Preparation method of photoelectrochemical sensor for detecting T-2 toxin

Through a spliced ​​photoelectrochemical sensor that combines lanthanum nitriate with cadmium sulfide and strontium titanate, the operation complexity and stability problems in T-2 toxin detection are solved using the triple helical structure and the recognition mechanism of DNA enzymes, and the operation complexity and stability problems in T-2 toxin detection are achieved. High sensitivity and rapid detection.

CN118937435APending Publication Date: 2024-11-12UNIV OF JINAN
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411245555.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-06
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing T-2 toxin detection methods have problems such as complex operation, poor sensitivity, high toxicity and long detection time. In the construction of traditional sensors, aptamers and toxins are prone to contamination and destruction of activity, resulting in insufficient stability and sensitivity.

Method used

Using lanthanum nitriate-sensitized indium sulfide as the base material, combined with strontium titanate as the marker, DNA activated DNA through the recognition and release probe DNA of the T-2 toxin, signal amplification is achieved, and a piecewise photoelectrochemical construction is constructed. Sensors that separate photoelectric testing and biomolecular identification processes, reduce interference and improve stability and sensitivity.

Benefits of technology

It realizes fast, sensitive and stable detection of T-2 toxins, with a detection limit of 0.021 pg/mL, a short response time, a wide linear range, good stability, simple and fast, and overcomes the shortcomings of traditional methods.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to a preparation method of a photoelectrochemical sensor for detecting T-2 toxin. The T-2 toxin has a toxic effect on a digestive system, a nervous system and a reproductive system. The protein mainly exists in cereals or cereal products and has potential threats to human health. Therefore, it is necessary to develop a method for rapidly detecting T-2 toxin. The invention provides a photoelectrochemical sensor for rapidly and sensitively detecting T-2 toxin based on strontium titanate signal quenching and a Mn < 2 + >-dependent DNAzyme auxiliary signal amplification strategy. DNAzyme with different concentrations is released according to the combination of T-2 toxins with different concentrations and aptamers thereof. In the presence of Mn < 2 + >, DNAzyme activates and cuts a substrate DNA (H1), and a DNA part connected with H2 is exposed, so that the DNA part is combined with H2 modified by strontium titanate. Strontium titanate and a heterojunction photoelectric material compete for a light source, so that the intensity of the light source received by the heterojunction is reduced, and due to the large specific surface area of strontium titanate, steric hindrance can be generated, and the mode effectively reduces the photoelectric conversion efficiency of the heterojunction material, so that signals are quenched, and the current is reduced. In the research, the T-2 toxin concentration and a photocurrent signal have a linear relationship in a relatively wide range of 0.0001-50 ng mL < 1 >, and the detection limit is as low as 0.021 pg / mL.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing a photoelectrochemical sensor for detecting T-2 toxin. Specifically, lanthanum nickelate-sensitized indium cadmium sulfide is used as a substrate material, strontium titanate is used as a signal quenching marker to mark a hairpin DNA-H2, and an aptamer and T-2 toxin recognize and release a probe DNA to activate a DNA enzyme recognition process to achieve the purpose of signal amplification to prepare a photoelectrochemical sensor for detecting T-2 toxin. The invention belongs to the field of new functional materials and biosensor detection technology. Background Art

[0002] T-2 toxin is considered to be the most toxic of type A trichothecenes, with strong toxic effects, including digestive system toxicity, neurotoxicity and reproductive toxicity; T-2 toxin is widely distributed in various grains, such as corn, barley, wheat and certain grain products. In view of the significant risks posed by T-2 toxin to human health and reproduction, there is an urgent need to develop a rapid, sensitive and highly selective detection method. At present, T-2 toxin has been detected using fluorescence, chemiluminescence, liquid chromatography-tandem mass spectrometry and gas chromatography-mass spectrometry; however, chromatographic analysis is complicated and cumbersome; fluorescence analysis has poor controllability and high toxicity; chemiluminescence immunoassay has a long detection time; the present invention designs a controlled release photoelectrochemical sensor, which has sensitive detection, less interference, good stability, and a detection limit of 0.021 pg / mL for T-2 toxin.

[0003] Indium cadmium sulfide, a typical semiconductor nanophotosensitive material, is simple to prepare, low in cost, and has good photoelectric response under visible light. After being sensitized by lanthanum nickelate, the absorption efficiency of visible light is greatly improved, and excellent photocurrent is obtained, providing a photoelectric response basis for subsequent tests. As a functional material, strontium titanate has the characteristics of high bandgap (3.2eV), excellent photocatalytic activity, and unique electromagnetic properties and redox catalytic activity. When strontium titanate is used as a marker, different concentrations of T-2 toxin will introduce different amounts of strontium titanate when detecting the target, thereby causing changes in photocurrent to achieve quantitative detection of the target. At the same time, the use of DNA enzymes that rely on manganese ion activation as a controlled release strategy overcomes the problem of easy contamination and activity destruction of aptamers and toxins in the construction process of traditional sensors, and improves the stability and sensitivity of the sensor.

[0004] Photoelectrochemical sensors are a type of detection device that determines the concentration of a substance to be detected based on the photoelectric conversion characteristics of a substance. The photoelectrochemical detection method has the characteristics of simple equipment, high sensitivity, and easy miniaturization. It has developed into an analytical method with great application potential and has broad application prospects in the fields of food, environment, and medicine. The present invention is based on an indium cadmium sulfide / lanthanum nickelate composite material as a base material and strontium titanate with a high bandgap as a marker. According to the different effects of different concentrations of the substance to be detected on the intensity of the light signal, the detection of T-2 toxin is achieved. The photoelectrochemical sensor prepared by the present invention has the characteristics of simple manufacture, low cost, rapid detection, and high sensitivity. It achieves stable and sensitive detection of T-2 toxin in the visible light range, effectively overcoming the shortcomings of the current detection methods for T-2 toxin. Summary of the invention

[0005] One of the purposes of the present invention is to use lanthanum nickelate sensitized indium cadmium sulfide nano-semiconductor photosensitive materials as substrate materials to generate photoelectric response. Lanthanum nickelate, as a good sensitizer, has a good matching energy level with indium cadmium sulfide, can improve the photoelectric performance of pure photosensitive materials, and provide a photocurrent basis for subsequent tests.

[0006] The second purpose of the present invention is to use a triple helix structure to encapsulate the probe. When T-2 toxin is present, T-2 will react with the aptamer in the triple helix structure, the structure will be destroyed, and the probe will be released. 2+ In the presence of , the probe activates the DNAzyme, which acts on the substrate DNA on the electrode surface, allowing the label to be introduced, thereby affecting the photocurrent response.

[0007] The third purpose of the present invention is to construct a spliced ​​photoelectrochemical sensor, which separates the photoelectric test of inorganic semiconductor materials from the specific recognition immune reaction between biological molecules, so that the photoelectrochemical test will not interfere with the immune reaction, and eliminates the inhibitory effect of biological molecules on electron transfer. It has low requirements on the photoelectric response of the substrate material and no other interference.

[0008] The fourth purpose of the present invention is that the present invention is based on the indium cadmium sulfide / lanthanum nickelate composite material as the base material, and uses strontium titanate with a high bandgap as a marker. According to the different effects of different concentrations of the analyte on the intensity of the light signal, the detection of T-2 toxin is achieved.

[0009] The technical solution of the present invention is as follows: 1. A method for preparing a photoelectrochemical sensor for detecting T-2 toxin, comprising the following steps: (1) Preparation of indium cadmium sulfide materials 0.10-0.50 g of cadmium nitrate tetrahydrate was dissolved in 150-200 mL of deionized water, and then 0.30-0.60 g of indium nitrate hydrate and 0.20-0.50 g of thioacetamide were slowly added. After stirring at room temperature for 0.5-2 h, the mixed solution was transferred to a high-pressure reactor and reacted at 120-160 °C for 10-14 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 40-80 °C for 10-12 h to obtain a yellow indium cadmium sulfide material. (2) Preparation of lanthanum nickel oxide materials 0.30-0.60 g of lanthanum nitrate hexahydrate and 0.20-0.30 g of nickel nitrate hexahydrate were dissolved in 80-100 mL of deionized water, stirred evenly at room temperature, and quickly added with 20-30 mL of 0.30-0.40 mol / L sodium hydroxide aqueous solution. After stirring at room temperature for 10-30 min, the mixed solution was reacted at 40-60 °C for 4-6 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 40-60 °C, and the dried sample was calcined at 600-650 °C for 2-3 h to obtain black lanthanum nickelate nanomaterials. (3) Preparation of strontium titanate nanomaterials 3 to 4 mL of 2.5 to 3.0 mol / L tetrabutyl titanate was dissolved in 40 to 60 mL of ethanolamine, and then 30 to 40 mL of 1 to 3 mol / L sodium hydroxide aqueous solution was added to the solution, and then 10 to 20 mL of 1 to 3 mol / L strontium acetate aqueous solution was gradually added, and the above suspension was transferred to an autoclave and reacted at 160 to 180 °C for 20 to 24 h. The product was washed with anhydrous ethanol and ultrapure water for 3 times each. After washing, the product was vacuum dried at 50 to 60 °C overnight to obtain strontium titanate nanomaterials; (4) Preparation of strontium titanate-linked hairpin DNA (H2) Take H2 with a concentration of 6 to 8 μmol / L and heat it at 95 to 100 °C for 5 to 10 min, add tris(2-chloroethyl)phosphate with a concentration of 3 to 6 mmol / L under light-proof conditions and let it stand at room temperature for 2 to 4 h to reduce disulfide bonds. H2 and strontium titanate are connected by metal thiol. The specific steps are as follows: Take 80 to 120 μL of strontium titanate with a concentration of 5 to 10 mg / mL and mix it with 80 to 120 μL of H2 with a concentration of 6 to 8 μmol / L, shake it at 35 to 40 °C for 10 to 15 h, add 100 to 300 μL of tris(hydroxymethyl)aminomethane hydrochloride and 40 to 60 μL of bovine serum albumin solution after centrifugation, continue to shake it at 35 to 40 °C for 30 to 60 min, and store the product at 4 °C for use; (5) Preparation of triple helix and double helix structures 6 ~ 10 μmol / L H1 and 6 ~ 10 μmol / L H2 were heated at 95 ~ 100 ℃ for 5 ~ 10 min, and naturally cooled at room temperature for 2 ~ 6 h to obtain a hairpin structure. 6 ~ 10 μmol / L T-2 toxin aptamer and 6 ~ 10μmol / L probe were mixed in equal proportions in binding buffer, heated at 95 ~ 100 ℃ for 5 ~ 10 min, and cooled at room temperature for 2 ~ 8 h to form a triple helix structure (THMS). DNA enzyme (DNAzyme) and capture DNA (cDNA) were mixed in equal volumes, heated to 95 ~ 100 ℃ for 5 ~ 10 min, and then cooled to room temperature to form a double helix structure (DNAzyme-off). (6) Preparation of photoelectrochemical sensors 1) Ultrasonic cleaning of ITO conductive glass was carried out with detergent, acetone, ethanol and ultrapure water in sequence, and then dried with nitrogen gas; 2) Take 6 µL of an aqueous solution of 2 to 6 mg / mL indium cadmium sulfide and drop it onto the conductive surface of the ITO conductive glass. o Dry in a dryer C; 3) Continue to drip 6 µL of 2 ~ 6 mg / mL lanthanum nickelate aqueous solution on the modified electrode surface. o Dry naturally at C; 4) Add 6 μL of 3 ~ 6 mmol / L thioglycolic acid (TGA) and incubate at room temperature for 40 ~ 60 min to introduce carboxyl groups. Then add 6 μL of a mixture of 15 mg / mL N-hydroxysuccinimide (NHS) and 30 mg / mL 1-ethyl-3-(3-dimethylaminopropyl) carbodiimide hydrochloride (EDC) and incubate at room temperature for 40 ~ 60 min to activate the carboxyl groups. 5) Add 3 μL of 6 ~ 8 μmol / L H1 and 3 μL of 1 ~ 4 μmol / L DNAzyme-off to the modified electrode, incubate at 37 °C for 2 ~ 4 h, then continue to add 6 μL of 0.1 wt% bovine serum albumin to block the active site, and gently wash with Tris-HCl buffer at each step. Store at 4 °C in the dark for later use; 6) Mix 10 μL T-2 solution of different concentrations with 90 μL THMS in 100 μL 1x binding buffer for 30 min, mix 7 μL solution with 3 μL 10 ~ 20 mmol / L manganese chloride and drop it on the electrode surface. After 60 min, drop 8 μL strontium titanate-H2 on the electrode surface and incubate for 80 ~ 120 min. The sensor is constructed. Finally, measure in 10 mmol / L Tris-HCl buffer solution with pH = 7.4.

[0010] 2. The detection method of the photoelectrochemical sensor prepared as claimed in claim 1, comprising the following steps: (1) The test was performed using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode in a Tris-HCl buffer solution with a pH of 7.4; (2) Prepare sensors for detecting different concentrations of T-2 toxin and test them using the time-current method, setting the voltage to -0.1 ~ 0.1 V, the running time to 120 s, and the light source wavelength to 400 ~ 450 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Substitute the T-2 toxin standard solution for the T-2 toxin sample solution to be tested.

[0011] Beneficial results of the present invention (1) The present invention uses lanthanum nickelate-sensitized indium cadmium sulfide as a photosensitive substrate material, which solves the problem of low photoelectric conversion efficiency of pure lanthanum nickelate and pure indium cadmium sulfide; (2) The present invention uses a triple helix structure to encapsulate the probe. When T-2 toxin is present, T-2 reacts with the aptamer in the triple helix structure, the structure is destroyed, and the probe is released. In the presence of manganese ions, the probe activates the DNAzyme and acts on the substrate DNA on the electrode surface, so that the marker can be introduced, thereby affecting the photocurrent response; (3) The present invention adopts a spliced ​​photoelectrochemical sensor to separate the photoelectric test process of semiconductor materials from the specific immune recognition reaction process between biological molecules. On the one hand, it reduces the requirements for the photoelectric response of the substrate material. On the other hand, the biomolecule recognition process is carried out separately and will not be destroyed by the photoelectric test process. In addition, other interference effects in the layer-by-layer modification process of the sensor are reduced. (4) The photoelectrochemical sensor prepared by the present invention is used for the detection of T-2 toxin, has a short response time, a low detection limit, a wide linear range, and good stability, and can realize simple, fast, highly sensitive and highly stable detection.

[0012] Specific implementation plan.

[0013] Example 1 Preparation of photoelectrochemical sensor (1) Preparation of indium cadmium sulfide materials 0.15 g of cadmium nitrate tetrahydrate was dissolved in 150 mL of deionized water, and then 0.30 g of indium nitrate hydrate and 0.20 g of thioacetamide were slowly added. After stirring at room temperature for 1 h, the mixed solution was transferred to a high-pressure reactor and reacted at 120 °C for 10 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 40 °C for 10 h to obtain a yellow indium cadmium sulfide material. (2) Preparation of lanthanum nickel oxide materials 0.30 g of lanthanum nitrate hexahydrate and 0.20 g of nickel nitrate hexahydrate were dissolved in 100 mL of deionized water, stirred evenly at room temperature, and 20 mL of 0.30 mol / L sodium hydroxide aqueous solution was quickly added. After stirring at room temperature for 10 min, the mixed solution was reacted at 40 °C for 4 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 40 °C, and the dried sample was calcined at 600 °C for 2 h to obtain black lanthanum nickelate nanomaterials. (3) Preparation of strontium titanate nanomaterials 3 mL of 2.5 mol / L tetrabutyl titanate was dissolved in 40 mL of ethanolamine, and then 30 mL of 1 mol / L sodium hydroxide aqueous solution was added to the solution, and then 10 mL of 1 mol / L strontium acetate aqueous solution was gradually added, and the above suspension was transferred to an autoclave and reacted at 160 °C for 20 h. The product was washed with anhydrous ethanol and ultrapure water for 3 times each. After washing, the product was vacuum dried at 50 °C overnight to obtain strontium titanate nanomaterials; (4) Preparation of hairpin DNA (H2) linked to strontium titanate marker Take 6 μmol / L H2 and heat it at 95 °C for 5 min, add 3 mmol / L tris(2-chloroethyl) phosphate under light-proof conditions and stand at room temperature for 2 h to reduce disulfide bonds. H2 and strontium titanate are connected by metal thiol. The specific steps are as follows: take 80 μL of 5 mg / mL strontium titanate and 80 μL of 6 μmol / L H2 and mix them, shake at 35 °C for 10 h, centrifuge and add 100 μL tris(hydroxymethyl)aminomethane hydrochloride and 40 μL bovine serum albumin solution, continue to shake at 35 °C for 30 min, and store the product at 4 °C for use; (5) Preparation of triple helix and double helix structures 6 μmol / L H1 and 8 μmol / L H2 were heated at 95 °C for 5 min and cooled naturally at room temperature for 2 h to obtain a hairpin structure. 6 μmol / L T-2 toxin aptamer and 6 μmol / L probe were mixed in equal proportions in binding buffer, heated at 95 °C for 5 min and cooled at room temperature for 2 h to form a triple helix structure (THMS). DNAzyme and capture DNA (cDNA) were mixed in equal volumes, heated to 95 °C for 5 min and cooled to room temperature to form a double helix structure (DNAzyme-off). (6) Preparation of photoelectrochemical sensors 1) Ultrasonic cleaning of ITO conductive glass was carried out with detergent, acetone, ethanol and ultrapure water in sequence, and then dried with nitrogen gas; 2) Take 6 μL of 3 mg / mL indium cadmium sulfide aqueous solution and drop it onto the conductive surface of the ITO conductive glass. o Dry in a dryer C; 3) Continue to drip 6 μL of 3 mg / mL lanthanum nickelate aqueous solution on the modified electrode surface, and the electrode is heated at 60 o Dry naturally at C; 4) Add 6 μL of 3 mmol / L thioglycolic acid (TGA) and incubate at room temperature for 40 min to introduce carboxyl groups. Then add 6 μL of a mixture of 15 mg / mL N-hydroxysuccinimide (NHS) and 30 mg / mL 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride (EDC) and incubate at room temperature for 40 min to activate the carboxyl groups. 5) Add 3 μL of 6 μmol / L H1 and 3 μL of 1 μmol / L DNAzyme-off to the modified electrode. After incubation at 37 °C for 2 h, continue to add 6 μL of 0.1 wt% bovine serum albumin to block the active site. Gently wash with Tris-HCl buffer at each step. Store at 4 °C in the dark for future use; 6) Mix 10 μL T-2 solution of different concentrations with 90 μL THMS in 100 μL 1x binding buffer for 30 min, mix 7 μL solution with 3 μL 10 mmol / L manganese chloride and drop it on the electrode surface. After 60 min, drop 8 μL strontium titanate-H2 on the electrode surface and incubate for 80 min. The sensor is constructed. Finally, measure in 10 mmol / L Tris-HCl buffer solution with pH = 7.4.

[0014] Example 2 Architecture of Photoelectrochemical Sensor (1) Preparation of indium cadmium sulfide materials 0.20 g of cadmium nitrate tetrahydrate was dissolved in 155 mL of deionized water, and then 0.35 g of indium nitrate hydrate and 0.30 g of thioacetamide were slowly added. After stirring at room temperature for 1.5 h, the mixed solution was transferred to a high-pressure reactor and reacted at 140 °C for 12 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 50 °C for 11 h to obtain a yellow indium cadmium sulfide material. (2) Preparation of lanthanum nickel oxide materials Take 0.35 g of lanthanum nitrate hexahydrate and 0.25 g of nickel nitrate hexahydrate and dissolve them in 85 mL of deionized water. Stir them evenly at room temperature. Quickly add 30 mL of 0.35 mol / L sodium hydroxide aqueous solution. Stir at room temperature for 15 min. Then, react the mixed solution at 50 °C for 5 h. After the reaction, cool it to room temperature naturally. Wash the sediment with deionized water and ethanol three times each. After washing, dry the sediment in vacuum at 40 °C. Then, calcine the dried sample at 625 °C for 3 h to obtain black lanthanum nickelate nanomaterials. (3) Preparation of strontium titanate nanomaterials 3 mL of 3.25 mol / L tetrabutyl titanate was dissolved in 50 mL of ethanolamine, and then 30 mL of 2 mol / L sodium hydroxide aqueous solution was added to the solution, and then 10 mL of 2 mol / L strontium acetate aqueous solution was gradually added, and the above suspension was transferred to an autoclave and reacted at 170 °C for 22 h. The product was washed with anhydrous ethanol and ultrapure water for 3 times each. After washing, the product was vacuum dried at 50 °C overnight to obtain strontium titanate nanomaterials; (4) Preparation of hairpin DNA (H2) linked to strontium titanate marker Take 7 μmol / L H2 and heat it at 95 °C for 5 min, add 4 mmol / L tris(2-chloroethyl) phosphate under light-proof conditions and stand at room temperature for 2 h to reduce disulfide bonds. H2 and strontium titanate are connected by metal thiol. The specific steps are as follows: take 90 μL of 5 mg / mL strontium titanate and 90 μL of 7 μmol / L H2, mix them, shake at 36 °C for 11 h, add 150 μL tris(hydroxymethyl)aminomethane hydrochloride and 40 μL bovine serum albumin solution after centrifugation, continue to shake at 36 °C for 35 min, and store the product at 4 °C for use; (5) Preparation of triple helix and double helix structures 7 μmol / L H1 and 7 μmol / L H2 were heated at 95 °C for 5 min and cooled naturally at room temperature for 2 h to obtain a hairpin structure. 7 μmol / L T-2 toxin aptamer and 7 μmol / L probe were mixed in equal proportions in binding buffer, heated at 95 °C for 5 min and cooled at room temperature for 2 h to form a triple helix structure (THMS). DNAzyme and capture DNA (cDNA) were mixed in equal volumes, heated to 95 °C for 5 min and cooled to room temperature to form a double helix structure (DNAzyme-off). (6) Preparation of photoelectrochemical sensors 1) Ultrasonic cleaning of ITO conductive glass was carried out with detergent, acetone, ethanol and ultrapure water in sequence, and then dried with nitrogen gas; 2) Take 6 μL of 4 mg / mL indium cadmium sulfide aqueous solution and drop it onto the conductive surface of the ITO conductive glass. o Dry in a dryer C; 3) Continue to drip 6 μL of 4 mg / mL lanthanum nickelate aqueous solution on the modified electrode surface, and the electrode is heated at 60 o Dry naturally at C; 4) Add 6 μL of 4 mmol / L thioglycolic acid (TGA) and incubate at room temperature for 50 min to introduce carboxyl groups. Then add 6 μL of a mixture of 15 mg / mL N-hydroxysuccinimide (NHS) and 30 mg / mL 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride (EDC) and incubate at room temperature for 50 min to activate the carboxyl groups. 5) Add 3 μL of 7 μmol / L H1 and 3 μL of 3 μmol / L DNAzyme-off to the modified electrode. After incubation at 37 °C for 3 h, continue to add 6 μL of 0.1 wt% bovine serum albumin to block the active site. Gently wash with Tris-HCl buffer at each step. Store at 4 °C in the dark for future use; 6) Mix 10 μL T-2 solution of different concentrations with 90 μL THMS in 100 μL 1x binding buffer for 30 min. Mix 7 μL of the solution with 3 μL 15 mmol / L manganese chloride and drop it on the electrode surface. After 60 min, drop 8 μL strontium titanate-H2 on the electrode surface and incubate for 90 min. The sensor is constructed. Finally, measure in 10 mmol / L Tris-HCl buffer solution with pH = 7.4.

[0015] Example 3 Construction of photoelectrochemical immunosensor (1) Preparation of indium cadmium sulfide materials 0.20 g of cadmium nitrate tetrahydrate was dissolved in 160 mL of deionized water, and then 0.40 g of indium nitrate hydrate and 0.25 g of thioacetamide were slowly added. After stirring at room temperature for 1.5 h, the mixed solution was transferred to a high-pressure reactor and reacted at 160 °C for 12 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 60 °C for 12 h to obtain a yellow indium cadmium sulfide material. (2) Preparation of lanthanum nickel oxide materials 0.43 g of lanthanum nitrate hexahydrate and 0.29 g of nickel nitrate hexahydrate were dissolved in 80 mL of deionized water, stirred evenly at room temperature, and 20 mL of 0.38 mol / L sodium hydroxide aqueous solution was quickly added. After stirring at room temperature for 10 min, the mixed solution was reacted at 60 °C for 4 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 60 °C, and the dried sample was calcined at 650 °C for 2 h to obtain black lanthanum nickelate nanomaterials. (3) Preparation of strontium titanate nanomaterials 3.42 mL of 2.86 mol / L tetrabutyl titanate was dissolved in 40 mL of ethanolamine, and then 30 mL of 3 mol / L sodium hydroxide aqueous solution was added to the solution, and then 10 mL of 1 mol / L strontium acetate aqueous solution was gradually added, and the above suspension was transferred to an autoclave and reacted at 180 °C for 24 h. The product was washed with anhydrous ethanol and ultrapure water for 3 times each. After washing, the product was vacuum dried at 60 °C overnight to obtain strontium titanate nanomaterials; (4) Preparation of hairpin DNA (H2) linked to strontium titanate marker Take 8 μmol / L H2 and heat it at 95 °C for 5 min, add 3 mmol / L tris(2-chloroethyl) phosphate under light-proof conditions and stand at room temperature for 2 h to reduce disulfide bonds. H2 and strontium titanate are connected by metal thiol. The specific steps are as follows: take 90 μL of 5 mg / mL strontium titanate and 90 μL of 8 μmol / L H2 and mix them, shake at 36 °C for 12 h, add 200 μL tris(hydroxymethyl)aminomethane hydrochloride and 50 μL bovine serum albumin solution after centrifugation, continue to shake at 37 °C for 40 min, and store the product at 4 °C for use; (5) Preparation of triple helix and double helix structures 6 μmol / L H1 and 8 μmol / L H2 were heated at 95 °C for 5 min and cooled naturally at room temperature for 2 h to obtain a hairpin structure. 6 μmol / L T-2 toxin aptamer and 6 μmol / L probe were mixed in equal proportions in binding buffer, heated at 95 °C for 5 min and cooled at room temperature for 2 h to form a triple helix structure (THMS). DNAzyme and capture DNA (cDNA) were mixed in equal volumes, heated to 95 °C for 5 min and cooled to room temperature to form a double helix structure (DNAzyme-off). (6) Preparation of photoelectrochemical sensors 1) Ultrasonic cleaning of ITO conductive glass was carried out with detergent, acetone, ethanol and ultrapure water in sequence, and then dried with nitrogen gas; 2) Take 6 μL of 5 mg / mL indium cadmium sulfide aqueous solution and drop it onto the conductive surface of the ITO conductive glass. o Dry in a dryer C; 3) Continue to drip 6 μL of 5 mg / mL lanthanum nickelate aqueous solution on the modified electrode surface, and the electrode is heated at 60 o Dry naturally at C; 4) Add 6 μL of 3 mmol / L thioglycolic acid (TGA) and incubate at room temperature for 40 min to introduce carboxyl groups. Then add 6 μL of a mixture of 15 mg / mL N-hydroxysuccinimide (NHS) and 30 mg / mL 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride (EDC) and incubate at room temperature for 40 min to activate the carboxyl groups. 5) Add 3 μL of 7 μmol / L H1 and 3 μL of 3 μmol / L DNAzyme-off to the modified electrode. After incubation at 37 °C for 3 h, continue to add 6 μL of 0.1 wt% bovine serum albumin to block the active site. Gently wash with Tris-HCl buffer at each step. Store at 4 °C in the dark for future use; 6) Mix 10 μL T-2 solution of different concentrations with 90 μL THMS in 100 μL 1x binding buffer for 30 min. Mix 7 μL of the solution with 3 μL 15 mmol / L manganese chloride and drop it on the electrode surface. After 60 min, drop 8 μL strontium titanate-H2 on the electrode surface and incubate for 90 min. The sensor is constructed. Finally, measure in 10 mmol / L Tris-HCl buffer solution with pH = 7.4.

[0016] Example 4 Detection of T-2 toxin (1) The test was performed using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode in a Tris buffer solution with a pH of 7.4; (2) Configure sensors to detect different concentrations of T-2 toxin and test them using the time-current method, setting the voltage to -0.1 V, the running time to 120 s, and the light source wavelength to 400 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Substitute the T-2 toxin standard solution for the T-2 toxin sample solution to be tested.

[0017] Example 5 Detection of T-2 toxin (1) The test was performed using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode in a Tris buffer solution with a pH of 7.4; (2) Configure sensors to detect different concentrations of T-2 toxin and test them using the time-current method, setting the voltage to 0 V, the running time to 120 s, and the light source wavelength to 425 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Substitute the T-2 toxin standard solution for the T-2 toxin sample solution to be tested.

[0018] Example 6 Detection of T-2 toxin (1) The test was performed using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode in a Tris buffer solution with a pH of 7.4; (2) Configure sensors to detect different concentrations of T-2 toxin and test them using the time-current method, setting the voltage to 0.1 V, the running time to 120 s, and the light source wavelength to 450 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Substitute the T-2 toxin standard solution for the T-2 toxin sample solution to be tested.

Claims

1. A method for preparing a photoelectrochemical sensor for detecting T-2 toxin, characterized in that: The following steps are involved: (1) Preparation of indium cadmium sulfide materials 0.10-0.50 g of cadmium nitrate tetrahydrate was dissolved in 150-200 mL of deionized water, and then 0.30-0.60 g of indium nitrate hydrate and 0.20-0.50 g of thioacetamide were slowly added. After stirring at room temperature for 0.5-2 h, the mixed solution was transferred to a high-pressure reactor and reacted at 120-160 °C for 10-14 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 40-80 °C for 10-12 h to obtain a yellow indium cadmium sulfide material. (2) Preparation of lanthanum nickel oxide materials 0.30-0.60 g of lanthanum nitrate hexahydrate and 0.20-0.30 g of nickel nitrate hexahydrate were dissolved in 80-100 mL of deionized water, stirred evenly at room temperature, and quickly added with 20-30 mL of 0.30-0.40 mol / L sodium hydroxide aqueous solution. After stirring at room temperature for 10-30 min, the mixed solution was reacted at 40-60 °C for 4-6 h. After the reaction was completed, it was naturally cooled to room temperature. The sediment was washed with deionized water and ethanol for 3 times each. After washing, the obtained precipitate was vacuum dried at 40-60 °C, and the dried sample was calcined at 600-650 °C for 2-3 h to obtain black lanthanum nickelate nanomaterials. (3) Preparation of strontium titanate nanomaterials 3 to 4 mL of 2.5 to 3.0 mol / L tetrabutyl titanate was dissolved in 40 to 60 mL of ethanolamine, and then 30 to 40 mL of 1 to 3 mol / L sodium hydroxide aqueous solution was added to the solution, and then 10 to 20 mL of 1 to 3 mol / L strontium acetate aqueous solution was gradually added, and the above suspension was transferred to an autoclave and reacted at 160 to 180 °C for 20 to 24 h. The product was washed with anhydrous ethanol and ultrapure water for 3 times each. After washing, the product was vacuum dried at 50 to 60 °C overnight to obtain strontium titanate nanomaterials; (4) Preparation of strontium titanate-linked hairpin DNA (H2) Take H2 with a concentration of 6 to 8 μmol / L and heat it at 95 to 100 °C for 5 to 10 min, add tris(2-chloroethyl)phosphate with a concentration of 3 to 6 mmol / L under light-proof conditions and let it stand at room temperature for 2 to 4 h to reduce disulfide bonds. H2 and strontium titanate are connected by metal thiol. The specific steps are as follows: Take 80 to 120 µL of strontium titanate with a concentration of 5 to 10 mg / mL and mix it with 80 to 120µL of H2 with a concentration of 6 to 8 μmol / L, shake it at 35 to 40 °C for 10 to 15 h, add 100 to 300µL of tris(hydroxymethyl)aminomethane hydrochloride and 40 to 60 µL of bovine serum albumin solution after centrifugation, continue to shake it at 35 to 40 °C for 30 to 60 min, and store the product at 4 °C for later use; (5) Preparation of triple helix and double helix structures 6 ~ 10 μmol / L H1 and 6 ~ 10 μmol / L H2 were heated at 95 ~ 100 ℃ for 5 ~ 10 min, and naturally cooled at room temperature for 2 ~ 6 h to obtain a hairpin structure. 6 ~ 10 μmol / L T-2 toxin aptamer and 6 ~ 10 μmol / L probe were mixed in equal proportions in binding buffer, heated at 95 ~ 100 ℃ for 5 ~ 10 min, and cooled at room temperature for 2 ~ 8 h to form a triple helix structure (THMS). DNA enzyme (DNAzyme) and capture DNA (cDNA) were mixed in equal volumes, heated to 95 ~ 100 ℃ for 5 ~ 10 min, and then cooled to room temperature to form a double helix structure (DNAzyme-off). (6) Preparation of photoelectrochemical sensors 1) Ultrasonic cleaning of ITO conductive glass was carried out with detergent, acetone, ethanol and ultrapure water in sequence, and then dried with nitrogen gas; 2) Take 6 µL of an aqueous solution of 2 to 6 mg / mL indium cadmium sulfide and drop it onto the conductive surface of the ITO conductive glass. o Dry in a dryer C; 3) Continue to drip 6 µL of 2 ~ 6 mg / mL lanthanum nickelate aqueous solution on the modified electrode surface. o Dry naturally at C; 4) Add 6 μL of 3 ~ 6 mmol / L thioglycolic acid (TGA) and incubate at room temperature for 40 ~ 60 min to introduce carboxyl groups. Then add 6 μL of a mixture of 15 mg / mL N-hydroxysuccinimide (NHS) and 30 mg / mL 1-ethyl-3-(3-dimethylaminopropyl) carbodiimide hydrochloride (EDC) and incubate at room temperature for 40 ~ 60 min to activate the carboxyl groups. 5) Add 3 μL of 6 ~ 8 μmol / L H1 and 3 μL of 1 ~ 4 μmol / L DNAzyme-off to the modified electrode, incubate at 37 °C for 2 ~ 4 h, then continue to add 6 μL of 0.1 wt% bovine serum albumin to block the active site, and gently wash with Tris-HCl buffer at each step. Store at 4 °C in the dark for later use; 6) Mix 10 μL T-2 solution of different concentrations with 90 μL THMS in 100 μL 1x binding buffer for 30 min, mix 7 μL solution with 3 μL 10 ~ 20 mmol / L manganese chloride and drop it on the electrode surface. After 60 min, drop 8 μL strontium titanate-H2 on the electrode surface and incubate for 80 ~ 120 min. The sensor is constructed. Finally, measure in 10 mmol / L Tris-HCl buffer solution with pH = 7.

4.

2. The detection method of the photoelectrochemical sensor prepared as claimed in claim 1, comprising the following steps: (1) The test was performed using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode in a Tris-HCl buffer solution with a pH of 7.4; (2) Prepare sensors for detecting different concentrations of T-2 toxin and test them using the time-current method, setting the voltage to -0.1 ~ 0.1 V, the running time to 120 s, and the light source wavelength to 400 ~ 450 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Substitute the T-2 toxin standard solution for the T-2 toxin sample solution to be tested.

Citation Information

Cited By

  • Antibiotic resistance gene photoelectric detection sensor as well as preparation method and application thereof

    CN119959324A