Fuel Cell Systems
The fuel cell system with molten metal electrodes and regenerative endothermic reactions addresses inefficiencies in existing heat-to-electricity conversion, providing compact and efficient electricity generation for high-power applications.
Patent Information
- Application Number
- JP2024520879
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-07
- Filing Date
- 2022-10-03
- Publication Date
- 2024-11-14
AI Technical Summary
Existing technologies for converting heat to electrical energy are inefficient, bulky, and require significant energy losses, making them unsuitable for high-power applications like industrial electricity production and vehicle energy supply, and they suffer from issues like dendrite formation and electrode wear.
A fuel cell system with molten metal electrodes, solid electrolytes, and a regenerator that regenerates consumed products through endothermic reactions, allowing for compact and efficient electricity generation without external fuels.
The system achieves high efficiency and compactness, enabling continuous electricity production with minimal energy loss, suitable for high-power applications like industrial energy production and vehicle supply.
Smart Images

Figure 2024542303000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the field of electricity generation from heat by using electrochemical cells with solid electrolytes. [Background technology]
[0002] To date, the conversion of heat into electrical energy is mostly carried out by turbines, internal combustion engines or Rankine cycles. These conversion methods have limited efficiency and result in considerable energy losses, most often dissipated in rivers, air or oceans. Moreover, on the one hand, their yields of 30% to 60% do not allow the use of certain new energy sources, in particular nuclear fusion, which requires large amounts of electrical energy to function, and on the other hand, these technologies are accompanied by the generation of heat during the conversion to electricity.
[0003] Conventional electric batteries are capable of converting chemical energy into electrical energy, however, conventional designs are constructed with solid electrodes that wear out and must be discarded or removed for replacement, and unless these batteries are designed to be rechargeable, the conventional designs make it difficult to use them for industrial-scale electricity production or to power vehicles.
[0004] Moreover, the use of coated solid electrodes typically results in the formation of dendrites adjacent to the electrodes, which are products of the redox reactions that occur during the production of energy. These coatings and dendrites cause significant energy dissipation due to the Joule effect and reduce the performance qualities of the battery.
[0005] Liquid metal batteries are particularly able to overcome the problem of dendrite formation and their development dates back to the 1960s, when the first batteries with fused electrodes of the Na-Sn type were proposed.
[0006] No. 3,245,836 describes a cell whose electrodes consist of molten sodium and molten tin separated by a liquid NaCl electrolyte impregnated in a porous separator. Metallic sodium is oxidized at the negative electrode and sodium ions are reduced at the positive electrode, where the metallic sodium is mixed with the tin.
[0007] A regenerator allows the tin to be separated from the sodium by heat treatment and pure metal to be reinjected into the cell to compensate for the consumption of sodium at the negative electrode and the contamination of tin by sodium at the positive electrode.
[0008] However, the liquid electrolyte of the cell, and also the presence of solid separators between each electrode and the electrolyte, make the cell very bulky and reduce its efficiency.
[0009] The following paper: Next-Generation Liquid Metal Batteries Based on the Chemistry of Fusible Alloys, ACS Cent. Sci., 2020, 6, 1355-1366 describes some recent avenues for the development of liquid metal batteries.
[0010] International Publication No. WO2017 / 201228 discloses a SOFC (Solid Oxide Fuel Cell) that uses a hydrocarbon as a fuel or oxidant.
[0011] US Patent Application Publication No. US2018 / 3745141 and US Patent Application Publication No. US2015 / 311545 disclose systems comprising two SOFCs.
[0012] International Publication No. WO2008 / 138923 discloses a fuel cell using a solid carbon-based substrate.
[0013] International Publication No. WO2008 / 044083 discloses a galvanic cell using a liquid electrolyte.
[0014] US Patent Application Publication No. US2011014526 discloses a fuel cell that uses a carbon-containing fuel or oxidant.
[0015] International Publication No. WO2014 / 201274 discloses metal-based electrodes for gas separation and evolution.
[0016] However, to the inventor's knowledge, there are few solutions proposing a method for regenerating the electrodes and / or the fuel by carrying out an endothermic chemical reaction. Summary of the Invention [Problem to be solved by the invention]
[0017] Despite these developments, there remains a need to benefit from systems that include compact, high-performance cells that enable the efficient generation of electricity from a variety of thermal sources. [Means for solving the problem]
[0018] The present invention aims to address this need and provides a fuel cell system, comprising: Cathode, an anode, wherein at least one of the anode and the cathode comprises, in a molten state, at least one metal, at least one metal hydroxide or at least one metal oxide; a solid electrolyte disposed between the cathode and the anode; At least one regenerator for regenerating, by reaction, at least one product constituting at least one of the anode and the cathode, or a fuel or an oxidant consumed at at least one of the anode or the cathode. This object is achieved by proposing a fuel cell system as described above, which comprises:
[0019] The regenerator may regenerate from at least one of the products of at least one of the oxidation or reduction reactions occurring at the anode or the cathode, the product consisting of a metal, metal alloy or metal oxide produced at the anode or the cathode during the production of electricity by the cell.
[0020] The invention makes available means of generating electricity that make it possible, in particular, to supply energy production facilities that consume large amounts of electricity and can release large amounts of heat at high temperatures, such as energy production facilities by controlled nuclear fusion. The cell according to the invention can exhibit high efficiency while remaining of a relatively compact volume.
[0021] In the sense of the present invention, the term "cell system" denotes a system that allows the production, continuous or intermittent, of electricity and total or partial regeneration.
[0022] The regeneration can regenerate at least one of the products constituting the anode or the cathode, or the fuel or oxidant consumed by an endothermic reaction at the anode or the cathode, The regenerated fuel or oxidant can be different from molecular oxygen.
[0023] The reaction therefore requires only the supply of heat and no other reactants other than possibly molecular oxygen. No fuel is required other than the products recovered from the oxidation or reduction reactions occurring at the anode or cathode. In particular, the regeneration does not require the use of a fuel external to the system.
[0024] Preferably, the electrodes, i.e. the anode and the cathode, have the form of the compartments. The regenerator can also be in the form of a compartment separated from the electrode compartments. One or more regeneration products can be reinjected into the electrodes through a pipe external to the electrode compartment.
[0025] [Summary of the invention]
[0026] Molten metal
[0027] The anode preferably comprises a metal in a molten state. The cathode may comprise a metal, a metal hydroxide or a metal oxide in a molten state.
[0028] The metal in the molten state can be a fuel or can be an oxidizer. It can also be.
[0029] The metal may be selected from zinc, lithium, magnesium, aluminum, lead, sodium, cesium, rubidium, copper, tin and alloys thereof. Preferably, the metal is zinc.
[0030] Thus, the cell can be configured to produce or consume at the anode or cathode a metal oxide or metal hydroxide selected from zinc oxide (ZnO), lithium oxide (LiO), magnesium oxide (MgO), alumina (AlO), lead oxide (PbO), lead dioxide (PbO), sodium oxide (NaO), cesium oxide (CsO), rubidium oxide (RbO), copper (II) oxide (CuO), copper (I) oxide (CuO), copper (III) oxide (CuO), manganese dioxide (MnO), sodium hydroxide (NaOH), manganese hydroxide, manganite (MnOOH), zinc hydroxide (Zn(OH)), and combinations thereof.
[0031] In particular, the cell can be arranged to consume manganese dioxide at the cathode.
[0032] solid electrolyte
[0033] The solid electrolyte is (i) O 2- Ion exchange membrane, or (ii) A solid acid; or (iii) an anion exchange membrane, or (iv) Metal ion exchange membrane can be selected from:
[0034] The O 2- The ion exchange membrane can be a solid oxide.
[0035] The battery system can include a separator between the anode and the electrolyte, where the separator is O 2- The separation membrane is an ion exchanger. The separation membrane can contain ceria.
[0036] Solid Oxide Electrolyte
[0037] The cell may be a solid oxide cell, known as a SOFC. The electrolyte may be in the form of a solid oxide.
[0038] The fuel cell system can be configured to operate at temperatures between 280°C and 100°C.
[0039] The solid oxide is yttria-stabilized zirconia (referred to as YSZ), scandia-stabilized zirconia (referred to as ScSZ), ceria-salt ceramic composites (called CSCs), erbia-cation-stabilized bismuth (ERB), gadolinium-doped ceria (referred to as GDC), samaria-doped ceria (called SDC), a ceria / bismuth-oxide bilayered electrolyte (referred to as GDC-ESB) formed from a layer of gadolinium doped with ceria and a layer of bismuth oxide stabilized with erbia; Strontium iron oxide SrFeO2, and combinations thereof It can be selected from, but is not limited to, the following:
[0040] The last four solid oxides mentioned above can be used at cell operating temperatures of, for example, 600°C to 800°C, which can be particularly useful for metals with low melting points, and the last electrolyte can be used at 500°C.
[0041] The solid oxide may be composed of iron and strontium having the formula SrFeO2, whereby from 280° C. to O 2- Ions can pass through.
[0042] In the case of a solid oxide cell, the reaction at the anode is as follows: M+O 2- → MO+2e - and the reaction at the cathode is as follows: 1 / 2O2+2e - → 2O 2- Here, M is a metal, for example zinc Zn.
[0043] O 2- The ions can come from the separation of molecular oxygen by donating electrons to the electrode of the cell which absorbs molecular oxygen. The molecular oxygen can come from air or from a zeolite concentrator which extracts molecular oxygen from air.
[0044] The oxygen absorbing electrode, particularly the cathode, can include lanthanum strontium manganite or lanthanum strontium cobalt ferrite. The lanthanum strontium manganite can be protected from an electrolyte including yttria stabilized zirconia (referred to as YSZ) by a film of gadolinium doped ceria (referred to as GDC). Such a film can have a thickness of approximately 0.5 μm.
[0045] The metal oxide MO, e.g. zinc oxide ZnO, is then displaced by the molten metal and discharged together with the nonoxidized liquid metal, which is subsequently preferably separated from the molten metal by settling or in a centrifuge and, if the metal oxide is less dense than the molten metal itself, is extracted from the center of the molten metal, which is also extracted from the other end.
[0046] The metal oxide is regenerated to give the metal, preferably by chemical means and the supply of heat, and the potentially produced oxygen can be recycled to supply the cathode.
[0047] Solid Acid Cell (SAFC)
[0048] In an alternative embodiment of the invention, the electrolyte is a solid acid, such as cesium dihydrogen phosphate (CsH2PO4), etc. The cathode can be composed of manganese dioxide (MnO2), advantageously mixed with carbon molecules to enhance its electrical conductivity.
[0049] Water is delivered to the anode at high pressure such that the electrolyte pressure is kept high, e.g. 3 GPa or 30 atmospheres, to prevent its decomposition at the temperature of the molten metal of the anode, e.g. 440°C for zinc and 240°C for lithium, preferably under a water vapor partial pressure of greater than 0.1 atmosphere, e.g. 1 atmosphere.
[0050] The reaction at the anode is then: M+H2O → MOH+H + +2e - and the reaction at the cathode is as follows: 1 or more MnO2+H + +e - → 1 or more MnO(OH) Here, M is a metal, for example lithium Li, and MOH is its hydroxide, for example LiOH, or, for example, M is zinc and MOH is its hydroxide Zn(OH)2.
[0051] The metal hydroxide MOH, e.g. lithium hydroxide LiOH, is then displaced by the molten metal and discharged with the nonoxidized liquid metal. The metal oxide is then preferably separated from the molten metal by settling or centrifugation and extracted from its center, where the metal hydroxide is less dense than the metal itself, and the metal is also extracted from the other end.
[0052] The metal hydroxide is preferably regenerated by chemical means and the supply of heat and optionally electricity, for example by the chemical reactions described below, to give the metal, where a portion of the electricity produced by the cell can be used in one of the reactions used to regenerate the metal hydroxide to give the metal.
[0053] The manganese dioxide cathode converted to manganite can be reused by melting it, for example at 550° C., the manganite can then be extracted by filtration, precipitation or centrifugation, and the manganese oxide can then be regenerated by oxidizing the manganite MnO(OH) to give manganese oxide MnO2 at approximately 300° C.
[0054] Anion Exchange Electrolytes
[0055] In an alternative embodiment of the invention, the electrolyte is OH -Membranes that conduct anions, such as hexamethyl trimethylammonium-functionalized Diels-Alder polyphenylene (called HTMA-DAPP) or low density polyethylene-benzyltrimethylammonium (called LDPE-BTMA).
[0056] For an anion exchange cell, the cathode can be manganese dioxide, preferably manganese dioxide containing carbon nanoparticles to enhance electrical conductivity, and the anode can be a metal M liquid at a temperature tolerable by the electrolyte, such as sodium at 100° C. When water is introduced to the cathode, the following electrochemical reaction occurs: At the cathode: MnO2 + H2O + e - → MnOOH+OH - and at the anode: M+OH - → MOH+e - .
[0057] The metal hydroxide MOH, e.g. zinc hydroxide Zn(OH)2, is then displaced by the molten metal and discharged with the non-oxidized liquid metal. The metal hydroxide is then preferably separated from the molten metal by settling or in a centrifuge and, if the metal oxide is less dense than the molten metal itself, is extracted from the center of the molten metal, which is also extracted from the other end.
[0058] The water circulating under pressure in and around the manganese dioxide cathode can advantageously be filtered to extract manganite therefrom. The manganite dioxide cathode can also contain manganite, circulate around an endless screw and be transported to a vessel or reactor where it can be melted, for example at 550° C., and reused, and the manganite can then be extracted by filtration, precipitation or centrifugation and produced by oxidation of the manganite MnO(OH) to give manganese oxide MnO2 at approximately 300° C. according to the reaction: MnO(OH)+1 / 2O2 → MnO2+1 / 2H2O
[0059] Regeneration of the anode can be accomplished in the same manner as solid acid cells.
[0060] Metal ion exchange membrane cell
[0061] The solid electrolyte can be a conductor of metal ions, for example Na3PS4, β-alumina, solid-state polymer electrolytes (called SPE), especially NaClO4 and TiO2 nanoparticles, sodium superionic conductors (called NASICON), especially Na3Zr2Si2PO 12 (NZSP), Na 11 Sn2PS 12 Or Na 2.88 Sb 0.88 W 0.12 β-alumina preferably contains metal ions that must be transported as electrolytes, such as sodium Na + Ion, potassium K + Ion, Lithium Li + Ion, Silver Ag + Ion, hydride H + Ion, lead Pb 2+Ion, Strontium Sr 2+ Ion, Barium Ba 2+ ions, is complexed with one of
[0062] The ionized metal at one electrode passes through the permeable membrane and bonds with the metal at the other electrode, combining to form an alloy.
[0063] The two metals can be, for example, tin and sodium, where the cell is preferably operated at a temperature where the two metals are liquid, for example 240° C. for a tin / sodium cell.
[0064] In an alternative form, the two metals can be tin and potassium operated with an electrolyte, for example an electrolyte consisting of β-alumina, at, for example, 240° C. The alloy can be heated to a temperature, for example 870° C., at which it dissociates into the metals, at which temperature the tin is liquid while the potassium is a gas.
[0065] Reserve
[0066] At the anode and / or at the cathode, at least one of the electrodes, indeed at each of the electrodes, the metal, metal hydroxide or metal oxide consumed can advantageously come from at least one reserve, in particular a reserve of this metal or oxide.
[0067] One of the reserves can be in solid form, in particular in the form of beads, whereby the beads are melted for introduction in the liquid state at the electrode.
[0068] The metal, metal hydroxide or oxide can be present in this reserve in various forms, in particular in solid form, for example in the form of powder, granules, beads or ingots, for example the metal or oxide is in the form of beads, for example in the form of beads with a diameter of 1 mm. These materials can for example be cut into beads by intermittent injection of a noble gas into the pipe of a liquid material, for example a molten metal, molten metal oxide, molten metal hydroxide, melted at a temperature close to the solidification of the liquid material. The metal present in the reserve is preferably melted before being introduced at the electrode that consumes it.
[0069] Regenerator
[0070] The term "regenerator" refers to a system that allows at least one of the redox reaction products to be recovered, possibly mixed with the reaction products, and processed to produce one or more chemical entities that can be used as fuels or oxidants for use at or introduced at the electrode.
[0071] The or one of the products of the chemical reaction at at least one of the electrodes can be separated from the reaction products, which can be performed by static or non-static sedimentation or by centrifugation.
[0072] The regenerator may use physical separation.
[0073] physical separation
[0074] To allow for extended continuous operation, the or one of the products of the chemical reaction at at least one of the electrodes is separated from the reaction products.
[0075] This separation is preferably carried out physically, in particular by sedimentation or by centrifugation.
[0076] The regenerator may thus comprise a centrifuge for centrifuging the mixture emerging from the electrodes, so that the metal oxides, which are less dense than the metal, can be extracted from the centre of the centrifuge, and the metals liberated from the oxides are recovered at the periphery.
[0077] If desired, multiple centrifugation stages can be provided.
[0078] At least one of the mixed or separated products of the chemical reaction at at least one of the electrodes can be stored in the tank.
[0079] The regenerator may include a centrifuge to extract metal oxides from the molten metal of the anode. Alternatively, the regenerator may work by sedimentation, especially when two substances are immiscible and have different densities, for example one is a liquid and the other is a solid that floats on the liquid.
[0080] The product stored in the tank can be pre-cooled, in particular in the opposite direction to the product that is introduced and used at one of the two electrodes, and is then preferably cut into round beads before solidifying.
[0081] Manganite MnOOH extracted from water can be stored in powder form.
[0082] chemical regeneration
[0083] In addition to or as an alternative to physical separation, the process of regenerating at least one of the products consumed at at least one of the electrodes can include a chemical reaction.
[0084] The reaction that allows the regeneration or one of the reactions that allows the regeneration of one of the reactants is endothermic. In the presence of hydrogen or carbon, the oxide can be reduced while supplying heat. Alternatively, this reaction may not require hydrogen or carbon. Molecular oxygen can also be produced by reducing the oxide without supplying hydrogen or carbon. Preferably, when the regeneration step includes multiple reactions, at least one reaction is endothermic.
[0085] One of the regenerated products can be reintroduced into the system as an electrode consisting of a metal or metal oxide, or in the form of a fuel or oxidant, particularly where molecular hydrogen or molecular oxygen are involved.
[0086] For example, if zinc oxide needs to be regenerated, it can be converted to zinc metal by hydrogenation at approximately 1000° C., according to the reaction: ZnO+H2→ Zn+H2O.
[0087] The reaction is endothermic, where ZnO and H2 are recovered from the electrode or from the products of another reaction belonging to the regeneration process.
[0088] If magnesium oxide needs to be regenerated to provide magnesium, Pidgeon reduction can be used: MgO+C → Mg+CO Carbon monoxide can be converted to carbon at high temperatures, e.g., 650° C., by the exothermic Boudouard reaction: 2CO → CO2+C. Carbon dioxide can be removed from the carbon monoxide and carbon dioxide mixture, e.g., by absorbing carbon dioxide on lithium orthosilicate (Li4SiO4) and then cycling in a carbon dioxide pipeline at low pressure, e.g., 0.04 atm, for desorption. The carbon dioxide is then converted to carbon monoxide and molecular oxygen by high temperature electrolysis.
[0089] The reaction is endothermic, where MgO and C are recovered from the electrode or from the products of another reaction belonging to the regeneration process.
[0090] Manganite (MnOOH) can be oxidized to give manganese oxide (MnO2) by one of the reactions: MnOOH+1 / 2O2→ MnO2+1 / 2H2O at 300℃.
[0091] The reaction is endothermic, where MgOOH and O2 are withdrawn from the electrodes or derived from the air.
[0092] One of the reactions is the reduction of zinc oxide to give zinc: ZnO → Zn+1 / 2O2.
[0093] The reaction is endothermic, where ZnO is recovered from the electrode.
[0094] One of the reactions can be the conversion of zinc hydroxide to give zinc oxide, or the conversion of lithium hydroxide to give lithium oxide: Zn(OH)2 → ZnO+H2O, 2LiOH → Li2O+H2O, for example, above 550°C and under a water vapor pressure of 120 mmHg or 0.15 atm.
[0095] One of the reactions is the reduction of zinc oxide to zinc at the expense of molecular hydrogen: ZnO+H2→ Zn+H2O.
[0096] One such reaction is the reduction of cesium oxide by reaction with magnesium: Cs2O+Mg → 2Cs+MgO Here, the magnesium oxide is regenerated, for example as described above.
[0097] One of the reactions is the reduction of lithium oxide by reaction with magnesium: Li2O+Mg → 2Li+MgO Here, the magnesium oxide is regenerated to give magnesium, for example as described above.
[0098] One such reaction is the reduction of rubidium oxide by reaction with magnesium: Rb2O+Mg → 2Rb+MgO Here, the magnesium oxide is regenerated, for example as described above.
[0099] One of the reactions can be the reduction of zinc oxide with carbon monoxide: ZnO+CO → Zn+CO2
[0100] The reaction is endothermic, where ZnO and CO are recovered from the electrode or from the products of another reaction belonging to a regeneration process.
[0101] One of the reactions is the regeneration of sodium hydroxide to give sodium, which can be obtained from the following reaction: 4Fe+6NaOH → 2Fe2O3+6Na+3H2, endothermic at 500℃ Fe2O3+3CO → 2Fe+3CO2 Here, carbon dioxide is regenerated by high-temperature electrolysis to give carbon monoxide.
[0102] Iron, sodium hydroxide and carbon monoxide are recovered from the electrodes.
[0103] The regenerator may in particular comprise a device for the regeneration of the alloy by heat, as shown for example in US 3,245,836. The sodium-potassium alloy may be heated, preferably above 578°C, above which the alloy between the two metals disappears, leaving only the space for the two metals.
[0104] One of the reactions is reduction by carbon.
[0105] High-temperature electrolysis of carbon monoxide
[0106] One of the reactions is the reduction of carbon dioxide to give carbon monoxide by high temperature electrolysis: CO2 → CO+1 / 2O2.
[0107] Carbon dioxide can be converted to carbon monoxide by a high temperature electrolytic cell, for example at 750° C., where the electrolyte of the cell is O 2- It is a conductor of ions. The electrolyte can be formed, for example, of a 150 μm thick layer of 10Sc1CeSZ (ZrO2 doped with 10% of the molecules as Sc2O3 molecules and 1% of the molecules as CeO2 molecules). Each side of the electrolyte can be covered with a 35-50 μm thick layer of porous GDC (gadolinium doped with ceria), which on the oxygen outlet side can be permeated with a 3 mol / L solution of cerium and praseodymium (molar ratio of 8 molecules of cerium per 2 molecules of praseodymium) and on the carbon dioxide and carbon monoxide side can be permeated with a 3 mol / L solution of cerium nitrate and gadolinium nitrate with a Ce:Gd ratio of 8 / 2. The electrodes can be formed, for example, as one of 180 ηm thick platinum or nickel strips formed with 10 μm spacing and glued to the GDC layer by platinum paste. Alternatively, the high temperature electrolytic cell can be of the Ny-YSZ or Ni-SDC type.
[0108] A voltage of 1 to 2 V, preferably 1.19 V, can be applied to the electrodes, where the terminals are connected to the electrodes bonded to the surfaces through which the carbon dioxide and carbon monoxide flow, for example at a pressure of 1 atmosphere, preferably laminar flow.
[0109] All or part of the power for the electrolysis is provided by a cell.
[0110] High temperature electrolysis of metal sulfides
[0111] One of the reactions can be the reduction of metal sulfides by high temperature electrolysis using an electrolyte that conducts metal ions, such as β-alumina: M x S → xM+S, at temperatures where the metal sulfide is liquid.
[0112] Conductive electrodes, such as platinum or carbon, may be used and the metal, either gas or preferably liquid, is evolved at one electrode while gaseous sulfur is evolved at the other electrode.
[0113] The cell is preferably powered by electricity discharged from another metal sulfide cell, operating at a lower temperature but in which both sulfur and metal are liquid. The voltage difference between the operating voltages of the two cells can advantageously be used to supply current to an external device, and the metals and sulfur extracted from the regenerator can preferably be cooled countercurrently to the metal sulfides going to regeneration.
[0114] The metal M can be, for example, potassium, lithium (in the latter two cases, the reaction is M2S → 2M+S) or lead (in the latter case, the reaction is MS → M+S). The cells can be operated, for example, at 120°C, 180°C and 330°C, respectively, and the regeneration temperatures can be, for example, 850°C, 950°C and 1150°C, respectively.
[0115] The metal can be sodium and the regeneration temperature can be, for example, 1177° C. or higher. The reaction can be written as follows: 2Na+S → Na2S.
[0116] Storage
[0117] At least one of the reaction products at at least one of the electrodes can be stored in a tank, especially if the latter is not carried out continuously, with a view to a further processing. This reaction product can be stored mixed with the reaction product or can be stored unmixed.
[0118] The product stored in the tank may be pre-cooled, in particular to counter-flow with the product reaching the electrode, the latter being heated to ensure that it remains molten or in its liquid state at the electrode.
[0119] The product intended to be stored in the tank may, before solidification, be formed into small sized, non-continuous elements that are easy to handle, for example formed into beads, and then arranged in this form within the tank.
[0120] For example, manganite extracted from water can be stored in powder form.
[0121] One or more of the products resulting from the separation or from the chemical regeneration can be stored as described above or can be reintroduced as a liquid metal, liquid metal hydroxide or liquid metal oxide electrode after treatment.
[0122] Operating temperature
[0123] The operating temperature of the cell is chosen as a function of the material from which it is made, it is in particular between 280°C and 1100°C.
[0124] The operating temperature of the cell may be different from the temperature of one or more of the chemical regeneration reactions. The temperature of the cell depends on the metals, oxides and hydroxides used, especially their melting points. It is selected to be within the operating range of the electrolyte temperature and above the temperature of any metal, oxide or hydroxide selected to be in a liquid state. The operating temperature of the electrolyte may be influenced by the partial water pressure of the atmosphere surrounding the electrolyte, especially in the case of solid acid type solid electrolytes, such as cesium dihydrogen phosphate.
[0125] Use of carbon in the cathode
[0126] When the cathode comprises manganese dioxide MnO2, it may or may not be mixed with carbon molecules. By mixing manganese dioxide MnO2 with carbon molecules, the electrical conductivity of the cathode can be increased.
[0127] heat source
[0128] The heat required for regeneration of the cell electrodes and / or oxidant and fuel can be provided by burning a fuel, e.g., hydrogen, gasoline, diesel, biodiesel, ethanol, in air, preferably in oxygen, extracted from the air, e.g., by a zeolite filtration system.
[0129] This allows the efficiency of conversion from thermal energy to electrical energy to be improved by a factor of 3, for example, compared to a heat engine. In addition, depending on the fuel that generates the heat required for the regeneration reaction and the oxidant, e.g., hydrogen, alcohol or biodiesel, e.g., oxygen extracted from the air using a zeolite filter, the formation of NOx can be avoided, especially when they do not contain nitrogen. Thus, the efficiency of conversion from hydrogen chemical energy to electrical energy can be improved by approximately 50% compared to conventional hydrogen fuel cells.
[0130] The heat can come, for example, from a solar furnace, or from the ground if a deep enough well is drilled and the heat is extracted from it, or from the ground if all or part of the regenerator is installed therein.
[0131] The heat can also come from the combustion of fossil fuels, from the combustion of biofuels, such as wood or straw, or from the combustion of household waste.
[0132] The heat can be derived from nuclear energy, such as that described above including accelerated ion fusion nuclear energy, where a portion of the electrical energy produced by the cell is advantageously used to create and accelerate the ions.
[0133] Working Example
[0134] Example 1
[0135] Electricity is generated by the decomposition of oxygen at the cathode and the oxidation of liquid zinc at the anode, where the cathode is made of lanthanum strontium manganite and the electrolyte is made of yttria stabilized zirconia (YSZ) and has a thickness of, for example, 10 μm.
[0136] The cell operates at, for example, 830° C., and the heat released by the cell, in addition to the heat from the outside, is used to produce hydrogen by the sulfur-iodine cycle, where the temperature of 1000° C. required for the hydrogenation of zinc oxide is provided by the external heat. It is therefore estimated that 93.5% of the heat from the outside can be converted into electrical energy.
[0137] By using zinc as the metal, zinc oxide can be regenerated to give zinc by the following reaction consuming molecular hydrogen: ZnO+H2 → Zn+H2O
[0138] The reaction can be carried out in a mixture of 87% molecular nitrogen and 13% hydrogen at approximately 1000° C. It can also be advantageously carried out without the use of molecular nitrogen, preferably in the absence of water.
[0139] In an alternative form, the above-mentioned reactions for hydrogenation of zinc oxide can be used by using as heat the energy released by the combustion of hydrogen in air or with molecular oxygen advantageously extracted from the air by the zeolite. This option can be advantageous to avoid the production of nitrogen oxides. The heat released from the fuel cell can also be recycled to the reactions for hydrogenation of zinc oxide and the reactions for oxidation of manganites.
[0140] As a further alternative, the reaction for hydrogenation of zinc oxide can be carried out by using hydrogen resulting from a process for the production of hydrogen by the sulfur-iodine cycle or also by the oxide-cerium cycle, which utilizes high heat to produce hydrogen at 120° C. with a small heat release, and the heat energy loss is estimated to be approximately 15%. This is because the reaction I2+SO2+2H2O→2HI+H2SO4 can release 15% of the heat required for the two endothermic reactions: 2H2SO4 → 2SO2+2H2O+O2 and 2HI →I2+H2.
[0141] Alternatively, zinc oxide can be reduced with external heat to give metallic zinc at high temperatures, especially above 1727° C. For example, molecular oxygen can be separated from zinc by bringing the gas mixture to a pressure such that the partial pressure of gaseous zinc reaches the pressure at which gaseous zinc becomes liquid, i.e., approximately 30 GPa. Thus, the efficiency of heat to electricity conversion can be equal to that of a fuel cell.
[0142] Alternatively, zinc can also be regenerated by reduction with carbon at temperatures between 1280°C and 1320°C, or with carbon monoxide at approximately 950°C, both reactions being endothermic and producing zinc and carbon dioxide, which is regenerated to give carbon monoxide by high temperature electrolysis, which itself is converted to carbon and carbon dioxide by an exothermic reaction: 2CO → C+CO2, at 1 atm.
[0143] When regeneration is performed by carbon monoxide itself regenerated by high-temperature electrolysis, the proportion of power supplied to the regeneration electrolysis in the total chemical energy supplied to the regeneration of the electrodes is approximately 34% according to the inventor's calculations.
[0144] Alternatively, the heat can also come from, for example, a solar furnace, or from the earth if a sufficiently deep well is dug and the heat is extracted from it, or from the earth if all or part of the regeneration device is installed therein, or from fossil energy, or from biofuels, such as wood or straw, or from the burning of household waste, or from nuclear energy, such as the above-mentioned nuclear energy including accelerated ion fusion nuclear energy, with part of the generated electrical energy then advantageously being used for the production and acceleration of the ions.
[0145] Example 2
[0146] Electricity generation by decomposition of water at the cathode and oxidation of liquid zinc at the anode, where the cathode is made of manganese dioxide MnO2 and the electrolyte is made of cesium dihydrogen phosphate CsH2PO4, for example having a thickness of 10 μm. The cell operates at, for example, 440° C. For regeneration of the electrodes, zinc hydroxide is converted to zinc oxide, for example at 80° C. or higher, which itself is reduced to metal by external heat at high temperatures, for example above 1727° C. Manganite formed by reduction of manganese dioxide is converted to manganese dioxide by oxidation, the heat being provided by the heat released by the operation of the cell and by external heat. Thus, the efficiency of converting the heat to electricity can be close to 1, if the heat released by the cell does not exceed the heat absorbed by the manganite.
[0147] Example 3
[0148] Electricity is generated by the decomposition of water at the cathode and the oxidation of liquid rubidium at the anode, where the cathode is made of manganese dioxide MnO2 and the electrolyte is made of cesium dihydrogen phosphate CsH2PO4 (solid acid) and has a thickness of, for example, 10 μm. The cell operates, for example, at 300 °C. For regeneration, rubidium hydroxide is reduced to rubidium oxide at 90 °C, which is itself converted to rubidium by oxidation with magnesium, which is reduced to magnesium by the Pidgeon reaction, followed by the conversion of carbon monoxide to carbon and carbon dioxide, which is then converted to carbon monoxide by high-temperature electrolysis. Manganite formed by the reduction of manganese dioxide is converted to manganese dioxide by oxidation at 300 °C, where the heat is provided by the heat released by the operation of the cell and by the conversion of carbon monoxide to carbon and external heat. If the heat released by the cell does not exceed the heat absorbed by the manganites, the efficiency of converting the heat to electricity approaches unity.
[0149] Example 4
[0150] Electricity is generated by the decomposition of water at the cathode and the oxidation of liquid rubidium at the anode, where the cathode is, for example, carbon impregnated with platinum nanoparticles and the electrolyte is Nafion®, which is a proton exchange membrane. The cell operates, for example, at 100° C. For regeneration, rubidium hydroxide is reduced to rubidium oxide at 90° C., which is itself converted to rubidium by oxidation with magnesium, which is reduced to magnesium, for example, by the Pidgeon reaction, and subsequently, carbon monoxide is converted, for example, by an exothermic reaction, to carbon and carbon dioxide. Thus, the efficiency of heat conversion to electricity can be higher than that of the fuel cell, and all or part of the heat released from the cell at 100° C. and the conversion of carbon monoxide to carbon and carbon dioxide are used for the conversion of rubidium hydroxide to rubidium oxide.
[0151] Liquid electrode circulation
[0152] Liquid metal, liquid metal oxide or liquid metal hydroxide can be circulated in millifluidic channels, preferably 1 mm deep, 2 mm wide and 0.5 mm apart, made for example of silicon dioxide, where one side is covered with one or more membranes acting as an electrolyte, particularly when the liquid is a poor electrical conductor, for example a metal oxide, metal hydroxide or sulphur, or preferably made of a material which is a good electrical conductor, for example carbon or stainless steel, so that the surface of the material in which the channels are inscribed can advantageously be covered with an electrical insulator in the parts that come into contact with the electrolyte.
[0153] The millifluidic channels can be used for heat exchange, especially countercurrentwise heat exchanges.
[0154] The metal in the molten state can be obtained from a molten metal ingot, for example a metal ingot melted with the same heat source used for the regeneration of the electrodes.
[0155] Another subject of the invention, independently or in combination with the above, is an apparatus for generating electricity, comprising a fuel cell or a fuel cell system as described above and a system for regenerating the metal oxide produced at the anode to give the metal.
[0156] The regenerated metal can be used to supply metal in the molten state to the anode.
[0157] The apparatus may include a centrifuge to extract metal oxides from the molten metal of the anode.
[0158] Another subject of the invention, independently or in combination with the above, is in particular a process for producing electricity by means of a fuel cell or by means of a fuel cell system as described above, in which a metal oxide is produced at the anode, the anode comprising the metal in the molten state.
[0159] The metal oxide produced at the anode can be discharged by circulating the metal in the molten state.
[0160] The metal oxides can be separated from the non-oxidized metals in the molten state by settling or centrifugation.
[0161] The centrifugation can be done in a centrifuge where the metal oxide is extracted from the center and, if the metal oxide is less dense than the metal itself, the metal is also extracted at the other end.
[0162] The metal oxide produced can subsequently be regenerated to provide the metal, as detailed above.
[0163] Complete Cycle
[0164] Another subject of the invention, independently or in combination with the above, is a process that makes it possible to produce electricity by decomposition of oxygen at the cathode and oxidation of liquid zinc at the anode, where the cathode is made of lanthanum strontium manganite and the electrolyte is made of yttria stabilized zirconia (YSZ), has a thickness of 10 μm, which is a solid oxide. The cell operates at 830° C. and the heat released by the cell, in addition to external heat, is used to produce hydrogen by the sulfur-iodine cycle, where the heat of 1100° C. required for the hydrogenation of zinc oxide is provided by external heat. According to the inventor's calculations, 89% of the heat coming from the outside can be converted into electrical energy.
[0165] Another subject of the invention, independently or in combination with the above, is a process that makes it possible to produce electricity by decomposition of oxygen at the cathode and oxidation of liquid zinc at the anode, where the cathode is made of lanthanum strontium manganite and the electrolyte is made of yttria-stabilized zirconia (YSZ), has a thickness of 10 μm, and is a solid oxide. The cell operates, for example, at 880° C. Zinc oxide is reduced to metallic zinc at 1727° C. using external heat. The efficiency of converting heat into electricity can therefore be made equal to the efficiency of the fuel cell.
[0166] Another subject of the invention, independently or in combination with the above, is a process that makes it possible to produce electricity by decomposition of water at the cathode and hydroxylation of liquid sodium at the anode, where the cathode is made of manganese dioxide MnO2 and the electrolyte is made of LDPE-BTMA, has a thickness of 55 μm and is an anion exchange membrane. The cell operates, for example, at 100 ° C. For regeneration, sodium hydroxide is converted at 500 ° C to sodium and iron (III) oxide, where the iron (III) oxide is reduced to iron and carbon dioxide by carbon monoxide and the carbon dioxide is oxidized by high-temperature electrolysis. Manganite produced by reduction of manganese dioxide is converted to manganese dioxide by oxidation with oxygen at 300 ° C, by the release of heat due to the operation of the cell and / or by the supply of heat from an external source. Thus, the efficiency of converting the heat to electricity can be close to 1, provided that the heat released by the cell does not exceed the heat absorbed by the manganite.
[0167] Another subject of the invention, independently or in combination with the above, is a process making it possible to generate electricity by decomposition of oxygen at the cathode and oxidation of liquid rubidium at the anode, where the cathode is made of lanthanum strontium manganite and the electrolyte is GDC-ESB, has a thickness of 10 μm and is a solid oxide electrolyte. The cell operates, for example, at 500° C. For regeneration, rubidium oxide is reduced to rubidium by oxidation with magnesium, where the magnesium oxide is reduced to magnesium by carbonization, for example at 2300° C., and subsequently carbon monoxide is converted to carbon and molecular oxygen by an endothermic high-temperature electrolysis reaction.
[0168] Purpose
[0169] Another subject of the invention is the use of a fuel cell or a fuel cell system as described above, either independently or in combination with the above.
[0170] The cell according to the invention makes it possible in particular to produce electricity for vehicles, homes, industries or public purposes.
[0171] The fuel cell according to the invention can be used to generate electrical current for example for industry, for the home, for vehicles or for energy production devices, in particular electrical energy devices, which require high power for their operation. This can be for example for accelerated ion fusion or electrolysis of alumina.
[0172] The heat released by the cell can be advantageously used to generate hydrogen, in particular by the iodine-sulfur cycle, thereby regenerating metal oxides to give metals.
[0173] Another subject of the invention is the use of a fuel cell or a fuel cell system as described above, independently or in combination with the above, in which the heat is provided by: Combustion of a fuel (e.g., fuel extracted from the air by a zeolite filtration system), such as hydrogen, gasoline, diesel, biodiesel, ethanol, in air or preferably in oxygen; solar furnaces, or underground if wells of sufficient depth are dug and the heat is extracted therefrom, or underground if the regenerator is wholly or partly placed therein; the burning of fossil fuels, the burning of biofuels, such as wood or straw, or the burning of household waste, Nuclear energy, in particular accelerated ion fusion nuclear energy, preferably a portion of the generated electrical energy, preferably a portion of the generated electrical energy used for the creation and acceleration of said ions.
[0174] It is also possible to produce electricity to energize or co-power devices for nuclear fusion or devices for producing neutrons by accelerated ions, in particular for accelerating ions for the purpose of fusion nuclear reactions.
[0175] The heat released from the fuel cell can also be recycled to one or more of the reactions mentioned above, but can also be recycled to oxidize the manganites. [Brief description of the drawings]
[0176] [Figure 1] FIG. 1 diagrammatically and partially represents an example of a system according to the invention. [Diagram 2] FIG. 2 diagrammatically and partially represents another example of a system according to the invention. [Diagram 3] FIG. 3 diagrammatically and partially represents another example of a system according to the invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0177] In FIG. 1, an example of a cell system 11 according to the present invention is shown.
[0178] The cell system comprises a battery having electrodes 1 and 8 connected to respective electrical terminals 9 and 10. The electrodes 1 and 8 have the form of compartments.
[0179] Electrode 1 and electrode 8 are separated by a solid electrolyte 7 .
[0180] The electrode 1 consists of a metal or metal oxide in liquid state, which is recycled in a regenerator 4 where it is regenerated by the supply of heat 3 and then reinjected into the electrode 1 compartment of the cell.
[0181] The electrode 8, or fuel supplied to the electrode 8, is ionized by electrons supplied or withdrawn by the terminal 10 of the cell 11. In addition, the ions pass through the solid electrolyte 7 and react with the liquid electrode 1 together with the electrons withdrawn or supplied by the terminal 9.
[0182] The cell 11, its electrodes 1 containing metals or metal oxides in liquid state, is recycled in one or more chemical reactors 4 with the supply of heat 3 and then reinjected into the container of liquid electrode 1 via pipe 5.
[0183] Part of the regeneration products, for example metals or oxygen corresponding to the ions that have passed through the electrolyte 7, can be reintroduced into the electrode 8 compartment via the pipe 6.
[0184] In one example, the anode is formed of molten zinc, which circulates in a circuit which ensures, on the one hand, the supply of metal to be consumed and, on the other hand, the extraction of oxides.
[0185] The cell may also allow for the conversion of the oxide to the metal to occur continuously, or alternatively, the conversion is performed discontinuously.
[0186] The electrolyte is a solid oxide, such as lanthanum strontium cobalt ferrite, advantageously separated from the molten metal by a layer of ceria, and the electrolyte is free of O 2 which oxidizes the metal. 2- ions through the O 2- The ions come from the separation of molecular oxygen by the supply of electrons to the cathode of the cell, which may consist of, for example, lanthanum strontium manganite, and is supplied, for example, from ambient air or oxygen-enriched air from a zeolite concentrator, or from regeneration of metal oxides to give the metal.
[0187] The reaction at the anode is as follows: M+O - → MO+e - and the reaction at the cathode is: 1 / 2O2+2e - → O 2- Here, M is a metal, for example zinc Zn.
[0188] The regenerator separates the zinc from the oxide formed and may include a centrifuge to extract the zinc oxide from the molten zinc which circulates to the anode.
[0189] The oxide can be stored until it is reduced to the metal. The zinc liberated from the oxide can be returned to the anode.
[0190] An alternative configuration in which the two electrodes 1 and 8 are regenerated by different chemical reactions will now be described with reference to FIG.
[0191] In this figure 2, the second electrode 8 contains molten metal or metal oxide, for example magnesium dioxide MnO2. This electrode 8 is also thermally regenerated by heat 14 in one or more reactors 13. Products from the regeneration of electrode 1 can be reinjected into the compartment of electrode 8 via pipe 12 or into the regenerator 13 of electrode 8.
[0192] An alternative embodiment using liquid sulfur and producing metal sulfides will now be described with reference to FIG.
[0193] The compartments 101 of the system contain liquid metal and liquid sulfur, respectively, separated by a solid electrolyte 102. Metal ions M + Or M ++ The metal sulfide M is a solid metal sulfide formed following oxidation of the metal. x S is extracted by a filter, centrifuge or settler 104, then heated in a heat exchanger 105 and then in a heating device 107 to which external energy is supplied. Thus, the metal sulfide M x S is brought to a temperature that is used for its conversion by electrolysis in a compartment of the regenerator 110 separated by an electrolyte 109. A regeneration voltage is applied to the electrodes 108 of the regenerator 110.
[0194] The regenerated metal M, preferably in liquid form, is transferred via pipe 111 to the metal compartment of section 101 of the system while being cooled in heat exchanger 105 .
[0195] The regenerated sulfur S, preferably in gaseous form, is transferred via pipe 112 to the sulfur section of section 101 of the system while passing through heat exchanger 105, where it is cooled and liquefied.
Claims
1. 1. An electrochemical reaction fuel cell system, comprising: Cathode (8), an anode (1), wherein at least one of the anode and the cathode comprises, in a molten state, at least one metal, at least one metal hydroxide or at least one metal oxide; a solid electrolyte (7) disposed between the cathode and the anode; at least one regenerator (4) for regenerating, by reaction, at least one product constituting at least one of the anodes or at least one of the cathodes, or a fuel or an oxidant consumed at at least one of the anodes or at least one of the cathodes, starting from at least one of the redox reaction products recovered at at least one of the anodes and at least one of the cathodes; It is equipped with wherein one of the regeneration products is reintroduced into the fuel cell system as an electrode consisting of a liquid metal or liquid metal oxide, or in the form of a fuel or oxidant, and one of the reactions enabling the regeneration, or one of the reactions enabling the regeneration of one of the reactants of the redox reaction, is endothermic, The fuel cell system.
2. 2. The fuel cell system of claim 1, wherein the anode (1) comprises a metal in the molten state.
3. 3. The fuel cell system of claim 1, wherein the cathode (8) comprises a metal oxide in the molten state.
4. 4. The fuel cell system of claim 3, wherein the molten metal is selected from zinc, lithium, magnesium, aluminum, lead, sodium, cesium, rubidium, copper and tin.
5. Zinc oxide (ZnO), lithium oxide (Li 2 O), magnesium oxide (MgO), alumina (Al 2 O 3 ), lead oxide (PbO), lead dioxide (PbO 2 ), sodium oxide (Na 2 O), Cesium oxide (Cs 2 O), rubidium oxide (Rb 2 O), copper(II) oxide (CuO), copper(I) oxide (Cu 2 O), copper(III) oxide (Cu 2 O 3 ), manganese dioxide (MnO 2 ), sodium hydroxide (NaOH), manganese hydroxide, manganite (MnOOH), and zinc hydroxide (Zn(OH) 2 5. The fuel cell system according to claim 1, wherein the fuel cell system is configured to produce or consume at the anode (1) or at the cathode (8) a metal oxide or metal hydroxide selected from the group consisting of:
6. (i) O 2- Ion exchange membrane, or (ii) A solid acid; or (iii) an anion exchange membrane, or (iv) Metal ion exchange membrane 6. The fuel cell system according to claim 1, further comprising a solid electrolyte (7) selected from the group consisting of:
7. A separator is included between the anode (1) and the electrolyte (7), where the separator is O 2- 7. The fuel cell system according to claim 6, which is an ion exchanger.
8. The fuel cell system of claim 7 , wherein the separation membrane comprises ceria.
9. 9. A fuel cell system according to claim 7 or 8, comprising an electrolyte (7) in the form of a solid oxide.
10. A fuel cell system according to any one of claims 7 to 9, configured to operate at a temperature between 280°C and 1100°C.
11. The solid oxide is yttria-stabilized zirconia (known as YSZ); Scandia-stabilized zirconia (referred to as ScSZ), ceria-salt ceramic composites (called CSCs), Erbia-cation stabilized bismuth (referred to as ERB), gadolinium-doped ceria (referred to as GDC); Samaritan doped celia (called SDC), a ceria / bismuth oxide bilayer electrolyte (called GDC-ESB) formed from a layer of gadolinium doped with ceria and a layer of bismuth oxide stabilized with erbia; Strontium Iron Oxide SrFeO 2 , and combinations thereof The fuel cell system of claim 9 , wherein the fuel cell is selected from the group consisting of:
12. O 2- 12. The fuel cell system according to claim 1, wherein the ions originate from the dissociation of molecular oxygen by donating electrons to the electrode of the cell which absorbs molecular oxygen.
13. 13. The fuel cell system according to any one of claims 1 to 12, wherein the metal, the metal hydroxide or the metal oxide consumed at the anode (1) and / or at the cathode (8) comes from at least one reserve.
14. 14. The fuel cell system according to claim 13, wherein one of the reserves is in solid form, in particular in the form of beads, and wherein the beads are melted for being introduced in the liquid state into the electrodes (1, 8).
15. 15. The fuel cell system according to any one of the preceding claims, wherein the or one of the products of the chemical reaction at at least one of the electrodes (1, 8) is separated from the reaction products.
16. 16. The fuel cell system of claim 15, wherein the separation is performed by static or non-static settling or by centrifugation.
17. 10. The fuel cell system of claim 1, wherein one of the reactions enabling the regeneration of one of the reactants of the redox reaction is endothermic.
18. 2. The fuel cell system of claim 1, wherein all or part of the electricity for electrolysis is provided by the fuel cell (11).
19. Use of a fuel cell system according to any one of claims 1 to 18 for producing electricity for vehicles, homes, industries or public use and / or for supplying or co-supplying energy to devices for nuclear fusion or for the production of neutrons by accelerated ions.
20. 20. A method of using a fuel cell system according to any one of the preceding claims, wherein heat released from the fuel cell (11) is recycled for one or more of the above mentioned reactions, but potentially also for the oxidation of manganese.
Citation Information
Patent Citations
Management and Utilization of Sulfur in Molten Metal Anode Solid Oxide Fuel Cells
JP2017517838A
Molten metal anode solid oxide fuel cells for transportation-related auxiliary power units.
JP2019517124A
Self-sustainable solid oxide fuel cell system and method for powering gas wells
JP2020524873A
High temperature direct coal fuel cell
US20110014526A1
Thermally regenerative electrochemical converter and mehtod for converting thermal energy into electrical energy by the converter
WO2008044083A2