Roll for manufacturing electrodes of secondary batteries and electrode manufacturing device using the same

The roll structure with complementary stretching and adjustable step rings addresses thickness differences in electrode manufacturing, preventing wrinkles and deformation while adapting to varying dimensions without frequent roll changes.

JP2024543431AActive Publication Date: 2024-11-21LG ENERGY SOLUTION LTD

Patent Information

Application Number
JP2024527654
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-04-15
Filing Date
2022-11-10
Publication Date
2024-11-21
Estimated Expiration
2042-11-10

AI Technical Summary

Technical Problem

Existing electrode manufacturing processes face issues with wrinkles and deformation due to differences in thickness between coated and uncoated areas, leading to folds and disconnections during the rolling process, requiring frequent roll replacements for varying electrode dimensions.

Method used

A roll structure with a base surface and a stepped surface, where the stepped surface has a higher linear velocity and friction coefficient than the base surface, ensuring complementary stretching and reduced rolling rate differences between coated and uncoated areas, using detachable step rings to adapt to varying electrode dimensions.

Benefits of technology

Prevents wrinkles and deformation in uncoated areas, allows flexible roll adaptation to changing electrode dimensions, and reduces the need for frequent roll replacements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543431000001_ABST
    Figure 2024543431000001_ABST
Patent Text Reader

Abstract

The present invention is an electrode manufacturing apparatus for rolling and transporting a sheet-like electrode having an active material layer applied to at least one surface of a metal foil having a first surface and a second surface that is the reverse surface of the first surface. At least one of a rolling roll for rolling the electrode and a traveling roll for transporting the electrode after rolling includes a base roll having a predetermined diameter and a base surface provided on its outer periphery; and a step ring that is connected to the outer periphery of the base roll and has a step surface with a diameter expanded from that of the base surface. The step ring is detachably connected to the base roll. The size of the step is different from the thickness of the active material layer. The friction coefficient measured on the surface of the step surface is different from the friction coefficient of the base surface. The elastic modulus of the step ring is smaller than the elastic modulus of the base roll.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application claims priority based on Korean Patent Application No. 10-2021-0155217 dated November 11, 2021 and Korean Patent Application No. 10-2022-0046994 dated April 15, 2022, and all contents disclosed in the documents of the Korean patent application are incorporated by reference into this specification.

[0002] The present invention relates to a roll for manufacturing an electrode for a secondary battery, and more particularly, to a roll structure capable of uniformly stretching an electrode despite a difference in thickness between an area coated with an active material layer and an area not coated with an active material layer, and capable of preventing deformation of the electrode during transportation after stretching. [Background technology]

[0003] As technology for mobile devices develops and demand increases, the demand for secondary batteries as an energy source is growing rapidly. In recent years, the use of secondary batteries as a power source for electric vehicles (EVs) and hybrid electric vehicles (HEVs) has become a reality, and among these secondary batteries, there is a high demand for lithium secondary batteries, which have high energy density, high discharge voltage and output stability.

[0004] Secondary batteries are also classified according to the structure of the electrode assembly having a positive electrode / separator / negative electrode structure. Representative examples include a jelly roll (wound type) electrode assembly in which long sheet-like positive and negative electrodes are wound with a separator interposed therebetween, a stack type (lamination type) electrode assembly in which a plurality of positive and negative electrodes cut into units of a predetermined size are stacked in sequence with a separator interposed therebetween, and a stack-holding type electrode assembly in which a unit cell, for example, a bi-cell or full cell, in which positive and negative electrodes of a predetermined unit are stacked with a separator interposed therebetween is wound up.

[0005] To manufacture these electrode assemblies, sheet-shaped electrodes corresponding to the positive and negative electrodes must first be manufactured. The sheet-shaped electrodes include a support portion in which an active material layer is applied or coated on the surface of a sheet, and a plain portion in which the active material layer is not applied. These sheet-shaped electrodes are manufactured from metal sheets that are wider and longer than the support portion, and therefore are manufactured in a multi-lane shape that extends long along the conveying direction. The multi-lane electrode sheet has a shape in which a plurality of plain portions extend in the length direction and are spaced apart in the width direction.

[0006] The electrode sheet has a thickness difference between the area where the active material layer is applied and the area where the active material layer is not applied. As a result, when the multi-lane electrode sheet is rolled by a rolling roll, a difference in the amount of elongation occurs between the maintenance area and the non-coated area, which causes folds and deformation in the non-coated area. In addition, when the electrode sheet with the deformed non-coated area travels on the transfer roll, the folds and deformation are severe, and the non-coated area may be folded and broken.

[0007] US2015-0360268A1 and KR2261491B1 disclose a technique for dealing with the difference in the amount of stretch between the plain part and the maintained part by providing a step in the roll to correspond to the thickness difference between the plain part and the maintained part of the electrode sheet. However, simply providing a step geometrically corresponding to the thickness difference between the plain part and the maintained part in the rolling roll only serves to immediately eliminate the creases that occur in the plain part due to the difference in the amount of stretch, and cannot prevent the creases from occurring in the plain part.

[0008] Ultimately, unless the difference between the amount of elongation of the metal foil in the maintenance area of ​​the electrode sheet and the amount of elongation of the metal foil in the non-coating area that occurs while the electrode sheet passes through the rolling rolls is eliminated, the deformation caused by the difference in the amount of elongation will inevitably reoccur as the electrode sheet continues to run.

[0009] Furthermore, the rolls described above must be replaced whenever the thickness of the active material layer of the electrode sheet to be manufactured is changed, which is troublesome. In addition, the rolls must be replaced every time an electrode sheet with a different position of the plain portion, i.e., a different lane position, is manufactured. In addition, every time a multi-lane electrode sheet with a different size is manufactured, a corresponding roll must be manufactured, which is troublesome. Summary of the Invention [Problem to be solved by the invention]

[0010] The present invention has been devised to solve the above-mentioned problems, and aims to provide a roll that can fundamentally prevent the occurrence of creases in the non-coated portion when an electrode is stretched due to a thickness difference between the non-coated portion and the maintenance portion, and an electrode manufacturing apparatus using the same.

[0011] The present invention aims to provide a roll that can flexibly accommodate changed electrode sheets even when the thickness of an active material layer of an electrode sheet to be processed or the position or width of an uncoated portion is changed, without the need to manufacture a whole roll corresponding to each changed electrode sheet, and an electrode manufacturing apparatus using the same.

[0012] The technical object of the present invention is not limited to the above-mentioned objects, and other objects and advantages of the present invention not mentioned can be understood from the following description and can be more clearly understood from the embodiments of the present invention. In addition, it is easy to understand that the objects and advantages of the present invention can be realized by the means and combinations thereof set forth in the claims. [Means for solving the problem]

[0013] In order to solve the above-mentioned problems, the present invention provides an electrode manufacturing apparatus that rolls and transports a sheet-like electrode having an active material layer applied to at least one surface of a metal foil having a first surface and a second surface that is the reverse surface of the first surface.

[0014] The electrode manufacturing apparatus includes a rolling roll for rolling the electrode, and a traveling roll for transporting the electrode after rolling.

[0015] The rolling rolls may be a pair. The electrode may be rolled under pressure while passing between the pair of rolling rolls.

[0016] The number of the traveling roll may be at least one, and more than one.

[0017] Each traveling roll can be in contact with either the first surface or the second surface of the electrode.

[0018] The traveling rolls may be disposed above and below the electrode at different positions in the traveling direction of the electrode.

[0019] The traveling rolls can be arranged above and below the electrode at the same position in the traveling direction of the electrode.

[0020] The electrode may include a support region where an active material layer is applied to a surface of a metal foil, and a non-coated region where no active material layer is applied to the surface of the metal foil.

[0021] The sustaining area and the non-coating area may be provided on a first surface of the electrode.

[0022] The sustaining area and the non-coating area may be provided on a second surface of the electrode.

[0023] The maintaining region and the non-coating region may be provided on both the first surface and the second surface of the electrode, and the non-coating region and the maintaining region provided on the first surface and the second surface may correspond to each other.

[0024] The uncoated regions may extend in the running direction (length direction) of the electrode.

[0025] The uncoated regions may be a plurality of regions spaced apart from one another along the width direction of the electrode.

[0026] The thickness of the non-coating region of the electrode may be thinner than the thickness of the sustaining region.

[0027] At least one of the rolling rolls and the traveling rolls can have a base surface having a predetermined diameter and a stepped surface having a diameter larger than that of the base surface.

[0028] For example, the rolling roll may have both the base surface and the stepped surface, and the traveling roll may have only the base surface without the stepped surface.

[0029] As another example, the rolling roll may have only a base surface without the stepped surface, and the traveling roll may have both a base surface and a stepped surface.

[0030] As another example, the rolling roll may have both the base surface and the stepped surface, and the traveling roll may also have both the base surface and the stepped surface.

[0031] As another example, among the multiple traveling rolls, one or more traveling rolls located near the rolling roll may have both a base surface and a step surface, and the traveling rolls located behind them may have only a base surface.

[0032] The stepped surface may be provided in a ring shape at a position corresponding to the uncoated region of the electrode.

[0033] The roll may include a base roll having a predetermined diameter and a step ring coupled to an outer periphery of the base roll.

[0034] The base roll may have a cylindrical base surface on its outer periphery.

[0035] The step ring may have an outer circumferential surface that is provided with a step surface having a diameter expanded greater than that of the base surface.

[0036] The step between the base surface and the stepped surface may correspond to the step between the maintaining portion and the uncoated portion, i.e., the step between the surface of the active material layer and the surface of the exposed metal foil. Thus, the linear velocity of the stepped surface of the roll rotating at the same rotation speed may be greater than the linear velocity of the base surface. That is, the linear velocity of the stepped surface in contact with the surface of the uncoated portion may be greater than the linear velocity of the base surface in contact with the surface of the maintaining portion. If the linear velocity of the stepped surface in contact with the surface of the uncoated portion is greater, a greater tension acts on the metal foil of the uncoated portion than on the metal foil of the maintaining portion, and therefore the amount of elongation of the metal foil of the uncoated portion can be further increased.

[0037] In the rolling roll, a step between the base surface and the step surface may be smaller than a step between the maintenance portion and the non-coated portion, whereby a large pressure of the base surface acts on the maintenance portion, and rolling can be performed smoothly.

[0038] The rolling roll may have only a base surface, whereby the pressure of the base surface against the retaining portion is large, and rolling can be performed smoothly.

[0039] In the traveling roll, a step between the base surface and the stepped surface may be larger than a step between the maintenance portion and the uncoated portion, so that the pressure of the stepped surface acts on the uncoated portion to increase the elongation amount of the uncoated portion, thereby reducing the difference between the elongation amount of the metal foil in the maintenance portion area and the elongation amount of the metal foil in the uncoated portion area that occurs while passing through the rolling rolls.

[0040] A traveling roll having both a base surface and a stepped surface may be disposed immediately behind the mill roll.

[0041] When the difference between the amount of extension of the metal foil in the maintained portion and the amount of extension of the metal foil in the uncoated portion is eliminated to a predetermined ratio or more by a traveling roll having both a base surface and a step surface, a traveling roll having only a base surface can be placed in the traveling path located behind it.

[0042] The predetermined ratio may be determined within a range in which the non-coated portion does not deform during the running process, depending on the difference between the extension amount of the metal foil in the support portion and the extension amount of the metal foil in the non-coated portion.

[0043] In the roll, the base surface is defined by the base roll and the step surface is defined by the step ring.

[0044] The base surface may contact a surface of the support portion, and the step surface may contact the uncoated portion.

[0045] The position where the step ring is installed may correspond to the position of the uncoated region of the electrode that contacts the roll.

[0046] The width of the step ring may correspond to the width of the solid area corresponding to the step ring, or may be smaller, such as within about 1 mm.

[0047] The coefficient of friction measured on the surface of the step surface provided on the outer periphery of the step ring may be greater than the coefficient of friction of the base surface provided on the outer periphery of the base roll.

[0048] The step surface having a higher coefficient of friction than the base surface may be complementary to the surface of the active material layer of the electrode having a higher coefficient of friction than the surface of the metal foil.

[0049] This allows a balance between the coefficient of friction between the base surface and the active material layer and the coefficient of friction between the step surface and the metal foil, thereby further reducing the rolling ratio difference between the maintenance portion and the uncoated portion.

[0050] Such a roll structure in which the friction coefficient of the step ring is greater than the friction coefficient of the base surface can be applied to, for example, a rolling roll.

[0051] The coefficient of friction measured on the surface of the step surface provided on the outer periphery of the step ring may be smaller than the coefficient of friction of the base surface provided on the outer periphery of the base roll.

[0052] This prevents the force transmitted to the electrode sheet by the rotational force of the roll from concentrating on the relatively narrow uncoated portion, thereby preventing excessive deformation of the uncoated portion and ensuring the durability of the step ring.

[0053] In this manner, the roll structure in which the friction coefficient of the step ring is smaller than that of the base surface can be applied to, for example, a traveling roll.

[0054] The elastic modulus of the step ring may be smaller than that of the base roll. When this structure is applied to the rolling roll, the rolling effect can be further improved. When this structure is applied to the traveling roll, it is possible to prevent excessive deformation of the non-coated portion and ensure the durability of the step ring.

[0055] The base roll may include a first metal material, and the step ring may include a second metal material that is softer than the first metal material. Alternatively, the base roll may include a metal material, and the step ring may include a synthetic resin material.

[0056] This allows the rolling ratio of the non-coated portion to be improved, and the difference therebetween with the rolling ratio of the maintained portion to be further reduced.

[0057] The base roll and step ring may be provided as separate parts.

[0058] This allows the step ring to be removably coupled to the base roll.

[0059] The roll can be manufactured by providing a stepped ring on the outer periphery of a prepared base roll.

[0060] The step ring can be adhesively or glued to the base roll.

[0061] The step ring may be implemented by winding the band around the base roll once or more than once.

[0062] The band may be made of a material coated with PTFE (Polytetrafluoroethylene).

[0063] The step ring can be fixed to the base roll by a method in which the step ring is elastically deformed to expand its inner diameter, sandwiched between the base roll, and elastically restored to a reduced inner diameter.

[0064] The step ring is press-fitted axially onto the outer periphery of the base roll, and to facilitate such press-fitting, the step ring may be softer than the base roll.

[0065] The step ring can be fixed to the base roll by a method in which the step ring is thermally expanded, its inner diameter is expanded, and the step ring is sandwiched between the base roll and frozen so that its inner diameter is reduced. For the convenience of these shrink fittings, the base roll includes a first metal material, and the step ring can include a second metal material having a thermal expansion coefficient larger than that of the first metal material.

[0066] According to the present invention, the rolls of the electrode manufacturing apparatus are replaceable depending on the size and shape of the electrode that the rolls are to wind.

[0067] The roll replacement method for the electrode manufacturing apparatus includes a step of removing a step ring that has already been joined to a base roll, separating the step ring from the base roll, and further a step of reinstalling the step ring, joining another step ring to the base roll.

[0068] In the step of removing the step ring, an adhesive or bonding layer between the inner peripheral surface of the step ring and the outer peripheral surface of the base roll can be removed.

[0069] In the step of removing the step ring, the step ring can be removed from the base roll in an elastically or thermally deformed state so that its diameter expands.

[0070] In a step of removing the step ring, the step ring may be axially extruded from the base roll.

[0071] In the step of reinstalling the step ring, the inner peripheral surface of the step ring and the outer peripheral surface of the base roll can be adhered or bonded.

[0072] In the step of reinstalling the step ring, the step ring may be sandwiched between the base rolls in an elastically or thermally deformed state so that the diameter of the step ring is expanded.

[0073] In the step of reinstalling the step ring, the step ring may be axially press-fitted into the base roll. Effect of the Invention

[0074] According to the present invention, the plain portion and the maintenance portion have different elongation rates when passing through the rolling rolls, and a complementary elongation is performed in a traveling roll disposed behind the rolling roll, thereby preventing the occurrence of creases in the metal foil in the plain portion.

[0075] According to the present invention, the size of the step between the base surface and the step surface is determined to suit the characteristics of the rolling roll and the traveling roll, the friction coefficients of the base surface and the step surface are differentiated, and different elastic coefficients are applied to the base roll and the step ring, thereby making it possible to fundamentally prevent creases from occurring in the plain portion.

[0076] In the present invention, the roll is configured by detachably providing the base roll constituting the base surface and the step ring constituting the step surface, so that even if the thickness of the active material layer of the electrode sheet to be processed is changed or the position or width of the uncoated portion is changed, the roll can be easily configured to correspond to the changed electrode sheet. This reduces the trouble of having to prepare a separate roll every time the size or shape of the electrode is changed.

[0077] The above-mentioned effects and specific effects of the present invention will be described in conjunction with the following description of the preferred embodiment of the invention. [Brief description of the drawings]

[0078] [Figure 1] 1 is a perspective view showing an embodiment of an electrode that is rolled by an electrode manufacturing apparatus of the present invention; [Diagram 2] 1 is a plan view showing an embodiment of an electrode that is rolled by an electrode manufacturing apparatus of the present invention. [Diagram 3] 1A and 1B are perspective views, viewed from a first direction, illustrating a state in which an electrode is traveling through an electrode manufacturing apparatus according to the present invention and a state in which the electrode is omitted. [Figure 4] 1A and 1B are perspective views, viewed from a first direction, illustrating a state in which an electrode is traveling through an electrode manufacturing apparatus according to the present invention and a state in which the electrode is omitted. [Diagram 5] 4A to 4C are perspective views showing a state in which an electrode is traveling on an electrode manufacturing apparatus according to the present invention and a state in which the electrode is omitted, as viewed from a second direction different from the first direction. [Figure 6] 4A to 4C are perspective views showing a state in which an electrode is traveling on an electrode manufacturing apparatus according to the present invention and a state in which the electrode is omitted, as viewed from a second direction different from the first direction. [Figure 7]3A and 3B are side views and top view showing a state in which an electrode is transported through the electrode manufacturing apparatus according to the present invention. [Figure 8] 3A and 3B are plan views respectively seen from the side and above showing a state in which an electrode is transported through the electrode manufacturing apparatus according to the present invention. [Figure 9] 1A to 1C are views showing a first embodiment of an assembly process of a base roll and a step ring of a roll of an electrode manufacturing apparatus. [Figure 10] 11A to 11C are views showing a second embodiment of an assembly process of a base roll and a step ring of an electrode manufacturing apparatus. [Figure 11] 13A to 13C are views showing a third embodiment of an assembly process of a base roll and a step ring of an electrode manufacturing apparatus. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0079] The above-mentioned objects, features and advantages will be described in detail below with reference to the accompanying drawings, so that a person having ordinary skill in the art to which the present invention pertains can easily implement the technical idea of ​​the present invention. In describing the present invention, if a detailed description of a known technology according to the present invention is deemed to obscure the gist of the present invention, the detailed description will be omitted. Hereinafter, preferred embodiments according to the present invention will be described in detail with reference to the accompanying drawings. The same reference numerals in the drawings are used to indicate the same or similar components.

[0080] Although the terms "first", "second", etc. are used to indicate various components, it is understood that these components are not limited by these terms. These terms are used merely to distinguish one component from another, and it is understood that a first component may also be a second component unless otherwise specified.

[0081] Throughout the specification, unless otherwise specified to the contrary, each element may be singular or plural.

[0082] Hereinafter, when an arbitrary structure is arranged on the "top (or bottom)" of a component or "above (or below)" a component, it means that the arbitrary structure is not only arranged in contact with the upper surface (or lower surface) of the component, but also that other structures may be interposed between the component and the arbitrary structure arranged on (or below) the component.

[0083] In addition, when a component is described as being "coupled," "coupled," or "connected" to another component, it should be understood that the components may be directly coupled or connected to each other, but that there may be other components "intervening" between each component, or each component may be "coupled," "coupled," or "connected" via other components.

[0084] As used herein, singular expressions include plural expressions unless the context clearly indicates otherwise. In this application, the terms "comprise" or "include" should not be interpreted as including all of the components or steps described in the specification, but should be interpreted as including some components or steps that may not be included, or may further include additional components or steps.

[0085] In addition, the singular expressions used in this specification include the plural expressions unless the context clearly indicates otherwise. The terms "comprise" or "include" in this application should not be interpreted as including all of the components or steps described in the specification, but should be interpreted as including some components or steps that may not be included, or may further include additional components or steps.

[0086] In the entire specification, "A and / or B" means A, B, or A and B, unless otherwise specified, and "C to D" means C or more and D or less, unless otherwise specified.

[0087] In the following, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings.

[0088] In describing the embodiments, the length direction of the electrode means the direction in which the electrode is transported, and the width direction of the electrode means the direction corresponding to the width of the roll.

[0089] <Electrode sheet> An embodiment of an electrode used in the electrode manufacturing apparatus of the present invention will be described below with reference to Figures 1 and 2. The electrode 10 includes a sheet-like metal foil 20 having a predetermined width and extending in the length direction. An active material layer 30 is applied or coated on a first surface 21 and a second surface 22, which are the front and back surfaces of the metal foil.

[0090] The active material layer 30 can be applied to at least one of the first surface 21 and the second surface 22. In the embodiment, a structure in which the active material layer 30 is applied to both surfaces is exemplified.

[0091] When the active material layer 30 is applied to the surface of the metal foil 20, there may be an area where the active material layer 30 is applied and an area where the active material layer 30 is not applied. In this case, one or more uncoated area 12 areas where the active material layer 30 is not applied may extend long in the length direction within the maintaining area 13 area of ​​the active material layer 30. In addition, the uncoated area 12 areas and the maintaining area 13 areas provided on the first surface 21 and the second surface 22 may be formed at positions corresponding to each other.

[0092] In the embodiment, two lanes of plain portion 12 are provided inside active material layer 30 in the width direction, but the number of lanes of plain portion 12 may vary from one to two or more. When plain portion 12 has a plurality of lanes, the plain portion 12 regions may be arranged at a distance from one another along the width direction of the electrode.

[0093] As a result, the sustaining portion 13 region and the non-coating portion 12 region may have a certain width and extend in the running direction (length direction) of the electrode.

[0094] The thickness of the non-coating portion 12 area of ​​the electrode 10 is thinner than the thickness of the maintaining portion 13 area.

[0095] Said electrode 10 can constitute either the positive or negative plate of a secondary battery.

[0096] In the present invention, the positive electrode active material coated on the positive electrode plate and the negative electrode active material coated on the negative electrode plate may be any active material known in the art without any limitations.

[0097] The positive electrode active material is a layered compound such as lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2), or a compound substituted with one or more transition metals; 1+x Mn 2-x Lithium manganese oxides (LiMnO2), such as LiMnO3, LiMn2O3, and LiMnO2; lithium copper oxide (Li2CuO2); vanadium oxides, such as LiV3O8, LiFe3O4, V2O5, and Cu2V2O7; and the chemical formula LiNi 1-x M x Lithium nickel oxide with nickel site represented by the chemical formula LiMn2-xM2O2 (where M=Co, Mn, Al, Cu, Fe, Mg, B, or Ga, and x=0.01 to 0.3); x Lithium intercalation materials include, but are not limited to, lithium manganese composite oxides represented by Li2Mn3MO8 (wherein M is Co, Ni, Fe, Cr, Zn, or Ta, and x is 0.01 to 0.1); LiMn2O4 in which part of the lithium in the chemical formula is replaced with an alkaline earth metal ion; disulfide compounds; Fe2(MoO4)3, or composite oxides formed by a combination of these.

[0098] The metal foil, i.e., the positive electrode current collector, has a thickness of, for example, 3 to 500 μm. The positive electrode current collector is not particularly limited as long as it does not induce chemical changes in the battery and has conductivity, and for example, stainless steel, aluminum, nickel, titanium, plastic carbon, or aluminum or stainless steel surface-treated with carbon, nickel, titanium, silver, etc. can be used. The electrode current collector can be formed with fine irregularities on its surface to increase the adhesive strength of the positive electrode active material, and can be in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.

[0099] A conductive material can be further mixed into the positive electrode active material particles. These conductive materials are added, for example, in an amount of 1 to 50% by weight based on the total weight of the mixture containing the positive electrode active material. These conductive materials are not particularly limited as long as they do not induce chemical changes in the battery and have high conductivity, and examples of the conductive materials that can be used include graphite such as natural graphite and artificial graphite; carbon black such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, and samar black; conductive fibers such as carbon fiber and metal fiber; metal powders such as carbon fluoride, aluminum, and nickel powder; conductive whiskers such as zinc oxide and potassium titanate; conductive oxides such as titanium oxide; and conductive materials such as polyphenylene derivatives.

[0100] In addition, the negative electrode is fabricated by coating and drying negative electrode active material particles on a negative electrode current collector, which is a metal foil, and may further include components such as the aforementioned conductive material, binder, and solvent, as necessary.

[0101] The negative electrode current collector has, for example, a thickness of 3 to 500 μm. These negative electrode current collectors are not particularly limited as long as they do not induce chemical changes in the battery and have conductivity. For example, copper, stainless steel, aluminum, nickel, titanium, plastic carbon, those surface-treated with carbon, nickel, titanium, silver, etc. on the surface of copper or stainless steel, aluminum-cadmium alloy, etc. can be used. Also, similar to the positive electrode current collector, fine irregularities can be formed on the surface to strengthen the binding force of the negative electrode active material, and it can be used in various forms such as films, sheets, foils, nets, porous bodies, foams, non-woven fabric bodies, etc.

[0102] The negative electrode active material is, for example, carbon such as graphitizable carbon and graphite-based carbon; Li x Fe2O3 (0 ≦ x ≦ 1), Li x WO2 (0 ≦ x ≦ 1), Sn x Me 1-x Me’yO z (Me: Mn, Fe, Pb, Ge; Me’: Al, B, P, Si, Group 1, Group 2, Group 3 elements of the periodic table, halogen; 0 < x ≦ 1; 1 ≦ y ≦ 3; 1 ≦ z ≦ 8) metal composite oxides; lithium metal; lithium alloys; silicon-based alloys; tin-based alloys; oxides such as SnO, SnO2, PbO, PbO2, Pb2O3, Pb3O4, Sb2O3, Sb2O4, Sb2O5, GeO, GeO2, Bi2O3, Bi2O4, Bi2O5; conductive polymers such as polyacetylene; Li-Co-Ni-based materials, etc. can be used.

[0103] The binder polymer usable in the electrode is a component that aids in binding between the electrode active material particles and the conductive material and between the electrode current collector, and is added in an amount of, for example, 1 to 50 wt % based on the total weight of the mixture including the electrode active material. Examples of these binder polymers include polyvinylidene fluoride-co-hexafluoropropylene (PVdF), polyvinylidene fluoride-co-trichloroethylene, polymethylmethacrylate, polybutylacrylate, polyacrylonitrile, polyvinylpyrrolidone, polyvinylacetate, ethylene-vinyl acetate copolymer, polyethylene oxide, polyarylate, cellulose acetate, cellulose acetate butyrate, and cellulose acetate propionate. The binder polymer may be any one selected from the group consisting of cellulose acetate propionate, cyanoethyl pullulan, cyanoethyl polyvinyl alcohol, cyanoethyl cellulose, cyanoethyl sucrose, pullulan, and carboxyl methyl cellulose, or a mixture of two or more of these, but is not limited thereto.

[0104] Non-limiting examples of the solvent used in the preparation of the electrode include acetone, tetrahydrofuran, methylene chloride, chloroform, dimethylformamide, N-methyl-2-pyrrolidone (NMP), cyclohexane, water, or mixtures thereof, etc. These solvents provide an appropriate level of viscosity so that a slurry coating layer can be formed at a desired level on the surface of the electrode current collector.

[0105] The negative electrode may include a current collector; and a negative electrode active material layer located on at least one surface of the current collector and including a negative electrode active material, a binder polymer, and a conductive material, the negative electrode active material layer including a lower layer region that contacts the current collector and an upper layer region that contacts the lower layer region and extends to a surface of the negative electrode active material layer, and the lower layer region and the upper layer region each independently include at least one of graphite and a silicon-based compound as a negative electrode active material.

[0106] The lower layer region may include natural graphite as a negative electrode active material, and the upper layer region may include artificial graphite as a negative electrode active material.

[0107] The lower layer region and the upper layer region may each independently further include a silicon-based compound as a negative electrode active material.

[0108] The silicon-based compound is SiO x (0≦x≦2) and SiC.

[0109] According to an embodiment of the present invention, the negative electrode may be manufactured by coating and drying a lower layer slurry containing a lower layer negative electrode active material on a current collector to form a lower layer region, and then coating and drying an upper layer slurry containing an upper layer negative electrode active material on the lower layer region to form an upper layer region.

[0110] According to an embodiment of the present invention, the negative electrode may be manufactured by a method including the steps of: preparing a lower layer slurry including a lower layer negative electrode active material and an upper layer slurry including an upper layer negative electrode active material; coating one surface of a negative electrode current collector with the lower layer slurry, and coating the upper layer slurry on the lower layer slurry simultaneously or with a predetermined time lag; and drying the coated lower layer slurry and upper layer slurry simultaneously to form an active material layer.

[0111] In the latter method, a mixed region (intermixing) where different types of active materials are mixed with each other may exist at the contact portion between the lower layer region and the upper layer region in the negative electrode. This is because, when a lower layer slurry containing a lower layer negative electrode active material and an upper layer slurry containing an upper layer negative electrode active material are coated on a current collector simultaneously or successively with a very short time lag and then simultaneously dried to form an active material layer, a certain mixed region is generated at the interface where the lower layer slurry and the upper layer slurry come into contact before drying, and then the mixed region is formed into a layer shape as the mixture region while drying.

[0112] In the negative electrode active material layer according to an embodiment of the present invention, the weight ratio (or load ratio per unit area) of the upper layer region to the lower layer region may be 20:80 to 50:50, specifically, 25:75 to 50:50.

[0113] The thicknesses of the lower and upper regions of the negative electrode active material layer of the present invention may not be completely equal to the thicknesses of the coated lower layer slurry and the coated upper layer slurry, but the thickness ratio of the lower and upper regions of the negative electrode active material layer of the present invention finally obtained as a result of a drying or selective rolling process may be equal to the thickness ratio of the coated lower layer slurry and the coated upper layer slurry.

[0114] The first slurry is coated, and the second slurry is coated on the first slurry at the same time or after a predetermined time difference, and according to an embodiment of the present invention, the predetermined time difference may be 0.6 seconds or less, or 0.02 seconds to 0.6 seconds, or 0.02 seconds to 0.06 seconds, or 0.02 seconds to 0.03 seconds. In this way, when the first slurry and the second slurry are coated, a time difference occurs due to coating equipment, so it is more preferable to coat the first slurry and the second slurry at the same time. The method of coating the second slurry on the first slurry can use an apparatus such as a double slot die.

[0115] The step of forming the active material layer may further include a step of rolling the active material layer after the drying step, wherein the rolling may be performed by a method commonly used in the art, such as roll pressing, at a pressure of 1 to 20 MPa and a temperature of 15 to 30°C.

[0116] The step of simultaneously drying the coated lower layer slurry and the upper layer slurry to form an active material layer can be performed by a method commonly used in the art using a combination of a hot air dryer and an infrared dryer.

[0117] The weight % of the first binder polymer in the solid content of the lower layer slurry may be the same as or greater than the weight % of the second binder polymer in the solid content of the upper layer slurry. According to one embodiment of the present invention, the weight % of the first binder polymer in the solid content of the lower layer slurry may be 1.0 to 4.2 times, 1.5 to 3.6 times, or 1.5 to 3 times greater than the weight % of the second binder polymer in the solid content of the upper layer slurry.

[0118] In this case, when the ratio of the weight percentage of the first binder in the coated lower layer slurry to the weight percentage of the second binder in the coated upper layer slurry satisfies the above range, the amount of binder in the lower layer region is not too small, so that detachment of the electrode layer does not occur, and the amount of binder in the upper layer region is not too large, so that the resistance of the upper layer of the electrode is reduced, which is advantageous for fast charging performance.

[0119] The weight percentage of the first binder polymer in the solid content of the lower layer slurry may be 2 to 30 weight%, or 5 to 20 weight%, or 5 to 20 weight%, and the weight percentage of the second binder polymer in the solid content of the upper layer slurry may be 0.5 to 20 weight%, or 1 to 15 weight%, or 1 to 10 weight%, or 2 to 5 weight%.

[0120] The total proportion (wt %) of the first binder polymer and the second binder polymer in the total solid content of the lower layer slurry and the upper layer slurry may be 2 to 20 wt %, or 5 to 15 wt %.

[0121] <Electrode manufacturing equipment> Hereinafter, the electrode manufacturing apparatus of the present invention, which performs the rolling step using the roll press, will be described with reference to Figs.

[0122] The electrode manufacturing apparatus of the present invention can include a rolling roll (A) that rolls the above-mentioned sheet-like electrode 10, a traveling roll (B) that transports it, and a tension roll (C) that adjusts the tension of the electrode 10. The traveling roll (B) may be located before the rolling roll (A), but since the form of the roll 40 according to the present invention only needs to be located after the rolling roll (A), the embodiment discloses the traveling roll (B) and tension roll (C) after the rolling roll (A).

[0123] In the embodiment, a pair of the reduction rolls (A) are provided. The electrode 10 may be rolled while passing between the pair of reduction rolls (A).

[0124] The number of the traveling roll (B) may be at least one, and may be more than one. Each traveling roll (B) can contact either the first surface 21 or the second surface 22 of the electrode. The arrangement of the traveling roll (B) and the tension roll (C) shown in the embodiment is merely an example, and it is a matter of course that the technical scope of the present invention is not limited to the arrangement of these rolls.

[0125] The rolling roll (A) and the traveling roll (B) arranged behind the rolling roll (A) can have a base surface 413 having a predetermined diameter and a step surface 422 having a diameter larger than that.

[0126] The step surface 422 can be provided in a ring shape at a position corresponding to the uncoated portion 12 of the electrode 10 sliding through the electrode manufacturing apparatus.

[0127] The base surface 413 and stepped surface 422 may be provided on a roll 40 that is fabricated as one piece.

[0128] Alternatively, the part providing the base surface 413 and the part providing the step surface 422 may be manufactured as separate parts and then bonded to each other to provide the roll 40.

[0129] The base surface 413 is defined by the outer circumferential surface of the base roll 41 having a predetermined diameter. That is, the base roll 41 may be provided with a cylindrical base surface 413 on its outer periphery.

[0130] The step surface 422 is defined by a step ring 42 that is joined to the outer periphery of the base roll 41. That is, the step ring 42 can have a step surface 422 whose outer periphery has a diameter expanded larger than that of the base surface 413.

[0131] In this way, when the base roll 41 and the step ring 42 are manufactured as different parts, different materials can be used. Different materials have different inherent properties. For example, the base roll 41 and the step ring 42 may be made of materials with different elastic coefficients, may be made of materials of different series (metal, synthetic resin, etc.) themselves, and can be made of materials with different properties such as softness and thermal expansion coefficient.

[0132] The step, i.e., the difference in radius, between the base surface 413 and the step surface 422 can substantially correspond to the step between the supporting portion 13 and the uncoated portion 12, i.e., the step, i.e., the height difference, between the surface of the active material layer 30 and the exposed surface of the metal foil 20.

[0133] Thereby, the base surface 413 can contact the surface of the support portion 13 , and the step surface 422 can contact the surface of the non-coating portion 12 .

[0134] Furthermore, the position where the step ring 42 is installed on the base roll 41 can correspond to the position of the uncoated portion 12 region of the electrode 10 with which the roll 40 comes into contact.

[0135] The width of the step ring 42 may correspond to the width of the area of ​​the plain portion 12 corresponding to the step ring 42, or may be smaller than that, for example, within about 1 mm.

[0136] The coefficient of friction measured on the surface of the step surface 422 provided on the outer periphery of the step ring 42 may be different from the coefficient of friction of the base surface 413 provided on the outer periphery of the base roll 41 .

[0137] Similarly, the coefficient of friction of the surface of the support portion 13 of the electrode 10 and the coefficient of friction of the surface of the non-coated portion 12 may be different from each other.

[0138] The difference in friction coefficient between the step surface 422 and the base surface 413 may be complementary to the difference in friction coefficient between the surface of the non-coated portion 12 and the surface of the maintaining portion 13.

[0139] For example, when the coefficient of friction of the retaining portion 13 is greater than the coefficient of friction of the non-coated portion 12 , the coefficient of friction of the stepped surface 422 may be greater than the coefficient of friction of the base surface 413 .

[0140] Also, for example, the friction coefficient of the retaining portion 13 may be greater than the friction coefficient of the non-coated portion 12 , and the friction coefficient of the step surface 422 may be greater than the friction coefficient of the base surface 413 .

[0141] As a result, a frictional force may act when the metal foil 20 is pressed by the stepped surface 422, similar to the frictional force acting when the active material layer 30 is pressed by the base surface 413. As a result, when the electrode 10 is rolled while passing through the rolling roll (A), the rolling ratio difference between the maintenance portion 13 and the uncoated portion 12 may be further reduced.

[0142] The elastic modulus of the step ring 42 may be smaller than that of the base roll 41. For example, the base roll 41 may include a first metal material, and the step ring 42 may include a second metal material that is softer than the first metal material. Alternatively, the base roll 41 may include a metal material, and the step ring 42 may include a synthetic resin material. This can improve the rolling ratio of the non-coated portion and further reduce the difference with the rolling ratio of the maintained portion.

[0143] In the electrode manufacturing apparatus, the rolling roll (A) is configured as a roll 40 equipped with a step ring 42, and the traveling roll (B) located behind it is also configured as a roll 40 equipped with a step ring 42, but two or more traveling rolls (B) are provided, one of which contacts the first surface 21 of the electrode 10 and the other one of which contacts the second surface of the electrode 10, so that deformation of the uncoated portion 12 that may occur in the rolling roll (A) can be restored by the step ring 42 of the traveling roll (B) during the transport and traveling process.

[0144] <Roll replacement> According to the present invention, the roll 40 of the electrode manufacturing apparatus is replaceable depending on the size and shape of the electrode 10 that the roll 40 winds.

[0145] As described above, the position of the step ring 42 is set to correspond to the position of the uncoated portion 12, and the width of the step ring 42 is set to correspond to the width of the uncoated portion 12. Therefore, when the number, position, or width of lanes of the uncoated portion 12 of the electrode 10 applied to the electrode manufacturing apparatus varies, all of the rolls 40 to which the step rings 42 are applied must be replaced.

[0146] In the roll 40 of the present invention, the base roll 41 and the step ring 42 are provided as separate parts, but the step ring 42 is provided so as to be detachably connected to the base roll 41.

[0147] Thus, it is possible to accommodate electrodes 10 of different shapes by simply configuring the width of the step ring 42 applied to one base roll 41 to be different from each other, without providing any separate rolls corresponding to electrodes 10 of different shapes. In other words, manufacturing the base roll 41 and the step ring 42 as separate parts made of different materials not only makes it possible to more precisely control the interaction between the roll 40 and the electrode 10 during the rolling and transporting process, as described above, but also brings about a great advantage in the method of providing the roll 40 corresponding to the electrode 10.

[0148] Referring to Figure 9, a method of attaching the step ring 42 to the base roll 41 may be to first elastically deform the step ring 42 to expand its inner diameter and clamp it between the base roll 41, and then elastically restore the step ring 42 so that the inner diameter of the step ring 42 shrinks, thereby pressing the inner surface of the step ring 42 against the outer surface of the base roll 41.

[0149] Of course, according to this, in a state where the step ring 42 has already been joined to the base roll 41, the step ring 42 can be separated from the base roll 41 by performing the above joining method in the reverse order.

[0150] The step ring 42 may be made of a material having a sufficiently small elastic modulus and a wide range of elastic deformation to allow elastic deformation, such as a rubber ring.

[0151] Next, the step ring 42 can be fixed to the base roll 41 by a method in which the step ring 42 is thermally expanded to expand its inner diameter, and then frozen to reduce its inner diameter. For the convenience of this shrink fitting, the base roll 41 can include a first metal material, and the step ring 42 can include a second metal material having a larger thermal expansion coefficient than the first metal material. The selection of these materials provides further convenience when separating the step ring 42 coupled to the base roll 41.

[0152] 10, the step ring 42 can be press-fitted axially onto the outer periphery of the base roll 41. To facilitate such press-fitting, the step ring 42 may be softer than the base roll 41. This is of course also advantageous in the extrusion process that separates the step ring 42 from the base roll 41.

[0153] 11, the step ring 42 can be attached to the base roll 41 by wrapping the circumference of the base roll 41 with a tape or a band once or several times. In this case, the step ring 42 can be adhered or bonded to the base roll 41. When the step ring 42 is to be separated from the base roll 41, the adhesion or bond can be broken to separate the step ring 42 from the base roll 41.

[0154] As a result, the method for replacing the roll 40 of the electrode manufacturing equipment includes a step of removing the step ring 42 already attached to the base roll 41, separating it from the base roll 41, and further a step ring reinstallation step of attaching another step ring 42 to the base roll 41.

[0155] As described above, in the step of removing the step ring, the step ring 42 can be removed from the base roll 41 in an elastically or thermally deformed state so that its diameter expands.

[0156] Alternatively, the step ring 42 can be extruded axially from the base roll 41 .

[0157] Alternatively, the adhesive or bonding layer between the inner peripheral surface of the step ring 42 and the outer peripheral surface of the base roll 41 can be removed.

[0158] In the step of reinstalling the step ring, the step ring 42 can be clamped between the base roll 41 in an elastically or thermally deformed state so that its diameter expands.

[0159] Alternatively, the step ring 42 can be press-fitted axially into the base roll 41 .

[0160] Alternatively, the inner peripheral surface of the step ring 42 and the outer peripheral surface of the base roll 41 may be adhered or bonded to each other.

[0161] It should be understood that the above-described embodiments are illustrative in all respects and are not limiting, and the scope of the present invention is defined by the following claims rather than the above detailed description. All modifications and variations that can be achieved within the meaning and scope of the following claims, as well as equivalent concepts, should be interpreted as being included in the scope of the present invention.

[0162] Although the present invention has been described above with reference to the illustrative drawings, the present invention is not limited to the embodiments and drawings disclosed in this specification, and various modifications may be made by ordinary skilled artisans within the scope of the technical concept of the present invention. Even if the effects of the configuration of the present invention are not explicitly described and explained while describing the embodiments of the present invention, it is natural that the effects that can be predicted by the configuration should also be recognized. [Explanation of symbols]

[0163] 10 electrodes 12 Plain area 13 Maintenance Department 20 Metal Foil 21 Page 1 22 Side 2 30 Active material layer 40 rolls 41 Bass Roll 413 Base surface 42 Step Ring 422 Step surface A Roller B Travel roll C Tension roll

Claims

1. An electrode manufacturing apparatus for rolling and transferring a sheet-like electrode having an active material layer (30) applied to at least one surface of a metal foil (20) having a first surface (21) and a second surface (22) that is the reverse surface of the first surface, comprising: At least one of a rolling roll for rolling the electrode and a traveling roll for transporting the electrode after rolling (40) is A base roll (41) having a predetermined diameter and having a base surface (413) on its outer periphery; and a step ring (42) connected to the outer periphery of the base roll (41) and having a step surface (422) having a diameter expanded form greater than that of the base surface (413); Equipped with Electrode manufacturing equipment.

2. The rolling roll does not include the step ring (42), and the running roll includes the step ring (42). The electrode manufacturing apparatus according to claim 1 .

3. Both the rolling roll and the running roll are provided with the step ring (42). The electrode manufacturing apparatus according to claim 1 .

4. Among the multiple traveling rolls, one or more traveling rolls located near the rolling roll include both a base roll and a step ring, and a traveling roll arranged behind the base roll does not include a step ring. The electrode manufacturing apparatus according to claim 1 .

5. The step ring (42) is detachably coupled to the base roll (41). The electrode manufacturing apparatus according to any one of claims 1 to 4.

6. The coefficient of friction measured on the surface of the step surface (422) provided on the outer periphery of the step ring (42) is greater than the coefficient of friction of the base surface (413) provided on the outer periphery of the base roll (41); The electrode manufacturing apparatus according to claim 1 .

7. The step between the step surface (422) and the base surface (413) is smaller than the thickness of the active material layer (30). The electrode manufacturing apparatus according to claim 1 .

8. The step ring (42) is provided on the rolling roll.

8. An electrode manufacturing apparatus according to claim 6 or 7.

9. The coefficient of friction measured on the surface of the step surface (422) provided on the outer periphery of the step ring (42) is smaller than the coefficient of friction of the base surface (413) provided on the outer periphery of the base roll (41); The electrode manufacturing apparatus according to claim 1 .

10. The step between the step surface (422) and the base surface (413) is greater than the thickness of the active material layer (30). The electrode manufacturing apparatus according to claim 1 .

11. The step ring 42 is provided on the traveling roll.

11. An electrode manufacturing apparatus according to claim 9 or 10.

12. The elastic modulus of the step ring (42) is smaller than the elastic modulus of the base roll (41). The electrode manufacturing apparatus according to claim 1 .

13. The base roll (41) includes a metal material, and the step ring (42) includes a synthetic resin material. The electrode manufacturing apparatus according to claim 1 .

14. The base roll (41) includes a first metal material, and the step ring (42) includes a second metal material softer than the first metal material. The electrode manufacturing apparatus according to claim 1 .

15. The base roll (41) includes a first metal material, and the step ring (42) includes a second metal material having a thermal expansion coefficient greater than that of the first metal material. The electrode manufacturing apparatus according to claim 1 .

16. The step ring (42) is formed by winding a band around the outer periphery of the base roll (41) once or twice or more times. The electrode manufacturing apparatus according to claim 1 .

17. A base roll (41) having a predetermined diameter and having a base surface (413) on its outer periphery; and a step ring (42) connected to the outer periphery of the base roll (41) and having a step surface (422) having a diameter expanded form greater than that of the base surface (413); A method of making a roll (40) comprising: Providing the base roll (41); and A step of installing the step ring (42) on the outer periphery of the base roll (41); Including, How to make rolls.

18. The step ring (42) is sandwiched between the base roll (41) in a state in which the step ring (42) is elastically deformed so that its diameter expands. A method for making the roll of claim 17.

19. The step ring (42) is sandwiched between the base rolls (41) in a heated state so that its diameter expands, and is cooled in the sandwiched state. A method for making the roll of claim 17.

20. The step ring (42) is formed by winding a band around the outer periphery of the base roll (41) once or twice or more times. A method for making the roll of claim 17.

Citation Information

Patent Citations

  • Rolling apparatus

    JP1993028990A

  • Press device for electrode material and press-processing method

    JP2014103068A

  • Method for manufacturing secondary battery

    JP2016181345A

  • Electrode plate production apparatus

    JP2018106813A

  • Electrode Rolling Device Capable of Preventing Swell or Wrinkle of Electrode Sheet by Rolling Work

    KR1020160141448A

Cited By

  • Manufacturing method of electrode for secondary battery

    JP2024098274A

  • Method for manufacturing secondary battery electrodes

    JP7677355B2