Method, device and application of heat storage and release by solid-state phase transition of glassy crystals and actively controllable pressure caloric effect materials
By employing pressure-caloric effect materials with a glassy crystalline phase, the method addresses the limitations of conventional solid-solid phase transition materials, enabling long-term storage and controllable heat release for efficient heat utilization.
Patent Information
- Application Number
- JP2024527055
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-01-13
- Filing Date
- 2022-01-19
- Publication Date
- 2024-10-28
- Estimated Expiration
- 2042-01-19
AI Technical Summary
Conventional solid-solid phase transition materials lack the ability to accurately control heat release time and are limited by spontaneous phase transitions, making them unsuitable for long-distance transportation and use in low-temperature environments.
A method involving the use of pressure-caloric effect materials with a glassy crystalline phase, where the material is heated to a plastic crystalline phase, rapidly cooled to a glassy phase, and then controlled through pressure to manage heat release.
Enables long-term storage and controllable heat release, allowing for long-distance transportation and efficient heat utilization in various environments.
Smart Images

Figure 2024539410000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the technical field of solid-state phase change energy storage, in particular to a method, device and application of heat storage and release by solid-state phase change of glassy crystals and their actively controllable barocaloric materials. [Background technology]
[0002] Climate change is a global problem facing mankind, and greenhouse gases continue to increase as countries emit carbon dioxide, posing a threat to the ecosystem. Against this background, countries around the world have adopted global agreements to reduce greenhouse gas emissions, and China has also put forward the strategic goals of "carbon peaking" and "carbon neutrality". The use of clean energy and improving energy efficiency are effective ways to achieve the goal of carbon neutrality. However, current data shows that 72% of energy is wasted in the energy conversion process around the world. It is mainly dissipated in the form of thermal energy, so it cannot be effectively utilized, resulting in a decrease in energy utilization efficiency and the dissipation of fossil energy. The recovery and utilization of thermal energy plays an extensive and important role in achieving sustainable energy utilization. Thermal storage technology is a technology that has been gradually developed with the aim of solving the problems caused by the mismatch between the supply and demand of thermal energy in time, space, or intensity by using thermal storage materials as a medium to store thermal energy such as solar heat, geothermal heat, industrial waste heat, and low-grade waste heat, and releasing it when needed, thereby maximizing the energy utilization of the entire system. Therefore, the development of high-performance heat storage materials is an important approach to improve energy utilization, reduce energy consumption, and ultimately solve the carbon emission problem.
[0003] Latent heat storage technology based on phase change materials uses the phase transition process of the material itself to absorb and release heat, thereby realizing heat storage and utilization. Compared with sensible heat storage technology, phase change latent heat storage materials have a more stable energy output, and the amount of heat stored per unit volume is several times that of sensible heat storage materials. Among them, solid-solid phase change heat storage materials do not generate liquid phase during the phase transition process, and the volume change before and after the phase transition is relatively small. It is considered the most ideal heat storage method because it is non-toxic and non-corrosive, has low requirements for the container material and processing technology, has a small degree of supercooling, and has a long service life. However, traditional solid-solid phase change materials have a small latent heat of phase transition and limited heat storage capacity. At the same time, the phase transition behavior of traditional solid-solid phase change materials is completely dependent on the change in ambient temperature, and when the ambient temperature gradually decreases, it will spontaneously undergo phase transition, resulting in uncontrollable heat release, and it is impossible to accurately control the time of heat release, and lacks the initiative in heat quantity control. As a result, such materials cannot be transported long distances or used in low temperature environments with a wide temperature range, significantly limiting the recovery and utilization of thermal energy. As the demand for heat storage technology increases, the development of solid-state phase transition heat storage materials that have high heat storage performance and can actively control heat release has become a new challenge.
[0004] Solid-solid phase transition materials involve three phase structures: crystalline, plastic crystal, and glassy crystal. The crystalline phase is a completely ordered and regular state, including the orientation of the crystal lattice and the structural units. The plastic crystal phase is a highly disordered state, in which the orientation of the organic molecules or inorganic structural units that make up the material is completely disordered, but the position of the center of mass still maintains a long-range regular crystal lattice. The degree of order of the glassy crystal phase is intermediate between the crystalline and plastic crystal phases, in which the center of mass is ordered but disoriented (frozen state). Not all solid-state phase transition materials have these three phase structures simultaneously; only some materials have the plastic crystal phase simultaneously, and only a small proportion of plastic crystal materials have the glassy crystal phase.
[0005] Barocaloric refers to the phenomenon in which pressure causes a phase transition and produces a caloric effect. In recent years, the applicant's team has made breakthroughs in the research of barocaloric materials that have barocaloric effects, and the entropy change of some barocaloric materials is several hundred Jkg. -1 K -1 In the pressure caloric effect refrigeration technology, a reversible pressure caloric effect is a prerequisite for realizing the application of efficient solid-state refrigeration technology. However, the applicant's team discovered during the research of pressure caloric effect materials with a glassy crystalline phase that the pressure caloric effect is irreversible. That is, this kind of material with a glassy crystalline phase can change from an ordered crystalline phase to a plastic crystalline phase during the heating process, but during the cooling process, even at temperatures much lower than the phase transition point, no reversible phase transition still occurs. Therefore, such a pressure caloric effect material with an irreversible pressure caloric effect cannot actually be used as a pressure caloric effect refrigeration material, although the entropy change is very large. Surprisingly, based on the irreversible phase transition of this kind of pressure caloric effect material with a glassy crystalline phase, it is expected to realize long-term, wide temperature range, and cross-regional heat storage. This is because this kind of material with a glassy crystalline phase does not spontaneously undergo phase transition even when the temperature is reduced. One of the reasons for this result is that this kind of pressure caloric effect material is frozen at supercooling during the rapid cooling process, forming a glassy crystalline phase. Instead of directly transforming into a fully ordered, regular, low-temperature ordered phase, the material in the glassy crystalline phase still has a large amount of entropy, ensuring sufficient heat storage, since a large amount of disorder is preserved and frozen.
[0006] In addition, similar to the pressure-driven phase transition of pressure caloric effect materials, the plastic crystal phase is quenched to form a glassy crystal phase, and then the hydrostatic pressure is applied to realize the phase transition from the glassy crystal phase to a low-temperature ordered crystal phase, thereby achieving the purpose of releasing latent heat. The glassy crystal phase can be pressure-controlled, so that when this type of pressure caloric effect material is used as a heat storage material, a means for accurately controlling the heat release time is provided. Therefore, it is expected that the effective combination of the plastic crystal phase and the glassy crystal phase of this type of pressure caloric effect material will break through the limitations of current phase transition heat storage materials in solid-solid pressure caloric effect materials, and realize accurate control of long-distance and long-term heat storage and heat release time across temperature zones. Summary of the Invention
[0007] In order to overcome the above problems in the storage and release of heat by solid-state phase transition, the objective of the present invention is to provide a pressure-driven solid-state heat storage and release method, device and application which can actively control the heat release.
[0008] In order to achieve the above objectives, the technical solutions adopted in the present invention are as follows:
[0009] A method for controllable solid-state phase transition heat storage and dissipation of pressure caloric effect materials, comprising the following three steps: Step 1: heating a pressure caloric effect material sample to a high-temperature plastic crystalline phase state; Step 2: rapidly cooling the pressure caloric effect material in the high-temperature plastic crystalline phase to obtain a pressure caloric effect material in the glassy crystalline phase; realizing long-term thermal energy storage in the pressure caloric effect material in the glassy crystalline phase; Step 3: when heat dissipation is required, applying pressure as a driving method to suppress heat dissipation, thereby realizing controllable storage, transfer and utilization of thermal energy.
[0010] In step 2, the rapid cooling method for obtaining a glassy crystalline phase includes cooling at a cooling rate of ≧2K / min, or instantaneously cooling the high-temperature plastic crystalline phase sample with ice water or liquid nitrogen. In step 3, the pressure application method includes hydrostatic pressure or needle pressure. The pressure caloric effect material includes 2-amino-2-methyl-1,3-propanediol (CH 3 )C(CH 2 )(CH 2 OH) 2 (AMP), m-carborane C 2 B 10 H 12 , 1-cyanoadamantane C 11 H 15 N (CAN), Adamantanone C 10 H 14 O (AON), and pentachloronitrobenzene C 6 C l5 NO 2 (PCNB).
[0011] When the pressure caloric effect material is 2-amino-2-methyl-1,3-propanediol (AMP), a phase transition occurs at 355K, absorbing heat and changing into a high-temperature plastic crystalline phase, with a corresponding enthalpy change of 215 Jg -1 and the entropy change is 606 Jkg -1 K -1 When 2-amino-2-methyl-1,3-propanediol (AMP) in the high-temperature plastic crystalline phase is rapidly cooled to a low temperature of 273 K, a glassy crystalline phase is obtained. The glassy crystalline phase of 2-amino-2-methyl-1,3-propanediol (AMP) can be stored at 273 K or heated to temperatures below room temperature for a long period of time to store heat. 2-amino-2-methyl-1,3-propanediol (AMP) does not spontaneously undergo a phase transition and release heat. When 2-amino-2-methyl-1,3-propanediol (AMP) is held at a temperature of 273 K and pressures of 67 bar or more are applied, a significant heat release peak occurs. The corresponding enthalpy change is 133 Jg-1 and the entropy change is 487 Jkg -1 K -1 It is.
[0012] A heat storage and heat exchange device containing a pressure caloric effect material, the device including a heating unit, a rapid cooling unit and a pressurizing unit. The heating unit is used to make the pressure caloric effect material into a high-temperature plastic crystal phase. The rapid cooling unit is used to rapidly cool the pressure caloric effect material in the high-temperature plastic crystal phase to obtain a pressure caloric effect material in a glass crystal phase. The pressurizing unit applies hydrostatic pressure or pinprick pressure to the pressure caloric effect material when heat needs to be released, thereby controlling the release of heat and realizing the controllable storage, transfer and utilization of thermal energy. The pressure caloric effect material is preferably a pressure caloric effect material having a glass crystal phase, and further preferably is 2-amino-2-methyl-1,3-propanediol (CH 3 )C(CH 2 )(CH 2 OH) 2 (AMP), m-carborane C 2 B 10 H 12 , 1-cyanoadamantane C 11 H 15 N (CAN), Adamantanone C 10 H 14 O (AON), and pentachloronitrobenzene C 6 C l5 NO 2 (PCNB).
[0013] A method for recycling waste heat from a thermal power plant, comprising: absorbing heat from equipment such as the pipeline of a cooling tower of a power plant, the blowdown component of a boiler, and the exhaust component of a deaerator in a power plant, using the pressure calorific effect material having a glassy crystalline phase of the present invention, causing the material to undergo a phase transition to a high-temperature plastic crystalline phase, and then transforming the material from the high-temperature plastic crystalline phase to a glassy crystalline phase; and maintaining the glassy crystalline phase of the material to realize heat storage at a low temperature, and finally releasing and utilizing the heat by applying pressure.
[0014] A method for storing solar energy comprises absorbing heat generated by a solar collector using the pneumatic caloric effect material having a glassy crystalline phase of the present invention, causing the material to undergo a phase transition to a high-temperature plastic crystalline phase, and then transforming the material from the high-temperature plastic crystalline phase to a glassy crystalline phase. By maintaining the glassy crystalline phase of the material, heat storage at low temperatures is realized, and finally, the heat can be released and utilized by applying pressure.
[0015] A method for recycling and utilizing waste heat in a computer room of a data center, comprising: absorbing heat generated in the data center using a pneumatic caloric effect material having a glassy crystalline phase of the present invention, causing the material to undergo a phase transition to a high-temperature plastic crystalline phase, and then transforming the material from the high-temperature plastic crystalline phase to a glassy crystalline phase; maintaining the glassy crystalline phase of the material allows heat storage at low temperatures, and finally releasing and utilizing the heat by applying pressure.
[0016] The advantages and beneficial effects of the present invention are as follows: 1. Conventional phase change heat storage materials cannot accurately control the heat release time. The heat release time depends only on the temperature of the surrounding environment, and long-distance transportation and use cannot be realized. For example, people can only heat up a solar cooker when the sun is up, but by the time they are ready to cook dinner, the solar cooker may have dissipated all of its stored heat into the cool night air. The present invention organically combines the plastic crystalline phase and glassy crystalline phase of the pressure calorific effect material and utilizes the respective characteristics and advantages of these two phases to solve the limitations of conventional solid-solid phase change heat storage materials, such as small phase transition latent heat, small heat storage, inability to realize long-distance transportation, and inability to accurately control the heat release time.
[0017] 2. The solution of the present invention can be used to absorb waste heat in multiple scenarios. Based on the large entropy change characteristics of the plastic crystal phase transition process, an efficient cooling effect of the heat source is achieved. Compared with traditional solid-solid phase transition heat storage materials, the plastic crystal phase transition process can generate huge latent heat and entropy change. Because the plastic crystal phase is a highly disordered state, the orientation of the structural unit molecules of the material is completely disordered, but the center of mass positions form a regular lattice over a long distance. Because the disorder of the molecular orientation is significantly large, the entropy change during the solid phase transition becomes larger than the melting entropy, and the proportion of the disordered degree of freedom in the total degree of freedom of the system approaches the limit of maintaining the rigidity of the solid. The huge phase change entropy change can absorb a large amount of heat generated from the heat source, effectively reducing the temperature of the heat source, and achieving an efficient refrigeration effect.
[0018] 3. The solution of the present invention makes full use of the properties of the glassy crystalline phase of the pressure calorific effect material to achieve long-term storage and long-distance transport of heat. The glassy crystalline phase is an intermediate metastable state formed when the material transforms from a high-temperature plastic crystalline phase to a low-temperature ordered crystalline phase. Rapid cooling freezes the disordered state of the material at high temperatures by supercooling. This avoids the full orientation ordering that usually occurs at low temperatures. The presence of a disordered state in the glassy crystalline phase causes a large entropy change. At the same time, since there is an energy barrier between the glassy crystalline phase and the low-temperature ordered crystalline phase, this state can be stored at a low temperature for a long time without spontaneously transitioning to the low-temperature crystalline phase, allowing long-distance heat transport, unless it is affected by an external field.
[0019] 4. As with other barocaloric materials, the phase transition from the glassy crystalline phase to the ordered crystalline phase can be achieved by applying hydrostatic pressure or other methods, which releases a large amount of latent heat of phase transition. This process is simple to operate, has low economic costs, and does not require harsh and complicated equipment or working conditions. This allows controllable heat release and utilization by applying hydrostatic pressure or needle pressure to barocaloric materials in low temperature environments such as near the freezing point or in situations where heat utilization is required.
[0020] 5. The phase transition behavior of the present invention is all solid-solid phase transition, and has the advantages of small volume change, no phase separation, no liquid leakage, low corrosiveness, and simple device. 2-Amino-2-methyl-1,3-propanediol (CH 3 )C(CH 2 )(CH 2 OH) 2 Take AMP for example. Compared with other solid-solid phase transition materials, its heat storage capacity has a great advantage. The entropy change is 487Jkg -1 K -1 It even reaches.
[0021] 6. The solution of the present invention can be applied to the recycling of waste heat in thermal power plants, transferring and storing waste heat in pressure calorific materials, and transporting the recovered waste heat long distances to low temperature environments where heating is required. In the scene where heat is needed, the heat is released with less pressure to achieve the purpose of heating. The present invention can also be applied to the long-term storage and utilization of solar energy, the recycling of waste heat in computer rooms of data centers, etc., and has a wide range of application potential. [Brief description of the drawings]
[0022] [Figure 1] 1 is a schematic diagram of the phase transition process and heat absorption and release of a barocaloric material having a glassy crystalline phase. FIG. [Diagram 2] This is a heat flow curve of AMP during the heating process from a low-temperature ordered crystalline phase to a high-temperature plastic crystalline phase. [Diagram 3] 1 is a heat flow curve of AMP during cooling from a high-temperature plastic crystalline phase to a glassy crystalline phase. [Figure 4] 1 shows the heat flow curves when pressure is applied to the AMP glassy crystalline phase in an adiabatic state at 273 K to achieve heat dissipation. [Diagram 5] 1 is a temperature change curve when pressure is applied to the AMP glassy crystalline phase at room temperature to achieve heat dissipation. [Figure 6] 1 shows the cyclic heat flow curves of AMP between the high temperature plastic crystalline phase and the glassy crystalline phase. [Figure 7] 1 shows the heat flow curve of the glassy crystalline phase of AMP maintained at 273 K for 24 hours. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] In order to better understand the present invention, the present invention is illustrated by the following examples, which are intended to further illustrate the features and advantages of the present invention and are not intended to limit the scope of the claims.
[0024] The solution of the present invention is a controllable solid-state phase transition heat storage and release method of pressure caloric effect materials, which includes:
[0025] Step 1: Heat the pressure caloric effect material sample to the high-temperature plastic crystalline phase. Heating methods include, but are not limited to, using the sample chamber of a microcalorimeter to increase the temperature or using a heating stage to directly heat the sample.
[0026] Step 2: Rapidly cool the high-temperature plastic crystal phase barocaloric material to obtain a glassy crystal phase barocaloric material. This achieves long-term thermal energy storage in the barocaloric material. The glassy crystal phase is an intermediate metastable state formed during the transformation of the barocaloric material into an ordered crystal, and is obtained by sufficiently rapid cooling of the high-temperature disordered state of the plastic crystal phase. Rapid cooling freezes the high-temperature disordered state of the plastic crystal phase by supercooling, thereby avoiding the full orientation ordering that usually occurs at low temperatures. Due to the existence of a disordered state in the glassy crystal phase, the material in that state still retains a large amount of entropy change. This state allows long-distance heat transport without spontaneously transitioning to a low-temperature crystalline phase even when stored at a low temperature for a long time unless affected by an external field. Methods of rapid cooling include, but are not limited to, rapid cooling at a cooling rate of ≧2K / min, or instantaneous cooling of the high-temperature plastic phase sample with ice water or liquid nitrogen.
[0027] Step 3: When a small external pressure is applied to the glassy crystalline phase material at low temperature, a phase transition from glassy crystal to regular crystal is achieved, and the disordered state of the molecules undergoes a complete orientation and order transformation, accompanied by a large entropy change, and the release of heat is also achieved. When heat needs to be released, hydrostatic pressure or pinprick pressure is used as the driving method to control the release of heat and realize controllable heat storage, transfer and utilization.
[0028] The solution of the present invention also relates to a heat storage and heat exchange device containing a pressure caloric effect material. The device includes a heating unit, a rapid cooling unit, and a pressurizing unit. The heating unit is used to make the pressure caloric effect material into a high-temperature plastic crystalline phase. The rapid cooling unit is used to rapidly cool the pressure caloric effect material in a high-temperature plastic crystalline phase to obtain a pressure caloric effect material in a glassy crystalline phase. When heat needs to be released, the pressurizing unit applies hydrostatic pressure or pinprick pressure to the pressure caloric effect material to control the release of heat, thereby realizing the controllable storage, transfer, and utilization of thermal energy. Figure 1 shows the cycle process. The pressure caloric effect material is used as an energy transfer material in a heat storage and heat exchange device, and realizes the solid-state refrigeration function by utilizing the endothermic process of transition from a low-temperature regular crystalline phase to a high-temperature plastic crystalline phase. The phase transition from a glassy crystalline phase to a low-temperature regular crystalline phase is achieved by a driving method such as hydrostatic pressure, thereby realizing the heat storage and utilization function of solid-state phase transition.
[0029] The pressure calorie effect material of the present invention is a pressure calorie effect material having a glassy crystal phase, and is preferably a plastic crystal material having a glassy crystal phase. Since a plastic crystal material is a type of highly disordered solid material, the orientation of the structural unit molecules is completely disordered, but the center of gravity positions form a regular lattice over a long distance, so it is also called a rotationally disordered crystal. Since the disorder of the molecular orientation is extremely large, the entropy change during the solid phase transition becomes larger than the melting entropy, and the ratio of the disordered degree of freedom to the total degree of freedom of the system approaches the limit for maintaining the rigidity of the solid. The weak interaction between molecules results in a very large compressibility, and the intermolecular interaction can be adjusted even with a small pressure, causing a phase transition between an ordered phase and a disordered phase, which results in a change in entropy. In the case of a glassy crystal phase, compared to a plastic crystal phase, the center of gravity positions maintain a long-range ordered state, but the orientation disorder state of the organic molecules and inorganic structural units is frozen by supercooling, and is no longer in a completely disordered rotation state. Nevertheless, the glassy crystalline phase still has a high degree of disorder compared to conventional crystalline phases. Table 1 shows the specific differences between various phase structures and states. Therefore, the plastic crystalline barocaloric effect material with a glassy crystalline phase has properties such as large phase transition entropy change, pressure-tunable phase transition and controllability of entropy change, and these features are fully applicable to the method, apparatus, and application of the present invention. The barocaloric effect material used in the embodiments of the present invention is a barocaloric effect material with a glassy crystalline phase, and preferably 2-amino-2-methyl-1,3-propanediol ((CH 3 )C(CH 2 )(CH 2 OH) 2 (AMP), m-carborane C 2 B 10 H 12 , 1-cyanoadamantane C 11 H 15 N (CAN), Adamantanone C 10 H 14 O (AON), and pentachloronitrobenzene C 6 C l5 NO 2(PCNB). Among these, 2-amino-2-methyl-1,3-propanediol (CH 3 )C(CH 2 )(CH 2 OH) 2 (AMP), or m-carborane C 2 B 10 H 12 More preferably, 2-amino-2-methyl-1,3-propanediol (CH 3 )C(CH 2 )(CH 2 OH) 2 (AMP) is even more preferable.
[0030] [Table 1]
[0031] The application of the present invention also includes recycling waste heat in thermal power plants. In one embodiment, a pressure caloric effect material with a low temperature regular crystalline phase and a glassy crystalline phase is placed in the cooling tower of a power plant, and when the circulating cooling water heated by waste heat flows through the pressure caloric effect material, the material changes from a low temperature phase to a high temperature plastic crystalline phase, and the waste heat is transferred to the material and stored. At the same time, the circulating water is cooled and continues to flow around to recover waste heat from the power plant. After the high temperature plastic crystalline phase material is rapidly cooled, it changes to a glassy crystalline phase. This can realize the long-distance transportation of the waste heat collection material to the low temperature environment that needs heating. When heat is needed, the material changes from the glassy crystalline phase to the low temperature regular crystalline phase by applying a smaller pressure, achieving the purpose of releasing heat for heating.
[0032] The application of the present invention also includes the use of a pressure caloric effect material with a glassy crystalline phase to store solar energy. In one embodiment, the pressure caloric effect material is used to absorb heat generated by a solar collector. For example, the pressure caloric effect material is placed in a solar collector or heat storage component, and the material undergoes a phase transition to a high-temperature plastic crystal. The material then changes from the high-temperature plastic crystal phase to a glassy crystalline phase, and maintains the glassy crystalline phase to achieve low-temperature heat storage, and finally releases and utilizes the heat by applying pressure.
[0033] The application of the present invention also includes recycling waste heat in computer rooms of data centers. In one embodiment, a pneumatic caloric effect material with a glassy crystalline phase is used to absorb heat generated in a data center. For example, the pneumatic caloric effect material is placed at the heat-dissipating end of a data center host, and the material undergoes a phase transition to a high-temperature plastic crystalline phase state when subjected to heat. The material then changes from the high-temperature plastic crystalline phase to a glassy crystalline phase. By maintaining the material in the glassy crystalline phase state, heat storage at low temperatures is realized, and finally, the heat is released and utilized by applying pressure.
[0034] In the following, 2-amino-2-methyl-1,3-propanediol (CH 3 )C(CH 2 )(CH 2 OH) 2 Taking (AMP) as an example, a preferred embodiment of the present invention will be described in detail.
[0035] First embodiment for obtaining a glassy crystalline phase: A bulk sample of AMP in the low-temperature regular crystalline phase was placed in an airtight high-pressure sample cell, and the empty comparative sample cell was placed in the sample chamber of a μDSC7 (Setalam, France) microcalorimeter. The two sample cells were purged with nitrogen using a booster device to maintain atmospheric pressure (0.1 MPa), and the sample was heated from 228 K to 383 K at a heating rate of 2 K / min. The heat flow data of the sample was recorded and shown in the curve in Figure 2. AMP undergoes a phase transition at 355 K, and the corresponding enthalpy change is 215 Jg. -1, the entropy change is 606 Jkg -1 K -1 It can be seen that this process can absorb heat from a heat source to achieve a cooling effect. The endothermic peak that appears around 381K corresponds to the melting point of AMP. In this way, a high-temperature plastic crystal phase of AMP is obtained.
[0036] Next, the sample in the high-temperature plastic crystalline phase is quenched to a low-temperature state of 273 K at a cooling rate of more than 2 K / min, and the high-temperature disordered state of the sample is frozen by supercooling, which avoids the fully oriented ordering that usually occurs at low temperatures. Finally, AMP transitions to a glassy crystalline phase state. The recorded heat flow data of the sample is shown in the curve in Figure 3. It can be seen that a heat dissipation peak appears at 378 K, which corresponds to the freezing point of AMP. Unlike the heating process, no obvious heat dissipation peak was observed during the cooling process below that point. This feature can be used to store and transport heat without being affected by spontaneous phase transitions due to cooling.
[0037] Second embodiment for obtaining a glassy crystalline phase: When a powder sample of AMP in the ordered crystalline phase is placed in a glass container at room temperature and heated using a heating device such as a heating table, and the temperature exceeds the thermal phase transition temperature of AMP (the transition from the low-temperature ordered crystalline phase to the high-temperature plastic crystalline phase), AMP in the high-temperature plastic crystalline phase is obtained. By rapidly cooling the AMP in this state with ice water or liquid nitrogen, the high-temperature disordered state is instantly frozen by supercooling, and a glassy crystalline phase state is obtained.
[0038] Thermal Energy Storage: By storing the obtained glassy crystalline phase continuously at 273 K or by heating to a temperature below room temperature, AMP can be maintained in the glassy crystalline phase for a long period of time without spontaneously changing to a low-temperature ordered crystalline phase. This feature allows AMP materials in the glassy crystalline phase to be used in a variety of low-temperature environments and avoids spontaneous phase transitions due to temperature changes, making it possible to transport them over long distances without spontaneous phase transitions or heat dissipation.
[0039] Controllable Heat Release: The glassy crystalline phase AMP material obtained in the first embodiment is stored continuously at a temperature of 273K. After 2 hours of keeping in this state, a booster device is used to flow nitrogen into the two sample cells, and the gas pressure is instantly increased to 67 bar, and the heat flow data of the sample is recorded and shown in the curve in Figure 4. When a pressure of 67 bar is applied to the AMP glassy crystalline phase in the keeping state at a temperature of 273K, the sample shows an obvious heat release peak, which corresponds to the heat generation process of the phase transition from the AMP glassy crystalline phase to the low-temperature phase under pressure. The corresponding enthalpy change value is 133 Jg -1 , the entropy change is 487 Jkg -1 K -1 This result indicates that the heat stored in the AMP glassy crystalline phase can be controlled by applying a small pressure to achieve active heat release. The transformation of AMP from the glassy crystalline phase to the ordered crystalline phase can be achieved by applying pressure. This phase transition is accompanied by the release of a large amount of latent heat, thereby achieving the controlled release and controllable utilization of the heat stored inside the AMP material.
[0040] For the sample obtained by the second embodiment, a K-type thermocouple is used to measure and monitor the temperature of the AMP material in the glassy crystalline phase state stored at room temperature in real time. When the temperature is constant at room temperature, a sharp object such as a needle is used to pierce and apply pressure to cause a phase transition from the glassy crystalline phase to a low-temperature regular crystalline phase, and the temperature of the sample is monitored in real time at the same time. The results are shown in the curves of Figure 5. Simultaneously with the phase transition, the temperature of the sample rises instantly, and under imperfect adiabatic conditions, the temperature change is shown to reach 32.5K, thereby achieving the active release and controllable utilization of the accumulated heat.
[0041] Heating / cooling cycle process of AMP from high temperature phase to glassy crystal: The AMP sample in the low-temperature ordered crystalline phase was placed in an airtight high-pressure sample cell, and the comparison sample cell was placed empty in the sample chamber of a μDSC7 (Setalam, France) microcalorimeter. Nitrogen was flowed into the two sample cells using a booster device to maintain normal pressure (0.1 MPa), and the sample was heated from 273 K to 383 K at a heating rate of 2 K / min, and then cooled to 273 K at a cooling rate of 2 K / min. The above process was repeated six times, and the heat flow data of the sample was recorded and shown in the curve in Figure 6. The results show that AMP can be cycled in the temperature range from high temperature to 273 K, without any transition from the glassy crystalline phase to the low-temperature ordered phase during the heating or cooling process.
[0042] Stability of AMP glassy crystalline phase over time: The AMP sample with low-temperature regular crystalline phase was placed in an airtight high-pressure sample cell, and the control sample cell was left empty and placed in the sample chamber of a μDSC7 (Setalam, France) microcalorimeter. Nitrogen was introduced into the two sample cells using a booster device to maintain normal pressure (0.1 MPa), and the sample was heated from 273 K to 383 K at a heating rate of 2 K / min, and then cooled to 273 K at a cooling rate of 2 K / min. The temperature was then set to 273 K and kept for 24 hours, and the heat flow data of the sample was recorded and shown in the curve in Figure 7. This result indicates that the glassy crystalline phase of AMP can be stably stored in an environment at an ambient temperature of 273 K and has aging stability. This feature ensures the thermal energy storage of this type of material in a low-temperature environment.
[0043] Application Example 1 of the method and material of the present invention in solid-state phase change heat storage: Usually, the actual thermal efficiency of a thermal power plant is low, and about 60% of the heat is taken away by the circulating cooling water of the condenser and released to the environment. The cooling water circulating in the power plant is a low-grade thermal energy, and the range of direct use is limited, so in the past, a direct discharge method by a cooling tower was used. Meanwhile, in the production process of a thermal power plant, various waste heat is generated, such as steam leakage of the shaft seal, boiler blowdown, exhaust of the deaerator, etc., which are all processes that carry waste heat. This amount of heat has been directly released to the environment without being utilized until now. The released heat not only causes thermal pollution to the environment, but also reduces the energy efficiency of the thermal power plant. In the above heat generation and heat dissipation process, the low-temperature regular crystalline AMP is placed in the pipelines of the cooling tower, boiler blowdown component, deaerator exhaust component and other equipment of the power plant, so that when the temperature of the above pipeline or component exceeds 355K, the AMP changes from a low-temperature phase to a high-temperature plastic crystalline phase, thereby transferring and storing the waste heat in the AMP, and at the same time, the cooling of the pipeline or component is achieved. After the waste heat is recovered, when the ambient temperature is reduced, the AMP will gradually transform from the high-temperature phase to the glassy crystalline phase without changing to the low-temperature regular crystalline phase, realizing heat storage without energy loss. The reduction in the ambient temperature does not cause spontaneous phase transition and heat release. Therefore, AMP in the glassy crystalline phase can be transported over long distances and can be transported to remote low-temperature environments (e.g., below 273K). Finally, in scenarios where heat needs to be used, the AMP can be transformed from the glassy crystalline phase to the low-temperature regular crystalline phase by applying a small pressure, and this process is accompanied by the release of a large amount of latent heat. The purpose of controlling the phase transition and actively controlling heat release by utilizing pressure stimulation is realized.
[0044] Application Example 2 of the method and material of the present invention in solid-state phase change heat storage: Solar energy is a clean renewable energy, and among renewable energy, solar energy is the most widely distributed and the easiest to utilize. However, solar energy is very intermittent and unstable. In order to operate the utilization of solar energy stably, a heat storage device to store solar energy is required. Based on the above solar heat storage scenario, the low-temperature regular crystalline phase AMP can be placed in a solar heat collector or heat storage component, and when the above heat is collected and the temperature of the AMP exceeds 355K, the AMP changes from the low-temperature phase to the high-temperature plastic crystalline phase, and the thermal energy generated by the solar energy is transferred to the AMP and stored. After collecting a large amount of heat, when the ambient temperature drops rapidly, the AMP gradually transforms from the high-temperature phase to the glassy crystalline phase without changing to the low-temperature regular crystalline phase, thereby realizing heat storage. The drop in the ambient temperature does not cause spontaneous phase transition and release of heat. Therefore, the AMP in the glassy crystalline phase can be transported over long distances and can be transported to remote low-temperature environments (e.g., below 273K). Finally, in scenarios requiring the use of heat, AMP can be transformed from a glassy crystalline phase to a low-temperature ordered crystalline phase by applying a small amount of pressure. This process is accompanied by the release of a large amount of latent heat. By controlling the phase transition, the aim of actively controlling the heat release can be realized by utilizing pressure stimulation.
[0045] Application Example 3 of the method and material of the present invention in solid-state phase change heat storage: Data centers are becoming more and more popular around the world. On the one hand, 5G is gradually moving towards large-scale commercial use, and data centers, as carriers of information processing equipment, are shouldering enormous business needs. On the other hand, data centers are included in the national "new infrastructure" strategic category, becoming an important part of the national information infrastructure construction and an important support for building a "dual circulation of the economy" pattern. However, the rapid increase in the power consumption of a single machine in a data center will directly lead to a significant increase in the temperature of the equipment in the computer room, which not only impairs the performance of the equipment, but also consumes a lot of power costs for the operation of refrigeration equipment such as air conditioners. For such applications, for example, an AMP with a low-temperature regular crystalline phase can be installed at the heat dissipation end of a data center host, and when the heat dissipation temperature exceeds 355K, the AMP undergoes a phase transition from a low-temperature phase to a high-temperature plastic crystalline phase, which allows the heat to be transferred to the AMP and stored. After collecting a large amount of heat, when the ambient temperature drops rapidly, the AMP will gradually transform from a high-temperature phase to a glassy crystalline phase without changing to a low-temperature regular crystalline phase, thereby realizing heat storage. A decrease in the ambient temperature does not result in spontaneous phase transition and heat release. Therefore, AMP in the glassy crystalline phase can be transported over long distances and can be transported to remote low-temperature environments (e.g., below 273 K). Finally, in scenarios where the use of heat is required, AMP can be transformed from the glassy crystalline phase to a low-temperature ordered crystalline phase by applying a small pressure. This process is accompanied by the release of a large amount of latent heat. The objective of controlling the phase transition and actively controlling heat release using pressure stimulation is realized.
[0046] The above-mentioned embodiments are only intended to explain the technical concepts and features of the present invention. The purpose is to enable those skilled in the art to understand the contents of the present invention and implement them accordingly, and is not intended to limit the protection scope of the present invention. On the contrary, any effective changes or modifications made based on the spirit of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for controllable solid-state phase change heat storage and release in a pressure caloric effect material, comprising the steps of: Step 1: A barocaloric material sample is heated to a high temperature plastic crystalline phase. Step 2: quenching the high temperature plastic crystal phase pneumatic caloric effect material to obtain a glass crystal phase pneumatic caloric effect material, so as to achieve long-term thermal energy storage in the glass crystal phase pneumatic caloric effect material. Step 3: When heat needs to be released, pressure is applied as a driving method to control the release of heat, realizing the controllable storage, transfer and utilization of thermal energy.
2. 2. The method according to claim 1, characterized in that in step 2, the rapid cooling method for obtaining the glassy crystalline phase includes cooling at a cooling rate of 2 K / min or more, or instantly cooling the sample of the high-temperature plastic crystalline phase with ice water or liquid nitrogen.
3. 2. The method according to claim 1, wherein in step 3, the method of applying pressure includes hydrostatic pressure or needle pressure.
4. 2. The method of claim 1, wherein the pneumatic caloric effect material is a pneumatic caloric effect material having a glassy crystalline phase.
5. The pressure calorie effect material is 2-amino-2-methyl-1,3-propanediol (CH 3 ) C(CH 2 ) (CH 2 O.H. 2 (AMP), m-carborane C 2 B 10 H 12 , 1-cyanoadamantane C 11 H 15 N (CAN), Adamantanone C 10 H 14 O (AON), and pentachloronitrobenzene C 6 C l5 NO 25. The method of claim 4, wherein the polycyclic aromatic hydrocarbons (PAH) are one or more of the following:
6. When the pressure caloric effect material is 2-amino-2-methyl-1,3-propanediol (AMP), a phase transition occurs at 355K, absorbing heat and changing into a high-temperature plastic crystalline phase state, and the corresponding enthalpy change value is 215 Jg -1 , the entropy change is 606 Jkg -1 K -1 The method according to claim 5, characterized in that
7. The method according to claim 5, characterized in that when 2-amino-2-methyl-1,3-propanediol (AMP) in a high-temperature plastic crystalline phase state is quenched to a low-temperature state of 273K, a glassy crystalline phase state is obtained.
8. The method according to claim 5, characterized in that when the obtained 2-amino-2-methyl-1,3-propanediol (AMP) in a glassy crystalline phase state is stored at 273 K or heated to a temperature below room temperature, spontaneous phase transition and heat release do not occur, and heat is stored in the 2-amino-2-methyl-1,3-propanediol (AMP) material for a long period of time.
9. When pressure is applied to 2-amino-2-methyl-1,3-propanediol (AMP) at 273 K, a clear exothermic peak appears, and the corresponding enthalpy change is 133 Jg. -1 The entropy change is 487 Jkg -1 K -1 The method according to claim 8, characterized in that
10. 10. The method according to claim 9, characterized in that the applied pressure value is equal to or greater than 67 bar.
11. A heat storage and heat exchange device with a pressure caloric effect material, comprising a heating unit, a rapid cooling unit and a pressurizing unit. The heating unit is used to heat the pressure caloric effect material to a high-temperature plastic crystal phase. The rapid cooling unit is used to rapidly cool the high-temperature plastic crystal phase pressure caloric effect material to obtain a glass crystal phase pressure caloric effect material. The pressurizing unit applies hydrostatic pressure or pinprick pressure to the pressure caloric effect material when heat needs to be released, thereby controlling the release of heat and realizing the controllable storage, transfer and utilization of thermal energy.
12. In the heat storage and heat exchange device according to claim 11, the pressure calorific effect material is 2-amino-2-methyl-1,3-propanediol (CH 3 ) C(CH 2 ) (CH 2 O.H. 2 (AMP), m-carborane C 2 B 10 H 12 , 1-cyanoadamantane C 11 H 15 N (CAN), Adamantanone C 10 H 14 O (AON), and pentachloronitrobenzene C 6 C l5 NO 2 (PCNB).
13. A method for recycling waste heat from a thermal power plant, comprising: absorbing heat from equipment such as a cooling tower pipeline, a boiler blowdown component, and a deaerator exhaust component in a power plant by using the pressure calorific effect material according to claim 1, causing the material to undergo a phase transition to a high-temperature plastic crystalline phase, and then transforming the material from the high-temperature plastic crystalline phase to a glassy crystalline phase; maintaining the material in the glassy crystalline phase state, thereby realizing heat storage at a low temperature; and finally releasing and utilizing the heat by applying pressure.
14. A method for storing solar energy, comprising: absorbing heat generated by a solar collector using the pressure calorific effect material according to claim 1, causing the material to undergo a phase transition to a high-temperature plastic crystalline phase, and then transforming the material from the high-temperature plastic crystalline phase to a glassy crystalline phase; maintaining the material in the glassy crystalline phase allows heat storage at low temperatures; and finally releasing and utilizing the heat by applying pressure.
15. A method for recycling waste heat from computer rooms in data centers, comprising: absorbing heat generated from the data center using the pressure calorie effect material according to claim 1, causing the material to undergo a phase transition to a high-temperature plastic crystalline phase, and then transforming the material from the high-temperature plastic crystalline phase to a glassy crystalline phase; maintaining the material in the glassy crystalline phase allows heat storage at low temperatures; and finally releasing and utilizing the heat by applying pressure.
Citation Information
Patent Citations
Heat storage medium, heat storage device and method for using heat storage medium
JP2019077831A
Use of barocaloric materials and barocaloric devices
JP2019537642A
Heat storage / radiation layer-forming composition, heat storage / radiation layer comprising the composition, and heat storage / radiation laminate
JP2020076031A
Heat storage and radiation material, and manufacturing method therefor