Submerged entry nozzle with continuous circumferential wavy ribs

The submerged nozzle with a wavy-trajectory annular protrusion sleeve effectively addresses vortex-induced erosion, enhancing service life and material efficiency by minimizing frictional forces.

JP2024540655APending Publication Date: 2024-10-31VESUVIUS GROUP SA
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024531069
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-24
Filing Date
2022-11-24
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing submerged nozzles in continuous casting processes suffer from high erosion rates due to frictional forces caused by molten metal vortices, despite the use of corrosion-resistant sleeves, as they do not effectively mitigate the vortex-induced erosion.

Method used

A submerged nozzle design featuring a corrosion-resistant sleeve with annular protrusions that follow a periodic wavy trajectory, reducing the amplitude and frequency of vortices, thereby minimizing frictional forces and erosion.

Benefits of technology

The design significantly reduces erosion rates by up to 98%, extending the nozzle's service life and reducing material usage, while maintaining operational efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024540655000001_ABST
    Figure 2024540655000001_ABST
Patent Text Reader

Abstract

The present invention relates to a submerged entry nozzle for casting molten metal into a mold, comprising a corrosion-resistant sleeve (2) made of a material resistant to erosion, provided on a tubular portion and extending along a longitudinal axis (Z), the corrosion-resistant sleeve comprising at least one annular projection (2p) extending radially outwardly over the entire circumference of the corrosion-resistant sleeve (2) beyond a recessed portion (2r) of the corrosion-resistant sleeve, the at least one annular projection (2p) following a periodic wavy trajectory oscillating between one or more peaks located closest to a first end and a corresponding number of one or more valleys located closest to a second end, the periodic wavy trajectory being defined by an amplitude (A) of more than 5 mm and a frequency (P) comprising 1 to 20 peak-valley-peak periods per 2π rad.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to submerged entry nozzles for continuous casting of molten metal, including submerged entry nozzles (SEN), submerged entry shrouds (SES), and monoblock tundish nozzle plates (MTNP), collectively referred to as submerged entry nozzles. Submerged entry nozzles according to various embodiments of the present invention are configured to be coupled to molten metal vessels, such as tundishes and ladles. [Background technology]

[0002] In a continuous metal forming process, a metal melt is transferred from one metallurgical vessel to another, a mold, or a die. For example, a ladle is filled with metal melt from a furnace and driven over a tundish to discharge the molten metal from the ladle through a ladle shroud into the tundish. The metal melt is then cast from the tundish outlet through an injection nozzle into a mold or die to continuously form slabs, billets, beams, thin slabs, and the like. To avoid contamination and oxidation of the metal melt, the nozzle directing the flow from the vessel to the other vessel or mold or die is submerged below the level of the molten metal. The flow of the metal melt from the ladle to the tundish and from the tundish to the mold or die is driven by gravity. The flow rate can be controlled by slide gates in fluid communication with the ladle and tundish outlets. The ladle slide gate can be used to control the flow rate from the ladle and also to interrupt the flow at a closed position. Similarly, a tundish slide gate can be used to control the flow rate from the tundish and interrupt the flow at a sealed location. Often the flow rate from the tundish is controlled by a stopper instead of a slide gate.

[0003] Mold fluxes are synthetic slags constituted by a complex mixture of oxides, minerals and carbonaceous materials applied at the meniscus height (i.e. at the surface of the liquid metal) in the mold or die to ensure various functions including heat insulation, prevention of reoxidation and trapping of inclusions. Mold fluxes can have various compositions but usually contain one or more selections of silica, calcia, sodium oxide, alumina and magnesia. Depending on their composition, mold fluxes are generally more corrosive to the refractory material forming the submerged nozzle than the liquid metal itself. In the following, the terms "slag" and "mold flux" are used interchangeably.

[0004] The process of continuous casting into a mold is very complex and involves many variables including the casting speed, the vibration characteristics of the mold, the steel type, and the mold dimensions, all of which affect the flow conditions of the metal from the SEN into the mold. As illustrated in FIG. 1, the liquid metal flowing out of the outlet of the SEN follows a complex flow pattern due to vortices that are formed when the metal, flowing rapidly out of the nozzle, strikes the mold wall. A portion of the molten metal (21) that reaches the cold wall of the mold (11) forms a shell (21s) of frozen metal. A further portion of the liquid metal flow is driven upwards and reaches the slag or mold flux (22) that contains the mold powder (22p) and molten mold powder (22m). This upward flow captures a portion of the mold flux (both mold powder and molten mold powder) and drives it downwards again at high speed along the outer wall of the SEN, creating significant frictional forces on the outer wall of the SEN. The impingement of the flows coming from different directions against the SEN can create vortices. In addition to the above discussed erosive action of the mold flux (22) on the outer wall of the SEN, these vortices add frictional erosion of the same outer wall, thus increasing the erosion rate of the outer wall of the SEN. The term "erosion" is subsequently used to encompass any loss or deterioration of material of the outer wall of the SEN caused by any one of friction, erosion, etc. The term "corrosion" is subsequently the process of chemical or electrochemical erosion of material resulting in the degradation of the material and its properties.

[0005] For the reasons mentioned above, a corrosion-resistant sleeve made of a material more resistant to corrosion than the refractory material forming the tubular body of the submerged nozzle is often provided on the tubular body and extends over the section of the tubular body corresponding to the location of the slag. Corrosion-resistant sleeves are well known in the art and examples are described, for example, in KR2012 / 0134451, which describes different types of corrosion-resistant sleeves, KR2006 / 0101717, which describes a corrosion-resistant sleeve that can be screwed onto the tubular part of the submerged nozzle, and KR2016 / 0060986, which describes the composition of a corrosion-resistant sleeve.

[0006] FR27163011 describes a movable corrosion-resistant sleeve provided with an internal thread configured to engage a mating external thread in the tubular part of the submerged nozzle. The position of the corrosion-resistant sleeve can thus be varied along the axis of the tubular part. JPS57115953 describes a corrosion-resistant sleeve made of two half shells that can be clamped onto the tubular part of the submerged nozzle and held in place by wires covered with amorphous refractory. CN207127252U describes a corrosion-resistant sleeve with protrusions that extend radially around the tubular part of the submerged nozzle. The protrusions are symmetrical with respect to a plane perpendicular to the longitudinal axis of the tubular part.

[0007] To date, the solutions proposed to reduce the erosion rate have mainly focused on finding materials that are more resistant to the aggressive environment of such systems. Although the use of ever more resistant materials for the erosion-resistant sleeve would be beneficial for the service life of the submerged nozzle, no solutions have been proposed in the art to reduce the magnitude of the frictional forces on these materials that form the erosion-resistant sleeve. There is a need for such a solution, which would allow even further extension of the service life of a submerged nozzle provided with a erosion-resistant sleeve made of any erosion-resistant material. Summary of the Invention

[0008] The immersion nozzles according to various embodiments of the present invention, on the one hand, · a corrosion-resistant sleeve surrounding the nozzle at the location where erosion is most severe, and on the other hand, · has enhanced resistance to erosion by at least one annular protrusion surrounding the corrosion-resistant sleeve according to a specific pattern to reduce the amplitude of the molten metal vortex that causes most of the erosion.

[0009] The object of the present invention includes an improved immersion nozzle for casting molten metal into a mold. According to at least one embodiment, the immersion nozzle comprises a tubular portion and a corrosion-resistant sleeve.

[0010] The tubular portion is made of a first material and extends along a longitudinal axis (Z) over a tube length (L1) between a first end and a second end. The tubular portion has an inner bore (1b) that extends along the longitudinal axis (Z) from an inlet that axially opens at or adjacent to the first end to at least one outlet that opens at or adjacent to the second end.

[0011] The corrosion-resistant sleeve is made of a second material that is different from the first material and is more resistant to erosion and corrosion. In other words, the second material is selected to be more resistant to erosion than the first material, and similarly, the second material is selected to be more resistant to corrosion than the first material. In one embodiment, the second material includes, for example, zirconia. The corrosion-resistant sleeve is provided on the tubular portion, extends circumferentially (e.g., circumscribes) over the entire circumference of the tubular portion, and extends along the longitudinal axis (Z) over a sleeve length (L2) that is shorter than the tube length (L1) (i.e., L2 < L1). The corrosion-resistant sleeve has a concave portion in the thinnest cross-section defined by a major diameter (DM) and a minor diameter (dm), and the ratio of the minor diameter to the major diameter (dm / DM) includes 0.7 to 1.0.

[0012] According to at least one embodiment, an immersion nozzle for casting molten metal into a mold is · A tubular portion (1) made of a first material, the tubular portion being · extending along a longitudinal axis (Z) over a tube length (L1) between a first end and a second end of the dipping nozzle, · having an inner bore (1b) extending along the longitudinal axis (Z) from an inlet (1i) that axially opens at or adjacent to the first end to at least one outlet (1o) that opens at or adjacent to the second end, the tubular portion (1), · A corrosion-resistant sleeve (2) made of a second material that is more resistant to erosion than the first material, the corrosion-resistant sleeve being · circumscribing the entire circumference of the tubular portion and extending along the longitudinal axis (Z) over a sleeve length (L2) that is shorter than the tube length (L1) (i.e., L2 < L1), · having a concave portion (2r) in the thinnest cross-section defined by a major diameter (DM) and a minor diameter (dm), the ratio of the minor diameter to the major diameter (dm / DM) being 0.7 to 1.0, the corrosion-resistant sleeve (2).

[0013] In at least one embodiment, the corrosion-resistant sleeve comprises at least one annular protrusion (2p) that extends radially outwardly beyond the concave portion (2r) by a protrusion distance (a) over the entire circumference of the corrosion-resistant sleeve (2), and the at least one annular protrusion (2p) follows a trajectory that reciprocates between one or more peak points that are closest to the first end and a corresponding number of one or more valley points that are closest to the second end. The at least one annular protrusion is clearly made of the second material and is preferably integral with the corrosion-resistant sleeve. The at least one annular protrusion preferably forms a closed loop around the tubular portion of the dipping nozzle of the present invention. The at least one annular protrusion is located on the outer surface of the corrosion-resistant sleeve. The at least one annular protrusion is designed to be in direct contact with the molten metal. The present invention provides a corrosion-resistant sleeve having at least one annular protrusion (2p) that extends radially outwardly beyond the recessed portion by a protrusion distance (a) around the entire circumference of the corrosion-resistant sleeve. The at least one annular protrusion (2p) follows a periodic wavy path that alternates between one or more peak points located closest to a first end and a corresponding number of one or more valley points located closest to a second end. The periodic wavy path is defined by an amplitude (A) and a frequency (P). A closed loop of annular protrusions has as many peak points as valley points. In other words, each peak point has only one peak point and one valley point corresponding thereto. The distance, measured along the longitudinal axis (Z), that separates the peak points from the valley points defines the amplitude (A) of the path followed by the annular protrusion. The number of peaks (or valleys) per revolution around the tubular portion defines the frequency (P) of the path followed by the annular projection.

[0014] The amplitude (A) of the periodic wavy path is greater than 5 mm (i.e., A>5 mm) as measured along the longitudinal axis (Z) between adjacent peaks and valleys. The frequency (P) of the periodic wavy path is defined as the number of peak-to-valley periods per 2π rad of the circumference, and includes 1 to 20 peak-valley-peak periods per 2π rad (i.e., P=1 to 20), and preferably includes 2 to 5.

[0015] The periodic wavy trajectory may be in the form of a rounded wavy trajectory, preferably a sinusoidal trajectory, or is in the form of a chevron trajectory, and the amplitude (A) measured between adjacent peaks and valleys of the annular protrusion is preferably constant for all adjacent peaks and valleys of the annular protrusion.

[0016] The submerged nozzle according to the invention may comprise one, two, three, four, five or more annular projections (2p) distributed along the longitudinal axis (Z). According to some embodiments, in case of two or more projections, the projections do not touch each other, are preferably identical to each other and more preferably parallel to each other.

[0017] The cross section along a plane containing the longitudinal axis (Z) of the one or more annular protrusions may be selected from among rounded, trapezoidal, square, or triangular.

[0018] The annular protrusion protrudes radially from the recess by a protruding distance (a) such that the ratio (a / Dra) of the protruding distance (a) of the annular protrusion to the average recess diameter (Dra) of the recess may be 1-30% (i.e., a / Dra=1-30%), preferably 5-20%, and the average recess diameter (Dra) is defined as the average of the major axis and minor axis of the recess (2r) (i.e., Dra=1 / 2(DM+dm)). For example, the annular protrusion protrudes radially from the recess by a protruding distance (a) of 5-50 mm (i.e., a=5-50 mm), preferably 8-25 mm.

[0019] The length ratio (L2 / L1) of the sleeve length (L2) to the tube length (L1) may comprise 10-50%, preferably 20-40%. At least two annular protrusions are preferably distributed over the sleeve length (L2) of the corrosion-resistant sleeve. The amplitude ratio (A / L2) of the amplitude (A) to the sleeve length (L2) may comprise 2%-100%, preferably 5%-50%.

[0020] The annular projection (2p) may have a width (b), measured along the longitudinal axis (Z), comprised between 5 and 50 mm, preferably between 10 and 40 mm, more preferably the width (b) is 25±10 mm.

[0021] The invention proposes a particular design of an anti-corrosion sleeve, which makes it possible to reduce the speed of the metal flowing along the wall of the submerged entry nozzle and thus the frictional forces. This has the advantage of reducing the erosion rate and therefore further extending the service life of the submerged entry nozzle. These and other advantages of the invention are explained in more detail in the following sections.

[0022] The invention also relates to a process for reducing erosion of a submerged entry nozzle during continuous casting of molten metal into a mould. The process comprises coupling the inlet of the submerged entry nozzle with the outlet engaged with the mould to a molten metal vessel and casting metal from the molten metal vessel through the bore of the submerged entry nozzle into the mould. The submerged entry nozzle of the process is as described above, with at least one annular projection being submerged below the height of the slag in the mould. In this way, the formation of vortices, which are the main cause of erosion, cannot continue to expand.

[0023] The present invention relates to A molten metal vessel containing molten metal and having a casting outlet; A mould or tundish located below the casting outlet along its longitudinal axis (Z), a submerged nozzle comprising an inner bore extending along a longitudinal axis (Z) from an inlet opening axially at or adjacent to a first end to at least one outlet opening at or adjacent to a second end, The present invention also relates to a casting installation, wherein the submerged entry nozzle is coupled to a molten metal vessel such that an inlet of the submerged entry nozzle is in fluid communication with the casting outlet and such that an outlet of the submerged entry nozzle is inside a mould or tundish.

[0024] The casting equipment of the present invention is characterized in that the submerged nozzle is as described above. [Brief description of the drawings]

[0025] [Figure 1] FIG. 1 shows a side cutaway view of a prior art (PA) submerged entry nozzle dispensing liquid metal into a mold with corresponding flow behavior and slag capture. [Diagram 2] Figure 2(a) shows a side cutaway view of a submerged entry nozzle (SEN) that dispenses liquid metal into a mold, according to various embodiments of the present invention, and Figure 2(b) shows a side cutaway view of a submerged entry nozzle (SEN) that dispenses liquid metal into a mold, according to various embodiments of the present invention, and a monoblock tundish nozzle plate (MTNP), according to various embodiments of the present invention. [Diagram 3] Figure 3(a) shows a cutaway side view and cross section (BB) of two embodiments of a submerged entry nozzle according to various embodiments of the present invention, and Figure 3(b) shows a cutaway side view and cross section (AA) of two embodiments of a submerged entry nozzle according to various embodiments of the present invention. [Figure 4] FIG. 4(a) shows a submerged nozzle with different number (N) of annular protrusions of different frequencies (P), amplitudes (A) on a corrosion-resistant sleeve of length (L2) measured along the longitudinal axis (Z) according to various embodiments of the present invention. FIG. 4(b) shows a submerged nozzle with different number (N) of annular protrusions of different frequencies (P), amplitudes (A) on a corrosion-resistant sleeve of length (L2) measured along the longitudinal axis (Z) according to various embodiments of the present invention. FIG. 4(c) shows a submerged nozzle with different number (N) of annular protrusions of different frequencies (P), amplitudes (A) on a corrosion-resistant sleeve of length (L2) measured along the longitudinal axis (Z) according to various embodiments of the present invention. FIG. 4(d) shows a partial cross-sectional view of a nozzle showing two annular protrusions according to various embodiments of the present invention. [Diagram 5] FIG. 5(a) shows an embodiment of a submerged nozzle with N=5 identical annular projections with a frequency P=1 according to at least one embodiment of the present invention, showing a perspective view. The wavy trajectory of the annular projections defines a chevron according to at least one embodiment of the present invention. FIG. 5(b) shows an embodiment of a submerged nozzle with N=5 identical annular projections with a frequency P=1 according to at least one embodiment of the present invention, showing an expanded circumference of the corrosion-resistant sleeve. The wavy trajectory of the annular projections defines a chevron according to at least one embodiment of the present invention. [Figure 6]Figure 6(a) shows an embodiment of a submerged nozzle with N=5 identical annular projections of frequency P=2, according to at least one embodiment of the present invention, showing a perspective view. The wavy trajectory of the annular projections defines chevrons, according to at least one embodiment of the present invention. Figure 6(b) shows an embodiment of a submerged nozzle with N=5 identical annular projections of frequency P=2, according to at least one embodiment of the present invention, showing an expanded circumference of the corrosion-resistant sleeve. The wavy trajectory of the annular projections defines chevrons, according to at least one embodiment of the present invention. [Figure 7] Figure 7(a) shows an embodiment of a submerged nozzle with N=5 identical annular projections with a frequency P=1 according to at least one embodiment of the present invention, showing a perspective view. The wavy trajectory of the annular projections is rounded (sinusoidal). Figure 7(b) shows an embodiment of a submerged nozzle with N=5 identical annular projections with a frequency P=1 according to at least one embodiment of the present invention, showing an expanded circumference of the corrosion-resistant sleeve. The wavy trajectory of the annular projections is rounded (sinusoidal). [Figure 8] Figure 8(a) shows an embodiment of a submerged nozzle with N=5 identical annular projections with a frequency P=2 according to at least one embodiment of the present invention, showing a perspective view. The wavy trajectory of the annular projections is rounded (sinusoidal) according to at least one embodiment of the present invention. Figure 8(b) shows an embodiment of a submerged nozzle with N=5 identical annular projections with a frequency P=2 according to at least one embodiment of the present invention, showing an expanded circumference of the corrosion-resistant sleeve. The wavy trajectory of the annular projections is rounded (sinusoidal) according to at least one embodiment of the present invention. [Figure 9]FIG. 9(a) shows an embodiment of a submerged nozzle with N=5 annular protrusions with different amplitudes (A) of frequency P=2 according to at least one embodiment of the present invention, showing a perspective view. The wavy trajectory of the annular protrusions defines a chevron according to at least one embodiment of the present invention. FIG. 9(b) shows an embodiment of a submerged nozzle with N=5 annular protrusions with different amplitudes (A) of frequency P=2 according to at least one embodiment of the present invention, showing an expanded circumference of the corrosion-resistant sleeve. The wavy trajectory of the annular protrusions defines a chevron according to at least one embodiment of the present invention. [Figure 10] Figure 10(a) shows various embodiments of the cross-sectional geometry of the annular protrusion. Figure 10(b) shows various embodiments of the cross-sectional geometry of the annular protrusion. Figure 10(c) shows various embodiments of the cross-sectional geometry of the annular protrusion. Figure 10(d) shows various embodiments of the cross-sectional geometry of the annular protrusion. Figure 10(e) shows various embodiments of the cross-sectional geometry of the annular protrusion. [Figure 11] FIG. 1 shows a graph of friction forces measured on the surface of the corrosion resistant sleeve of prior art first (a) and second (b) submerged nozzles compared to a third submerged nozzle (c) made in accordance with at least one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0026] As illustrated in FIG. 2, the submerged entry nozzle according to the invention is configured to cast molten metal (21) into a mold (11). The submerged entry nozzle according to the invention may also be used to fill a tundish from a ladle. The expression "submerged entry nozzle" is used herein to refer generically to any nozzle configured to dispense liquid metal through one or more outlets, the one or more outlets being submerged below the level of the liquid metal. This includes, among others, the submerged entry nozzle (SEN) (see FIG. 2(a)), the submerged entry shroud (SES) and the monoblock tundish nozzle plate (MTNP) (see FIG. 2(b)). As illustrated in FIG. 3(a) and FIG. 3(b), the submerged entry nozzle comprises a tubular portion (1) and a corrosion-resistant sleeve (2) provided on the tubular portion (1).

[0027] The tubular portion (1) is made of a first material, typically a refractory ceramic material that is thermally stable and permeable to gases released from the flowing metal. Materials used for the tubular portion (1) of the submerged nozzle are well known in the art and may include, for example, Al2O3-C based refractory materials. Other materials may include silicon dioxide, spinel, etc.

[0028] The tubular portion extends along a longitudinal axis (Z) over a tubular length (L1) between a first end and a second end. The tubular portion comprises an inner bore (1b) extending along the longitudinal axis (Z) from an inlet (1i) opening axially at or adjacent to the first end to at least one outlet (1o) opening at or adjacent to the second end. One outlet (1o) may open at the second end coaxially with the longitudinal axis (Z), as shown in FIG. 3(b), and / or one or more outlets (1o) may open radially, as shown in FIGS. 2, 3(a), and 4(a)-4(c). The present invention is not limited to any particular configuration of the one or more outlets (1o).

[0029] The corrosion-resistant sleeve (2) is made of a second material that is different from the first material and is more resistant to erosion and corrosion. The second material is well-known in the art and is described, for example, in JPS6397344 and KR1020160060986. The second material typically includes zirconia and sometimes includes other materials such as graphite and SiC. The corrosion-resistant sleeve, on the one hand, exhibits higher resistance to the corrosive action of the mold flux (or slag) (22) and, to a lesser extent, the corrosive action of the molten metal (21), and on the other hand, is sometimes mixed with the captured mold flux (22) formed on the surface of the wall of the immersion nozzle, and finally presents higher resistance to the erosive action of the vortex of the liquid metal that causes the frictional force leading to the deterioration of the immersion nozzle. The second material may include another material similar to zirconia, as long as the corrosion resistance of the second material is higher than that of the first material, as can be easily understood by those skilled in the art.

[0030] The corrosion-resistant sleeve (2) is provided on the tubular portion (1) and extends circumferentially over the entire circumference of the tubular portion. For example, the corrosion-resistant sleeve circumscribes the entire circumference of the tubular portion. Also, the corrosion-resistant sleeve extends along the longitudinal axis (Z) over a sleeve length (L2) that is shorter than the tube length (L1) (i.e., L2 < L1). KR2006 / 101717 describes a corrosion-resistant sleeve that can be reversibly screwed onto the tubular portion of the immersion nozzle. The corrosion-resistant sleeve (2) can be at the same height as the tubular portion (1). The corrosion-resistant sleeve (2) can be recessed with respect to the tubular portion (1), but preferably protrudes from the tubular portion (1) to form a small step of about 1 to 5 mm, preferably 2 to 3 mm.

[0031] The present invention focuses on submerged nozzles (and corresponding corrosion-resistant sleeves (2)) with a substantially circular or elliptical cross-section with an aspect ratio (dm / DM) of minor diameter (dm) to major diameter (DM) of 0.7 to 1.0 inclusive. The corrosion-resistant sleeve (2) has a concave portion (2r) of the thinnest cross-section defined by the minor diameter (dm) and the major diameter (DM). For a circular cross-section where DM=dm, to simplify reading, we have decided to refer to the diameter Dr=DM=dm. This is illustrated in the two cross-sectional cutaway views below in each of Figures 3(a) and 3(b), which show an elliptical cross-section of major and minor diameters (DM, dm) (top view) and a circular cross-section of diameter (Dr) (bottom view).

[0032] A further advantageous aspect of the invention is that the corrosion-resistant sleeve comprises at least one annular protrusion (2p) forming a rib extending radially outward beyond the recessed portion (2r) by a protrusion distance (a) around the entire circumference of the corrosion-resistant sleeve (2). The at least one annular protrusion (2p) follows a wavy path around the corrosion-resistant sleeve that shuttles between one or more peak points located closest to the first end and a corresponding number of one or more valley points located closest to the second end. In some embodiments, the wavy path can be periodic. In some embodiments, the periodic wavy path is a closed path that can be defined by an amplitude (A) and a frequency (P).

[0033] The amplitude (A) is the distance measured along the longitudinal axis (Z) separating a peak to a valley. If the period includes several valleys and peaks, the amplitude is defined as the maximum distance separating a valley from adjacent peaks in the period. The amplitude of the annular protrusion according to the present invention is greater than 5 mm (i.e., A>5 mm) measured along the longitudinal axis (Z) between adjacent peaks and valleys. The amplitude of the annular protrusion is preferably comprised between 10 mm and 450 mm, more preferably between 15 mm and 150 mm, more preferably between 20 mm and 100 mm, and most preferably between 25 mm and 75 mm.

[0034] The frequency (P) is defined as the number of peak-to-valley periods per 2π rad of the circumference. The frequency of the annular protrusion according to the present invention includes 1 to 20 peak-valley-peak periods per 2π rad (i.e., P=1 to 20), and preferably includes a frequency (P) of 2 to 10, more preferably 3 to 5. Figures 4(a), 5(a) and 5(b), and 7(a) and 7(b) show an annular protrusion (2p) with a frequency P=1. Figures 4(b), 6(a) and 6(b), and 8(a) and 8(b) show an annular protrusion (2p) with a frequency P=2, and Figure 4(c) shows an annular protrusion with a frequency P=10. Although frequency P=1 does not define a periodic wavy trajectory over 2π rad, as can be seen in the expanded representations of Figures 5(b), 7(b) and 9(b), it is considered herein as defining a periodic wavy trajectory over a number (n) of revolutions (n ​​2π rad). Preferably, for frequency P=1, the wavy trajectory must include at least one axis of symmetry parallel to the longitudinal axis (Z) to be considered periodic.

[0035] With respect to the geometry of the annular protrusions, each of the one or more annular protrusions defines a closed-loop periodic wavy trajectory. In a first embodiment, the periodic wavy trajectory may be in the form of a rounded wavy trajectory, as illustrated in Fig. 7(a), Fig. 7(b), and Fig. 8(a), Fig. 8(b). For example, the periodic wavy trajectory may be in the form of a sinusoidal trajectory. In an alternative embodiment, as illustrated in Fig. 5(a), Fig. 5(b), and Fig. 6(a), Fig. 6(b), the periodic wavy trajectory may be in the form of a chevron. In a preferred embodiment, the amplitude (A) measured between adjacent peaks and valleys of the annular protrusions is constant for all adjacent peaks and valleys of the annular protrusions. As mentioned above, for a frequency of P=1, it is preferred to have at least one axis of symmetry parallel to the longitudinal axis (Z) at an angle of π rad, as illustrated in Fig. 5(a), Fig. 5(b), and Fig. 7(a), Fig. 7(b). A period P=1, 2, 3, 4, or 5 is preferred for each rotation (2π rad).

[0036] As shown in Fig. 4(d), Fig. 10(a)-Fig. 10(e), the cross section of one or more annular protrusions (2p) along a plane including the longitudinal axis (Z) may be selected from among rounded, trapezoidal, square, or triangular. Other geometric shapes can also be envisaged. The protruding distance (a) of the annular protrusion (2p) is defined as the maximum distance separating the recessed portion (2r) directly adjacent to the annular protrusion (2p) and the tip portion furthest from said recessed portion for each azimuth angle around the longitudinal axis (Z). If the annular protrusion (2p) defines a linear ridge (e.g., having a rounded or triangular cross section as illustrated in Fig. 10(a) and Fig. 10(e)), the tip portion follows the ridge and defines a wavy geometric shape of the annular protrusion (2p). Where the cross section of the annular protrusion (2) defines a flat plateau parallel to the longitudinal axis as illustrated in Figures 10(b) to 10(d), the tip portion is the plateau itself and the wavy geometry of the annular protrusion (2p) follows a line contained in the plateau that is equidistant from the edge of the plateau.

[0037] In a preferred embodiment, the annular protrusion (2p) radially protrudes from the immediately adjacent recessed portion (2r) by a protrusion distance (a) such that the ratio (a / Dra) of the protrusion distance (a) of the annular protrusion (2p) to the average recessed portion diameter (Dra) of the recessed portion (2r) is comprised between 1 and 30% (i.e. a / Dra=1-30%), preferably between 5 and 20%. The average recessed portion diameter (Dra) is defined as the average of the major and minor diameters of the recessed portion (2r) (i.e. Dra=1 / 2(DM+dm)). For a submerged nozzle of circular cross section, Dra=Dr. The annular protrusion (2p) may radially protrude from the immediately adjacent recessed portion (2r) by a protrusion distance (a) comprised between 5 mm and 50 mm (i.e. a=5-50 mm), preferably between 8 mm and 25 mm. It should be noted that the protrusion distance (a) is not necessarily constant and may vary depending on the azimuth angle. For example, a mold will generally have a wide side and a narrow side, and in some cases the protrusion distance (a) may be lower facing the wide side to leave enough space between the wide side and the annular protrusion (2p) for the metal to flow freely between them. Alternatively, the protrusion distance (a) may be constant around the entire circumference of the annular protrusion (2p).

[0038] Referring to Figures 4(a) to 4(c), the amplitude ratio (A / L2) of the amplitude (A) to the sleeve length (L2) may include 2% to 100%, preferably 5% to 50%. When the submerged nozzle includes a single annular protrusion (2p), the amplitude may range throughout the aforementioned range. When the submerged nozzle includes two or more annular protrusions (2p), the amplitude ratio is preferably less than 40% (i.e., A / L2<40%). The length ratio (L2 / L1) of the sleeve length (L2) to the tube length (L1) may include 10 to 50%, preferably 20 to 40%.

[0039] As illustrated in Fig. 4(d), Fig. 10(a)-Fig. 10(e), the width (b) measured along the longitudinal axis (Z) of the annular protrusion (2p) may comprise 5-50 mm, preferably 10-40 mm, more preferably the width (b) is 25±10 mm. The width (b) is defined as the distance (b) measured along the longitudinal axis (Z) separating the two recessed portions (2r) located on each side of the annular protrusion. This also applies when the two recessed portions (2r) located on each side of the annular protrusion do not have the same diameter, as shown, for example, in Fig. 10(d). In a preferred embodiment, the width (b) of the annular protrusion (2p) is constant over its entire circumference. Alternatively, the width (b) of the annular protrusion (2p) may vary with the azimuth angle around the longitudinal axis (Z).

[0040] As described above, the second material can be any corrosion resistant material known in the art, such as those described in, for example, JPS6397344 and KR1020160060986. The second material typically includes zirconia, either pure or with other materials such as graphite and SiC.

[0041] Various embodiments have two or more annular protrusions (2p). Although FIG. 4(a) shows a submerged nozzle with a single annular protrusion (2p) in the corrosion-resistant sleeve (2), the submerged nozzle can have a number of annular protrusions greater than one (N≧1), for example as shown in FIGS. 4(b)-4(d), 5(a) and 5(b)-9(a) and 9(b). The number of annular protrusions (N) can be 2, 3, 4, 5, 6, or even more. The two or more annular protrusions (2p) are distributed along the length (L2) of the corrosion-resistant sleeve (2) without contacting each other. For example, in preferred embodiments illustrated in FIGS. 5(a) and 5(b)-8(a) and 8(b), at least two annular protrusions (2p), preferably all annular protrusions, are identical to each other. In the most preferred embodiment, the identical annular protrusions are arranged parallel to each other. The distance (d2p) separating the peak of a first annular projection from the peak of a second annular projection adjacent to the first annular projection may be constant over the entire circumference of the two annular projections (2p). All annular projections (2p) of a submerged nozzle are preferably separated from each other by the same distance (d2p).

[0042] Alternatively, the two or more annular protrusions are not identical and are not necessarily parallel to each other (see Figures 9(a) and 9(b)). The distance (d2p) separating two adjacent annular protrusions may vary with the azimuth angle relative to the longitudinal axis (Z). All annular protrusions may be separated by different distances (d2p) from each other.

[0043] At least two annular protrusions (2p) may be distributed over the sleeve length (L2) of the corrosion-resistant sleeve (2), when the length ratio (L2 / L1) of the sleeve length (L2) to the pipe length (L1) is comprised between 10% and 50%, preferably between 20% and 40%. The two or more annular protrusions (2p) are preferably distributed over 50% to 100%, preferably between 80% and 95% of the sleeve length (L2).

[0044] As shown in FIGS. 3(b) and 4(a), in addition to one or more annular protrusions (2p) of the corrosion-resistant sleeve (2), the immersion nozzle of the present invention may include one or more additional annular protrusions (1p) located within the section of the tubular portion (1) included between the corrosion-resistant sleeve (2) and one or more outlets (1o). The additional annular protrusions may have the same geometry as those considered with respect to the annular protrusions (2p) within the corrosion-resistant sleeve (2), and may differ only in material, which material is the same first material as that used in the tubular portion (1). The additional protrusions (1p) may be identical, and preferably may be parallel or different with respect to the annular protrusions (2p) within the corrosion-resistant sleeve (2).

[0045] The process for reducing erosion of the immersion nozzle may involve the following steps. The present invention also relates to a process for reducing erosion of an immersion nozzle during continuous casting of molten metal into a mold. The process comprises · coupling the inlet (1i) of the immersion nozzle to the molten metal container (31) with the outlet (1o) engaged with the mold (11), · casting metal from the molten metal container through the bore (1b) of the immersion nozzle into the mold.

[0046] The immersion nozzle comprises a corrosion-resistant sleeve provided with at least one annular protrusion (2p), and at least one annular protrusion (2p) is immersed below the height of the slag or mold flux (22) within the mold (11). The height of the slag is referred to herein as the meniscus.

[0047] The height of the meniscus changes during the casting operation. At all times during the casting operation, the distance separating the meniscus from the first annular protrusion (2p) closest to the inlet is preferably less than twice the average diameter (Dra) of the concave portion (2r) closest to the inlet (i.e., distance < 2Dra), preferably less than Dra (i.e., distance < Dra), where for an elliptical immersion nozzle, Dra = (DM + dm) / 2, and for a circular immersion nozzle having DM = dm = Dr, Dra = Dr.

[0048] Preferably, at least one annular protrusion (2p) is completely submerged below the meniscus throughout the entire casting operation.

[0049] The casting installation may include the following aspects: The present invention also relates to a casting installation comprising: (1) a molten metal vessel (31) containing molten metal and having a casting outlet (31o), (2) a mold (11) or a second metal vessel disposed below the casting outlet (31o) along a longitudinal axis (Z), and (3) a submerged nozzle comprising an inner bore (1b) extending along the longitudinal axis (Z) from an inlet (1i) opening axially at or adjacent to a first end to at least one outlet (1o) opening at or adjacent to a second end.

[0050] The submerged entry nozzle is coupled to the molten metal vessel such that its inlet (1i) is in fluid communication with the casting outlet (31o) and such that its outlet (1o) is inside the mould or second metal vessel, and in the installation of the present invention the submerged entry nozzle comprises a corrosion resistant sleeve provided with at least one annular projection (2p) as discussed above.

[0051] The molten metal container (31) is typically a tundish that casts metal into a mold through the submerged entry nozzle of the present invention, which may alternatively be coupled to a ladle that dispenses liquid metal into the tundish through the submerged entry nozzle.

[0052] The present invention makes it possible to extend the service life of a given size submerged nozzle, or conversely to maintain a similar service life with thinner walls and less material used. The corrosion caused by the mold flux "statically" contacting the wall of the submerged nozzle is slowed down by the use of a corrosion-resistant sleeve, as is generally known in the art. On the other hand, the present invention significantly increases the resistance of the submerged nozzle to erosion compared to prior art submerged nozzles, by significantly reducing the frictional forces caused by the vortexes of liquid metal and slag rubbing against the submerged nozzle. The most severe erosion is caused by the vortexes that drag the flux powder from the surface of the slag down against the submerged nozzle (see FIG. 1). This erosion process is particularly evident at the interface between the corrosion-resistant sleeve (2) and the tubular part (1) closest to the submerged outlet (1o). The annular protrusion (2p) of the submerged nozzle significantly reduces this interface erosion phenomenon.

[0053] Figure 11 graphs the frictional forces measured on the surface of the corrosion-resistant sleeve of the first (a) and second (b) submerged entry nozzles of the prior art and (c) the third submerged entry nozzle according to the invention. Figure 11 shows a graph of the frictional forces in the region of high powder concentration. The tubular parts (1) of all submerged entry nozzles have a circular cross section with the same diameter (D1). The corrosion-resistant sleeves of all submerged entry nozzles have the same sleeve length (L2) and are made of the same second material. The corrosion-resistant sleeves of the first and second submerged entry nozzles (a) and (b) of the prior art have a smooth cylindrical surface of a constant diameter, and (1) the corrosion-resistant sleeve (2) of the first submerged entry nozzle (a) of the prior art has a sleeve diameter (Dr) equal to the diameter of the tubular portion (Dr=D1), and (2) the corrosion-resistant sleeve (2) of the second submerged entry nozzle (b) of the prior art has a sleeve diameter (Dp) equal to the diameter of the tubular portion (D1) plus twice the projection distance (a) (Dp=D1+2a).

[0054] The corrosion-resistant sleeve (2) of the third submerged nozzle (c) of the present invention has N=5 identical annular protrusions (2p) with a frequency P=2 evenly distributed over the sleeve length (L2). The annular protrusions are separated from each other by recessed portions (2r) of the same diameter (Dr) (Dr=D1) as the tubular portion (1). The protrusions (2p) extend radially beyond the recessed portions (2r) by a distance (a), defining a protrusion diameter (Dp) equal to the sleeve diameter of the second submerged nozzle (b) of the prior art. The protrusion diameter (Dp) may be about 10-40% larger than the diameter (D1) of the tubular portion (i.e., Dp=110%D1-140%D1), preferably about 20-30% larger than D1 (i.e., Dp=120%D1-130%D1). The protrusion diameter (Dp) is not necessarily constant. On the one hand, the projection distance (a) may be constant, but the submerged entry nozzle may have an elliptical cross section, so that D1+2a varies in the same way as D1. On the other hand, the projection distance (a) itself may vary with the azimuth angle, so that even for a submerged entry nozzle with a circular cross section diameter, the projection diameter (Dp) may vary in the same way as the projection distance (a) varies, and in the case of a nozzle with an elliptical cross section, the tubular portion diameter (D1) also varies in the same way.

[0055] Tests were performed in a water model, with floating powder added to the meniscus to simulate mold flux. Sensors were applied on the outer surface of the SEN and the friction force was recorded as a function of time. Figure 11 shows an example of results measured as a function of time on the three SENs mentioned above. The following observations were made: With an average friction force of about 14 mN, the first prior art SEN having a smooth corrosion resistant sleeve (2) flush with the tubular section (see dotted curve (a) in Figure 11) recorded the highest level of friction force against the outer wall of the SEN and resulted in the highest erosion rate among the three SENs tested. The second prior art submerged entry nozzle (see dashed curve (b) in Figure 11), with the smooth corrosion resistant sleeve (2) protruding from the tubular portion by the protrusion distance (a), resulted in an average friction force of 9 mN, which was significantly lower than the first prior art submerged entry nozzle. The submerged entry nozzle of the present invention (see solid curve (c) in FIG. 11 ) having a corrosion-resistant sleeve (2) with N=5 annular protrusions (2p) separated from one another by recessed portions (2r) of the same height as the tubular portion and protruding from the recessed portions by a protrusion distance (a) resulted in a significantly lower average friction of about 0.3 mN, i.e. about 30 times lower than the second prior art submerged entry nozzle (curve (b)) and 40-50 times lower than the first prior art submerged entry nozzle (curve (a)).

[0056] Several conclusions can be drawn from the above results. First, by comparing the first prior art submerged entry nozzle with the second prior art submerged entry nozzle (curves (a) and (b) in FIG. 11), it can be concluded that by raising the corrosion-resistant sleeve by the protruding distance (a), the average friction force can be reduced by about 35%. This solution requires using a larger amount of the second material, which is more expensive than the first material. Second, by comparing the submerged entry nozzle according to the present invention with the first and second prior art submerged entry nozzles (curve (c) in FIG. 11 with curves (a) and (b)), by adding an annular protrusion (2p) according to the invention, the maximum thickness of which is equal to the protrusion distance (a), to the corrosion-resistant sleeve (2) of the first prior art submerged nozzle of the same height, the average friction force can be reduced by about 98%; It can be concluded that by removing parts of the second material from the raised corrosion-resistant sleeve (2) of the second prior art submerged nozzle (=curve (b)) to form annular protrusions (2p) according to the invention separated from each other by recessed parts (2r) of diameter (Dr) equal to the diameter (D1) of the tubular part (i.e. Dr=D1), the average friction force can be reduced by about 97%.

[0057] Due to such a drastic reduction in the erosive forces exerted on the outer wall of the submerged nozzle, the service life of the submerged nozzle according to the invention is significantly increased: since the erosion is slowed down, a smaller amount of second material is required.

[0058] The submerged entry nozzle of the present invention represents a breakthrough in the improvement of the erosion problems associated with the complex flow patterns followed by the liquid metal flowing out of the submerged entry nozzle into the mold (11). The average frictional forces exerted on the outer wall of the submerged entry nozzle have been virtually eliminated. Without wishing to be bound by any theory, it is believed that the one or more protrusions prevent the continuous growth of the strength of the vortex formed by the liquid metal as it impinges against the wall of the submerged entry nozzle as it flows towards and along said wall. In the case of a smooth surface, for example as in the case of the first prior art submerged entry nozzle in FIG. 11 (=curve (a)), a vortex formed at one point of the wall grows, being fed by the liquid metal flowing freely from a different direction. With a raised corrosion-resistant sleeve (for example as in curve (b) in FIG. 11), the flow of liquid metal flowing from the top to the bottom towards the outlet (1o) is deflected by the step of the protrusion distance (a) and cannot contribute as efficiently to the continuous growth of the vortex. However, in FIG. 11, after about 30 seconds, curves (a) and (b) can be seen to merge, suggesting that this vertical flow eventually stabilizes and becomes more steady, and therefore contributes steadily to the growth of any vortices thus formed.

[0059] The annular protrusions (2p) according to the invention are believed to deflect the liquid metal flowing from various directions. As they form a closed loop, they deflect the top-down vertical flow as discussed above for the raised corrosion-resistant sleeve, but due to their wavy geometry of amplitude (A), they also deflect the liquid metal flowing against the wall (i.e. transverse to the longitudinal axis (Z)). By deflecting the two main flow directions believed to be responsible for the formation and growth of vortices, the vortices remain small and isolated, and the effect on friction reduction is surprisingly clear, as shown by comparing curve (c) in FIG. 11 with curves (a) and (b) of the prior art.

[0060] The disruption of the primary flow is also believed to reduce the amount of mold flux (22), and in particular the amount of mold powder (22p), that is dragged into the liquid metal against the walls of the SEN, thereby reducing the amount of powder that needs to be replenished to maintain a stable mold flux (22) layer, reducing contamination of the metal parts, and, since the mold powder (22p) is highly corrosive, reducing the erosion rate of the SEN walls.

[0061] This significant reduction in erosion allows the thickness of the corrosion-resistant sleeve (2) required to maintain the required service life of the submerged nozzle to be correspondingly reduced, which results in savings in the production of metal sheets and parts, since the second material is generally more expensive than the first material of the tubular portion (1). [Table 1]

Claims

1. 1. A submerged entry nozzle for casting molten metal into a mould, comprising: A tubular portion (1) made of a first material, said tubular portion having: extending along a longitudinal axis (Z) over a tube length (L1) between a first end and a second end of the submerged nozzle; a tubular portion (1) comprising an inner bore (1b) extending along said longitudinal axis (Z) from an inlet (1i) opening axially at or adjacent said first end to at least one outlet (1o) opening at or adjacent said second end; A corrosion-resistant sleeve (2) made of a second material different from the first material and more resistant to erosion, said corrosion-resistant sleeve comprising: - circumscribing the entire circumference of said tubular portion and extending along said longitudinal axis (Z) over a sleeve length (L2) that is less than said tube length (L1) (i.e. L2<L1); a corrosion-resistant sleeve (2) having a recessed portion (2r) of thinnest cross-section defined by a major diameter (DM) and a minor diameter (dm), the ratio of said minor diameter to said major diameter (dm / DM) being between 0.7 and 1.0; 1. The submerged nozzle according to claim 1 , wherein the corrosion-resistant sleeve comprises at least one annular protrusion (2p) extending radially outwardly beyond the recessed portion (2r) by a protrusion distance (a) over the entire circumference of the corrosion-resistant sleeve (2), and wherein the at least one annular protrusion (2p) follows a trajectory around the tubular portion that shuttles between one or more peak points located closest to the first end and a corresponding number of one or more valley points located closest to the second end.

2. The trajectory is a wavy trajectory, or preferably a periodic wavy trajectory, the periodic wavy trajectory being an amplitude (A) measured along the longitudinal axis (Z) between adjacent peaks and valleys that exceeds 5 mm (i.e., A>5 mm); and The submerged nozzle according to claim 1, defined by a frequency (P) defined as the number of peak-to-valley periods per 2π rad of circumference, comprising from 1 to 20 peak-to-valley-peak periods per 2π rad (i.e. P=1 to 20), preferably wherein said frequency (P) is between 2 and 5 inclusive.

3. 3. The submerged nozzle according to claim 2, wherein an amplitude ratio (A / L2) of the amplitude (A) to the sleeve length (L2) is between 2% and 100%, preferably between 5% and 50%.

4. 4. The submerged nozzle according to claim 2 or 3, wherein the periodic wavy trajectory is in the form of a rounded wavy trajectory, preferably a sinusoidal trajectory, or a chevron trajectory, and wherein the amplitude (A), measured between adjacent peak and valley points of an annular projection (2p), is preferably constant for all adjacent peak and valley points of the annular projection (2p).

5. 5. The submerged nozzle according to any one of claims 1 to 4, comprising one, two, three, four, five or more annular protrusions (2p) distributed along the longitudinal axis (Z), and in case of two or more protrusions, said protrusions do not touch each other, are preferably identical to each other and more preferably parallel to each other.

6. 6. The submerged nozzle according to any one of the preceding claims, wherein a cross-section of the one or more annular projections (2p) taken along a plane containing the longitudinal axis (Z) is selected from one or more of the following: rounded, trapezoidal, square and triangular.

7. The submerged nozzle according to any one of claims 1 to 6, wherein the annular protrusion (2p) protrudes radially from the recessed portion (2r) by a protruding distance (a) such that a ratio (a / Dra) of the protruding distance (a) of the annular protrusion (2p) to an average recessed portion diameter (Dra) of the recessed portion (2r) is 1 to 30% (i.e., a / Dra = 1 to 30%), preferably 5 to 20%, and the average recessed portion diameter (Dra) is defined as the average of the major axis and the minor axis of the recessed portion (2r) (i.e., Dra = 1 / 2 (DM + dm)).

8. The submerged nozzle according to any one of claims 1 to 7, wherein the annular projection (2p) radially projects from the recessed portion (2r) by a projection distance (a) of 5 to 50 mm (i.e. a = 5 to 50 mm), preferably 8 to 25 mm.

9. 9. The submerged nozzle according to claim 1, wherein the length ratio (L2 / L1) of the sleeve length (L2) to the tube length (L1) is 10-50%, preferably 20-40%, and wherein at least two annular projections (2p) are distributed over the sleeve length (L2) of the corrosion-resistant sleeve (2).

10. 10. The submerged nozzle according to any one of the preceding claims, wherein the width (b) of the annular protrusion (2p), measured along the longitudinal axis (Z), is between 5 and 50 mm, preferably between 10 and 40 mm, more preferably said width (b) is 25±10 mm.

11. The submerged nozzle according to any one of claims 1 to 10, wherein the second material comprises zirconia.

12. The submerged nozzle according to any one of the preceding claims, wherein said at least one annular projection (2p) forms a closed loop around the tubular portion of the submerged nozzle.

13. 1. A process for reducing erosion of a submerged entry nozzle during continuous casting of molten metal into a mold, comprising: - coupling the inlet (1i) of the submerged entry nozzle to a molten metal container (31) with the outlet (1o) of said submerged entry nozzle in fluid communication with the mould (21); - casting metal from the molten metal container through the bore (1b) of the submerged nozzle into the mould, A process, characterized in that the submerged nozzle is as claimed in any one of the preceding claims, and in that at least one annular projection (2p) is immersed below the level of the slug (22) in the mould (11).

14. A casting facility comprising: a molten metal vessel (31) containing molten metal and having a casting outlet (31o); a mould (11) provided below the casting outlet (31o); a submerged nozzle comprising an inner bore (1b) extending along a longitudinal axis (Z) from an inlet (1i) opening axially at or adjacent to a first end to at least one outlet (1o) opening at or adjacent to a second end, the submerged entry nozzle is coupled to the molten metal vessel such that the inlet (1i) of the submerged entry nozzle is in fluid communication with the casting outlet (31o) and such that the outlet (1o) of the submerged entry nozzle is inside the mould; A casting facility, characterized in that the submerged nozzle is as defined in any one of claims 1 to 10.

Citation Information

Patent Citations

  • Installation for continuous casting of liquid metal, notably steel

    FR2763011A1

  • Immersion nozzle for continuous casting

    JP1982115953A

  • Dipping nozzle for cast steel

    JP1988303679A

  • Asymmetric slab nozzle and metallurgical assembly for casting metals including same - Patents.com

    JP2020519450A