Carbon nanotube dispersion, its manufacturing method, electrode slurry composition containing the same, electrode containing the same, and lithium secondary battery containing the same

The carbon nanotube dispersion with specific dispersants and alkali metal salts addresses the dispersibility challenge, enhancing electrode manufacturing efficiency and battery performance by maintaining low viscosity and preventing agglomeration.

JP2024539495AActive Publication Date: 2024-10-28BETTERIAL CO LTD

Patent Information

Application Number
JP2024547396
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-10-18
Filing Date
2022-10-19
Publication Date
2024-10-28
Estimated Expiration
2042-10-19

AI Technical Summary

Technical Problem

Conventional conductive materials like carbon black require high amounts to achieve sufficient conductivity, reducing the electrode active material content and battery capacity, while carbon nanotubes offer high conductivity at lower amounts but face challenges in dispersing efficiently in aqueous solutions.

Method used

A carbon nanotube dispersion is developed using a first dispersant with an amide group and a second dispersant with an aromatic ring, maintaining low viscosity and preventing agglomeration, enhanced by the use of alkali metal salts and specific pH conditions, ensuring improved dispersibility and processability.

Benefits of technology

The carbon nanotube dispersion achieves low viscosity, enhances dispersibility, and improves coating properties, facilitating efficient electrode manufacturing with improved conductivity and reduced agglomeration, leading to better battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024539495000001
    Figure 2024539495000001
  • Figure 2024539495000002
    Figure 2024539495000002
  • Figure 2024539495000003
    Figure 2024539495000003
Patent Text Reader

Abstract

The present specification relates to a method for producing a dispersion medium comprising: a carbon nanotube; a first dispersant having an amide group; and a second dispersant having an aromatic ring; and the dispersion medium is heated at 25° C. for 15 seconds. -1 The present invention relates to a carbon nanotube dispersion having a viscosity of 2,000 cPs or less at a shear rate of 1000 rpm, a method for producing the same, an electrode slurry composition containing the same, an electrode containing the same, and a lithium secondary battery containing the same.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This specification claims the benefit of the filing date of No. 10-2021-0139170 filed with the Korean Intellectual Property Office on October 19, 2021, and No. 10-2022-0133711 filed with the Korean Intellectual Property Office on October 18, 2022, the contents of which are incorporated herein by reference. The present specification relates to a carbon nanotube dispersion, a method for producing the same, an electrode slurry composition containing the same, an electrode containing the same, and a lithium secondary battery containing the same. [Background technology]

[0002] A secondary battery is a battery that can be repeatedly used through a discharge process in which chemical energy is converted into electrical energy and a charging process in the reverse direction. A secondary battery is composed of a positive electrode, a negative electrode, an electrolyte, and a separator, and the positive electrode and the negative electrode are generally composed of an electrode current collector and an electrode active material layer formed on the electrode current collector. The electrode active material layer is manufactured by applying an electrode slurry composition containing an electrode active material, a conductive material, a binder, etc., onto an electrode current collector, drying it, and rolling it. The conductive material is used to improve the conductivity of the electrode active material, and conventionally, dot-shaped conductive materials such as carbon black have been mainly used. However, since the dot-shaped conductive material does not have a high effect of improving electrical conductivity, it must be used in excess to obtain a sufficient effect, which reduces the content of the electrode active material and reduces the battery capacity. In order to solve these problems, there have been many attempts to use highly conductive carbon nanotubes (CNTs) as a conductive material. Carbon nanotubes can achieve high conductivity even in small amounts, so when carbon nanotubes are used, the amount of conductive material can be significantly reduced compared to when carbon black is used, which has the advantage of increasing the electrical capacity. In order to utilize carbon nanotubes as a negative electrode conductive material, it is necessary to produce a low-viscosity aqueous dispersion from the viewpoint of processability. Polyvinylpyrrolidone (PVP), a dispersant having an amide group, is a polymer surfactant that is used as a dispersant, emulsifier, thickener, etc. in various dispersion systems and is known to be effective when dispersing carbon nanotubes (Patent Document 1). Polyacids containing a carboxy group, such as polyacrylic acid and tannic acid, are also known to be effective in dispersing carbon nanotubes. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Korean Patent Publication No. 10-2011-0118460 [Non-patent literature]

[0004] [Non-Patent Document 1] Toxicol.Res., 2015,4, 160-168 Summary of the Invention [Problem to be solved by the invention]

[0005] The present specification provides a carbon nanotube dispersion, a method for producing the same, an electrode slurry composition containing the same, an electrode containing the same, and a lithium secondary battery containing the same. [Means for solving the problem]

[0006] One embodiment of the present invention comprises a carbon nanotube and a first dispersant having an amide group; a second dispersant having an aromatic ring; 25℃ and 15sec -1 The present invention provides a carbon nanotube dispersion having a viscosity of 2,000 cPs or less at a shear rate of 1000 g / mol / L. Another embodiment of the present invention is a method for producing a semiconductor device comprising: a first dispersant having an amide group; and a second dispersant having an aromatic ring. Another embodiment of the present invention provides an electrode slurry composition comprising the above-mentioned carbon nanotube dispersion, an electrode active material and a binder. Another embodiment of the present invention provides an electrode comprising an electrode active material layer formed by the electrode slurry composition described above. Another embodiment of the present invention provides a lithium secondary battery including the electrode described above. Effect of the Invention

[0007] The carbon nanotube dispersion according to one embodiment of the present invention has a significantly low viscosity, and has an effect of improving the dispersibility of carbon nanotubes in the dispersion. The carbon nanotube dispersion according to an embodiment of the present invention has excellent coating properties and processability when used to manufacture an electrode. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] The present invention will be described in detail below. The carbon nanotube dispersion according to an embodiment of the present invention means a dispersion containing carbon nanotubes. Specifically, it means that carbon nanotubes are dispersed in the dispersion and are not aggregated with each other. One embodiment of the present invention includes carbon nanotubes, a first dispersant having an amide group, and a second dispersant having an aromatic ring, and is heated at 25° C. for 15 seconds. -1 The present invention provides a carbon nanotube dispersion having a viscosity of 2,000 cPs or less at a shear rate of 1000 g / mol / L.

[0009] The carbon nanotube dispersion contains a first dispersant having an amide group and a second dispersant having an aromatic ring, thereby reducing the viscosity of the dispersion. In particular, the complex structure of the second dispersant having an aromatic ring can effectively reduce the viscosity of the dispersion. In particular, when the second dispersant contains a functional group (hydroxyl or carboxyl group), the oxygen of the amide group contained in the first dispersant and the functional group (hydroxyl or carboxyl group) of the second dispersant form hydrogen bonds with each other, which has the effect of contributing to a decrease in the viscosity of the dispersion. However, there is a problem that the hydrogen bonds are too strong and insoluble matter or aggregates (complexes) are formed. In this case, there are many restrictions on the selection of dispersants, such as the need to adjust the contents of the first dispersant and the second dispersant, or to use only specific types of first dispersant and / or second dispersant.

[0010] The present inventors have developed a dispersion in which the phenomenon of aggregation between the first and second dispersants described above is improved, even though the dispersion contains the above-mentioned dispersants, and have completed the present invention. The improvement in the aggregation phenomenon can be confirmed by producing a carbon nanotube dispersion containing these substances, leaving it for a certain period of time, and then visually observing whether or not aggregation occurs. The carbon nanotube dispersion according to an embodiment of the present invention has a characteristic that the carbon nanotubes have excellent conductivity, but the dispersibility of the carbon nanotubes is improved and the aggregation of the carbon nanotubes is minimized. The above characteristic can be confirmed by the extremely low viscosity of the dispersion.

[0011] In one embodiment of the present invention, the carbon nanotube dispersion liquid is heated at 25° C. for 15 seconds. -1The viscosity at a shear rate of 2,000 cPs or less, 1,000 cPs or less, 800 cPs or less, 700 cPs or less, or 500 cPs or less may be. Considering the object of the present invention, the lower the viscosity, the better, so the lower limit is not particularly limited, but may be 10 cPs or more, 30 cPs or more, or 50 cPs or more. When the above viscosity range is satisfied, the carbon nanotubes in the carbon nanotube dispersion do not aggregate with each other, and the processability is improved when used to manufacture an electrode. The viscosity of the carbon nanotube dispersion can be measured by a method commonly used in the field of this technology. For example, the viscosity of the carbon nanotube dispersion can be measured by a Brookfield DVNextCP Rheometer at a measurement temperature of 25° C. and a 15 sec -1 For more accurate measurement, the carbon nanotube dispersion liquid prepared can be stored at 25° C. for one week before measurement.

[0012] The viscosity of the carbon nanotube dispersion can be adjusted by adjusting the contents of the first dispersant and the second dispersant, or by adding an alkali metal salt to the dispersion, which will be described later.

[0013] In one embodiment of the present invention, the carbon nanotube dispersion liquid includes a first dispersant having an amide group and a second dispersant having an aromatic ring. The first dispersant having an amide group is effective in dispersing carbon nanotubes, and the viscosity of the dispersion liquid can be effectively reduced by the complex structure of the second dispersant having an aromatic ring. In addition, the oxygen of the amide group contained in the first dispersant and the functional group (hydroxyl group or carboxy group) of the second dispersant form hydrogen bonds with each other, which contributes to reducing the viscosity of the dispersion liquid. In one embodiment of the present invention, the first dispersant has an amide group, and is therefore capable of forming a hydrogen bond with a hydroxyl group or a carboxyl group of a second dispersant described below.

[0014] In one embodiment of the present invention, the first dispersant may include at least one selected from the group consisting of polyvinylpyrrolidone, polyester amide, polycarboxylic amide, polyamido amine, thioamido amine, and water soluble nylon. The first dispersant has an amide group, which allows it to exhibit an improved viscosity improving effect and an effect of suppressing the change in viscosity over time. In one embodiment of the present invention, the weight average molecular weight of the first dispersant may be 1,000 g / mol to 100,000 g / mol, preferably 2,000 g / mol to 80,000 g / mol, more preferably 2,000 g / mol to 30,000 g / mol, and more preferably 2,000 g / mol to 15,000 g / mol. If the weight average molecular weight of the first dispersant is less than 1,000 g / mol, the carbon nanotube dispersion performance may be reduced, and there is a risk of the first dispersant eluting during electrode production. If the weight average molecular weight of the first dispersant is more than 100,000 g / mol, there is a risk of the viscosity of the carbon nanotube dispersion increasing, and the coating property and processability may be reduced, so it is preferable to adjust it within the above range.

[0015] In one embodiment of the present invention, the second dispersant may contain a hydroxyl group or a carboxyl group. The second dispersant may form a hydrogen bond with the amide group of the first dispersant by having a hydroxyl group or a carboxyl group. In one embodiment of the present invention, the second dispersant may contain two or more aromatic rings. For example, the second dispersant may contain two or more aromatic rings. For example, the second dispersant may be one or more selected from the group consisting of baicalin, luteolin, taxifolin, myricetin, quercetin, rutin, catechin, epigallocatechin gallate, butein, piceatannol and tannic acid, and may be preferably tannic acid, quercetin, epigallocatechin gallate, or a combination thereof. In one embodiment of the present invention, when the first dispersant and the second dispersant are used simultaneously, the dispersion effect can be improved compared to when each dispersant is used alone.

[0016] In one embodiment of the present invention, the second dispersant may be a phenolic compound. The phenolic compound may include at least one structure selected from the group consisting of a phenol structure, a catechol structure, a gallol structure, and a naphthol structure, in which at least one of the aromatic rings is a phenol structure, a catechol structure, a benzene ring, two hydroxyl groups, the gallol structure, a benzene ring, and one hydroxyl group, respectively. The phenol structure is a structure in which one hydroxyl group is bonded to a benzene ring, the catechol structure is a structure in which two hydroxyl groups are bonded to a benzene ring, the gallol structure is a structure in which three hydroxyl groups are bonded to a benzene ring, and the naphthol structure is a structure in which one hydroxyl group is bonded to naphthalene.

[0017] In one embodiment of the present invention, the carbon nanotube dispersion liquid may contain the first dispersant and the second dispersant in a weight ratio of 1:10 to 10:1. Preferably, the weight ratio may be 1:5 to 5:1, or 1:1 to 1:5. When the above range is satisfied, the dispersion effect of the carbon nanotubes can be improved and the viscosity of the dispersion liquid can be maintained low. In one embodiment of the present invention, the carbon nanotube is for improving the conductivity of the electrode, and the graphite sheet has a cylindrical shape with a nano-sized diameter and is sp 2The graphite sheet has a bond structure. At this time, the graphite sheet shows conductive or semiconductive properties depending on the angle and structure at which it is rolled up. Carbon nanotubes can be classified into single-walled carbon nanotubes (SWCNT), double-walled carbon nanotubes (DWCNT), and multi-walled carbon nanotubes (MWCNT) according to the number of bonds forming the wall, and these carbon nanotubes can be appropriately selected according to the use of the dispersion. In addition, the carbon nanotubes may have a secondary shape formed by agglomerating or arranging a plurality of carbon nanotubes, for example, a bundle-type carbon nanotube in which a plurality of carbon nanotubes are arranged or aligned in a certain direction, or an entangled-type carbon nanotube in which a plurality of carbon nanotubes are entangled in a ball or potato shape without a certain direction. In one embodiment of the present invention, the carbon nanotubes may be single-walled carbon nanotubes (SWCNTs).

[0018] In one embodiment of the present invention, the specific surface area (BET) of the carbon nanotubes is 10 m 2 / g~5,000m 2 / g, preferably 30m 2 / g~3,000m 2 / g, more preferably 50m 2 / g~2,000m 2 When the above numerical range is satisfied, the conductivity can be improved. The specific surface area (BET) of the carbon nanotubes can vary depending on the type of the carbon nanotubes.

[0019] In one embodiment of the present invention, the specific surface area (BET) of the single-walled carbon nanotubes is 800 m 2 / g~5,000m 2 / g, preferably 800m 2 / g~3,000m 2 / g, more preferably 900m 2 / g~2,000m 2 When the above numerical range is satisfied, an excellent effect of improving conductivity can be obtained. In one embodiment of the present invention, the carbon nanotubes may have an average particle size (D50) of 0.1 μm to 20 μm. Preferably, the average particle size (D50) may be 0.5 μm to 1 μm, 1 μm to 5 μm, or 2 μm to 4 μm. The average particle size (D50) refers to a particle size that corresponds to 50% of the cumulative number in a particle size distribution curve of the carbon nanotubes. The average particle size (D50) may be measured, for example, by using a laser diffraction method. Within the above range, the carbon nanotubes do not aggregate with each other, and dispersibility can be improved.

[0020] In one embodiment of the present invention, the content of the carbon nanotubes may be 0.01 wt% to 20 wt% based on the total weight of the carbon nanotube dispersion. Preferably, it may be 0.1 wt% to 10 wt% or 0.1 wt% to 8 wt%. The content of the carbon nanotubes may be appropriately adjusted depending on the specific surface area of ​​the carbon nanotubes used. For example, when the specific surface area is 800 m 2 When carbon nanotubes having a specific surface area of ​​100 / g or more are used, the content of the carbon nanotubes may be about 0.01wt% to 5wt%, preferably 0.01wt% to 3wt%, and more preferably 0.01wt% to 2wt% based on the total weight of the carbon nanotube dispersion. If the specific surface area and content of the carbon nanotubes are outside the above ranges, problems such as a reduced loading amount during electrode production, increased process costs, reduced adhesive strength due to binder migration during drying of the electrode, and increased viscosity of the carbon nanotube dispersion may occur. In one embodiment of the present invention, the carbon nanotube may include two or more carbon nanotube units. The carbon nanotube units may have a graphite sheet having a cylindrical shape with a nano-sized diameter, and may have a sp 2 It has a bond structure.

[0021] In one embodiment of the present invention, the diameter of the carbon nanotube unit may be 1 to 200 nm, 1 to 150 nm, or 1 to 100 nm, which can improve the dispersibility of carbon nanotubes and prevent an increase in resistance when applied to an electrode. In one embodiment of the present invention, the length of the carbon nanotube unit may be 0.1 μm to 200 μm, 0.1 μm to 150 μm, or 0.5 μm to 100 μm, which can improve the dispersibility of carbon nanotubes and prevent an increase in resistance when applied to an electrode. In one embodiment of the present invention, the aspect ratio (length / diameter) of the carbon nanotubes may be 5 to 50,000 or 10 to 15,000. Within the above numerical range, the dispersibility of the carbon nanotubes can be improved, and an increase in resistance when applied to an electrode can be prevented.

[0022] In one embodiment of the present invention, the carbon nanotube dispersion liquid may contain an alkali metal element. The carbon nanotube dispersion liquid of the present invention may improve the dispersibility of a material contained in the dispersion liquid by containing the alkali metal element. Specifically, the first dispersant and the second dispersant contained in the dispersion liquid may form a complex with each other, but such a complex has low solubility in a solvent such as water, which increases the viscosity of the dispersion liquid. However, the alkali metal contained in the carbon nanotube dispersion liquid of the present invention disintegrates the complex, thereby solving the above problem. In one embodiment of the present invention, the alkali metal may be in the form of an alkali metal salt, although the form is not particularly limited thereto. In one embodiment of the present invention, the content of the alkali metal element may be 1 ppm to 300 ppm, 5 ppm to 200 ppm, or 5 ppm to 150 ppm based on the entire carbon nanotube dispersion.

[0023] In one embodiment of the present invention, the carbon nanotube dispersion liquid may contain one or more alkali metal salts selected from the group consisting of KOH, NaOH, LiOH, KOHH2O, NaOHH2O, LiOHH2O, K2CO3, Na2CO3, and LiCO3. In one embodiment of the present invention, the first dispersant includes a polyvinylpyrrolidone resin, and the molar ratio of the alkali metal salt may be 60 mol or less based on 100 mol of vinylpyrrolidone units contained in the polyvinylpyrrolidone resin. Preferably, it may be 30 mol or less or 25 mol or less. The lower limit of the content is not particularly limited, but may be 0.1 mol or more, 1 mol or more, or 2 mol or more. When the above range is satisfied, the viscosity of the carbon nanotube dispersion is preferably 20 mol or less at 25° C. and 15 sec. -1 The shear rate can be adjusted to 2,000 cPs or less.

[0024] The molar ratio of the alkali metal salt can be calculated using the molecular weight of the alkali metal salt and the vinylidone unit, and the weight percentage of the alkali metal salt and polyvinylidone, specifically, by the following formula 3. [Formula 3] Molar ratio of alkali metal salt={(weight % of alkali metal salt) / (molecular weight of alkali metal salt)} / {(weight % of polyvinylidone) / (molecular weight of vinylidone unit)}*100 For example, if the contents of polyvinylpyrrolidone and alkali metal salt (LiOH) are 0.6 wt% and 0.01 wt%, respectively, based on the total weight of the dispersion, the molecular weight of the alkali metal salt (LiOH) is 24 g / mol, and the molecular weight of the vinylidone unit is 111.14 g / mol, the molar ratio of the alkali metal salt is calculated to be 7.7 mol based on 100 mol of vinylpyrrolidone units [7.7 = {(0.01) / (24)} / {(0.6) / (111.14)}*100].

[0025] The vinylpyrrolidone unit means a unit consisting of a 5-membered lactam linked to a vinyl group, and refers to a unit constituting the polyvinylpyrrolidone resin. Specifically, it may be a unit represented by the following Chemical Formula 2 among polyvinylpyrrolidone represented by the following Chemical Formula 1:

[0026] [ka]

[0027] [ka]

[0028] In an embodiment of the present invention, the carbon nanotube dispersion may further include a solvent, which is used to linearly disperse the carbon nanotubes and supply them as the carbon nanotube dispersion to prevent aggregation when the carbon nanotubes are directly mixed with an electrode active material and used as an electrode slurry composition. In one embodiment of the present invention, the solvent may be an aqueous solvent. For example, the aqueous solvent may be water. In this case, there is an advantage that the viscosity of the dispersion can be easily adjusted.

[0029] In one embodiment of the present invention, the pH of the carbon nanotube dispersion liquid may be 3 to 10. Preferably, it may be 4 to 9 or 5 to 8. In the above numerical range, the above-mentioned phenomenon of the first dispersant and the second dispersant agglomerating can be further suppressed. Specifically, when the pH of the dispersion liquid is out of the above numerical range, the surface charge strength of the first dispersant and the second dispersant may be too strong or too weak, and the hydrogen bond may be too strong, causing a large aggregation phenomenon. In this case, by adjusting the pH of the dispersion liquid to the above numerical range, the phenomenon of the first dispersant and the second dispersant agglomerating can be further suppressed. The pH can be measured at 25°C.

[0030] In one embodiment of the present invention, the value represented by the following formula 1 of the carbon nanotube dispersion may be 2 to 10. Preferably, it may be 2 to 6.5 or 3 to 6. The value represented by the following formula 1 is the shear fluidization index of the dispersion, and means the ratio of the viscosities measured at different shear rates. When the above range is satisfied, it is possible to prevent the viscosity from becoming too high in a stationary state, which would cause a decrease in fluidity, thereby enabling uniform mixing during electrode production. In addition, it is possible to prevent sedimentation of carbon nanotube particles, thereby improving storage stability.

[0031] [Formula 1] Shear Thinning index (STI)=V low / V high In formula 1, V low is 25℃ and 15sec -1 is the viscosity of the dispersion measured at a shear rate of V high is 25℃ and 150sec -1 is the viscosity of the dispersion measured at a shear rate of In one embodiment of the present invention, the value calculated from the following formula 2 of the carbon nanotube dispersion may be 1 to 5. Preferably, it may be 1 to 3 or 1.1 to 2. The value calculated from the following formula 2 indicates the relationship between the shear thinning index (STI) characteristic of the above-mentioned dispersion and the average particle size of the carbon nanotubes contained in the dispersion.

[0032] In general, when the particle size (D50) of the carbon nanotubes is too small, the carbon nanotubes tend to aggregate with each other, increasing the shear thinning index (STI) of the dispersion. Also, when the particle size (D50) of the carbon nanotubes is too large, the carbon nanotubes tend to be insufficiently dispersed and form a network structure, increasing the overall viscosity and shear thinning index (STI) of the dispersion. However, the carbon nanotube dispersion according to one embodiment of the present invention has an effect of improving the viscosity stability over time of the entire dispersion even when the particle size of the carbon nanotubes is small, by adjusting the value calculated by the following formula 2 to the above numerical range.

[0033]

number

[0034] In formula 2, STI is the Shear Thinning Index (STI) of the dispersion, D50 is the average particle size (D50) of the carbon nanotubes.

[0035] One embodiment of the present invention comprises a carbon nanotube and a first dispersant having an amide group; The present invention provides a method for producing the above-mentioned carbon nanotube dispersion liquid, the method including the step of mixing the first dispersant with a second dispersant having an aromatic ring.

[0036] In one embodiment of the present invention, the step of mixing the carbon nanotubes, the first dispersant having an amide group, and the second dispersant having an aromatic ring may be performed under a temperature condition that does not change the physical properties, for example, at a temperature of 50° C. or less, more specifically, at a temperature of 5° C. to 50° C. In an embodiment of the present invention, the method may further include dispersing the carbon nanotubes in a dispersion liquid.

[0037] In one embodiment of the present invention, the step of dispersing the carbon nanotubes in the dispersion liquid may be performed by a method such as a ball mill, a bead mill, a disc mill, a basket mill, or a high pressure homogenizer, and more specifically, may be performed by a milling method using a disc mill or a high pressure homogenizer. In the milling using the disk mill, the size of the beads can be appropriately determined depending on the type and amount of the carbon nanotubes and the type of the dispersant, and specifically, the diameter of the beads can be 0.1 mm to 5 mm, more specifically, 0.5 mm to 4 mm. The bead milling process can be performed at a speed of 2,000 rpm to 10,000 rpm, more specifically, 5,000 rpm to 9,000 rpm.

[0038] Milling using the high-pressure homogenizer is carried out, for example, by pressurizing the mixture with a plunger pump of the high-pressure homogenizer and forcing it through a gap in a homogenizing valve, and by forces such as cavitation, shear, impact, and explosion when passing through the gap.

[0039] The milling by the high-pressure homogenizer can be performed at a speed of 2,000 rpm to 10,000 rpm, and more specifically, it can be performed at a speed of 2,000 rpm to 5,000 rpm.

[0040] The milling by the high-pressure homogenizer can be performed under pressure conditions of 500 bar to 3,000 bar, and more specifically, it can be performed under pressure conditions of 1,000 bar to 2,000 bar. In one embodiment of the present invention, the step of dispersing the carbon nanotubes in a dispersion can be performed for 10 minutes to 120 minutes, and more specifically, for 20 minutes to 90 minutes so that the carbon nanotubes can be sufficiently dispersed.

[0041] One embodiment of the present invention provides an electrode slurry composition containing the above-described carbon nanotube dispersion, an electrode active material, and a binder. In one embodiment of the present invention, the electrode active material includes a silicon-based electrode active material. The silicon-based electrode active material can include one or more selected from the group consisting of metallic silicon (Si), silicon oxide (SiOx, where 0 < x < 2), silicon carbide (SiC), and Si-Y alloy (where Y is an element selected from the group consisting of an alkali metal, an alkaline earth metal, a Group 13 element, a Group 14 element, a transition metal, a rare earth element, and combinations thereof, and is not Si). The element Y can be selected from the group consisting of Mg, Ca, Sr, Ba, Ra, Sc, Y, Ti, Zr, Hf, Rf, V, Nb, Ta, Db, Cr, Mo, W, Sg, Tc, Re, Bh, Fe, Pb, Ru, Os, Hs, Rh, Ir, Pd, Pt, Cu, Ag, Au, Zn, Cd, B, Al, Ga, Sn, In, Ti, Ge, P, As, Sb, Bi, S, Se, Te, Po, and combinations thereof.

[0042] In one embodiment of the present invention, the silicon-based electrode active material exhibits higher capacity characteristics than the carbon-based electrode active material, and therefore, when the silicon-based electrode active material is further included, better capacity characteristics can be obtained. However, since the silicon-based electrode active material has a large volume change during charging and discharging, the battery characteristics are rapidly reduced when charging and discharging are repeated, resulting in insufficient cycle characteristics, which has made commercialization difficult. However, when carbon nanotubes are used as a conductive material as in the present invention, the cycle characteristics can be improved when the silicon-based electrode active material is applied. Therefore, by using the electrode slurry composition of the present invention, which includes the carbon nanotube dispersion liquid of the present invention and the silicon-based electrode active material, a secondary battery with excellent capacity characteristics and cycle characteristics can be realized.

[0043] In one embodiment of the present invention, the electrode active material may further include other types of electrode active materials in addition to the silicon-based electrode active material. Examples of the other types of electrode active materials include carbonaceous materials such as artificial graphite, natural graphite, graphitized carbon fiber, and amorphous carbon; metallic compounds capable of being alloyed with lithium, such as Al, Sn, Pb, Zn, Bi, In, Mg, Ga, Cd, Si alloys, Sn alloys, and Al alloys; metallic oxides capable of doping and dedoping lithium, such as SnO2, vanadium oxide, and lithium vanadium oxide; and composites containing the metallic compounds and carbonaceous materials, such as Sn-C composites, among which carbonaceous materials are particularly preferred.

[0044] In one embodiment of the present invention, the total amount of the electrode active material, including the silicon-based electrode active material and other types of electrode active material, may be 70 to 99 wt%, preferably 80 to 98 wt%, based on the total solid content in the electrode slurry composition. When the content of the electrode active material satisfies the above range, excellent capacity characteristics can be achieved. In one embodiment of the present invention, the binder is for ensuring adhesive strength between active materials or between an active material and a current collector, and may be a general binder used in the art, and is not particularly limited in type. Examples of the binder include polyvinylidene fluoride (PVDF), vinylidene fluoride-hexafluoropropylene copolymer (PVDF-co-HFP), polyvinyl alcohol, polyacrylonitrile, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene polymer (EPDM), sulfonated-EPDM, styrene-butadiene rubber (SBR), fluororubber, or various copolymers thereof, and one or a mixture of two or more of these may be used.

[0045] In one embodiment of the present invention, the binder may be included in an amount of 5 wt% or less, preferably 1 to 3 wt%, based on the total solid content of the electrode slurry composition. When the binder content satisfies the above range, it is possible to achieve excellent electrode adhesion while minimizing the increase in electrode resistance.

[0046] In an embodiment of the present invention, the electrode slurry composition may further include a solvent as necessary for adjusting viscosity, etc. In this case, the solvent may be water, an organic solvent, or a mixture thereof. Examples of the organic solvent include amide polar organic solvents such as dimethylformamide (DMF), diethylformamide, dimethylacetamide (DMAc), and N-methylpyrrolidone (NMP); alcohols such as methanol, ethanol, 1-propanol, 2-propanol (isopropyl alcohol), 1-butanol (n-butanol), 2-methyl-1-propanol (isobutanol), 2-butanol (sec-butanol), 1-methyl-2-propanol (tert-butanol), pentanol, hexanol, heptanol, and octanol; glycols such as ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, 1,3-propanediol, 1,3-butanediol, 1,5-pentanediol, and hexylene glycol; glycerin, trimethylolpropane, pentaerythritol, and sorbitol. glycol ethers such as ethylene glycol monomethyl ether, diethylene glycol monomethyl ether, triethylene glycol monomethyl ether, tetraethylene glycol monomethyl ether, ethylene glycol monoethyl ether, diethylene glycol monoethyl ether, triethylene glycol monoethyl ether, tetraethylene glycol monoethyl ether, ethylene glycol monobutyl ether, diethylene glycol monobutyl ether, triethylene glycol monobutyl ether, or tetraethylene glycol monobutyl ether; ketones such as acetone, methyl ethyl ketone, methyl propyl ketone, or cyclopentanone; esters such as ethyl acetate, γ-butyl lactone, and ε-propiolactone, and any one or a mixture of two or more of these can be used, but are not limited to these. In an embodiment of the present invention, the electrode slurry composition may further include additives such as a viscosity modifier and a filler, if necessary.

[0047] An embodiment of the present invention provides an electrode including an electrode active material layer formed by the above-mentioned electrode slurry composition. Specifically, the electrode can be manufactured by applying the above-mentioned electrode slurry composition of the present invention and drying it to form an electrode active material layer. More specifically, the electrode active material layer can be formed by applying the electrode slurry composition on an electrode collector and drying it, or by applying the electrode slurry composition on a separate support and peeling it off from the support to form a film and laminating it on the entire electrode collector. If necessary, a rolling process can be further performed after forming the electrode active material layer by the above-mentioned method. In this case, the drying and rolling can be performed under appropriate conditions taking into account the physical properties of the electrode to be finally manufactured, and are not particularly limited.

[0048] In one embodiment of the present invention, the electrode current collector is not particularly limited as long as it is a material that has conductivity without inducing a chemical change in the battery. For example, copper, stainless steel, aluminum, nickel, titanium, alloys thereof, those whose surfaces are surface-treated with carbon, nickel, titanium, silver, or the like, or calcined carbon can be used. In one embodiment of the present invention, the electrode current collector may have a thickness of typically 3 μm to 500 μm, and may have fine irregularities formed on the surface of the current collector to enhance the bonding strength of the electrode active material. The electrode current collector may be used in various forms, such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc. In one embodiment of the invention, the electrode may be a cathode. One embodiment of the present invention provides a lithium secondary battery including the electrode described above.

[0049] One embodiment of the present invention provides a lithium secondary battery comprising: a positive electrode; a negative electrode; and a separator and an electrolyte disposed between the positive electrode and the negative electrode, wherein at least one of the positive electrode and the negative electrode is the above-mentioned electrode. In one embodiment of the present invention, the separator separates the negative electrode and the positive electrode and provides a passage for lithium ions to move. Any separator that is generally used as a separator in a secondary battery may be used without any particular limitation. Specifically, the separator may be a porous polymer film, for example, a porous polymer film made of a polyolefin-based polymer such as an ethylene homopolymer, a propylene homopolymer, an ethylene / butene copolymer, an ethylene / hexene copolymer, or an ethylene / methacrylate copolymer, or a laminate structure of two or more layers thereof. In addition, a conventional porous nonwoven fabric, for example, a nonwoven fabric made of high-melting glass fiber, polyethylene terephthalate fiber, or the like, may be used. In addition, a coated separator containing a ceramic component or a polymeric material may be used to ensure heat resistance or mechanical strength, and may be selectively used in a single layer or multilayer structure. In one embodiment of the present invention, the electrolyte may be, but is not limited to, an organic liquid electrolyte, an inorganic liquid electrolyte, a solid polymer electrolyte, a gel-type polymer electrolyte, a solid inorganic electrolyte, or a molten inorganic electrolyte that can be used in the manufacture of a lithium secondary battery.

[0050] "Example" The present invention will now be described in further detail with reference to examples. <Physical property measurement method> The physical properties of the dispersions in the examples and comparative examples were measured by the following methods. Viscosity measurement Using Brookfield's DVNextCP Rheometer, the shear rate was set at 25°C and 15 sec -1 and 150sec -1 The measurements were performed after changing the setting to each of the following. Measurement of average particle size The laser diffraction method was used, and a commercially available laser diffraction particle size analyzer (Malvern Mastersizer3000) was used. The average particle size at 50% of the particle size distribution (D50) was calculated using the analyzer. Meanwhile, D10 and D90 refer to the particle sizes at 10% and 90% of the particle size distribution, respectively. pH Measurement The measurements were taken using an OHAUS ST3100 pH meter. After calibrating the electrode with a buffer solution at 25°C, the electrode was placed in the sample, stirred for 5 seconds, and then the pH was measured after waiting 30 seconds for the signal to stabilize. Solids Determination The measurement was performed using an OHAUS MB95 moisture analyzer. After placing about 3g of the sample on an aluminum sample plate, the initial weight was measured, and the sample was heated to 150℃ and the weight was measured. If the weight changed by less than 1mg for 60 seconds at 150℃, this was set as the dry weight, and the solid content was calculated using the following formula. %DC (solid content) = dry weight / starting weight x 100% Measurement of Shear Thinning Index (STI) Calculation was made according to the following formula 1.

[0051] [Formula 1] Shear Thinning Index (STI)=V low / V high In equation 1, V low is 25℃ and 15sec -1 is the viscosity of the dispersion measured at a shear rate of V high is 25℃ and 150sec -1 The viscosity of the dispersion is measured at a shear rate of 100 μm. Calculating the value calculated by Equation 2 The physical property values ​​represented by the following formula 2 were calculated. In this case, STI is the shear thinning index (STI) of the dispersion, and D50 is the average particle size (D50) of the carbon nanotubes.

[0052]

number

[0053] <Production of Dispersion> Example 1 1 kg of carbon nanotube dispersion was produced by mixing 0.4 wt% single-walled carbon nanotubes (TUBALL 01RW03, manufactured by OCSiAl), 0.45 wt% polyvinylpyrrolidone (K15, manufactured by Sigma-Aldrich) as a first dispersant, 0.15 wt% tannic acid (manufactured by Aldrich) as a second dispersant, and water as a solvent. At this time, the molar ratio of the alkali metal salt was 7.7 mol [={(0.0075) / (24)} / {(0.45) / (111.14)}*100] based on 100 mol of vinylpyrrolidone units according to the following formula 3.

[0054] [Formula 3] Molar ratio of alkali metal salt={(weight % of alkali metal salt) / (molecular weight of alkali metal salt)} / {(weight % of polyvinylidone) / (molecular weight of vinylidone unit)}*100 Examples and Comparative Examples For the remaining Examples and Comparative Examples, dispersions were prepared by changing the weight and type of each material as shown in Tables 1 and 2 below, and the physical properties were tested.

[0055] [Table 1]

[0056] [Table 2]

[0057] In Tables 1 and 2, K12, K15 and K17 are manufactured by Aldrich. From the above results, the dispersion liquid of the embodiment is -1 It was confirmed that the viscosity at the shear rate was 2,000 cPs or less. From the above results, when the dispersion liquid did not contain a tannic acid compound (Comparative Example 3), -1It was confirmed that the viscosity at a shear rate of 1000 cPs exceeded 5,000 cPs. If the viscosity characteristics are as described above, the coating properties of the dispersion are significantly reduced, making it difficult to apply the dispersion to processes. In addition, when the dispersion liquid did not contain an alkali metal salt (Comparative Example 1), -1 It was confirmed that the viscosity at a shear rate of 1000 cPs exceeded 2,000 cPs. If the viscosity characteristics are as described above, the coating properties of the dispersion are significantly reduced, making it difficult to apply the dispersion to processes. On the other hand, even when the dispersion liquid contains an excess of alkali metal salt, -1 It was confirmed that the viscosity at the shear rate exceeded 2,000 cPs (Comparative Example 2).

Claims

1. Carbon nanotubes, a first dispersant having an amide group; a second dispersant having an aromatic ring; 25°C and 15sec -1 The carbon nanotube dispersion has a viscosity of 2,000 cPs or less at a shear rate of 1000 s.

2. 2. The carbon nanotube dispersion of claim 1, wherein the first dispersant comprises at least one selected from the group consisting of polyvinylpyrrolidone, polyester amide, polycarboxylic amide, polyamido amine, thioamido amine, and water soluble nylon.

3. The carbon nanotube dispersion liquid according to claim 1 , wherein the second dispersant contains a hydroxyl group or a carboxyl group.

4. 2. The carbon nanotube dispersion according to claim 1, comprising the first dispersant and the second dispersant in a weight ratio of 1:10 to 10:

1.

5. The carbon nanotube dispersion according to claim 1 , wherein the carbon nanotubes are single-walled carbon nanotubes (SWCNTs).

6. 2. The carbon nanotube dispersion according to claim 1, wherein the carbon nanotubes have an average particle size (D50) of 0.1 μm to 20 μm.

7. 2. The carbon nanotube dispersion according to claim 1, wherein the carbon nanotube content is 0.01 wt % to 10 wt % based on the total weight of the carbon nanotube dispersion.

8. The carbon nanotube dispersion liquid according to claim 1 , further comprising an alkali metal element.

9. KOH, NaOH, LiOH, KOHH 2 O, NaOH 2 O, LiOHH 2 O.K. 2 CO 3 , Na 2 CO 3 and LiCO 3 2. The carbon nanotube dispersion liquid according to claim 1, further comprising one or more alkali metal salts selected from the group consisting of:

10. The first dispersant contains a polyvinylpyrrolidone resin, The carbon nanotube dispersion according to claim 9 , wherein a molar ratio of the alkali metal salt is 60 mol or less based on 100 mol of vinylpyrrolidone units contained in the polyvinylpyrrolidone resin.

11. 2. The carbon nanotube dispersion liquid according to claim 1, wherein the value represented by the following formula 1 is 2 to 10. [Formula 1] Shear Thinning Index (STI) = V low / V high (In the formula, V low is 25°C and 15sec -1 is the viscosity of the dispersion measured at a shear rate of V high is 25°C and 150 sec -1 The viscosity of the dispersion is measured at a shear rate of

12. 2. The carbon nanotube dispersion according to claim 1, wherein the value calculated from the following formula 2 is 1 to 5. [0010] (In Equation 2, STI is the shear thinning index (STI) of the dispersion, D50 is the average particle size (D50) of the carbon nanotubes.

13. Carbon nanotubes, a first dispersant having an amide group; The method for producing a carbon nanotube dispersion liquid according to any one of claims 1 to 12, further comprising a step of mixing a first dispersant having an aromatic ring with a second dispersant having an aromatic ring.

14. An electrode slurry composition comprising the carbon nanotube dispersion according to any one of claims 1 to 12, an electrode active material, and a binder.

15. An electrode comprising an electrode active material layer formed by the electrode slurry composition of claim 14.

16. The electrode of claim 15 , wherein the electrode is a negative electrode.

17. A lithium secondary battery comprising the electrode according to claim 16.

Citation Information

Patent Citations

  • Device for polishing the surface of the accessory string

    KR1020110118460A

Cited By

  • Carbon nanotube dispersion and its manufacturing method

    JP2025541265A

  • Carbon nanotube dispersion and method for producing the same

    JP7880017B2