Quasi-global cathode contact method for advanced patterning
The subpixel circuit with inorganic overhang structures and contact overhangs addresses leakage issues in OLED displays, enhancing pixel density and performance by reducing leakage and ensuring accurate material deposition.
Patent Information
- Application Number
- JP2024533030
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-06-03
- Filing Date
- 2022-11-30
- Publication Date
- 2024-11-08
Smart Images

Figure 2024541664000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD OF THE DISCLOSURE The embodiments described herein relate generally to displays. More particularly, the embodiments described herein relate to sub-pixel circuits and methods of forming sub-pixel circuits that may be used in displays, such as organic light emitting diode (OLED) displays. [Background technology]
[0002] Input devices, including display devices, can be used in a variety of electronic systems. An organic light-emitting diode (OLED) is a light-emitting diode (LED) in which an emissive electroluminescent layer is a film of organic compounds that emits light in response to an electric current. An OLED device is classified as a bottom-emitting device if the emitted light passes through a transparent or semi-transparent bottom electrode and a substrate on which the panel is fabricated. A top-emitting device is classified based on whether the light emitted from the OLED device exits through a lid that is added after the device is fabricated. OLEDs are currently used to create display devices in many electronic devices. An OLED device includes a number of subpixels defined by adjacent pixel-defining layer (PDL) structures. Each subpixel has an anode, an organic light-emitting diode (OLED) material disposed on the anode, and a cathode disposed on the OLED material. To power one or more subpixels, a local auxiliary grid is used to distribute the input current to the cathode of one or more subpixels. The use of a local auxiliary grid can increase leakage current. There remains a need for improved cathode contacts to improve OLED performance. Thus, there is a need in the art for sub-pixel circuits and methods of forming sub-pixel circuits that increase pixels per inch and improve OLED performance. Summary of the Invention
[0003] In one embodiment, a sub-circuit is provided. The sub-circuit comprises a metal grid disposed on an anode definition layer (ADL). The ADL exposes an anode disposed on a substrate. The sub-circuit further comprises an inorganic overhang structure disposed on the metal grid. Adjacent ADLs define a plurality of sub-pixels of the sub-circuit. Each sub-pixel of the plurality of sub-pixels includes an anode defined by the ADL, an organic light emitting diode (OLED) material disposed on and in contact with the anode, and a cathode disposed on the OLED material. The sub-circuit further comprises at least one contact overhang disposed on each auxiliary cathode line of the metal grid. The contact overhang is disposed between two sub-pixels of the plurality of sub-pixels, and the cathode contacts the contact overhang.
[0004] In another embodiment, a device is provided. The device comprises a substrate, a plurality of metal layers disposed on the substrate, and an anode definition layer (ADL) disposed on the plurality of metal layers and the substrate. The ADL defines an anode of the device. The device further comprises a metal grid disposed on the ADL. Adjacent ADLs define subpixels of the device. The device further comprises a plurality of subcircuits. Each subcircuit includes a metal grid disposed on the ADL, an inorganic overhang structure disposed on the metal grid, and a first plurality of subpixels. Each subpixel of the first plurality of subpixels includes an anode defined by the ADL, an organic light emitting diode (OLED) material disposed on and in contact with the anode, and a cathode disposed on the OLED material. The device further comprises at least one contact overhang disposed on each auxiliary cathode line of the metal grid. The contact overhang is disposed between two subpixels of the first plurality of subpixels, and the cathode contacts the contact overhang.
[0005] In yet another embodiment, a device is provided. The device comprises a substrate, a plurality of metal layers disposed on the substrate, and an anode-defining layer (ADL) disposed on the plurality of metal layers and the substrate. The ADL defines an anode of the device. The device further comprises a metal grid disposed on the ADL. Adjacent ADLs define subpixels of the device. The device further comprises a plurality of subcircuits. Each subcircuit includes a metal grid disposed on the ADL, an inorganic overhang structure disposed on the metal grid, and a first plurality of subpixels. Each subpixel of the first plurality of subpixels includes an anode defined by the ADL, an organic light-emitting diode (OLED) material disposed on and in contact with the anode, and a cathode disposed on the OLED material. The device further comprises at least one contact overhang disposed on each auxiliary cathode line of the metal grid. The contact overhang is disposed between two subpixels of the first plurality of subpixels, and the cathode contacts at least a stem portion of the at least one contact overhang. The at least one contact overhang includes a contact overhang ratio defined as a ratio of the overhang height to the overhang depth, the contact overhang ratio being from about 1.0:1.0 to about 1.0:1.5.
[0006] So that the foregoing features of the present disclosure can be understood in detail, the disclosure briefly summarized above may be more particularly described with reference to embodiments, some of which are illustrated in the accompanying drawings, in which it is noted, however, that the accompanying drawings depict only exemplary embodiments and therefore should not be considered as limiting the scope of the present disclosure, as other equally effective embodiments may be permitted. [Brief description of the drawings]
[0007] [Figure 1A] 1 is a schematic cross-sectional view of a sub-pixel circuit according to embodiments described herein. [Figure 1B] 1 is a schematic cross-sectional view of a sub-pixel circuit according to embodiments described herein. [Figure 1C] 1 is a schematic cross-sectional view of a sub-pixel circuit according to embodiments described herein. [Figure 1D] 1 is a schematic cross-sectional view of a sub-pixel circuit according to embodiments described herein. [Figure 1E] FIG. 2 is a schematic top view of a sub-pixel circuit according to embodiments described herein. [Figure 2A] 2 is a schematic cross-sectional view of a portion of a sub-pixel circuit according to embodiments described herein. [Figure 2B] 2 is a schematic cross-sectional view of a portion of a sub-pixel circuit according to embodiments described herein. [Diagram 3] FIG. 2 is a schematic top view of a sub-pixel circuit according to embodiments described herein. [Figure 4] FIG. 5 is a flow diagram of a method for forming the sub-pixel circuits shown in FIGS. 5A-5E and 6A-6B according to embodiments described herein. [Figure 5A] 4A-4D are schematic top-view diagrams of sub-pixel circuits during methods according to embodiments described herein. [Figure 5B] 4A-4D are schematic top-view diagrams of sub-pixel circuits during methods according to embodiments described herein. [Figure 5C] 4A-4D are schematic top-view diagrams of sub-pixel circuits during methods according to embodiments described herein. [Figure 5D] 4A-4D are schematic top-view diagrams of sub-pixel circuits during methods according to embodiments described herein. [Figure 5E] 4A-4D are schematic top-view diagrams of sub-pixel circuits during methods according to embodiments described herein. [Figure 6A] 1A-1C are schematic cross-sectional views of a sub-pixel circuit during a method according to embodiments described herein. [Figure 6B] 1A-1C are schematic cross-sectional views of a sub-pixel circuit during a method according to embodiments described herein. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] For ease of understanding, wherever possible, the same reference numerals have been used to designate identical elements that are common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.
[0009] The embodiments described herein generally relate to displays. More particularly, the embodiments described herein relate to subpixel circuits and methods of forming subpixel circuits that can be used in displays, such as organic light-emitting diode (OLED) displays. In one embodiment that can be combined with other embodiments described herein, the display is a top-emission (TE) OLED display. In another embodiment that can be combined with other embodiments described herein, the display is a passive matrix (PM) or active matrix (AM) OLED display. Each subpixel has an OLED material configured to emit white, red, green, blue, or other color light when energized. For example, the OLED material of a first subpixel emits red light when energized, the OLED material of a second subpixel emits green light when energized, and the OLED material of a third subpixel emits blue light when energized.
[0010] 1A and 1C are schematic cross-sectional views of a subpixel circuit 100. FIG. 1A is taken along the cut line of FIG. 1E. The subpixel circuit 100 includes a substrate 102. The substrate 102 includes, but is not limited to, silicon (Si), silicon dioxide (SiO2), fused silica, quartz, silicon carbide (SiC), germanium (Ge), silicon germanium (SiGe), indium phosphide (InP), gallium arsenide (GaAs), gallium nitride (GaN), silicon nitride (SiN), or sapphire-containing materials. A plurality of metal layers 104 are disposed on the substrate 102. The metal layers 104 are configured to act as anodes for the respective subpixels. The metal layers 104 include, but are not limited to, chromium, titanium, gold, silver, copper, aluminum, ITO, combinations thereof, or other suitable conductive materials. The metal layer 104 may be transparent or reflective, depending on whether the subpixel circuit 100 is used as a bottom-emission or top-emission display.
[0011] An anode definition layer (ADL) 108 is disposed on the metal layer 104 and the substrate 102. An opening in the ADL 108 exposes an anode 114 of the metal layer 104. Each subpixel 118 of the subpixel circuit 100 includes an anode 114. In one embodiment, the ADL 108 includes, but is not limited to, a polyimide material. In another embodiment, the ADL 108 includes a first inorganic insulator material. The first inorganic insulator material includes, but is not limited to, silicon oxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (Si2N2O), magnesium fluoride (MgF2), or a combination thereof.
[0012] In one embodiment, as shown in FIG. 1A, a pixel-defining layer (PDL) structure 110 is disposed on the substrate 102, the plurality of metal layers 104, and the ADL 108. The PDL structure 110 includes a second inorganic insulator material. The second inorganic insulator material includes, but is not limited to, silicon oxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (Si2N2O), magnesium fluoride (MgF2), or a combination thereof. In some embodiments, the first inorganic insulator material and the second inorganic insulator material are the same material. The adjacent PDL structure 110 defines each subpixel 118 and further defines the anode 114 of the metal layer 104 of the subpixel 118 of the subpixel circuit 100. In another embodiment, as shown in FIG. 1C, the PDL structure 110 is not provided. The adjacent ADL 108 defines each subpixel 118 of the subpixel circuit 100.
[0013] Prior to depositing the PDL structure 110 (if necessary) on the ADL 108, the metal grid 112 is disposed on the ADL 108. As shown in FIG. 1A, the PDL structure 110 is then disposed on the ADL 108 and the metal grid 112. Disposing the metal grid 112 on the ADL 108 insulates the metal grid 112. The metal grid 112 is disposed between each of the subpixels 118. The metal grid 112 includes a conductive material, such as a metal. For example, the metal grid 112 includes, but is not limited to, chromium, titanium, aluminum, ITO, or combinations thereof. The metal grid 112 has a metal grid width 116. The metal grid width 116 is at least 1 μm. In one example, the metal grid width 116 is about 10 μm. In another example, the metal grid width 116 is about 20 μm to about 30 μm.
[0014] A contact overhang 122 is formed on the metal grid 112. The contact overhang 122 includes, but is not limited to, a conductive metal-containing material. For example, the metal-containing material includes copper, titanium, aluminum, molybdenum, silver, indium tin oxide, indium zinc oxide, or a combination thereof. The contact overhang 122 includes a stem portion 128 and an overhang portion 130. The overhang portion 130 includes a bottom surface 132, a side surface 134, and a top surface 136. The bottom surface 132 of the overhang portion 130 is wider than the stem portion 128 to form a first overhang 138. The first overhang 138 allows the overhang portion 130 of the contact overhang 122 to create a shadowing effect on the stem portion 128. In one embodiment, which may be combined with other embodiments described herein, the metal-containing material of stem portion 128 is the same as the metal-containing material of overhang portion 130. In another embodiment, which may be combined with other embodiments described herein, the metal-containing material of stem portion 128 is different from the metal-containing material of overhang portion 130.
[0015] The subpixel circuit 100 includes a plurality of subpixels 118. The subpixel circuit 100 of the embodiments described herein may include one or more subpixels 118, such as a first subpixel and a second subpixel. Each subpixel 118 has an organic light-emitting diode (OLED) material 120. The OLED material 120 is disposed on the metal layer 104. In one example, as shown in FIG. 1A, the OLED material 120 is also disposed on the adjacent PDL structure 110. In another example, as shown in FIG. 1C, the OLED material 120 is also disposed on the ADL 108. The OLED material 120 may be deposited by evaporation deposition. The OLED material 120 is configured to emit white, red, green, blue, or other color light when energized. For example, the OLED material 120 of the subpixel 118 is configured to emit one of red light when energized, green light when energized, blue light when energized, or white light when energized. The OLED materials 120 can include one or more of a hole injection layer (HIL), a hole transport layer (HTL), an emissive layer (EML), and an electron transport layer (ETL).
[0016] A cathode 124 is disposed on the OLED material. The cathode 124 includes a conductive material, such as a metal. For example, the cathode 124 includes, but is not limited to, chromium, titanium, aluminum, ITO, or a combination thereof. The cathode 124 is disposed on the OLED material 120 of each subpixel 118. The shadowing effect of the first overhang 138 defines a deposition angle during deposition of the OLED material 120 and the cathode 124, respectively. The OLED material 120 does not contact the contact overhang 122 and the metal grid 112. The cathode 124 contacts at least the stem portion 128 of the contact overhang 122 and the metal grid 112. In some embodiments that can be combined with other embodiments described herein, the cathode 124 contacts the stem portion 128 and the overhang portion 130 of the contact overhang 122.
[0017] The contact overhang 122 includes an overhang depth 140. The overhang depth 140 is defined as the distance from the stem portion 128 to the side surface 134. The contact overhang 122 further includes an overhang height 142. In FIG. 1A, the overhang height 142 is defined as the distance from the PDL structure 110 to the bottom surface 132. In FIG. 1C, the overhang height 142 is defined as the distance from the ADL 108 to the bottom surface 132. A contact overhang ratio is defined as the ratio of the overhang height 142 to the overhang depth 140. The contact overhang ratio of the contact overhang 122 is about 1.0:0.5 to about 1.0:3.0. For example, the contact overhang ratio of the contact overhang 122 is about 1.0:1.5. The contact overhang ratio allows the cathode 124 to extend under the first overhang 138 such that the cathode 124 contacts at least the stem portion 128 of the contact overhang 122 .
[0018] Each subpixel 118 includes an encapsulation layer 126. The encapsulation layer 126 may be or correspond to a local passivation layer. The encapsulation layer 126 of each subpixel 118 is disposed on the cathode 124 (and the OLED material 120) and the PDL structure 110 (if provided). The encapsulation layer 126 includes a non-conductive inorganic material, such as a silicon-containing material. The silicon-containing material may include a Si3N4-containing material. In one embodiment that may be combined with other embodiments described herein, the encapsulation layer 126 extends along the stem portion 128 under at least a portion of the overhang portion 130 of the contact overhang 122. In some embodiments that may be combined with other embodiments described herein, the encapsulation layer 126 is disposed on the bottom surface 132 of the contact overhang 122. In some embodiments, which can be combined with other embodiments described herein, the encapsulation layer 126 is disposed on the side surfaces 134 of the contact overhangs 122 and on the top surfaces 136 of the contact overhangs 122 .
[0019] The subpixel circuit 100 may further include at least a global passivation layer 144 disposed on the contact overhang 122 and the encapsulation layer 126. An intermediate layer 146 may be disposed between the global passivation layer 144 and the contact overhang 122 and the encapsulation layer 126. The intermediate layer 146 may be an inkjet layer. The inkjet layer may include an acrylic material.
[0020] 1B and 1D are schematic cross-sectional views of a subpixel circuit 100. FIG. 1B is taken along the cut line of FIG. 1E. As previously described, the subpixel circuit 100 includes a metal grid 112, a contact overhang 122, an OLED material 120, a cathode 124, and an encapsulation layer 126. In one example, as shown in FIG. 1B, the subpixel circuit 100 includes a PDL structure 110. In another example, as shown in FIG. 1C, the subpixel circuit 100 does not include a PDL structure 110.
[0021] In one example, as shown in FIG. 1B, the inorganic overhang structure 148 is disposed on the PDL structure 110. In another example, as shown in FIG. 1D, the inorganic overhang structure 148 is disposed on the metal grid 112. The inorganic overhang structure 148 is fixed to the subpixel circuit 100. The inorganic overhang structure 148 further defines each subpixel 118 of the subpixel circuit 100. The inorganic overhang structure 148 includes at least one of a non-conductive inorganic material or a conductive inorganic material. The non-conductive inorganic material includes, but is not limited to, an inorganic silicon-containing material or a polymeric material. For example, the silicon-containing material includes an oxide or nitride of silicon, or a combination thereof. The conductive inorganic material includes, but is not limited to, a metal-containing material. For example, the metal-containing material includes copper, titanium, aluminum, molybdenum, silver, indium tin oxide, indium zinc oxide, or a combination thereof. The inorganic overhang structure 148 prevents the sequential deposition of the OLED material 120 and the cathode 124 .
[0022] The inorganic overhang structure 148 includes a structure stem portion 150 and a structure overhang portion 152. The structure overhang portion 152 includes a structure bottom surface 154, a structure side surface 156, and a structure top surface 158. The structure bottom surface 154 is wider than the structure stem portion 150 and forms a second overhang 160. The second overhang 160 allows the structure overhang portion 152 of the contact overhang 122 to shadow the structure stem portion 150. In one embodiment that can be combined with other embodiments described herein, the structure stem portion 150 and the structure overhang portion 152 include the same material. In another embodiment that can be combined with other embodiments described herein, the structure stem portion 150 and the structure overhang portion 152 include different materials.
[0023] The inorganic overhang structure 148 includes an overhang structure depth 162. The overhang structure depth 162 is defined as the distance from the apex 151 of the structure stem portion 150 to the structure side surface 156. The inorganic overhang structure 148 further includes an overhang structure height 164. In one example, as shown in FIG. 1B, the overhang structure height 164 is defined as the distance from the PDL structure 110 to the structure bottom surface 154. In another example, as shown in FIG. 1D, the overhang structure height 164 is defined as the distance from the metal grating 112 to the structure bottom surface 154. An overhang structure ratio is defined as the ratio of the overhang structure height 164 to the overhang structure depth 162. The overhang structure ratio of the inorganic overhang structure 148 is about 1.0:2.0 to about 1.0:3.0. The overhang structure ratio allows the cathode 124 to be deposited under the second overhang 160 such that the cathode 124 contacts the OLED material 120 under the second overhang 160. In one example, as shown in Figure 1B, the cathode 124 contacts the OLED material 120 and the PDL structure 110. In another example, as shown in Figure 1D, the cathode 124 contacts the OLED material 120 and the metal grid 112.
[0024] In one embodiment that can be combined with other embodiments described herein, the encapsulation layer 126 extends along the structural stem portion 150 beneath at least a portion of the structural overhang portion 152 of the inorganic overhang structure 148. In some embodiments that can be combined with other embodiments described herein, the encapsulation layer 126 is disposed on the structural bottom surface 154 of the inorganic overhang structure 148. In some embodiments that can be combined with other embodiments described herein, the encapsulation layer 126 is disposed on the structural side surface 156 of the inorganic overhang structure 148 and the structural top surface 158 of the inorganic overhang structure 148.
[0025] FIG. 1E is a schematic top view of a subpixel circuit 100. The subpixel circuit 100 shown in FIG. 1E corresponds to the subpixel circuit 100 shown in FIG. 1A and FIG. 1B. The subpixel circuit 100 includes a contact overhang 122 in a first configuration. As shown in FIG. 1E, the subpixel circuit 100 includes a plurality of pixel openings 166. Each pixel opening 166 is bordered by an adjacent inorganic overhang structure 148 that defines where each of the subpixels 118 is formed. The subpixel circuit 100 further includes a PDL structure 110 that further defines where each of the subpixels 118 is formed. The adjacent PDL structure 110 defines each subpixel and exposes the anode 114 of the metal layer 104 (i.e., the anode) of each subpixel of the subpixel circuit 100. The contact overhang 122 is disposed between adjacent subpixels 118. The contact overhang 122 is disposed within the exposed portion 168 of the PDL structure 110. An exposure 168 is formed in the PDL structure 110 to expose the metal grid 112 disposed on the ADL 108 below the PDL structure 110. The exposure 168 allows the contact overhang 122 to contact the metal grid 112.
[0026] 2A is a schematic cross-sectional view of a portion 205 of the subpixel circuit 100 shown in FIG. 1A. A contact overhang 122 is disposed in an exposed portion 168 of the PDL structure 110. The PDL structure 110 further includes an ADL 108 disposed below the PDL structure 110. The exposed portion 168 allows the contact overhang 122 to contact the metal grid 112. The portion 205 shows the OLED material 120, the cathode 124, and the encapsulation layer 126. The OLED material 120 does not contact the contact overhang 122. The cathode 124 contacts at least a stem portion 128 of the metal grid 112. In some embodiments that can be combined with other embodiments described herein, the cathode 124 contacts the PDL structure 110. The contact overhang 122 provides electrical contact to the metal grid 112. Thus, the cathode 124 in contact with the contact overhang 122 receives current from the metal grid 112 through the contact overhang 122. The contact overhang ratio provides deposition where the cathode 124 contacts the contact overhang 122. Furthermore, the deposition source can deposit the cathode 124 and the OLED material 120 at different angles to adjust where the cathode 124 and the OLED material 120 are located.
[0027] Device leakage occurs due to the minimum distance between the anode 114 and the cathode 124. In addition, device leakage may occur due to the OLED material 120 contacting the inorganic overhang structure 148. The contact overhang 122 is operable to reduce leakage in the subpixel circuit 300 by increasing the distance between the subpixel cathode contact (i.e., where the cathode 124 contacts the contact overhang 122) and the anode 114 of the metal layer 104 compared to other approaches. For example, the distance between the cathode contact (i.e., where the cathode 124 contacts the contact overhang 122) and the anode 114 of the metal layer 104 is about 10 mm to about 5 inches. The contact overhang 122 reduces the number of cathode contacts and increases the distance between the cathode contacts and the anode 114, thereby reducing the occurrence of leakage.
[0028] FIG. 2B is a schematic cross-sectional view of a portion 210 of the subpixel circuit 100 shown in FIG. 1B. An inorganic overhang structure 148 is disposed on the PDL structure 110. The PDL structure 110 further includes an ADL 108 disposed below the PDL structure 110. The portion 210 shows the OLED material 120, the cathode 124, and the encapsulation layer 126. The OLED material 120 does not contact the contact overhang 122. The cathode 124 does not contact the inorganic overhang structure 148. The overhang structure ratio provides a deposition in which the cathode 124 does not contact the inorganic overhang structure 148. Thus, the formation of the inorganic overhang structure 148 does not require the same precision. For example, the inorganic overhang structure 148 can be formed with less precision, as long as the overhang structure ratio prevents the sequential deposition of the OLED material 120 and the cathode 124. This design of the subpixel circuit 300 allows a top-emission display to be formed using the inorganic overhang structure 148 that is commonly used in bottom-emission displays. Bottom-emission displays use inorganic overhang structures 148 with lower photo-precision requirements.
[0029] FIG. 3 is a schematic top view of a subpixel circuit 300. The subpixel circuit 300 is an embodiment of the subpixel circuit 100 (shown in FIGS. 1A-1E) having a second configuration of contact overhangs 122. The contact overhangs 122 are disposed between adjacent subpixels 118. The subpixel circuit 300 includes an inorganic overhang structure 148. The subpixel circuit 300 includes a plurality of pixel openings 166. Each pixel opening 166 is bordered by an adjacent inorganic overhang structure 148 that defines where each of the subpixels 118 is formed. The adjacent PDL structures 110 and the adjacent inorganic overhang structures 148 define each subpixel 118. As shown in FIG. 3, the subpixel circuit 300 includes a 5×5 grid of subpixels 118 such that there are 25 subpixels 118. Each subpixel 118 is operable to emit light of a different color. For example, each sub-pixel 118 may emit one of red, green, blue, or white light when activated.
[0030] The sub-pixel circuit 300 includes sub-circuits C1, C2, C3, C4, . . . C N Subcircuits C1 to C N Each of the subcircuits C1 to C2 includes a plurality of subpixels 118. N corresponds to a plurality of metal layers 104 passing through the sub-pixel circuits 300 on the substrate 102. N includes one or more contact overhangs 122. The subpixel circuit 300 further includes a metal grid 112. The metal grid 112 is connected to a plurality of auxiliary cathode lines R1, R2, R3, R4, ... R M The auxiliary cathode lines R1 to R M The subcircuits C1 to C N The auxiliary cathode lines R1 to R2 of the metal grid 112 are perpendicular to the MThe metal layers 104 are disposed below the anode definition layer (ADL) 108. The metal layers 104 are perpendicular to the metal grid 112. Each of the contact overhangs 122 is connected to each of the auxiliary cathode lines R1-R2 of the metal grid 112. M Subcircuits C1 to C N and the number of auxiliary cathode lines R1 to R M By increasing the number of subpixels 118 on the subpixel circuit 300 .
[0031] The sub-pixel circuit 300 includes sub-circuits C1 to C N Each of the specific sub-circuits C1 to C2 can be activated individually. N A current is provided through the metal grid 112 to activate the corresponding sub-circuits C1-C. N Auxiliary cathode lines R1 to R2 having contact overhangs 122 M A voltage and / or current is provided to each of the metal grids 112. The current is provided through the metal grids 112 and flows to the contact overhangs 122. The metal grids 112 are connected to a common ground. In some embodiments that can be combined with other embodiments described herein, a negative voltage can be applied to the metal grids 112. In one embodiment that can be combined with other embodiments described herein, each metal grid 112 is electrically connected to a thin film transistor (not shown) on the substrate 102, which provides a current and / or voltage to each of the metal grids 112. The contact overhangs 122 are connected to the activated sub-circuits C1-C2. N The cathode 124 (shown in FIGS. 1A-1E) is in contact with the cathode 124.
[0032] An example of a current flow for activating a plurality of sub-pixels 118 of the sub-circuit C1 is shown by line 301. As shown in FIG. 3, the current flows through the metal grid 112 of the auxiliary cathode line R1. The current flows to the contact overhang 122 of the sub-circuit C1. The contact overhang 122 contacts the cathode 124 disposed along the sub-circuit C1. Thus, a current and / or voltage is operable to flow through the cathode 124 throughout the sub-circuit C1. The current flows from the cathode 124 to the OLED material 120 and into the metal layer 104 of the sub-circuit C1. A current can be provided to the metal layer 104 of the column I1 to activate the sub-pixels 118 of the sub-circuit C1.
[0033] Subcircuits C1 to C N The sub-pixels 118 are operable to emit light. N In one embodiment, which may be combined with other embodiments described herein, the subcircuits C1-C N In another embodiment, which can be combined with other embodiments described herein, the sub-circuits C1-C N Each of the sub-pixels 118 of the first sub-circuit C1 is operable to emit light of a different color, for example, the sub-pixels 118 of the first sub-circuit C1 emit red light, the sub-pixels 118 of the second sub-circuit C2 emit green light, the sub-pixels 118 of the third sub-circuit C3 emit blue light, and the sub-pixels 118 of the fourth sub-circuit C4 emit white light.
[0034] Contact overhangs 122 may be disposed in the sub-pixel circuits 300 as desired. N Each of the sub-circuits C1 to C2 includes at least one contact overhang 122. NEach of the contact overhangs 122 may include two or more contact overhangs 122. The contact overhangs 122 are positioned such that there is a distance between adjacent contact overhangs 122 of about 50 mm to about 7 inches.
[0035] FIG. 4 is a flow diagram of a method 400 for forming the subpixel circuit 100 shown in FIGS. 5A-5E and 6A-6B. The method 400 corresponds to the subpixel circuit 100 shown in FIGS. 1A-1B. FIGS. 5A-5E are schematic top views of the subpixel circuit 100 during the method 400. FIGS. 6A-6B are schematic cross-sectional views of the subpixel circuit 100 during the method 400. For ease of explanation, the method 400 will be described with reference to a subpixel circuit 100 having contact overhangs 122 in a first configuration. However, the method 400 may be performed to form any subpixel circuit (e.g., subpixel circuit 300) having contact overhangs 122 in any configuration.
[0036] In operation 401, as shown in Figure 5A, a plurality of metal layers 104 are disposed on a substrate 102. The plurality of metal layers 104 may be patterned on the substrate 102. In one embodiment, which may be combined with other embodiments described herein, the metal layers 104 are pre-patterned on the substrate 102. For example, the substrate 102 is a pre-patterned indium tin oxide (ITO) glass substrate.
[0037] In operation 402, an anode definition layer (ADL) 108 is disposed on the substrate 102 and the plurality of metal layers 104, as shown in FIG. 5B. The ADL 108 is further patterned to expose anodes 114 of the plurality of metal layers 104 (i.e., anodes). Each of the anodes 114 is associated with an individual subpixel 118 to be formed, such as the plurality of subpixels 118 shown in FIG. 1E. The ADL 108 can be patterned by patterning a photoresist coating and subsequent etching.
[0038] In operation 403, as shown in FIG. 5C, a metal grid 112 is disposed on the ADL 108. The metal grid 112 is disposed between exposed portions of the plurality of metal layers 104. The metal grid 112 is disposed perpendicular to the plurality of metal layers 104. The metal grid 112 is insulated by the ADL 108.
[0039] In operation 404, the PDL structure 110 is disposed over the metal grid 112 and the ADL 108, as shown in Figure 5D. The PDL structure 110 is further patterned to form an exposure 168 in the PDL structure 110. The exposure 168 exposes the metal grid 112 underneath. The PDL structure 110 waterproofs the metal grid 112.
[0040] In operation 405, a plurality of inorganic overhang structures 148 are formed, as shown in FIG. 5E. The plurality of inorganic overhang structures 148 are formed on the PDL structure 110. The plurality of inorganic overhang structures 148 are formed on either side of exposed portions of the plurality of metal layers 104. The plurality of inorganic overhang structures 148 are formed parallel to the plurality of metal layers 104. The plurality of inorganic overhang structures 148 includes a second overhang 160. An adjacent PDL structure 110 and an adjacent inorganic overhang structure 148 define a respective subpixel 118.
[0041] In operation 406, contact overhangs 122 are formed on the exposed portions 168, as shown in FIG. 6A. The contact overhangs 122 are formed on the exposed portions 168 and contact the metal grid 112 disposed thereunder. The contact overhangs 122 are formed between adjacent subpixels 118. The number of contact overhangs 122 that can be formed is not limited. Each subpixel does not need a contact overhang 122 because the subpixel circuitry that is formed controls each subcircuit individually. By using the contact overhangs 122, larger displays can be formed. The contact overhangs 122 include a first overhang 138.
[0042] In operation 407, the OLED material 120, the cathode 124, and the encapsulation layer 126 are disposed as shown in FIG. 6B. The OLED material 120, the cathode 124, and the encapsulation layer 126 are deposited by evaporation. The shadowing of the first overhang 138 and the second overhang 160 defines the evaporation of the OLED material 120 and the cathode 124, respectively. The shadowing effect of the contact overhang 122 and the inorganic overhang structure 148 defines the angle at which the OLED material 120 and the cathode 124 are deposited during evaporation. For example, the evaporation angle defined by the first overhang 138 causes the cathode 124 to extend under the first overhang 138 and contact the contact overhang 122. The evaporation angle defined by the second overhang 160 causes the cathode 124 to not contact the contact overhang 122. Additionally, the deposition source is operable to deposit the OLED material 120 and the cathode 124 at different deposition angles to further define where the OLED material 120 and the cathode 124 are deposited. Operation 407 can be repeated for each additional subpixel 118. In operation 408, an intermediate layer 146 and a global passivation layer 144 are disposed, as shown in FIG. 1B.
[0043] In summary, the embodiments described herein relate to a sub-pixel circuit and a method of forming the sub-pixel circuit that may be used in a display, such as an organic light emitting diode (OLED) display. The sub-pixel circuit includes a plurality of contact overhangs. The plurality of contact overhangs are disposed between adjacent sub-pixels of the formed sub-pixel circuit. The contact overhangs are formed on a metal grid disposed through a PDL structure. A cathode is deposited by evaporation to contact the contact overhangs. The metal grid is perpendicular to a plurality of metal layers disposed on a substrate. To activate an individual sub-circuit of the sub-pixel circuit, a current is applied to the metal grid. The current flows to the contact overhang and the cathode of the sub-circuit to be activated. The current flows through the OLED material to one of the plurality of metal layers to activate one of the sub-circuits of the sub-pixel. The contact overhangs allow the overhang structure of the sub-circuit to be formed with less precision. The contact overhangs also reduce the occurrence of device leakage, thus improving the performance of the sub-circuit.
[0044] While the foregoing is directed to embodiments of the disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof, the scope of which is determined by the following claims.
Claims
1. A subcircuit comprising: a metal grid disposed on an anode definition layer (ADL), the ADL exposing an anode disposed on a substrate; an inorganic overhang structure disposed on the metal grid, adjacent ADLs defining a plurality of sub-pixels of the sub-circuit, each sub-pixel of the plurality of sub-pixels comprising: an anode defined by the ADL; an organic light emitting diode (OLED) material disposed on and in contact with the anode; a cathode disposed over the OLED material; an inorganic overhang structure comprising: at least one contact overhang disposed on each auxiliary cathode line of the metal grid, the contact overhang being disposed between two subpixels of the plurality of subpixels, and the cathode contacting the contact overhang; A subcircuit comprising:
2. The subcircuit of claim 1 , further comprising a pixel definition layer (PDL) structure disposed on the ADL, an adjacent PDL structure further defining the plurality of subpixels of the subcircuit.
3. The subcircuit of claim 2 , wherein the at least one contact overhang is disposed in an exposed portion of the PDL structure to expose the metal grid.
4. 2. The sub-circuit of claim 1, wherein each sub-pixel of the plurality of sub-pixels further comprises an encapsulation layer disposed over the cathode, the contact overhang, the at least one contact overhang, and the inorganic overhang structure.
5. The subcircuit of claim 4 , wherein the encapsulation layer contacts a structural stem portion and a structural bottom surface of the inorganic overhang structure.
6. The sub-circuit of claim 4 , further comprising an intermediate layer and a global passivation layer disposed on the inorganic overhang structure, the at least one contact overhang, and the encapsulation layer.
7. The sub-circuit of claim 1 , wherein the cathode of the sub-circuit contacts a stem portion of the at least one contact overhang.
8. 2. The sub-circuit of claim 1, wherein the sub-circuit is operable to be activated by applying a current to the respective auxiliary cathode line that contacts the at least one contact overhang.
9. A device, comprising: A substrate; a plurality of metal layers disposed on the substrate; an anode definition layer (ADL) disposed on the plurality of metal layers and the substrate, the ADL defining an anode of the device; a metal grid disposed on the ADL, adjacent ADLs defining subpixels of the device; a plurality of sub-circuits, each sub-circuit comprising: The metal grid disposed on the ADL; and an inorganic overhang structure disposed on the metal lattice; a first plurality of sub-pixels; wherein each subpixel in the first plurality of subpixels comprises: an anode defined by the ADL; an organic light emitting diode (OLED) material disposed on and in contact with the anode; a cathode disposed over the OLED material; a plurality of sub-circuits, at least one contact overhang disposed on each auxiliary cathode line of the metal grid, the contact overhang being disposed between two subpixels of the first plurality of subpixels, the cathode contacting the contact overhang; A device comprising:
10. 10. The device of claim 9, further comprising a pixel definition layer (PDL) structure disposed on the ADL, an adjacent PDL structure further defining the first plurality of subpixels of the subcircuit.
11. 11. The device of claim 10, wherein the metal grid is exposed through an exposed portion of the PDL structure, and the at least one contact overhang is disposed on the metal grid at the exposed portion.
12. 10. The device of claim 9, wherein each subpixel of the first plurality of subpixels further comprises an encapsulation layer disposed over the cathode, the contact overhang, the at least one contact overhang, and the inorganic overhang structure.
13. The device of claim 12 , wherein the encapsulation layer contacts a structure stem and a structure bottom surface of the inorganic overhang structure.
14. 13. The device of claim 12, further comprising an intermediate layer and a global passivation layer disposed on the inorganic overhang structure, the at least one contact overhang, and the encapsulation layer.
15. The device of claim 9 , wherein the cathode contacts at least a stem portion of the at least one contact overhang.
16. 10. The device of claim 9, wherein the inorganic overhang structure has an overhang structure ratio defined as a ratio of an overhang structure height to an overhang structure depth, the overhang structure ratio being from about 1.0:1.2 to about 1.0:1.
3.
17. 10. The device of claim 9, wherein the at least one contact overhang has a contact overhang ratio defined as a ratio of overhang height to overhang depth, the contact overhang ratio being from about 1.0:1.0 to about 1.0:1.
5.
18. 10. The device of claim 9, wherein the at least one contact overhang includes a stem portion and an overhang portion, the overhang portion being wider than the stem portion and forming a first overhang.
19. The device of claim 9 , wherein the plurality of metal layers are perpendicular to the metal grid.
20. A device, comprising: A substrate; a plurality of metal layers disposed on the substrate; an anode definition layer (ADL) disposed on the plurality of metal layers and the substrate, the ADL defining an anode of the device; a metal grid disposed on the ADL, adjacent ADLs defining subpixels of the device; a plurality of sub-circuits, each sub-circuit comprising: The metal grid disposed on the ADL; and an inorganic overhang structure disposed on the metal lattice; a first plurality of sub-pixels; wherein each subpixel in the first plurality of subpixels comprises: an anode defined by the ADL; an organic light emitting diode (OLED) material disposed on and in contact with the anode; a cathode disposed over the OLED material; a plurality of sub-circuits, at least one contact overhang disposed on each auxiliary cathode line of the metal grid, the contact overhang disposed between two subpixels of the first plurality of subpixels, the cathode contacting at least a stem portion of the at least one contact overhang, the at least one contact overhang comprising a contact overhang ratio defined as a ratio of an overhang height to an overhang depth, the contact overhang ratio being from about 1.0:1.0 to about 1.0:1.5; A device comprising: