Phase change memory gap
The PCM cell design with a toroidal gap in the insulator stack addresses heat transfer and energy efficiency issues, enhancing programming and reading speeds by isolating heat and reducing energy consumption.
Patent Information
- Application Number
- JP2024529430
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-17
- Filing Date
- 2022-10-28
- Publication Date
- 2024-11-11
- Estimated Expiration
- 2042-10-28
AI Technical Summary
Existing phase change memory (PCM) technologies face challenges in efficiently managing heat transfer and energy consumption due to the lack of effective thermal isolation and resistance tuning, which affects the speed and efficiency of programming and reading operations.
The PCM cell design incorporates a toroidal-shaped gap within an insulator stack surrounding the PCM material, utilizing materials with different etch rates to create gaps that enhance thermal isolation and reduce heat transfer, allowing for faster and more energy-efficient programming and reading operations.
The toroidal gap design improves the speed and efficiency of PCM cells by reducing heat transfer and energy consumption, enabling faster programming and reading operations while maintaining high resistance tuning capabilities.
Smart Images

Figure 2024541716000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to computer memories, and more particularly to phase change material memory devices that include voids. [Background technology]
[0002] Phase change memory (PCM) can be utilized for both training and inference in analog computations with respect to artificial intelligence. PCM structures can include phase change memristor devices that have tunable electrical conductivity and high overall device resistance along with high retention to minimize energy consumption. This tuning can be achieved by forming different structural states in which the ratio of crystalline and amorphous phases of the PCM material changes. The formation of these phases can occur by heating the PCM material at various amounts in a controlled manner. Summary of the Invention
[0003] According to an embodiment of the invention, a PCM cell includes a first electrode, a heater / PCM portion electrically connected to the first electrode, the heater / PCM portion including a PCM material, a second electrode electrically connected to the PCM material, and an electrical insulator stack surrounding a protruding liner, the stack including a plurality of first layers having a plurality of first inner surfaces facing the protruding liner, the plurality of first layers being made of a first material, and a plurality of second layers alternating with the plurality of first layers, the plurality of second layers being made of a second material different from the first material, the plurality of second layers having a plurality of second inner surfaces facing the protruding liner, the plurality of second inner surfaces offset from the plurality of first inner surfaces forming a plurality of gaps.
[0004] According to an embodiment of the invention, a method of manufacturing a PCM cell includes forming a first electrode and forming an electrical insulator stack on the first electrode, the stack including a plurality of first layers comprised of a first material and a plurality of second layers alternating with the plurality of first layers, the plurality of second layers comprised of a second material different from the first material. The method also includes forming a via in the stack, removing a portion of the plurality of second layers from the via while leaving the plurality of first layers intact, forming walls in the plurality of first layers in the via to create a plurality of gaps, forming a heater / PCM portion inside the walls, and forming a second electrode on the heater / PCM portion.
[0005] According to an embodiment of the invention, a PCM cell includes a first electrode, a heater / PCM portion electrically connected to the first electrode, the heater / PCM portion including a PCM material, a second electrode electrically connected to the PCM material, and an electrical insulator stack surrounding the protruding liner, the stack defining a plurality of gaps, each of the gaps having a toroidal shape, axially spaced apart from one or more other gaps, and surrounding a portion of the PCM material. [Brief description of the drawings]
[0006] [Figure 1A] 1 is a cross-sectional view of a PCM cell including an air gap according to an embodiment of the present invention. [Figure 1B] FIG. 1B is a cross-sectional view of the PCM cell of FIG. 1A including an amorphous zone in accordance with an embodiment of the present invention. [Diagram 2] 1B is a flowchart of a method for manufacturing the PCM cell of FIG. 1A according to an embodiment of the present invention. [Figure 3A] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3B] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3C]3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3D] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3E] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3F] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3G] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3H] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 3I] 3 is a cross-sectional view of the method of FIG. 2 for manufacturing a PCM cell according to an embodiment of the present invention. [Figure 4] 4 is a flowchart of an alternative method of manufacturing an alternative PCM cell in accordance with an embodiment of the present invention. [Figure 5A] 5 is a cross-sectional view of an alternative method of manufacturing an alternative PCM cell of FIG. 4 in accordance with an embodiment of the present invention. [Figure 5B] 5 is a cross-sectional view of an alternative method of manufacturing an alternative PCM cell of FIG. 4 in accordance with an embodiment of the present invention. [Figure 5C] 5 is a cross-sectional view of an alternative method of manufacturing an alternative PCM cell of FIG. 4 in accordance with an embodiment of the present invention. [Figure 5D] 5 is a cross-sectional view of an alternative method of manufacturing an alternative PCM cell of FIG. 4 in accordance with an embodiment of the present invention. [Figure 5E] 5 is a cross-sectional view of an alternative method of manufacturing an alternative PCM cell of FIG. 4 in accordance with an embodiment of the present invention. [Figure 5F] 5 is a cross-sectional view of an alternative method of manufacturing an alternative PCM cell of FIG. 4 in accordance with an embodiment of the present invention. [Figure 5G] 5 is a cross-sectional view of an alternative method of manufacturing an alternative PCM cell of FIG. 4 in accordance with an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] Various embodiments of the present invention are described herein with reference to the associated drawings. Alternative embodiments may be devised without departing from the scope of the present invention. It is noted that in the following description and drawings, various connections and positional relationships (e.g., above, below, adjacent, etc.) between elements are shown. Those connections and / or positional relationships can be direct or indirect unless otherwise specified, and the disclosure is not intended to be limited in this respect. Thus, the connection of entities can refer to direct or indirect connections, and the positional relationship between entities can be a direct or indirect positional relationship. As an example of an indirect positional relationship, in this description, reference to forming layer "A" on layer "B" includes the situation where one or more intermediate layers (e.g., layer "C" and layer "D") are between layer "A" and layer "B", as long as the relevant properties and functions of layer "A" and layer "B" are not significantly altered by the intermediate layers.
[0008] The following definitions and abbreviations are used in the interpretation of the claims and the specification. As used herein, the terms "comprises," "comprises," "includes," "includes," "has," "having," "containing," "containing," or any other variation thereof, are intended to cover a non-exclusive inclusion. For example, a composition, mixture, process, method, article, or device that includes a list of elements is not necessarily limited to only those elements, and may include other elements not expressly stated or inherent to such composition, mixture, process, method, article, or device. In addition, any numerical ranges included herein include the boundaries of those numerical ranges unless expressly stated otherwise.
[0009] In the following, for purposes of explanation, the terms "upper", "lower", "right", "left", "vertical", "horizontal", "top", "bottom" and their derivatives shall refer to the described structures and methods as oriented in the drawings. The terms "overlying", "atop", "on top", "positioned on" or "positioned atop" mean that a first element, such as a first structure, is on a second element, such as a second structure, and an intervening element, such as an interface structure, may be between the first and second elements. The term "direct contact" means that a first element, such as a first structure, and a second element, such as a second structure, are connected without any intermediate conductive, insulating or semiconducting layer at the interface between the two elements. It should be noted that the term "selective to", e.g., "a first element selective to a second element", means that the first element can be etched and the second element can act as an etch stop.
[0010] For the sake of brevity, conventional techniques related to the manufacture of semiconductor devices and integrated circuits (ICs) may or may not be described in detail herein. Additionally, various operations and process steps described herein may be incorporated into more comprehensive procedures or processes that include additional steps or functions not described in detail herein. In particular, because the various steps in the manufacture of semiconductor devices and semiconductor-based ICs are well known, for the sake of brevity, many conventional steps are described only briefly herein or omitted entirely without providing details of the well-known processes.
[0011] Generally, the various processes used to form the microchips that are packaged into ICs fall into four general categories: deposition, removal / etching, semiconductor doping, and patterning / lithography.
[0012] Deposition can be any process that grows, coats, or otherwise transfers material onto a wafer. Available techniques include physical vapor deposition (PVD), chemical vapor deposition (CVD), electrochemical deposition (ECD), molecular beam epitaxy (MBE), and more recently atomic layer deposition (ALD), among others. Another deposition technique is plasma enhanced chemical vapor deposition (PECVD), a process that uses energy in a plasma to drive reactions at the wafer surface that require higher temperatures than would otherwise be associated with conventional CVD. Energetic ion bombardment during PECVD deposition can also improve the electrical and mechanical properties of the film.
[0013] Removal / etching can be any process that removes material from a wafer. Examples include etching processes (either wet or dry), chemical-mechanical planarization (CMP), etc. One example of a removal process is ion beam etching (IBE). In general, IBE (or milling) refers to dry plasma etching methods that utilize a remote wide beam ion / plasma source to remove substrate material by means of physically inert and / or chemically reactive gases. Like other dry plasma etching techniques, IBE has advantages such as etch rate, anisotropy, selectivity, uniformity, aspect ratio, and minimal damage to the substrate. Another example of a dry removal process is reactive ion etching (RIE). In general, RIE uses a chemically reactive plasma to remove material deposited on the wafer. In RIE, plasma is generated under low pressure (vacuum) by an electromagnetic field. High energy ions from the RIE plasma bombard and react with the wafer surface, removing material.
[0014] Semiconductor doping can generally be the modification of electrical properties, for example by doping the source and drain of a transistor, by diffusion or by ion implantation, or both. These doping processes are followed by furnace annealing or rapid thermal annealing (RTA). The annealing serves to activate the implanted dopants. Films of both conductors (e.g., polysilicon, aluminum, copper, etc.) and insulators (e.g., various forms of silicon dioxide, silicon nitride, etc.) are used to connect and separate transistors and their components. Selective doping of different regions of a semiconductor substrate allows the conductivity of the substrate to be modified by the application of a voltage. By creating structures of these various components, millions of transistors can be built and wired together to form the complex circuits of modern microelectronic devices.
[0015] Semiconductor lithography can be the formation of a three-dimensional relief image or pattern on a semiconductor substrate for subsequent transfer of the pattern to a substrate. In semiconductor lithography, the pattern is formed by a light-sensitive polymer called photoresist. The steps of lithography and etching pattern transfer are repeated multiple times to build the complex structures that make up the circuit's transistors and the many wires that connect millions of transistors. Each pattern printed on the wafer is aligned to a pattern already formed, and conductors, insulators, and selectively doped regions are gradually built up to form the final device.
[0016] 1A and 1B are cross-sectional views of a PCM cell 100, for example for use in an integrated circuit (not shown). In the embodiment shown, PCM cell 100 includes a bottom wire 102, an insulator 104, a bottom electrode 106, an insulator 108, a wall 110, a protruding liner 112, a PCM material 114, a stack 116, a gap 118, an insulator 120, a top electrode 122, and a top wire 124.
[0017] In the embodiment shown, the bottom of the bottom electrode 106 is in direct contact and electrically connected to the top of the bottom wire 102, which can receive electrical signals from other components of the integrated circuit (not shown). The bottom of the protruding liner 112 is in direct contact and electrically connected to the top of the bottom electrode 106. The bottom and sides of the PCM material 114 are in direct contact and electrically and thermally connected to the inner surface of the protruding liner 112. The bottom of the top electrode 122 is in direct contact and electrically connected to the top of the PCM material 114. The bottom of the top wire 124 is in direct contact and electrically connected to the top of the top electrode 122, which can deliver electrical signals from the PCM cell 100 to other components of the integrated circuit (not shown).
[0018] In the embodiment shown, the wall 110 directly contacts and laterally surrounds the outside of the protruding liner 112. Thus, the wall 110 surrounds the protruding liner 112 on all parallel sides in at least one direction (e.g., the vertically extending sides as shown in FIG. 1A). The stack 116 generally laterally surrounds and selectively directly contacts the outside of the wall 110. More specifically, the stack 116 is an electrical insulator having a two-layer configuration including alternating A layers 128 and B layers 130. An inner surface 129 of the A layer 128 directly contacts and laterally surrounds the wall 110 in a corresponding axial cross section, while an inner surface 131 of the B layer 130 is laterally spaced away from the wall 110. This forms a series of axially spaced toroidal gaps 118 each surrounding the wall 110, the protruding liner 112, and a portion of the PCM material 114, with each gap 118 surrounded by two A layers 128, a B layer, and the wall 110. The gaps 118 are cavities within the stack 116, so there is no solid material contact with the outside of the wall 110 at the gaps 118. The bottom and top of the stack 116 are formed by the two A layers 128, which are in direct contact with the insulator 108, the bottom electrode 106, the insulator 120, and the top electrode 122, respectively. The top electrode 122 is also in direct contact with the insulator 120 and is surrounded laterally on the outside and axially on a portion of its top surface by the insulator 120, and the top wire 124 is in direct contact with the insulator 120 and is surrounded laterally by the insulator 120 on the outside.
[0019] 1A shows nine layers (i.e., five A layers 128 and four B layers 130), there may be fewer (e.g., three) or more (e.g., 21) layers. In addition, the A layers 128 and B layers 130 may be, for example, 2 nanometers (nm) to 20 nm thick. Furthermore, the thickness of the A layers 128 may be the same as or different from the thickness of the B layers 130.
[0020] In the embodiment shown, the A layer 128 and the B layer 130 are made of, for example, NBLoK, silicon nitride (SiN), aluminum oxide (Al2O3), aluminum nitride (AlN), silicon oxide (SiO2), or silicon oxycarbide (SiO X C Y ), the A layer 128 and the B layer 130 are composed of different materials such that a portion of the B layer 130 can be selectively removed (thereby forming the gap 118) without significantly removing the A layer 128. For example, the A layer 128 can be composed of SiN and the B layer 130 can be composed of AIN. The difference in the materials of the A layer 128 and the B layer 130 can be exploited during the fabrication of the PCM cell 100. For example, there is significant selectivity, e.g., with an etch rate ratio of 5:1, 10:1, or even greater (e.g., AIN:SiN or SiN:AIN), for the removal of AIN and the removal of SiN by some reactant and / or process. More specifically, SiN is amenable to removal using a RIE process, while AIN is resistant to the RIE process, such that SiN can be removed without significantly removing AIN. On the other hand, AIN is amenable to removal using certain wet etching processes and chemicals, while SiN is resistant to such processes, so that AIN may be removed without significant removal of SiN. In another example, the A layer 128 may be composed of SiO2 and the B layer 130 may be composed of Al2O3. Al2O3 has a higher selectivity to chlorine gas (Cl2), argon (Ar), and argon-boron-chlorine (Ar / B / Cl2) mixtures. Additionally, the etch rates of SiO2 and SiN are higher than those of carbon tetrafluoride (CF 4) and oxygen (O2), whereas the etch rate of Al2O3 is related to aluminum chloride (AlCl3) or a chlorine-boron trichloride (Cl2 / BCl3) mixture. Thus, the etch rates of fluorine (F), Cl2, sulfur hexafluoride (SF6), fluorocarbons (C x F y Gases such as SiO2, Ar, and hydrogen (H2) can provide selectivity in RIE between Al2O3 and SiN or SiO2.
[0021] In the embodiment shown, the insulators 104, 108, 120 and stack 116 structurally support and, optionally, electrically insulate and fill spaces between other components of the PCM cell 100. Thus, the outside of the bottom wire 102 is in direct contact with and laterally surrounded by the insulator 104, and the outside of the bottom electrode 106 is in direct contact with and laterally surrounded by the insulator 108. Additionally, the top surface of the stack 116, the outside and a portion of the top surface of the top electrode 122, and the outside of the top wire 124 are in direct contact with the insulator 120.
[0022] In the illustrated embodiment, the cross section (into the page of FIG. 1) of the various components and / or the entire PCM cell 100 may be circular, but in other embodiments may be rectangular, square, oval, or any other suitable shape. In addition, the width of the PCM material 114 is less than the width of the bottom electrode 106 and the top electrode 122, while the axial length of the PCM material 114 is significantly greater than its width. The PCM cell 100 may thereby be said to have a confined cell configuration, in which an electrical signal (i.e., current) can flow from the bottom electrode 106 to the top electrode 122 through the protruding liner 112 and the PCM material 114. In some embodiments, the PCM material 114 may be 20 nm to 50 nm in width and 30 nm to 100 nm in thickness (i.e., height).
[0023] In the embodiment shown, the bottom electrode 106 and the top electrode 122 are composed of a highly conductive material, such as a metal or metal compound, e.g., titanium nitride (TiN) or tungsten (W). The walls 110 include a highly resistive component composed of a dielectric (e.g., SiN) or a more resistive metal, e.g., tantalum nitride (TaN). The walls 110 may have a thickness, e.g., in the range of 5 nm to 50 nm. In addition, the protruding liner 112 is composed of a more resistive metal, e.g., TaN. The protruding liner 112 may have a thickness, e.g., in the range of 2 nm to 10 nm.
[0024] In the embodiment shown, the insulators 104, 108, 120 are composed of a dielectric (electrically insulating) material, such as, for example, SiN, SiO2, silicon nitride carbide (SiNC), or tetraethyl orthosilicate (TEOS). In some embodiments, all of the insulators 104, 108, 120 are the same material, while in other embodiments, different materials are used for some or all of the insulators 104, 108, 120. In some embodiments, the insulator 108 (and bottom electrode 106) has a thickness in the range of 10 nm to 100 nm.
[0025] In the embodiment shown, the PCM material 114 consists essentially of a phase change material such as a germanium-antimony-tellurium (GST) material, a gallium-antimony-tellurium (GaST) material, or a silver-iridium-antimony-telluride (AIST) material, although other materials may be used as desired. Examples of other PCM materials may include, but are not limited to, germanium-tellurium composites (GeTe), silicon-antimony-tellurium (Si-Sb-Te) alloys, gallium-antimony-tellurium (Ga-Sb-Te) alloys, germanium-bismuth-tellurium (Ge-Bi-Te) alloys, indium-tellurium (In-Se) alloys, arsenic-antimony-tellurium (As-Sb-Te) alloys, silver-indium-antimony-tellurium (Ag-In-Sb-Te) alloys, Ge-In-Sb-Te alloys, Ge-Sb alloys, Sb-Te alloys, Si-Sb alloys, Ge-Te alloys, and combinations thereof. The PCM material 114 may be undoped or doped (e.g., doped with one or more of oxygen (O), nitrogen (N), silicon (Si), or titanium (Ti)). The terms "composed essentially of" and "consist essentially of," as used herein with respect to the various layer materials, indicate that other materials, if present, do not substantially alter the basic properties of the recited material. For example, a PCM material 114 consisting essentially of GST material does not include other materials that substantially alter the basic properties of the GST material.
[0026] In the embodiment shown, the PCM cell 100 can be operated as a memory cell by passing a current pulse from the bottom electrode 106 to the top electrode 122 to program the PCM cell 100. This operation can be performed at various voltages and / or for various durations to read or write the value of the PCM cell 100. For example, to write, a high voltage (e.g., 1 volt (V) to 4 V) can be used for a short duration, which can cause the PCM material 114 to heat itself (by resistive heating) above its melting point. The PCM material 114 thereby performs the functions of a heater and a memory. After the flow of current stops, the PCM material 114 can cool rapidly, thereby forming an amorphous zone 126 in a process called "resetting." The amorphous zone 126 is a dome-shaped region of the PCM material 114 that has an amorphous configuration, while the remainder of the PCM material 114 is still of polycrystalline configuration. Generally, this amorphous configuration has no well-defined structure. However, localized, disorganized crystalline nuclei (i.e., small crystallized regions of the phase change material 114) may be present in the amorphous zones 126. The creation of the amorphous zones 126 may increase the electrical resistance of the entire PCM cell 100 compared to a purely polycrystalline configuration (such as the PCM cell 100 of FIG. 1A). These resistance values of the PCM cell 100 may be read, for example, by sending a current pulse at a low voltage (e.g., 0.2 V) from the bottom electrode 106 to the top electrode 122, without changing the state of the PCM material 114 (including the state of the amorphous zones 126) or the resistance value of the PCM cell 100.
[0027] Additionally, the PCM material 114 may be rewritten back to an exclusively polycrystalline configuration by "setting" the PCM cell 100. One method for setting the PCM material 114 may use a high voltage (e.g., 1V-4V) electrical pulse for a short period of time (e.g., 10 nanoseconds (ns)) that may cause the PCM material 114 to heat above its crystallization point but not to reach its melting point. Because the crystallization temperature is lower than the melting temperature, the PCM material 114 may anneal to form crystals after the flow of current has stopped. Another method for setting the PCM material 114 may use an electrical pulse with a relatively long (e.g., 1 microsecond) trailing edge (as opposed to a square pulse with a relatively short trailing edge on the order of a few nanoseconds) that is strong enough to heat the PCM material 114 above its melting point, after which the PCM material 114 is slowly cooled to allow the crystals to form. Either of these processes causes the electrical resistance across the polycrystalline-only PCM cell 100 to decrease, compared to a PCM cell 100 that includes an amorphous zone 126 (such as the PCM cell 100 of FIG. 1B). This new resistance can then be read using a current at a low voltage (e.g., 0.2 V) without changing either the state of the PCM material 114 or the resistance of the PCM cell 100.
[0028] In some embodiments, the melting temperature of the PCM material 114 is about 600° C. In some embodiments, the crystallization temperature of the PCM material 114 is about 180° C. In addition, the process of setting and resetting the PCM cell 100 can occur repeatedly, and in some embodiments, different amorphous zones 126 having different resistances can be created in the PCM material 114 (e.g., due to the inclusion of different sized amorphous zones 126 and / or different amounts of crystallization nuclei in the amorphous zones 126). This allows the PCM cell 100 to have a variety of different resistances that can be created by varying the reset parameters. Thereby, if the PCM cell 100 is considered to represent information digits, these digits may be non-binary (as opposed to traditional bits). However, in some embodiments, the PCM cell 100 can be used as a bit by including or not including uniform amorphous zones 126 in the PCM material 114. In such an embodiment, the PCM cell 100 may have a high resistance (also known as a low voltage output or a "0") or a low resistance (also known as a high voltage output or a "1").
[0029] The components and configuration of the PCM cell 100 allow the gap 118 to reduce thermal conduction away from the PCM material 114 because the gap 118 has a lower thermal conductivity than the B layer 130 does. This allows more of the heat generated in the PCM material 114 to remain within the PCM material 114, thereby improving the speed and efficiency of the PCM cell 100 and reducing the amount of energy required to tune / program the PCM cell 100. Additionally, degradation of the performance of the PCM cell 100 is also reduced, with the bottom wire 102 and top wire 124 heating less than they would be without the gap 118. Additionally, the protruding liner 112 thermally insulates the bottom electrode 106 from the PCM material 114, further improving the efficiency of the PCM cell 100.
[0030] Figure 2 is a flow chart of a method 200 of manufacturing a PCM cell 100. Figures 3A-3I are a series of diagrams of a method 200 of manufacturing a PCM cell 100. Figures 2 and 3A-3I will now be described in conjunction with one another, with each operation of the method 200 being illustrated by one of the Figures 3A-3I. Additionally, during this description, reference may be made to features of the PCM cell 100 shown in Figures 1A and / or 1B.
[0031] In the illustrated embodiment, the method 200 begins at operation 202, where a two-layer dielectric block 332 is formed over the bottom electrode 106 and the insulator 108. At operation 204, a mask 334 is formed over the block 332. The mask 334 is comprised of an organic planarization layer (OPL) 336, a silicon with anti-reflective coating (SiARC) 338, and a photoresist layer 340. The photoresist layer 340 includes gaps 342 for the formation of vias 344 during operation 206. More specifically, the vias 344 have a width smaller than the width of the bottom electrode 106, for example 20 nm. The vias 344 are formed by etching each layer of the block 332 in the same way, after which the mask 334 is removed.
[0032] In operation 208, the block 332 is selectively etched, for example using a wet process or an RIE process, to remove a portion of one type of bilayer dielectric material in the via 344 while leaving the other type of bilayer dielectric material intact. Thereby, in operation 208, a pore 346 is formed such that the stack 116 (including the A layer 128 and the B layer 130) has an inner surface 131 of the B layer 130 offset from the inner surface 129 of the A layer 128. In operation 210, a TaN layer 348 is formed on the stack 116 using a CVD or PVD process. Thereby, the TaN layer 348 follows the inner edge of the A layer 128 and avoids contact with the B layer 130, isolating the pore 346 into the cavity 350 and the gap 118. The formation of the gap 118 occurs under conditions of the CVD or PVD process, between which a vacuum exists. The vacuum may be, for example, a pressure of 10 milliTorr (mTorr) or less, which keeps some fluid (e.g., air) sealed within the gap 118. In some embodiments, an ALD process is used in operation 210 instead of CVD or PVD. However, if ALD is used, the resulting TaN layer 348 may penetrate further into the pores 346 toward the B layer 130, making the gap 118 smaller. This may reduce the thermal insulation of the stack 116, as air has a lower thermal conductivity than the dielectric material.
[0033] In operation 212, the TaN layer 348 is etched, for example using a RIE process, to remove its horizontal portions, thereby forming the walls 110 in addition to exposing the bottom electrode 106 and the stack 116. In operation 214, a protruding layer 352 and a PCM layer 354 are deposited inside the walls 110. More specifically, the protruding layer 352 is formed on the stack 116, the walls 110, and the bottom electrode 106, and the PCM layer 354 is formed on the protruding layer 352. In operation 216, chemical mechanical polishing (CMP) is performed to remove excess material from the protruding layer 352 and the PCM layer 354 to form the protruding liner 112 and the PCM material 114 adjacent to the stack 116, respectively. In operation 218, an insulator 120, a top electrode 122, and a top wire 124 are formed over the stack 116, the walls 110, the protruding liner 112, and the PCM material 114, respectively.
[0034] The components, configuration, and operation of the PCM cell 100 and method 200 allow for gaps 118 to form around the PCM material 114. This can occur because the B layer 130 is susceptible to at least one material removal process and the A layer 128 is resistant to this material removal process.
[0035] FIG. 4 is a flow chart of a method 400 of manufacturing a PCM cell 500. FIGS. 5A-5G are a series of cross-sectional views of the method 400 of manufacturing a PCM cell 500. FIG. 4 and FIG. 5A-5G will now be described in conjunction with one another, with each operation of the method 400 being illustrated by one of FIG. 5A-5G. During this description, reference may be made to features of PCM cell 100 (shown in FIG. 1) and PCM cell 500 (shown in FIG. 5G). Features in PCM cell 500 that are the same as PCM cell 100 may have the same reference numbers, and features in PCM cell 500 that are similar to features of PCM cell 100 may have reference numbers that are 400 higher.
[0036] In some embodiments, method 400 begins with operation 210 of method 200 (shown in FIG. 3E), while in other embodiments, method 400 begins after operation 212 of method 200 (shown in FIG. 3F). FIGS. 5A-5I illustrate the latter embodiment. In operation 414, a TiN layer 556 and a high electrical resistance layer 558 are deposited on the inside of the wall 110. More specifically, the TiN layer 556 is formed on the stack 116, the wall 110, and the bottom electrode 106, and a high electrical resistance layer 558 is formed on the TiN layer 556, which may be composed of, for example, SiN or highly resistive TaN. In operation 416, chemical mechanical polishing (CMP) is performed to remove excess material from the TiN layer 556 and the high electrical resistance layer 558 to form the heater 560 adjacent to the stack 116. At operation 418, a PCM layer 562, a TiN layer 564, and a SiN layer 566 are formed over the stack 116 and the heater 560. In some embodiments, the PCM layer 562 is about 80 nm thick, the TiN layer 564 is about 75 nm thick, and the SiN layer 566 is about 220 nm thick. In some embodiments, prior to operation 418, a protruding liner 568 (shown in phantom because it is not included in subsequent steps of method 400) is formed over the stack 116 and the heater 560.
[0037] In operation 420, masking and etching are performed to form the PCM material 514, the top electrode 522, and the hard mask 570, which expose the stack 116. In the embodiment shown, the lateral widths of the PCM material 514 and the top electrode 522 are the same, while the width of the heater 560 is reduced relatively significantly (e.g., by ⅓ to ⅙ or about ⅕). The PCM cell 500 can thereby be said to have a mushroom-shaped configuration, in which an electrical signal (i.e., current) can flow from the bottom electrode 104 to the top electrode 522 through the heater 560 and the PCM material 114. In contrast to the PCM cell 100, the PCM cell 500 includes a two-part heater / PCM portion comprised of the heater 560 and the separate PCM material 114. However, instead of relying on the PCM material 514 to heat itself, a heater 560 is used to program the PCM material 514, but the memory function can be operated in the same manner as the PCM cell 100.
[0038] At operation 422, an encapsulation layer 572 is formed over the stack 116, the PCM material 514, the top electrode 522, and the hard mask 570. The encapsulation layer 572 may be composed of, for example, SiN or silicon carbonitride (SiCN). At operation 424, an etch is performed to expose the insulator 108 to form an encapsulator 574 and a cap 576. At operation 426, an insulator 520 and a top wire 524 are formed over the insulator 108, the stack 116, the top electrode 522, the encapsulant 574, and the cap 576, respectively, to complete the PCM cell 500.
[0039] The components, configuration, and operation of the PCM cell 500 and method 400 allow for a gap 118 to form around the heater 560. This can occur because the B layer 130 is susceptible to at least one material removal process and the A layer 128 is resistant to this material removal process.
[0040] The description of various embodiments of the present invention is presented for illustrative purposes, but is not intended to be exhaustive and is not limited to the disclosed embodiments. Many changes and modifications will be apparent to those skilled in the art without departing from the scope of the described embodiments. The terms used in this specification are selected to best explain the principles of the embodiments, practical applications, or technical improvements beyond the technology found in the market, or to allow other skilled in the art to understand the embodiments disclosed herein.
[0041] In a preferred embodiment of the invention described herein, a phase change memory (PCM) cell is provided that includes a first electrode, a heater / PCM portion electrically connected to the first electrode, the heater / PCM portion including a PCM material, a second electrode electrically connected to the PCM material, and an electrical insulator stack surrounding the protruding liner, the stack defining a plurality of gaps, each of the gaps having a toroidal shape, axially spaced apart from one or more other gaps, and surrounding a portion of the heater / PCM portion. The stack preferably includes a plurality of first layers and a plurality of second layers alternating with the plurality of first layers, each gap being surrounded by two of the plurality of first layers and one of the plurality of second layers. The PCM cell may further include a protruding liner in direct contact with the first electrode, the second electrode, and the PCM material. The PCM cell may further include a wall in direct contact with the protruding liner and the stack. Each gap may further be surrounded by a wall. Each gap may surround a portion of the wall.The heater / PCM portion may further comprise a heater constructed from a highly electrically resistive material that is separate from the PCM material.
Claims
1. 1. A phase change memory (PCM) cell, comprising: A first electrode; a heater / PCM portion electrically connected to the first electrode, the heater / PCM portion including a PCM material; a second electrode electrically connected to the PCM material; an electrical insulation stack surrounding at least a portion of the heater / PCM section; wherein the stack comprises: a plurality of first layers constructed from a first material and having a plurality of first inner surfaces facing the heater / PCM portion; and a plurality of second layers alternating with the plurality of first layers, the plurality of second layers being composed of a second material different from the first material, the plurality of second layers having a plurality of second inner surfaces facing towards the heater / PCM portion; The PCM cell, wherein the second inner sides offset from the first inner sides form a plurality of gaps.
2. The PCM cell of claim 1 further comprising a protruding liner in direct contact with the first electrode, the second electrode, and the PCM material.
3. The PCM cell of claim 2 further comprising a wall in direct contact with said protruding liner and said stack.
4. The PCM cell of claim 3 , wherein each of the plurality of gaps is bounded by two of the plurality of first layers, one of the plurality of second layers, and the wall.
5. the plurality of first layers are in direct contact with the wall; The PCM cell of claim 3 , wherein the plurality of second layers are spaced apart from the wall.
6. The PCM cell of claim 3 , wherein each gap is further surrounded by said walls.
7. the first material is resistant to a material removal process; The PCM cell of claim 1 , wherein the second material is susceptible to the material removal process.
8. 10. The PCM cell of claim 1, wherein said heater / PCM portion further comprises a heater constructed from a highly electrically resistive material separate from said PCM material.
9. 1. A method for manufacturing a phase change memory (PCM) cell, comprising the steps of: forming a first electrode; forming an electrical insulator stack over the first electrode, the stack comprising: a plurality of first layers constructed from a first material; and forming a plurality of second layers alternating with the plurality of first layers, the plurality of second layers being composed of a second material different from the first material; forming a via in the stack; removing portions of the plurality of second layers from the vias while leaving the plurality of first layers intact; forming walls in the first layers within the vias to create gaps; forming a heater / PCM portion inside said wall; forming a second electrode over the heater / PCM portion; A method comprising:
10. The method of claim 9 , wherein each of the plurality of gaps is bounded by two of the plurality of first layers, one of the plurality of second layers, and the wall.
11. 10. The method of claim 9, further comprising forming a protruding liner over the first electrode and the wall prior to forming the heater / PCM portion, such that the protruding liner is located between the wall and the heater / PCM portion.
12. The method of claim 9 , wherein forming the heater / PCM portion inside the wall comprises depositing a PCM material inside the wall and over the stack.
13. forming said heater / PCM portion inside said wall; depositing a highly electrically resistive material inside the walls and over the stack to form a heater; depositing a PCM material over the heater and over the stack; 10. The method of claim 9, comprising:
Citation Information
Patent Citations
Phase change memory element
JP2008283163A
Semiconductor device, and method of manufacturing the same
JP2012059827A
Phase change memory device
JP2012209548A
Phase change memory device employing thermally insulating voids and sloped trench, and a method of making same