Coil embedded inductor using ferrite core and its manufacturing method
The coil-embedded inductor with a ferrite core and divided ferrite structure addresses the limitations of conventional inductors by improving inductance, reducing size and weight, and enhancing heat dissipation, offering a more efficient and cost-effective solution.
Patent Information
- Application Number
- JP2024527416
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-10
- Filing Date
- 2022-07-22
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-07-22
AI Technical Summary
Conventional inductor manufacturing methods face limitations in achieving high inductance characteristics, are costly, and struggle with heat dissipation due to the use of soft magnetic molding liquids and plastic resin containers, which also hinder miniaturization and weight reduction.
A coil-embedded inductor using a ferrite core is designed with a ferrite core unit having a cavity filled with a magnetic molding liquid, where the ferrite core is divided into multiple parts with gaps to distribute magnetic flux density, and an insulating frame maintains insulation and heat dissipation, using a plastic resin with high thermal conductivity.
The design improves inductance characteristics, reduces volume and weight, and enhances heat dissipation, resulting in a more efficient and cost-effective inductor.
Smart Images

Figure 2024541324000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a coil-embedded inductor using a ferrite core and a manufacturing method thereof, and more particularly to a coil-embedded inductor using a ferrite core that can prevent local concentration of magnetic flux density and improve inductance characteristics, and a manufacturing method thereof. [Background technology]
[0002] Inductors, along with capacitors, are essential passive elements used in power conversion devices and play a role in reducing current ripple. These inductors are used in a variety of applications, including eco-friendly cars, solar inverters, ESS, and air conditioner inverters, and there is an increasing demand for high inductance characteristics, low loss, and compact size and weight reduction.
[0003] The conventional method for manufacturing inductors involves compressing and molding metal powder to form a magnetic core, and then inserting a wound coil. However, this method has limitations in terms of the shape and size of the powder magnetic core, which limits the ability to manufacture inductors of various shapes. Furthermore, the complexity of the processes from assembling the core to assembling the finished product increases the manufacturing costs of the inductors.
[0004] For this reason, research has recently been conducted into inductors manufactured by hardening a soft magnetic molding liquid. Inductors using such soft magnetic molding liquid have the advantage that they can be manufactured into a variety of shapes that are impossible to manufacture using conventional powder magnetic cores, and the manufacturing process is simple, making it possible to significantly reduce the manufacturing costs of the inductors.
[0005] However, since the magnetic permeability range of the soft magnetic molding liquid is 26 to 60μ, there is a limit in that it is not possible to achieve high inductance characteristics compared to general magnetic cores.
[0006] Furthermore, a separate container having the shape of the mold is required to inject the magnetic paste, which increases the volume and cost of the inductor.
[0007] In particular, plastic resin with high heat resistance is used as the material for the container, and in the case of an inductor in which the coil is embedded in such highly heat-resistant plastic resin, there is a problem in that it is difficult for the internal heat to be dissipated to the outside by the container made of plastic resin.
[0008] The contents described above as the background art are intended to provide an understanding of the background to the present invention, and should not be construed as an admission that they constitute prior art known to those of ordinary skill in the art. Summary of the Invention [Problem to be solved by the invention]
[0009] The present invention provides a coil-embedded inductor using a ferrite core that can prevent local concentration of magnetic flux density and improve inductance characteristics, and a method for manufacturing the same.
[0010] In particular, the present invention provides a coil-embedded inductor using a ferrite core, which prevents magnetic flux density from concentrating inside by forming a container made of a ferrite core on the outside where the magnetic flux density is relatively low, and which improves inductance characteristics while achieving miniaturization and weight reduction by filling a magnetic molding liquid for forming a magnetic body inside a container-shaped cavity made of a ferrite core, which has a smaller specific gravity than a magnetic body, and a manufacturing method thereof.
[0011] The technical problem that the present invention aims to achieve is not limited to the above-mentioned technical problem, and other technical problems not mentioned will be clearly understood by a person having ordinary skill in the art from the description of the present invention. [Means for solving the problem]
[0012] According to one embodiment of the present invention, a coil-embedded inductor using a ferrite core includes a ferrite core unit having an open side and a cavity formed therein, a coil unit having an insulating insert formed of an insulating plastic injection material on the surface of a wound coil and disposed in the cavity of the ferrite core unit, and a magnetic body formed by filling the remaining portion of the cavity of the ferrite core unit where the coil unit is not disposed with a magnetic molding liquid and hardening the magnetic body.
[0013] The ferrite core unit is divided into a plurality of ferrite cores, which are spaced apart from each other with gaps therebetween.
[0014] The plurality of ferrite cores are arranged along a magnetic path direction formed by the coil unit such that at least one gap formed in the ferrite core unit is formed along the magnetic path direction.
[0015] The ferrite core unit includes a first ferrite core that surrounds the circumferential direction in which the coil provided in the coil unit is wound, and a pair of second ferrite cores that surround both ends of the coil provided in the coil unit, and the first ferrite core and the pair of second ferrite cores are arranged at a distance from each other.
[0016] The insulating frame is formed of an insulating plastic injection material and is disposed in a gap formed in the ferrite core unit.
[0017] The insulating frame includes a frame body surrounding an outer peripheral surface of the first ferrite core, and a gap plate disposed in a gap between the first ferrite core and the second ferrite core.
[0018] The ferrite core unit has a relative permeability larger than that of the magnetic body.
[0019] The ferrite core unit has a relative magnetic permeability of 200μ or more, and the magnetic body has a relative magnetic permeability of 26 to 60μ.
[0020] The insulating insert of the coil unit is characterized in that it is made of a plastic resin having a thermal conductivity of 2 W / mk or more.
[0021] Meanwhile, a manufacturing method of a coil-embedded inductor using a ferrite core according to one embodiment of the present invention includes the steps of (I) preparing a magnetic molding liquid, (II) preparing a coil unit whose surface is insulated with plastic resin, (III) preparing a ferrite core unit having a cavity into which the magnetic molding liquid is filled, (IV) placing the coil unit in the cavity of the ferrite core unit, (V) filling the cavity of the ferrite core unit with the prepared magnetic molding liquid, and (VI) hardening the magnetic molding liquid filled in the ferrite core unit to form a magnetic body that is integrated with the ferrite core unit and the coil unit.
[0022] In the step (I), the magnetic molding liquid has a relative permeability of 26 to 60μ, and in the step (III), the ferrite core unit has a relative permeability of 200μ or more.
[0023] In the step (I), the density of the magnetic molding liquid is 5.5 to 6.5 g / cc.
[0024] The step (I) includes the steps of (I-1) preparing an organic vehicle by stirring a polymer resin and a solvent, and (I-2) preparing a magnetic molding liquid by kneading a magnetic powder with the organic vehicle.
[0025] In the process (I-1), the polymer resin includes one or more selected from the group consisting of an epoxy resin, an epoxy acrylate resin, an acrylic resin, a silicone resin, a phenoxy resin, and a urethane resin.
[0026] In the process (I-2), the magnetic powder includes one or more selected from the group consisting of pure iron, carbonyl iron, iron-silicon alloy (Fe-Si alloy), iron-silicon-chromium alloy (Fe-Si-Cr alloy), sand dust (Fe-Si-Al alloy), permalloy, molybdenum permalloy (Mo-permalloy) and amorphous powder.
[0027] In the process (I-2), the magnetic powder is characterized in that it is a mixture of two or more types of magnetic powders having different average particle sizes.
[0028] The (II) step includes: (II-1) preparing a wound coil; and (II-2) injecting plastic resin into a mold into which the prepared coil is inserted to prepare a coil unit.
[0029] In the process (II-2), the plastic resin is characterized in that it has a thermal conductivity of 2 W / mk or more.
[0030] In the step (II-2), the plastic resin is injected in at least two separate steps.
[0031] The step (III) includes the steps of: (III-1) preparing a ferrite core divided into a plurality of pieces; and (III-2) spacing the ferrite core divided into a plurality of pieces along the magnetic path direction formed by the coil unit so that at least one gap is formed along the magnetic path direction.
[0032] The step (III) further includes the steps of (III-3) preparing an insulating frame in which the multiple divided ferrite cores are fixed at a distance from each other, and (III-4) mounting the multiple divided ferrite cores at a distance from each other on the prepared insulating frame so that gaps are maintained between the multiple divided ferrite cores. Effect of the Invention
[0033] According to the embodiment of the present invention, the following effects can be expected.
[0034] First, by disposing a ferrite core with high magnetic permeability and low saturation magnetic flux density on the outside of an inductor with a relatively low magnetic flux density, the inductance characteristics can be improved compared to inductors manufactured by hardening only a conventional soft magnetic molding liquid.
[0035] Second, by replacing a separate non-magnetic container for filling the magnetic molding liquid with a ferrite core, a volume reduction effect can be expected.
[0036] Third, by using a ferrite core, which has a smaller specific gravity than metal powder, a weight reduction effect can be expected.
[0037] According to the embodiment of the present invention, the effects of the present invention are not limited to the above effects, but include all effects that can be inferred from the configuration of the invention described in the detailed description of the present invention or the claims. [Brief description of the drawings]
[0038] [Figure 1] 1 is a perspective view showing a coil-embedded inductor using a ferrite core according to an embodiment of the present invention; [Diagram 2] 1 is an exploded perspective view showing a coil-embedded inductor using a ferrite core according to an embodiment of the present invention; [Diagram 3] 1 is a perspective view showing steps for manufacturing a coil-embedded inductor using a ferrite core according to an embodiment of the present invention; [Figure 4] 1 is a procedural diagram showing steps for manufacturing a coil-embedded inductor using a ferrite core according to an embodiment of the present invention. [Diagram 5] 11 is a graph comparing inductance, which is a magnetic characteristic, of inductors according to a comparative example and an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0039] Hereinafter, the embodiments of the present invention will be described in more detail with reference to the accompanying drawings. However, the present invention is not limited to the embodiments disclosed below, and may be realized in various different forms. The embodiments are provided only to complete the disclosure of the present invention and to enable those skilled in the art to fully understand the scope of the invention. In the drawings, the same reference numerals refer to the same elements.
[0040] FIG. 1 is an oblique view showing a coil-embedded inductor using a ferrite core according to one embodiment of the present invention, FIG. 2 is an exploded oblique view showing a coil-embedded inductor using a ferrite core according to one embodiment of the present invention, and FIG. 3 is an oblique view showing the steps of manufacturing a coil-embedded inductor using a ferrite core according to one embodiment of the present invention.
[0041] As shown in the figure, the coil-embedded inductor using a ferrite core according to one embodiment of the present invention mainly includes a ferrite core unit 100, a coil unit 200, and a magnetic body 300.
[0042] The ferrite core unit 100 is a means having one open surface and a cavity 101 formed therein, and serving as a container when molding the magnetic body 300. In particular, the ferrite core unit 100 serves as a container in this embodiment and also serves to prevent magnetic flux density from concentrating locally in the inner region of the inductor, thereby improving the inductance characteristics.
[0043] Therefore, it is preferable that the ferrite core unit 100 has a smaller specific gravity and a larger relative magnetic permeability than a magnetic body.
[0044] From this point of view, it is preferable that the ferrite core 110 constituting the ferrite core unit 100 is manufactured using ferrite having a relative magnetic permeability of 200μ or more.
[0045] In particular, in order to improve the DC superimposition characteristics of the ferrite core 110, the ferrite core unit 100 divides the ferrite core 110 into a plurality of pieces, which are spaced apart while maintaining gaps between each piece.
[0046] In this case, it is preferable to arrange a plurality of divided ferrite cores 110 along the magnetic path direction so that at least one gap is formed in the ferrite core unit 100 along the magnetic path direction formed by the coil unit 200.
[0047] For example, as shown in FIG. 2, the ferrite core unit 100 includes a first ferrite core 111 that surrounds the circumferential direction in which the coil 210 provided in the coil unit 200 is wound, and a pair of second ferrite cores 112 that surround both ends of the coil 210 provided in the coil unit 200.
[0048] At this time, the first ferrite core 111 and the pair of second ferrite cores 112 are disposed at a distance from each other to form a gap 102 therebetween. For example, the gap 102 formed by separating the first ferrite core 111 and the pair of second ferrite cores 112 from each other may be set to 1 mm. Of course, the number and size of the gaps 102 are preferably determined according to the inductance characteristics required for the inductor.
[0049] In particular, in order to maintain the posture of the first ferrite core 111 and the pair of second ferrite cores 112 and stably form the gap 102, an insulating frame 120 formed from a plastic injection molding of an insulating material may be disposed in the gap 102 formed in the ferrite core unit 100.
[0050] In this case, the insulating frame 120 includes a frame body 121 surrounding the outer peripheral surface of the first ferrite core 111 , and a gap plate 122 disposed in the gap 102 between the first ferrite core 111 and the second ferrite core 112 .
[0051] The frame body 121 is formed in a plate shape bent into a shape of the letter “⊂”. In addition, a pair of gap plates 122 are integrally formed on the inner peripheral surface of the frame body 121.
[0052] In this case, it is preferable that the insulating frame 120 is formed by injecting plastic resin. Of course, the insulating frame 120 is not limited to plastic resin as long as it can maintain insulation.
[0053] Furthermore, a fastening portion 123 may be formed on the outer circumferential surface of the frame body 121, which allows the inductor to be fixed to a bolt within the power conversion device.
[0054] The coil unit 200 is constructed by forming an insulating insert 220 made of an insulating plastic injection molded on the surface of a wound coil 210.
[0055] At this time, the insulating insert 220 is preferably made of a plastic resin having a thermal conductivity of 2 W / mk or more, so that the heat generated from the coil during the operation of the inductor can be smoothly transferred to the outside and dissipated.
[0056] The magnetic body 300 is formed by filling the remaining portion of the cavity 101 of the ferrite core unit 100 where the coil unit 200 is not disposed with a magnetic molding liquid 310 and then hardening it.
[0057] Therefore, the magnetic body 300 is maintained in a state separated by the coil 210 and the insulating insert 220 that constitute the coil unit 200 .
[0058] At this time, the relative magnetic permeability of the magnetic body 300 is smaller than the relative magnetic permeability of the first ferrite core 111 and the second ferrite core 112 constituting the ferrite core unit 100. For example, the relative magnetic permeability of the magnetic body 300 is 26 to 60μ.
[0059] A method for manufacturing a coil-embedded inductor using a ferrite core configured as above will be described with reference to the drawings.
[0060] FIG. 3 is an oblique view showing the steps for manufacturing a coil-embedded inductor using a ferrite core according to one embodiment of the present invention, and FIG. 4 is a procedural diagram showing the steps for manufacturing a coil-embedded inductor using a ferrite core according to one embodiment of the present invention.
[0061] As shown in the figure, a manufacturing method for a coil-embedded inductor using a ferrite core according to one embodiment of the present invention includes the steps of (I) preparing a magnetic molding liquid, (II) preparing a coil unit whose surface is insulated with plastic resin, (III) preparing a ferrite core unit having a cavity into which the magnetic molding liquid is filled, (IV) placing the coil unit in the cavity of the ferrite core unit, (V) filling the cavity of the ferrite core unit with the prepared magnetic molding liquid, and (VI) hardening the magnetic molding liquid filled in the ferrite core unit to form a magnetic body that is integrated with the ferrite core unit and the coil unit.
[0062] Each of the above steps will now be described in more detail.
[0063] (I) Preparing a magnetic molding liquid The step of preparing a magnetic molding liquid is a step of preparing a magnetic molding liquid 310 for forming the magnetic body 300 in the internal region having a high magnetic flux density when manufacturing an inductor. The step of preparing the magnetic molding liquid is carried out through, for example, the following detailed steps, but it is not necessary to only go through such detailed steps.
[0064] (I-1) A process of preparing an organic vehicle by mixing a polymer resin and a solvent The polymer resin and the solvent are stirred to produce an organic vehicle. The polymer resin may be one or more polymer resins selected from the group consisting of, but not limited to, epoxy resins, epoxy acrylate resins, acrylic resins, silicone resins, phenoxy resins, and urethane resins.
[0065] The polymer resin functions as a binder for the magnetic powder, and such functions include, but are not limited to, a structural material that maintains the shape of the magnetic core, a function that provides chemical resistance to various organic solvents, a function that bonds and supports the magnetic powder and additives in the organic vehicle to each other so that they can maintain a desired shape, and a function that fills the spaces between the magnetic powder to increase the insulation of the magnetic body and increase the resistivity of the magnetic core to reduce eddy current loss in the magnetic body.
[0066] The solvent may include, but is not limited to, one or more selected from the group consisting of methyl cellosolve, ethyl cellosolve, butyl cellosolve, butyl cellosolve acetate, aliphatic alcohol, terpineol, dihydro-terpineol, ethylene glycol, ethylcarbitol, butyl carbitol, butyl carbitol acetate, texanol, methyl ethyl ketone, ethyl acetate, and cyclohexanone. The composition ratio of the polymer resin to the solvent is suggested to be 50-60 wt% of the polymer resin and 40-50 wt% of the solvent. If the polymer resin is less than 50wt% or the solvent is more than 50wt%, the binding function of the polymer resin will be reduced, and problems with the strength of the inductor may occur, such as partial detachment of the magnetic powder after the magnetic molding liquid hardens or partial cracks occurring in the magnetic core. If the polymer resin is more than 60wt% or the solvent is less than 50wt%, the amount of polymer resin will be excessive, and the magnetic molding liquid may leak out due to swelling of the polymer when it hardens.
[0067] Additionally, the components of the organic vehicle can affect the hardened density of the magnetic molding fluid; increasing the proportion of higher density material in the organic vehicle will increase the hardened density of the magnetic molding fluid, and increasing the proportion of lower density material in the organic vehicle will decrease the hardened density of the magnetic molding fluid.
[0068] The organic vehicle may contain one or more additives selected from the group consisting of a dispersant, a stabilizer, a catalyst, and a catalyst activator. If the polymer resin is not uniformly distributed in the solvent and may aggregate, a dispersant can be added to prevent such aggregation, if it is necessary to suppress chemical changes or state changes in the organic vehicle, a stabilizer can be added, and if the polymer resin and the solvent are not mixed smoothly, a catalyst or a catalyst activator can be used to promote the reaction.
[0069] The process of preparing the organic vehicle by stirring the polymer resin and the solvent (including the additive if an additive is added) can be carried out using a mechanical stirrer at a predetermined rpm for a predetermined time. There is no upper limit to the stirring time, but attention should be paid to the minimum time required to ensure uniform stirring, which varies depending on the type of polymer resin, the type of solvent, and the composition between the polymer resin and the solvent, and must be determined on a case-by-case basis. After stirring, the prepared organic vehicle may be further subjected to a process of filtering out impurities using a sieve and degassing. Degassing will be described in detail later.
[0070] (I-2) A process of preparing a magnetic molding liquid by kneading magnetic powder with an organic vehicle. The magnetic molding liquid is produced by kneading the magnetic powder with the organic vehicle. The magnetic powder and the organic vehicle are weighed and put into a kneader, and kneaded for a predetermined time so that the magnetic powder and the organic vehicle are uniformly mixed. There is no upper limit to the time required for the kneading process, but it is necessary to pay attention to the minimum time required to ensure uniform kneading, which varies depending on the type of magnetic powder, the ingredients and composition of the organic vehicle, and the composition between the magnetic powder and the organic vehicle, and must be determined on a case-by-case basis.
[0071] The magnetic powder may include, but is not limited to, one or more selected from the group consisting of pure iron, carbonyl iron, iron-silicon alloy (Fe-Si alloy), iron-silicon-chromium alloy (Fe-Si-Cr alloy), sandust (Fe-Si-Al alloy), permalloy, molybdenum permalloy (Mo-permalloy), and amorphous powder.
[0072] We suggest that the average particle size of the magnetic powder be 10 to 150 μm. If the average particle size of the magnetic powder exceeds 150 μm, the filling rate of the magnetic powder will decrease, resulting in a decrease in hardening density, and problems such as clogging of the nozzle of the dispenser when injecting the magnetic molding liquid may occur. If the average particle size of the magnetic powder is less than 10 μm, eddy current loss in the magnetic core may become an issue, and the organic vehicle may not be able to sufficiently fill the spaces between the magnetic powder particles, which may cause problems with the strength of the magnetic core.
[0073] The magnetic powder may be formed by mixing two or more kinds of magnetic powders having different average particle sizes. In this case, the magnetic powders having a smaller average particle size are located between the magnetic powders having a larger average particle size, and as a result, the hardening density of the magnetic molding liquid can be increased. The hardening density of the magnetic molding liquid will be described later. For mixing two or more kinds of magnetic powders having different average particle sizes, it is proposed to mix a first magnetic powder having an average particle size of 2 to 5 μm, a second magnetic powder having an average particle size of 10 to 20 μm, and a third magnetic powder having an average particle size of 50 to 150 μm. This is because the magnetic powders having a smaller average particle size are located between the magnetic powders having a larger average particle size.
[0074] The magnetic molding liquid preferably has a composition ratio of 94-98wt% magnetic powder and 2-6wt% organic vehicle. If the magnetic powder exceeds 98wt% or the organic vehicle is less than 2wt%, the amount of magnetic powder is excessive, and it may be impossible to manufacture the magnetic molding liquid by filling the magnetic powder, and the amount of organic vehicle is too small, so that the flowability of the magnetic molding liquid is low in terms of rheology when the magnetic molding liquid is injected into the case, and partial cracks may occur in the magnetic core, and the binding function of the polymer resin is reduced, so that the magnetic powder may partially detach after the magnetic molding liquid is hardened, and eddy current loss may increase in the magnetic core. If the magnetic powder is less than 94 wt% or the organic vehicle is more than 6 wt%, there are advantages in terms of rheology, but the amount of organic vehicle is excessive, reducing the loading amount of the magnetic powder, which may reduce the relative permeability of the magnetic core and reduce the inductance characteristics, and if the amount of polymer resin is excessive, the polymer may swell when the magnetic molding liquid hardens, causing the magnetic molding liquid to flow out of the case cavity.
[0075] In addition, the magnetic molding liquid produced with the above composition ratio preferably has a relative magnetic permeability of 26μ or more. This is because if the relative magnetic permeability of the magnetic molding liquid is less than 26μ, the inductance characteristics will decrease. On the other hand, if the relative magnetic permeability of the magnetic molding liquid exceeds 60μ, there is a drawback that the manufacturing cost of the magnetic molding liquid increases. For this reason, the relative magnetic permeability of the magnetic molding liquid is preferably about 26 to 60μ.
[0076] The reason for limiting the range of the relative magnetic permeability of the magnetic molding liquid in this way is that, within the range of use of the inductor of the present invention, it is required to have high inductance in the low current region and to maintain the inductance even in the high current region. This is in proportion to the efficiency characteristics of the system, and takes into consideration the relative magnetic permeability that may occur when manufacturing the magnetic molding liquid with the above composition ratio.
[0077] One of the performance requirements for magnetic molding liquid is the hardening density of the magnetic molding liquid, which is directly related to the composition ratio of the magnetic powder and the organic vehicle. Considering that the density of the magnetic powder is greater than that of the organic vehicle, the density of the magnetic molding liquid increases as the ratio of the magnetic powder increases, which means that the relative permeability of the magnetic molding liquid increases. Conversely, the density of the magnetic molding liquid decreases as the ratio of the magnetic powder decreases, which means that the relative permeability of the magnetic molding liquid decreases, but there is also a point that the eddy current loss decreases. In terms of such relative permeability and eddy current loss, we propose that the density of the magnetic molding liquid be 5.5 to 6.5 g / cc. This ensures high permeability overall and can reduce eddy current loss to a certain extent.
[0078] Before proceeding to the next step, a curing agent and / or a curing accelerator may be added to the magnetic molding liquid in order to accelerate the curing of the magnetic molding liquid, and the curing agent may be, but is not limited to, an aliphatic amine, modified aliphatic amine, aromatic amine, modified aromatic amine, acid anhydride, polyamide, or imidazole, which are amines, and the curing accelerator may be, but is not limited to, Lewis acid, alcohol, phenol, alkylphenol, carboxylic acid, tertiary amine, or imidazole. By using these, the time required for curing the magnetic molding liquid can be shortened.
[0079] Also, before proceeding to the next step, the magnetic molding liquid can be degassed. Degassing means removing air bubbles contained in the magnetic molding liquid, and this air bubble removal process can improve inductance loss. Also, air bubbles present in the magnetic molding liquid not only reduce the impact resistance of the magnetic core, but also induce cracks inside the magnetic core if moisture penetrates the air bubbles, so the degassing process of the magnetic molding liquid is very important. In a method of degassing the magnetic molding liquid, the magnetic molding liquid can be rotated and revolved using a commercially available agitator / defoamer to degas it, but the method is not limited to this.
[0080] (II) Preparing a coil unit
[0081] (II-1) The process of preparing the wound coil The coil 210 is prepared by winding into a circular, oval or rectangular shape. In this case, the shape and material of the coil 210 are not limited to a specific shape and material, and are preferably determined according to the shape of the inductor and the inductance characteristics required for the inductor.
[0082] (II-2) The process of preparing the coil unit The process of preparing the coil unit is a process of injecting plastic resin onto the surface of the prepared coil 210 so as to maintain insulation between the coil 210 and the magnetic molding liquid 310 when the magnetic molding liquid 310 is subsequently filled into the cavity of the ferrite core unit 100.
[0083] More specifically, the prepared coil 210 is inserted into a mold, and plastic resin is injected into the cavity of the mold to form an insulating insert 220 on the surface of the coil 210, thereby preparing the coil unit 200.
[0084] At this time, the injection process may be performed two or more times to inject the insulating insert 220 into a desired shape.
[0085] In addition, the plastic resin injected to mold the insulating insert 220 is preferably a heat dissipating plastic resin having a thermal conductivity of W / mk or more so that the heat of the coil 210 can be easily dissipated to the outside.
[0086] (III) Preparing a ferrite core unit This is a step of preparing a ferrite core unit 100 having a cavity 101 formed therein into which the magnetic molding liquid 310 is to be filled.
[0087] At this time, the ferrite core unit 100 serves as a container into which the magnetic molding liquid 310 is filled.
[0088] (III-1) The process of preparing the ferrite core The ferrite core 110 is prepared by dividing it into a plurality of pieces. At this time, the ferrite core 110 is made of a material that is generally used for inductors, and detailed description of the characteristics and manufacturing method of each piece will be omitted.
[0089] However, the ferrite core 110 prepared in this embodiment is prepared to achieve magnetic properties that cannot be achieved by the magnetic molding liquid 310, and it is important that the ferrite core 110 has a larger relative permeability than the magnetic molding liquid 310. For example, the relative permeability of the ferrite core 110 is preferably 200μ or more. On the other hand, the upper limit value for the relative permeability of the ferrite core 110 is not particularly limited.
[0090] (III-2) The process of arranging the divided ferrite cores at intervals In order to improve the DC superimposition characteristics, the ferrite core 110 is divided into a plurality of pieces, which are spaced apart while maintaining gaps 102 between each piece.
[0091] In this case, it is preferable that the divided ferrite core 110 is arranged at a distance from one another in a state where it is divided into multiple pieces along the magnetic path direction formed by the coil unit 200 so that at least one gap 102 is formed along the magnetic path direction.
[0092] For example, the ferrite core 110 includes a first ferrite core 111 arranged in an approximate "⊂" shape surrounding the circumferential direction in which the coil 210 provided in the coil unit 200 is wound, and a pair of flat second ferrite cores 112 surrounding both ends of the coil 210 provided in the coil unit 200.
[0093] Therefore, by arranging the second ferrite core 112 at both ends of the first ferrite core 111, one side is opened while maintaining the shape of a substantially rectangular parallelepiped, and a cavity 101 can be formed inside.
[0094] (III-3) Preparation of the insulating frame The process of preparing the insulating frame is a process of preparing the insulating frame 120 for fixing the ferrite core 110 divided into a plurality of pieces in a spaced apart state.
[0095] In this case, the insulating frame 120 may be provided in a shape including a frame main body 121 surrounding the outer peripheral surface of the first ferrite core 111 and a gap plate 122 arranged in the gap 102 between the first ferrite core 111 and the second ferrite core 112.
[0096] (III-4) Attaching the ferrite core to the insulating frame The divided ferrite cores 110 are attached to a prepared insulating frame 120 at intervals so that gaps 102 are maintained between the divided ferrite cores 110.
[0097] At this time, in order to attach the ferrite core 110, an epoxy or silicone adhesive may be injected into the attachment portion with the insulating frame 120. The adhesive may be injected into the joining surface of the ferrite core 110 using a syringe or a dispenser, but other methods are not excluded. The adhesive is preferably cured in a curing oven at 80° C. or higher, or left at room temperature to be naturally cured.
[0098] (IV) placing the coil unit in the cavity of the ferrite core unit; This is a step of placing the prepared coil unit 200 in the cavity 101 formed in the ferrite core unit 100. Most of the coil unit 200 is placed in the cavity 101 formed in the ferrite core unit 100, and both side ends of the coil 210 constituting the coil unit 200 are placed so as to be exposed to the outside of the cavity 101 formed in the ferrite core unit 100 for connection to other components.
[0099] (V) A step of filling the cavity of the ferrite core unit with the prepared magnetic molding liquid. The step of filling the magnetic molding liquid is a step of filling the cavity 101 formed in the ferrite core unit 100 with the prepared magnetic molding liquid 310 in order to integrate the magnetic molding liquid 310 and the ferrite core unit 100 together.
[0100] At this time, the magnetic molding liquid 310 is injected into the cavity 101 formed in the ferrite core unit 100 through an upper portion of the cavity 101. The magnetic molding liquid 310 may be injected into the cavity 101 of the ferrite core unit 100 using a pump and a tube or a dispenser, but other methods are not excluded.
[0101] (VI) Forming a magnetic material This is a step in which the magnetic molding liquid 310 filled in the ferrite core unit 100 is hardened to form the magnetic body 300 that is integrated with the ferrite core unit 100 and the coil unit 200.
[0102] The method for curing the magnetic molding liquid 310 is preferably vacuum curing, in which the magnetic molding liquid 310 is cured in a vacuum atmosphere, but is not limited thereto.
[0103] When the magnetic molding liquid 310 is evacuated, there is an advantage that air bubbles in the magnetic molding liquid can be removed by appropriately setting the temperature and curing time.
[0104] After the inductor is prepared by the above method, the enamel coating on the coil end is removed to form a current-carrying portion of the coil to form a current-carrying path for connecting the inductor to a circuit component. The coating can be removed by chemical or mechanical methods. The coil end can then be attached to the circuit component by welding, soldering, bolts, or other connections, or can be made to be flexibly attached by connecting coated stranded wires.
[0105] The present invention will be described below with reference to examples and comparative examples.
[0106] [Example: Manufacturing of coil-embedded inductor using magnetic molding liquid with magnetic permeability of 35μ and ferrite core with magnetic permeability of 2000μ] To manufacture a coil-embedded inductor with an inductance characteristic of 1,000 μH, a magnetic molding liquid with a relative permeability of 35 μ was first prepared by kneading epoxy resin, iron-silicon-chromium alloy powder, sand dust powder, and other magnetic powders (one or more selected from the above-mentioned possible magnetic powders).
[0107] In addition, a square coil with 9.0 mm (width) x 0.5 mm (thickness) and 36 turns was prepared and inserted using plastic injection molding to prepare a coil unit. After that, an insulating frame was prepared to form a gap of 1 mm in the magnetic path direction, and five ferrite cores with a relative magnetic permeability of 2,000 μ were attached to the insulating frame.
[0108] Thereafter, the coil unit was placed in the cavity of the ferrite core unit, and the magnetic molding liquid was injected and filled into the cavity. The ferrite core unit filled with the magnetic molding liquid was then placed in a vacuum oven, and the magnetic molding liquid was vacuum cured.
[0109] As a result, a coil-embedded inductor measuring 68 mm (width) × 52 mm (length) × 48 mm (height) was manufactured.
[0110] [Comparative example: Coil-embedded inductor manufactured using soft magnetic molding liquid with relative permeability of 60μ] To manufacture an inductor (comparison example) with an inductance characteristic of 900 μH, an inductor of the same size and volume as the example was manufactured in the same manner as the example by injecting and applying a magnetic molding liquid with a relative permeability of 60 μ to the entire plastic case.
[0111] [Experimental example: Inductance measurement] The inductance of the coil-embedded inductors manufactured in the examples and comparative examples was measured using a precision LCR meter (Keysight E4980A), and the results are shown in FIG.
[0112] As can be seen from FIG. 5, compared to the comparative example, the embodiment ensures high inductance even at low currents, and it was confirmed that high inductance can be ensured in most sections up to the maximum load current region.
[0113] Therefore, it was confirmed that by using a coil-embedded inductor in which a magnetic molding liquid is applied inside a ferrite core unit, it is possible to manufacture a coil-embedded inductor having a higher inductance than an inductor that uses only a magnetic molding liquid.
[0114] Although the present invention has been described with reference to the accompanying drawings and the above preferred embodiments, the present invention is not limited thereto, but is limited by the following claims. Therefore, a person having ordinary skill in the art may modify and change the present invention in various ways without departing from the technical spirit of the following claims. [Explanation of symbols]
[0115] 100: Ferrite core unit 101: Cavity 102: gap 110: ferrite core 111: First ferrite core 112: Second ferrite core 120: Insulating frame 121: Frame body 122: gap plate 123: fastening part 200: Coil unit 210: Coil 220: Insulating insert 300: Magnetic material 310: Magnetic molding fluid
Claims
1. A ferrite core unit having an open surface and a cavity formed therein; A coil unit in which an insulating insert made of an insulating plastic injection material is formed on a surface of a wound coil and placed in a cavity of the ferrite core unit; and a magnetic body formed by filling a remaining portion of the cavity of the ferrite core unit where the coil unit is not disposed with a magnetic molding liquid and hardening the magnetic body. A coil embedded inductor using a ferrite core.
2. The ferrite core unit is divided into a plurality of ferrite cores, which are spaced apart from each other with gaps maintained therebetween. A coil-embedded inductor using the ferrite core according to claim 1.
3. The plurality of ferrite cores are arranged along a magnetic path direction such that at least one gap is formed in the ferrite core unit along the magnetic path direction formed by the coil unit. A coil-embedded inductor using the ferrite core according to claim 2.
4. The ferrite core unit is A first ferrite core that surrounds the circumferential direction in which the coil provided in the coil unit is wound; a pair of second ferrite cores surrounding both ends of a coil provided in the coil unit; The first ferrite core and the pair of second ferrite cores are spaced apart from each other. A coil-embedded inductor using the ferrite core according to claim 3.
5. An insulating frame formed of an insulating plastic injection material is disposed in the gap formed in the ferrite core unit. A coil-embedded inductor using the ferrite core according to claim 4.
6. The insulating frame includes: a frame body surrounding an outer peripheral surface of the first ferrite core; a gap plate disposed in the gap between the first ferrite core and the second ferrite core. A coil-embedded inductor using the ferrite core according to claim 5.
7. The relative permeability of the ferrite core unit is greater than the relative permeability of the magnetic body. A coil-embedded inductor using the ferrite core according to claim 1.
8. The relative permeability of the ferrite core unit is 200μ or more, The relative magnetic permeability of the magnetic material is 26 to 60μ. A coil embedded inductor using the ferrite core according to claim 7.
9. The insulating insert of the coil unit is formed of a plastic resin having a thermal conductivity of 2 W / m-k or more. A coil-embedded inductor using the ferrite core according to claim 1.
10. (I) providing a magnetic molding liquid; (II) preparing a coil unit having a surface insulated with plastic resin; (III) preparing a ferrite core unit having a cavity formed therein to be filled with the magnetic molding liquid; (IV) placing the coil unit in a cavity of the ferrite core unit; (V) filling the cavity of the ferrite core unit with the prepared magnetic molding liquid; (VI) hardening the magnetic molding liquid filled in the ferrite core unit to form a magnetic body integrated with the ferrite core unit and the coil unit.
4. A method for manufacturing an embedded coil inductor using a ferrite core.
11. In the step (I), the relative permeability of the magnetic molding liquid is 26 to 60 μm; In the step (III), the relative permeability of the ferrite core unit is 200μ or more. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 10.
12. In step (I), the density of the magnetic molding liquid is 5.5 to 6.5 g / cc. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 11.
13. The step (I) comprises: (I-1) preparing an organic vehicle by stirring a polymer resin and a solvent; (I-2) a step of kneading the magnetic powder with the organic vehicle to prepare a magnetic molding liquid. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 10.
14. In the process (I-1), The polymer resin includes one or more selected from the group consisting of epoxy resin, epoxy acrylate resin, acrylic resin, silicone resin, phenoxy resin, and urethane resin. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 13.
15. In the process (I-2), The magnetic powder includes one or more selected from the group consisting of pure iron, carbonyl iron, iron-silicon alloy (Fe-Si alloy), iron-silicon-chromium alloy (Fe-Si-Cr alloy), sand dust (Fe-Si-Al alloy), permalloy, molybdenum permalloy (Mo-permalloy) and amorphous powder. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 13.
16. In the process (I-2), The magnetic powder is a mixture of two or more types of magnetic powder having different average particle sizes. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 13.
17. The step (II) comprises: (II-1) preparing a wound coil; (II-2) A step of preparing a coil unit by injecting plastic resin into a mold into which the prepared coil is inserted. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 10.
18. In the step (II-2), the plastic resin has a thermal conductivity of 2 W / m-k or more. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 17.
19. In the step (II-2), the plastic resin is injected in at least two separate steps. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 17.
20. The step (III) comprises: (III-1) preparing a ferrite core divided into a plurality of pieces; (III-2) A step of disposing a ferrite core divided into a plurality of pieces along a magnetic path direction formed by the coil unit so that at least one gap is formed along the magnetic path direction. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 10.
21. The step (III) comprises: (III-3) preparing an insulating frame for fixing the plurality of divided ferrite cores in a spaced apart state; (III-4) A process of mounting the divided ferrite cores on the prepared insulating frame at a distance so that gaps are maintained between the divided ferrite cores. A method for manufacturing a coil-embedded inductor using the ferrite core according to claim 19.
Citation Information
Patent Citations
Inductor
JP1983040814U
Coil-sealing resin-forming reactor and its manufacturing method
JP2007027185A
Manufacturing method of coil-embedded inductor using soft magnetic molding liquid and its coil-embedded inductor
JP2018514937A