PROTRUSIVE LINERS ON PHASE CHANGE MEMORY CELL SIDEWALLS - Patent application
The PCM cell with a mushroom structure and dual liners addresses resistive drift issues by providing additional current paths, enhancing tuning fidelity and reducing noise, thus improving performance.
Patent Information
- Application Number
- JP2024505345
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-29
- Filing Date
- 2022-09-27
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2042-09-27
AI Technical Summary
Phase Change Memory (PCM) materials are susceptible to resistive drift, which negatively impacts tuning fidelity and can be exacerbated by shrinking dimensions, leading to increased resistance drift and circuit noise.
A PCM cell with a mushroom structure incorporating a first and second protruding liner, each made of different materials, electrically connected to electrodes and the PCM material, to provide additional current paths and reduce resistance drift.
The mushroom structure reduces resistance drift, lowers read resistance, enhances control over heater operation, and increases the dynamic range of the PCM cell, improving tuning fidelity and reducing circuit noise.
Smart Images

Figure 2024536675000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to computer memories, and more particularly to phase change material memory devices having protruding liners.
[0002] Phase Change Memory (PCM) can be used for both training and inference in analog computing for artificial intelligence. PCM structures can include phase change memristor devices with tunable conductivity and high overall device resistance with high retention to minimize energy consumption. Tuning can be achieved by varying the ratio of crystalline and amorphous phases in the PCM material to form different structural states. However, PCM materials can be subject to resistance drift, which can adversely affect the fidelity of tuning. Summary of the Invention
[0003] According to an embodiment of the present disclosure, a PCM cell having a mushroom structure includes a first electrode, a heater electrically connected to the first electrode, a first protruding liner electrically connected to the heater, a PCM material electrically connected to the first protruding liner, a second electrode electrically connected to the PCM material, and a second protruding liner electrically connected to the first protruding liner and the second electrode.
[0004] According to an embodiment of the present disclosure, a PCM cell includes a first electrode, a first protruding liner electrically connected to the first electrode (first protruding liner comprising a first material), a PCM material electrically connected to the first protruding liner, a second electrode electrically connected to the PCM material, a second protruding liner electrically connected to the first protruding liner and the second electrode (second protruding liner comprising a second material), where the second material is different from the first material.
[0005] According to an embodiment of the present disclosure, a method of manufacturing a PCM cell includes forming a first electrode, forming a first protruding liner electrically connected to the first electrode, forming a PCM material on the first protruding liner, forming a second electrode on the PCM material, and forming a second protruding liner (in contact with the first protruding liner, the PCM material, and the second electrode). [Brief description of the drawings]
[0006] [Figure 1A] 1 is a cross-sectional view of a PCM cell including a sidewall protruding liner according to an embodiment of the present disclosure.
[0007] [Figure 1B] FIG. 1B is a cross-sectional view of the PCM cell of FIG. 1A including smaller amorphous regions according to an embodiment of the present disclosure.
[0008] [Figure 1C] FIG. 1B is a cross-sectional view of the PCM cell of FIG. 1A including larger amorphous regions according to an embodiment of the present disclosure.
[0009] [Diagram 2] 1B is a flow chart of a method for manufacturing the PCM cell of FIG. 1A according to an embodiment of the present disclosure.
[0010] [Figure 3A] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3B] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3C] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3D] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3E] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3F]3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3G] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3H] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure. [Figure 3I] 3A-3C are a series of cross-sectional views of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present disclosure.
[0011] [Figure 4A] 1B is a graph of resistance versus current for various liner electrical resistivities of the PCM cell of FIG. 1A in accordance with an embodiment of the present disclosure.
[0012] [Figure 4B] 1B is a graph of resistance versus current for various liner thickness ratios of the PCM cell of FIG. 1A in accordance with an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Various embodiments of the present disclosure are described herein with reference to the associated drawings. Alternative embodiments may be devised without departing from the scope of the present disclosure. It should be noted that in the following description and drawings, various connections and relationships (e.g., above, below, adjacent, etc.) are shown between elements. These connections and / or relationships may be direct or indirect unless otherwise specified, and the present disclosure is not intended to be limiting in this respect. Thus, the coupling of entities may refer to either direct or indirect coupling, and the relationship between entities may be a direct or indirect relationship. As an example of an indirect relationship, a reference herein to forming layer "A" on layer "B" includes the situation where one or more intermediate layers (e.g., layers ("C" and "D") are between layer "A" and layer "B" as long as the relevant properties and functions of layer "A" and layer "B" are not substantially altered by the intermediate layers.
[0014] The following definitions and abbreviations are used in interpreting the claims and the specification. As used herein, the terms "comprises," "comprising," "includes," "including," "has," "having," "contains," or "containing," or any other variation thereof, are intended to cover a non-exclusive inclusion. For example, a composition, mixture, process, method, article, or device that includes a list of elements is not necessarily limited to only those elements, but may include other elements not expressly listed or inherent to such composition, mixture, process, method, article, or device. Additionally, any numerical range contained herein includes its boundaries unless expressly stated otherwise.
[0015] For purposes of the following description, the terms "upper," "lower," "right," "left," "vertical," "horizontal," "top," "bottom," and derivatives thereof, shall refer to the structures and methods described as oriented in the drawings. The terms "overlying," "atop," "on top," "positioned on," or "positioned atop" mean that a first element, such as a first structure, is on a second element, such as a second structure, and that an intervening element, such as an interface structure, may be between the first and second elements. The term "direct contact" means that a first element, such as a first structure, and a second element, such as a second structure, are connected without any intermediate conductive, insulating, or semiconducting layers at the interface of the two elements. It should be noted that the term "selective," such as "a first element selective to a second element," means that the first element can be etched and the second element can act as an etch stop.
[0016] For the sake of brevity, conventional techniques associated with the manufacture of semiconductor devices and integrated circuits (ICs) may or may not be described in detail herein. Moreover, various tasks and process steps described herein may be incorporated into a more comprehensive procedure or process having additional steps or functions not described in detail herein. In particular, because the various steps in the manufacture of semiconductor devices and semiconductor-based ICs are well known, for the sake of brevity, many conventional steps are only briefly described herein or are omitted entirely without providing details of the well-known processes.
[0017] Generally, the various processes used to form microchips that are packaged into ICs fall into four general categories: film deposition, removal / etching, semiconductor doping, and patterning / lithography.
[0018] Deposition can be any process that grows, coats, or otherwise transfers material onto a wafer. Available techniques include Physical Vapor Deposition (PVD), Chemical Vapor Deposition (CVD), Electrochemical Deposition (ECD), Molecular Beam Epitaxy (MBE), and more recently Atomic Layer Deposition (ALD). Another deposition technique is Plasma Enhanced Chemical Vapor Deposition (PECVD), a process that uses the energy in a plasma to induce reactions at the wafer surface that would otherwise require higher temperatures associated with traditional CVD. High energy ion bombardment during PECVD deposition can also improve the electrical and mechanical properties of the film.
[0019] Removal / etching can be any process that removes material from the wafer. Examples include etching processes (either wet or dry), Chemical Mechanical Planarization (CMP), and the like. One example of a removal process is Ion Beam Etching (IBE). In general, IBE (or milling) refers to dry plasma etching methods that utilize a remote broad beam ion / plasma source to remove substrate material by physically inert and / or chemically reactive gas means. As with other dry plasma etching techniques, IBE offers advantages such as etch rate, anisotropy, selectivity, uniformity, aspect ratio, and minimal substrate damage. Another example of a dry removal process is Reactive Ion Etching (RIE). In general, RIE uses a chemically reactive plasma to remove material deposited on the wafer. In RIE, the plasma is generated by an electromagnetic field under low pressure (vacuum). High energy ions from the RIE plasma attack the wafer surface and react with it to remove material.
[0020] Semiconductor doping can be the modification of electrical properties, for example, by doping the source and drain of a transistor, typically by diffusion and / or ion implantation. These doping processes are followed by a furnace anneal or rapid thermal anneal ("Rapid Thermal Annealing" (RTA)). The anneal serves to activate the implanted dopants. To connect and isolate the transistors and their components, both conductor (e.g., polysilicon, aluminum, copper, etc.) and insulator (e.g., various forms of silicon dioxide, silicon nitride, etc.) films are used. By selectively doping different regions of a semiconductor substrate, the conductivity of the substrate can be altered by applying a voltage. By creating structures of these various components, millions of transistors can be constructed and wired together to form the complex circuits of modern microelectronic devices.
[0021] Semiconductor lithography involves the creation of three-dimensional relief images or patterns on a semiconductor substrate that can then be transferred to the substrate. In semiconductor lithography, the patterns are formed with a light-sensitive polymer called a photoresist. The lithography and etching pattern transfer steps are repeated multiple times to build the complex structures that make up the transistors and the numerous wires that connect the millions of transistors in a circuit. Each pattern printed on the wafer is aligned with previously formed patterns, and conductors, insulators, and selectively doped regions are gradually built up to form the final device.
[0022] 1A-1C are cross-sectional views of a PCM cell 100, for example for use in an integrated circuit (not shown). In the illustrated embodiment, the PCM cell 100 includes a bottom interconnect 102, a bottom electrode 104, an insulator 106, a heater 108, an insulator 110, a bottom protruding liner (PL) 112, a PCM material 114, a sidewall PL 116, an insulator 120, a top electrode 122, and a top interconnect 124.
[0023] In the illustrated embodiment, the bottom of the bottom electrode 104 is in direct contact and electrically connected to the top of the bottom wiring 102, which can receive electrical signals from other components of the integrated circuit (not shown). The bottom of the heater 108 is in direct contact and electrically connected to the top of the bottom electrode 104. The bottom of the bottom PL 112 is in direct contact and electrically and thermally connected to the top of the heater 108. The bottom of the PCM material 114 is in direct contact and electrically and thermally connected to the top of the bottom PL 112. The bottom of the top electrode 122 is in direct contact and electrically connected to the top of the PCM material 114. The bottom of the top wiring 124 is in direct contact and electrically connected to the top of the top electrode 122, and the top wiring 124 can convey electrical signals from the PCM cell 100 to other components of the integrated circuit (not shown).
[0024] In the illustrated embodiment, the bottom of the sidewall PL116 is in direct contact with and electrically and thermally connected to the top of the bottom PL112. Furthermore, the inside of the sidewall PL116 is in direct contact with and electrically and thermally connected to the outside of the PCM material 114, so that the sidewall PL116 laterally surrounds the outside of the PCM material 114. The sidewall PL116 thereby surrounds all parallel sides in one direction (e.g., vertically extending sides as shown in FIG. 1A) over the entire longitudinal length of the PCM material 114 and is adjacent to the end of the PCM material 114 (e.g., horizontally extending bottom as shown in FIG. 1A) that is covered by the bottom PL112. In the illustrated embodiment, the PCM material 114 has a cylindrical shape (e.g., as opposed to a prismatic shape), which means that only one lateral outside is surrounded. Furthermore, the inside of the sidewall PL116 is in direct contact with and electrically connected to the outside of the top electrode 122.
[0025] In the illustrated embodiment, the insulators 106, 110, 120 optionally structurally support, electrically insulate, and fill spaces between other components of the PCM cell 100 as needed. Thus, the outside of the bottom electrode 104 is in direct contact with and is laterally surrounded by the insulator 106, the outside of the heater 108 is in direct contact with and is laterally surrounded by the insulator 110. Additionally, the bottom side of the bottom PL 112 is in direct contact with and axially adjacent the insulator 110, and the sidewall PL and top trace 124 are in direct contact with and laterally and axially adjacent the insulator 120.
[0026] In the illustrated embodiment, the cross section of the PCM cell 100 (in the plane of the paper in FIGS. 1A-1C) may be circular, but in other embodiments, it may be rectangular, square, oval, or any other suitable shape. Furthermore, the widths of the PCM material 114, bottom PL 112, and top electrode 122 are the same, while the width of the heater 108 is substantially reduced (e.g., 3-7 times smaller, or about 5 times smaller). The PCM cell 100 may thereby be said to have a mushroom structure, through which an electrical signal (i.e., current) may flow from the bottom electrode 104 to the top electrode 122 through the heater 108, bottom PL 112, and PCM material 114.
[0027] In the illustrated embodiment, the bottom electrode 104 and the top electrode 122 are constructed from highly conductive materials such as metals or metal compounds, e.g., titanium nitride (TiN) or tungsten (W). The heater 108 is constructed from TiN or a highly resistive metal, e.g., titanium tungsten (TiW), tantalum nitride (TaN), or titanium aluminide (TiAl), and is an electrode with a relatively narrow cross-sectional area that focuses the current through the PCM cell 100. This allows the heater 108 to generate heat by resistive heating during an electrical pulse, which can be used to selectively change the temperature of the PCM material 114, e.g., above the crystallization and melting temperatures of the PCM material 114. Additionally, the heater 108 can be constructed from multiple different conductive materials that can be arranged in multiple layers.
[0028] In the illustrated embodiment, the insulators 106, 110, 120 are made of a material such as, for example, silicon nitride (SiN), silicon oxide (SiO 2), silicon carbide nitride (SiNC), or tetraethyl orthosilicate (TEOS). In some embodiments, all of the insulators 106, 110, 120 are the same material, while in other embodiments, different materials are used for some or all of the insulators 106, 110, 120. Additionally, the bottom PL 112 and sidewalls PL 116 are composed of moderately electrically resistive materials such as metals and / or semiconductors (e.g., TaN; tungsten nitride (WN); amorphous carbon (aC); doped aC; transparent conductive oxides such as tin-doped indium oxide (ITO), aluminum zirconium oxide (AZO), and highly resistive metal chalcogenides (e.g., titanium selenide (TiSe)), and other less conductive metal nitrides). The materials that compose the bottom PL 112 and sidewalls PL 116 can be the same or different. Additionally, the material that makes up bottom PL 112 and sidewall PL 116 has a higher electrical resistivity than the polycrystalline phase of PCM material 114 , but a lower electrical resistivity than the amorphous phase of PCM material 114 .
[0029] In the illustrated embodiment, the PCM material 114 consists essentially of a phase change material such as germanium-antimony-tellurium (GST), gallium-antimony-tellurium (GaST), or silver-iridium-antimony-telluride (AIST) material, although other materials may be used as desired. Examples of other PCM materials may include, but are not limited to, germanium-tellurium compound materials (GeTe), silicon-antimony-tellurium (Si-Sb-Te) alloys, gallium-antimony-tellurium (Ga-Sb-Te) alloys, germanium-bismuth-tellurium (Ge-Bi-Te) alloys, indium-tellurium (In-Te) alloys, arsenic-antimony-tellurium (As-Sb-Te) alloys, silver-indium-antimony-tellurium (Ag-In-Sb-Te) alloys, Ge-In-Sb-Te alloys, Ge-Sb alloys, Sb-Te alloys, Si-Sb alloys, Ge-Te alloys, and combinations thereof. The PCM material 114 may be undoped or doped (e.g., doped with one or more of oxygen (O), nitrogen (N), silicon (Si), or Ti). The terms "consisting essentially of" and "consisting essentially of" as used herein with respect to materials of different layers indicate that the presence of other materials does not substantially alter the basic properties of the listed materials. For example, a PCM material 114 consisting essentially of GST material does not include other materials that substantially alter the basic properties of the GST material.
[0030] In the illustrated embodiment, the PCM cell 100 can be operated as a memory cell by passing a current pulse from the bottom electrode 104 to the top electrode 122 to program the PCM cell 100. This can be done at various voltages and / or for various durations to read or write values on the PCM cell 100. For example, to write, a high voltage (e.g., 1 volt (V) to 4 V) can be used for a short period of time, which allows the heater 108 to locally heat the PCM material 114 above its melting point. When the current flow stops, the PCM material 114 can rapidly cool and an amorphous region 126 can form in a process called "reset." Region 126 is a dome-shaped region of the PCM material 114 that has an amorphous structure, while the remainder of the PCM material 114 is still polycrystalline (labeled "126B" in FIG. 1B and "126C" in FIG. 1C). Generally, this amorphous structure does not have a well-defined structure. However, there may be localized loose crystalline nuclei (i.e., small crystallized regions of the phase change material 114) in the regions 126. The formation of the regions 126 may increase the electrical resistance of the entire PCM cell 100 compared to a single polycrystalline structure (such as the PCM cell 100 of FIG. 1A). These resistance values of the PCM cell 100 can be read without changing the state of the PCM material 114 (including the state of the regions 126) or the resistance value of the PCM cell 100, for example, by sending a current pulse at a low voltage (e.g., 0.2 V) from the bottom electrode 104 to the top electrode 122.
[0031] Additionally, the PCM material 114 can be reprogrammed back to a single polycrystalline structure by "setting" the PCM cell 100. One method of reprogramming the PCM material 114 uses a high voltage electrical pulse (e.g., 1 V to 4 V) for a short period of time (e.g., 10 nanoseconds (ns)), which heats the PCM material 114 above its crystallization point, but not to its melting point. Because the crystallization temperature is lower than the melting temperature, the PCM material 114 can be annealed to form crystals when the current flow stops. Another method of reprogramming the PCM material 114 uses an electrical pulse with a relatively long trailing edge (e.g., 1 microsecond) that is strong enough to heat the PCM material 114 above its melting point (as opposed to a square pulse with a relatively short trailing edge on the order of nanoseconds), after which the PCM material 114 can be slowly cooled to form crystals. Either of these processes reduces the electrical resistance across the PCM cell 100 compared to having an amorphous region 126. This new resistance value can then be read using a current at a low voltage (eg, 0.2V) without changing the state of the PCM material 114 or the resistance value of the PCM cell 100.
[0032] In some embodiments, the melting temperature of the PCM material 114 is about 600° C. In some embodiments, the crystallization temperature of the PCM material 114 is about 180° C. Furthermore, the process of setting and resetting the PCM cell 100 can be repeated, and in some embodiments, different regions 126 having different resistances can be created in the PCM material 114 (e.g., due to having different sizes of the regions 126 and / or amounts of crystallization nuclei in the regions 126). This allows the PCM cell 100 to have a variety of different resistances that can be created by varying the reset parameters. Thereby, if the PCM cell 100 is considered to represent digits of information, these digits can be non-binary (as opposed to traditional bits). However, in some embodiments, the PCM cell 100 can be used as a bit by either having or not having uniform regions 126 in the PCM material 114. In such embodiments, the PCM cell 100 can have a high resistance (aka low voltage output or "0") or a low resistance (aka high voltage output or "1").
[0033] The components and configuration of the PCM cell 100 allow for additional current paths through the PCM cell 100. Instead of current flowing only from the bottom PL 112 to the top electrode 122 through the PCM material 114, current can also flow from the bottom PL 112 to the top electrode 122 through the sidewall PL 116. As previously discussed, the sidewall PL 116 has an electrical resistivity between the polycrystalline PCM material 114 and the amorphous PCM material 114 (e.g., region 126). This allows current to pass primarily through the PCM material 114 when there is contact with the bottom PL 112 (such as region 126B), but allows current to pass primarily through at least a portion of the sidewall PL 116 when region 126 covers the entire bottom PL 112 (such as region 126C).
[0034] Such a capability may be beneficial considering that the PCM cell 100 may suffer from resistance drift due to the inherent drift of the amorphized PCM material (i.e., region 126B). The PCM cell 100 may also suffer from circuit noise that may be ameliorated by incorporating bottom PL 112 and sidewall PL 116. The drift problem is further exacerbated by scaling the PCM cell 100 to small dimensions below about 60 nanometers (nm), where the amorphized volume of the PCM material may extend across the lateral width of the PCM material 114, forming region 126C. In the absence of sidewall PL 116, region 126C would result in the primary current flow across the amorphized PCM material, resulting in resistance drift within the PCM cell 100. While a larger PCM cell may have only a bottom PL (because the amorphous region does not cover the entire width of the PCM material), PCM cell 100 uses sidewall PL 116 to extend the benefits of bottom PL 112 to the sides of PCM material 114. These benefits may include reduced resistance drift, lower read resistance (so that PCM cell 100 can be read using a lower current pulse that has less impact on region 126), reduced noise when reading, increased control of heater 108, lower set resistance, and increased dynamic range of PCM cell 100.
[0035] 1A-1C depict one embodiment of the present disclosure, which includes alternative embodiments. For example, the PCM cell 100 may have a non-mushroom structure, such as a confined cell. Such a structure may lack a separate heater and instead rely on a bottom electrode to modulate the PCM material.
[0036] Figure 2 is a flow chart of a method 200 of manufacturing a PCM cell 100. Figures 3A-3I are a series of diagrams of a method 200 of manufacturing a PCM cell 100. Figures 2 and 3A-3I will now be described in conjunction with each other, with each operation of the method 200 being represented by one of Figures 3A-3I. Additionally, during this discussion, reference may be made to features of the PCM cell 100 shown in Figures 1A-1C.
[0037] In the illustrated embodiment, the method 200 begins at operation 202, where an insulating layer 328 is formed on the bottom electrode 104 and the insulator 106. In operation 204, a via 330 is formed in the insulating layer 328, for example, using an etch to form the insulator 110. In operation 206, a heater layer (not shown) is formed on the insulator 110 down to the bottom electrode 104, including the via 330, and a chemical mechanical polishing (CMP) is performed to remove excess metal to form the heater 108 adjacent the insulator 110. In operation 208, a bottom PL layer 334 is formed on the heater 108 and the insulator 110. Additionally, a PCM layer 336, a TiN layer 338, and a SiN layer 340 are formed on the bottom PL 112. In some embodiments, the PCM layer 336 is about 80 nm thick, the TiN layer 338 is about 75 nm thick, and the SiN layer 340 is about 220 nm thick. In operation 210 , masking and etching are performed to form the bottom PL 112 , the PCM material 114 , and the top electrode 122 .
[0038] In the illustrated embodiment, in operation 212, a sidewall PL layer 342 is formed (e.g., using ALD) in contact with the insulator 110, the bottom PL 112, the PCM material 114, and the top electrode 122. In operation 214, a portion of the sidewall PL layer 342 is selectively removed (e.g., using directional RIE or directional sputter etching) to form the sidewall PL 116. In operation 216, the insulator 110, the sidewall PL 116, and the top electrode 122 are encapsulated by forming an insulating layer 344 thereover. In operation 218, a hole 346 is formed in the insulating layer 344 to form the insulator 120, and a top wiring 124 is formed in the hole 346 and over the top electrode 122.
[0039] The components, configuration, and operation of the PCM cell 100 and method 200 allow the sidewall PL116 to be formed independently from the bottom PL112. This means that some or all of the parameters and properties (e.g., material, thickness, etc.) of the sidewall PL116 can be the same or different as desired from the bottom PL112. Varying such parameters / properties can result in differences between the bottom PL112 and the sidewall PL116, such as, for example, their electrical resistivities and / or electrical resistances.
[0040] FIG 4A is a graph of resistance versus current for various possible liner electrical resistivities for the PCM cell 100 (shown in FIG 1A). Since resistance is equal to resistivity times length divided by area, the graph is created assuming that the dimensions of the sidewall PL116 and bottom PL112 remain constant as their resistance ratio changes. FIG 4A includes a curve 448 representing a 1:1 ratio of the resistivity of the sidewall PL116 (shown in FIG 1A) to the resistivity of the bottom PL112 (shown in FIG 1A), a curve 450 representing a 2:1 ratio of the resistivity of the sidewall PL116 to the resistivity of the bottom PL112, and a curve 452 representing a 4:1 ratio of the resistivity of the sidewall PL116 to the resistivity of the bottom PL112. In some embodiments, sidewall PL116 can be an ALD film (e.g., for conformality), such as AlN, TiN, or TaN, and bottom PL112 can be a PVD film, such as aC or TaN. The resistivities of sidewall PL116 and bottom PL112 can then be adjusted, for example, by doping, to obtain the ratio of curves 448, 450, and 452.
[0041] In the illustrated embodiment, the current is displayed using a linear scale while the resistance is displayed using a logarithmic scale. Although not shown on the graph, if the PCM cell 100 did not include sidewall PL116 at all, the resistance would be substantially higher than curve 452 at higher currents. Furthermore, if the ratio of the resistivity of the sidewall PL116 to the resistivity of the bottom PL112 were reduced to less than 1:1, the resistance at higher currents would be lower than curve 448.
[0042] As shown by the graph, assuming region 126C reaches the end of PCM material 114 (as shown in FIG. 1C), increasing the relative resistivity of sidewall PL 116 allows for higher dynamic range and resolution / contrast between tuning states. However, such configurations may lead to increased resistance drift, so different configurations (e.g., resistance ratios) can be selected based on various advantages and disadvantages.
[0043] FIG. 4B is a graph of resistance versus current for various possible liner thickness ratios for the PCM cell 100 (shown in FIG. 1A). Since resistance is equal to resistivity times length divided by area, the graph is made assuming that the resistivity, length, and diameter of the sidewall PL116 and bottom PL112 remain constant as their thickness ratios change. FIG. 4B includes a curve 454 representing a 1:1 ratio of the thickness of the sidewall PL116 (shown in FIG. 1A) to the thickness of the bottom PL112 (shown in FIG. 1A), a curve 456 representing a 1:2 ratio of the thickness of the sidewall PL116 to the thickness of the bottom PL112, and a curve 458 representing a 1:4 ratio of the thickness of the sidewall PL116 to the thickness of the bottom PL112. In some embodiments, the thickness of the sidewall PL116 can be between 1 nm and 10 nm, and the thickness of the bottom PL112 can be between 1 nm and 5 nm. Thereby, for example, curve 454 can be obtained using a sidewall PL116 that is 4 nm thick and a bottom PL112 that is 4 nm thick, curve 456 can be obtained using a sidewall PL116 that is 2 nm thick and a bottom PL112 that is 4 nm thick, and curve 458 can be obtained using a sidewall PL116 that is 1 nm thick with a bottom PL112 that is 4 nm thick.
[0044] In the illustrated embodiment, the current is displayed using a linear scale while the resistance is displayed using a logarithmic scale. Although not shown on the graph, if the PCM cell 100 did not include sidewall PL116 at all, the resistance would be substantially higher than curve 458 at higher currents. Furthermore, if the ratio of the thickness of the sidewall PL116 to the thickness of the bottom PL112 were increased beyond 1:1, the resistance would be lower than curve 454 at higher currents.
[0045] Assuming that region 126C reaches the end of the PCM material 114 (as shown in FIG. 1C) as shown by the graph, increasing the relative thickness of the sidewall PL 116 allows for higher dynamic range and resolution / contrast between tuning states. However, such configurations may lead to increased resistance drift, so different configurations (e.g., thickness ratios) can be selected based on different advantages and disadvantages. Furthermore, both thickness and electrical resistivity can be varied to provide the appropriate electrical resistance for the sidewall PL 116 and bottom PL 112 of a given structure.
[0046] The description of various embodiments of the present invention is presented for illustrative purposes, but is not intended to be exhaustive or limited to the disclosed embodiments. Many modifications and variations will be apparent to those skilled in the art without departing from the scope and spirit of the described embodiments. The terms used in this specification are selected to best explain the principles of the embodiments, practical applications, or technical improvements beyond the art found in the market, or to enable other skilled in the art to understand the embodiments disclosed herein.
Claims
1. A phase change memory (PCM) cell having a mushroom structure, the PCM cell comprising: A first electrode; a heater electrically connected to the first electrode; a first protruding liner electrically connected to the heater; a PCM material electrically connected to the first protruding liner; a second electrode electrically connected to the PCM material; and a second protruding liner electrically connected to the first protruding liner and the second electrode; A PCM cell comprising:
2. the heater has a first width; the PCM material has a second width; 2. The PCM cell of claim 1, wherein the second width is greater than or equal to three times the first width.
3. The PCM cell of claim 2 , wherein the second width is approximately five times greater than the first width.
4. the first protruding liner is constructed from a first material; the second protruding liner is constructed from a second material; and 4. A PCM cell according to claim 1, wherein the second material is different from the first material.
5. the first material has a higher electrical resistivity in a polycrystalline phase than the PCM material and a lower electrical resistivity in an amorphous phase than the PCM material; and 5. The PCM cell of claim 4, wherein the second material has a higher electrical resistivity in a polycrystalline phase than the PCM material and a lower electrical resistivity in an amorphous phase than the PCM material.
6. the first protruding liner extends along an edge of the PCM material; 6. A PCM cell according to claim 1, wherein the second protruding liner extends along a side of the PCM material adjacent the edge.
7. the first protruding liner covers the edge of the PCM material; The PCM cell of claim 6 , wherein the second protruding liner surrounds the side of the PCM material along its entire longitudinal length.
8. A first electrode; a first protruding liner electrically connected to the first electrode, the first protruding liner having a first material; a PCM material electrically connected to the first protruding liner; a second electrode electrically connected to the PCM material; and a second protruding liner electrically connected to the first protruding liner and the second electrode, the second protruding liner having a second material; wherein the second material is different from the first material. A phase change memory (PCM) cell comprising:
9. The PCM cell of claim 8 further comprising a heater electrically connected to the first electrode and the first protruding liner.
10. the heater has a first width; the PCM material has a second width; 10. The PCM cell of claim 9, wherein the second width is greater than or equal to three times the first width.
11. the first protruding liner covers an edge of the PCM material; and 11. A PCM cell according to any one of claims 8 to 10, wherein the second protruding liner surrounds a side of the PCM material adjacent the end over its entire longitudinal length.
12. the first material has a higher electrical resistivity in a polycrystalline phase than the PCM material and a lower electrical resistivity in an amorphous phase than the PCM material; and 12. A PCM cell according to any one of claims 8 to 11, wherein the second material has a higher electrical resistivity in a polycrystalline phase than the PCM material and a lower electrical resistivity in an amorphous phase than the PCM material.
13. the first material has a first electrical resistivity; the second material has a second electrical resistivity; 13. The PCM cell of claim 8, wherein the second electrical resistivity is greater than or equal to twice the first electrical resistivity.
14. the first protruding liner has a first thickness; the second protruding liner has a second thickness; 14. A PCM cell according to any one of claims 8 to 13, wherein the second thickness is less than or equal to half the first thickness.
15. 1. A method of manufacturing a phase change memory (PCM) cell, the method comprising the steps of forming a first electrode; forming a first protruding liner electrically connected to the first electrode; forming a PCM material on the first protruding liner; forming a second electrode on the PCM material; and The method comprises forming a second protruding liner in contact with the first protruding liner, the PCM material, and the second electrode.
16. The method of claim 15 , further comprising forming a heater on the first electrode, wherein the first protruding liner is formed on the heater.
17. the heater has a first width; 17. The method of claim 16, wherein the PCM material has a second width; the second width being greater than or equal to three times the first width.
18. the first protruding liner is constructed from a first material; the second protruding liner is constructed from a second material; and 18. The method of any one of claims 15 to 17, wherein the second material is different from the first material.
19. 20. The method of claim 18, wherein the second material has a higher electrical resistivity in a polycrystalline phase than the PCM material and a lower electrical resistivity in an amorphous phase than the PCM material.
20. 20. The method of claim 19, wherein the first material has a higher electrical resistivity in a polycrystalline phase than the PCM material and a lower electrical resistivity in an amorphous phase than the PCM material.
Citation Information
Patent Citations
Phase change memory device for multibit storage
EP2034536A1
Phase change memory device for multi-bit storage device
JP2009071314A
Phase change memory using multiple stacks of PCM material
JP2023513219A
Stackable cross-point phase-change material memory array with a resistive liner
US10763307B1
Phase change memory using multiple phase change layers and multiple heat conductors
US20200395537A1