Paper container

The paper container design with a composite base material and strategic resin layer configuration addresses resin boiling and joint deterioration in microwave heating, ensuring reliable, aesthetically pleasing, and environmentally friendly food storage.

JP2024170216APending Publication Date: 2024-12-06TOYO ALUMINUM EKCO PRODUCTS KK
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023087251
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-26
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

Conventional paper containers with resin layers experience resin boiling and poor appearance when heated in a microwave oven due to trapped water vapor, and the joints may deteriorate, leading to potential shape loss and psychological anxiety.

Method used

A paper container design with a composite base material comprising a base layer, a first resin layer on one side, and a second resin layer on the other side, where the moisture permeability of the composite base material excluding the second resin layer is higher than that excluding the first resin layer, with adhesion between sides maintained at 4.0 N/cm to 20.0 N/cm, and specific resin layer thicknesses and materials are used to facilitate water vapor permeation and prevent peeling.

Benefits of technology

The design effectively prevents resin boiling, maintains container shape, and ensures strong adhesion, making it suitable for storing foods with moisture or oil, and is environmentally friendly by reducing fossil resource use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024170216000001_ABST
    Figure 2024170216000001_ABST
Patent Text Reader

Abstract

To provide a paper container that is less prone to appearance defects even when heated in a microwave oven and whose composite material has excellent bonding (adhesion) with one side and the other side.SOLUTION: A paper container is composed by forming one sheet of base paper which is made of a composite base material 7 consisting of a paper base material layer 10, a first resin layer 11 formed on one side of the base material layer 10, and a second resin layer 12 formed on the other side of the base material layer 10. The moisture permeability of a portion of the composite base material 7 excluding the second resin layer 12 is higher than that of a portion of the composite base material 7 excluding the first resin layer 11, and the adhesiveness of the composite base material 7 when one side 13 and the other side 14 are bonded is 4.0 N / cm or more and 20.0 N / cm or less. This configuration allows water vapor from moisture in the base material layer to permeate through the first resin layer during microwave heating and also prevents peeling of the composite base material from the one side and the other side.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a paper container, and more particularly to a paper container obtained by molding a single blank and used as a paper tray for storing food or the like. [Background technology]

[0002] Conventionally, as a lightweight and cost-effective food storage container, there is a plastic container made of a synthetic resin such as polypropylene. However, in recent years, the use of plastic containers has been refrained from due to the microplastics problem, and instead of plastic containers, there is a tendency to prefer the use of paper containers mainly made of paper.

[0003] As such a paper container, Patent Document 1 discloses one in which a single sheet of paperboard base paper (paper blank) is provided with a plurality of linear stripes extending substantially radially toward the outer periphery, and the paper container is formed by press molding. The flange end of the paper container is formed with a rolled edge.

[0004] However, the paper container described in Patent Document 1 is formed using a method similar to deep drawing of paper, so if an attempt is made to make the paper container deeper, there is a risk that the paper will tear during forming, making it difficult to manufacture deep paper containers.

[0005] Therefore, as a paper container with a deep depth manufactured from a single paper blank, Patent Document 2 proposes a paper container in which a blank of a predetermined shape is folded to form a bottom and side portions, and the corner portions are folded and glued to give it a deep shape.

[0006] In such paper containers, since the contents may contain a lot of moisture, such as frozen foods, it is preferable to form a resin layer on at least one side of the paperboard base paper that will be the inner side in order to impart water resistance and oil resistance. However, when the corners are folded and glued as in Patent Document 2, the container shape is maintained by providing resin layers on both sides of the paperboard base paper and heat welding or high-frequency welding the corners with the resin layers, but if the bonding at the corners is weak, the container shape may not be maintained.

[0007] Patent Document 3 shows a paper container that solves these problems.

[0008] FIG. 5 is a perspective view showing the external shape of a conventional paper container shown in Patent Document 3, and FIG. 6 is an enlarged end view of the VI-VI line shown in FIG.

[0009] Referring to FIG. 5, the paper container 51 is composed of a bottom 52, a side wall 53 rising from the periphery of the bottom 52, and a flat flange 55 extending outward from a rising end 54 of the side wall 53. Referring to FIG. 6, the bottom 52 is composed of a composite substrate 57 including a base layer 60 made of paper and resin layers 61a and 61b made of polyethylene terephthalate (hereinafter referred to as "PET") laminated on both sides of the base layer 60. The side wall 53 is also composed of the composite substrate 57. The corners are folded and welded, and the flange joints at the corners, i.e., the one side 63 and the other side 64 of the composite substrate 57, are welded by high-frequency welding so that the adhesion is within a predetermined range. This prevents peeling at the interface of the resin layers, improving the reliability of the paper container. [Prior art documents] [Patent documents]

[0010] [Patent Document 1] Japanese Patent Application Publication No. 10-071656 [Patent Document 2] JP 2000-255546 A [Patent Document 3] JP 2021-160744 A Summary of the Invention [Problem to be solved by the invention]

[0011] In some cases, frozen foods and the like are stored in a conventional paper container as shown in Patent Document 3, and are heated in a microwave oven when eaten.

[0012] FIG. 7 is a diagram showing the state of the surface of the composite substrate shown in FIG. 6 after a paper container made of the composite substrate is heated in a microwave oven.

[0013] 7, when frozen food or the like is placed in a paper container and heated in a microwave oven before eating, a phenomenon was discovered in which countless fine bubbles are generated on the resin layer surface 65 of the composite substrate, causing the surface to appear as if it were boiling up. Hereinafter, this phenomenon will be referred to as "resin boiling."

[0014] When a paper container is irradiated with microwaves by heating in a microwave oven, the water molecules contained in the base layer made of paper constituting the composite substrate vibrate at high speed and are heated to become water vapor. However, the resin layer made of PET is difficult for water vapor to pass through, and since the PET resin is laminated on both sides of the base layer, there is no place for the water vapor to escape, and as a result, countless fine bubbles due to water vapor are generated on the surface of the resin layer. In the conventional paper container shown in Patent Document 3 as described above, when heated in a microwave oven, the resin boils, making it look bad and causing a poor appearance. In some cases, the bonding state between the resin layers deteriorates, and there is a risk that the container shape cannot be maintained. Furthermore, it also causes psychological anxiety to the eater. If a resin layer is laminated on only one side of the base layer, there will be no poor appearance when heated in a microwave oven, but in the first place, it will not be possible to bond (adhere) one side and the other side of the composite substrate, and it will not be possible to form it into a paper container.

[0015] This invention has been made to solve the above-mentioned problems, and aims to provide a paper container that is less likely to suffer from poor appearance even when heated in a microwave oven and has excellent bonding (adhesion) with one side and the other side of a composite substrate. [Means for solving the problem]

[0016] In order to achieve the above object, the invention described in claim 1 is a paper container composed of a composite substrate having a base layer made of paper, a first resin layer containing a resin formed on one side of the base layer, and a second resin layer containing a resin formed on the other side of the base layer, wherein the moisture permeability of the portion of the composite substrate excluding the second resin layer is higher than the moisture permeability of the portion of the composite substrate excluding the first resin layer, and the adhesion when the one side and the other side of the composite substrate are bonded is 4.0 N / cm or more and 20.0 N / cm or less.

[0017] With this configuration, effect 1 can be obtained in that water vapor from the moisture in the substrate layer permeates through the first resin layer during heating in a microwave oven, and peeling between the one surface and the other surface of the composite substrate is prevented.

[0018] The invention described in claim 2 is the same as the invention described in claim 1, in which the ratio (B / A) of the moisture permeability B of the composite substrate excluding the second resin layer to the moisture permeability A of the substrate layer alone is 0.6 or more.

[0019] With this configuration, effect 2 can be obtained in that water vapor from moisture in the base layer can more easily permeate through the first resin layer during heating in a microwave oven.

[0020] The invention described in claim 3 is the structure of the invention described in claim 1 or claim 2, wherein the moisture permeability of the composite substrate excluding the second resin layer is 80 g / m 2 ·h or more.

[0021] With this configuration, effect 3 can be obtained in that water vapor from moisture in the base layer can more reliably permeate through the first resin layer during heating in a microwave oven.

[0022] The invention described in claim 4 has the configuration of the invention described in claim 1 or claim 2, wherein the thickness of the first resin layer is 0.5 μm or more and 10 μm or less, the thickness of the second resin layer is 10 μm or more and 50 μm or less, and the thickness of the first resin layer is smaller than the thickness of the second resin layer.

[0023] With this configuration, effect 4 can be obtained, that is, water vapor from the moisture in the base layer can more reliably permeate through the first resin layer during heating in a microwave oven.

[0024] The invention described in claim 5 is the same as the invention described in claim 1 or 2, in which the second resin layer contains a polyester-based resin or a polyolefin-based resin.

[0025] With this configuration, it is possible to impart water resistance and oil resistance to the second resin layer side of the composite substrate, and also to obtain effect 5 that the adhesion to the first resin layer is improved.

[0026] The invention described in claim 6 is the same as the invention described in claim 1 or 2, in which the first resin layer contains at least a urethane resin.

[0027] With this configuration, water vapor from the moisture in the base material layer can be easily transmitted through the first resin layer during microwave heating, and the adhesion to the second resin layer is improved. Also, the oil resistance of the first resin layer of the composite base material is improved.

[0028] The invention described in claim 7 has the configuration of the invention described in claim 1 or claim 2, in which the first resin layer is on the outer surface side and contains at least a urethane resin, and the second resin layer is on the inner surface side and contains a polyester-based resin or a polyolefin-based resin.

[0029] This provides the inner surface of the paper container with water resistance and oil resistance, and also ensures that water vapor from the moisture in the base material layer can easily pass through from the outer surface when heated in a microwave oven. Also, the oil resistance of the first resin layer of the composite base material is improved, which is effect 7.

[0030] The invention described in claim 8 has the configuration of the invention described in claim 1 or claim 2, and is provided with a bottom and a side wall rising from the peripheral edge of the bottom, and one side and the other side of the composite substrate are welded by high-frequency welding at the corners of the side wall.

[0031] With this configuration, effect 8 can be obtained, that is, the stability of the molding of the paper container is improved.

[0032] The invention as recited in claim 9 is the same as the invention as recited in claim 8, in which the side wall portion further comprises a flat flange extending outward from the rising end portion thereof.

[0033] With this configuration, an effect 9 can be obtained in which the flange serves as a handle.

[0034] The invention as recited in claim 10 is the structure as recited in claim 9, in which one surface and the other surface of the composite substrate are bonded to the rear surface of the flange at the corner portion of the side wall.

[0035] With this configuration, an effect 10 can be obtained in that the bonding area can be made large. Effect of the Invention

[0036] As described above, the invention described in claim 1 provides the above-mentioned effect 1, so that the appearance of the paper container is less likely to be impaired when heated in a microwave oven, and the bonding (adhesion) between one surface and the other surface of the composite substrate is excellent.

[0037] The invention as set forth in claim 2 provides the above-mentioned action 2 in addition to the effect of the invention as set forth in claim 1, so that the appearance of the paper container is less likely to be impaired when heated in a microwave oven.

[0038] The invention as set forth in claim 3 provides the above-mentioned action 3 in addition to the effects of the invention as set forth in claim 1 or 2, so that the appearance of the paper container is further prevented from becoming poor when heated in a microwave oven.

[0039] The invention as set forth in claim 4 provides the above-mentioned action 4 in addition to the effects of the invention as set forth in claim 1 or 2, so that the appearance of the paper container is further prevented from becoming poor when heated in a microwave oven.

[0040] The invention described in claim 5 has the effects of the invention described in claim 1 or 2, and in addition thereto, provides the above-mentioned action 5, making it possible to provide a container suitable for storing food containing moisture or oil.

[0041] The invention of claim 6 provides the above-mentioned action 6 in addition to the effects of the invention of claim 1 or claim 2, so that the appearance of the paper container is further prevented from being deteriorated when heated in a microwave oven, and the paper container has even better bonding (adhesion) between one side and the other side of the composite substrate. Also, the container is more suitable for storing foods containing oil.

[0042] The invention described in claim 7 provides the above-mentioned effect 7 in addition to the effects of the invention described in claim 1 or claim 2, making it possible to further reduce the occurrence of defects in the appearance of the paper container when heated in a microwave oven and to make the container suitable for storing foods that contain moisture or oil.

[0043] The invention as recited in claim 8 provides the above-mentioned action 8 in addition to the effects of the invention as recited in claim 1 or 2, thereby improving the reliability of the paper container.

[0044] The invention as set forth in claim 9 provides the above-mentioned action 9 in addition to the effect of the invention as set forth in claim 8, and is therefore convenient for use when the contents become hot.

[0045] The invention recited in claim 10 provides the above-mentioned action 10 in addition to the effect of the invention recited in claim 9, thereby improving the reliability of the paper container. [Brief description of the drawings]

[0046] [Figure 1] 1 is a perspective view showing the appearance of a paper container according to an embodiment of the present invention. [Diagram 2] FIG. 2 is an enlarged end view of the line II-II shown in FIG. [Diagram 3] FIG. 2 is a plan view showing a blank for constructing the paper container shown in FIG. [Figure 4] 2 is a perspective view showing the back structure of the paper container shown in FIG. 1. [Diagram 5] FIG. 1 is a perspective view showing the appearance of a conventional paper container shown in Patent Document 3. [Figure 6] FIG. 6 is an enlarged end view of the VI-VI line shown in FIG. 5. [Figure 7] FIG. 7 is a diagram showing the state of a paper container made of the composite substrate shown in FIG. 6 after it has been heated in a microwave oven. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0047] FIG. 1 is a perspective view showing the appearance of a paper container according to an embodiment of the present invention, and FIG. 2 is an enlarged end view taken along line II-II shown in FIG.

[0048] 1 and 2, the paper container 1 is mainly composed of a rectangular bottom 2, a pair of first side walls 3a, 3b rising from each of a pair of opposing long sides of the bottom 2, and a pair of second side walls 4a, 4b rising from each of a pair of opposing short sides of the bottom 2. The first side walls 3a, 3b are provided with first flat flanges 5a, 5b extending outward from rising ends 8a, 8b. The second side walls 4a, 4b are provided with second flat flanges 6a, 6b extending outward from rising ends 9a, 9b.

[0049] Referring to FIG. 2, the bottom 2 is composed of a composite substrate 7 including a substrate layer 10 made of paper, a first resin layer 11 formed on one side of the substrate layer 10 (the outer side of the paper container 1), and a second resin layer 12 formed on the other side of the substrate layer (the inner side of the paper container 1). The outer side of the paper container 1 refers to the outer side of the sidewalls (the first sidewalls 3 and the second sidewalls 4), and the inner side of the paper container 1 refers to the inner side of the sidewalls. The first resin layer 11 is laminated on one side of the substrate layer 10 by coating, and the second resin layer 12 is laminated on the other side of the substrate layer 10 by extrusion lamination. The first resin layer 11 has a thickness of 5 μm, and the second resin layer 12 has a thickness of 30 μm. The first sidewalls 3a, 3b and the second sidewalls 4a, 4b are also composed of the composite substrate 7.

[0050] The composite substrate 7 is configured so that the moisture permeability of a portion excluding the second resin layer 12 is higher than the moisture permeability of a portion excluding the first resin layer 11 of the composite substrate 7. The effects of this configuration will be described later.

[0051] Next, a method for constructing such a paper container 1 will be described.

[0052] First, the second resin layer 12 is laminated by extrusion lamination onto the other side of the base layer 10 of the paper base material, and the first resin layer 11 is laminated by coating onto one side of the base layer 10 to form the composite base material 7. The composite base material 7 is then punched into a predetermined shape to form a blank.

[0053] FIG. 3 is a plan view showing a blank for constructing the paper container shown in FIG.

[0054] Referring to Figure 3, the blank 17 is composed of a rectangular bottom blank 18 that corresponds to the bottom 2 of the paper container 1 (see Figure 1, etc.), a pair of first side wall blanks 19a, 19b extending outward from each of a pair of opposing long sides of the bottom blank 18, a pair of second side wall blanks 20a, 20b extending outward from each of a pair of opposing short sides of the bottom blank 18, first lateral tongue pieces 21a, 21b extending from the center of the outer edge of each of the first side wall blanks 19a, 19b, joining tongue pieces 22a, 22b, 22c, 22d extending from the outer edges of each end of the first side wall blanks 19a, 19b on the second side wall blanks 20a, 20b side, and second lateral tongue pieces 23a, 23b extending from the outer edges of each of the second side wall blanks 20a, 20b.

[0055] Next, with the second resin layer 12 facing the inner surface of the paper container 1, the blank 17 is folded in a mountain fold along the mountain fold line 24 shown by the dashed line in Figure 3, and in a valley fold along the valley fold line 25 shown by the dotted line in the same figure, to form a container shape.

[0056] FIG. 4 is a perspective view showing the back structure of the paper container shown in FIG.

[0057] Referring to Figures 3 and 4, the bottom blank 18 of the blank 17 forms the bottom 2 of the paper container 1, the first side wall blanks 19a, 19b form the first side wall portions 3a, 3b, the second side wall blanks 20a, 20b form the second side wall portions 4a, 4b, the first side tongues 21a, 21b form the first flanges 5a, 5b, and the second side tongues 23a, 23b form the second flanges 6a, 6b.

[0058] The ends of the joining tongues 22a-22d and the first flanges 5a, 5b are arranged on the back surfaces of the second flanges 6a, 6b. Then, while maintaining the container shape, one side (back surface) of the second flanges 6a, 6b, the other side (front surface) of the joining tongues 22a-22d, and the other side (front surface) of the first flanges 5a, 5b are welded by high-frequency welding at the corners of the side walls (first side wall 3 and second side wall 4), respectively, while pressing with a heated press mold. That is, the paper container 1 is constructed with the side walls (first side wall 3 and second side wall 4) rising from the periphery of the bottom 2. The corners of the side walls refer to the parts where the composite substrates overlap and are welded, and include the bonded parts (the joining tongues and parts of the flanges) on the back surfaces of the flanges and the unbonded parts of the side walls continuous therewith, which are shown as "A" parts in FIG. 4. Moreover, the adhesion between the one surface 13 and the other surface 14 of the composite substrate at the joint is 4.0 N / cm or more and 20.0 N / cm or less.

[0059] As described above, the paper container 1 is configured so that the moisture permeability of the portion of the composite substrate 7 excluding the second resin layer 12 is higher than the moisture permeability of the portion of the composite substrate 7 excluding the first resin layer 11. In addition, the adhesion when one side and the other side of the composite substrate are bonded is 4.0 N / cm or more and 20.0 N / cm or less. With this configuration, water vapor due to moisture in the substrate layer is transmitted through the first resin layer during microwave heating, and peeling from the one side and the other side of the composite substrate is prevented. Therefore, the appearance of the paper container is less likely to be deteriorated during microwave heating, and the bonding (adhesion) between the one side and the other side of the composite substrate is excellent.

[0060] Here, if the adhesion at the joints is low, the joints will easily peel off and the paper container will not be viable. In other words, in order to solve the problem of resin boiling, there are cases where a paper container will not be viable simply by increasing the moisture permeability, and the present invention achieves both moisture permeability and adhesion, thereby solving the problem of resin boiling, and achieving the effect of obtaining a highly reliable paper container that is less likely to have poor appearance and has excellent adhesion at the joints.

[0061] Furthermore, in the paper container 1, one surface 13 and the other surface 14 of the composite substrate 7 are welded by high-frequency welding at the corners, which improves the stability of the molding of the paper container, thereby improving reliability.

[0062] Furthermore, by providing flat flanges (first flange 5 and second flange 6) extending outward from the rising ends (rising end 8 of the first side wall portion and rising end 9 of the second side wall portion) of the side wall portions (first side wall portion 3 and second side wall portion 4), the flanges can be used as handles, making it convenient to use when the contents are hot.

[0063] Furthermore, since welding is performed on the rear surfaces of the flanges (first flange 5 and second flange 6), the welding points can be made large without impairing the design, thereby improving the reliability of the container.

[0064] In the paper container according to the embodiment of the present invention, the paper container has a specific shape, but the shape is not particularly limited. For example, the shape when viewed from above the opening of the paper container may be polygonal, circular, or substantially elliptical, but a polygonal shape from a square to an octagon is preferable for ease of molding. The size of the paper container is also not particularly limited.

[0065] Furthermore, in the paper container according to the embodiment of the present invention, the type of paper constituting the base layer is not particularly limited. Pure white roll paper, craft paper, parchment paper, ivory paper, Manila paper, card paper, cup paper, glassine paper, etc. can be used depending on the desired application. Furthermore, the thickness of the paper is not particularly limited, but is preferably 0.2 mm to 0.5 mm (basis weight 150 g / m 2 ~500g / m 2 By configuring in this way, it is possible to easily form the paper container and to reduce the cost of the paper container.

[0066] In the paper container according to the embodiment of the present invention, the type of resin constituting the first resin layer is not particularly limited, but the resin is one that has a higher moisture permeability than the composite substrate excluding the second resin layer (i.e., the substrate layer and the first resin layer). By using such a resin for the first resin layer, water vapor due to moisture in the substrate layer can pass through the first resin layer during microwave heating. In addition, the comparison of moisture permeability is not simply made between the resin layers, but is made between the substrate layer and the first resin layer and the second resin layer, respectively. This is because, during microwave heating, water molecules contained in the substrate layer turn into water vapor and attempt to pass through the resin layer, so the moisture permeability measured when the substrate layer and the first resin layer and the second resin layer are each combined is important.

[0067] Examples of the resin constituting the first resin layer include resins containing urethane resin. When the first resin layer contains urethane resin, it is preferable that the resin further contains rosin resin, and more preferably, the rosin resin is rosin and / or a rosin derivative, the urethane resin is a reaction product of polyol and polyisocyanate, and the weight average molecular weight of the urethane resin is 5,000 to 500,000. Urethane resin is also preferable in that it has high moisture permeability and high adhesion to the second resin layer described below. Therefore, it is possible to make the appearance of the paper container less likely to be poor when heated in a microwave oven, and to make the paper container have even better bonding (adhesion) with one side and the other side of the composite substrate. Examples of other resins include polyethyleneimine resin. Polyethyleneimine resin is also preferable in that it has high adhesion with the second resin layer described below. In addition, resins containing urethane resin and polyethyleneimine resin have high heat resistance, so that peeling of the adhesive part can be prevented even when the paper container is used for food to be heated in an oven. Among them, when a resin containing a urethane resin is used as the resin constituting the first resin layer, it is more preferable because it can also impart oil resistance to the first resin layer side of the composite substrate. Therefore, it can be a container more suitable for storing foods containing oil. Even if the resin constituting the first resin layer itself has low moisture permeability, when the thickness of the first resin layer is thin enough to allow water vapor to pass through, the moisture permeability of the part of the composite substrate excluding the second resin layer (i.e., the part of the substrate layer and the first resin layer) is relatively high compared to when the thickness of the first resin layer is thick, so it is possible to use such a resin. For example, although the resin itself has low moisture permeability, when it is laminated with a thin thickness as the first resin layer on the substrate layer, the moisture permeability of the part of the substrate layer and the first resin layer is high, and there are cases where no appearance defect occurs during microwave heating. In addition, the first resin layer may be composed of or contain a biomass resin derived from a living organism (derived from a biomass resource). In this case, the proportion of raw materials derived from fossil resources is reduced, which is useful for environmental conservation.

[0068] It is also preferable that the ratio (B / A) of the moisture permeability B of the composite substrate excluding the second resin layer (i.e., the substrate layer and first resin layer) to the moisture permeability A of the substrate layer alone is 0.6 or more. With this configuration, water vapor from the moisture in the substrate layer can more easily pass through the first resin layer during microwave heating, making it less likely that the paper container will have a poor appearance during microwave heating.

[0069] Furthermore, the moisture permeability of the portion of the composite substrate excluding the second resin layer (i.e., the portion of the substrate layer and the first resin layer) is 80 g / m 2 With this configuration, water vapor from the moisture in the base material layer can more reliably pass through the first resin layer during microwave heating, making it even more difficult for the appearance of the paper container to become poor during microwave heating.

[0070] In addition, in the paper container according to the embodiment of the present invention, the type of resin constituting the second resin layer is not particularly limited. Examples of the resin include polyester-based resins such as polyethylene terephthalate and polybutylene terephthalate, polyolefin-based resins such as polypropylene, polyethylene, and polymethylpentene, acrylic (methacrylic)-based resins, diene-based resins such as polybutadiene, and thermoplastic resins such as polycarbonate-based resins. In addition, in order to make the paper container more environmentally friendly, for example, biodegradable resins such as polylactic acid (PLA) can also be used. In addition, it is preferable to use polyester-based resins or polyolefin-based resins as the preferred resin types, because they have excellent adhesion when the composite substrates are bonded together, and the strength of the paper container is improved. In addition, water resistance and oil resistance can be imparted to the second resin layer side of the composite substrate. Therefore, the container can be made suitable for storing foods containing moisture and oil. Furthermore, it is more preferable that the polyester-based resin or polyolefin-based resin contains a biomass polyester-based resin or a biomass polyolefin-based resin derived from living organisms (biomass resources), since this reduces the amount of fossil resources used and improves carbon neutrality, thereby improving sustainability and contributing to environmental conservation.

[0071] Furthermore, among these, when a polyethylene terephthalate resin is used as the polyester-based resin, the polyethylene terephthalate resin is a copolymerized polyethylene terephthalate resin obtained by copolymerization with isophthalic acid, and it is preferable that the copolymerization ratio of isophthalic acid in the copolymerized polyethylene terephthalate resin is 1 mol % or more and less than 10 mol %, and the melting point is 235° C. or more and 250° C. or less. By configuring in this way, a paper container having high adhesion between the base material layer and the resin layer and high heat resistance can be obtained, which prevents molding defects of the paper container and is also suitable for use when the contents are at high temperatures or when a baking process is performed.

[0072] Furthermore, the polyethylene terephthalate resin in the present invention is preferably a biomass polyethylene terephthalate resin derived from a living organism (derived from a biomass resource) with a bio-based carbon content of 5% or more. The polyethylene terephthalate resin is a resin obtained by polycondensation of ethylene glycol and terephthalic acid as the main components, and most of it is derived from fossil resources. By making it into a biomass polyethylene terephthalate resin obtained from a living organism raw material such as sugar cane, the amount of fossil resources used can be reduced and carbon neutrality is improved, which improves sustainability and contributes to environmental conservation.

[0073] In the present invention, the bio-based carbon content, which is an index showing the proportion of biologically derived raw materials in the copolymerized polyethylene terephthalate resin, is preferably 5% or more, and more preferably 15% or more. The higher the bio-based carbon content, the lower the proportion of fossil resource-derived raw materials, making the paper container more environmentally friendly. On the other hand, as the proportion of the bio-based carbon content increases, the cost also increases, so it is more preferable that it is within an appropriate range. The bio-based carbon content can be indicated by the value of the C14 content obtained by a radiocarbon (C14) measurement method in accordance with ISO-16620-2 (equivalent to the ASTM-D6866 standard). That is, since fossil resources contain almost no C14, while biological resources contain a certain proportion of C14 (105.5 pMC), if the content of C14 in the copolymerized polyethylene terephthalate resin is PC14, the bio-based carbon content can be calculated by the following formula.

[0074] Bio-based carbon content (%) = PC14 / 105.5 x 100 Furthermore, in the paper container according to the embodiment of the present invention, the thickness of the resin layer is not particularly limited, but the second resin layer may have a thickness of, for example, 10 μm to 50 μm. In particular, a thickness within the range of 20 μm to 30 μm is preferable from the viewpoints of stable adhesion with the first resin and ensuring water resistance and oil resistance of the inner surface of the paper container.

[0075] It is also preferable that the thickness of the first resin layer is 0.5 μm or more and 10 μm or less, the thickness of the second resin layer is 10 μm or more and 50 μm or less, and the thickness of the first resin layer is smaller than the thickness of the second resin layer. This is because the thickness of the resin layer is related to moisture permeability, and when the moisture permeability of the part of the composite substrate excluding the second resin layer and the thickness of the first resin layer are in an appropriate range, water vapor due to moisture in the substrate layer can more reliably pass through from the first resin layer during microwave heating. By setting the above range, water vapor due to moisture in the substrate layer can more reliably pass through from the first resin layer during microwave heating, making it even less likely that the appearance of the paper container will be poor during microwave heating.

[0076] Furthermore, in the paper container according to the embodiment of the present invention, the lamination method of each of the first and second resin layers on the base layer is not particularly limited, and examples thereof include extrusion lamination, dry lamination, wet lamination, and coating of a resin solution (including print coating). It is preferable to use coating of a resin solution for the first resin layer and extrusion lamination for the second resin layer. Furthermore, for the second resin layer, the lamination of the resin can impart properties such as heat resistance, water resistance, and gas / liquid permeability resistance to the molded paper container. Furthermore, an anchor coat layer may be formed on the paper in advance during extrusion lamination. Furthermore, printing may be applied to the surface of the composite base material. Furthermore, corona treatment may be applied to the paper of the base layer.

[0077] Furthermore, in the paper container according to the embodiment of the present invention, it is preferable that the adhesion when one side and the other side of the composite substrate are bonded is 4.0 N / cm or more and 20.0 N / cm or less. By configuring in this way, peeling at the resin layer interface is prevented under normal use conditions as a paper container for storing food, thereby improving the reliability of the paper container. In addition, by being below the above upper limit value, it becomes easy to disassemble and dismantle the paper container to reduce the volume of waste after use as a paper container.

[0078] Furthermore, the paper container according to the embodiment of the present invention can be used for various purposes, including, but not limited to, storing food, and is particularly suitable as a deep-shaped paper container with increased storage volume.

[0079] Furthermore, although the paper container according to the embodiment of the present invention is manufactured by a specific manufacturing method, it may be manufactured by another method.

[0080] Furthermore, in the paper container according to the embodiment of the present invention, one side and the other side of the composite substrate are welded (bonded) by high-frequency welding, but other bonding methods such as ultrasonic welding may also be used. Furthermore, heating may also be used during bonding.

[0081] Furthermore, in the paper container according to the embodiment of the present invention, the flange is bonded on its back surface, but the flange may be bonded over a wide area including other areas, or may be bonded in areas other than the back surface of the flange.

[0082] Furthermore, although the paper container according to the embodiment of the present invention is provided with a flange, it is not necessarily required to provide a flange.

[0083] Furthermore, in the paper container according to the embodiment of the present invention, the corners of the side wall have a specific shape, but the shape is not particularly limited. When forming a paper container by folding as in the embodiment of the present invention, it is preferable to include a portion that is folded and bonded (welded) to maintain the container shape.

[0084] Furthermore, in the paper container according to the embodiment of the present invention, the composite substrate has three layers, namely, a substrate layer, a first resin layer, and a second resin layer, but may have four or more layers including a resin layer for the purpose of anchor coating or printing. Even when a plurality of resin layers are formed on one side of the substrate layer, all layers on the one side of the substrate layer are collectively referred to as the first resin layer. Also, even when a plurality of resin layers are formed on the other side of the substrate layer, all layers on the other side of the substrate layer are collectively referred to as the second resin layer.

[0085] Furthermore, in the paper container according to the embodiment of the present invention, the first resin layer is formed on the outer surface side of the paper container, and the second resin layer is formed on the inner surface side of the paper container, but these may be formed in reverse. When the first resin layer is formed on the outer surface side and the second resin layer is formed on the inner surface side, it is preferable that the first resin layer contains a urethane resin and the second resin layer contains a polyester resin or a polyolefin resin. This is because the urethane resin imparts water resistance and oil resistance to the inner surface side of the paper container, and because the urethane resin has high moisture permeability, water vapor due to moisture in the base layer can easily pass through from the outer surface side during microwave heating. Therefore, it is possible to further prevent the appearance of the paper container from being defective during microwave heating. In addition, when the urethane resin is contained, oil resistance can also be imparted, so the oil resistance of not only the second resin layer but also the first resin layer is improved. Therefore, the container can be made suitable for storing foods containing moisture and oil. EXAMPLES

[0086] The present invention will be described in detail below with reference to examples, although the embodiments of the present invention are not limited to the examples.

[0087] (Preparation of test specimen) First, in Example 1, the basis weight is 260 g / m 2 A paper substrate was prepared, and a solution containing urethane resin (a reaction product of polyol and polyisocyanate, weight average molecular weight: approximately 50,000) and rosin resin was applied to one side of the substrate and dried to form a 5 μm-thick resin layer as the first resin layer, and a 30 μm-thick resin layer made of polyethylene terephthalate resin was formed by extrusion lamination to prepare a composite substrate.

[0088] In Example 2, a composite substrate having the same configuration as Example 1 was prepared, except that a resin layer having a thickness of 5 μm was formed as the first resin layer by coating and drying a solution containing a polyethyleneimine resin.

[0089] In Comparative Example 1, a composite substrate was prepared having the same structure as in Example 1, except that a 30 μm-thick resin layer made of polyethylene terephthalate resin was formed on both sides of the paper substrate by extrusion lamination.

[0090] (Evaluation 1: Moisture permeability test) In order to measure the moisture permeability of the composite substrate in Example 1, Example 2, and Comparative Example 1 excluding the second resin layer, the paper substrate was used in the moisture permeability test without forming the second resin layer in advance, and only the first resin layer was formed, and test pieces were cut out from each to measure the moisture permeability. Also, as Reference Example 1, a test piece was cut out from the paper substrate alone, and the moisture permeability was measured. The moisture permeability test was measured by the A-1 method (calcium chloride method) of JIS L 1099. The measurement was performed so that the first resin layer side of the test piece faced the calcium chloride side. The results are shown in Table 1. In the moisture permeability test, the paper substrate was used without forming the second resin layer in advance, and only the first resin layer was formed, but it is presumed that the same results would be obtained even if the second resin layer was peeled off from the composite substrate on which the second resin layer was formed.

[0091] (Evaluation 2-1: Surface condition after microwave heating 1) The composite substrates in Examples 1, 2 and Comparative Example 1 and the paper substrate alone in Reference Example 1 were cut into 5 cm squares, placed in a microwave oven and heated at 600 W for 6 minutes, after which the change in the surface state was observed.

[0092] (Evaluation 2-2: Surface condition after microwave heating 2) Next, the composite substrates in Example 1, Example 2, and Comparative Example 1 were cut into blanks having the shapes shown in FIG. 3, respectively, and the blanks were folded so that the second resin layer side (polyethylene terephthalate resin side) was the inner surface side of the paper container, and the blanks were pressed under pressure while maintaining the container shape, and the joints of the flanges of the paper containers were subjected to high-frequency welding to obtain paper containers having the shapes shown in FIG. 1. In addition, in Examples 1 and 2, the pressurization was performed with the press mold heated (about 85°C), and in Comparative Example 1, it was performed at room temperature. In addition, for adhesion, high-frequency welding was performed on the back side of the joints of the flanges of the paper containers with a 40MHz transistor-type high-frequency oscillator at an output of 1800W for 1.5 seconds. Each of the obtained paper containers was placed in a microwave oven with commercially available frozen pasta (manufactured by Nippun Co., Ltd., product name: Oh My Premium Colorful Vegetable Peperoncino) contained therein, and the change in the surface state of the paper containers after heating at 600W for 6 minutes was observed.

[0093] The results are shown in Table 1.

[0094] [Table 1] (Evaluation 3: Adhesion test) Using the composite substrates of Example 1, Example 2 and Comparative Example 1, five paper containers each were produced in the same manner as in Evaluation 2-2.

[0095] From each of the test paper containers, the bonded portion on the back surface of the flange (the joining tongue and part of the flange) and the continuous unbonded portion on the side wall were cut out as test pieces, shown as part "A" in Figure 4 above. A tensile testing machine (manufactured by Shimadzu Corporation, product name: Autograph, model number: AGS-X) was used to hold the two ends of the unbonded portion and perform a 180° peel test at a tensile speed of 100 mm / min to test the adhesion between one side and the other side of the composite substrate.

[0096] The results are shown in Table 2 below.

[0097] [Table 2] Referring to Table 2, the adhesion of Examples 1 and 2 was 4.0 N / cm or more, which is a suitable adhesion. Therefore, from Tables 1 and 2, it was confirmed that the paper container of the present invention is less likely to suffer from poor appearance due to resin boiling after heating in a microwave oven, and has excellent bonding (adhesion) with one side and the other side of the composite substrate.

[0098] (Rating 4: Heat resistance test) In the same manner as in Evaluation 2-2, ten paper containers were produced using the composite substrates of Example 1, Example 2, and Comparative Example 1. As Reference Example 1, a single paper substrate was prepared.

[0099] Each test paper container was heated in an oven at 220°C for 10 minutes in an empty state without anything inside, and the presence or absence of peeling of the adhesive portion of the paper container was visually confirmed. Ten paper containers were used for each of Example 1, Example 2, and Comparative Example 1. If peeling was not observed at the adhesive portion of any of the ten paper containers, it was evaluated as "no adhesive peeling", and if peeling was observed at the adhesive portion of even one of the ten paper containers, it was evaluated as "adhesive peeling". Note that Reference Example 1 was a paper base material alone, so it was not possible to evaluate whether it could be formed into a paper container. The results are shown in Table 3.

[0100] Referring to Table 3, in Examples 1 and 2, no peeling was observed at the bonded portions even after heating, and the container shape was maintained. Therefore, it was confirmed that the paper container of the present invention has heat resistance.

[0101] In addition, by comparing Example 1 and Example 2 with Reference Example 1 with reference to Tables 1 to 3, although resin boiling does not occur in Reference Example 1, it is not possible to form the paper base material alone because it cannot be bonded, and it is not viable as a paper container. From this, it can be said that a reliable paper container that does not cause resin boiling needs to have both high moisture permeability and high adhesion at the joints. In contrast, the results obtained were that Example 1 and Example 2 have moisture permeability to the extent that resin boiling does not occur, have high adhesion at the joints, and no peeling at the joints is observed even after heating. Therefore, it was confirmed that the paper container of the present invention is a highly reliable paper container that is unlikely to cause appearance defects when heated in a microwave oven by achieving both high moisture permeability and high adhesion at the bonded parts.

[0102] (Rating 5: Oil resistance test) Test pieces were cut out in a size of 50 mm square from the composite substrates in Example 1, Example 2, and Comparative Example 1, and from the paper substrate alone in Reference Example 1, and 10 test pieces were prepared for each.

[0103] The evaluation was performed using a test method based on JAPAN TAPPI Paper and Pulp Test Method No. 41:2000 "Paper and Paperboard Oil Repellency Test Method Kit Method". However, for the test, only the test liquid of Kit No. 2 (a mixture of 180 ml of castor oil, 10 ml of toluene, and 10 ml of heptane) was used, and the state of penetration of the test liquid into the test piece after operations a) to c) of "6. Operation" of JAPAN TAPPI Paper and Pulp Test Method No. 41 was evaluated. Evaluation was performed by holding the test piece up to light and evaluating its state before (Evaluation 5-1) and when it was illuminated (Evaluation 5-2), and an overall evaluation was performed based on the results of Evaluation 5-1 and Evaluation 5-2. The overall evaluation was performed according to the following criteria. ◎: Both ratings 5-1 and 5-2: "Oil stains are not visible" 〇: One of the ratings of 5-1 and 5-2, "Oil stains are not visible" ×: Both ratings 5-1 and 5-2: "Oil stains are visible" The results are shown in Table 3.

[0104] [Table 3] Referring to Table 3, without the watermark, no oil stains were visible in Example 1. Therefore, it was confirmed that in the paper container of the present invention, the resin constituting the first resin layer contains a urethane resin, which improves oil resistance. [Explanation of symbols]

[0105] 1. Paper containers 2…Bottom 3...First side wall 4...Second side wall 5...First flange 6...Second flange 7…Composite base material 8...Rising end 9…Rising end 10…Base material layer 11...First resin layer 12…Second resin layer 13...One side of the composite substrate 14...Other surface of composite substrate In addition, the same symbols in each drawing indicate the same or corresponding parts.

Claims

1. A paper container made of a composite substrate including a base layer made of paper, a first resin layer containing a resin formed on one side of the base layer, and a second resin layer containing a resin formed on the other side of the base layer, The moisture permeability of a portion of the composite substrate excluding the second resin layer is higher than the moisture permeability of a portion of the composite substrate excluding the first resin layer, The paper container has an adhesion strength of 4.0 N / cm or more and 20.0 N / cm or less when one surface and the other surface of the composite substrate are bonded to each other.

2. The paper container according to claim 1, wherein the ratio (B / A) of the moisture permeability B of the composite substrate excluding the second resin layer to the moisture permeability A of the substrate layer alone is 0.6 or more.

3. The moisture permeability of the composite substrate excluding the second resin layer is 80 g / m 2 The paper container according to claim 1 or 2, having a thickness of h or more.

4. The paper container according to claim 1 or 2, wherein the thickness of the first resin layer is 0.5 μm or more and 10 μm or less, the thickness of the second resin layer is 10 μm or more and 50 μm or less, and the thickness of the first resin layer is smaller than the thickness of the second resin layer.

5. The paper container according to claim 1 or 2, wherein the second resin layer contains a polyester-based resin or a polyolefin-based resin.

6. The paper container according to claim 1 or 2, wherein the first resin layer contains at least a urethane resin.

7. The first resin layer is on an outer surface side and contains at least a urethane resin, The paper container according to claim 1 or 2, wherein the second resin layer is on the inner surface side and contains a polyester-based resin or a polyolefin-based resin.

8. A bottom portion and a side wall portion rising from a peripheral edge of the bottom portion, The paper container according to claim 1 or 2, wherein the one surface and the other surface of the composite substrate are welded by high frequency welding at corner portions of the side wall portion.

9. 9. The paper container of claim 8, wherein the sidewall further comprises a flat flange extending outwardly from the upstanding end thereof.

10. The paper container according to claim 9 , wherein the one surface and the other surface of the composite substrate are bonded to a rear surface of the flange at the corner portion of the side wall portion.

Citation Information

Patent Citations

  • Base board, paper container, and method and apparatus for forming paper container

    JP1998071656A

  • Blank for tray container

    JP2000255546A

  • Vessel

    JP2021160744A