viscosity is too low, devitrification is likely to occur during production. On the other hand, if the liquidus viscosity is 3.40 or more, production by the roll method or the like is easy, if it is 3.50 or more, production by the casting method or the like is easy, and if it is 3.70 or more, production by the fusion method or the like is easy, which is preferable.
[0089] <Method of manufacturing crystallized glass> The production of the crystallized glass of the present invention preferably includes a melting step of melting a mixture of glass raw materials and Fe2O3 raw materials, and a crystallization step of forming the molten glass into a predetermined shape to obtain crystallized glass.
[0090] First, a mixture of glass raw materials and Fe2O3 raw materials is melted (melting process). For example, the mixture can be placed in a crucible and melted in an electric furnace at 1000 to 2000°C for 3 to 5 hours. Note that glass melting is not limited to the above method, and flame melting using a burner or the like, melting by laser irradiation, melting by plasma, etc. can be used as appropriate.
[0091] As the glass raw material, it is preferable to use glass cullet. The type of glass cullet is not particularly limited as long as the desired glass composition can be obtained, but for example, glass cullet of residential window glass, vehicle window glass, display glass, fiber glass, architectural glass, optical glass, pharmaceutical and medical glass, semiconductor material glass, and solar cell support glass is preferably used as the raw material. Since the above glass is required to have an improved recycling rate, the use of glass cullet made of the above glass can particularly contribute to the recycling and upcycling of glass. However, instead of using glass cullet, powder raw materials such as oxides, hydroxides, carbonates, and nitrates may be mixed to form the glass raw material. Also, a mixture of powder raw materials and glass cullet may be used as the glass raw material. As the Fe2O3 raw material, it is preferable to use Fe2O3 powder raw material.
[0092] Next, the molten glass is formed into a predetermined shape to obtain crystallized glass (crystallization step). At this time, the molten glass may be crystallized at the same time as cooling, or after obtaining glass (raw glass) solidified into a predetermined shape, the raw glass may be heat-treated to crystallize. The glass melt may be held at a high temperature (1000°C or higher) to crystallize. The shape of the crystallized glass and the raw glass is not particularly limited, and may be, for example, plate-like, fibrous, film-like, block-like, powder-like, spherical, or hollow. For example, a crystallized glass sample may be obtained by performing heat treatment at less than 300 to 1000°C and then slowly cooling. Either heat treatment may be performed only at a certain temperature, or may be performed stepwise by holding at two or more levels of temperature, or may be performed while applying a temperature gradient. Crystallization may be promoted by applying or irradiating sound waves or electromagnetic waves.
[0093] When it is desired to obtain sufficient thermal shock resistance, it is preferable to control the cooling rate to sufficiently relax the structure of the remaining glass phase.For example, the average cooling rate from 800°C to 25°C is preferably 100000°C / h, 50000°C / h, 20000°C / h, 10000°C / h, 5000°C / h, 2000°C / h, 1000°C / h, 500°C / h, 300°C / h, 100°C / h, 50°C / h, 20°C / h, 15°C / h, 10°C / h, 5°C / h, 3°C / h, 2°C / h, 1°C / h, 0.5°C / h, and particularly 0.1°C / h, in the inner part of the thickness that is the furthest from the surface of the crystallized glass. In addition, when dimensional stability over a long period of time is desired, it is further preferably 0.05°C / h or less, 0.01°C / h or less, 0.005°C / h or less, 0.001°C / h or less, 0.0005°C / h or less, and particularly preferably 0.0001°C / h or less. Except for the case of physical strengthening treatment by air cooling, water cooling, etc., it is desirable that the cooling rate of the crystallized glass is close to the cooling rate from the surface to the part of the inner thickness farthest from the surface. The value obtained by dividing the cooling rate of the part of the inner thickness farthest from the surface by the cooling rate of the surface is preferably 0.0001 to 1, 0.001 to 1, 0.01 to 1, 0.1 to 1, 0.5 to 1, 0.8 to 1, 0.9 to 1, and particularly preferably 1. By being close to 1, residual strain is unlikely to occur at all positions of the crystallized glass, and long-term dimensional stability is easily obtained. The cooling rate of the surface can be estimated using a contact thermometer or a radiation thermometer, and the internal temperature can be estimated by placing the high-temperature crystallized glass in a cooling medium and measuring the heat quantity and rate of heat change of the cooling medium, and then using this numerical data and the specific heat and thermal conductivity of the crystallized glass and the cooling medium.
[0094] The crystallized glass of the present invention is not limited to the above-mentioned manufacturing method. For example, the mixture may be melted by irradiating laser while floating. For example, the mixture may be melted in a continuous furnace that combines burner heating and electric heating. For example, the up-draw method, down-draw method, slit method, overflow (fusion) method or hand-blowing method may be used. In addition, the glass melt may be poured onto a liquid with a high specific gravity, and the glass composition may be solidified into a plate shape.
[0095] The crystallized glass of the present invention may be subjected to chemical strengthening. The processing conditions of the chemical strengthening process may be appropriately selected, such as the processing time and processing temperature, taking into consideration the glass composition, the degree of crystallization, the type of molten salt, and the like. For example, a glass composition containing a large amount of Na2O that may be contained in the remaining glass may be selected, or the degree of crystallization may be intentionally reduced, so that chemical strengthening after crystallization is easier. In addition, the molten salt may contain an alkali metal such as Li, Na, or K alone or in combination. Furthermore, in addition to the usual one-stage strengthening, multi-stage chemical strengthening may be selected.
[0096] <Heavy metal recovery material> The crystallized glass of the present invention can be suitably used as a heavy metal recovery material. In other words, the heavy metal recovery material of the present invention is characterized by being made of crystallized glass containing 20-80% Fe2O3 by mass % and containing magnetic crystals. By containing a large amount of Fe2O3 in this way, the crystallized glass of the present invention can adsorb heavy metals. The heavy metal is not particularly limited, but can be used as a recovery material for, for example, cadmium, arsenic, chromium, copper or lead.
[0097] The form of the heavy metal recovery material is not particularly limited, and may be, for example, powder, granules, small pieces, etc. In particular, from the viewpoint of widening the contact area with the heavy metal, a powder form is preferable. The average particle size (D50) of the heavy metal recovery material is preferably, for example, 10 to 200 μm. Here, the "average particle size D50" refers to a value measured by a laser diffraction device, and represents the particle size at which the integrated amount is 50% accumulated from the smallest particle in a volume-based cumulative particle size distribution curve measured by a laser diffraction method.
[0098] The amount of the heavy metal recovery material added to the heavy metal recovery source is, by weight, preferably 0.1% or more, 0.5% or more, 1% or more, particularly preferably 2% or more, and preferably 10% or less, 8% or less, particularly preferably 5% or less. If the amount of the heavy metal recovery material added is too small, the heavy metal recovery effect cannot be sufficiently obtained. If the amount added is too large, the recovery cost increases. Examples of the heavy metal recovery source include soil and heavy metal-containing liquid.
[0099] <Soil conditioner> The crystallized glass of the present invention can be particularly preferably used as a soil conditioner. In other words, the soil conditioner of the present invention is characterized by being composed of crystallized glass containing 20-80% Fe2O3 by mass % and containing magnetic crystals. As described above, the crystallized glass of the present invention contains magnetic crystals, so it is attracted to a magnet. In addition, since it contains a large amount of Fe2O3, it can effectively adsorb heavy metals. Therefore, when the crystallized glass of the present invention is spread in soil as a soil conditioner, it can be adsorbed and collected using a magnet. Specifically, the method for recovering heavy metals of the present invention is characterized by comprising an adsorption step of adsorbing heavy metals to the crystallized glass containing magnetic crystals, and a recovery step of recovering the crystallized glass after adsorption of the heavy metals with a magnet. In particular, it can be preferably used for recovering heavy metals in soil.
[0100] The crystallized glass of the present invention is not limited to the use of heavy metal recovery material and soil modifier.For example, the crystallized glass of the present invention can be suitably used as water quality improvement material, ion exchange material, adsorbent, and fertilizer additive.In addition, the crystallized glass of the present invention can be suitably used as thermoelectric conversion material, semiconductor material, communication material, building material, chemical reaction material, heat-resistant material, space material, medical material, etc. EXAMPLES
[0101] The present invention will be described below based on examples, but the present invention is not limited to the following examples.
[0102] Tables 1 and 2 show examples (Examples 1 to 9) of the present invention.
[0103] [Table 1]
[0104] [Table 2]
[0105] The samples were prepared as follows. First, Fe2O3 powder raw material and glass cullet were mixed to prepare glass raw material. The obtained glass raw material was melted at 1500°C for 4 hours and then rolled to a thickness of 5 mm. In Examples 1 to 5 and 7 to 9, the molten glass was crystallized when rolled. After roll forming, the glass was annealed at 400°C for 3 hours using a slow cooling furnace and slowly cooled to room temperature at 100°C / h to obtain a crystallized glass sample. In Example 6, the solidified raw glass after slow cooling was placed in an electric furnace heated to 900°C and held for 5 hours to crystallize. After crystallization, the glass was annealed at 400°C for 3 hours and slowly cooled to room temperature at 100°C / h to obtain a crystallized glass sample. In Table 1, Sn+Fe+V+Ni+Cr+Mo means SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3. K / (Li+Na+K) means K2O / (Li2O+Na2O+K2O). (Si+P) / (Si+Al+P) means (SiO2+P2O5) / (SiO2+Al2O3+P2O5). Si / (B+P+Zr+Hf+Ti+Sn) means SiO2 / (B2O3+P2O5+ZrO2+HfO2+TiO2+SnO2). Si / (Mg+Ca+Sr+Ba+Zn) means SiO2 / (MgO+CaO+SrO+BaO+ZnO). Si / (Sn+Fe+V+Ni+Cr+Mo) means SiO2 / (SnO2+Fe2O3+V2O5+NiO+Cr2O3+MoO3).
[0106] The composition of the samples was analyzed as follows. The Pt and Rh contents were analyzed using an ICP-MS device (Agilent8800, manufactured by AGILEINT TECHNOLOGY). First, the prepared glass samples were crushed and wetted with pure water, and then perchloric acid, nitric acid, sulfuric acid, and hydrofluoric acid were added appropriately to melt them. The Pt and Rh contents of the samples were then measured using ICP-MS. The Pt and Rh contents of each measurement sample were determined based on a calibration curve prepared using a previously prepared Pt and Rh solution with known concentrations. The measurement mode was Pt:He gas / HMI (low mode) and Rh:HEHe gas / HMI (medium mode), and the mass numbers were Pt:198 and Rh:103. The Li2O content of the prepared samples was analyzed using an atomic absorption spectrometer (ContrAA600, manufactured by Analytik Jena). The flow of the melting of the glass samples and the use of the calibration curves were basically the same as those for the Pt and Rh analysis. Other components were measured by ICP-MS or atomic absorption spectrometry in the same way as Pt, Rh, and Li2O, or a glass sample with a known concentration that had been previously examined using an ICP-MS or atomic absorption spectrometry was used as a calibration curve sample, and a calibration curve was then created using an XRF analyzer (RIGAKU ZSX PrimusIV), after which the actual content of each component was determined from the XRF analysis value of the measured sample based on the calibration curve. During the XRF analysis, the tube voltage, tube current, exposure time, etc. were adjusted as necessary depending on the component being analyzed. Table 1 shows the analytical values of each sample.
[0107] The β-OH value can be measured using glass before crystallization. Since the crystallized glass of the present application contains Fe2O3 so as to crystallize, it is not easy to determine the β-OH value of the glass before crystallization. Therefore, in the present invention, glasses not containing Fe2O3 in each practical example are produced using the same raw material composition and manufacturing process, and their β-OH value is used and treated as the β-OH value before crystallization in the examples. The β-OH value was determined by measuring the transmittance of the glass using an infrared spectrophotometer (FT-IR Frontier manufactured by Perkin Elmer) and using the following formula. The scanning speed was 100 μm / min, and the sampling pitch was 1 cm. -1 The number of scans was 10 per measurement.
[0108] β-OH value = (1 / X) log(T1 / T2) X: Glass thickness T1: Transmittance at reference wave number 3846 cm-1 T2: Minimum transmittance at OH group absorption wave number around 3600 cm-1
[0109] The thermal expansion coefficient was measured in the temperature ranges of 30 to 300°C and 30 to 380°C using crystallized glass samples processed to 20mm x 3.8mmφ. A NETZSCH dilatometer was used for the measurements. The glass transition point (Tg) and yield point (Tf) of the crystallized glass were measured by calculating the temperature at which the slope of the thermal expansion changed in each thermal expansion curve.
[0110] The density was evaluated by the Archimedes method.
[0111] The precipitated crystals were evaluated using an X-ray diffractometer (Spectris Aeris). The scan mode was 2θ / θ measurement, the scan type was continuous scan, the scattering slit width was 9 mm, the divergence slit width was 1 / 4°, the receiving slit was open, the measurement range was 5 to 60°, the measurement step was 0.01°, and the scan speed was 1.5° / min. The main crystals and the crystal grain size were evaluated using the analysis software installed in the package of the same model.
[0112] The degree of crystallinity was evaluated by the powder method using an X-ray diffractometer (Rigaku RINT-2100). Specifically, the area of the halo corresponding to the amorphous mass and the area of the peak corresponding to the crystalline mass were calculated, and then the crystallinity was calculated using the formula [peak area] × 100 / [peak area + halo area] (%).
[0113] The Young's modulus, rigidity modulus and Poisson's ratio were measured at room temperature using a free resonance type elastic modulus measuring device (JE-RT3 manufactured by Nippon Technoplus) for plate samples (40 mm x 20 mm x 20 mm) whose surfaces had been polished with a polishing solution containing dispersed No. 1200 alumina powder.
[0114] The Seebeck coefficient and electrical resistance were measured in a low-pressure helium atmosphere using a thermoelectric property evaluation device ZEM-3 manufactured by Advance Riko Co., Ltd. The thermoelectric conversion index ZT was calculated by the following formula.
[0115] ZT=S 2 ×σ / κ Here, S is the Seebeck coefficient [V / K], σ is the electrical conductivity [S / m], and κ is the thermal conductivity [W / m K].
[0116] The carrier species, Hall coefficient, carrier concentration, sheet carrier concentration, and carrier mobility were measured at room temperature using a ResiTest8308 manufactured by Toyo Corporation, assuming a single carrier system.
[0117] The saturation magnetization was measured at room temperature using a vibrating sample magnetometer VSM manufactured by Toei Kogyo Co., Ltd.
[0118] In order to evaluate the adsorption capacity of heavy metals, etc., the amount of cadmium adsorption from a pseudo-contaminated aqueous solution was measured using a cadmium aqueous solution. First, the crystallized glass sample of Example 4 was crushed and sieved to 53 to 150 μm to prepare a powder sample. In addition, a cadmium standard solution (Cd 1000) manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. was diluted with pure water to prepare a 10 ppm cadmium aqueous solution of pH 7. 5 g of the powder sample was added to 200 mL of the 10 ppm cadmium aqueous solution, and the mixture was stirred at room temperature for 3 hours. Thereafter, the cadmium aqueous solution and the powder sample were separated using a funnel and filter paper, and the cadmium ion concentration in the filtered cadmium aqueous solution was analyzed using an ICP-MS device (Agilent8800 manufactured by AGILEINT TECHNOLOGY). The cadmium ion concentration after the test was divided by the cadmium ion concentration before the test (10 ppm) and multiplied by 100 to evaluate the amount of cadmium adsorption.
[0119] As is clear from Table 2, the crystallized glass samples of Examples 1 to 9 contained magnetic crystals. More specifically, the magnetic crystals contained magnetite (Fe3O4), maghemite (γ-Fe2O3), (Fe2O3)10.6667[γ-Fe2O3], Na 0.75 Ca 0.25Glass-ceramic samples containing Fe(Si2O6) were obtained. The saturation magnetization was 0.7-54.9 emu / cm 2 In Example 4, the amount of Cd adsorbed from the simulated contaminated aqueous solution was 1%.
[0120] In Example 5, the thermoelectric conversion index ZT was 0.0002. [Industrial Applicability]
[0121] The crystallized glass of the present invention can be suitably used as a heavy metal recovery material for adsorbing and recovering heavy metals and the like, and as a soil improver. The crystallized glass of the present invention can also be suitably used as a water quality improvement material, an ion exchange material, an adsorbent, and a fertilizer additive. Furthermore, since the crystallized glass of the present invention can have both a thermoelectric conversion function and electrical conductivity, it can be suitably used as a material for thermoelectric conversion members, semiconductor members, communication members, building members, chemical reaction members, heat-resistant members, space members, medical members, and the like. Furthermore, since the crystallized glass of the present invention can be produced using glass cullet, it can contribute to the recycling and upcycling of glass products and the realization of a sustainable society.
Claims
1. In mass%, Fe 2 O 3 A crystallized glass containing 20 to 80% magnetic crystals.
2. The crystallized glass further comprises, in mass %, SiO 2 0-80%, Al 2 O 3 0-80%, B 2 O 3 0-80%, P 2 O 5 0-80%, Li 2 O 0-50%, Na 2 O 0-50%, K 2 O 0-50%, MgO 0-50%, CaO 0-50%, SrO 0-50%, BaO 0-50%, ZnO 0-50%, ZrO 2 0-50%, HfO 2 0-50%, TiO 2 0-50%, SnO 2 0-50%, V 2 O 5 0-50%, NiO 0-80%, Cr 2 O 3 0-80%, MoO 3 The crystallized glass according to claim 1, containing 0 to 80%.
3. In mass%, SnO 2 +Fe 2 O 3 +V 2 O 5 +NiO+Cr 2 O 3 +MoO 3 The crystallized glass according to claim 1 or 2, containing 20% or more of ZnO.
4. In terms of mass percentage, K 2 O / (Li 2 O+Na 2 O+K 2 3. The crystallized glass according to claim 1, wherein O) is 0.01 to 0.
99.
5. In terms of mass percentage, (SiO 2 +P 2 O 5 ) / (SiO 2 +Al 2 O 3 +P 2 O 5 3. The crystallized glass according to claim 1, wherein the value of n is 0.01 to 0.
99.
6. In terms of mass percentage, SiO 2 / (B 2 O 3 +P 2 O 5 + ZrO 2 + HfO 2 + TiO 2 + SnO 2 3. The crystallized glass according to claim 1, wherein n is 0.1 to 10,000.
7. In terms of mass percentage, SiO 2 3. The crystallized glass according to claim 1, wherein / (MgO+CaO+SrO+BaO+ZnO) is 0.1 to 10,000.
8. In terms of mass percentage, SiO 2 / (SnO 2 +Fe 2 O 3 +V 2 O 5 + NiO + Cr 2 O 3 +MoO 3 3. The crystallized glass according to claim 1, wherein n is 0.01 to 10.
9. In mass%, MoO 3 The crystallized glass according to claim 1 or 2, containing more than 0%.
10. The crystallized glass according to claim 1 or 2, containing, by mass%, 100 ppm or less of Pt.
11. The crystallized glass according to claim 1 or 2, containing, by mass%, 100 ppm or less of Rh.
12. 3. The crystallized glass according to claim 1, wherein the β-OH value of the base glass before crystallization is greater than 0 and less than 2 / mm.
13. 3. The crystallized glass according to claim 1, which has an absolute value of a Seebeck coefficient of 0.000001 V / K or more at any one or more temperature points between 25° C. and 400° C.
14. 3. The crystallized glass according to claim 1, which has a thermoelectric conversion index ZT of 0.00001 or more at any one or more temperature points from 25° C. to 400° C.
15. Carrier mobility is 0.0001 cm 2 The crystallized glass according to claim 1 or 2, wherein Vs is greater than or equal to 1. / Vs.
16. The crystallized glass according to claim 1 or 2, which is used as a heavy metal recovery material.
17. In mass%, Fe 2 O 3 A heavy metal recovery material comprising 20-80% crystallized glass containing magnetic crystals.
18. In mass%, Fe 2 O 3 A soil conditioner comprising 20-80% crystallized glass containing magnetic crystals.
19. A method for producing crystallized glass according to claim 1 or 2, Glass raw materials and Fe 2 O 3 a melting step for melting the mixture of raw materials; A crystallization step of forming the molten glass into a predetermined shape to obtain crystallized glass; A method for producing crystallized glass comprising the steps of:
20. an adsorption step of adsorbing heavy metals to the crystallized glass containing magnetic crystals; a recovery step of recovering the crystallized glass after the heavy metal adsorption with a magnet; The method for recovering heavy metals comprises:
21. 21. The method for recovering heavy metals according to claim 20, wherein heavy metals are recovered from soil.
Citation Information
Patent Citations
Lignin-containing member for improving soil, and method for improving soil
JP2012188492A