Method for manufacturing a tire equipped with an electronic device

By integrating a transponder in a rubber housing on the inner tire surface before vulcanization, the method addresses damage and malfunction issues, ensuring efficient and economical tire production.

JP2024543327AActive Publication Date: 2024-11-21BRIDGESTONE EURO NV SA
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2024525360
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-29
Filing Date
2022-10-27
Publication Date
2024-11-21
Estimated Expiration
2042-10-27

AI Technical Summary

Technical Problem

The integration of transponders in tires during the vulcanization process leads to potential damage due to high pressures and temperatures, causing surfacing, malfunction, and air leaks, increasing manufacturing time and costs.

Method used

A method involving a transponder housed in a rubber structure with specific dimensions and composition, applied to the inner surface of a green tire before vulcanization, ensuring protection and strong adhesion, avoiding direct contact with high pressures and temperatures.

Benefits of technology

Prevents transponder damage and air leaks, reduces manufacturing time and costs, while maintaining tire integrity and performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543327000001_ABST
    Figure 2024543327000001_ABST
Patent Text Reader

Abstract

A method for manufacturing a tire (8) equipped with an electronic device (1), comprising the steps of inserting the electronic device (1) between a first strip of rubber (6) and a second strip of rubber (7), the first strip of rubber (6) and the second strip of rubber (7) surrounding the electronic device (1) which itself defines a housing (5), applying the housing (5) to an inner liner (13) of a green tire (8) such that the first strip of rubber (6) is in direct contact with the inner liner (13) and the second strip of rubber (7) is separated from the inner liner (13) by the intervention of the first strip of rubber (6), and subjecting the green tire (8) equipped with the housing (5) to a vulcanization process, the first strip of rubber (6) being entirely made of green rubber, while the second strip of rubber (7) is made of rubber that has only been partially vulcanized, i.e. rubber where vulcanization has been initiated but not completed.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing a tire equipped with an electronic device, in particular a transponder. [Background technology]

[0002] In recent years, so-called "smart" tyres have appeared which form active components of modern motor vehicles and which are able to provide information about the type of tyre fitted, about the condition of the tyre and also about the environmental conditions.

[0003] A "smart" tire is typically equipped with a transponder (i.e., an electronic device adapted to communicate over radio frequencies) that allows remote communication (both with the vehicle on which the tire is mounted and with operators who need to inspect or change the tire) about the tire's identification, characteristics, and history.

[0004] Recently, it has been proposed to integrate "Radio Frequency Identification (RFID)" technology, based on the presence of a transponder, with "Tire Pressure Monitoring System (TPMS)" technology, which measures the effective tire pressure by storing the effective tire pressure within the transponder and then using the transponder itself to communicate the effective tire pressure information remotely.

[0005] The transponder intended to be coupled to the tire is pre-inserted into a rubber housing that completely surrounds it on all sides. To then couple the transponder to the tire, it can be attached to the inner surface of the tire (typically on top of the inner liner that ensures the tire's airtightness) or it can be integrated inside the tire's sidewall (i.e., it is placed in the middle of the various layers that make up the tire's sidewall). The attachment of the transponder to the inner surface of the tire ensures that the tire will have the expected performance, since the presence of a foreign object does not change the structure of the tire in any way. The transponder may be attached to the inner surface of the tire when it is still green (i.e., before the tire is vulcanized) or after the tire has been vulcanized.

[0006] The tire is initially moistened with a lubricant layer, the function of which is to facilitate the removal of the tire from the vulcanization mold at the end of the vulcanization process (alternatively, the blisters of the vulcanization mold may be moistened using a lubricant). As a result, the surface of the vulcanized tire has a lubricant layer that must be locally removed (for example by cleaning with a laser beam) in the areas where the transponder is to be applied (otherwise the transponder would not be able to adhere with sufficient force to the tire surface). Therefore, if the transponder is to be attached to the inner surface of the tire after it has been vulcanized, an additional process (cleaning of the areas where the transponder is to be applied) is required, which increases production times and costs.

[0007] Additionally, to adequately adhere the transponder to the surface of the cured tire, it is necessary to use an adhesive that is strong enough, compatible with the rubber compound that makes up the tire's innerliner, and that does not compromise the integrity of the tire's innerliner, which also represents an additional cost from an economic and environmental standpoint.

[0008] Therefore, in order to reduce manufacturing time and costs, it is preferable to attach the transponder to the inner surface of the tire when the tire is still green (i.e., before the tire is vulcanized). However, it has been observed that the high pressure and high temperature reached during the vulcanization process often cause parts of the transponder to appear outside its rubber housing (the so-called "surfacing" phenomenon), causing the transponder to malfunction (if not completely fail). In addition, the high pressure and high temperature reached during the vulcanization process often cause parts of the transponder to come into contact with the carcass cord, causing the transponder to malfunction (if not completely fail) and negatively interfering with the operation of the carcass cord. Finally, the high pressure and high temperature reached during the vulcanization process can cause irregularities in the inner liner (especially at the edge of the rubber housing of the transponder), which in the long term can cause the inner liner to crack and lead to air leakage. Summary of the Invention

[0009] The object of the present invention is to provide a method for manufacturing a tire equipped with an electronic device, which avoids damage to the tire or the electronic device and at the same time is easy and economical to implement.

[0010] According to the present invention there is provided a method for manufacturing a tire equipped with an electronic device, as claimed in the accompanying claims.

[0011] The following claims, which form an integral part of this specification, describe preferred embodiments of the invention.

[0012] The invention will now be described with reference to the accompanying drawings, which show exemplary, non-limiting embodiments. [Brief description of the drawings]

[0013] [Figure 1] FIG. 2 is a schematic diagram of a transponder inserted into a rubber housing. [Diagram 2]2 is a cross-sectional view of the transponder of FIG. 1 taken along line II-II. [Diagram 3] 3 is a cross-sectional view of the transponder of FIG. 1 taken along the line III-III. [Figure 4] FIG. 2 is a perspective view of the transponder of FIG. 1. [Diagram 5] FIG. 2 is an exploded perspective view of the transponder of FIG. 1. [Figure 6] 2 is a graph showing the change in strength of rubber as the vulcanization process progresses. [Figure 7] 1 is a graph showing the change in adhesion of rubber as the vulcanization process progresses. [Figure 8] FIG. 2 is a schematic cross-sectional view of a tire to which the transponder of FIG. 1 is applied. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] In Fig. 1, the number 1 refers in its entirety to a transponder, i.e. an electronic device (usually passive, i.e. without its own power source) capable of storing information and communicating by means of radio frequencies. In other words, the transponder 1 is a "smart label" of small dimensions suitable to respond to remote polling on the part of a specific fixed or mobile equipment called a reader (or polling device). The reader is capable of reading and / or modifying the information contained in the transponder 1 being polled, as well as communicating with the transponder 1 itself by radio frequencies. The transponder 1 is therefore part of a wireless reading and / or writing system operating according to the so-called "radio frequency identification (RFID)" technology.

[0015] As shown in Figure 1, the transponder 1 comprises an electronic circuit 2 (i.e., a microchip) with a non-volatile memory (typically EEPROM or FRAM, the latter being more expensive but technologically more advanced), an antenna 3 connected to the electronic circuit 2, and a support 4, often defined as a "substrate" (which may comprise, for example, a thin sheet of copper-clad vetronite, FR4, or other similar material) that supports both the electronic circuit 2 and the antenna 3. As will be explained in more detail below, the support 4 may also be absent. In the embodiment shown in Figure 1, the antenna 3 is a dipole antenna (or simply a dipole), with two equally open arms implemented using a linear conductor through which a current flows and which radiates an electromagnetic field remotely.

[0016] In use, the antenna 3 receives electromagnetic signals which, by electromagnetic induction, induce a potential difference in the antenna 3, which causes a current to circulate in the electronic circuit 2 and power it. When thus activated, the electronic circuit 2 uses the antenna 3 to transmit data contained in its memory and, if necessary, to modify the data contained in said memory.

[0017] As shown in Figures 1, 2 and 3, the transponder 1 is inserted into a rubber housing 5 comprising two strips 6 and 7 of green rubber superimposed and pressed against one another. In general, the two green rubber strips 6 and 7 of the housing 5 are longer / wider than the transponder 1 (i.e. than the electronic circuit 2 and the antenna 3).

[0018] According to an alternative embodiment (not shown), the support 4 is absent and its function is taken over by the rubber strips 6 and 7 of the housing 5 .

[0019] According to a preferred (but obviously non-limiting) embodiment, the thickness T of the housing 5 (within the transponder 1) before vulcanization is 2.3-2.9 mm (and for example equal to 2.6 mm), the width W of the housing 5 before vulcanization is about 20-45 mm (and for example equal to 40 mm) and the length L of the housing 5 before vulcanization is about 70-90 mm (and for example equal to 80 mm). According to a preferred embodiment, the thickness T of the housing 5 before vulcanization is equal to the thickness of the transponder 1 plus a thickness of 0.4-0.5 mm per side (i.e. 0.8-1.0 mm in total). Thus, the two rubber strips 6 and 7 before vulcanization have the same thickness (equal to 0.4-0.5 mm), but this thickness is selected so that between the transponder 1 and the outer surface of each rubber strip 6 or 7 before vulcanization there is a rubber thickness of at least 0.5 mm (more generally, at least 0.4 mm), i.e. at least 0.5 mm (0.4 mm) of rubber is provided between the transponder 1 and the outer surface of each rubber strip 6 or 7 before vulcanization. According to this rule, if the maximum thickness of the transponder 1 (i.e. in its thickest area) is 1.6 mm, then the thickness T of the housing 5 (with the transponder 1 in it) before vulcanization will be equal to 2.6 mm. If the transponder 1 is thicker or thinner, the thickness T of the housing 5 will be thicker or thinner as well.

[0020] As a result, the two rubber strips 6 and 7 before vulcanization have the same thickness, which is equal to half the thickness of the transponder 1 plus approximately 0.4 to 0.5 mm.

[0021] When the two rubber strips 6 and 7 before vulcanization have the same thickness, which is equal to half the thickness of the transponder 1 plus about 0.4-0.5 mm, there is a layer of rubber between the transponder 1 (enclosed between the two rubber strips 6 and 7) and the outer surface of the two rubber strips 6 and 7 before vulcanization, with a thickness of about 0.4-0.5 mm. This thickness of unvulcanized rubber ensures that at the end of the vulcanization process, between the transponder 1 (enclosed between the two rubber strips 6 and 7) and the outer surface of the two vulcanized rubber strips 6 and 7, there is a layer of vulcanized rubber with a thickness of at least 0.2 mm (i.e. not less than 0.2-0.3 mm and generally slightly greater than 0.2-0.3 mm). In other words, the final result obtained at the end of the vulcanization process is that the transponder 1 (enclosed between the two rubber strips 6 and 7) is covered (and "protected" by) at least 0.2-0.3 mm of vulcanized rubber.

[0022] Typically, the length L of the housing 5 before vulcanization is equal to the length of the transponder 1 plus 2-5 mm per side (ie 4-10 mm in total).

[0023] In the embodiment shown in the attached drawings, the rubber strip 7 is slightly smaller (i.e. narrower and shorter) than the underlying rubber strip 6 (the difference in size between the two rubber strips 6 and 7 before vulcanization is between 0.5 mm and 8 mm). In this regard, it is important to note that the rubber strip 7 being slightly smaller (i.e. narrower and shorter) than the underlying rubber strip 6 provides the following technical effect: the rubber step in the inner liner of the tire, which creates a block to the air flow during vulcanization, is reduced (assumed to be substantially cone-shaped) during vulcanization, and various molding defects can be avoided. According to another embodiment (not shown), the rubber strip 7 has exactly the same size as the underlying rubber strip 6. In particular, in the embodiment shown in the attached drawings, the rubber strip 6 has a pre-vulcanization length L of 75 to 85 mm (preferably 80 mm), a pre-vulcanization width W of 20 to 45 mm (preferably 40 mm) and a pre-vulcanization thickness T of 1.2 to 1.4 mm (preferably 1.3 mm). Instead, the rubber strip 7 has a pre-vulcanization length L of 65 to 75 mm (preferably 70 mm), a pre-vulcanization width W of 33 to 37 mm (preferably 35 mm) and a pre-vulcanization thickness T of 1.2 to 1.4 mm (preferably 1.3 mm).

[0024] According to a preferred embodiment, in plan view, each rubber strip 6 or 7 has two small rounded ends so as to have no sharp edges.

[0025] The rubber strip 6 consists of fully green rubber (i.e. rubber that has not been vulcanized at all, even partially), whereas the rubber strip 7 consists of only partially vulcanized rubber (i.e. rubber where the vulcanization has been initiated but not completed, i.e. neither fully green nor fully vulcanized). In particular, the rubber strip 7 consists of 20-40% vulcanized rubber, i.e. rubber that has undergone 20-40% vulcanization (as described in more detail below).

[0026] As shown in Figures 6 and 7, as the percentage of vulcanization %C progresses from 0% (corresponding to fully green rubber) to 100% (corresponding to fully vulcanized rubber), the ability of the rubber to form thioether bonds (i.e., its ability to attach to other materials) decreases, as shown in Figure 7, while at the same time the stiffness R of the rubber increases, as shown in Figure 6. In mechanics of materials, stiffness is the ability of a body to resist (resist) elastic deformation caused by an external force, and its inverse is called yieldability or flexibility. The ratio between the external force and the elastic deformation is called the "Young's modulus", or modulus of elasticity (where its unit of measurement is N / m 2 Young's modulus is known as the stiffness of a material and represents a direct measurement of the stiffness of a material (the lower the Young's modulus, the less stiff the material is and therefore the easier it is to deform).

[0027] Generally, the percentage of vulcanization %C is measured based on the period of time the rubber was exposed to the vulcanization temperature (typically 160-180°C, or more commonly 140-200°C). Thus, a percentage of vulcanization %C equal to 50% indicates that the rubber was exposed to the vulcanization temperature for 50% of the time required to achieve complete vulcanization.

[0028] According to the preferred embodiment shown in FIG. 6, the rubber strip 7 has a maximum stiffness R MAX Of these, the rubber has a stiffness R of 20% (R1) to 40% (R2) (alternatively, stiffness R is the maximum stiffness R reached at the completion of vulcanization). MAX (It may be between 20-25% and 50% of the total stiffness R). As mentioned above, the stiffness R may be measured using the corresponding "Young's modulus" or elasticity modulus, so that an increase in stiffness R corresponds to an increase in the "Young's modulus". In particular, the rubber strip 7 consists of a rubber having a tangent elastic constant of 50 Nm to 100 Nm (more typically, 40 Nm to 120 Nm).

[0029] Preferably, the two rubber strips 6 and 7 consist of one and the same type of rubber compound, but alternatively, the two rubber strips 6 and 7 could consist of two different types of rubber compounds.

[0030] As shown in FIG. 8, the housing 5 containing the transponder 1 is coupled (mounted) to a tire 8 with a toroidal case 9. The toroidal case 9 has two side flaps, since it is partially folded on itself (i.e. two layers overlapped between, usually called "turn-up"). On either side of the carcass 9, two annular beads 10 are provided, each of which is surrounded by the carcass 9. The carcass 9 supports an annular tread 11 by means of an intervening tread belt 12. Inside the body ply 9, an inner liner 13 is arranged, which is airtight, constitutes an inner lining and has the function of keeping air in the tire 8 and maintaining the tire pressure of that same tire 8 over time.

[0031] The construction of the tire 8 includes inserting the transponder 1 between two rubber strips 6, and then configuring the housing 5 by applying (attaching) the housing 5 to the inner liner 13 of the green tire 8 so that the rubber strips 6 are in direct contact with the inner liner 13 and the rubber strips 7 are separated from the inner liner 13 by the interposition of the rubber strips 6 (i.e., the rubber strips 6 are on the side of the inner liner 13 and the rubber strips 7 are on the opposite side to the inner liner 13).

[0032] Once the housing 5 (containing the transponder 1 therein) is applied to the inner liner 13 of the green tire 8, the green tire 8 with the housing 5 undergoes a vulcanization process, at the end of which the housing 5 (containing the transponder 1 therein) becomes an integral and inseparable part of the tire 8. Of course, the housing 5 may be applied to the inner liner 13 of the green tire 8 in any position, and the one shown in Figure 8 is just one possible, non-limiting example.

[0033] According to a preferred (but non-binding) embodiment shown in Figure 8, the housing 5 is applied to the inner liner 13 of the green tire 8 at the sidewall of the tire 8 and in such a way that the centre of the housing 5 has a radial height, measured from the radially innermost part across the tread, that is less than 50% of the cross-sectional height SH of the tire (also measured radially). In this regard, it is important to note that the housing 5 is preferably applied to the inner liner 13 of the green tire 8 such that the width W of the housing 5 is oriented radially, the length L of the housing 5 is oriented circumferentially and the thickness T of the housing 5 is oriented axially.

[0034] The embodiments described herein may be combined without departing from the scope of protection of the present invention.

[0035] The manufacturing method described above has many advantages.

[0036] Firstly, the above-described manufacturing method is very simple and economical insofar as it involves carrying out few operations that are easily automated: essentially, when compared to the manufacture of tires without a transponder 1, only the addition of fastening the housing 5 to the green tire 8 (an operation that can be carried out before the so-called "tip-turning", when the green tire 8 is still flat).

[0037] Furthermore, the above-described manufacturing method makes it possible to avoid high pressures and temperatures reached during the vulcanization process that would cause parts of the transponder 1 to appear on the outside of its rubber housing 5 (the so-called "surfacing" phenomenon), to avoid high pressures and temperatures reached during the vulcanization process that would cause parts of the transponder 1 to come into contact with the cord of the case 9, and to prevent the high pressures and temperatures reached during the vulcanization process from causing unevenness in the inner liner 13.

[0038] Finally, the manufacturing method described above ensures a sufficiently strong and durable attachment of the transponder 1 to the tire 8, thereby avoiding the risk of the transponder 1 becoming detached, even partially, from the tire 8.

[0039] It is important to emphasize that the fact that, in plan view, each strip of rubber 6 or 7 has two small rounded ends (so as to have no sharp edges) is important because the absence of sharp edges (which would be there if the shape, in plan view, was instead perfectly rectangular) reduces the stresses that the housing 5 transmits to the inner liner 13 during the vulcanization process. [Explanation of symbols]

[0040] 1 Transponder 2 Electronic circuit 3 Antennas 4 Support 5. Housing 6. Strip 7. Strip 8 Tires 9. Carcass 10 Beads 11 Tread 12 Treadbelt 13 Inner Liner L Length W width T Thickness SH Section height

Claims

1. A method for manufacturing a tire (8) equipped with an electronic device (1), comprising the steps of: inserting said electronic device (1) between a first rubber strip (6) and a second rubber strip (7), said first rubber strip (6) and said second rubber strip (7) surrounding said electronic device (1) defining itself a housing (5) therebetween; applying said housing (5) to an inner liner (13) of a green tire (8) such that said first strip of rubber (6) is in direct contact with said inner liner (13) and said second strip of rubber (7) is separated from said inner liner (13) by the interposition of said first strip of rubber (6); subjecting said green tire (8) with said housing (5) to a vulcanization process; Including, said first rubber strip (6) consisting entirely of green rubber; A method of manufacture, wherein said second rubber strip (7) consists of only partially vulcanized rubber, i.e. rubber where vulcanization has been initiated but not completed.

2. A method according to claim 1, wherein said second strip of rubber (7) consists of 20-40% vulcanized rubber, ie rubber that has undergone 20-40% vulcanization.

3. The second rubber strip (7) has a maximum stiffness (R MAX 3. The method according to claim 1, wherein the rubber has a rigidity (R) of 25% to 50% of the total rigidity (R).

4. A method according to claim 1, 2 or 3, wherein the second strip of rubber (7) consists of a rubber having a tangent elastic constant between 40 Nm and 120 Nm.

5. A method according to any one of the preceding claims, wherein the housing (5) before vulcanisation has a total thickness (T) equal to the thickness of the electronic device (1) plus 0.5 mm per side.

6. A method according to any one of the preceding claims, in which there is a rubber thickness (T) between the electronic device (1) and the outer surface of each rubber strip (6, 7) before vulcanisation of at least 0.4 mm, preferably at least 0.5 mm.

7. A method according to any one of the preceding claims, in which there is a rubber thickness (T) between the electronic device (1) and the outer surface of each rubber strip (6, 7) after vulcanisation of at least 0.2 mm, preferably at least 0.3 mm.

8. A method according to any one of the preceding claims, wherein the second rubber strip (7) is smaller than the first rubber strip (6).

9. A method according to claim 8, wherein the size difference between the two rubber strips (6, 7) is between 0.5 mm and 8 mm.

10. A method according to any one of the preceding claims, wherein in plan view each rubber strip (6 or 7) has two small rounded ends so as not to have sharp edges.

11. A method according to any one of the preceding claims, wherein the two strips of rubber (6, 7) have the same thickness, equal to half the thickness of the electronic device (1) plus 0.5 mm.

12. said first strip of rubber (6) has a length (L) of 75-85 mm, a width (W) of 20-45 mm and a thickness of 1.2-1.4 mm; A method according to any one of the preceding claims, wherein said second strip of rubber (7) has a length (L) of 65 to 75 mm, a width (W) of 33 to 37 mm and a thickness of 1.2 to 1.4 mm.

13. Method according to any one of claims 1 to 12, wherein the housing (5) is applied to the inner liner (13) of a green tire (8) at the sidewall of the tire (8) and in such a way that a centre of the housing (5) has a radial height, measured from its radially innermost part across the tread, that is less than 50% of the section height (SH) of the tire (8).

Citation Information

Patent Citations

  • Manufacturing method of tire with electronic component

    JP2007137037A

  • IC tag, pneumatic tire fitted with it and method for fitting IC tag

    JP2008137615A

  • System for attaching electronic device or other item to pneumatic tire

    JP2013112342A

  • RFID tag, tire with built-in RFID tag, and manufacturing method for RFID tag

    JP2021093606A

  • IC tag, pneumatic tire fitted with the same, and method of fitting IC tag

    US20100032066A1