Optimization methods to achieve energy savings

A coating with nanosized metal oxide and binder induces vibrational alignment in electromechanical devices, addressing energy loss issues by aligning electron spins and reducing resistivity for improved energy efficiency.

JP2024543854APending Publication Date: 2024-11-26アー エン シアウ
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2024529405
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-16
Filing Date
2022-10-27
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Existing methods fail to effectively reduce energy loss as heat due to irregular electron motion in electromechanical devices, leading to inefficient energy usage and increased costs.

Method used

A coating composition comprising nanosized particulate metal oxide, a binder, and a liquid carrier is applied to the surface of electromechanical devices, induced to vibrate at specific frequencies to align electron spins uniformly, reducing energy loss through vibrational alignment.

Benefits of technology

The coating method significantly reduces energy loss as heat and electrical resistivity, enhancing energy efficiency and reducing electricity costs by aligning electron spins and minimizing collisions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543854000001
    Figure 2024543854000001
  • Figure 2024543854000002
    Figure 2024543854000002
  • Figure 2024543854000003
    Figure 2024543854000003
Patent Text Reader

Abstract

The present invention relates to a method for reducing energy loss from an electromechanical device, comprising the steps of preparing a coating composition comprising a nano-sized particulate metal oxide, a binder and a liquid carrier, bombarding the composition with a vibrational force having a frequency of 20-500 kHz for at least 24 hours to produce energetic excited states in the atoms of the composition, and coating a surface of the device or a casing surrounding the device with the composition.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to optimization methods for achieving energy savings, and in particular to methods for inducing electronic vibration alignment in electromechanical devices to reduce energy loss as heat during electrical current flow. [Background technology]

[0002] Electricity has become an inevitable necessity for humans, and without electricity, human life would be in chaos. However, electricity can be costly because existing methods of generating electricity or electrical energy rely mainly on non-renewable resources. Recently, people have been paying attention to ways to minimize energy consumption or optimize energy usage in order to reduce costs and minimize the negative impacts on the environment that result from the extraction of energy from non-renewable resources.

[0003] More and more research efforts are being made to find ways to reduce energy usage or to use energy efficiently. Energy audits are conducted to find possibilities to reduce the energy input to a system without adversely affecting performance or output. Energy-saving materials such as superconductors, which have higher electrical conductivity and lower electrical resistance, are also being developed as alternatives to traditional conductive materials. Although some reduction in energy usage can be achieved, a significant amount of energy loss as heat is inevitable due to random and irregular electron spins.

[0004] Electricity involves the flow of electrons in a closed electric circuit. Typically, the flowing electrons move in a free and random manner, flowing in more or less straight paths, thus causing collisions between the atoms of the circuit. Due to the random motion of the electrons before reaching the load, a significant amount of energy is lost as heat. The extent of energy loss also depends on the specifications of the conductive wire used, such as material, diameter, length, resistivity and temperature. Summary of the Invention [Problem to be solved by the invention]

[0005] In view of the above problems, there is a need for further optimization of energy usage, where less energy is required to drive the current and less energy is lost due to random electron motion. It is therefore desirable to develop a method to improve the flow of electrons or reduce the random electron motion. The present invention provides a solution to this problem. [Means for solving the problem]

[0006] One object of the present invention is to provide an optimization method for achieving energy savings in electromechanical devices by coating a composition on the surface of the device.

[0007] Another object of the present invention is to provide the use of a coating on the surface of an electromechanical device, which coating makes it possible to induce electronic vibrational alignment in the device, thereby allowing a reduction in energy losses or an optimization of energy consumption.

[0008] It is yet another object of the present invention to provide a composition for use in a coating on a surface of an electrochemical device, the coating being capable of inducing electronic vibrational alignment therein.

[0009] It is yet another object of the present invention to reduce the cost of electricity by reducing the energy usage of electromechanical devices.

[0010] At least one of the above objects is addressed in whole or in part, and an embodiment of the present invention describes a method for reducing energy loss from an electromechanical device, comprising the steps of preparing a coating composition comprising a nano-sized particulate metal oxide, a binder and a liquid carrier, bombarding the composition with a vibrational force having a frequency of 20-500 kHz for at least 24 hours to produce energetic excited states in the atoms of the composition, and coating a surface of the device or a casing surrounding the device with the composition.

[0011] In one preferred embodiment of the present invention, it is disclosed that the electromechanical device is an electrical switchboard, a cable, a surface of a termination box or a surface of a junction box.

[0012] Preferably, the metal oxide is an oxide of aluminum, iron, magnesium, lithium, potassium, copper, tourmaline or mixtures thereof.

[0013] Preferably, the binder is an acrylic polymer.

[0014] Preferably, the liquid carrier is water.

[0015] More preferably, the water is reverse osmosis water or purified water.

[0016] In another preferred embodiment of the present invention, it is disclosed that the composition used in the method comprises 0.1-30 parts by weight of a metal oxide, 0.1-10 parts by weight of a binder, and 50-90 parts by weight of a liquid carrier.

[0017] In a further embodiment of the present invention, it is disclosed that the coating has a thickness of at least 100 μm.

[0018] It will be readily appreciated by one skilled in the art that the present invention is well adapted to carry out the objects and attain the ends and advantages set forth above and inherent therein, and the embodiments described herein are not intended as limitations on the scope of the invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] The present invention relates to optimization methods for achieving energy savings, and in particular to methods for inducing electronic vibration alignment in electromechanical devices to reduce energy loss as heat during electrical current flow.

[0020] The present invention will be described below according to the preferred embodiment of the present invention by referring to the accompanying description and drawings. However, it should be understood that the description is limited to the preferred embodiment of the present invention only for facilitating the discussion of the present invention, and it is assumed that a person skilled in the art can devise various modifications without departing from the scope of the appended claims.

[0021] The present invention discloses a method for reducing energy loss from an electromechanical device, comprising the steps of preparing a coating composition comprising a nano-sized particulate metal oxide, a binder and a liquid carrier, bombarding the composition with a vibrational force having a frequency of 20-500 kHz for at least 24 hours to produce energetic excited states in the atoms of the composition, and coating a surface of the device or a casing surrounding the device with the composition.

[0022] In a preferred embodiment of the present invention, energy losses in electromechanical devices, such as, but not limited to, electrical distribution boards, cables, termination boxes or junction boxes, are reduced by coating any surface of the device with a composition comprising nano-sized particulate metal oxide, binder and water. The surface of the device may not be limited to any type of material and may be made of glass, plastic material, metal or rubber. Preferably, the coating has a thickness of at least 100 μm so that the beneficial effects on the device are sufficiently obtained, as described below. However, it is not necessary to have a coating thickness of more than 100 μm, since there is no or only minimal improvement in the beneficial effects with further thickness.

[0023] The atoms of the coating retain enough energy to vibrate them at a pre-determined frequency similar to the natural frequency of the device for a certain time. When the surface of the device is coated, the atoms of the coating transfer vibrational energy to the atoms of the device, particularly the atoms of the conductive wire, in all directions at distances ranging from 0 mm to 300 mm. The atoms of the device are thereby induced to vibrate at similar frequencies. In particular, the atoms of the device vibrate at their natural frequency where resonance occurs. Electron vibration alignment occurs in the affected area of ​​the device, which forces the irregularly spinning electrons to align and make their spins uniform. Thus, collisions between atoms in the affected area of ​​the device are minimized and energy loss as heat due to friction between atoms is minimized. The electrical resistivity of the device is also reduced.

[0024] The composition can be uniformly coated on the surface of the electromechanical device by any coating method, such as, but not limited to, hand spraying. It should be mentioned that the surface to be coated should be clean and free of solid impurities in order to enhance the bonding of the composition to the surface. After the composition is coated on the surface, the coating can be cured at room temperature. Advantageously, the atoms of the composition will maintain vibrational energy for at least 12 months. After that, recoating of the composition may be required.

[0025] According to a preferred embodiment of the present invention, the composition preferably comprises nano-sized scale metal oxide particles. Smaller particle sizes are preferred since more surface area is available for the acquisition, retention and release of vibrational energy. The metal of the metal oxide may be selected from the group consisting of, but not limited to, aluminum, iron, magnesium, lithium, potassium, copper, tourmaline or mixtures thereof. One skilled in the art should not limit the metal oxide to one type of metal oxide, rather, it may be a mixture of two or more types of metal oxide. High conductivity metals are preferred because they can hold a larger charge and therefore a higher capacity and capacity to maintain vibrational energy that is subsequently transferred to the coated device. Preferably, the composition comprises 0.1 to 50 parts by weight of metal oxide. The amount of energy transferred to induce resonance may not be sufficient with less than 0.1 parts by weight of metal oxide. However, any amount of metal oxide above 50 parts by weight does not provide additional beneficial effects.

[0026] The metal oxide particles are contained in a liquid carrier, so that the prepared composition is easy to apply and coat on a surface. The liquid carrier also functions as a medium to transfer energy from an energy source to the metal oxide or from the metal oxide to the atoms of the device. Any kind of liquid carrier that does not react with the metal oxide can be used. Preferably, the liquid carrier is water. More preferably, the alcohol can be selected from reverse osmosis water or purified water. Preferably, the composition comprises 50-90 parts by weight of the liquid carrier.

[0027] As described by the preferred embodiment of the present invention, a binder is required to ensure that the coating is adequately bonded to the surface being coated. Preferably, the binder is an acrylic polymer. More preferably, the acrylic polymer may be selected from polymethylmethacrylate, styrene, acrylates or methacrylates. Any acrylic binder that allows the composition to be cured at room temperature in a short curing time may be used. Preferably, the composition comprises 0.1 to 10 parts by weight of the binder.

[0028] The composition for use in the method described in any of the above descriptions can be prepared using the following method. The metal oxide, binder and liquid carrier are mixed uniformly one by one. The mixing order is preferably binder, liquid carrier and metal oxide. It should be noted that the metal oxide should not be added before the liquid carrier to achieve a uniform mixture. More preferably, the composition is homogenized by operating a sonic mixer at a frequency of 20 kHz to 40 kHz for at least more than 1 hour. However, it is not necessary to mix the composition for more than 2 hours to achieve a uniform mixture. Any other method of homogenizing the mixture can be adopted. During homogenization, the nanoparticle metal oxide can be further broken down to a smaller size with a larger surface area for the acquisition, retention and release of vibrational energy.

[0029] The mixture is then subjected to impact with a vibrational force of a frequency between 20 kHz and 100 KHz for at least 24 hours in order to store the energy in the nanoparticles. This vibrational force can be provided in any form. However, it should be noted that the vibrational force should not be induced by any kind of magnetic field, which may cause damage to the device due to the magnetic energy maintained in the atoms of the composition. Preferably, the vibrational force is provided by ultrasonic means. A sufficiently long impact time is required so that the atoms of the composition, especially the atoms of the metal oxide, can acquire and maintain the energy from the vibrational force for a certain period of time. The atoms of the composition with the energy are excited to vibrate violently for a certain period of time at a frequency similar to the frequency of the vibrational force.

[0030] The homogenization step and the impact step can be performed in one operation where only ultrasonic treatment is utilized. After mixing of the composition, the mixture is subjected to ultrasonic treatment, thereby performing homogenization and energy harvesting simultaneously. The ultrasonic frequency is preferably 20kHz to 100KHz, and the treatment is preferably continued for at least 24 hours, more preferably at least 48 hours. However, compositions produced using one operation method are prone to phase separation. Although phase separation may not affect the performance of the composition, the aesthetic appearance of the composition may not be acceptable to the user.

[0031] Alternatively, the homogenization and impact steps can be performed in two separate operations, where only ultrasonication is further utilized. The binder and the liquid carrier are mixed and homogenized by an ultrasonic mixer at a frequency of 20 kHz to 40 kHz for at least 1 hour, preferably not more than 2 hours. The metal oxide is then added to the homogenized mixture. The resulting mixture is subjected to ultrasonication at a frequency of 20 kHz to 100 kHz for at least 24 hours, more preferably at least 48 hours. EXAMPLES

[0032] The following non-limiting examples are provided to illustrate preferred embodiments of the invention.

[0033] Example 1 The compositions shown in Table 1 are mixed one by one. The mixture is subjected to ultrasonic treatment at a frequency of 50 kHz for 24 hours.

[0034] [Table 1]

[0035] Example 2 The composition is as shown in Table 2. Acrylate, styrene and methanol are mixed one by one and homogenized in an ultrasonic mixer at a frequency of 28 kHz for 1 hour. Then copper oxide is added. The mixture is subjected to ultrasonic treatment at a frequency of 60 kHz for 24 hours.

[0036] [Table 2]

[0037] Example 3 The compositions shown in Table 3 are mixed one by one. The mixture is subjected to ultrasonic treatment at a frequency of 40 kHz for 24 hours.

[0038] [Table 3]

[0039] The composition is as shown in Table 2. The methacrylate, acrylate and water are mixed one by one and homogenized in an ultrasonic mixer at a frequency of 30 kHz for 1 hour. Then, aluminum oxide and copper oxide are added. The mixture is subjected to ultrasonic treatment at a frequency of 40 kHz for 24 hours.

[0040] Example 4 The composition used in Example 3 is coated onto the clean surface of the cable. The effect of the cable with and without the coating on the electrical usage of four electrical circuits is tested.

[0041] The first and second circuits use alternative current sources of 240V, 50Hz, single phase. For the first circuit, the voltage supplied to the circuit is maintained at 5V, while for the second circuit, the current is maintained at 4.0A. Two cables of length 30cm, one coated and the other uncoated, are connected in parallel for the first circuit and in series for the second circuit. Ammeters and voltmeters are connected to measure the current and voltage drop across the cables.

[0042] The current and voltage across the cables in the first and second circuits over time are shown in Table 4.

[0043] [Table 4]

[0044] In the first circuit, the coated cable will have a higher current at a constant voltage. In the second circuit, the coated cable will have a lower voltage drop at a constant current. The effect shown in both circuits is that the electrical resistivity of the coated cable will be reduced.

[0045] In the third and fourth circuits, a 30V DC power supply is used. For the fourth circuit, the current is maintained at 3.0A. Similarly, two cables of 30cm length, one coated and one uncoated, are connected in parallel in the third circuit and in series in the fourth circuit. Ammeters and voltmeters are connected to measure the current and voltage drop across the cables.

[0046] The current and voltage over time across the cables in the third and fourth circuits are shown in Tables 5 and 6, respectively.

[0047] [Table 5]

[0048] [Table 6]

[0049] In the third circuit, the coated cable will have a higher current at a constant voltage. In the fourth circuit, the coated cable will have a lower voltage drop at a constant current. The effect shown in both circuits is that the electrical resistivity of the coated cable will be reduced.

[0050] The present disclosure includes what is contained in the appended claims and the above description. While the present invention has been particularly described in certain preferred forms thereof, it will be understood that the present disclosure of the preferred forms is given by way of example only, and that numerous changes in the details of construction and in the combination and arrangement of parts may be made without departing from the scope of the invention.

Claims

1. 1. A method for reducing energy loss from an electromechanical device, comprising: preparing a coating composition comprising a nano-sized particulate metal oxide, a binder and a liquid carrier; bombarding the composition with a vibrational force at a frequency of 20-500 kHz for at least 24 hours to produce energetic excited states in the atoms of the composition; coating a surface of the device or a casing surrounding the device with the composition; The method includes:

2. The method of claim 1 , wherein the electromechanical device is an electrical switchboard, a cable, a surface of a termination box, or a surface of a junction box.

3. 3. The method of claim 1 or 2, wherein the metal oxide is an oxide of aluminum, iron, magnesium, lithium, potassium, copper, tourmaline or a mixture thereof.

4. The method according to any one of claims 1 to 3, wherein the binder is an acrylic polymer.

5. The method according to any one of claims 1 to 4, wherein the liquid carrier is water.

6. The method of claim 5 , wherein the water is reverse osmosis water or purified water.

7. The method of any one of claims 1 to 6, wherein the composition comprises 0.1 to 30 parts by weight of a metal oxide, 0.1 to 10 parts by weight of a binder, and 50 to 90 parts by weight of a liquid carrier.

8. The method according to any one of claims 1 to 7, wherein the coating has a thickness of at least 100 μm.

Citation Information

Patent Citations

  • Composite coating for groundwall insulation, method of manufacture thereof and article derived therefrom

    JP2007181814A

  • A method of optimising energy usage

    WO2016186570A1