Method for patterning photonic devices

The combination of anisotropic dry and isotropic wet etching processes using hydrogen bromide and chlorine gas mixtures addresses the limitations of existing etching methods, achieving faster and more precise patterning of electro-optic components with reduced defects.

JP2024537838APending Publication Date: 2024-10-16CYQUANTUM CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024519983
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-01
Filing Date
2022-10-03
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

Existing methods for patterning and etching wafer stacks in electro-optic modulators and switches face limitations in precision, efficiency, and material selectivity, leading to defects and increased processing times.

Method used

An etching method involving a combination of anisotropic dry etching and isotropic wet etching processes, using hydrogen bromide and chlorine gas mixtures, is employed to pattern metal oxide layers such as barium titanate and strontium titanate, with optional use of hard masks like silicon dioxide and silicon nitride, to improve selectivity and reduce defects.

Benefits of technology

The method achieves faster etch rates, reduces defects, and enhances control over critical dimensions and profile, resulting in higher precision and reduced processing times for electro-optic components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024537838000001_ABST
    Figure 2024537838000001_ABST
Patent Text Reader

Abstract

The etching method includes forming a metal oxide layer, including a barium titanate layer or a strontium titanate layer, on a substrate; forming a patterned masking layer on the metal oxide layer; performing an anisotropic dry etching process to etch the metal oxide layer in areas not covered by the patterned masking layer; and performing an isotropic wet etching process to remove residues not removed by the anisotropic dry etching process to form a patterned metal oxide layer.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] SUMMARY OF THE DISCLOSURE Embodiments herein generally relate to methods for etching materials to produce components of electro-optical devices such as phase shifters and switches. [Background technology]

[0002] Electro-optic (EO) modulators and optical switches are useful components for the control and manipulation of optical signals. Some EO modulators utilize free-carrier electrorefraction, free-carrier electroabsorption, the Pockels effect, or the DC Kerr effect to modify optical properties during operation, for example, to change the phase of light propagating through the EO modulator or switch. Optical phase modulators can be used in integrated optical systems, waveguide structures, integrated optoelectronics, etc. Summary of the Invention [Problem to be solved by the invention]

[0003] Despite the advances being made in the field of EO modulators and switches, there is a continuing need for improvements in the methods and systems associated with patterning and etching wafer stacks used in EO modulators, switches, and related devices. [Means for solving the problem]

[0004] In one embodiment, an etching method includes forming a metal oxide layer, including a barium titanate layer or a strontium titanate layer, on a substrate; forming a patterned masking layer on the metal oxide layer; performing an anisotropic dry etching process to etch the metal oxide layer in areas not covered by the patterned masking layer; and performing an isotropic wet etching process to remove residues not removed by the anisotropic dry etching process to form a patterned metal oxide layer.

[0005] In a further embodiment, an etching method includes forming a metal oxide layer including a barium titanate layer or a strontium titanate layer on a substrate, forming a patterned masking layer on the metal oxide layer, performing a first anisotropic dry etching process to etch the metal oxide layer in areas not covered by the patterned masking layer, and performing a second anisotropic dry etching process having a higher ion bombardment than the first anisotropic dry etching process to remove residue not removed by the first anisotropic dry etching process and form a patterned metal oxide layer.

[0006] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate exemplary embodiments of the present disclosure and, together with the general description given above and the detailed description given below, serve to explain features of the present disclosure. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a simplified schematic diagram illustrating an optical switch according to various embodiments. [Diagram 2] FIG. 2 is a schematic diagram of a pre-fabricated wafer including stack layers, according to various embodiments. [Figure 3A] FIG. 3A is a simplified schematic diagram showing a cross section of a waveguide structure showing the direction of an induced electric field according to various embodiments. [Figure 3B] FIG. 3B is a simplified schematic diagram showing a cross section of a waveguide structure according to various embodiments. [Figure 4] FIG. 4 is a simplified schematic diagram illustrating a top view of a waveguide structure, according to various embodiments. [Diagram 5] FIG. 5 is a schematic diagram of a wafer etching apparatus, according to various embodiments. [Figure 6] FIG. 6 is a schematic diagram illustrating an ion milling etching procedure. [Figure 7]FIG. 7 is a schematic illustration of etching an electro-optic layer using an ionized partial gas mixture, according to various embodiments. [Figure 8] FIG. 8 is a schematic illustration of a thin SiO 2 hard mask that can be used to etch a wafer, according to various embodiments. [Figure 9] FIG. 9 is a schematic illustration of a thin Si3N4 hard mask that can be used to etch a wafer, according to various embodiments. [Figure 10] FIG. 10 is a schematic illustration of a thick SiO 2 hard mask that can be used to etch a wafer, according to various embodiments. [Figure 11] FIG. 11 is a schematic illustration of a thick Si3N4 hard mask that can be used to etch a wafer, according to various embodiments. [Figure 12A] FIG. 12A is a cross-sectional side view of an intermediate structure that can be used in forming an optical component, according to various embodiments. [Figure 12B] FIG. 12B is a cross-sectional side view of a further intermediate structure that can be used in forming an optical component, according to various embodiments. [Figure 12C] FIG. 12C is a cross-sectional side view of a further intermediate structure that can be used in forming an optical component, according to various embodiments. [Figure 13A] FIG. 13A is a cross-sectional view of an optical component according to various embodiments. [Figure 13B] FIG. 13B is a cross-sectional view of an optical component according to various embodiments. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Various embodiments will now be described in detail with reference to the accompanying drawings. The drawings, which are not necessarily to scale, are intended to illustrate various features of the present disclosure. Wherever possible, the same reference numbers will be used throughout the drawings to refer to the same or like parts. References made to specific examples and implementations are for illustrative purposes only and are not intended to limit the scope of the disclosure or the claims.

[0009] It will also be understood that, although terms such as "first", "second", etc. are used in some cases herein to describe various elements, these elements should not be limited by these terms. These terms are used only to distinguish one element from another. For example, a first electrode layer can be referred to as a second electrode layer, and similarly, a second electrode layer can be referred to as a first electrode layer, without departing from the scope of the various embodiments described. The first electrode layer and the second electrode layer are both electrode layers, but are not the same electrode layer.

[0010] The disclosed embodiments relate to etching and patterning methods for constructing components of optical systems. Although example embodiments are provided in the context of integrated optical systems that include active optical devices, the disclosure is not limited to such examples and has broad applicability to a variety of optical and optoelectronic systems.

[0011] According to some embodiments, the active photonic devices described herein utilize electro-optic effects such as free carrier induced refractive index change in semiconductors, Pockels effect, and / or DC Kerr effect to perform modulation and / or switching of optical signals. Thus, the embodiments are applicable to both modulators where transmitted light is modulated either ON or OFF, or where light is modulated by partial change in transmittance, as well as optical switches where transmitted light is output on a first output (e.g., a waveguide) or a second output (e.g., a waveguide) or optical switches with three or more outputs and two or more inputs. Thus, the embodiments of the present disclosure are applicable to various system configurations including M(input)×N(output) systems utilizing the methods, devices, and techniques discussed herein. Some embodiments also relate to electro-optic phase shifter devices, also referred to herein as phase adjustment sections, that can be used within the switches or modulators.

[0012] FIG. 1 is a simplified schematic diagram illustrating an optical switch according to various embodiments. Referring to FIG. 1, switch 100 includes two inputs, input 1 and input 2, and two outputs, output 1 and output 2. As an example, the inputs and outputs of switch 100 can be implemented as optical waveguides configured to support single-mode or multimode optical beams. As an example, switch 100 can be implemented as a Mach-Zehnder interferometer coupled to a set of 50 / 50 beam splitters 105 and 107, respectively. As shown in FIG. 1, input 1 and input 2 are optically coupled to a first 50 / 50 beam splitter 105, also referred to as a directional coupler. The first 50 / 50 beam splitter 105 receives light from input 1 or input 2 and directs 50% of the input light from input 1 to waveguide 110 and 50% of the input light from input 1 to waveguide 112 through evanescent coupling within the 50 / 50 beam splitter. At the same time, the first 50 / 50 beam splitter 105 directs 50% of the input light from input 2 to waveguide 110 and 50% of the input light from input 2 to waveguide 112. If only the input light from input 1 is considered, this input light is split evenly between waveguide 110 and waveguide 112.

[0013] Mach-Zehnder interferometer 120 includes phase adjustment section 122. A voltage V0 can be applied across the waveguide in phase adjustment section 122 such that the waveguide can have a controllably altered refractive index in phase adjustment section 122. Because the light in waveguides 110 and 112 can continue to have a well-defined phase relationship (e.g., in phase, 180 degrees out of phase, etc.) after propagating through first 50 / 50 beam splitter 105, phase adjustment in phase adjustment section 122 can introduce a predetermined phase difference between the light propagating in waveguide 130 and the light propagating in waveguide 132. Depending on the phase relationship between the light propagating in waveguide 130 and the light propagating in waveguide 132, the output light may be present at output 1 (e.g., if the light beams are in phase) or at output 2 (e.g., if the light beams are out of phase), thereby providing a switching function such that light is directed to output 1 or output 2 as a function of the voltage V applied to phase adjustment section 122. Although a single active arm is shown in Figure 1, in other embodiments, both arms of the Mach-Zehnder interferometer may include a phase adjustment section.

[0014] In comparison to all-optical switch technology, electro-optical switch technology uses an electrical bias (e.g., V0 in FIG. 1) applied across the active area of ​​the switch to create an optical change. The electric field and / or current induced by the application of this voltage bias causes a change in one or more optical properties of the active area, such as refractive index or absorbance. Although a Mach-Zehnder interferometer implementation is shown in FIG. 1, the present disclosure is not limited to this particular switch architecture and other phase adjustment devices, including ring resonator designs, Mach-Zehnder modulators, generalized Mach-Zehnder modulators, etc., are also within the scope of the present disclosure.

[0015] The optical switch shown in FIG. 1 may include a waveguide structure patterned from a wafer. FIG. 2 illustrates an exemplary wafer that may be received from a wafer manufacturer and etched according to embodiments described herein to produce a waveguide structure. FIG. 2 illustrates a cross-section of a first wafer including a layer stack that may be received as part of the fabrication process of the various devices described herein, according to various embodiments. As illustrated, a first insulating substrate layer 202 may be (optionally) disposed below a seed layer 204, which is disposed below an electro-optic layer 206, which is (optionally) disposed below an electrode layer 208, which is (optionally) disposed below a second insulating substrate layer 210. Alternatively, the electrode layer 208 may be disposed between the electro-optic layer 206 and the first insulating substrate layer 202. Although FIG. 2 illustrates that each of the five layers 202-210 are present, any one or more of these layers may be absent in various embodiments. In other words, the first wafer can be of various types depending on the particular fabrication method used, and the seed layer, electrode layer, and second substrate layer may or may not be optionally present as desired. One or more of the layers shown in Figure 2 can be chemically etched to produce electro-optical components according to embodiments described herein.

[0016] Each of the layers of the wafer can be any of a variety of types of materials. For example, the electrode layer 208 can include a conductive material such as a metal, or alternatively, can be composed of a semiconductor material. In various embodiments, the electrode layer can include one of gallium arsenide (GaAs), aluminum gallium arsenide (AlGaAs) / GaAs heterostructures, indium gallium arsenide (InGaAs) / GaAs heterostructures, zinc oxide (ZnO), zinc sulfide (ZnS), indium oxide (InO), doped silicon, strontium titanate (STO), doped STO, barium titanate (BTO), barium strontium titanate (BST), hafnium oxide, lithium niobate, zirconium oxide, titanium oxide, graphene oxide, tantalum oxide, lead zirconate titanate (PZT), lead lanthanum zirconium titanate (PLZT), barium strontium niobate (SBN), aluminum oxide, aluminum oxide, doped variants or solid solutions thereof, or a two-dimensional electron gas. For embodiments in which the electrode layer may include doped STO, the STO may be either niobium doped or lanthanum doped, or may include vacancies, according to various embodiments.

[0017] In various embodiments, the electro-optic layer 206 can include one or more of STO, BTO, BST, hafnium oxide, lithium niobate, zirconium oxide, titanium oxide, graphene oxide, tantalum oxide, PZT, PLZT, SBN, aluminum oxide, aluminum oxide, or doped variants or solid solutions thereof. The electro-optic layer can be constructed from a transparent material that has a refractive index greater than the refractive index of the first and second insulating substrate layers in some embodiments.

[0018] FIG. 3A is a simplified schematic diagram showing a cross section of an exemplary completed waveguide structure according to some embodiments. In FIG. 3A, the direction of the induced electric field is indicated with an arrow. The waveguide structure shown in FIG. 3A can be fabricated from the wafer shown in FIG. 2 by performing the etching techniques of the embodiments described herein. FIG. 3A shows two electrical contacts, each of which includes a lead (330 and 332) connected to an electrode (340 and 342). It should be noted that as used herein, the term "electrode" refers to a device component that directly couples to the waveguide structure (e.g., to modify the voltage drop across the waveguide structure and actuate the photonic switch). Additionally, the term "lead" can refer to a back-end structure that couples the electrode to other components of the device (e.g., the lead can couple the electrode to a controllable voltage source), but is isolated from the waveguide structure and is not directly coupled to the waveguide structure. In some embodiments, the lead can be composed of a metal (e.g., copper, gold, etc.) or alternatively a semiconductor material.

[0019] As shown, Figure 3A shows a photonic device that includes a first cladding layer 310 and a second cladding layer 312 on either side of a waveguide. Note that the terms "first" and "second" are intended merely to distinguish between the two cladding layers, e.g., the term "first cladding layer" can refer to a cladding layer on either side of a waveguide.

[0020] 3A further illustrates a slab layer 320 including a first material coupled to a first electrode of the first electrical contact and a second electrode of the second electrical contact. In some embodiments, the waveguide structure further includes a ridge portion 351 comprised of the first material (or a different material) and coupled to the slab layer, the ridge portion being disposed between the first electrical contact and the second electrical contact.

[0021] As shown in Figure 3A, the small arrows indicate the induced electric field direction, which is generally oriented along the positive x-direction through the electrodes of the device. The electric field is convexly curved both above and below the electrodes as shown. Additionally, the large arrow 350 pointing in the positive x-direction indicates the direction of polarization of the optical mode that may travel through the slab layer and the waveguide.

[0022] 3B illustrates an architecture in which a ridge portion of the waveguide structure 351 is disposed on the top side of the slab layer and extends into the first cladding layer 312, with the first and second electrodes coupled to the slab layer on the bottom side of the slab layer opposite the top side. As shown, the combination of the ridge portion and slab layer has a first thickness 362 that is greater than the second thickness 360 of the slab layer 320 alone, with the excess of the first thickness over the second thickness extending into the first cladding layer 312 on the top side of the slab layer 320. As shown in FIG. 3B, the first and second electrodes 340 and 342 can be coupled to the slab layer 320 on the bottom side of the slab layer opposite the top side. Additionally, the first electrical contact 330 can be coupled to the first electrode 340 by penetrating the slab layer 320 from the top side of the slab layer to the bottom side of the slab layer, and the second electrical contact 332 can be coupled to the second electrode 342 by penetrating the slab layer 320 from the top side of the slab layer to the bottom side of the slab layer.

[0023] 4 is a top-down view of the photonic phase shifter architecture of FIGs. 3A and 3B that can be patterned according to embodiments described herein. As shown, the phase shifter can include first and second leads 430 and 432, first and second electrodes 440 and 442, a slab (e.g., waveguide) layer 420, and a ridge portion 451 of the waveguide structure.

[0024] FIG. 5 is a schematic diagram illustrating a wafer etching apparatus 600 according to some embodiments. The illustrated wafer etching apparatus is one example of a wafer etching apparatus. In other embodiments, various other types of apparatus can be used to perform the etching processes described herein. As shown, process gases (e.g., a combination of HBr and Cl2, among others) can be inserted through the top of the etching process chamber 602 and can be dispersed over the upper region of the chamber using a showerhead 604. As shown, an inductor coil 606 wrapped around the chamber 602 is connected to a high frequency (HF) radio frequency (RF) generator (e.g., a 60 MHz RF generator) 608 configured to introduce a fast oscillating magnetic field into the chamber 602.

[0025] The induced oscillating magnetic field can interact with the process gas and ionize the gas. At the bottom of the chamber 602, a low frequency (LF) RF generator (e.g., a typically 13.5 MHz generator, or another frequency) 610 can be capacitively coupled to a pedestal 612 to introduce an oscillating capacitive charge onto the top surface of the pedestal. This LF oscillating charge accelerates ionized gas particles downward to collide with a wafer (e.g., a substrate including one or more layers to be etched) 614 positioned on the pedestal 612 to chemically etch the wafer. Finally, gaseous chemical by-products of the chemical etching reaction can be pumped through a low intensity pump 616 at the bottom of the chamber 602.

[0026] The construction of components of the electro-optical systems described above can involve etching processes that transform wafers into electro-optical components such as waveguide structures. Conventional methods of wafer etching exhibit limitations, and embodiments herein present improved methods of wafer etching.

[0027] FIG. 6 illustrates an ion milling method for etching BTO (i.e., BaTiO3). BTO is a difficult material to pattern using reactive ion etching (RIE) because it does not form volatile by-products with fluorine or chlorine, the halogen compounds commonly used in plasma etching. The chemical by-products of etching BTO using conventional fluorine and chlorine are non-volatile below about 1500° C. Thus, these by-products may not desorb from the wafer at the temperatures and pressures available in an RIE chamber. As a result, as shown in FIG. 6, some previous implementations of patterning a BTO layer 20 have focused on ion beam etching using argon, a process that is slow and has little selectivity to the mask (e.g., silicon oxide hard mask) 22. During ion milling, argon ions are accelerated toward the BTO surface and physically dislodge barium and titanium atoms. These atoms are then pumped out through an exhaust tube. However, the etched atoms can often redeposit elsewhere on the surface of the wafer, causing undesirable defects. In addition, ion milling is non-selective because effective use of the hard mask may require the hard mask 22 to be thicker than the desired patterning depth, which can result in increased material costs and etch times.

[0028] To address these and other concerns, embodiments herein provide a method in which a BTO layer 20 is etched using a mixture of hydrogen bromide (HBr) and chlorine (Cl2) to form volatile by-products BaBr2 and TiCl4, respectively. As shown in FIG. 7, a partial gas mixture of HBr and Cl2 is ionized, and the ionized gas is used to etch the BTO. BaBr2 becomes volatile at 120° C. at 1 atmosphere pressure, which is well within the feasibility of a conventional RIE chamber. In various embodiments, some integration scheme with a SiO2 hardmask 22 or a Si3N4 hardmask 24 can be used to pattern the wafer, since both materials are compatible with HBr / Cl2-containing chemistries.

[0029] In some embodiments, the presence of oxygen, hydrogen, and / or argon ions in the plasma can aid in the formation of BaBr2. The oxygen, hydrogen, and / or argon ions can be accelerated toward the surface at lower energies compared to those used in ion milling. The Br and Cl radicals are electrically neutral and can diffuse to the wafer surface. Both by-products easily desorb from the wafer surface and can be pumped out of the chamber without redepositing on the wafer.

[0030] An additional advantage is that the HBr / Cl2 mixture is selective to SiO2 or Si3N4 hardmasks. The etch rate of BTO is also faster using chemically assisted etching compared to physical ion milling processes, and chemically assisted etching has a lower risk of striations that result in line edge roughness. Figures 8-11 show various methods of utilizing a hardmask when patterning the electro-optic layer, according to various embodiments.

[0031] FIG. 8 illustrates the use of a SiO2 hard mask 22 to pattern the BTO layer 20. In one embodiment, the BTO layer 20 can be used as the slab / ridge electro-optic layer 320 in the device of FIG. 3B. The SiO2 hard mask 22 is selected because this material is highly selective to SiO2 in HBr-based plasmas. The hard mask 22 can be patterned in a prior step. Optionally, an STO layer 40 can be disposed under the BTO layer 20. The STO layer 40 can be used to form the dielectric electrodes 340, 342 of FIG. 3B. The STO layer 40 can be patterned prior to forming the BTO layer 20 by any suitable method, such as ion milling. The optional STO layer 40 and the BTO layer 20 can be formed over an insulating substrate layer 202, such as a silicon dioxide layer or a silicon nitride layer, as described above with respect to FIG. 2.

[0032] The insulating substrate layer 202 may be a temporary layer that is subsequently removed or may be retained as a cladding layer in the final electro-optical device. Additionally, a seed layer 204 may also be optionally formed under the BTO layer 20 as described above. The seed layer 204 may be subsequently removed or may be retained in the final electro-optical device. As shown, the BTO layer 20 is etched using HBr / Cl2 chemistry. In addition to the two main etch gases, O2 is added for selectivity and profile control over the SiO2 hard mask 22, and Argon is added to provide energy in the form of ion bombardment.

[0033] 9 illustrates the use of a silicon nitride (Si3N4) hardmask 24 to pattern the BTO layer 20. Silicon nitride is similar to silicon dioxide in that it is difficult to etch using HBr, which results in high selectivity similar to that of the SiO2 hardmask 22, and the BTO layer 20 is etched using the HBr / Cl2 chemistry. In addition to the two main etch gases, O2 is added for profile control and argon is added to provide energy in the form of ion bombardment, just like with the SiO2 hardmask.

[0034] FIG. 10 shows a SiO2 hard mask 22 similar to that shown in FIG. 8 that can be used to pattern the BTO layer 20 in some embodiments. The hard mask 22 is thicker than in FIG. 8 due to the increased etch depth. The BTO layer 20 and the STO layer 40 are etched together using HBr / Cl2 chemistry, or, optionally, by etching the STO layer 40 using ion milling after the BTO layer 20 is etched using HBr / Cl2 chemistry. In addition to the two main etch gases, O2 is added for selectivity and profile control to the SiO2 hard mask 22, and argon is added to provide energy in the form of ion bombardment. In this embodiment, the entire BTO stack is etched and the process stops on the underlying SiO2 insulating substrate layer 202.

[0035] FIG. 11 shows a Si3N4 hard mask 24 similar to that shown in FIG. 9 that can be used to pattern the BTO layer 20. The hard mask 24 is thicker than that shown in FIG. 9 to accommodate the increased etch depth. The BTO layer 20 and the STO layer 40 are etched together using HBr / Cl2 chemistry, or, optionally, by etching the STO layer 40 using ion milling after the BTO layer 20 is etched using HBr / Cl2 chemistry. In addition to the two main etch gases, O2 is added for selectivity and profile control to the silicon nitride hard mask 22, and argon is added to provide energy in the form of ion bombardment. In this embodiment, the entire BTO stack is etched and the process stops on the underlying SiO2 insulating substrate layer 202.

[0036] The embodiments described herein for etching the BTO layer 20 provide advantages over existing methods such as ion milling using argon ions mixed with fluorine. The by-products produced by the embodiments herein easily desorb from the surface, so that the wafer produced (i.e., the insulating substrate layer 202 supporting the etched BTO layer 20) can exit the process chamber 602 shown in FIG. 5 with fewer defects compared to wafers produced using ion milling processes. In addition, chemically assisted etching has a faster etch rate, resulting in shorter processing times. Furthermore, the etching methods described according to some embodiments can have more adjustable parameters such as pressure, power and gas composition that allow for improved control of the process. The embodiments herein provide improved selectivity to hard masks, simplifying process integration. The chemical etching methods described herein are less physical than ion milling, reducing the risk of striations and edge channeling that further cause line edge roughness.

[0037] In some embodiments, HBr may react with moisture from the air and redeposit on the wafer. This redeposition is called time-dependent haze and can be dissolved during wafer cleaning. In some embodiments, unprocessed wafers can be physically separated from processed wafers. This can prevent haze from adhering to the surface of the unprocessed wafer and causing micromasking.

[0038] As mentioned above, patterning of BTO and STO thin films and materials using conventional plasma dry etching may not be effective in removing Ba and Sr atoms because BTO does not form volatile by-products with fluorine or chlorine, which are halogen compounds commonly used in plasma etching. Therefore, the use of such conventional techniques requires plasma dry etching with a high sputter component. However, the use of such a process results in faster erosion of the mask material and therefore reduced mask etch selectivity. In this regard, high sputter etching can increase micromask defects, residue, and surface roughness. Furthermore, this can cause preferential etching of Ti over Ba or Sr due to the higher volatility of Ti etch products. One approach to avoid these problems is to use an etching process based on HBr and Cl2, as described above with reference to Figures 7-11. In an alternative embodiment, a two-step dry / wet etch can be used, as described in more detail below.

[0039] An alternative embodiment uses a first plasma dry etch to pattern the BTO / STO material with high fidelity, followed by a wet etch to remove the Ba- and / or Sr-containing residues by creating Ba- and / or Sr-containing etch products (e.g., Ba- and / or Sr-containing compound residues as a result of a chemical reaction) that can be dissolved in aqueous solution. The use of a two-step dry / wet etch process can have advantages over the use of either dry or wet etching individually. In addition to the disadvantages of using dry etching alone as mentioned above, dry etching (e.g., ion beam etching or ion milling) may have slow etch rates and may not be available for the fabrication of 300 mm wafers. The use of isotropic wet etching alone may result in rough line edge features due to preferential etching of grain boundaries or other defects. Furthermore, maintaining tight critical dimension (CD) and profile control (such as sidewall angle) may be difficult due to wet etch rate variations and isotropic behavior.

[0040] BTO and / or STO thin film (i.e., layer) patterning can be performed using a masking layer. In some embodiments, photoresist can be used as the masking layer, while in other embodiments, other suitable masking materials (e.g., hard masks such as silicon oxide, silicon nitride, metal, carbon, etc.) may be used. The portions of the BTO or STO film that are not covered by the masking layer can be subjected to either a chemical reaction or physical bombardment, or a combination of these two processes, to remove the BTO film. In one embodiment, the unmasked portions of the BTO or STO film can be fully or partially etched using a two-step dry / wet etching process without leaving any film or process by-products.

[0041] In the first step, a plasma dry etching process, which is an anisotropic etching process, can be used to define the patterning structure. Such an anisotropic etch can be used to maintain the CD defined by the mask material and generate low line edge roughness defined by low edge roughness of the edges of the mask material. Since the plasma dry etch may not effectively remove the Ba- and / or Sr-containing residues (e.g., Ba- and / or Sr-containing compounds such as BaF2, BaCl2, SrF2 and / or SrCl2) remaining in the etched areas, a second step including a wet etch chemistry that also etches BTO and STO can be applied to remove the Ba- and / or Sr-containing residues, dissolve and remove the remaining Ba- and / or Sr-containing residues by dissolving the Ba or Sr compounds, or undercutting the portion of the film under the Ba- and / or Sr-containing residues. The wet etch can include a halogen-containing etchant chemistry that optionally contains at least one of an acid or an oxidizing agent. However, non-halogen containing etchant chemistries can also be used.

[0042] FIG. 12A is a vertical cross-sectional view of an intermediate structure 1200a that can be used to form an optical component, according to various embodiments. The intermediate structure 1200a can include an electro-optic layer 20L formed on a substrate 202. The electro-optic layer 20L can be deposited as a blanket (i.e., unpatterned) layer and can include an electro-optic material such as BTO or STO, as described above. The intermediate structure 1200a can further include a patterned masking layer, such as a photoresist masking layer 26. Alternatively, the SiO2 hard mask 22 or the Si3N4 hard mask 24 described above can be used instead as a masking layer. The patterned photoresist 26 can be formed by depositing a blanket layer (not shown) of a photoresist material and patterning the photoresist material using photolithography techniques to form the patterned photoresist 26. The patterned photoresist 26 can then be used as a mask layer to selectively etch the electro-optic layer 20L.

[0043] FIG. 12B is a longitudinal cross-sectional view of an intermediate structure 1200b that can be used to form an optical component, according to various embodiments. The intermediate structure 1200b of FIG. 12B includes an etched electro-optic layer 20 that can be formed after a first dry etching process is performed on the electro-optic layer 20L of FIG. 12A. In this embodiment, the dry etching may be stopped before etching through the entire thickness of the unmasked portion of the electro-optic layer 20L and before reaching the surface of the substrate 202. As shown in FIG. 12B, the etched electro-optic layer 20 may include various surface defects 1208 due to incomplete removal of the Ba and / or Sr components (e.g., Ba and / or Sr residues). As described in more detail below with reference to FIG. 12C, a wet etching process may then be performed to remove the surface defects 1208 and to further etch the etched electro-optic layer 20.

[0044] FIG. 12C is a vertical cross-sectional view of an intermediate structure 1200c that can be used to form an optical component, according to various embodiments. As shown in FIG. 12C, a wet etching process can be used to remove surface defects 1208 left behind by a dry etching process. In this embodiment, the wet etch may be stopped before etching through the entire thickness of the unmasked portions of the electro-optic layer 20 and before reaching the surface of the substrate 202. As mentioned above, the wet etch is an isotropic etch in contrast to the dry etch, which is an anisotropic etch. Thus, as shown in FIG. 12C, the wet etch can remove portions of the etched electro-optic layer 20 below the patterned photoresist 26, thereby creating an undercut region with tapered sidewalls 20S.

[0045] FIG. 13A is a longitudinal cross-sectional view of an optical component 1300a, according to one embodiment. The optical component 1300a can be formed using the process described above with reference to FIGS. 12A-12C. In this regard, a first dry etching process can be performed on the intermediate structure 1200a (see, for example, FIG. 12A) to produce the intermediate structure 1200b of FIG. 12B. A wet etching process can then be performed on the intermediate structure 1200b to remove surface defects 1208 and isotropically etch the portions of the etched electro-optic layer 20 underlying the patterned photoresist 26. The etched electro-optic layer 20 of FIG. 13A can include a ridge portion 20R having tapered sidewalls 20S and horizontal layer portions 20H located on each side of the ridge portion 20R on the substrate 202. At least the ridge portions 20R can function as a waveguide in the optical component 1300a. The electro-optical component 1300a may then be formed by removing the patterned photoresist 26 (e.g., with a chemical solvent or by ashing) and forming a first electrode 340 and a second electrode 342 on the horizontal portion 20H of the etched electro-optical layer 20.

[0046] FIG. 13B is a vertical cross-sectional view of an optical component 1300b according to an alternative embodiment. In this embodiment, the electro-optic layer 20 includes a BTO layer, and an additional STO layer 40 is formed between the substrate 202 and the BTO layer. In this embodiment, dry etching and / or wet etching can etch through the entire thickness of the unmasked portion of the electro-optic layer (e.g., BTO layer) 20 and reach the surface of the underlying STO layer 40. The etched electro-optic layer 20 includes only the ridge portion 20R with tapered sidewalls 20S that rest on the underlying STO layer 40. Portions of the STO layer 40 can function as dielectric electrodes, or additional electrodes 340, 342 can be formed on the STO layer 40, as shown in FIG. 13B.

[0047] The above-mentioned two-step etching method can be implemented using various techniques of dry etching process and wet etching process. For example, dry etching process can include RIE, capacitively coupled plasma RIE, inductively coupled plasma RIE, electron cyclotron resonance RIE, neutral density RIE, magnetically enhanced RIE, ion milling or ion beam etching, gas cluster ion beam etching, etc. Exemplary dry etchant chemistries can include Ar, BCl3, Cl2, C2HClF4, CHClF2, C4F8, C4F6, C5F8, CF4, CH4, CHF3, SF6, HBr, NF3, and / or halogen-containing etchants, etc. Etchant chemistries can further include various combinations of the above-referenced materials. These materials can further include gases including O2, H2, He, N2, CO, and combinations of the above-mentioned etching gases and gases.

[0048] Exemplary wet etchant chemistries can include hydrofluoric acid, buffered hydrofluoric acid using ammonium fluoride, buffered oxide etch (BOE), hydrochloric acid, sulfuric acid, nitric acid, phosphoric acid, acetic acid, citric acid, ammonium hydroxide, and combinations of the above acids or bases. The above combinations of the above acids or bases can further include an oxidizing agent, such as hydrogen peroxide.

[0049] In other embodiments, various other processes can be used. For example, ion beam etching (i.e., micromachining) can be used for the first etching step rather than dry plasma etching. The embodiment described above includes the use of photoresist as the etch mask 26. Alternatively, other materials (e.g., silicon oxide or silicon nitride, etc.) can be used for the etch mask. In the embodiment of Figures 12A-12C, the wet etching process was performed before removal of the patterned photoresist. Alternatively, the patterned photoresist can be removed before performing the wet etch. As described above, there are many ways to modify the wet etch chemistry that removes the residual etch products. In the embodiment described above, an anisotropic dry etch was followed by an isotropic wet etch. In further embodiments, the anisotropic dry etch can be followed by an isotropic dry etch, thereby undercutting the material underlying the Ba and / or Sr. The residual etch material can then be removed by rinsing the sample with a liquid.

[0050] In some embodiments, it may be advantageous to perform a wet etch before the dry etch. In this manner, an initial wet etch can act to clean the etch surface before the dry etch as well as to increase the taper of the sidewall 20S if increased taper is desired. In other embodiments, multiple sequences of dry / wet etches or other etch sequences (e.g., dry, wet, dry, wet; dry, dry; wet, wet; etc.) can be performed.

[0051] For example, a low ion bombardment dry etch, such as a chemical dry etch, can be performed first to maintain the etch mask 26. A high ion bombardment etch, such as a sputter etch or ion beam milling, can be performed after the low ion bombardment etch to remove residue. Thus, removal or damage to the etch mask 26 during the high ion bombardment etch is not significant, especially if the high ion bombardment etch is performed only to remove residue and for a shorter time than the low ion bombardment etch.

[0052] Thus, in various embodiments, any serial combination of ion beam etching, dry etching, and wet etching can be performed. Various tools such as spray tools, vapor tools, etching baths, etc. can also be used for the wet etching steps.

[0053] The above-described embodiments provide various advantages over conventional approaches that use only a single dry etch process. In a two-step etch process, critical feature dimensions with potentially low edge roughness can be formed using a dry etch process followed by a wet etch process to remove the non-volatilized residual elements of Ba and / or Sr. Since the residue does not need to be completely removed by the plasma dry etch, a hard mask material is not required for the dry etch step. This is because any residue remaining from the dry etch step can be removed by the wet etch step. Thus, a soft, removable mask material such as photoresist can be used as a mask for the dry etch process. The use of photoresist rather than a hard mask has advantages in that the process flow can be simplified. Additionally, the use of a plasma dry etch followed by a short wet etch can improve pattern CD and profile control compared to using a wet etch for the entire thickness of the material. The wet etch can also improve surface roughness resulting from the dry etch. Flexibility regarding the selection of the wet etch process can allow optimization of acid selection, solution composition, and solution concentration.

[0054] The etching methods described above can be used in many applications, including photonics (e.g., electro-optical materials, devices with oxide perovskite materials, optical switches, interferometers, etc.); microelectromechanical systems (MEMS) (e.g., the disclosed embodiments can be used in thermal detectors, etching pixels in focal plane arrays (FPAs) and bolometers using oxide perovskite materials); communications systems (e.g., the disclosed embodiments can be used to pattern reflectarray antennas); memory devices (e.g., the disclosed embodiments can be used to pattern thin film capacitors and thin film varactors, such as DRAMs with BTO, STO, or BST layers); high-k dielectrics, etc.

[0055] The foregoing description is provided merely as an illustrative example and is not intended to require or imply that the steps of the various embodiments must be performed in the order presented. As one skilled in the art can appreciate, the order of steps in the foregoing embodiments may be performed in any order. Terms such as "thereafter," "then," and "next" are not necessarily intended to limit the order of steps, and these terms may be used to guide the reader through the method description. Furthermore, when claim elements are referred to in the singular, for example, using the articles "a," "an," or "the," such elements should not be construed as being limited to the singular. Furthermore, any step or component of any embodiment described herein may be used in any other embodiment.

[0056] The previous description of the disclosed aspects is provided to enable any person skilled in the art to make and / or use the disclosed embodiments. Various modifications to these aspects will be readily apparent to those skilled in the art, and the generic principles defined herein may be applied to other aspects without departing from the scope of the present disclosure. Thus, the embodiments of the present disclosure are not intended to be limited to the aspects shown herein but are to be accorded the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. forming a metal oxide layer, including a barium titanate layer or a strontium titanate layer, on a substrate; forming a patterned masking layer over the metal oxide layer; performing an anisotropic dry etching process to etch the metal oxide layer in areas not covered by the patterned masking layer; performing an isotropic wet etching process to remove residues not removed by the anisotropic dry etching process to form a patterned metal oxide layer; An etching method comprising:

2. The method of claim 1 , wherein the isotropic wet etching process forms undercut etch areas in the metal oxide layer beneath portions of the patterned masking layer.

3. 2. The method of claim 1, wherein the anisotropic dry etching process comprises one or more of reactive ion etching (RIE), capacitively coupled plasma RIE, inductively coupled plasma RIE, electron cyclotron resonance RIE, neutral density RIE, magnetically enhanced RIE, ion milling or ion beam etching, or gas cluster ion beam etching.

4. The anisotropic dry etching process is carried out using Ar, BCl 3 , Cl 2 , C 2 HClF 4 , CHClF 2 , C 4 F 8 , C 4 F 6 , C 5 F 8 , C.F. 4 , C.H. 4 , C.H.F. 3 , S.F. 6 , HBr, or NF 3 The method of claim 1 , further comprising using at least one etchant agent comprising:

5. The at least one etchant agent is O 2 , H 2 , He, N 2 5. The method of claim 4, further comprising at least one of: CO;

6. The method of claim 1 , wherein the anisotropic dry etching process comprises a dry plasma etching process or an ion beam etching process.

7. 10. The method of claim 1, wherein the isotropic wet etching process uses at least one etchant agent including hydrofluoric acid, buffered hydrofluoric acid using ammonium fluoride, buffered oxide etch, hydrochloric acid, sulfuric acid, nitric acid, phosphoric acid, acetic acid, citric acid, ammonium hydroxide, or mixtures thereof.

8. The method of claim 1 , wherein the residue comprises at least one of a barium compound or a strontium compound.

9. The method of claim 1 , wherein the patterned masking layer comprises a photoresist.

10. 10. The method of claim 9, further comprising removing the patterned masking layer before performing the isotropic wet etching process.

11. The method of claim 1 , wherein the patterned metal oxide layer includes a ridge portion having tapered sidewalls and horizontal layer portions located on each side of the ridge portion above the substrate.

12. The method of claim 11 , wherein the patterned metal oxide layer comprises a waveguide layer of a Mach-Zehnder interferometer.

13. The method of claim 11 , wherein the metal oxide layer comprises the barium titanate layer.

14. The method of claim 13 , further comprising forming a first electrode and a second electrode on the horizontal layer portion.

15. The method of claim 11 , wherein the metal oxide layer comprises the strontium titanate layer.

16. 2. The method of claim 1, wherein the step of forming the metal oxide layer comprises forming the strontium titanate layer on a substrate and forming the barium titanate layer on the strontium titanate layer.

17. 17. The method of claim 16, wherein the patterned metal oxide layer includes a barium titanate ridge portion having tapered sidewalls overlying the strontium titanate layer.

18. The method of claim 17 , wherein the barium titanate ridge portion comprises a waveguide layer of a Mach-Zehnder interferometer.

19. forming a metal oxide layer, including a barium titanate layer or a strontium titanate layer, on a substrate; forming a patterned masking layer over the metal oxide layer; performing a first anisotropic dry etching process to etch the metal oxide layer in areas not covered by the patterned masking layer; performing a second anisotropic dry etching process having a higher ion bombardment than the first anisotropic dry etching process to remove residues not removed by the first anisotropic dry etching process and form a patterned metal oxide layer; An etching method comprising:

20. 20. The method of claim 19, wherein the patterned masking layer comprises a photoresist and the residue comprises at least one of a barium compound or a strontium compound.

Citation Information

Patent Citations

  • Thin film high-dielectric capacitor

    JP1998223840A

  • Method for cleaning surface of plasma etched composite oxide substrate

    JP1999111688A

  • Controlled trimming of hardmasks for transistor gates

    JP2004512682A

  • electro-optic modulator

    JP2018511084A

  • Phase shifter employing transparent electrodes

    US20210278738A1