Medical devices and processes for manufacturing products, in particular medical devices
A balloon catheter with a multilayer structure comprising a metal and elastomeric layer serves as a sensor to accurately measure blood vessel elasticity, addressing the lack of detailed mechanical property assessment in current medical technologies for atherosclerotic diseases.
Patent Information
- Application Number
- JP2024525921
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-04-08
- Filing Date
- 2022-11-04
- Publication Date
- 2024-11-13
AI Technical Summary
Current medical technologies lack simple sensors for accurately assessing the mechanical properties of blood vessels, particularly in the context of atherosclerotic diseases, which are essential for advanced intraoperative diagnosis and treatment.
A medical device, specifically a balloon catheter, is designed with a multilayer structure comprising a metal layer and an elastomeric material layer, which can be used as a sensor unit to determine tissue elasticity by correlating resistance changes with balloon expansion, allowing for detailed mechanical property measurements.
The multilayer structure enables precise determination of blood vessel elasticity, facilitating improved diagnosis and treatment of vascular diseases by providing detailed mechanical property information without direct tissue contact.
Smart Images

Figure 2024542054000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to medical devices, products, more particularly processes for manufacturing medical devices, and multi-layer structures, more particularly multi-layer structures in the form of sensor units. [Background technology]
[0002] The prevalence of arteriosclerotic diseases is high and ever increasing, so advanced intraoperative diagnosis and treatment are of fundamental, social and economic importance. The digitalization of regulated medical applications requires secure databases and, for that, complementary and independent processes to obtain information. Various, sometimes redundant, sensors contribute to this. The procedures used to date in arteriosclerotic diseases, e.g. imaging methods (contrast angiography, Doppler, intravascular ultrasound) to assess the severity of vascular changes due to the disease, are limited to the analysis of the vessel diameter and thus the degree of stenosis. Therapeutic decisions can be improved by more detailed segmentation, but for this additional information on the mechanical properties of the vessel wall is required. Modern complex intravascular ultrasound systems are used in research, especially to gain insight into the local vascular structure, but simple sensor solutions for use in daily clinical practice that can fill the information gap, especially on the mechanical tissue properties, are not yet on the market. Summary of the Invention [Means for solving the problem]
[0003] It is an object of the present invention to provide a medical device, product, more particularly a process for producing a medical device, and further a multi-layer structure, which addresses in particular the market gap mentioned at the beginning.
[0004] This object is achieved by a medical device having the features of independent claim 1, a process for producing a product according to claim 15, and a multi-layer structure according to claim 16. Preferred embodiments of the invention are the subject of the dependent claims and the following description. The language of all claims is incorporated herein by express reference.
[0005] According to a first aspect, the present invention relates to a medical device, more particularly to a medical device in the form of a balloon catheter.
[0006] The medical device has at least one multi-layer structure, the at least one multi-layer structure being arranged one on top of the other. at least one metal layer, at least one layer of elastomeric material; The layer may include or consist of:
[0007] For purposes of the present invention, the expression "at least one multi-layer structure" may mean only one multi-layer structure or may mean a plurality of multi-layer structures, i.e., two or more multi-layer structures.
[0008] For purposes of the present invention, the multilayer structure may be more particularly formed as a laminate and / or film-like structure, more particularly a metal-polymer laminate composite, preferably a metal-polymer laminate film. Furthermore, for purposes of the present invention, the multilayer structure may be more particularly referred to as a metal-polymer multilayer composite structure, more particularly a metal-polymer bilayer composite structure.
[0009] For the purposes of the present invention, the expression "at least one metal layer" may mean only one metal layer or may mean a plurality of metal layers, i.e., two or more metal layers.
[0010] For the purposes of the present invention, the expression "metal layer" means a layer which comprises at least one metal, more particularly at least one metal in elemental form or in the form of an alloy, or a layer which is composed of at least one metal, more particularly at least one metal in elemental form or in the form of an alloy.
[0011] For purposes of the present invention, the expression "at least one elastomeric material layer" may mean, for purposes of the present invention, only one elastomeric material layer or may mean a plurality of elastomeric material layers, i.e., two or more elastomeric material layers.
[0012] For the purposes of the present invention, the expression "elastomeric material layer" means a layer comprising at least one elastomeric material, more particularly at least one elastomer, preferably at least one hyperelastic polymer, or a layer composed of at least one elastomeric material, more particularly at least one elastomer, preferably at least one hyperelastic polymer.
[0013] For the purposes of the present invention, the expression "hyperelastic polymer" is understood to mean a polymer, more particularly an elastomer having hyperelastic properties, and more particularly an elastomer having high reversible stretchability.
[0014] At least one metal layer preferably has a varying surface morphology, which is preferably designed to affect, more particularly increase or decrease, the sensitivity, more particularly the resistance behavior, to mechanical stress, more particularly stretching.
[0015] The invention is based in particular on the surprising discovery that the multi-layer structure provided by the invention can be used as a sensor unit in medicine, more particularly for determining the elasticity of tissues, preferably in particular the elasticity of hollow organs such as blood vessels.
[0016] In one embodiment of the present invention, the at least one elastomeric material layer is selected from the group consisting of elastomers, thermoplastic elastomers, thermoplastic polyamide elastomers, thermoplastic copolyester elastomers, olefin-based thermoplastic elastomers, thermoplastic styrene block copolymers, urethane-based thermoplastic elastomers, olefin-based thermoplastic vulcanizates, olefin-based crosslinked thermoplastic elastomers, natural rubber vulcanizates, synthetic rubber vulcanizates, styrene-butadiene rubber, butadiene rubber (BR), acrylonitrile-butadiene rubber (NBR), butyl rubber (IIR), ethylene-propylene-diene rubber (EPD), and the like. M), chloroprene rubber (CR), polyisoprene rubber (IR), polyalkylsiloxane, polydimethylsiloxane, silicone rubber, silicone elastomer, methyl silicone, vinyl methyl silicone, phenyl vinyl methyl silicone, phenyl modified silicone, fluoro alkyl silicone, fluoro vinyl methyl silicone, and a mixture of at least two of the aforementioned elastomeric materials, more particularly a superelastic material, is included or is composed of at least one elastomeric material, more particularly a superelastic material, selected from the group consisting of:
[0017] Preferably, at least one layer of elastomeric material comprises or is composed of a polyalkylsiloxane, more particularly polydimethylsiloxane.
[0018] Furthermore, the at least one layer of elastomeric material may more particularly be formed as a film.
[0019] More particularly, at least one layer of elastomeric material may be formed, more particularly directly or indirectly, on a surface of the medical device, more particularly on the outer and / or inner surface, preferably on the outer surface.
[0020] In a further embodiment of the invention, the at least one elastomeric material layer has a layer thickness of 0.0001 mm to 0.2 mm, more particularly 0.0005 mm to 0.1 mm, preferably 0.001 mm to 0.05 mm.
[0021] In a further embodiment of the invention, the at least one metal layer comprises or is composed of at least one metal, more particularly a metal in elemental form or in the form of an alloy, selected from the group consisting of gold, platinum, indium, tin, copper, silver, gallium and a mixture, preferably an alloy, of at least two of the aforementioned metals.
[0022] Furthermore, the at least one metal layer may more particularly be formed as a film.
[0023] Further, the at least one metal layer may be serpentine in shape and cover or coat the at least one elastomeric material layer at least in certain portions or areas, more particularly only in certain portions or areas, or continuously.
[0024] Preferably, the thickness of the at least one metal layer is less than the thickness of the at least one elastomeric material layer.
[0025] In a further embodiment of the invention, the at least one metal layer has a layer thickness of less than or equal to 150 nm, more particularly between 10 nm and 100 nm, preferably between 40 nm and 80 nm.
[0026] In a further embodiment of the present invention, at least one elastomeric material layer is covered or coated, more particularly directly or indirectly, by at least one metal layer. In addition, at least one elastomeric material layer may in principle be covered or coated completely, i.e. continuously or over the entire surface area, or partially, i.e. only in certain parts or in certain areas, by at least one metal layer. However, at least one elastomeric material layer is preferably only partially covered or coated by at least one metal layer. Particularly preferably, at least one elastomeric material layer is covered or coated only in certain parts or in certain areas directly by at least one metal layer.
[0027] In a further embodiment of the present invention, at least one adhesive layer is disposed or formed between the at least one metal layer and the at least one elastomeric material layer.
[0028] For purposes of the present invention, the phrase "at least one adhesive layer" can mean only one adhesive layer or can mean a plurality of adhesive layers, i.e., two or more adhesive layers.
[0029] For the purposes of the present invention, the expression "adhesion layer" means a layer comprising or consisting of at least one material capable of allowing and / or improving adhesion between at least one metal layer and at least one layer of elastomeric material.
[0030] Furthermore, the at least one adhesive layer may directly or indirectly cover or coat the at least one elastomeric material layer. More specifically, the at least one adhesive layer may cover or coat the at least one elastomeric material layer completely, i.e. continuously or over the entire surface area, or only partially, i.e. in specific parts or specific areas. However, the at least one adhesive layer preferably only partially covers the at least one elastomeric material layer.
[0031] Furthermore, the at least one metal layer may directly or indirectly cover or coat the at least one adhesive layer. More specifically, the at least one metal layer may cover or coat the at least one adhesive layer completely, i.e. continuously or over the entire surface area, or only partially, i.e. in specific parts or specific areas. However, the at least one metal layer preferably completely covers the at least one adhesive layer.
[0032] In a further embodiment of the invention, the at least one adhesive layer is covered or coated, more particularly directly, preferably completely, by the at least one metal layer, and the at least one elastomeric material layer is covered or coated, more particularly directly, preferably only in certain parts or in certain areas, by the at least one adhesive layer.
[0033] In a further embodiment of the invention, the at least one adhesion layer comprises or consists of at least one material selected from the group consisting of titanium, aluminum, chromium, and a mixture of at least two of the foregoing materials.
[0034] Furthermore, the at least one adhesive layer may more particularly be formed as a film.
[0035] Further, the at least one adhesive layer may be serpentine in shape, at least in certain portions or areas, more particularly only in certain portions or areas, or continuously, covering or coating the at least one elastomeric material layer.
[0036] Preferably, the thickness of the at least one adhesive layer is less than the thickness of the at least one elastomeric material layer.
[0037] More particularly, the thickness of the at least one adhesive layer may be less than the thickness of the at least one metal layer.
[0038] Preferably, at least one adhesion layer has a layer thickness of less than or equal to 20 nm, more particularly between 3 nm and 20 nm, preferably between 4 nm and 10 nm.
[0039] In a further embodiment of the invention, the at least one metal layer and / or the at least one adhesive layer are formed as conductor tracks. The one or more conductor tracks are configured to transmit an electrical measurement signal. In order to evaluate the electrical measurement signal, in this embodiment of the invention, the at least one metal layer and / or the at least one adhesive layer may be in contact or contactable with an evaluation unit for evaluating the electrical measurement signal via electrical conduction.
[0040] In a further embodiment of the invention, the at least one multilayer structure further comprises at least one additional elastomeric material layer, i.e. only one additional elastomeric material layer, or multiple, i.e. two or more elastomeric material layers. Preferably, the at least one metal layer is covered or coated, more particularly directly or indirectly, preferably directly, by the at least one additional elastomeric material layer.
[0041] Preferably, the thickness of the at least one metal layer is less than the thickness of the at least one additional elastomeric material layer.
[0042] More preferably, the thickness of the at least one adhesive layer is less than the thickness of the at least one additional layer of elastomeric material.
[0043] The at least one additional layer of elastomeric material may have a layer thickness of 0.001 mm to 0.15 mm, more particularly 0.001 mm to 0.1 mm, preferably 0.001 mm to 0.05 mm.
[0044] Furthermore, the at least one additional layer of elastomeric material may be more particularly formed as a film.
[0045] Furthermore, the at least one additional elastomeric material layer and the at least one elastomeric material layer may be identical or different in shape, in particular with regard to the elastomeric material and / or layer thickness.
[0046] In addition, the at least one additional elastomeric material layer, more particularly independent of the at least one elastomeric material layer, may be selected from the group consisting of elastomers, thermoplastic elastomers, thermoplastic polyamide elastomers, thermoplastic copolyester elastomers, olefin-based thermoplastic elastomers, thermoplastic styrene block copolymers, urethane-based thermoplastic elastomers, olefin-based thermoplastic vulcanizates, olefin-based crosslinked thermoplastic elastomers, natural rubber vulcanizates, synthetic rubber vulcanizates, styrene-butadiene rubber, butadiene rubber (BR), acrylonitrile-butadiene rubber (NBR), butyl rubber (IIR), ethylene- It may comprise or be composed of an elastomeric material, more particularly a superelastic material, selected from the group consisting of propylene-diene rubber (EPDM), chloroprene rubber (CR), polyisoprene rubber (IR), polyalkylsiloxane, polydimethylsiloxane, silicone rubber, silicone elastomer, methyl silicone, vinyl methyl silicone, phenyl vinyl methyl silicone, phenyl modified silicone, fluoroalkyl silicone, fluorovinyl methyl silicone, and a mixture of at least two of the foregoing elastomeric materials.
[0047] Preferably, the at least one additional layer of elastomeric material comprises or is composed of a polyalkylsiloxane, more particularly polydimethylsiloxane.
[0048] In a further embodiment of the invention, at least one multilayer structure or at least one metal layer has a varying surface morphology. More particularly, at least one multilayer structure or at least one metal layer may have corrugated and / or non-corrugated surface areas. Preferably, at least one multilayer structure or at least one metal layer has surface areas with cracks, more particularly microcracks, more particularly corrugated and / or non-corrugated surface areas, and / or surface areas without cracks, more particularly corrugated and / or non-corrugated surface areas. Particularly preferably, at least one multilayer structure or at least one metal layer has surface areas with cracks, more particularly microcracks, more particularly corrugated and / or non-corrugated surface areas, and corrugated surface areas without cracks. The varying surface morphology advantageously makes it possible to selectively influence, more particularly increase or decrease, the sensitivity of the at least one metal layer to mechanical stresses, more particularly to stretching.
[0049] For the purposes of the present invention, the expression "microcracks" is understood to mean cracks having at least one dimension in the micrometer and / or nanometer range, more particularly selected from the group consisting of length, width, depth and a combination of at least two of the aforementioned dimensions, more particularly in the range of 1 nm to 5 μm, more particularly 10 nm to 2 μm, preferably 20 nm to 1 μm. The formation of the cracks preferably depends on the applied coating parameters and / or on the pretreatment of the surface of at least one layer of elastomeric material.
[0050] For the purposes of the present invention, the expression "crack-free corrugated surface area" is understood to mean a discontinuously repeated corrugated deformation of the surface of at least one metal layer, preferably caused by compressive stresses in the at least one metal layer, more particularly by deformation of at least one underlying elastomeric material layer. Preferably, the crack-free corrugated surface area has at least one dimension in the micrometer and / or nanometer range, more particularly selected from the group consisting of period length and amplitude in the range of 10 nm to 15 μm, more particularly 20 nm to 10 μm, preferably 40 nm to 6 μm, and more particularly selected from the group consisting of combinations of the two aforementioned dimensions.
[0051] In a further embodiment of the invention, the at least one multi-layer structure is a part of the surface, more particularly the outer surface and / or the inner surface, of the medical device. More particularly, the medical device, more particularly the outer surface and / or the inner surface of the medical device, may be coated, preferably at least in certain parts or in certain areas, with the at least one multi-layer structure.
[0052] In a further embodiment of the invention, at least one multi-layer structure is part of, integrated into, or formed within the wall of the medical device.
[0053] Furthermore, the at least one multi-layer structure may in principle be formed in the longitudinal and / or transverse or circumferential direction of the medical device. Preferably, the at least one multi-layer structure is formed in the circumferential direction of the medical device.
[0054] Additionally, at least one of the multi-layer structures may be formed as a strip.
[0055] More particularly, the medical device may have multiple, more particularly strip-like, multi-layer structures formed longitudinally and / or laterally or circumferentially about the medical device.
[0056] In a further embodiment of the invention, the medical device is curved, more particularly cylindrically curved in shape.
[0057] Preferably, the medical device is cylindrical, more particularly hollow cylindrical, or tubular.
[0058] In a further embodiment of the invention, the medical device is in the form of a catheter, preferably a balloon catheter.
[0059] For the purposes of the present invention, the expression "balloon catheter" is understood to mean a catheter, more particularly a catheter made of plastic, rubber, silicon, metal or glass, and equipped with a balloon, which can be inflated, i.e. expanded, by compressed air or liquid.
[0060] For example, the catheter may take the form of an angiography catheter, an embolus removal catheter, a cardiac catheter, a peripheral venous catheter, a central venous catheter, a Broviac catheter, a Fogarty catheter, a Hickman catheter, a Swan-Ganz catheter, an endotracheal catheter, a bronchial catheter, a bladder catheter, a nephrostomy catheter, a ureteral catheter, an enterostomy catheter, a Chardon catheter, a Demers-Katheter, a balloon perfusion catheter, a flow-directed catheter, a pigtail catheter, or a double-J catheter.
[0061] The catheter is particularly preferably in the form of a balloon catheter, more particularly a plastic catheter with a balloon (blocking balloon) at its tip that can be inflated with compressed air or liquid. The balloon catheter may be designed, for example, for angioplasty, more particularly percutaneous transluminal coronary angioplasty (PTCA), embolectomy, valvuloplasty, more particularly heart valve stenosis, catheterization of the bladder, blocking or dilating the bronchi.
[0062] Particularly preferably, the medical device takes the form of a balloon catheter, the balloon of the balloon catheter comprising at least one multi-layer structure.
[0063] In a further embodiment of the invention, the at least one multi-layer structure constitutes at least one sensor unit, more particularly at least one tactile sensor unit. Preferably, the at least one sensor unit takes the form of at least one sensor stack, more particularly a sensor stack with a layer structure. The at least one sensor unit is preferably set up for recording a measurement variable, more particularly a physical measurement variable, and for converting this into a measurement signal, preferably an electrical measurement signal. The measurement variable may be more particularly a mechanical property, for example stretchability or elasticity, or a structural and / or functional parameter of a tissue, more particularly a hollow organ, preferably a blood vessel, more particularly an artery. Alternatively or in combination, the measurement variable may be temperature, hydrostatic pressure, or other measurement variables, more particularly variables of interest in therapy and / or diagnosis.
[0064] Preferably, the at least one sensor unit is configured to record a measurement variable characterizing a blood vessel, more particularly an artery, such as stretchability or elasticity, which has the advantage that it allows the diagnosis, more particularly intraoperative diagnosis, and / or optimization of the treatment of vascular diseases, more particularly arteriosclerotic diseases.
[0065] If the medical device takes the form of, for example, a balloon catheter and at least one multi-layer structure forms part of the balloon of the balloon catheter, it is advantageously possible to determine the elasticity of the blood vessel, more particularly of the artery, in particular tactilely, for example by recording a resistance, more particularly an electrical resistance, via the sensor unit, which resistance correlates with the expansion / inflation of the balloon of the balloon catheter and with the pressure used to expand / inflate the balloon of the balloon catheter and in particular increases reversibly in a linear and / or non-linear manner, and which allows the elasticity of the blood vessel, more particularly of the artery, to be interpreted, in particular by comparing it with a reference behavior without contact with the surrounding tissue.
[0066] According to a second aspect, the present invention relates to a process for manufacturing a product, preferably a medical device, in particular a medical device according to the first aspect of the invention. The product may more particularly be formed as a metal-polymer laminate composite, more particularly a metal-polymer laminate film, more particularly a thin metal-polymer laminate film. The process comprises the following steps: a) producing at least one multi-layer structure having at least one metal layer, more particularly a metal layer with a varying surface morphology, and at least one layer of an elastomeric material; b) transferring the at least one multi-layer structure to a substrate to form a substrate including the at least one multi-layer structure.
[0067] Preferably, step b) is carried out prior to the use of the substrate, in particular as a medical device, so as to avoid any relevant changes in the surface morphology of the at least one metallic layer.
[0068] The substrate used may in principle be planar, i.e. horizontal or flat, but it is preferred to use non-planar, more particularly curved, substrates. It is preferred to use cylindrical or cylindrically curved substrates, more particularly hollow cylindrical or tubular substrates, or conical substrates. Preferably, the substrate is a precursor, more particularly a component such as a blank, part or semi-finished product of a medical device.
[0069] When carrying out step a), the at least one multilayer structure is preferably produced on a transfer film, more particularly a semi-compliant transfer film, which is preferably placed on a carrier. In other words, the at least one multilayer structure is preferably produced on a carrier functionalized or coated with a transfer film. Preferably, the transfer film is removable from the carrier, more particularly peelable. The carrier used may be, for example, a wafer, more particularly in the form of a circular or rectangular, more particularly rectangular or square slice. Suitable wafers may be produced from monocrystalline or polycrystalline blanks ("ingots"). Furthermore, the wafer may comprise or consist of monocrystalline silicon and / or another material, for example selected from the group consisting of silicon carbide, gallium arsenide, indium phosphide, and mixtures of at least two of the aforementioned materials. Furthermore, the wafer may have a thickness of, for example, 0.5 mm. As transfer film, it is possible to use a film having, for example, an acrylic and / or methacrylic adhesive layer or adhesive surface. Preferably, the decrease in adhesion of the adhesive layer or adhesive surface is brought about by exposure to UV light, so that the carrier film can advantageously be peeled off more easily from the carrier, while the adhesion to the carrier remains strong enough to avoid premature peeling of the carrier film in further process steps. In addition to the adhesive layer, the transfer film may comprise further layers, more particularly non-adhesive layers, for example of polyethylene terephthalate. The transfer film can be placed on the substrate, for example with a layer thickness of 40 μm to 240 μm, in particular 60 μm to 155 μm, preferably 75 μm to 120 μm. Preferably, the substrate is coated on one side with the transfer film, more particularly by adhesion.
[0070] Preferably, the at least one elastomeric material layer is applied on the transfer film when carrying out step a), more particularly by spin-coating. In principle, the at least one elastomeric material layer may be applied directly or indirectly on the transfer film, but in order to avoid contact of the at least one elastomeric material layer with UV light and the associated possible deterioration of the at least one elastomeric material layer, it is preferably applied after exposing the transfer film to UV light to reduce adhesion. Preferably, the at least one elastomeric material layer is applied directly on the transfer film. Furthermore, the at least one elastomeric material layer may be applied only partially on the transfer film, i.e. only in specific parts or specific areas, or continuously, i.e. over the entire surface area. Preferably, the at least one elastomeric material layer is applied continuously on the transfer film. Then, preferably, the at least one metal layer is applied on the at least one elastomeric material layer. In principle, the at least one metal layer may be applied directly or indirectly on the at least one elastomeric material layer. Furthermore, the at least one metal layer may be applied only partially on the at least one elastomeric material layer, i.e. only in certain parts or certain areas, or continuously, i.e. over the entire surface area. Preferably, the at least one metal layer is applied continuously on the at least one elastomeric material layer. When performing spin-coating, the elastomeric material layer, more precisely the elastomeric material or its precursor, more particularly in the form of a curable prepolymer (preferably in the form of a viscous curable prepolymer that does not contain air), can be spin-coated on the transfer film at a speed of, for example, 400 rpm (revolutions per minute) to 3000 rpm, more particularly 500 rpm to 2000 rpm, preferably 600 rpm to 900 rpm. Furthermore, the spin-coating may be performed for a period of 30 seconds to 120 seconds, in particular 45 seconds to 90 seconds, preferably 60 seconds to 80 seconds. In principle, the spin-coating can be performed at different speeds and for different periods.This advantageously allows to improve the uniformity of the at least one elastomeric material layer obtained. At particularly high spin speeds, the acceleration in rpm / s (revolutions per minute per second) may also be varied up to the desired spin speed. This ensures a uniform flow behavior and uniform wetting after the initial application of the precursor of the elastomeric material, in particular the prepolymer. The acceleration may here be varied from 100 rpm / s to 1000 rpm / s, in particular from 150 rpm / s to 800 rpm / s, preferably from 200 rpm / s to 400 rpm / s. A vacuum or reduced pressure is then preferably applied, for example for 10 to 20 minutes. This advantageously allows to form a defect-free, preferably uniform elastomeric material layer, more particularly an elastomeric material layer in the form of a film. The elastomeric material may then be cured, for example at a temperature between 25° C. and 120° C., in particular for a period between 30 minutes and 48 hours. The curing of the elastomeric material layer may preferably be carried out in an oven.
[0071] Preferably, the at least one metal layer is applied onto the at least one elastomeric material layer by a process of structuring the surface of the at least one elastomeric material layer, more particularly by photolithography, followed by a vacuum-based coating process, more particularly by physical vapor deposition, preferably thermal evaporation, more particularly directly or indirectly.
[0072] Preferably, the at least one adhesive layer is first applied on the at least one elastomeric material layer in at least certain parts or certain areas, more particularly only in certain parts or certain areas, or continuously, i.e. over the entire surface area, in particular directly or indirectly, by a process of building up the surface of the at least one elastomeric material layer, more particularly by photolithography and a subsequent vacuum-based coating process, more particularly by physical vapor deposition, preferably by thermal evaporation, and then the at least one metal layer is applied on the at least one adhesive layer in at least certain parts or certain areas, more particularly by a process of building up the surface of the at least one elastomeric material layer, more particularly by photolithography and a subsequent vacuum-based coating process, more particularly by physical vapor deposition, more particularly directly or indirectly, preferably directly, while maintaining a vacuum or reduced pressure, more particularly by forming the at least one adhesive layer using a reactive metal.
[0073] To carry out photolithography, a photoresist is preferably first applied onto the at least one elastomeric material layer. The photoresist used can in principle be a positive or negative resist. A positive resist is understood to mean a photoresist which is removed in the areas which have been altered, more particularly those which have been irradiated with light. A negative resist is understood to mean a photoresist which is removed in the areas which have not been altered, more particularly those which have not been exposed to light. It is preferable to use a negative resist as the photoresist. Preferably, the photoresist is applied onto the at least one elastomeric material layer by spin coating. The spin coating can be carried out, for example, at a speed of 1000 rpm to 4000 rpm, more particularly 2000 rpm to 3000 rpm, more particularly for a period of 45 seconds to 90 seconds, preferably 60 seconds to 75 seconds. The photoresist applied onto the at least one elastomeric material layer can then be heated, more particularly at a temperature of 90 ° C to 110 ° C, more particularly for a period of 90 seconds to 2 minutes. This causes the solvents present in the photoresist, in particular propylene glycol monomethyl ether acetate (PGMEA), to be released and the photoresist to be stabilized. A photomask is then laminated onto the photoresist applied onto at least one layer of elastomeric material. The photomask used can in principle be a mask made of high-purity quartz glass or calcium fluoride. The photomask can also be provided, for example on one side, with a chrome layer, in particular a structured chrome layer.
[0074] The next step in photolithography is preferably exposure to light, which advantageously transfers the image of the photomask onto the photoresist. This results in a lithographic mask that allows further processing, preferably by chemical and / or physical processes. The exposure to light is preferably at least 50 mJ / cm 2 . 2 to 150 mJ / cm 2 , especially 60 mJ / cm 2 to 120 mJ / cm 2 , preferably 70 mJ / cm 2to 100 mJ / cm 2 The radiation source used may be, for example, a mercury lamp, more particularly a high-pressure mercury lamp. High-pressure mercury lamp is understood to mean a mercury lamp with an operating pressure of up to about 1 MPa, which is reached after a few minutes of warm-up. The light used to expose the photoresist may more particularly have a wavelength of 280 nm to 700 nm, more particularly 300 nm to 500 nm, preferably 350 nm to 450 nm.
[0075] After exposure, it is possible to carry out a heating step, more particularly at a temperature of from 100°C to 180°C, preferably from 100°C to 120°C, more particularly for a heating step of from 2 minutes 30 seconds to 3 minutes 30 seconds, preferably for 2 minutes 50 seconds to 3 minutes.
[0076] After the heating step, the exposed photoresist, together with the carrier, the transfer film, and the at least one layer of elastomeric material, can be transferred directly to a preheated oven. The oven is preferably preheated to a temperature lower than that of the heating step described in the previous paragraph. Preferably, the oven is preheated to a temperature of 100° C.
[0077] After the above mentioned heating step, more particularly before the photoresist is developed as described below, preferably after switching off the above mentioned oven, the photoresist can be cooled, more particularly to a temperature of 18° C. to 30° C., preferably 20° C. to 25° C. The photoresist can be further cooled, more particularly over a period of 5 hours, which advantageously prevents the formation of cracks in the photoresist.
[0078] Finally, when performing photolithography, the photoresist is preferably developed. This essentially dissolves the light-exposed areas of the photoresist, or, more particularly, dissolves the unexposed areas of the photoresist, if the photoresist is hardened by exposure to light. A developer is preferably used to develop the photoresist. This allows the soluble areas of the photoresist to be dissolved and then removed, for example by wet chemical spraying, immersion or dripping. The developer used may be, for example, an aqueous solution containing tetramethylammonium hydroxide (TMAH). Alternatively, a buffered aqueous sodium hydroxide solution, a buffered aqueous potassium hydroxide solution, or a developer based on sodium phosphate and sodium metasilicate may be used. The development of the photoresist may be carried out, for example, for a period of 1 minute 30 seconds to 2 minutes 20 seconds, more particularly 1 minute 50 seconds to 2 minutes 10 seconds. It may then be rinsed with water, more particularly deionized water, and dried under an inert gas, more particularly nitrogen.
[0079] Alternatively, structuring of the surface of at least one elastomeric material layer can be carried out using an aperture mask or stencil mask, for example a mask comprising or consisting of nickel or a nickel-phosphorus alloy, followed by exposure to ultraviolet radiation.
[0080] In order to be able to affect a changing surface morphology after deposition of at least one metal layer with or without at least one adhesion layer in different areas, it is possible to carry out a selective plasma treatment of the surface of the elastomeric material layer, in particular before the introduction of the elastomeric material layer into the coating chamber. For this purpose, the photolithographic masking and / or the corresponding stencil mask carried out for this purpose may be designed to expose only the part of the surface that will be subsequently coated with at least one metal layer and optionally with at least one adhesion layer. By introducing it into the plasma chamber and exposing the exposed surface to the plasma, the surface properties of the elastomeric material surface can be changed, thus influencing the surface morphology of the at least one metal layer in these areas that will be subsequently formed during deposition. The effect of the plasma on the surface of the at least one elastomeric material layer also depends on the choice of process gas and the process parameters. In order to influence the layer growth such that a corrugated closed surface is formed, in particular oxygen can be used as process gas, preferably with a plasma power of 50 W to 150 W, a process pressure of 0.5 mbar to 1.5 mbar and a process gas flow rate of 100 sccm (standard cubic centimeters per minute) to 700 sccm, preferably 300 sccm to 500 sccm. The duration of the plasma treatment is 5 to 40 seconds, more particularly 10 to 35 seconds, preferably 15 to 30 seconds.
[0081] The physical vapor deposition may be selected from the group consisting of thermal evaporation, electron beam evaporation, laser beam evaporation, arc evaporation, molecular beam epitaxy, sputtering, ion beam assisted deposition, ion plating, ICB techniques, and a combination of at least two of the aforementioned physical vapor depositions. In physical vapor deposition, the material to be deposited is generally present in solid form in a coating chamber, which is in a near vacuum. As a result of bombardment by a laser beam, magnetically deflected ions or electrons, arc discharge, or heating (especially to near the boiling point), the material, also called the target, is evaporated. The evaporated material travels ballistically or under the guidance of an electric field in the coating chamber, colliding with the part to be coated to form a layer. To ensure that the evaporated particles actually reach the part to be coated and are not lost due to scattering by gas particles, the operation is usually carried out under reduced pressure. Typical operating pressures are 10 -4 The range is from Pa to 10 Pa.
[0082] After applying the at least one metal layer onto the at least one adhesive layer and / or onto the at least one elastomeric material layer, the photomask constituting the unexposed areas of the photoresist is preferably removed. The unexposed areas of the photoresist are preferably removed with an organic solvent, such as acetone.
[0083] If an aperture mask or stencil mask is used to structure the surface of the at least one elastomeric material layer, the mask is preferably removed, e.g. by peeling off, after application of the at least one metal layer onto the at least one adhesive layer and / or the at least one elastomeric material layer.
[0084] When carrying out step a), it is preferred that at least one additional elastomeric material layer is applied onto the at least one metal layer, more particularly by spin-coating. For further features and advantages, in particular those relating to the at least one additional elastomeric material layer and to spin-coating, reference is made in full to the above description. The features and advantages described in particular in relation to the at least one elastomeric material layer also apply to the at least one additional elastomeric material layer.
[0085] Various contacting techniques can be employed to contact the at least one metal layer with the at least one adhesive layer between the at least one elastomeric material layer and the at least one additional elastomeric material layer. For example, contacting can be performed at predefined pockets in the at least one additional elastomeric material layer, where a conductive connection is formed, for example by a conductive viscous paste, between defined contact pads of the at least one metal layer with the at least one adhesive layer and leads leading to the evaluation periphery, embedded in the at least one additional elastomeric material layer.
[0086] More preferably, before carrying out step b), the at least one multi-layer structure is removed, more particularly peeled off, together with the transfer film from the carrier.
[0087] More preferably, before carrying out step b), the substrate is placed on a core to form a cylindrical, tubular or conical substrate. The core is useful for this purpose to be cylindrical, tubular or conical. More particularly, the core may be in the form of a stamp. Furthermore, the core may comprise or consist of a metal. The metal may be, for example, aluminum.
[0088] Preferably, the cylindrical, tubular or conical substrate is peeled off from the core and the core is replaced by a water-soluble material, more particularly a water-soluble wax. In other words, the previous core is replaced by a core, preferably composed of a water-soluble core, more particularly a water-soluble wax. The water-soluble wax may have a melting point of 50°C to 60°C, in particular 55°C to 60°C. Preferably, the peeling off of the cylindrical, tubular or conical substrate from the core and / or the replacement of the core by the water-soluble material is carried out in a molding tool or mould, more particularly a molding tool or mould composed of multiple parts that can be opened and closed, preferably composed of two parts. Preferably, the molding tool or mould has a shape that corresponds to the shape of the product to be produced, especially when in the assembled or closed state.
[0089] Preferably, at least one multi-layer structure is then transferred to a cylindrical, tubular or conical shaped substrate, this step being preferably carried out outside of a forming tool or mould.
[0090] The water-soluble substances are then removed, in particular by rinsing with water. This step can preferably be carried out in a molding tool or mould, which advantageously makes it possible to avoid undesirable stresses on the at least one multi-layer structure.
[0091] When carrying out step b), the at least one multilayer structure is preferably applied onto the substrate using a transfer film. Preferably, the transfer film is removed after forming a connection, preferably a material connection, between the at least one multilayer structure, more particularly at least one elastomeric material layer and / or at least one additional elastomeric material layer of the at least one multilayer structure, and the substrate. The connection may be influenced, for example, by curing or crosslinking of the elastomeric material or precursor, more particularly a prepolymer, more particularly based on the formation of a covalent bond. Alternatively or in combination, the connection may be based on the formation of a non-covalent bond, more particularly selected from the group consisting of van der Waals forces, hydrogen bonds, ionic bonds, coordination bonds, and a combination of at least two of the aforementioned non-covalent bonds. Furthermore, the connection between the at least one multilayer structure, more particularly at least one elastomeric material layer and / or at least one additional elastomeric material layer of the at least one multilayer structure, and the substrate may be formed in a molding tool or mold, more particularly in the already mentioned molding tool or mold. For this purpose, the substrate comprising the at least one multilayer structure may remain in the molding tool or mould for 12 hours to 72 hours, more particularly 24 hours to 48 hours, more particularly at a temperature of 18°C to 30°C, preferably 20°C to 25°C.
[0092] More preferably, the process further comprises the following step c): - overmolding, more particularly by injection molding, an additional elastomeric material onto the substrate provided with the at least one multilayer structure, more particularly onto the substrate provided with the at least one multilayer structure transferred onto the substrate.
[0093] This advantageously makes it possible to establish the final, i.e. definite, shape of the substrate with the at least one multi-layer structure and thus the shape of the product to be manufactured.
[0094] Preferably, step c) is (also) carried out in a forming tool or mould, more particularly in a forming tool or mould as already mentioned.
[0095] With regard to further features and advantages of the process, reference is made in its entirety to the statements made under the first aspect of the invention, which also apply to the process according to the second aspect of the invention.
[0096] According to a third aspect, the present invention relates to a multi-layer structure, more particularly a sensor or sensor unit, comprising the following layers arranged one on top of the other: at least one metal layer; at least one layer of elastomeric material.
[0097] With regard to further features and advantages of the multilayer structure, in particular with regard to the at least one metal layer and the at least one elastomeric material layer, and more particularly with regard to the optionally present at least one adhesive layer, reference is made in full to the above descriptions, and more particularly to those made below in the first aspect of the invention, which also apply to the multilayer structure according to the third aspect of the invention.
[0098] According to a fourth aspect, the present invention relates to a process for manufacturing a multi-layer structure, more particularly to a process according to the third aspect of the invention, comprising the following steps: a) applying at least one layer of elastomeric material onto a transfer film; b) applying at least one metal layer onto the at least one elastomeric material layer; or a) applying at least one layer of elastomeric material onto a transfer film; b) applying at least one adhesive layer onto the at least one elastomeric material layer; c) applying at least one metal layer onto the at least one adhesive layer.
[0099] Preferably, the transfer film is mounted on a carrier.
[0100] When carrying out step a), the at least one elastomeric material layer may be applied directly or indirectly onto the transfer film. Preferably, when carrying out step a), the transfer film is completely, i.e. continuously or over the entire surface area, covered or coated with the at least one elastomeric material layer.
[0101] Furthermore, when carrying out step b), the at least one metal layer or the at least one adhesive layer may be applied directly or indirectly onto the at least one elastomeric material layer. The at least one elastomeric material layer may in principle be covered or coated completely or only in certain parts or in certain areas with the at least one metal layer or the at least one adhesive layer. Preferably, the at least one metal layer or the at least one adhesive layer covers or coats the at least one elastomeric material layer only in certain parts or in certain areas.
[0102] Furthermore, when carrying out step c), the at least one metal layer may be applied directly or indirectly onto the at least one adhesive layer. The at least one adhesive layer may in principle be completely covered or coated with the at least one metal layer or only in certain parts or areas. Preferably, the at least one metal layer completely covers or coats the at least one adhesive layer.
[0103] With regard to further features and advantages of the process, in particular those relating to the at least one metal layer, the at least one elastomeric material layer and the at least one adhesive layer, reference is made in full to the above descriptions, and more particularly to those made under the second aspect of the invention, which also apply to the process according to the fourth aspect of the invention.
[0104] Further features and advantages of the invention will become apparent from the claims and the following description of preferred embodiments with reference to the figures and examples. The features of the invention may be realized individually or in combination with one another. The embodiments described below serve to further elucidate the invention, without the invention being limited thereto. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0105] Examples Section 1. Experimental Method 1.1 MPBC sample design Metal-polymer multilayer composites, specifically metal-polymer bilayer composites (MPBCs), were used, with a thin (~100 μm) polydimethylsiloxane membrane (PDMS membrane) functionalized with a 40 nm gold layer. Two construction methods were used: one using a conventional photolithographic process and the other using an aperture mask. The gold metallization creates stretch-sensitive regions and regions containing leads whose resistance changes only slightly under stress. The leads have a self-similar serpentine structure. The sensor region employs a stretch-sensitive surface with microcracks. An example of a functionalized metal-polymer multilayer composite structure is shown in Figure 1.
[0106] 1.2 Substrate preparation The main steps of the process are shown in Figure 2. A 4-inch wafer 1 with a thickness of 0.5 mm, polished on one side, was used as a handling platform. A UV-sensitive dicing film 2 (also called saw film), consisting of polyethylene terephthalate (PET) (Adwill D-203, 50 μm), was transferred onto the wafer 1 with a soft foam roller 3. The mounted film 2 was cut with a scalpel along the wafer edge, after which it was irradiated with UV light 4 to reduce adhesion to the wafer 1 (specialized equipment with five Ster-L-Ray® low-pressure mercury lamps). The minimum dose was approximately 160 mJ / cm. 2The adhesion strength is reduced to approximately 1% of its original value (from 772.2N / m to 5.8N / m according to the datasheet). To ensure a uniform and maximum reduction in adhesion strength, UV activation is performed with a dose of approximately 250mJ / cm 2 The process was carried out in increasing amounts and under nitrogen atmosphere to prevent ozone generation. After UV treatment, degassed bubble-free PDMS prepolymer 5 (Sylgard 184® Elastomer Kit, mixing ratio 10:1 (base to curing agent), mixed using a Thinky 250-ARE planetary centrifugal mixer) was applied onto the film 2 covered handling wafer 1 by spin coating at 600 rpm (acceleration 200 rpm / s) for 60 seconds. It was then vacuumed (10 minutes) to ensure a uniform film without defects, followed by curing in an oven at 90° C. for 30 minutes.
[0107] 1.3 Construction of PDMS membrane For photolithographic construction, a negative lift-off photoresist 6 (AZ nLOF® 2070, Merck KGaA) was applied directly to the PDMS surface by spin coating at 3000 rpm (acceleration 1000 rpm / s) for 60 s. A soft bake at 100 °C for 2 min on a hotplate resulted in a photoresist thickness of approximately 6.5 μm. Exposure 7 through a chrome mask 8 was performed using a Suss MA6 mask aligner (350 W high pressure mercury lamp) with a dose of 70 mJ / cm. 2 The subsequent bake (post-exposure bake, PEB) was performed on a hotplate at 115 °C for 3 min. To prevent cracks in the stabilized photoresist layer as a result of the different thermal expansion coefficients of the layers that make up the multilayer structure, the exposed wafers were immediately transferred to an oven preheated to 100 °C. They were slowly cooled down to room temperature over a period of 5 h. For development, AZ developer (Merck KGaA, undiluted, fast configuration) was prepared in a laboratory jar on an analog orbital shaker (RS-OS 5 Phoenix Instruments). The structure was developed for 1 min 50 s with slight movement of the liquid, then rinsed with deionized water and dried under a stream of nitrogen.
[0108] For building the metal layer with an aperture mask process, a 50 μm nickel stencil mask9 manufactured by applied microSWISS in a suitable UV-LIGA process was used. As this mask had the outer dimensions of a standard 4-inch wafer, the mechanics of a Suss MA6 mask aligner were used to attach the mask to the PDMS membrane surface by flat alignment and magnets. The surface-to-surface contact of the PDMS and the smooth mask surface ensured stable positioning by van der Waals interactions without the need for further fixation.
[0109] 1.4 PVD metal deposition and peeling Deposition 10 was performed by thermal evaporation in an Edwards Auto 306 vacuum coating unit. To improve adhesion of the 40 nm gold cover layer, first an intermediate titanium layer of 4 nm was deposited under vacuum (approximately 2 × 10 -6 The film was deposited at 1000 nm (1000 MPa) without breaking. After the coating process, the photoresist was dissolved in acetone, the liquid was slightly agitated, and the resulting multilayer system was either rinsed with deionized water or the aperture mask was gently peeled off from the PDMS surface. The UV-activated stabilized transfer film 2 could then be easily peeled off from the wafer 1 without significant stress on the thin functionalized PDMS membrane 6.
[0110] 2. Transcription process Figure 3 shows the process of transferring to a cylindrical PDMS base substrate 11. The cylindrical substrate 11 was cast in a special polymethyl methacrylate (PMMA) mold with a constant outer diameter of 10 mm. The wall thickness was 400 μm in most areas and 200 μm only in certain areas. Since the prescribed transfer adopted PDMS-PDMS connection by partial curing, it was actually efficient to apply an intervening PDMS connection layer by spin coating before peeling off the film. PDMS-PDMS connection by partial curing allows high connection strength and is easy to implement. Here, a thin PDMS layer with a thickness of about 60 μm was applied by spin coating on the top surface of the constructed layer at 900 rpm for 60 s (acceleration 200 rpm / s), and then cured at 50 °C for 45 min. This resulted in a stabilized PDMS film while maintaining an adhesion comparable to that of an intermediate layer of adhesive. Next, the relevant parts of the sample were pre-cut with a scalpel, the stabilizing transfer film 2 was peeled off from the handling wafer with tweezers (see step 4 in Figure 2), and the partially cured PDMS surface was attached to the appropriate position of the cylindrical base 11 (step 1 in Figure 3). After that, the sample was placed into a cylindrical PMMA mold 12 and left at room temperature for 48 hours to fully cure. As a final step, the transfer film 2 was peeled off from the binding membrane layer 13 (Figure 3, step 2), and further cast process (Figure 3, step 3+4) was performed, followed by curing at room temperature for 48 hours to obtain a uniform cylindrical sensor.
[0111] 3. Characteristics and Results After the final step, the finished PDMS cylinder had to be carefully removed from the mold to ensure that the morphology of the transferred metal was not altered by undefined stresses. Therefore, the inner part of the mold, which defines the variable wall thickness of the PDMS base cylinder, was replaced with a water-soluble adhesive wax (2-M19 soluble stick wax from Paramelt) before the transfer process. For this reason, the subsequent curing process of the connection process and the final casting process had to be performed at low temperatures to avoid melting the wax (drop melting point about 57 °C).
[0112] Figure 4 shows the finished PDMS cylinder incorporating the sensor structure. As proof of the claim that the process allows handling and transfer of fragile surface morphologies, different surfaces (with microcracks and wavy interrupted structures) were introduced by selective plasma pretreatment and by varying the deposition rate. At each step, the same structures were investigated by SEM (Philips XL30) to characterize the morphology in the initial state before connection after peeling off the handling wafer and in the final state on the cylindrical base. To characterize the morphology after transfer to the cylindrical base, a special aluminum holder was used that simulated the curvature of the PDMS base.
[0113] Figure 5 shows selected morphological regions of the prepared sample at each relevant step of the described manipulation. As can be seen, the frangible crack morphology did not change during film handling, the only change being a slight compression due to bending of the cylindrical base (Figure 5c), while no delamination or crack propagation was observed. Furthermore, simple two-wire resistance measurements showed that the electrical integrity of the structure was maintained at around 4 kΩ.
[0114] As there are various options for the process of connecting the membrane to the substrate, a 90° peel test (see DIN EN 28510-1:2014) was performed to measure the peel force required to peel the cover film from the PDMS membrane (step 2, Fig. 3). For this purpose, a specimen with a 100 μm PDMS membrane, fabricated according to the substrate preparation process described above (step 1, Fig. 2), was peeled off from the PDMS surface connected to the handling wafer and the polished side of a precut wafer piece (30 mm wide) after activation with oxygen plasma (100 W for 30 s). The transferred film was then attached to the load cell of the peel test device and tested at a constant speed of 50 mm / min and a peel angle of 90°. The test was limited by the size of the wafer and the width of the flat (the wafer was cut perpendicular to the main flat near the edge of the flat), so that the maximum peel length was 90 mm and the peel width used was 20 mm. To exclude edge effects, a total of five samples were tested and analyzed with peel lengths between 20 mm and 80 mm. The average peel force was 0.07 N / mm (SD 0.011 N / mm). [Table 1]
Claims
1. 1. A medical device, more particularly a medical device in the form of a balloon catheter, comprising: At least one multi-layer structure, the at least one multi-layer structure being arranged one on top of the other; at least one metal layer; at least one layer of elastomeric material.
2. The at least one elastomeric material layer may be selected from the group consisting of elastomer, thermoplastic elastomer, thermoplastic polyamide elastomer, thermoplastic copolyester elastomer, olefin-based thermoplastic elastomer, thermoplastic styrene block copolymer, urethane-based thermoplastic elastomer, olefin-based thermoplastic vulcanizate, olefin-based crosslinked thermoplastic elastomer, natural rubber vulcanizate, synthetic rubber vulcanizate, styrene-butadiene rubber, butadiene rubber (BR), acrylonitrile-butadiene rubber (NBR), butyl rubber (IIR), ethylene-propylene-diene rubber (EPDM), chloroprene rubber, ethylene-propylene-diene rubber (EPDM), ...
2. The medical device of claim 1, comprising or composed of an elastomeric material, more particularly a superelastic material, selected from the group consisting of: methacrylic rubber (CR), polyisoprene rubber (IR), polyalkylsiloxane, polydimethylsiloxane, silicone rubber, silicone elastomer, methyl silicone, vinyl methyl silicone, phenyl vinyl methyl silicone, phenyl modified silicone, fluoroalkyl silicone, fluorovinyl methyl silicone, and a mixture of at least two of the preceding elastomeric materials.
3. 3. The medical device of claim 1 or 2, wherein the at least one metal layer comprises or is composed of at least one metal, more particularly a metal in elemental form or a metal in the form of an alloy, selected from the group consisting of gold, platinum, indium, tin, copper, silver, gallium and alloys of at least two of the aforementioned metals.
4. 10. The medical device according to any one of the preceding claims, wherein the at least one elastomeric material layer has a layer thickness of 0.0001 mm to 0.2 mm, more particularly 0.0005 mm to 0.1 mm, preferably 0.001 mm to 0.05 mm, and the at least one metal layer has a layer thickness of less than or equal to 150 nm, more particularly 10 nm to 100 nm, preferably 40 nm to 80 nm.
5. 10. The medical device of any one of the preceding claims, wherein the at least one metal layer directly overlies the at least one elastomeric material layer.
6. 10. The medical device of any one of the preceding claims, wherein at least one adhesive layer is formed between the at least one metal layer and the at least one elastomeric material layer.
7. 7. The medical device of claim 6, wherein the at least one metal layer directly and completely covers the at least one adhesive layer, and the at least one adhesive layer directly and only in certain areas covers the at least one elastomeric material layer.
8. 8. The medical device of claim 6 or 7, wherein the at least one adhesion layer comprises or is composed of at least one material selected from the group consisting of titanium, aluminum, chromium, and a mixture of at least two of the foregoing materials.
9. 10. The medical device of any one of the preceding claims, wherein the at least one multi-layer structure further comprises at least one additional layer of elastomeric material directly overlying the at least one metal layer.
10. 10. The medical device of any one of the preceding claims, wherein the at least one multilayer structure or the at least one metal layer has a varying surface morphology, more particularly surface areas with cracks, more particularly microcracks, and surface areas without cracks, more particularly corrugated surface areas without cracks.
11. 10. The medical device according to any one of the preceding claims, wherein said at least one multi-layer structure forms part of a surface of said medical device or is integrated into a wall of said medical device.
12. 10. The medical device according to any one of the preceding claims, wherein the medical implement is of curved shape, more particularly cylindrically curved shape, preferably hollow cylindrical or tubular.
13. 10. The medical device of any one of the preceding claims, wherein the medical device is in the form of a balloon catheter, the balloon of the balloon catheter comprising the at least one multi-layer structure.
14. 10. The medical device according to any one of the preceding claims, wherein said at least one multi-layer structure constitutes a sensor unit of said medical device.
15. A process for producing a product, more particularly a process for producing a product according to any of the preceding claims, comprising: a) producing at least one multi-layer structure having at least one metal layer and at least one elastomeric material layer; b) transferring the at least one multi-layer structure to a substrate to form a substrate having the at least one multi-layer structure.
16. A multi-layer structure, more particularly a multi-layer structure in the form of a sensor unit, arranged one on top of the other, at least one metal layer; at least one layer of elastomeric material.
17. 17. The multilayer structure of claim 16, further characterized by the features of the features of at least one of claims 1 to 14.