New anode materials for lithium and sodium batteries.

Carbon nanofiber networks address the inefficiencies of graphite anodes by enhancing ion diffusion and conductivity in lithium and sodium batteries, improving charge/discharge rates and capacity.

JP2024540214APending Publication Date: 2024-10-31CARBONX IP 9 BV
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2024525833
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-26
Filing Date
2022-10-25
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing lithium and sodium batteries face challenges such as low coulombic efficiency, poor rate capacity, and slow diffusion rates of ions in graphite anodes, leading to suboptimal charge/discharge rates and energy density, particularly in sodium batteries where sodium ions are larger and harder to accommodate.

Method used

The use of carbon networks comprising carbon nanofibers as active anode materials, which provide high electronic conductivity and porosity, allowing for faster ion diffusion and improved charge/discharge rates through a crystalline structure with interconnected nanofibers.

Benefits of technology

The carbon nanofiber networks enhance the capacity, lifetime, and coulombic efficiency of lithium and sodium batteries, enabling rapid charging and discharging times, with the potential to replace graphite as the primary anode material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024540214000010
    Figure 2024540214000010
  • Figure 2024540214000011
    Figure 2024540214000011
  • Figure 2024540214000012
    Figure 2024540214000012
Patent Text Reader

Abstract

The present invention resides in the use of a porous, chemically interconnected carbon network with carbon nanofibers as an electrochemically active material in the anode of a lithium or sodium battery. It has been found that the carbon network with carbon nanofibers can be beneficially used in the anode of a lithium or sodium battery when added in an amount of 10-100% by weight. The benefits include high capacity, high lifetime (stability over long periods of cycling), high charge and discharge rates, and resilience during manufacture and use. The porous, chemically interconnected carbon network with carbon nanofibers can be used in the anode of lithium or sodium batteries in many technological areas, for example in smartphones, laptops, and electric and hybrid vehicles.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention is in the field of lithium and sodium batteries. In particular, the present invention relates to improved anodes in rechargeable lithium and sodium batteries. The present invention preferably relates to sodium-ion and lithium-ion batteries, most preferably lithium-ion batteries. [Background technology]

[0002] There are various types of batteries available, but today lithium is the first choice for the negative electrode material. The reason is the specific capacity of lithium, which is much higher than that of zinc and lead, for example. Lithium is the lightest and most electropositive metal with high energy and power density. The demand for lithium batteries or "lithium secondary batteries" continues to increase, especially as a power source for portable electronic devices, such as smartphones or laptops (including their liquid crystal displays (LCD) or organic light emitting diodes (OLED)), energy storage for power generation equipment (i.e., from surplus wind and solar renewable energy), uninterruptible power supplies (UPS), and a power source for driving the motors of electric and hybrid vehicles.

[0003] Lithium batteries are the most widely used power batteries, but the production of lithium batteries faces great challenges, such as increasing scarcity of lithium resources, rising prices of upstream materials, and low recycling rates. To overcome these challenges of lithium batteries, sodium batteries, which utilize the intercalation process of sodium ions between the positive and negative electrodes, have become a solid alternative choice. The advantages of sodium batteries are that the reserves of sodium resources are much more abundant than those of lithium, their distribution is more widespread, and the cost of sodium is much lower than that of lithium, and for these reasons, sodium batteries have the potential to replace lithium batteries as long as challenges such as low coulombic efficiency and poor rate capacity are overcome or reduced to a satisfactory equilibrium point.

[0004] Lithium and sodium batteries are typically composed of four main components: a cathode, an anode, a separator, and an electrolyte. The electrolyte serves as a conductive medium through which lithium ions can be transported to and from the electrodes. The electrolyte may be either solid-state or liquid. In the context of this invention, "lithium battery" or "sodium battery" includes both solid-state (with solid electrolyte) and liquid-state (with liquid electrolyte) batteries. In the context of this invention, the terms "lithium ion battery" and "sodium ion battery" are reserved for battery technologies with liquid electrolytes.

[0005] The cathode of a lithium battery generally comprises a lithium-metal-oxide, such as lithium cobalt oxide (LiCoO2). Materials commonly used as active materials in the anode of a lithium battery are intercalation compounds, alloys, and conversion compounds (transition metal oxides).

[0006] Of the intercalation compounds used in lithium battery anodes, the most common is graphite. Another common compound used in lithium battery anodes is silicon or silicon-based compounds. Generally, silicon materials have a higher specific capacity compared to graphite. Overall, graphite has remained the predominant intercalation anode material in commercial lithium batteries to date, as it is safe to perform and offers low working potential, low cost, and good cycle life, along with sufficient energy density for many portable power applications. However, batteries using graphite anodes usually suffer from the relatively slow diffusion rate of lithium ions into carbon materials (10 -12 cm 2 / s to 10 -6 cm 2 / s), this characteristic, combined with the suboptimal electronic conductivity, makes the charge / discharge rates of graphite alone suboptimal, thus resulting in long charge and discharge times for the battery.

[0007] To improve the charge / discharge rate of the battery, conductive additives are traditionally added to the anode active material to improve the electronic conductivity of the anode (Roselin et al., "Recent Advances and Perspectives of Carbon-Based Nanostructures as Anode Materials for Li-ion Batteries", Materials 2019, 12, 1229). These additives build a conductive interpenetrating network to increase and maintain the electrical conductivity of the electrode, allowing for faster charging and discharging. In addition, the conductive additives absorb and hold the electrolyte, providing intimate contact between the lithium or sodium ions and the active material. Conductive additives for lithium and sodium batteries are generally carbon nanomaterials selected from conductive carbon black, Super P, acetylene black, carbon nanofibers and carbon nanotubes, all of which exhibit low weight, high chemical inertia and high specific surface area (Zhang Q et al., "Carbon nanomaterials used as conductive additives in lithium ion batteries", Recent Pat Nanotechnol., 2010 Jun;4(2):100-10).

[0008] Conductive carbon black has been used as a conductive additive to electrochemically active materials in anodes or cathodes to improve electronic conductivity and thus improve the charge and discharge rates of the battery. However, in a few cases, carbon black has been tested as an active material in anodes. For example, WO1998 / 038685 discloses thermal carbon black with an average particle size larger than 100 nm, in particular a rechargeable battery using an anode comprising 85-95% thermal carbon black, about 0-10% conductive black and about 5% binder. Nevertheless, thermal carbon black exhibits low crystallinity resulting in low electrical conductivity, high brittleness and a wide particle size distribution of spherical particles resulting in non-uniform properties between batches. Therefore, thermal carbon black is not suitable for manufacturing or daily use due to its physical stability in lithium or sodium batteries. Therefore, carbon black has not found any commercial application in lithium or sodium batteries other than in the form of a conductive additive.

[0009] US2021 / 184206 and KR101162588 disclose carbon nanotubes as additives in anode materials, however, the specific capacity and charge and discharge rates were found to be still relatively low.

[0010] Sodium batteries pose their own challenges. For example, sodium ions (1.02 Å) are 55% larger than lithium ions (0.69 Å), making it more difficult to reversibly accommodate sodium ions in the anode. In fact, graphite materials commercially used as anodes in lithium batteries have not been able to achieve acceptable performance in sodium batteries, as the graphite anodes used to date in sodium batteries absorb too little sodium, making the sodium battery less powerful due to the inevitable reduction in energy storage density caused by low cell voltage. To overcome the limitations of graphite as an anode material, alternative anode materials, such as red phosphorus (P), have been used. However, (1) native red P has a very low electrical conductivity (approximately 10 -14 Scm -1 );(2) The large volume expansion during sodiation / desodiumation can result in significant capacity fade (Wang et al., "Influence of Conductive additives on the stability of red phosphorus-carbon anodes for sodium-ion batteries", Scientific Reports 2019.9:946). Therefore, there is also a need to find alternative anode materials in sodium batteries.

[0011] For both sodium and lithium batteries, there remains a need in the art to find alternative anode materials with high capacity and high lithium or sodium ion diffusion rates that can help improve the energy and power density of the cells. More specifically, the properties of the active materials in the anode need to be further developed to obtain lithium or sodium batteries with high capacity and long life with fast charge / discharge rates and physical properties that allow safe manufacture and use. Summary of the Invention

[0012] The inventors have discovered that carbon networks comprising carbon nanofibers may be beneficially used as active anode materials in place of currently used active anode materials in lithium or sodium batteries to the extent that they achieve all of the above goals in the art, particularly high dosage, long life (stability over extended cycling), and high charge and discharge rates, while possessing physical properties that allow for safe manufacture and use.

[0013] Advantageously, the inventors have found that an anode comprising a carbon network comprising carbon nanofibers according to the invention, as an active anode material, can contribute to the capacity of a lithium or sodium battery through differential intercalation of lithium or sodium ions. The lifetime (stability over long-term cycling) can be improved by improving the electronic conductivity; see Table 4 herein. Due to the high electronic conductivity of the carbon network comprising carbon nanofibers according to the invention (e.g., compared to that of graphite), the reversibility of the charge / discharge process is enhanced when using the carbon network comprising carbon nanofibers according to the invention as an anode material. Importantly, the inventors have also found that the charge and discharge rate can be improved by the carbon network comprising carbon nanofibers according to the invention; see Figures 5, 7 and 8 herein. The inventors have also found that the coulombic efficiency is improved by the carbon network comprising carbon nanofibers according to the invention; see Figure 9 herein.

[0014] Without wishing to be bound by any theory, the inventors believe that these advantageous properties can be attributed to the inherent electronic conductivity and open pore structure of the network due to the crystallinity, accessible porosity, filament length to diameter ratio, and d-spacing that facilitate the diffusion of lithium or sodium ions. Furthermore, the graphite crystallites in the carbon network comprising the carbon nanofibers of the present invention are arranged into nano-sized filaments, which greatly reduces the diffusion path length of the lithium or sodium ions during intercalation, since the lithium or sodium ions have to travel a shorter distance from the exterior to the center of the carbon material. Collectively, these improved properties result in improved conductivity routes.

[0015] The mechanism hypothesized by the authors to explain this advantageous effect is that, while other anode materials, such as graphite, exhibit particle dimensions in the μm range, the carbon network comprising carbon nanofibers according to the invention represents a micron-sized nanostructured material with highly conductive filaments of 50 nm thickness, which facilitate the transport of electrons and the intercalation of lithium or sodium ions, thus reducing the diffusion times.

[0016] In addition, the inventors have found that the use of carbon networks comprising carbon nanofibers according to the invention as anode materials in batteries exhibits higher capacity and longer life values ​​compared to common active anode materials, such as graphite. This allows for higher charge / discharge rates and therefore reduced charging times for batteries. In particular, it allows the manufacture of batteries that are charged in minutes (e.g., 6 minutes) instead of hours.

[0017] In a preferred embodiment, these porous carbon networks form intraparticle porous networks, where the carbon nanofibers are interconnected by chemical bonds through connectors with other carbon nanofibers in the network, where the pores in the network have an intraparticle pore diameter size of 5-150 nm using mercury intrusion porosimetry according to ASTM D4404-10, where the carbon nanofibers have an average aspect ratio of fiber length to thickness of at least 2, and preferably have a d-spacing of 0.340-0.5 nm, more preferably 0.35-0.45 nm, and even more preferably 0.355-0.375 nm. Importantly, this d-spacing is larger than that of other anode active materials, such as graphite (0.335 nm), facilitating the intercalation of lithium or sodium ions. This large d-spacing is particularly beneficial for the intercalation of sodium ions in sodium batteries due to the large volume of sodium ions.

[0018] The present invention therefore resides in the use of carbon networks comprising carbon nanofibers as active components in the anodes of lithium or sodium batteries, anodes comprising carbon networks comprising these carbon nanofibers, and lithium or sodium batteries comprising these anodes. The present invention also relates in the broadest sense to solid-state lithium and sodium batteries, the present invention preferably relates to lithium-ion and sodium-ion batteries, more preferably to lithium-ion batteries. [Brief description of the drawings]

[0019] [Figure 1A]Schematic diagram of a continuous furnace carbon black production process according to the present invention, containing along the axis of a reactor 3 a combustion zone 3 a, a reaction zone 3 b and a termination zone 3 c, by burning a fuel a in an oxygen-containing gas b and generating a flow of hot waste gas a1 in the combustion zone by passing the waste gas a1 from the combustion zone 3 a to the reaction zone 3 b, spraying (atomizing) a single-phase emulsion c in the reaction zone 3 b containing the hot waste gas, carbonizing said emulsion at high temperature and quenching or stopping the reaction in the termination zone 3 c by spraying water d, in order to obtain a crystalline carbon network e according to the present invention. [Figure 1B] Schematic diagram of a semi-batch carbon black production process in which a single-phase emulsion c is sprayed through nozzle 4 at the top of reactor 3 into hot reaction zone 3b, the hot emulsion is carbonized in reaction zone 3b, and the crystalline carbon network e is collected at the bottom of the reactor. In addition, there are two gas inlets entering the reactor from the top for adding an inert gas f, preferably nitrogen, for oxygen level control and / or exhaustion, and for introducing a carbon-containing gas g, preferably acetylene or ethylene, into the reactor. [Diagram 2] Schematic side view of a lithium or sodium battery according to the invention, exemplified herein as a lithium or sodium ion battery, including an anode 5 comprising a carbon network comprising carbon nanofibers according to an embodiment of the invention. The lithium or sodium ion battery also comprises a cathode 6, a separator 7 between the anode and the cathode, and an electrolyte 8. Release of electrons from the anode to the cathode (oxidation) and release of lithium or sodium ions occurs during a discharge cycle. [Diagram 3] 2 is a graph showing the specific capacity of a lithium ion battery anode comprising a carbon network comprising carbon nanofibers according to the present invention. [Figure 4] Graph showing Nyquist plots for synthetic graphite, Grade A and Grade B. [Diagram 5]1 is a graph showing the cycling capability at various C-rates of a lithium ion battery anode comprising a carbon network comprising carbon nanofibers according to the present invention, capacity versus cycles, and a series of cycles at different C-rates. [Figure 6] 2 is a graph showing the specific capacity of a lithium ion battery anode comprising a carbon network comprising carbon nanofibers according to the present invention. [Figure 7] 1 is a graph showing the cycling capability at various C-rates of a lithium ion battery anode comprising a carbon network comprising carbon nanofibers according to the present invention, capacity versus cycles, and a series of cycles at different C-rates. [Figure 8] Graph showing capacity retention over cycling with increasing C-rate as shown in rate capacity testing. [Figure 9A] Graph showing the coulombic efficiency as discharge and corresponding charge at different cycle numbers, Figure 9A corresponds to grade C. For half cells, the coulombic efficiency % is calculated as: (charge / discharge) x 100. [Figure 9B] Graph showing the coulombic efficiency as discharge and corresponding charge at different cycle numbers, Figure 9B corresponds to grade D. For half cells, the coulombic efficiency % is calculated as: (charge / discharge) x 100. [Figure 9C] Graph showing the coulombic efficiency as discharge and corresponding charge at different cycle numbers. Figure 9C corresponds to synthetic graphite (AG). For half cells, the coulombic efficiency % is calculated as: (charge / discharge) x 100. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] 1. Use of a porous, chemically interconnected carbon network comprising carbon nanofibers as the electrochemically active material in the anode of a rechargeable lithium or sodium battery.

[0021] 2. Use according to embodiment 1, in which the carbon network comprising carbon nanofibers represents 10 to 100% by weight, preferably more than 10% by weight and less than 100% by weight, of the total mass of the anode.

[0022] 3. The use according to aspect 1 or 2, wherein the carbon network comprises crystalline carbon nanofibers.

[0023] 4. The use according to any one of the preceding aspects, wherein the carbon nanofibers have an average fiber length of 30 to 10,000 nm.

[0024] 5. The use of any one of the preceding aspects, wherein the porous carbon network forms an intraparticle porous network, wherein the carbon nanofibers are interconnected by chemical bonds through connectors with other carbon nanofibers in the network, wherein the pores in the network have an intraparticle pore diameter size of 5-150 nm using mercury intrusion porosimetry according to ASTM D4404-10, and wherein the carbon nanofibers have an average aspect ratio of fiber length to thickness of at least 2, preferably with a d-spacing in the range of 0.340-0.5 nm.

[0025] 6. The use of any one of the preceding aspects, wherein the lithium or sodium battery is suitable for and is included in smartphones, laptops, digital cameras and camcorders, as uninterruptible power supplies (UPS), as energy storage in power generation equipment, in medical and communication systems, and in electric and / or hybrid vehicles.

[0026] 7. A lithium or sodium battery anode comprising a porous, chemically interconnected carbon network comprising carbon nanofibers as the electrochemically active material.

[0027] 8. A lithium or sodium battery anode comprising a porous, chemically interconnected carbon network comprising carbon nanofibers, representing 10-100% by weight, preferably more than 10% by weight and less than 100% by weight, of the total mass of the anode.

[0028] 9. The lithium or sodium battery anode of embodiment 7 or 8, wherein the porous carbon network forms an intraparticle porous network, wherein the carbon nanofibers are interconnected by chemical bonds with other carbon nanofibers in the network via connectors, and wherein the pores in the network have an intraparticle pore diameter size of 5 to 150 nm using mercury intrusion porosimetry according to ASTM D4404-10, and the carbon nanofibers have an average aspect ratio of fiber length to thickness of at least 2, and preferably have a d-spacing of 0.340 to 0.5 nm.

[0029] 10. A rechargeable lithium or sodium battery comprising an anode according to any one of aspects 7 to 9.

[0030] 11. The lithium or sodium battery of embodiment 10, wherein the battery is suitable for inclusion in smartphones, laptops, digital cameras and camcorders, as uninterruptible power supplies (UPS), as energy storage in power generation equipment, in medical and communication systems, and in electric and / or hybrid vehicles.

[0031] 12. Use according to any one of aspects 1 to 6, a lithium or sodium battery anode according to any one of aspects 7 to 9, or a lithium or sodium battery according to aspect 10 or 11, wherein the carbon network is obtained by a process for producing a crystalline carbon network by injecting a water-in-oil, oil-in-water or bicontinuous microemulsion c comprising metal catalyst nanoparticles into a reactor 3 containing a reaction zone 3b and a termination zone 3c at a temperature above 600° C., preferably above 700° C., more preferably above 900° C., even more preferably above 1000° C., more preferably above 1100° C., preferably at most 3000° C., more preferably at most 2500° C., most preferably at most 2000° C., to produce a crystalline carbon network e, transporting these networks e to a termination zone 3c, and quenching or stopping the formation of the crystalline carbon network in the termination zone by spraying into water d.

[0032] 13. A battery-powered device comprising a lithium or sodium battery anode according to any one of aspects 7-9, or a lithium or sodium battery according to aspect 10 or 11.

[0033] 14. The device of aspect 13, which is a smartphone, a laptop, an energy storage device for a power generation device, or an electric or hybrid vehicle.

[0034] 15. A lithium or sodium battery anode comprising, as electrochemically active material, a porous, chemically interconnected carbon network comprising carbon nanofibers, representing 10 to 100% by weight, preferably more than 10% by weight and less than 100% by weight, of the total mass of the anode.

[0035] 16. The battery anode of embodiment 8 or 9, wherein the battery is a lithium battery, and wherein the anode contains 0.1 to 90 wt. % of an additional active material, and wherein the additional active material is graphite, silicon, a silicon-based compound (SiO2), or a combination thereof.

[0036] 17. The battery anode of embodiment 16, wherein the additional active material is silicon, a silicon-based compound (SiO2), or a combination thereof, and wherein the silicon, a silicon-based compound (SiO2), or a combination thereof is mixed with a carbon network comprising carbon nanofibers in the anode, or the carbon network comprising carbon nanofibers is coated with the silicon, a silicon-based compound (SiO2), or a combination thereof.

[0037] The following is copied from Roselin (Roselin et al., "Recent Advances and Perspectives of Carbon-Based Nanostructures as Anode Materials for Li-ion Batteries", Materials 2019, 12, 1229), the contents of which are incorporated herein by reference, describing the operating principles of batteries as exemplified by lithium-ion (Li-ion) batteries.

[0038] A battery is a device that changes chemical energy into electrical energy through electrochemical oxidation-reduction reactions (redox reactions). The essential electrochemical unit that accomplishes such energy change is known as a "cell." A battery contains a group of interconnected cells. The number of cells utilized depends on the capacity and voltage desired for a particular application. A small number of electrochemical cells are linked in parallel in an array to obtain a lithium-ion battery of the indicated voltage and capacity. Each cell contains the following parts: a negative terminal (anode) where electrochemical oxidation occurs during discharge; a positive terminal (cathode) where electrochemical reduction occurs; an electrolyte that facilitates the transport of ions from one electrode to another; a separator that provides electronic isolation between the electrodes; and a casing that contains the other cell parts. Lithium-ion cells use a solid reductant as the anode and a solid oxidant as the cathode.

[0039] The cathode materials used in the majority of commercial Li-ion batteries are LiCoO2 or LiNiO2, and the anode materials are carbonaceous. During charging of the cell, the cathode material releases Li ions into the electrolyte, and electrons are extracted from the cathode by applying an external field and then transferred to the anode. Charge-compensating Li ions are attracted by the negative electrode and then inserted into the negative electrode. During discharging of the cell, the reverse reaction occurs: the anode provides the intercalated Li ions to the electrolyte and provides electrons to the external circuit. At the cathode, Li ions intercalate from the electrolyte and provide charge from the external circuit. Common carbon anode materials are graphite or coke types, or a combination of both, and common cathode materials include LiMn2O4, LiCoO2, and LiNiO2. The electrolyte can be either solid or liquid. Liquid electrolytes are usually non-aqueous solutions of Li salts and various solvents, including ethers, esters, and carbonates. The cell reactions occurring at the cathode and anode during charging and discharging of the cell are represented as follows (Equations (1)-(4)): Charging At the cathode: LiMO2 → Li 1-x MO2+xLi + +xe - (1) At the anode: xLi + +xe - +C→Li x C (2) Discharging At the cathode: Li 1-x MO2+xLi + +xe - →LiMO2(3) At the anode: Li x C → xLi + +xe - +C (4) When the electrodes are connected to an external load, electrons flow through an external circuit and ions move through the electrolyte. The flow of charge results from electrochemical (i.e. redox) reactions at the electrodes, involving chemical species and electrons, that occur at various voltages. The output voltage of the battery is given by the voltage difference between the two redox reactions. In primary batteries, the redox reactions cannot be reversed and are meant to be discharged once, whereas in secondary (i.e. rechargeable) batteries, the redox reactions are reversible, resulting in multiple charge and discharge cycles. The above examples of electrochemical reactions of lithium-ion batteries may be extended, mutatis mutandis, to other types of lithium or sodium batteries.

[0040] The present invention relates to secondary or rechargeable batteries, and in particular to providing a carbon source (at the anode) in the redox reaction (2) above. In the context of the present invention, "lithium battery" or "sodium battery" includes both solid-state (with solid electrolyte) and liquid-state (with liquid electrolyte) batteries. In the context of the present invention, the terms "lithium ion battery" and "sodium ion battery" are reserved for battery technologies with liquid electrolytes.

[0041] In a first aspect, the present invention can be described as the use of a porous, chemically interconnected carbon network comprising carbon nanofibers (i.e. a porous carbon network comprising chemically interconnected carbon nanofibers) as an active material in the anode of a lithium or sodium battery. In this context, "active material in the anode" should be understood as a material in the anode that spontaneously participates in the electrochemical charge and / or discharge reactions and provides a carbon-based material for Li-ion intercalation / deintercalation during charge and discharge, respectively.

[0042] In this regard, the present invention resides in an anode for a lithium or sodium battery comprising a porous, chemically interconnected carbon network comprising carbon nanofibers (i.e. a porous carbon network comprising chemically interconnected carbon nanofibers). In a preferred embodiment, the anode consists essentially of the network according to the present invention, preferably at least 80% by weight, more preferably at least 90% by weight, and most preferably 95-100% by weight of the anode.

[0043] The use of these networks as the sole anode active material is particularly advantageous, but even partial replacement of the anode active material leads to improved properties. Therefore, the present invention also pertains to an anode for a lithium or sodium battery comprising a porous, chemically interconnected carbon network comprising carbon nanofibers in an amount of 10-100% by weight of the anode, preferably more than 10% by weight and less than 100% by weight, more preferably 40-95% by weight and even more preferably 50-90% by weight, the remainder being preferably an additional anode material capable of intercalating and releasing lithium or sodium ions. Preferably, the anode according to the present invention may contain 0.1-90% by weight, preferably 0.1-30% by weight and most preferably 0.1-10% by weight of additional active material. In the case of a lithium battery, the additional active material in the anode is preferably an intercalation compound, such as graphite, an alloy, such as tin, a silicon-based alloy, and / or a conversion compound, such as a transition metal oxide (MO, where M is Sn, Mo, Ga, Zn, Si, Ge, Co, Ni, Cu, or Fe). In a preferred embodiment, the additional active material in the anode of the lithium battery is graphite. In the case of a lithium battery, the additional active material in the anode is preferably an intercalation compound, such as graphite, an alloy, such as tin, a silicon-based alloy, a silicon or silicon-based compound, such as SiO2, and / or a conversion compound, such as a transition metal oxide (MO, where M is Sn, Mo, Ga, Zn, Si, Ge, Co, Ni, Cu, or Fe). In a preferred embodiment, the additional active material in the anode of the lithium battery is graphite, silicon, a silicon-based compound (SiO2), or a combination thereof. In another preferred embodiment, the additional active material in the anode of the lithium battery is silicon, a silicon-based compound (SiO2), or a combination thereof. Most preferably, the additional active material is silicon or graphite.When the additional active material in the anode is silicon, a silicon-based compound (SiO2), or a combination thereof, the silicon, the silicon-based compound (SiO2), or a combination thereof is mixed with the carbon network comprising the carbon nanofibers of the present invention in the anode, or the carbon network comprising the carbon nanofibers of the present invention is coated with the silicon, the silicon-based compound (SiO2), or a combination thereof. For sodium batteries, preferably, the additional active material in the anode is an oxide for intercalation type anode, such as TiO2, an oxide for conversion type anode, such as Fe2O3, or an oxide for conversion alloying type anode, such as Sn. x O2 and Sb2O3, or "hard carbon", are disordered carbon materials consisting of non-graphitizable, non-crystalline and amorphous carbon structures.

[0044] Synthetic graphite, commonly used as an active material in battery anodes, exhibits a particle size distribution D50 of 19.0-23.0 μm, in contrast to the carbon network of the present invention, which exhibits a filament diameter size distribution D50 of 70-250 nm, and the inventors hypothesize that the smaller filament diameter size distribution (μm vs. nm scale) of the carbon network of the present invention compared to that of graphite, along with the higher conductivity, reduces the diffusion time of the intercalated ions when compared to the graphite anode. In addition, synthetic graphite typically has a particle size distribution D50 of 4.2 nm. 2 / g, whereas the specific surface area of ​​the carbon network of the present invention is preferably between 40 and 200 m 2 / g, which results in a shorter diffusion length for these ions due to their intercalation capacity and affinity for the more exposed vacancies at the surface. The smaller crystallite size and open pore structure therefore provide improved diffusion, resulting in increased charge and / or discharge rates.

[0045] Among the advantageous effects of the use of the carbon network according to the invention in lithium or sodium batteries, the anode is more electrically conductive, based on EIS data. In addition, the carbon network passes higher levels of Fe and / or other metals without problems, which increases the industrial application and safety of the anode. The carbon network according to the invention also has a large distance of intermediate layers, which allows the viscosity to remain reduced even when used in large amounts in the anode. In fact, the carbon network according to the invention can be added in increased amounts without adversely affecting the viscosity.

[0046] The present invention also relates to a secondary or rechargeable lithium or sodium battery comprising the lithium or sodium anode described above, respectively. Preferably, the secondary or rechargeable battery is a secondary or rechargeable lithium-ion or sodium-ion battery, most preferably a lithium-ion battery. In addition to the aforementioned lithium or sodium anode, the lithium or sodium battery also comprises a cathode, an electrolyte, and preferably a separator between the anode and the cathode.

[0047] For lithium batteries, the active material in the cathode is preferably lithium or sodium metal, alkali metal, and / or lithium or sodium metal oxide. In a preferred embodiment, for lithium cathodes, the active material is LiCoO2 or LiMn2O4. In another preferred embodiment, the active material in the cathode is lithium iron phosphate (LiFePO4). For sodium batteries, the active material in the cathode is preferably O3-type layered metal oxide, such as NaFeO2, P2-type layered metal oxide, such as Na 0.6 MnO2, two-phase layered metal oxides, e.g. Na 0.78 Ni 0.2 Fe 0.38 Mn 0.42O2, or an oxide with anionic redox capability. Preferably, the active material in the cathode of a sodium battery is sodium oxide (NaMO2, M=V, Fe, Mn, Cu, Co, and Ni), sodium phosphate (Na7V3(P2O7)4, NaFePO4, transition metal oxides (VO5), or Prussian Blue (PB, Na2M[Fe(CN)6]).

[0048] The electrolyte of a lithium or sodium battery may be liquid or solid state. The liquid electrolyte may comprise an organic solvent and a salt of an alkali metal, preferably a lithium or sodium salt for lithium-ion and sodium-ion batteries, respectively. The liquid electrolyte of a lithium battery may comprise an organic solvent and a salt of an alkali metal, preferably a lithium salt. The liquid electrolyte of a sodium battery may comprise an organic solvent and a sodium salt. For example, the organic solvent may be one or more of ethylene carbonate (EC), propylene carbonate (PC), ethyl methyl carbonate (EMC) and diethyl carbonate (DEC), and the sodium salt may be NaPF6, NaClO4, NaBCl4, NaSO3CF3 and Na(CH3)C6H4SO3. The electrolyte of a lithium or sodium battery may also be solid state and may comprise an inorganic ceramic / glass ceramic, an organic polymer and / or a ceramic-polymer composite electrolyte. Preferably, the electrolyte is a liquid electrolyte.

[0049] The lithium or sodium battery separator may comprise one or more of glass fiber, non-woven fabric, polyethylene, polypropylene and polyvinylidene fluoride. Preferably, the lithium or sodium battery separator is polypropylene.

[0050] The anode for lithium or sodium battery according to the invention may comprise conventional additives (non-active materials) together with the porous and chemically interconnected carbon network comprising carbon nanofibers to further improve the electrochemical performance of the lithium or sodium battery according to the invention. In particular, these additives may be added to build a conductive permeating network to increase and maintain the electrical conductivity of the electrode, allowing faster charging and discharging, as well as to absorb and retain electrolyte, allowing intimate contact between the lithium or sodium ions and the active materials. It is considered within the purview of the skilled artisan to select suitable conductive additives available in the art. In a preferred embodiment, the anode according to the invention may comprise 0.1-10 wt%, preferably 0.1-5.0 wt%, most preferably 0.1-3.0 wt% of one or more conductive additives selected from superconducting carbon, conductive carbon black, Ketjen black, carbon dots, Super P, acetylene black, carbon nanofibers, graphene and carbon nanotubes, all of which exhibit excellent properties, such as low weight, high chemical inertia and high specific surface area. In a preferred embodiment, the conductive additive is carbon black.

[0051] Binder materials are responsible for maintaining a strong connection between the electrode and the contacts as well as for holding the active material particles in the electrolyte of a lithium or sodium battery. These binding materials are mostly inert and have an important role in the manufacturability of the battery. The anode for a lithium or sodium battery according to the present invention may comprise 0.1-10% by weight, preferably 2-8% by weight, most preferably 4-6% by weight of a binder, such as styrene butadiene rubber (SBR), water-based acrylic resin (water-based acrylic resin), carboxymethyl cellulose (CMC), polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), ethylene-vinyl acetate copolymer (EVA) and polyvinyl alcohol (PVA). Preferably, the binder is selected from SBR-based and PVDF-based binders. Most preferably, the binder is PVDF-based.

[0052] The anode for lithium or sodium battery or lithium or sodium battery of the present invention is particularly suitable for use in the manufacture of battery-powered electric devices. Thus, the present invention extends to at least one anode for lithium or sodium battery comprising a porous, chemically interconnected carbon network comprising carbon nanofibers according to the present invention, or at least one lithium or sodium battery, a battery-powered electric device. Here, the battery-powered electric device may be a smartphone, a laptop, a digital camera and a camcorder, as an uninterrupted power supply (UPS), as an energy storage for power generation equipment (i.e. from surplus wind and solar renewable energy), medical and communication systems, and electric and / or hybrid vehicles. Preferably, the anode for lithium or sodium battery or lithium or sodium battery according to the present invention is used in uninterrupted power supply (UPS) systems, portable consumer electronics, and electric and / or hybrid vehicles. Considering the advantages offered by these networks when used in lithium or sodium battery anodes, the above list of applications is non-exhaustive. [Carbon network with carbon nanofibers] The porous chemically interconnected carbon network comprising carbon nanofibers or the porous carbon network comprising chemically interconnected carbon nanofibers is preferably characterized as follows.

[0053] Those skilled in the art will understand that a porous network refers to a three-dimensional structure that allows fluids or gases to pass through. A porous network can also be described as a porous medium or a porous material. The porous crystalline carbon network according to the present invention (or the porous carbon network particles according to the present invention) can also be viewed as a large molecule in which carbon atoms are originally interconnected by covalent bonds. Here, referring to a porous network made by a plurality of molecules or particles, it is understood that the porous carbon network particles are particles with chemically interconnected (i.e., covalently bonded) fibers with intraparticle porosity, as opposed to interparticle porosity, in which the pores are formed by the spaces between physically aggregated particles or molecules. In the context of the present invention, the carbon network particles according to the present invention can also be viewed as large molecules in which the pores are embedded, and therefore the intraparticle porosity can also be described as intramolecular porosity. Thus, intraparticle porosity and intramolecular porosity have the same meaning in the present document and can be used interchangeably.

[0054] The network of the present invention can be seen as one large molecule, so there is no need to fuse the particles or parts of the network together. Therefore, the carbon network with porous, chemically interconnected carbon nanofibers is preferred to be a carbon network with non-fused, intraparticle-porous, chemically interconnected, crystalline carbon nanofibers with intraparticle porosity. Without being bound by theory, it is believed that the advantage of having a crystalline network with intraparticle porosity over an (amorphous) network with interparticle porosity is that it is firstly more robust and more resilient to crushing or breaking when a force is applied. For comparison purposes, carbon black consists of aggregates or agglomerates of spherical particles that can form a three-dimensional structure, with the spheres fused together with amorphous connections that have weaker porosity. The pores between the particles are weaker and more prone to collapse due to particle-particle interfaces. The pores within the particles are stronger due to the covalently bonded structure with crystalline arrangements that surround them, and can withstand large forces and pressures without collapsing. This is in sharp contrast to conventional carbon black, which consists of aggregates or agglomerates of spherical particles that may form a three-dimensional structure, where the spheres are fused together (not chemically "interconnected") with amorphous connections between the individual particles. In summary, intraparticle porosity (the trademark for the network of the present invention) refers to the situation where the carbon atoms surrounding the pores are covalently connected in crystalline form, whereas interparticle porosity refers to the pores being between particles that are physically aggregated or agglomerated, or between particles that have amorphous connections. The intraparticle pore volume can be characterized in terms of mercury intrusion porosimetry (ASTM D4404-10) or nitrogen absorption method (ISO 9277:10). The pore volume of the porous carbon network of the present invention is measured using mercury intrusion porosimetry (ASTM D4404-10) and is in the range of 0.05 to 5 cm. 3 / g, preferably 0.1 to 4 cm 3 / g, more preferably 0.3 to 3.5 cm 3 / g, most preferably 0.5 to 3 cm 3 / g. Additionally, or alternatively, the carbon network comprising carbon nanofibers may be characterized as having an intraparticle pore diameter size of 5-200 nm, preferably 10-150 nm, and most preferably 20-130 nm, as measured using mercury intrusion porosimetry (ASTM D4404-10). Following the same ASTM test method, the network may have an interparticle pore diameter of 10-500 μm, more preferably 80-400 μm.

[0055] The porous network is preferably characterized by a d-spacing of 0.34-0.5 nm, more preferably 0.35-0.45 nm, and even more preferably 0.355-0.375 nm. The d-spacing is measured by XRD. Importantly, this d-spacing facilitates the intercalation of lithium or sodium ions. This is particularly beneficial for the intercalation of sodium ions in sodium batteries due to the large volume of sodium ions.

[0056] Those skilled in the art will readily understand that the term chemically interconnected in the context of a carbon network comprising porous, chemically interconnected carbon nanofibers implies that the carbon nanofibers are interconnected to other carbon nanofibers by chemical bonds. It is also understood that chemical bonds are synonymous with molecular or covalent bonds. Typically, the locations where carbon nanofibers are connected are referred to as connections or fiber connections and may therefore be conveniently designated as "covalent connections". These terms are used interchangeably in this document. In the carbon network according to the invention, the connections are formed by carbon atoms that are covalently connected. It further follows that the length of the fiber is defined as the distance between connections connected by the fibrous carbon material.

[0057] In a preferred embodiment, at least a portion of the fibers in the carbon network comprising the carbon nanofibers of the present invention are crystalline carbon nanofibers. Preferably, at least 20% by weight of the carbon in the carbon network of the present invention is crystalline, more preferably at least 40% by weight, even more preferably at least 60% by weight, even more preferably at least 80% by weight, and most preferably at least 90% by weight. Alternatively, the amount of crystalline carbon is 20-90% by weight, more preferably 30-70% by weight, more preferably 40-50% by weight, compared to the total carbon in the carbon network of the present invention. Here, "crystallinity" has its usual meaning and refers to the degree of structural order in a material. In other words, the carbon atoms in the nanofibers are arranged in a more or less regular and periodic manner. The area or volume that is crystalline can be expressed as crystallites. Carbon crystallites are therefore individual carbon crystals.

[0058] A measure of the size of the carbon crystallites is the stacking height of the graphitic layers. Standard ASTM grade carbon black has stacking heights of graphitic layers in the range of 11-13 Å (angstroms) within these crystallites. In a preferred embodiment, the carbon network comprising the carbon nanofibers of the invention preferably has a stacking height of at least 15 Å (angstroms), preferably at least 16 Å, more preferably at least 17 Å, even more preferably at least 18 Å, even more preferably at least 19 Å, and even more preferably at least 20 Å. If necessary, carbon networks containing crystallites as large as 100 Å (angstroms) can be produced. Thus, the carbon networks of the invention have stacking heights of 15-100 Å (angstroms), more preferably up to 80 Å, even more preferably up to 60 Å, even more preferably up to 40 Å, and even more preferably up to 30 Å. It is therefore understood that the stacking height of the graphitic layers within the crystallites in the carbon network of the present invention is 15 to 90 Å (angstroms), more preferably 16 to 70 Å, even more preferably 17 to 50 Å, still more preferably 18 to 30 Å, and most preferably up to 25 Å.

[0059] A carbon network comprising porous, chemically interconnected carbon nanofibers may be defined as having chemically interconnected carbon nanofibers, where the carbon nanofibers are interconnected through parts of the connections, and where a plurality (typically 3 or more, preferably at least 10 or more) of nanofibers are covalently bonded. The carbon nanofibers are part between the connections of the network. The fibers are typically solid (i.e., non-hollow) and elongated, preferably having an average diameter or thickness of 1-500 nm, preferably 5-350 nm, more preferably up to 100 nm, in one embodiment 10-100 nm, compared to an average particle size of 10-400 nm for carbon black particles. In one embodiment, the average fiber length (i.e., the average distance between two connections) is preferably in the range of 30-10,000 nm, more preferably 50-5,000 nm, more preferably 100-5,000 nm, more preferably at least 200-5,000 nm, and may be determined, for example, using SEM.

[0060] The nanofibers or structures may be described in terms of an average aspect ratio of fiber length to thickness of at least 2, preferably at least 3, more preferably at least 4, most preferably at least 5, and preferably at most less than 50; in sharp contrast to the amorphous (physically associated) aggregates formed from spherical particles obtained through conventional carbon black manufacturing. The average aspect ratio of fiber length to thickness may be determined, for example, using SEM.

[0061] A carbon nanofiber structure can be defined as a carbon network formed by chemically interconnected (covalently bonded) carbon nanofibers. The carbon network has a three-dimensional organization with gaps between the carbon nanofibers (intracene porosity, see above) accessible to a continuous phase, which may be a liquid (e.g., a solvent or aqueous phase), a gas, or any other phase. The carbon network is at least 0.5 μm in diameter, preferably at least 1 μm in diameter, preferably at least 5 μm in diameter, more preferably at least 10 μm in diameter, even more preferably at least 20 μm in diameter, and most preferably at least 25 μm in diameter in all dimensions. Alternatively, the carbon network is at least 1 μm in diameter in two dimensions and at least 5 μm in diameter, preferably at least 10 μm in diameter, more preferably at least 20 μm in diameter, and most preferably at least 25 μm in diameter in the other dimensions. Here, and also throughout this document, the term dimension is used in the usual way to refer to a spatial dimension. There are three spatial dimensions that are mutually orthogonal and define a space in the usual physical sense. Further, the carbon network may be at least 10 μm in diameter in two dimensions and at least 15 μm in diameter in the other dimension, preferably at least 20 μm in diameter, more preferably at least 25 μm in diameter, more preferably at least 30 μm in diameter, and most preferably at least 50 μm in diameter. These measurements are based on laser diffraction.

[0062] The carbon network comprising carbon nanofibers may have a volume-based aggregate size of 0.1 to 100 μm, preferably 1 to 50 μm, more preferably 1 to 40 μm, more preferably 5 to 35 μm, more preferably 5 to 25 μm, and most preferably 5 to 20 μm, as measured using laser diffraction (ISO 13320-1) or dynamic light scattering analysis. In a most preferred embodiment, the network has a volume-based aggregate size of 5 to 10 μm, as measured using laser diffraction (ISO 13320-1) or dynamic light scattering analysis. The network preferably has an advantageously narrow filament diameter size distribution, especially compared to traditional carbon blacks. The filament diameter size distribution may be characterized as between 10 nm and 200 nm, preferably 10 to 100 nm, as determined using transmission electron microscopy and measuring the diameter of the fibers. The network may be characterized by a set strength between 0.5 and 1, more preferably between 0.6 and 1, as determined by the c-OAN / OAN ratio measured according to ASTM D3493-16 / ASTM D2414-16, respectively. The c-OAN is preferably 20-200 cc / 100 g. This is a high strength that advantageously prevents the collapse of the internal porosity even in high pressure applications.

[0063] The porous, chemically interconnected carbon network comprising carbon nanofibers may also comprise carbon black particles incorporated as part of the network. These particles are found deep in the connections between the carbon nanofibers, but there may also be carbon black particles present in other parts of the network. The carbon black particles preferably have a diameter at least 0.5 times that of the carbon nanofibers, more preferably at least the same diameter as the carbon nanofibers, even more preferably at least twice the diameter of the carbon nanofibers, even more preferably at least three times the diameter of the carbon nanofibers, even more preferably at least four times the diameter of the carbon nanofibers, and most preferably at least five times the diameter of the carbon nanofibers. It is preferred that the diameter of the carbon black particles is no more than 10 times the diameter of the carbon nanofibers. Such a mixed network is designated a hybrid network.

[0064] The porous and chemically interconnected carbon network with carbon nanofibers has a functionalized surface. In other words, the surface is provided with groups that change the hydrophobic nature of the surface (typical of carbon) to a more hydrophilic nature. The surface of the carbon network is provided with carboxyl, hydroxyl and phenolic groups. These groups add some polarity to the surface and may change the properties of the compound material in which the functionalized carbon network is embedded. The surface area of ​​the carbon network with carbon nanofibers, measured according to the Brunauer-Emmett-Teller (BET) method (ISO 9277:10), is preferably between 15 and 300 m. 2 / g, more preferably 20 to 270m 2 / g, and more preferably 30 to 250 m 2 / g, most preferably 30 to 210 m 2 / g.

[0065] The porous and chemically interconnected carbon network with carbon nanofibers contains only a small amount of metal catalyst nanoparticles, typically at least 10 ppm based on the weight of the carbon network with carbon nanofibers. These are the fingerprints of the preparation method. There is a preferred amount of metal nanoparticles of 5000 ppm or less, more preferably 3000 ppm or less, especially 2000 ppm or less, based on the weight of the network measured by ICP-OES (Inductively Coupled Plasma Optical Emission Spectroscopy). These metal particles are also embedded in the network. These particles can have an average particle size between 1 nm and 100 nm. Preferably, the particles are monodisperse particles with a deviation from the average particle size within 10%, more preferably within 5%. Non-limiting examples of nanoparticles contained in the carbon network with carbon nanofibers are noble metals (Pt, Pd, Au, Ag), iron group elements (Fe, Co and Ni), Ru and Cu. Suitable metal complexes include (i) platinum precursors, such as HPtCl; HPtCl·xH0; KPtCl; KPtCl·xH0; Pt(NH)(NO); Pt(CHO), (ii) ruthenium precursors, such as Ru(NO)(NO); Ru(dip)Cl [dip=4,7-diphenyl-1,10-phenanthroline]; RuCl, or (iii) palladium precursors, such as Pd(NO). or (iv) a nickel precursor, for example NiCl2 or NiCl2·xH2O; Ni(NO3)2; Ni(NO3)2·xH2O; Ni(CH3COO)2; Ni(CH3COO)2·xH2O; Ni(AOT)2 [AOT = bis(2-ethylhexyl)sulfosuccinate], where x may be any integer selected from 1, 2, 3, 4, 5, 6, 7, 8, 9 or 10, typically 6, 7 or 8.

[0066] Porous, chemically interconnected carbon networks comprising carbon nanofibers are preferably obtained by a process for the production of crystalline carbon networks in a reactor 3 containing a reaction zone 3b and a termination zone 3c, by injecting a thermodynamically stable water-in-oil, oil-in-water or bicontinuous microemulsion c, preferably a water-in-oil or bicontinuous microemulsion c, bicontinuous microemulsion c, comprising metal catalyst nanoparticles, into the reaction zone 3b at a temperature above 600° C., preferably above 700° C., more preferably above 900° C., even more preferably above 1000° C., more preferably above 1100° C., preferably at most 3000° C., more preferably at most 2500° C., most preferably at most 2000° C., in order to produce crystalline carbon networks e, transporting these networks e to the termination zone 3c, and quenching or stopping the formation of the crystalline carbon networks in the termination zone by spraying into water d.

[0067] In a more preferred embodiment, the network is a furnace-type carbon black reactor 3, which contains, along the axis of the reactor 3, a combustion zone 3a, a reaction zone 3b and a termination zone 3c, and which comprises burning a fuel a in an oxygen-containing gas b and passing waste gas a1 from the combustion zone 3a to the reaction zone 3b to generate a flow of hot waste gas a1 in the combustion zone, and in the reaction zone 3b containing the hot waste gas, a water-in-oil, oil-in-water or bicontinuous microemulsion c, preferably a water-in-oil or bicontinuous microemulsion b, to obtain a crystalline carbon network e. and carbonizing the emulsion at a temperature above 600° C., preferably above 700° C., more preferably above 900° C., even more preferably above 1000° C., more preferably above 1100° C., preferably at most 3000° C., more preferably at most 2500° C., most preferably at most 2000° C., and quenching or stopping the reaction in a termination zone 3 c by spraying into water d.

[0068] In the above, "chemically interconnected" is understood to mean that the nanofibers are covalently bonded to one another and are distinct from physical aggregates.

[0069] The network is preferably obtained by the above process, where further processing details are provided in the section headed "Process for obtaining a carbon network comprising carbon nanofibers" herein below, and in FIG. 1A. [Process for obtaining a carbon network with carbon nanofibers] The process for obtaining the porous, chemically interconnected carbon network comprising carbon nanofibers can best be described as a modified carbon black production process, where "modified" is understood to mean that a suitable oil, preferably an oil comprising at least 14C atoms (greater than C14), such as a carbon black feedstock oil (CBFS), is provided to the reaction zone of a carbon black reactor as part of a single-phase emulsion, which is a thermodynamically stable water-in-oil, oil-in-water or bicontinuous microemulsion, preferably a water-in-oil or bicontinuous microemulsion, most preferably a bicontinuous microemulsion, comprising metal catalyst nanoparticles. The emulsion is preferably provided to the reaction zone by spraying, thus atomizing, the emulsion into droplets. The process can be carried out in batch or semi-batch mode, but the modified carbon black production process is advantageously carried out as a continuous process. The single-phase emulsion is a microemulsion comprising metal catalyst nanoparticles. The preferred single-phase emulsion comprises CBFS oil, which may also be referred to in the context of the present invention as an "emulsified CBFS".

[0070] The process for the production of carbon networks can be carried out in a reactor 3 containing a reaction zone 3b and a termination zone 3c by injecting a single-phase emulsion c, which is a water-in-oil, oil-in-water or bicontinuous microemulsion c, preferably a water-in-oil or bicontinuous microemulsion c, most preferably a bicontinuous microemulsion c, into the reaction zone 3b at a temperature above 600° C., preferably above 700° C., more preferably above 900° C., even more preferably above 1000° C., more preferably above 1100° C., preferably up to 3000° C., more preferably up to 2500° C., most preferably up to 2000° C., in order to produce a carbon network with porous and chemically interconnected carbon nanofibers, in which the single-phase emulsion e is sprayed into the reaction zone 3b, and quenching or stopping the formation of the carbon network with porous and chemically interconnected carbon nanofibers by spraying into water d. The single-phase emulsion is preferably sprayed into the reaction zone. Please refer to Figure 1A.

[0071] Alternatively, a process for the production of a porous, chemically interconnected carbon network comprising carbon nanofibers comprises burning a fuel a in an oxygen-containing gas b in a furnace-type carbon black reactor 3, which contains a combustion zone 3a, a reaction zone 3b and a termination zone 3c along the axis of the reactor 3, and generating a flow of hot waste gas a1 in the combustion zone by passing the waste gas a1 from the combustion zone 3a to the reaction zone 3b, and producing a single-phase emulsion c according to the invention, preferably water-in-oil, oil-in-water or bicontinuous microemulsion c, preferably water-in-oil or This is carried out by spraying (atomizing) a bicontinuous microemulsion c, most preferably a bicontinuous microemulsion c, carbonizing the emulsion at high temperatures (temperatures above 600°C, preferably above 700°C, more preferably above 900°C, even more preferably above 1000°C, more preferably above 1100°C, preferably up to 3000°C, more preferably up to 2500°C, most preferably up to 2000°C), and quenching or stopping the reaction in a termination zone 3c (i.e. the formation of a porous, chemically interconnected carbon network with carbon nanofibers) by spraying into water d. The reaction zone 3b is equipped with at least one inlet (preferably a nozzle) for introducing the emulsion, preferably by atomization. Reference is made to FIG. 1A.

[0072] The residence time for the emulsion in the reaction zone of the furnace carbon black reactor may be relatively short, preferably in the range of 1-1000 ms, more preferably 10-100 ms. Longer residence times may have an effect on the properties of the carbon network. An example may be the size of the crystallites, which are larger when longer residence times are used.

[0073] In accordance with conventional carbon black manufacturing processes, the oil phase may be aromatic and / or aliphatic, preferably comprising at least 50% by weight C14 or higher, more preferably at least 70% by weight C14 or higher (based on the total weight of oil). A list of typical oils that may be used, but is not limited to obtaining a stable emulsion, is carbon black feedstock oil (CBFS), phenolic oil, anthracene oil, (short-medium-long chain) fatty acids, fatty acid esters and paraffins. The oil is preferably C14 or higher. In one aspect, the oil preferably has high aromaticity. Within this field, aromaticity is preferably characterized in terms of the Bureau of Mines Correlation Index (BMCI). The oil preferably has a BMCI greater than 50. In one aspect, the oil has low aromaticity, preferably a BMCI less than 15.

[0074] CBFS is an economically attractive oil source in the context of the present invention, preferably a heavy hydrocarbon mix comprising mainly C14-C50, the sum of C14-C50 preferably amounting to at least 50% by weight of the feedstock, more preferably at least 70% by weight. Some of the most important feedstocks used to produce carbon black include clarified slurry oil (CSO) obtained from fluid catalytic cracking of light oils, ethylene cracker residue from naphtha steam cracking, and coal tar oil. The presence of paraffins (smaller than C15) substantially reduces compatibility, and higher aromaticity is preferred. The concentration of aromatics determines the rate at which carbon nuclei are formed. Carbon black feedstocks preferably have a high BMCI and can provide high yields with minimal heat input, thus reducing the cost of production. In a preferred embodiment, and based on current CBFS specifications, the oil, including the mixture of oils, has a BMCI value of greater than 120. It is not difficult for a person skilled in the art to understand which are suitable CBFS, but it is noted, merely as a guideline, that the BMCI value for the CBFS (from the point of view of yield) is preferably greater than 120, even more preferably greater than 132. The amount of asphaltenes in the oil is preferably less than 10% by weight, preferably less than 5.0% by weight of the CBFS. The CBFS preferably has a low sulfur content, since sulfur adversely affects the quality of the product, leading to lower yields and corroding equipment.

[0075] It is preferred that the sulfur content of the oil according to ASTM D1619 be less than 8.0 wt.%, preferably less than 4.0 wt.%, more preferably less than 2.0 wt.%.

[0076] The emulsion, preferably the emulsion with CBFS, is a "single-phase emulsion", which is understood to mean that the oil and water phases appear optically as one miscible mixture, showing no physical separation of oil, water or surfactant to the naked eye. The single-phase emulsion is a water-in-oil, oil-in-water or bicontinuous microemulsion, preferably a water-in-oil or bicontinuous microemulsion, most preferably a bicontinuous microemulsion. The process of complete emulsion breakage (coalescence), i.e., the system separates into bulk oil and water phases, is generally believed to be controlled by four different droplet disappearance mechanisms: Brownian flocculation, creaming, sedimentation flocculation, and disproportionation.

[0077] The amount of water and oil is not considered critical, provided that the above microemulsion is obtained, but it is noted that a reduced amount of water (and an increased amount of oil) improves the yield. The water content is typically between 5% and 50% by weight of the emulsion, preferably 10-40% by weight, even more preferably up to 30% by weight, more preferably 10-20% by weight of the emulsion. Higher amounts of water may be considered, but at the expense of yield. Without wishing to be bound by any theory, the inventors believe that the shape and morphology of the network thus obtained is attributable to the aqueous phase.

[0078] The choice of surfactant is not considered to be a limiting factor, as long as the combination of oil, water and surfactant results in a stable microemulsion as defined herein above. As a further guide to the skilled artisan, it is noted that surfactants can be selected based on the hydrophobicity or hydrophilicity of the system, i.e., hydrophilic-lipophilic balance (HLB). The HLB of a surfactant is a measure of the degree to which the surfactant is hydrophilic or lipophilic, and is determined by calculating values ​​for different regions of the molecule by the Griffin or Davies method. The appropriate HLB value depends on the type of oil and the amount of oil and water in the emulsion, and can be easily determined by the skilled artisan based on the requirement of maintaining a thermodynamically stable single-phase emulsion as defined herein above. It has been found that emulsions with more than 50% by weight of oil and preferably less than 30% by weight of water phase are best stabilized by surfactants with HLB values ​​of more than 7, preferably more than 8, more preferably more than 9, and most preferably more than 10. On the other hand, emulsions with 50% or less by weight of oil are best stabilized by surfactants with HLB values ​​less than 12, preferably less than 11, more preferably less than 10, most preferably less than 9, especially less than 8. The surfactant is preferably selected to be compatible with the oil phase. When the oil is an emulsion with a CBFS, surfactants with high aromaticity are preferred by the CBFS, and oils with low BMCI, such as those characterized by a BMCI less than 15, are best stabilized using aliphatic surfactants. The surfactant can be cationic, anionic or nonionic, or a mixture thereof. To increase the yield, one or more nonionic surfactants are preferred, since no residual ions are left in the final product. To obtain a clean tail gas stream, the surfactant structure is preferably low in sulfur and nitrogen, preferably sulfur and nitrogen-free. Non-limiting examples of typical non-ionic surfactants that can be used to obtain a stable emulsion are the commercially available series Tween, Span, Hypermer, Pluronic, Emulan, Neodol, Triton X and Tergitol.

[0079] In the context of the present invention, a microemulsion is a dispersion made of water, oil (preferably CBFS) and surfactant, which is an optically homogeneous and thermodynamically stable liquid, with the diameter of the dispersed domains varying from approximately 1 to 500 nm, preferably 1 to 100 nm, usually 10 to 50 nm. In a microemulsion, the domains of the dispersed phase are either particulate (i.e. droplets) or interconnected (giving a bicontinuous microemulsion). In a preferred embodiment, the surfactant tail forms a continuous network in the oil phase of the water-in-oil, oil-in-water or bicontinuous microemulsion, preferably the water-in-oil or bicontinuous microemulsion, most preferably the bicontinuous microemulsion. The water domains should contain a metal catalyst, preferably with an average particle size between 1 nm and 100 nm.

[0080] The single-phase emulsion, i.e. water-in-oil, oil-in-water or bicontinuous microemulsion, preferably water-in-oil or bicontinuous microemulsion, most preferably bicontinuous microemulsion, further comprises metal catalyst nanoparticles, preferably having an average particle size between 1 nm and 100 nm. Those skilled in the art find ample guidance in the field of carbon nanotubes (CNTs) to produce and use these types of nanoparticles. These metal nanoparticles have been found to improve network formation, both in terms of speed and yield, and reproducibility. Methods for producing suitable metal nanoparticles can be found in Vinciguerra et al., "Growth mechanisms in chemical vapour deposited carbon nanotubes," Nanotechnology (2003) 14, 655; Perez-Cabero et al., "Growing mechanism of CNTs: a kinetic approach," J. Catal. (2004) 224, 197-205; Gavillet et al., "Microscopic mechanisms for the catalyst assisted growth of single-wall carbon nanotubes," Carbon. (2002) 40, 1649-1663, and Amelinckx et al., "A formation mechanism for catalytically grown helix-shaped graphite nanotubes," Science (1994) 265, 635-639, the contents of which with respect to producing metal nanoparticles are incorporated herein by reference.

[0081] Metal catalyst nanoparticles are used in water-in-oil, oil-in-water or bicontinuous microemulsions, preferably water-in-oil or bicontinuous microemulsions, most preferably bicontinuous microemulsions. Advantageously, the uniformity of the metal particles is controlled by mixing a first (bicontinuous) microemulsion, in which the aqueous phase contains a metal complex salt that can ultimately be reduced to metal particles, with a second (bicontinuous) microemulsion, in which the aqueous phase contains a reducing agent capable of reducing the metal complex salt, and upon mixing, the metal complex is reduced, thus forming the metal particles. The controlled (bicontinuous) emulsion environment stabilizes the particles against sintering or Ostwald ripening. The size, concentration and durability of the catalyst particles are easily controlled. It is considered routine experimentation to adjust the average metal particle size within the above ranges, for example by modifying the molar ratio of metal precursor to reducing agent. Smaller particles are obtained by increasing the relative amount of reducing agent. The metal particles thus obtained are monodisperse, with deviations from the average particle size preferably within 10%, more preferably within 5%. Furthermore, the present technology does not restrict the actual metal precursors, as long as they can be reduced. Non-limiting examples of nanoparticles included in the carbon network comprising carbon nanofibers are noble metals (Pt, Pd, Au, Ag), iron group elements (Fe, Co and Ni), Ru and Cu.Suitable metal complexes include (i) platinum precursors, such as HPtCl; HPtCl·xH0; KPtCl; KPtCl·xH0; Pt(NH)(NO); Pt(CHO), (ii) ruthenium precursors, such as Ru(NO)(NO); Ru(dip)Cl [dip=4,7-diphenyl-1,10-phenanthroline]; RuCl, or (iii) palladium precursors, such as Pd(NO). 2, or (iv) nickel precursors, such as NiCl2 or NiCl2·xH2O; Ni(NO3)2; Ni(NO3)2·xH2O; Ni(CH3COO)2; Ni(CH3COO)2·xH2O; Ni(AOT)2 [AOT=bis(2-ethylhexyl)sulfosuccinate], where x can be any integer selected from 1, 2, 3, 4, 5, 6, 7, 8, 9 or 10, typically 6, 7 or 8. Non-limiting suitable reducing agents are hydrogen gas, sodium boron hydride, sodium bisulfate, hydrazine or hydrazine hydrate, ethylene glycol, methanol and ethanol. Citric acid and dodecylamine are also suitable. The type of metal precursor is not essential to the invention. The metal of the particles of the (bicontinuous) microemulsion is preferably selected from the group consisting of Pt, Pd, Au, Ag, Fe, Co, Ni, Ru and Cu, and mixtures thereof, in order to control the morphology of the carbon structure network finally formed. The metal nanoparticles are finally embedded inside these structures, and the metal particles are physically attached to the structures. Although there is no minimum concentration of metal particles at which these networks are formed (indeed, the networks are formed using the modified carbon black manufacturing process according to the invention), it has been found that the yield increases with the metal particle concentration. In a preferred embodiment, the active metal concentration is at least 1 mM, preferably at least 5 mM, preferably at least 10 mM, more preferably at least 15 mM, more preferably at least 20 mM, in particular at least 25 mM, most preferably up to 3500 mM, preferably up to 3000 mM. In one embodiment, the metal nanoparticles comprise up to 250 μM. There is a catalyst concentration relative to the amount of aqueous phase of the (bicontinuous) microemulsion.

[0082] Atomization of the single phase emulsion, preferably an emulsion comprising a CBFS, is preferably achieved by spraying using a nozzle system 4, whereby the emulsion droplets come into contact with the hot waste gas a1 in the reaction zone 3b, resulting in traditional carbonization, network formation and subsequent aggregation to produce the carbon network according to the invention. The injection step preferably involves high temperatures above 600°C, preferably between 700°C and 3000°C, more preferably between 900°C and 2500°C, more preferably between 1100°C and 2000°C. [Example] EXAMPLES

[0083] Characterization of lithium-ion battery anodes comprising carbon networks comprising carbon nanofibers according to the present invention The performance of lithium ion battery anodes comprising carbon networks with carbon nanofibers according to the present invention ("carbon networks") grades A, B, C and D was compared with that of lithium ion battery anodes with synthetic graphite (AG) as active material and conductive carbon black (Super C65). Both grades A and B were produced in a furnace-type carbon black reactor by using the same feedstock. The residence times for grades A and B were in the range of 400-800 ms and 10-100 ms, respectively (based on theoretical model). Grades D and C were also produced in a furnace-type carbon black reactor by using the same feedstock and the same residence times as A and B, respectively. Grade D was produced by using a 30% higher feed rate compared to A, while grade C was produced by using a 30% lower feed rate compared to B. (Anode paste preparation) PVDF in mg quantities was dissolved in NMP (7.00 g) using mechanical stirring for 45 min. Carbon in g quantities was added and 4 mm diameter glass beads (1.0 g) were also added to increase shear during mixing. The paste was mixed in a Speedmixer (Hauschildt) at 2500 rpm for 2 min, followed by further mixing at 2500 rpm for 10 min to obtain the anode paste.

[0084] [Table 1]

[0085] (Anode preparation) The glass plate was thoroughly cleaned and dried using acetone. A few drops of NMP were added to the glass plate by capillary force to hold the copper foil (>99.9% Cu, 10 micron thickness, Nanografi) in place. The copper foil was cleaned using NMP and subsequently dried using a lint-free cloth. The anode paste was cast using a doctor blade set at the height specified in the table. The glass plate was transferred to an oven and kept at 110° C. overnight. The anode was punched out (14 mm diameter). (Half-cell preparation) The spring, spacer, lithium disk (15.6 mm), a few drops of electrolyte (EC / EMC 1:1 1M LiPF6), electrolyte (EC / EMC 1:1 1M LiPF6) soaked separator (20 mm), a few drops of electrolyte (EC / EMC 1:1 1M LiPF6), and anode facing down were crimped together in a CR2032 coin cell in a glove box. After removing the half cell from the glove box, it was immediately used for electrochemical testing.

[0086] [Table 2]

[0087] a) Capacity A fresh half-cell was discharged at a constant discharge current of 0.2C until the potential dropped to 0.01V (approximately 5 hours of discharge). The half-cell was then held at 0.01V for 1 hour or until the discharge current was less than 1% of the initial discharge current. The half-cell was then left to equilibrate for 1 hour before being charged at 0.2C to 2.0V (approximately 5 hours of charge). The half-cell was then held at 2.0V for 1 hour or until the charge current was less than 1% of the initial charge current. The capacity was calculated by multiplying the charge current by the time it took to reach 2.0V, including the current required to hold the potential at 2.0V for 1 hour.

[0088] [Table 3]

[0089] In the above table, AG% is the relative % of capacity compared to the TDS value of synthetic graphite (338.6 mAh / g). Electrochemical testing of anodes containing A and B in Li-ion half cells revealed that, contrary to expectations, the Li-ion capacity of A and B was (at least) comparable to that of synthetic graphite. b) Cycle ability (cycle life) The new half-cell was discharged at a constant discharge current of 0.2C until the potential dropped to 0.01V (approximately 5 hours of discharge). The half-cell was then held at 0.01V for 1 hour or until the discharge current was less than 1% of the initial discharge current. The half-cell was then left to equilibrate for 1 hour before being charged at 0.2C to 2.0V (approximately 5 hours of charge). The half-cell was then held at 2.0V for 1 hour or until the charge current was less than 1% of the initial charge current. This was a single cycle. The cycle was repeated (in terms of number of times) as many times as possible and the capacity loss was monitored as a function of cycles.

[0090] [Table 4]

[0091] The rate capacity test of grade A showed capacity retention at high charge / discharge rates. Also, the capacity loss during cycling was lower than expected. This is unexpected since usually the capacity is lower at higher charge / discharge rates and the capacity loss during cycling is larger at higher charge / discharge rates. Figure 3 further shows that grade A (squares) achieves a more stable specific capacity over time when compared to AG (triangles), while grade B (crosses) achieves a similar specific capacity over time when compared to AG (triangles). Similar to grade A, grades C and D showed capacity retention at high charge / discharge rates. Figure 6 shows that grades C (circles) and D (pluses) perform similarly to grade A (crosses) and have stable specific capacity over time when compared to AG (stars). The specific capacity of grade D remained stable for at least 128 cycles. c) Electrochemical Impedance Spectroscopy (EIS): Electrical impedance spectroscopy was performed at an open cell potential (E OC ) for a new half-cell. EIS spectra are recorded between 10 kHz and 0.1 Hz using 6 points per decade. The amplitude of the potential (sinusoidal) is set to 10 mV. A Randles-type equivalent circuit is used to model the data and R b (bulk impedance) and R SEI (solid electrolyte interface impedance) and R CT (charge transfer impedance) and W (Warburg coefficient related to Li-ion diffusivity).

[0092] [Table 5]

[0093] J.Electrochem.Sci.Technol.2020, 11(1), 1~13 1, Woosung Choi et al., J.Electrochem.Soc.2012, 159(7), A1034, Nobohiru Ogihara et al. 2 Quote from: The trend of change in cell resistance in the porous electrode is shown in Fig. 11(a) for the four parameters: electrical resistance (R e ) and the electrolyte bulk resistance (R sol ) and the ionic resistance in the pores (R ion ) and the charge transfer resistance (R ct ) and the temperature dependence. The plot can be written as a TLM for a cylindrical pore for the Faradaic process at all temperatures. As the temperature is decreased, R sol The true impedance component at 100 kHz, which determines the value of R, shifts slightly toward more positive values. ion The length of the 45° inclined line reflecting R increases. This indicates that as the temperature decreases, the two resistances increase somewhat. However, R ct The semicircle in the low frequency region, corresponding to R, is significantly enlarged as the temperature decreases. ct The temperature dependence of R sol or R ion The temperature dependence of the R ion is the resistance due to Li-ion diffusion. The slope length of the Warburg component is R ion This is obviously easier to compare qualitatively. In the Nyquist plot (EIS data) in Figure 4, the lines for grades A (squares) and B (triangles) are shorter (lower R ion ). Therefore, the internal resistivity of the Grade B anode is lower compared to that of synthetic graphite. Figure 4 also shows that the internal resistivity of Grade A (squares) is comparable to that of AG (circles), indicating superior Li-ion diffusivity in the carbon network.

[0094] The Li-ion diffusivity is given by the following equation: 1,3 can be quantified using:

[0095]

number

[0096] During the ceremony, V M Molar volume of active material F Faraday constant S electrode / electrolyte contact area σ Z img Slope vs.

[0097]

number

[0098]

number

[0099] Slope of the charge / discharge curve This equation demonstrates that, other quantities being equal, the Li-ion diffusivity is greater (faster diffusion, desirable in a battery) when σ is smaller.

[0100] Z img The slope of the graphite (i.e., the straight line in FIG. 4) should be less steep. As can be seen in the EIS data in FIG. 4, the slope of synthetic graphite (AG, circles) is steeper than that of grade B (triangles), indicating superior Li-ion diffusivity in the carbon network of grade B. Grade A (squares) exhibits a Li-ion diffusivity comparable to AG (circles), indicating superior Li-ion diffusivity in the carbon network. d) Charge / discharge rate: Cycle ability at various C rates

[0101] [Table 6]

[0102] The new half-cell was discharged at a constant discharge current of 0.5C until the potential dropped to 0.01V (about 2 hours discharge). The half-cell was then held at 0.01V for 1 hour or until the discharge current was less than 1% of the initial discharge current. The half-cell was then left to equilibrate for 1 hour and then charged at 0.5C to 2.0V (about 2 hours charge). The half-cell was then held at 2.0V for 1 hour or until the charge current was less than 1% of the initial charge current. This cycle was repeated 10 times. The discharge and charge currents were then changed to 1.0C (about 1 hour (discharge) charge) and this was repeated 10 times. The discharge and charge currents were then changed to 5.0C (12 minutes (discharge) charge) and this was repeated 10 times. The discharge and charge currents were then changed to 10.0C (6 minutes (discharge) charge) and this was repeated 10 times. Then, to observe the loss in capacity after these 55 cycles, the discharge and charge currents were changed back to 0.5C (about 2 hours charge), which was repeated 10 times. After 10 cycles at 10.0C for grades C, D, and AG, the discharge and charge currents were changed back to 20.0C (3 minutes charge), which was repeated 10 times. Then, to observe the loss in capacity after 66 cycles, the discharge and charge currents were changed back to 0.5C (about 2 hours charge), which was repeated 10 times. After 20.0C, the cycles with AG could not be completed due to material degradation.

[0103] Figure 5 shows that by using grade A (triangles), the capacity only decreased slightly (from 100% to 95%) while the C-rate increased from 0.5C to 10C. Moreover, when the C-rate was reduced from 10C to 0.5C at the end of the sequence, the initial capacity was fully restored (100%), which is a better behavior than that observed in the case of artificial graphite (AG, crosses). Grade B (circles) also presented a capacity value higher than that of AG (crosses).

[0104] Figures 7 and 8 show that for grade C (diamonds in Figure 7) and grade D (squares in Figure 7), the specific capacity only slightly decreased (from 100% to 90%) at 10C, and even up to 20C, it was still only slightly reduced (from 100% to 87%). When the C-rate was reduced from 20C to 0.5C, it was still possible to recover 95-97% of the initial capacity. In contrast, with AG (cross in Figure 7), at 20C, the capacity was significantly reduced (from 100% to 71%). When the C-rate was reduced from 20C to 0.5C, it was not possible to recover the initial capacity of AG (from 100% to 83%).

[0105] 9A, 9B and 9C show the coulombic efficiency for grade C, grade D and AG, respectively. Discharging corresponds to the lithiation process and charging corresponds to the delithiation process. For a half cell, the coulombic efficiency % is calculated as: (charge / discharge) x 100. It can be seen that the coulombic efficiency is almost 100% for grade C and grade D throughout the cycle from 0.5C to 20C and back to 0.5C, while for AG, it drops to around 60% from 10 to 20C.

Claims

1. Use of a porous, chemically interconnected carbon network comprising carbon nanofibers as the electrochemically active material in the anode of a rechargeable lithium or sodium battery.

2. The use according to claim 1, wherein the carbon network comprising carbon nanofibers represents 10-100% by weight of the total mass of the anode, preferably more than 10% and less than 100% by weight.

3. 3. The use according to claim 1 or 2, wherein the carbon network comprises crystalline carbon nanofibers.

4. The use according to any one of claims 1 to 3, wherein the carbon nanofibers have an average fibre length of 30 to 10,000 nm.

5. 5. The use according to any one of claims 1 to 4, wherein the porous carbon network forms an intraparticle porous network, the carbon nanofibers are interconnected with other carbon nanofibers in the carbon network by chemical bonds via connections, the pores in the carbon network have an intraparticle pore diameter size of 5 to 150 nm using mercury intrusion porosimetry according to ASTM D4404-10, and the carbon nanofibers have an average aspect ratio of fiber length to thickness of at least 2, preferably with a d-spacing in the range of 0.340 to 0.5 nm.

6. 6. The use according to any one of claims 1 to 5, wherein the rechargeable lithium or sodium battery is suitable for and is provided in smartphones, laptops, digital cameras and camcorders, as an uninterruptible power supply (UPS), as energy storage in power generation equipment, in medical and communication systems, and in electric and / or hybrid vehicles.

7. A lithium or sodium battery anode comprising a porous, chemically interconnected carbon network comprising carbon nanofibers as the electrochemically active material.

8. 1. A lithium or sodium battery anode comprising a porous, chemically interconnected carbon network comprising carbon nanofibers, representing 10-100% by weight, preferably more than 10% by weight and less than 100% by weight, of the total mass of the anode.

9. 9. The lithium or sodium battery anode of claim 7 or 8, wherein the porous carbon network forms an intraparticle porous network, the carbon nanofibers are interconnected with other carbon nanofibers in the carbon network by chemical bonds through connections, the pores in the carbon network have intraparticle pore diameter sizes of 5 to 150 nm using mercury intrusion porosimetry according to ASTM D4404-10, and the carbon nanofibers have an average aspect ratio of fiber length to thickness of at least 2, preferably with a d-spacing of 0.340 to 0.5 nm.

10. The battery is a lithium battery, the anode contains 0.1 to 90% by weight of an additional active material, and the additional active material is graphite, silicon, a silicon-based compound (SiO 2 10. The battery anode of claim 8 or 9, wherein said anode is selected from the group consisting of tungsten, tin, tantalum, tantalum hydroxide, tin ...

11. The additional active material is silicon, a silicon-based compound (SiO 2 ) or a combination thereof, 2 ) or a combination thereof is mixed with the carbon network comprising the carbon nanofibers in the anode, or the carbon network comprising the carbon nanofibers is preferably made of silicon, the silicon-based compound (SiO 2 11. The battery anode of claim 10, wherein the battery anode is coated with a metal oxide, a fluorine atom ...

12. A rechargeable lithium or sodium battery comprising a battery anode according to any one of claims 7 to 11.

13. 13. The rechargeable lithium or sodium battery of claim 12, wherein the rechargeable battery is suitable for use in smartphones, laptops, digital cameras and camcorders, as uninterruptible power supplies (UPS), as energy storage in power generation equipment, in medical and communication systems, and in electric and / or hybrid vehicles.

14. Use of a carbon network according to any one of claims 1 to 6, the carbon network being obtained by a process for producing a crystalline carbon network by injecting a water-in-oil, oil-in-water or bicontinuous microemulsion c comprising metal catalyst nanoparticles into a reactor 3 containing a reaction zone 3b and a termination zone 3c at a temperature above 600°C, preferably above 700°C, more preferably above 900°C, even more preferably above 1000°C, more preferably above 1100°C, preferably at most 3000°C, more preferably at most 2500°C, most preferably at most 2000°C, in order to produce a crystalline carbon network e, transporting these networks e to the termination zone 3c and quenching or stopping the formation of the crystalline carbon network in the termination zone by spraying into water d, a lithium or sodium battery anode according to any one of claims 7 to 11 or a rechargeable lithium or sodium battery according to claim 12 or 13.

15. 14. A battery-powered device comprising a lithium or sodium battery anode according to any one of claims 7 to 11 or a rechargeable lithium or sodium battery according to claim 12 or 13.

16. 16. The device of claim 15, wherein the device is a smart phone, a laptop, an energy storage device of a power generation unit, or an electric or hybrid vehicle.

17. 1. A lithium or sodium battery anode comprising, as electrochemically active material, a porous, chemically interconnected carbon network comprising carbon nanofibers, representing 10-100% by weight, preferably more than 10% by weight and less than 100% by weight, of the total mass of the anode.

Citation Information

Patent Citations

  • Negative electrode material, negative electrode using the same, lithium ion battery using that negative electrode, and lithium-polymer battery

    JP2004186067A

  • Negative electrode material, negative electrode using the same, and lithium ion secondary battery using the negative electrode

    JP2004303613A

  • Electrode for secondary battery, its manufacturing method, and secondary battery

    JP2008277128A

  • Porous carbon nanotube microspheres and manufacturing method and use thereof, metallic lithium-framework carbon composite material and manufacturing method thereof, negative electrode, and battery

    JP2017517467A

  • carbon composite materials

    JP2019504435A