Azeotrope and azeotrope-like compositions of perfluoroheptenes and fluoroethers and uses thereof

Azeotropic compositions of perfluoroheptene and fluorinated ethers address the flammability and fractionation issues of existing solvents, offering effective and safe cleaning for microelectronic components by maintaining consistent solvent properties.

JP2024543899APending Publication Date: 2024-11-26THE CHEMOURS CO FC LLC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024531111
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-23
Filing Date
2022-11-22
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Existing cleaning solvents for microelectronic components are flammable, toxic, and fractionate during use, leading to performance issues and environmental concerns, while alternative solvents like hydrofluorocarbons have limited solubility and require surfactants for effective use.

Method used

Development of azeotropic and azeotrope-like compositions of perfluoroheptene and fluorinated ethers, which are non-flammable, maintain consistent composition, and effectively remove flux residues and oils without damaging substrates, and can be reused without fractionation.

Benefits of technology

The compositions provide effective, safe, and reusable cleaning solutions for microelectronic components, ensuring consistent performance and environmental safety by maintaining solvent properties throughout use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543899000009
    Figure 2024543899000009
  • Figure 2024543899000010
    Figure 2024543899000010
  • Figure 2024543899000011
    Figure 2024543899000011
Patent Text Reader

Abstract

The present disclosure provides azeotropic and azeotrope-like compositions that are composed of perfluoroheptene and some fluoroethers. The present disclosure also provides methods of using the azeotropic and azeotrope-like compositions. Methods of use include removing residue from the surface of an object, depositing lubricants on the surface of an object, such as a magnetic media device, and cooling electronic components, comprising at least partially immersing the electrical component in a working fluid and transferring heat from the electrical component.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure is in the field of perfluoroheptene compositions that are azeotropic or azeotrope-like and are useful in cleaning applications as flux removers and for removing oil or residue from surfaces. [Background technology]

[0002] Flux residues are always present on microelectronic components assembled using rosin flux. As modern electronic circuit boards evolve toward increased circuit and component density, thorough board cleaning after soldering becomes a critical processing step. After soldering, the flux residues are often removed with organic solvents. The flux removal solvent should be non-flammable, low toxicity, and have high solvent power so that the flux and flux residues can be removed without damaging the substrate being cleaned. For proper operation in use, microelectronic components must be cleaned of flux residues, oils and greases, and particulates that may contaminate the surface after fabrication is complete.

[0003] In cleaning equipment, including vapor degreasing and vapor flux removal equipment, compositions may be lost during operation through leaks in shaft seals, hose connections, soldered joints, and broken lines. In addition, during maintenance procedures on the equipment, working compositions may be released into the atmosphere. If the composition is not a pure component, it may change when leaked or released from the equipment into the atmosphere, which may cause the composition remaining in the equipment to exhibit unacceptable performance. Therefore, it is desirable to use a composition that includes a single unsaturated fluorinated ether as a cleaning composition.

[0004] Since the elimination of nearly all previous chlorofluorocarbons (CFCs) and hydrochlorofluorocarbons (HCFCs) as a result of the Montreal Protocol, alternative non-ozone depleting solvents have become available. Although boiling point, flammability, and solvent strength properties can often be adjusted by preparing solvent mixtures, these mixtures are often unsatisfactory because they fractionate to an undesirable extent during use. Such solvent mixtures also fractionate during solvent distillation, which makes it virtually impossible to recover the solvent mixture of the original composition.

[0005] Many industries use aqueous compositions for the surface treatment of metals, ceramics, glass, and plastics. Cleaning, plating, and deposition of coatings are often carried out in aqueous media and are usually followed by a step in which residual water is removed. Methods used to remove such residual water include hot air drying, centrifugal drying, and solvent-based water displacement.

[0006] There is a need in the industry for improved methods for the deposition of fluorolubricants. The use of certain solvents, such as CFC-113 and PFC-5060, has been regulated due to their impact on the environment. Hydrofluorocarbons (HFCs) have been proposed as replacements for previously used CFC solvents in drying or dehydrating applications, but many HFCs have limited solubility in water. Thus, the use of surfactants to facilitate the removal of water from the substrate is necessary in many drying or dehydrating methods. Hydrophobic surfactants have been added to dehydrating or drying solvents to displace water from the substrate.

[0007] The main function of the dehydrating or drying solvent (unsaturated fluorinated ether solvent) in the dehydrating or drying composition is to reduce the amount of water on the surface of the substrate being dried. The main function of the surfactant is to displace the remaining water from the surface of the substrate. When the unsaturated fluorinated ether solvent is combined with the surfactant, a highly effective displaced drying composition is obtained.

[0008] Solvents used for this purpose must dissolve the fluorolubricant and form a substantially uniform or homogeneous coating of the fluorolubricant. Additionally, existing solvents have been found to require higher fluorolubricant concentrations to produce a given thickness coating, resulting in irregularities in the uniformity of the fluorolubricant coating.

[0009] The most advanced, highest density and lowest cost method of storing digital information involves writing and reading magnetic flux patterns from a rotating disk coated with a magnetic material. The magnetic layer, on which information in the form of bits is stored, is sputtered onto a metal support structure. An overcoat, usually a carbon-based material, is then placed over the magnetic layer for protection, and finally a lubricant is applied to the overcoat. A read-write head flies above the lubricant, and information is exchanged between the head and the magnetic layer. The distance between the read-write head and the magnetic layer is less than 100 angstroms.

[0010] Naturally, during normal disk drive applications, there will be contact between the head and the disk surface. The disk is lubricated to reduce wear due to sliding and flying contact. Fluorine-based lubricants are used as lubricants to reduce friction between the head and disk, thereby reducing wear and minimizing the possibility of disk failure.

[0011] Azeotropic solvent mixtures can have the properties necessary for flux removal, degreasing applications, and other cleaning needs. Azeotropic mixtures exhibit either a maximum or minimum boiling point and do not fractionate upon boiling. The inherent invariance of the composition under boiling conditions ensures that the ratio of the individual components of the mixture does not change during use, and the solubility properties remain constant as well. Summary of the Invention [Problem to be solved by the invention]

[0012] The present disclosure provides azeotropic or azeotrope-like compositions that are useful in semiconductor chip and circuit board cleaning, defluxing, and degreasing processes. The compositions of the present invention are non-flammable and do not fractionate, so they do not produce flammable compositions during use. In addition, used azeotropic solvent mixtures can be redistilled and reused without changing the composition.

[0013] Other application opportunities for these newly proposed working fluids exist in cooling of power electronics (TVs, mobile phones, monitors, drones, etc.), battery thermal management (automotive and stationary), e-powertrains, IGBTs, computer server systems, 5G networks, displays. The working fluid provides a medium for transporting heat or in passive evaporative cooling such as heat pipes. Important factors to consider for compatible use of these fluids include dielectric constant, dissipation factor or loss tangent, volume resistivity, dielectric strength, and non-flammability. These factors provide an envelope that must exist such that a fluid in direct contact with an electrified system is a non-conductive fluid. The molecule should also have structural characteristics, i.e., double bonds, that make it non-flammable, low GWP, and short atmospheric lifetime. Several novel fluid mixtures described below have been identified by the inventors that meet all of these requirements and meet the needs identified for this market.

[0014] Applications that can employ this solution include cooling electronic devices-data center servers, insulated-gate bipolar transistor (IGBT) devices, telecommunications infrastructure, military electronics, television (TV), cell phones, monitors, drones, automotive batteries, power trains for electric vehicles (EV), power electronics, avionics devices, power devices, and displays. In some applications, such as batteries, these working fluids may temporarily act as heating fluids, for example during cold weather start-up. The technical objective of the present invention is to provide novel specialty fluids for thermal management with a boiling point range close to ambient temperature and slightly higher, and these products are environmentally friendly (low GWP and ODP), non-flammable, non-conductive, and have sufficient heat transfer properties. [Means for solving the problem]

[0015] The present disclosure provides an azeotrope or azeotrope-like composition comprising perfluoroheptene and an effective amount of a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether (HFE-347pcF), nonafluorobutyl methyl ether (HFE-7100), and nonafluorobutyl ethyl ether (HFE-7200) to form an azeotrope composition.

[0016] The present disclosure further provides a method of removing residue from a surface of an article, the method comprising: (a) contacting the article with an azeotrope or azeotrope-like composition of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether; and (b) recovering the surface from the composition.

[0017] The present disclosure also provides a method of depositing a fluorolubricant on a surface of an article, the method comprising: (a) combining a fluorolubricant with a solvent, thereby forming a mixture, the solvent comprising an azeotropic or azeotrope-like composition of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether; (b) contacting the mixture with the surface of the article; and (c) evaporating the solvent from the surface of the article to form a fluorolubricant coating on the surface.

[0018] The present disclosure also provides an immersion cooling unit including an immersion cell defining an internal cavity. An electronic or electrical component is disposed within the internal cavity. A dielectric working fluid partially fills the internal cavity and at least partially immerses an energy storage device, IT equipment, computer server, or the like. The dielectric working fluid includes at least one of an azeotrope or azeotrope-like composition including perfluoroheptene and an effective amount of a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether (HFE-347pcF), nonafluorobutyl methyl ether (HFE-7100), and nonafluorobutyl ethyl ether (HFE-7200).

[0019] The present disclosure also provides a method for cooling electrically charged equipment, such as, but not limited to, energy storage devices (e.g., batteries), IT equipment, data centers, and computer servers, including those used in cryptocurrency mining applications, comprising at least partially immersing an electrical component in a working fluid and transferring heat from the electrical component using the working fluid, the working fluid comprising at least one of an azeotrope or azeotrope-like composition comprising perfluoroheptene and an effective amount of a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether (HFE-347pcF), nonafluorobutyl methyl ether (HFE-7100), and nonafluorobutyl ethyl ether (HFE-7200). [Brief description of the drawings]

[0020] To improve the understanding of the concepts presented herein, embodiments are illustrated in the accompanying drawings. [Figure 1] 1 is a graph showing the vapor-liquid equilibrium curve for a mixture of perfluoroheptene and HFE-347pcF. [Diagram 2] 1 is a graph showing the vapor-liquid equilibrium curve for a mixture of perfluoroheptene and HFE-7100. [Diagram 3] 1 is a graph showing the vapor-liquid equilibrium curve for a mixture of perfluoroheptene and HFE-7200. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] As used herein, the terms "comprises," "comprising," "includes," "including," "has," "having," or any other variation thereof, are intended to cover non-exclusive inclusions. For example, a process, method, article, or apparatus that includes a list of elements is not necessarily limited to only those elements, but may include other elements not expressly listed or inherent to such process, method, article, or apparatus. Furthermore, unless expressly stated to the contrary, "or" refers to an inclusive "or" and not an exclusive "or." For example, a condition A or B is satisfied by any one of the following: A is true (or present) and B is false (or absent), A is false (or absent) and B is true (or present), and both A and B are true (or present).

[0022] Additionally, the use of "a" or "an" is used to describe elements and components described herein. This is done merely for convenience and to give a general sense of the scope of the invention. This description should be interpreted to include one or at least one, and the singular also includes the plural unless it is clear that a different meaning is intended.

[0023] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this invention belongs. Although methods and materials similar or equivalent to those described herein can be used in the practice or testing of the embodiments of the present disclosure, suitable methods and materials are described below. All publications, patent applications, patents, and other references mentioned herein are incorporated by reference in their entirety, unless a specific passage is cited. In case of conflict, the present specification, including definitions, will take precedence. Furthermore, the materials, methods, and examples are merely illustrative and are not intended to be limiting.

[0024] Numerous aspects and embodiments have been described above, which are merely illustrative and not limiting, and after reading this specification, skilled artisans will appreciate that other aspects and embodiments are possible without departing from the scope of the invention.

[0025] Described herein are azeotropic and azeotrope-like compositions of perfluoroheptenes and fluorinated ethers, as described below. Also described herein are novel methods of using azeotropic or azeotrope-like compositions comprising perfluoroheptenes and fluorinated ethers.

[0026] In some embodiments, the perfluoroheptene comprises a mixture of perfluorohept-3-ene (PFO-161-14mcyy) and perfluorohept-2-ene (PFO-161-14myy). In some embodiments, the perfluoroheptene comprises about 85 to about 95% by weight perfluorohept-3-ene and about 5 to about 15% by weight perfluorohept-2-ene. In some embodiments, the perfluoroheptene comprises about 90% by weight perfluorohept-3-ene and about 10% by weight perfluorohept-2-ene. The nonafluorobutyl methyl ether comprises a mixture of nonafluoro-n-butyl methyl ether and nonafluoro-sec-butyl ethyl ether. The nonafluorobutyl ethyl ether comprises a mixture of nonafluoro-n-butyl ethyl ether and nonafluoro-sec-butyl ethyl ether. Nonafluorobutyl methyl ether and nonafluorobutyl ethyl ether are available from 3M Corporation as Novec 7100 and Novec 7200, respectively.

[0027] As used herein, an azeotropic composition is a constant boiling liquid mixture of two or more substances that distills without substantial change in composition and behaves as a constant boiling composition. A constant boiling composition characterized as azeotropic exhibits either a maximum or minimum boiling point compared to a non-azeotropic mixture of the same substances. In one embodiment, an azeotropic composition is a specific composition of two or more substances that exhibits a constant minimum or maximum temperature. In another embodiment, an azeotropic composition is a mixture of two or more substances that exhibits a constant minimum or maximum temperature over a range of compositions. Azeotropic compositions include homogeneous azeotropes, which are liquid mixtures of two or more substances that behave as a single substance in that the vapor produced by partial evaporation or distillation of the liquid has the same composition as the liquid. Azeotropic compositions, as used herein, also include heterogeneous azeotropes, where the liquid phase separates into two or more liquid phases. In these embodiments, at the azeotropic point, the vapor phase is in equilibrium with two liquid phases, with all three phases having different compositions. If the two equilibrium liquid phases of a heterogeneous azeotrope are combined and the composition of the total liquid phase is calculated, it will be identical to the composition of the vapor phase.

[0028] As used herein, the term "azeotrope-like composition", sometimes also referred to as "near azeotrope composition", refers to a constant boiling or substantially constant boiling liquid mixture of two or more substances that behaves as a single substance. One way to characterize an azeotrope-like composition is that the vapor generated by partial evaporation or distillation of a liquid has substantially the same composition as the liquid that was evaporated or distilled. That is, the mixture distills or refluxes with substantially no change in composition. Alternatively, an azeotrope-like composition may be characterized as a composition that has a boiling point temperature lower than the boiling points of each of the pure components.

[0029] Yet another way to characterize an azeotrope-like composition is that the bubble point pressure of the composition and the dew point vapor pressure of the composition at a particular temperature are substantially the same. Azeotrope-like compositions exhibit dew point pressures and bubble point pressures with substantially no pressure difference. Thus, the difference between the dew point pressure and the bubble point pressure at a given temperature will be a small value. It can be stated that a composition that has a difference between the dew point pressure and the bubble point pressure of 3 percent or less (based on the bubble point pressure) can be considered to be azeotrope-like.

[0030] In another embodiment, an azeotrope-like composition exhibits a boiling vapor at a temperature within 0.1° C. of the minimum or maximum boiling point of the azeotrope composition. In another embodiment, an azeotrope-like composition exhibits a boiling vapor at a temperature within 0.5° C. of the minimum or maximum boiling point of the azeotrope composition. In yet another embodiment, an azeotrope-like composition exhibits a boiling vapor at a temperature within 1.0° C. of the minimum or maximum boiling point of the azeotrope composition.

[0031] The composition of one embodiment of the present invention comprises perfluoroheptene and an effective amount of a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether (HFE-347pcF), nonafluorobutyl methyl ether (HFE-7100), and nonafluorobutyl ethyl ether (HFE-7200) to form an azeotropic composition, where "effective amount" is defined as an amount that, when combined with perfluoroheptene, results in the formation of an azeotrope or near-azeotrope.

[0032] Compositions may be formed that include azeotropic or azeotrope-like combinations of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether (HFE-347pcF), nonafluorobutyl methyl ether (HFE-7100), and nonafluorobutyl ethyl ether (HFE-7200). In one embodiment, these include compositions that include perfluoroheptene and 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether. In another embodiment, these include compositions that include perfluoroheptene and nonafluorobutyl methyl ether. In yet another embodiment, these include compositions that include perfluoroheptene and nonafluorobutyl ethyl ether.

[0033] In one embodiment, the azeotropic composition contains 31.7 to 47.8 weight percent perfluoroheptene and 52.2 to 68.3 weight percent HFE-347pcF. In another embodiment, the azeotropic composition contains 0.9 to 10.1 weight percent perfluoroheptene and 89.9 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotropic composition contains 79.5 to 84.8 weight percent perfluoroheptene and 15.2 to 20.5 weight percent HFE-7200.

[0034] In one embodiment, the azeotropic composition consists essentially of 31.7 to 47.8 weight percent perfluoroheptene and 52.2 to 68.3 weight percent HFE-347pcF. In another embodiment, the azeotropic composition consists essentially of 0.9 to 10.1 weight percent perfluoroheptene and 89.9 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotropic composition consists essentially of 79.5 to 84.8 weight percent perfluoroheptene and 15.2 to 20.5 weight percent HFE-7200.

[0035] In one embodiment, the azeotropic composition comprises 31.7 to 47.8 weight percent perfluoroheptene and 52.2 to 68.3 weight percent HFE-347pcF. In another embodiment, the azeotropic composition comprises 0.9 to 10.1 weight percent perfluoroheptene and 89.9 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotropic composition comprises 79.5 to 84.8 weight percent perfluoroheptene and 15.2 to 20.5 weight percent HFE-7200.

[0036] In another embodiment, the azeotrope-like composition contains 24 to 52 weight percent perfluoroheptene and 48 to 76 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition contains 0.9 to 14 weight percent perfluoroheptene and 86 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition contains 74.3 to 89.5 weight percent perfluoroheptene and 10.5 to 25.7 weight percent HFE-7200.

[0037] In another embodiment, the azeotrope-like composition consists essentially of 24 to 52 weight percent perfluoroheptene and 48 to 76 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition consists essentially of 0.9 to 14 weight percent perfluoroheptene and 86 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition consists essentially of 74.3 to 89.5 weight percent perfluoroheptene and 10.5 to 25.7 weight percent HFE-7200.

[0038] In another embodiment, the azeotrope-like composition comprises 24 to 52 weight percent perfluoroheptene and 48 to 76 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition comprises 0.9 to 14 weight percent perfluoroheptene and 86 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition comprises 74.3 to 89.5 weight percent perfluoroheptene and 10.5 to 25.7 weight percent HFE-7200.

[0039] In another embodiment, the azeotrope-like composition contains 16.8 to 56 weight percent perfluoroheptene and 44 to 83.2 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition contains 0.9 to 27.3 weight percent perfluoroheptene and 72.7 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition contains 67.8 to 93.4 weight percent perfluoroheptene and 6.6 to 32.2 weight percent HFE-7200.

[0040] In another embodiment, the azeotrope-like composition consists essentially of 16.8 to 56 weight percent perfluoroheptene and 44 to 83.2 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition consists essentially of 0.9 to 27.3 weight percent perfluoroheptene and 72.7 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition consists essentially of 67.8 to 93.4 weight percent perfluoroheptene and 6.6 to 32.2 weight percent HFE-7200.

[0041] In another embodiment, the azeotrope-like composition comprises 16.8 to 56 weight percent perfluoroheptene and 44 to 83.2 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition comprises 0.9 to 27.3 weight percent perfluoroheptene and 72.7 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition comprises 67.8 to 93.4 weight percent perfluoroheptene and 6.6 to 32.2 weight percent HFE-7200.

[0042] In another embodiment, the azeotrope-like composition includes 6.1 to 61.1 weight percent perfluoroheptene and 38.9 to 93.9 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition includes 0.9 to 40.3 weight percent perfluoroheptene and 59.7 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition includes 61.3 to 99.7 weight percent perfluoroheptene and 0.3 to 38.7 weight percent HFE-7200.

[0043] In another embodiment, the azeotrope-like composition consists essentially of 6.1 to 61.1 weight percent perfluoroheptene and 38.9 to 93.9 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition consists essentially of 0.9 to 40.3 weight percent perfluoroheptene and 59.7 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition consists essentially of 61.3 to 99.7 weight percent perfluoroheptene and 0.3 to 38.7 weight percent HFE-7200.

[0044] In another embodiment, the azeotrope-like composition comprises 6.1 to 61.1 weight percent perfluoroheptene and 38.9 to 93.9 weight percent HFE-347pcF. In another embodiment, the azeotrope-like composition comprises 0.9 to 40.3 weight percent perfluoroheptene and 59.7 to 99.1 weight percent HFE-7100. In yet another embodiment, the azeotrope-like composition comprises 61.3 to 99.7 weight percent perfluoroheptene and 0.3 to 38.7 weight percent HFE-7200.

[0045] In some embodiments, the compositions of the present application further comprise a stabilizer that reduces decomposition over time and at elevated temperatures.

[0046] The present application provides a composition comprising a perfluoroheptene azeotropic composition and an additional component selected from the group consisting of one or more antioxidants and one or more acid scavengers, or any mixture thereof.

[0047] In some embodiments, the one or more acidic antioxidants are selected from butylated hydroxytoluene (BHT), hydroquinone monomethyl ether (HQMME), 2-tert-butyl-6-methylphenol, 2-tert-butyl-5-methylphenol, and 2-tert-butyl-4-ethylphenol. In some embodiments, the one or more scavengers are selected from 1,3-dioxolane, 1,2-epoxybutane, and nitromethane.

[0048] Large-scale computer server systems can perform significant workloads and generate large amounts of heat during their operation. The majority of the heat is generated from their operation. Due in part to the amount of heat generated, these systems are typically mounted in a stacked configuration with large internal cooling fans and heat dissipating fins. As the size and density of these systems increase, the thermal challenges become even greater, eventually exceeding the capabilities of forced air systems.

[0049] Two-phase immersion cooling is an emerging cooling technology for the high-performance cooling market, such as those applied in high-performance high power density server systems, IT equipment used in data centers, and cryptocurrency mining facilities. It relies on heat absorbed in the process of evaporating the immersion liquid into a gas. The fluid used in this application must meet certain requirements to be viable during use. For example, the boiling point of the fluid should be in the range of 30-75°C. In general, this range accommodates maintaining a sufficiently cool temperature for the server components while allowing the generated heat to be sufficiently dissipated to an external heat sink. Alternatively, the operating temperature of the server and immersion cooling systems can be increased or decreased by using a closed system and increasing or decreasing the pressure within the system to increase or decrease the boiling point of a given fluid.

[0050] Single-phase immersion cooling has a long history in cooling computer servers. There is no phase change in single-phase immersion cooling. Instead, the liquid warms as it circulates through the computer server or heat generating device, and is then pumped through a heat exchanger for cooling before returning to the server or heat generating device, thus carrying heat away from these components. Fluids used in single-phase immersion cooling have the same requirements as in two-phase immersion cooling, except that their boiling points are typically higher than 30-75 °C to reduce evaporative losses.

[0051] An immersion cooler is provided that has an operating temperature range close to ambient temperature. Embodiments of the present disclosure provide an immersion cooler with a fluid for temperature management that is environmentally friendly (i.e., has a low global warming potential (GWP) and a low ozone depletion potential (ODP)) compared to, for example, concepts that do not include one or more of the features disclosed herein.

[0052] Also provided is a method of immersion cooling, where the device is a heat generating component, comprising at least partially immersing the heat generating component in a liquid state of the immersion cooling fluid and using the immersion cooling fluid to transfer heat from the heat generating component. Such devices include bulk energy storage devices, electrical components, IT equipment, computer servers, mechanical components, and optical components. Examples of devices of the present disclosure include, but are not limited to, microprocessors, wafers used to manufacture semiconductor devices, power control semiconductors, power distribution switchgear, power transformers, circuit boards, multi-chip modules, packaged and unpackaged semiconductor devices, lasers, fuel cells, electrochemical cells, and energy storage devices such as batteries. In some embodiments, the device may include a cooling device, a heating device, or a combination thereof.

[0053] In certain embodiments, the device may include an electronic device such as a processor, including a microprocessor. Microprocessors typically have a maximum operating temperature of about 85° C., so effective heat transfer is required under conditions of high throughput, i.e., high heat rejection rates. In other embodiments, the device may include an energy storage system, such as a battery. When rapidly charged or discharged, a battery may reject a significant amount of heat that must be effectively removed to avoid overheating, internal damage, thermal runaway to adjacent batteries, and potential fire. As these electronic and electrical devices become denser and more powerful, the amount of heat generated per unit time and unit volume increases. Thus, the mechanism of heat transfer plays a significant role in processor performance. Heat transfer fluids typically have good heat transfer performance, good electrical compatibility (even when used in “indirect contact” applications such as those employing cold plates), as well as low toxicity, low or non-flammability, and low environmental impact. Good electrical compatibility suggests that the heat transfer fluid candidate exhibits high dielectric strength, high volume resistivity, low dissipation factor, low dielectric constant, and low solvency for polar materials. Additionally, the heat transfer fluid should exhibit good material compatibility, i.e., should not adversely affect typical materials of construction.

[0054] Perfluorinated fluids such as Fluoroinert FC-72 and FC-3284 have a dielectric constant of less than 2.0, 10 15 It is generally understood that these fluids can exhibit excellent dielectric properties, such as high volume resistivity on the order of ohm-cm, and high dielectric strength. However, these fluids are also generally associated with high GWPs that are well outside the current requirements for many industrial applications. The GWP of Fluorinert FC-72 has been reported to be >9000. Hydrofluoroethers (HFEs) have lower GWPs, but are still unsatisfactory and typically have poorer dielectric properties compared to FC-72 and FC-3284. For example, Novec 7100 has a GWP of 297. Thus, there is a continuing need for immersion cooling working fluids that meet industrial dielectric applications while having a GWP at least as low as current HFEs. In another embodiment, the GWP of the working fluid is less than 100. In another embodiment, the disclosed compositions have a global warming potential (GWP) of 50 or less. As used herein, "GWP" is measured relative to the GWP of carbon dioxide, as defined in AR4 of the IPCC (Intergovernmental Panel on Climate Change), and is measured over a 100-year time horizon.

[0055] Because the new fluids have similar or superior heat transfer properties, including electrical surface-to-fluid thermal resistance, critical heat flux, and fluid-to-condenser thermal resistance, compared to existing fluids of higher GWP such as FC-72, FC-3284, HFE-7100, and HFE-7200, it is highly desirable to be able to substitute these fluids in existing systems without significant loss of thermal performance or mechanical modifications, and in new systems designed for FC-72, FC-3284, HFE-7100, and HFE-7200 without significant mechanical design changes. The practice of substituting a new fluid for an existing fluid in an existing system is often referred to as "retrofitting."

[0056] It is also desirable that because these fluids have similar normal boiling points compared to high GWP fluids such as FC-72, FC-3284, HFE-7100, and HFE-7200, they can be used to replace them in existing systems without significant mechanical or operational modifications, and in new systems without significant mechanical design changes.

[0057] It is also highly desirable that the new fluids provide at least the minimum dielectric properties required by the application, or even better dielectric properties, as compared to existing fluids such as FC-72, FC-3284, HFE-7100, and HFE-7200, and thus be able to replace these fluids in existing systems without significant electrical or mechanical modifications, and in new systems designed for FC-72, FC-3284, HFE-7100, and HFE-7200 without significant electrical or mechanical design changes. Desirable dielectric properties include high volume resistivity, low dielectric constant, high dielectric strength, and low loss tangent.

[0058] Suitable compounds and compositions useful alone or in combination as dielectric working fluids are shown in Table 1.

[0059] [Table 1]

[0060] In one embodiment, the working fluid may be selected from the group of azeotropic and azeotrope-like compositions listed in Table 1.

[0061] It can be seen that the proposed perfluoroheptene-based blend has superior dielectric properties in terms of lower dielectric constant and higher volume resistivity compared to HFE-7100 and HFE-7200. The perfluoroheptene-based blend also has a significantly lower GWP, at least about 95% lower than FC-72 and FC-3284.

[0062] An embodiment of an immersion cooling unit 100 is shown in FIG. The immersion cooling system 100 includes an immersion cell 110 that defines an internal cavity 120. A heat-generating charged component (e.g., an energy storage device) 130 to be cooled may be disposed within the internal cavity 120. A dielectric working fluid 140 partially fills the internal cavity 120. The dielectric working fluid 140 at least partially immerses the energy storage device 130. In some embodiments, the dielectric working fluid 140 substantially immerses the energy storage device 130. In one embodiment, the dielectric working fluid 140 completely immerses the energy storage device 130. A condensation coil 150 is additionally present within the internal cavity 120. The condensation coil 150 may be spatially located above at least a portion of the dielectric working fluid 140.

[0063] During operation, heat generated by the electrical components 130 heats the dielectric working fluid 140, vaporizing a portion of the dielectric working fluid 140. The vapor of the dielectric working fluid 140 contacts the condensing coil 150 above the dielectric working fluid 140, transferring thermal energy to the condensing coil 150 and allowing the condensed dielectric working fluid 140 to fall back into the liquid dielectric working fluid 140 below. The thermal energy transferred to the condensing coil 150 is transported outside the submerged cell 110 and released into the environment or to a cooling device via the heat exchanger 160. The released thermal energy can also be recovered and used for heating applications or for energy generation, such as a Rankine cycle.

[0064] The dielectric working fluid of the immersion cooler 100 is selected to undergo a phase transition from a liquid to a gaseous state over the operating temperature range of the immersion cooler 100. In some embodiments, the composition of the dielectric working fluid 140 includes one or more fluorinated compounds. In some embodiments, the dielectric working fluid 140 includes one or more compounds that include fluorine. In some embodiments, the operating temperature is at least 25° C., at least 30° C., at least 40° C., at least 50° C., at least 60° C., less than 100° C., less than 90° C., less than 80° C., less than 70° C., less than 60° C., and combinations thereof.

[0065] In one embodiment, the normal boiling point of the new low GWP dielectric fluid may be within at least 10° C. of the fluid being replaced. In another embodiment, the normal boiling point of the new low GWP dielectric fluid may be within 8° C. In yet another embodiment, the normal boiling point of the new low GWP dielectric fluid may be within 5° C.

[0066] The dielectric working fluid 140 may also be selected to exhibit a suitable dielectric constant, volume resistivity, dielectric strength, and loss tangent (dissipation factor) for direct contact with electrical components. In general, materials exhibiting a low dielectric constant, low loss tangent or dissipation factor, high volume resistivity, and high dielectric strength provide increased electrical insulation of the energy storage device or charging component 130 immersed therein, as well as reduced signal loss. In some embodiments, the dielectric constant of the dielectric working fluid 140 is less than about 8 over the operating frequency range (possibly up to 100 GHz), preferably less than HFE-7100 and HFE-7200. Suitable dielectric working fluids include compounds and mixtures having a dielectric constant less than 7.3, or less than 5.5, or less than 5.0, or less than 4.0, or less than 3.5, or less than 2.7 over the operating frequency range (up to about 100 GHz). Other embodiments include compounds and mixtures thereof having a dielectric constant greater than 1.0 and less than 8.0, greater than 2.0 and less than 7.3, greater than 2.5 and less than 5.5, or greater than 3.5 and less than 5.0.

[0067] In one embodiment, the dielectric constant of the new low GWP fluids is at least about 15% lower than HFE-7100 or HFE-7200. In another embodiment, the dielectric constant of the new low GWP fluids is at least about 25% lower than HFE-7100 or HFE-7200. In another embodiment, the dielectric constant of the new low GWP fluids is at least about 35% lower than HFE-7100 or HFE-7200. In another embodiment, the dielectric constant of the new low GWP fluids is at least about 50% lower than HFE-7100 or HFE-7200, even at frequencies up to about 60 GHz or as high as 100 GHz.

[0068] Another characteristic of a good working fluid is that it possesses a high volume resistivity. Volume resistivity is an intrinsic property that measures how strongly a material resists electrical current per unit length of unit cross section, and is typically expressed in units of ohm-cm or ohm-m. A higher volume resistivity means that the material is a better electrical insulator. The electrical resistance of a material can be calculated by multiplying the volume resistivity by the length and dividing by the cross-sectional area of ​​the material.

[0069] Thus, a dielectric fluid with a higher volume resistivity is desirable because it leads to higher electrical resistance and, as a result, lower current leakage. For example, current leakage can lead to self-discharge of energy storage devices such as batteries. This also means that for a given minimum resistance requirement, electrical components with different voltages can be placed closer together (smaller "L"), potentially leading to a more compact assembly. In one embodiment, an effective working fluid has a volume resistivity of at least 1×10 measured at 25° C. 10 In another embodiment, the effective working fluid has a volume resistivity of at least 1×10 11 In another embodiment, the effective working fluid has a volume resistivity of at least 1×10 12 It has a volume resistivity of ohm-cm. Water is known to have a very low volume resistivity. Therefore, a fluid with a high volume resistivity is also desirable, since it still maintains a sufficient level of actual volume resistivity when water is present in the fluid.

[0070] In one embodiment, the volume resistivity of the new low GWP fluid is about 1.0×10 11 In another embodiment, the volume resistivity is at least about one order of magnitude higher than HFE-7100 and 7200. In another embodiment, the volume resistivity is at least about two orders of magnitude higher than HFE-7100 and 7200. In another embodiment, the volume resistivity is at least about three orders of magnitude higher than HFE-7100 and 7200. In another embodiment, the volume resistivity is at least about four orders of magnitude higher than HFE-7100 and 7200.

[0071] Another important dielectric fluid property is the dielectric strength, defined as the maximum electric field or voltage per unit length that a material can withstand without undergoing electrical breakdown and becoming conductive. This is typically measured in units of kV / mm or kV / 0.1" gap. For a given distance or "gap", the voltage at which the material becomes conductive is called the breakdown voltage. A material with a higher dielectric strength is advantageous because it allows for a higher voltage between two conductors or allows the two conductors to be placed closer together, potentially leading to a more compact assembly. In one embodiment, the dielectric strength is greater than about 10 kV / 0.1" gap. In another embodiment, the dielectric strength is greater than about 20 kV / 0.1" gap. In yet another embodiment, the dielectric strength is greater than about 30 kV / 0.1" gap. In yet another embodiment, the dielectric strength is greater than about 35 kV / 0.1" gap.

[0072] The dielectric loss tangent, sometimes called the dissipation factor, is another important dielectric property, especially at high frequencies, due to its effect on signal attenuation or loss. It is defined as tan(δ), the ratio of the relative real to imaginary components of the dielectric constant. It is also a measure of the rate at which the energy carried by an electromagnetic field (RF) traveling through a dielectric is absorbed by that dielectric, i.e., it quantifies the dissipation of electromagnetic energy in the form of heat. Furthermore, the loss tangent is highly frequency dependent, and can increase especially above frequencies of 1 GHz, which may be found in applications such as data centers, 5G, and Wi-fi technologies. More importantly, the signal loss or attenuation per unit length, typically measured in dB / cm, is proportional to the loss tangent. In other words, for a signal traveling through a dielectric fluid, the higher the loss tangent of the fluid, the higher the signal loss per unit length, and consequently the shorter the distance it can travel. It is therefore highly desirable for a dielectric fluid to have low loss tangent values ​​at frequencies above 1 GHz and up to about 100 GHz. The fluids discovered by the present inventors exhibit highly beneficial values ​​of loss tangent at high frequencies.

[0073] The inventors have also discovered that the newly proposed low GWP fluids have comparable and sometimes lower values ​​of loss tangent compared to fluids such as HFE-7100 and HFE-7200, especially at high frequencies.

[0074] All the desirable dielectric properties mentioned above, high dielectric strength, low dielectric constant, low loss tangent, and high volume resistivity, must be present primarily in the liquid phase, but also in the gas phase.

[0075] Another desirable feature of the submersion cooling fluid relates to its ability to not significantly damage or react with materials of construction of IT and computer components such as cables, wires, seals, metals, and tanks exposed to the dielectric fluid, among other components.

[0076] It is also desirable that these fluids have similar interactions with electronic components compared to existing fluids so as to minimize part replacement.

[0077] Contamination control measures, such as filter systems, may be used to remove solid or liquid residues that may be generated as a result of reactivity with the materials of construction. Contamination control measures may also be used to maintain sufficiently low acid and water levels.

[0078] Typical non-condensable gases such as nitrogen and oxygen may also be present in the dielectric fluid and may be detrimental to boiling and condensation heat transfer. Therefore, systems having a dielectric two-phase fluid may be equipped with auxiliary devices that at least partially remove or control the level of non-condensables in the dielectric fluid.

[0079] The ability of the working fluid 140 to transport heat is related to the heat of vaporization of the dielectric working fluid 140. The greater the heat of vaporization of the dielectric working fluid 140, the greater the amount of energy the working fluid 140 will absorb during vaporization and transfer to the condensing coil 150 to be released during condensation.

[0080] It is also desirable that these fluids be non-flammable or exhibit no flash point. Standards such as ASTM D56, D1310, and E681 can be used to evaluate flammability.

[0081] Since the purpose of these fluids is to remove heat from the energy storage device, one important consideration is how beneficial the dielectric fluids are for two-phase heat transfer. More specifically, how beneficial these fluids are for heat transfer under pool boiling conditions. Pool boiling heat transfer is typically divided into different modes or regimes. 1) Free convection: occurs at small values ​​of "wall superheat" or "excess temperature", which is the difference between the saturation temperature of the fluid and the wall or surface temperature. 2) Nucleate boiling: occurs when there is sufficiently high superheat for bubbles to form and detach from the surface, significantly improving the heat transfer coefficient and heat flux. This mode is typically the preferred regime of boiling operation for heat removal. The nucleate boiling regime is found in the kW / m 2 The critical heat flux (CHF) has units of 1 / 2. Heat transfer devices are usually designed to operate at heat fluxes lower than the CHF. The critical heat flux is specific to each fluid and depends on several thermophysical properties. It can be measured experimentally or estimated through semi-empirical models such as those by Zuber (1958). Fluids with higher CHF are desirable because they can remove more heat per unit area for a given wall superheat. 3) Transition boiling: A vapor film starts to form on the surface and there is an oscillation between nucleate and film boiling. This regime is unstable and it is not desirable to operate. 4) Film boiling: In this regime, the wall superheat is so high that a vapor blanket forms between the liquid and the surface, significantly reducing the heat transfer coefficient. This regime is also undesirable to operate in.

[0082] These regimes are illustrated in FIG.

[0083] [Table 2]

[0084] Table 2 shows that the proposed HFO blends have CHFs comparable to, and sometimes higher than, the legacy fluids. In particular, all proposed blends have superior CHFs compared to legacy fluids with the high GWP FC-72. The perfluoroheptene and HFE-7100 blend has a CHF within only 10% of pure HFE-7100, while the perfluoroheptene and HFE-7200 blend is also within about 10% of HFE-7200 alone. Thermophysical properties were determined through REFPROP 10, while CHFs were obtained using Zuber's (1958) correlation at sea level pressure (101.325 kPa). Thermophysical properties of REFPROP 10 were obtained using experimental data. Another aspect of boiling heat transfer is the heat transfer coefficient in the nucleate boiling region. It is measured in units of heat removed (e.g., in units of watts) per unit of temperature difference between the surface and the bulk fluid (e.g., in units of Kelvin).

[0085] In one embodiment, it is highly desirable for new low GWP fluids to provide a critical heat flux that is equal to or higher than the higher or comparable GWP fluids they replace. In another embodiment, the new low GWP fluids should provide a critical heat flux that is 90% or greater. In yet another embodiment, the new low GWP fluids should provide a critical heat flux that is 80% or greater than the critical heat flux of the high or comparable GWP fluids, such that there is no significant change in the maximum heat flux dissipation in existing immersion cooling systems, or major design changes to immersion cooling systems designed for higher GWP fluids.

[0086] A higher boiling heat transfer coefficient is desirable because it leads to a lower overall thermal resistance, or lower temperature, of the electrical component being cooled. The boiling heat transfer coefficient and electrical component-to-fluid thermal resistance can be improved through the use of surface enhancements that increase the number of nucleation sites.

[0087] The electrical component-to-fluid thermal resistance can be determined by the inverse of the product between the boiling heat transfer coefficient and the heat transfer area of ​​the electronic / electrical component.

[0088] In one embodiment, the electrical component-to-fluid thermal resistance of the new fluid should be lower or comparable to that of the existing high GWP fluid. In another embodiment, the electrical component-to-fluid thermal resistance of the new fluid should be no more than 10% higher than that of the existing high GWP fluid or comparable GWP fluid. In yet another embodiment, the electrical component-to-fluid thermal resistance of the new fluid should be no more than 20% higher than that of the existing high GWP fluid or comparable GWP fluid, such that there is no significant increase in temperature of existing electronic devices or significant mechanical changes need to be implemented in the system design for the high GWP fluid.

[0089] Another important aspect of the fluid used in a two-phase immersion cooling system is its condensation heat transfer coefficient. Higher condensation heat transfer is desirable because it leads to a reduction in the vapor-to-condenser surface thermal resistance, or a lower temperature difference between the condensing vapor and the coolant that removes the heat. Condensation heat transfer can also be improved by surface enhancement.

[0090] The vapor-to-condenser surface thermal resistance can be determined by the inverse of the product between the condensation heat transfer coefficient and the heat transfer area of ​​the condenser.

[0091] In one embodiment, the vapor-to-condenser thermal resistance of the new fluid must be lower or comparable to the existing high GWP fluid. In another embodiment, the vapor-to-condenser thermal resistance of the new fluid must be no more than 10% higher than the existing high GWP fluid or comparable GWP fluid. In yet another embodiment, the vapor-to-condenser thermal resistance of the new fluid must be no more than 20% higher than the existing high GWP fluid or comparable GWP fluid without significant degradation of condenser performance or significant mechanical changes, e.g., increased heat transfer area, that need to be implemented in a condenser designed for the high GWP fluid or comparable GWP fluid.

[0092] A higher combined boiling and condensation heat transfer coefficient is highly desirable because it reduces the overall thermal resistance between the coolant and the electronic or electrical device, reducing the temperature difference between the two. A better heat transfer coefficient results in better heat removal, which can, for example, allow a battery immersed in the dielectric liquid to be charged at a faster rate without leading to potential thermal runaway.

[0093] The heat transfer coefficients can be measured experimentally or can be calculated using experimentally determined heat transfer correlations combined with experimentally determined thermophysical properties.

[0094] [Table 3]

[0095] In Table 3, the surface-to-fluid thermal resistance is calculated using the pool boiling heat transfer coefficient and the 4 cm 2 The pool boiling heat transfer coefficient was determined by the inverse product of the surface heat transfer area and the surface area of ​​the electron. 2 The heat flux of 0.2 m was obtained using Cooper's (1984) correlation for nucleate boiling at sea level pressure. The vapor-to-condenser surface thermal resistance was calculated using the condensation heat transfer coefficient and 2 The condensation heat transfer coefficient was obtained using the correlation of Dhir and Lienhard (1971) for external condensation on a tube bundle at sea level pressure and a temperature difference between the bulk fluid and the condenser surface of 8 K.

[0096] Table 2 shows that the claimed dielectric fluids have comparable heat resistance within about 10% compared to older fluids such as HFE-7100, HFE-7200, or FC-.

[0097] The power usage or efficiency of a data center can be quantified in terms of PUE (Power Utilization Effectiveness). The lower the PUE, or closer to 1.0, the lower the energy utilized to remove a given amount of heat from the data center. It is highly desirable for the immersion tank with dielectric fluid to operate with a PUE value close to 1.0. The PUE of an immersion cooling tank can be obtained by measuring the total energy dissipated by the immersed electronics and the energy consumed by the tank. Due to the similar dielectric, thermodynamic, and heat transfer properties, the proposed fluid can also be used to replace older high GWP fluids, e.g., FC-72, HFE-7100, HFE-7200, or equivalent GWP fluids, in existing equipment in a practice often referred to as "retrofitting." Retrofitting can be partial, when only a percentage of the existing fluid is replaced, or complete, when the entire fluid is replaced with the new low GWP fluid.

[0098] An embodiment of the submerged cooling unit 200 is shown in FIG. 2. The submerged cooling system 200 includes a submerged cell 210 that defines an internal cavity 220. An energy storage device 230 to be cooled may be disposed within the internal cavity 220. A dielectric working fluid 240 partially fills the internal cavity 220. The dielectric working fluid 240 at least partially submerges the energy storage device 230. In some embodiments, the dielectric working fluid 240 substantially submerges the energy storage device 230. In one embodiment, the dielectric working fluid 240 completely submerges the energy storage device 230. A cooling unit 250 is disposed external to the submerged cell 210. The cooling unit 250 is fluidly connected to the submerged cell 210. The cooling unit 250 is configured to fluidly receive at least a portion of the dielectric working fluid 240 from the submerged cell 210. The cooling unit 250 is further configured to extract heat from the dielectric working fluid 240, thereby reducing the temperature of the dielectric working fluid 240. In one embodiment, the cooling unit 250 includes a heat exchanger. In one embodiment, the heat transferred to the cooling unit 250 is released into the environment. The cooling unit 250 is further configured to return the cooled dielectric working fluid 240 to the submerged cooling cell 210. In some embodiments, a motive force may be provided to the dielectric working fluid 240. In one embodiment, the motive force may be provided by one or more circulation pumps 260. In one embodiment, the motive force may be provided by convection.

[0099] The dielectric working fluid of the immersion cooler 200 is selected to be in a liquid state over the operating temperature range of the immersion cooler 200. In some embodiments, the composition of the dielectric working fluid 240 includes one or more fluorinated compounds. In some embodiments, the dielectric working fluid 240 includes one or more compounds that include fluorine. In some embodiments, the operating temperature is at least 25° C., at least 30° C., at least 40° C., at least 50° C., at least 60° C., less than 100° C., less than 90° C., less than 80° C., less than 70° C., and combinations thereof.

[0100] Due to the same or better dielectric, thermodynamic, and heat transfer properties, the proposed fluids may also be used to replace legacy fluids, such as HFE-7100, HFE-7200, or other high GWP fluids, in existing equipment, a practice often referred to as "retrofit."

[0101] From a practical standpoint, liquid water is forced up into the headspace of the device during start-up and operation of the system. The presence of water in a cooling system, especially in the headspace, is undesirable. It can contribute to corrosion of metal parts in the headspace of the system. It can contribute to corrosion of metal parts in the headspace of the system. The presence of water in the dielectric fluid is due to the fact that water has a significantly lower resistivity (5×10 for distilled water). 5 ohm-cm), which can be detrimental to its dielectric properties.

[0102] Another embodiment of the present disclosure is a method of cleaning a surface, comprising: a. contacting a surface with a composition comprising a solvent, the solvent comprising an azeotrope or azeotrope-like composition of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether; b. recovering the surface from the composition.

[0103] In one embodiment, the compositions of the present invention are useful as cleaning compositions, cleaners, deposition solvents, and dehydration or drying solvents. In another embodiment, the present invention relates to a process for removing residue from a surface or substrate, comprising contacting the surface or substrate with a cleaning composition or cleaner of the present disclosure, and optionally recovering the surface or substrate substantially free of residue from the cleaning composition or cleaner.

[0104] In yet another embodiment, the present disclosure relates to a method for cleaning a surface by removing contaminants from the surface. The method for removing contaminants from a surface comprises contacting the surface having contaminants with the cleaning composition of the present invention to solubilize the contaminants, and optionally recovering the surface from the cleaning composition. The surface is then substantially free of contaminants. As mentioned above, contaminants or residues that can be removed by the present method include, but are not limited to, oil and grease, flux residues, and particulate contaminants.

[0105] In one embodiment of the present disclosure, the contacting method may be by spraying, flushing, wiping with the substrate, e.g., wiping with a cloth or paper incorporating the cleaning composition, In another embodiment of the present disclosure, the contacting method may be by immersing or soaking the item in a bath of the cleaning composition.

[0106] In one embodiment of the present disclosure, the recovery process is performed by removing the contacted surface from the cleaning composition bath (in a manner similar to that described for the method for depositing a fluorolubricant on a surface, as described below). In another embodiment of the present invention, the recovery process is performed by draining the cleaning composition that has been sprayed, flushed, or wiped onto the disk. Additionally, any residual cleaning composition that may remain after the previous step is completed may be evaporated, similar to the deposition method.

[0107] In one embodiment, the cleaning composition may further comprise a propellant. The aerosol propellant may assist in delivering the composition from a storage container to a surface in the form of an aerosol. The aerosol propellant is optionally included in the composition in an amount up to about 25 weight percent of the total composition. Representative aerosol propellants include air, nitrogen, carbon dioxide, 2,3,3,3-tetrafluoropropene (HFO-1234yf), trans-1,3,3,3-tetrafluoropropene (HFO-1234ze), 1,2,3,3,3-pentafluoropropene (HFO-1225ye), difluoromethane (CF2H2, HFC-32), trifluoromethane (CF-3H, HFC-23), difluoroethane (CHF 2CH3, HFC-152a), trifluoroethane (CH3CF3, HFC-143a, or CHF2CH2F, HFC-143), tetrafluoroethane (CF3CH2F, HFC-134a, or CF2HCF2H, HFC-134), pentafluoroethane (CF3CF2H, HFC-125), and hydrocarbons such as propane, butane, or pentane, dimethyl ether, or combinations thereof.

[0108] In another embodiment, the composition may further comprise at least one surfactant. The surfactant of the present disclosure includes all surfactants known in the art for dehydrating or drying substrates. Representative surfactants include alkyl phosphate amine salts (e.g., 1:1 salt of 2-ethylhexylamine and isooctyl phosphate); ethoxylated alcohols, mercaptans, or alkylphenols; quaternary ammonium salts of alkyl phosphates (with fluoroalkyl groups on either ammonium or phosphate); and mono- or dialkyl phosphates of fluorinated amines. Additional fluorinated surfactant compounds are described in U.S. Patent No. 5,908,822, which is incorporated herein by reference.

[0109] The amount of surfactant included in the dehydrating composition of the present invention may vary widely depending on the specific drying application for which the composition is used, but is readily apparent to one of ordinary skill in the art. In one embodiment, the amount of surfactant dissolved in the unsaturated fluorinated ether solvent is about 1 weight percent or less, based on the total weight of the surfactant / solvent composition. In another embodiment, a larger amount of surfactant may be used when treating a substrate that is to be dried after treatment with the composition with a solvent that contains no or minimal surfactant. In one embodiment, the amount of surfactant is at least about 50 parts per million (ppm, by weight). In another embodiment, the amount of surfactant is about 100 to about 5000 ppm. In yet another embodiment, the amount of surfactant used is about 200 to about 2000 ppm, based on the total weight of the dehydrating composition.

[0110] Optionally, the composition containing the solvent and surfactant for dehydration may contain other additives. Such additives include compounds that have antistatic properties (the ability to dissipate static charge from non-conductive substrates such as glass and silica). The use of antistatic additives in the dehydration composition of the present invention may be essential to prevent spots and stains when drying water or aqueous solutions from non-conductive parts such as glass lenses and mirrors. Most unsaturated fluoroether solvents of the present invention are also useful as dielectric fluids, i.e., they are poor conductors of electric current and do not easily dissipate static charge.

[0111] The boiling and general circulation of the dehydrating composition in conventional drying and washing equipment can generate static charges, especially at the end of the drying process when most of the water has been removed from the substrate. Such static charges can collect on the non-conductive surfaces of the substrate and prevent the water from being released from the surface. The remaining water can dry in place, causing undesirable spots and stains on the substrate. The static charges remaining on the substrate can drive off impurities from the washing process or attract impurities such as airborne lint, which can cause unacceptable washing performance.

[0112] In one embodiment, the desired antistatic additive is a polar compound that is soluble in the unsaturated fluorinated ether solvent and increases the conductivity of the unsaturated fluorinated ether solvent to dissipate static charge from the substrate. In another embodiment, the antistatic additive has a normal boiling point near the normal boiling point of the unsaturated fluorinated ether solvent and has minimal or no solubility in water. In yet another embodiment, the solubility of the antistatic additive in water is less than about 0.5 weight percent. In one embodiment, the solubility of the antistatic agent is at least 0.5 weight percent in the unsaturated fluorinated ether solvent. In one embodiment, the antistatic additive is nitromethane (CH3NO2).

[0113] In one embodiment, the dewatering composition containing the antistatic additive is effective in the dewatering and drying and rinsing steps of the process for dewatering or drying a substrate as described below.

[0114] Another embodiment is a method of dehydrating or drying a substrate, comprising the steps of: a) contacting the surface with a composition comprising a solvent, the solvent comprising an azeotrope or azeotrope-like composition of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether, and containing a surfactant, thereby dehydrating the substrate; b) recovering the dehydrated substrate from the composition.

[0115] In one embodiment, the dehydration and drying surfactant is at least 1 weight percent soluble, based on the total weight of the solvent / surfactant composition. In another embodiment, the dehydration or drying method of the present disclosure is highly effective in removing water from a wide range of substrates, including metals such as tungsten, copper, gold, beryllium, stainless steel, aluminum alloys, brass, etc.; glass and ceramic surfaces, such as glass, sapphire, borosilicate glass, alumina, silica, such as silicon wafers used in electronic circuits, calcined alumina, etc.; and plastics, such as polyolefins ("Alathon", Rynite®, "Tenite"), polyvinyl chloride, polystyrene (Styron), polytetrafluoroethylene (Teflon®), tetrafluoroethylene-ethylene copolymers (Tefzel®), polyvinylidene fluoride ("Kynar"), ionomers (Surlyn®), acrylonitrile, butyl ether ... Nitrile-butadiene-styrene polymers (Kralac®), phenol-formaldehyde copolymers, cellulose ("Ethocel"), epoxy resins, polyacetals (Delrin®), poly(p-phenylene oxide) (Noryl®), polyetherketones ("Ultrapek"), polyetheretherketones ("Victrex"), poly(butylene terephthalate) ("Valox"), polyarylates (Arylon®), liquid crystal polymers, polyimides (Vespel®), polyetherimides ("Ultem"), polyamideimides ("Torlon"), poly(p-phenylene sulfide) ("Rython"), polysulfones ("Udel"), and polyarylsulfones ("Rydel"). In another embodiment, the compositions for use in the present dehydration or drying methods are compatible with elastomers.

[0116] In one embodiment, the present disclosure relates to a process for removing (dehydrating) at least a portion of the water from the surface of a wet substrate, comprising contacting the substrate with the aforementioned dehydrating composition and then removing the substrate from contact with the dehydrating composition. In another embodiment, the water originally bound to the surface of the substrate is displaced by the solvent and / or surfactant and leaves with the dehydrating composition. As used herein, the term "at least a portion of the water" means that at least about 75 weight percent of the water on the surface of the substrate is removed per immersion cycle. As used herein, the term "immersion cycle" means one cycle that includes at least the step of immersing the substrate in the dehydrating composition.

[0117] Optionally, the minimal amount of surfactant remaining on the substrate may be further removed by contacting the substrate with a surfactant-free halocarbon solvent. Holding the article in solvent vapor or refluxing solvent further reduces the presence of surfactant remaining on the substrate. Removal of the solvent remaining on the surface of the substrate is effected by evaporation. The solvent may be evaporated at atmospheric or subatmospheric pressure, and temperatures above or below the boiling point of the halocarbon solvent may be used.

[0118] The method of contacting the substrate with the dehydrating composition is not critical and can vary widely.For example, the substrate can be immersed in the composition, or the substrate can be sprayed with the composition using conventional equipment.It is generally preferred to completely immerse the substrate, since this ensures that the composition contacts all exposed surfaces of the substrate.However, any other method that can easily provide such complete contact can be used.

[0119] The time for contacting the substrate with the dehydrating composition can vary widely. Typically, the contact time is up to about 5 minutes, although longer times may be used if necessary. In one embodiment of the dehydrating process, the contact time is from about 1 second to about 5 minutes. In another embodiment, the contact time for the dehydrating process is from about 15 seconds to about 4 minutes.

[0120] The contacting temperature can also vary widely depending on the boiling point of the composition. Generally, the contacting temperature is equal to or lower than the normal boiling point of the composition.

[0121] In one embodiment, the composition of the present disclosure may further contain a co-solvent. Such a co-solvent is desirable when the composition is used in cleaning conventional process residues from a substrate, for example, in removing soldering flux and degreasing machine parts that include the substrate of the present invention. Such co-solvents include alcohols (e.g., methanol, ethanol, isopropanol), ethers (e.g., diethyl ether, methyl tertiary-butyl ether), ketones (e.g., acetone), esters (e.g., ethyl acetate, methyl dodecanoate, isopropyl myristate, and dimethyl or diisobutyl esters of succinic acid, glutaric acid, or adipic acid, or mixtures thereof), ether alcohols (e.g., propylene glycol monopropyl ether, dipropylene glycol monobutyl ether, and tripropylene glycol monomethyl ether), and hydrocarbons (e.g., pentane, cyclopentane, hexane, cyclohexane, heptane, octane), and hydrochlorocarbons (e.g., trans-1,2-dichloroethylene). When such co-solvents are used with the present compositions for dewatering or cleaning a substrate, the co-solvent may be present in an amount of from about 1 weight percent to about 50 weight percent, based on the weight of the total composition.

[0122] The method of cleaning a surface may be applied to the same types of surfaces as the deposition methods described below. Semiconductor surfaces or magnetic media disks of silica, glass, metal or metal oxide, or carbon may have contaminants that are removed by the process of the present invention. In the method, contaminants may be removed from the disk by contacting the disk with a cleaning composition and recovering the disk from the cleaning composition.

[0123] In yet another embodiment, the present method also provides a method of removing contaminants from an article, part, component, substrate, or any other article or portion thereof by contacting the article with the cleaning composition of the present disclosure. As referred to herein, the term "article" is intended to refer to all such articles, parts, components, substrates, etc., and further to any surface or portion thereof.

[0124] As used herein, the term "contaminant" is intended to refer to any undesirable material or substance present on an article, even if such material is intentionally placed on the article. For example, in the manufacture of semiconductor devices, it is common to deposit a photoresist material on a substrate to form a mask for an etching operation, and then remove the photoresist material from the substrate. As used herein, the term "contaminant" is intended to encompass and include such photoresist materials. Hydrocarbon-based oils and greases, as well as dioctyl phthalate, are examples of contaminants that may be found on carbon-coated disks.

[0125] In one embodiment, the method of the present invention comprises contacting an article with the cleaning composition of the present invention in a vapor degreasing and solvent cleaning method. In one such embodiment, the vapor degreasing and solvent cleaning method comprises exposing the article to the vapor of the boiling cleaning composition, preferably at room temperature. The vapor condensing on the object has the advantage of providing a relatively clean, distilled cleaning composition for washing off grease or other contaminants. Thus, such a process has the additional advantage that the final evaporation of the cleaning composition from the object leaves a relatively small amount of residue, compared to when the object is simply washed with a liquid cleaning composition.

[0126] In another embodiment, in applications where the article contains difficult to remove contaminants, the method of the present invention includes elevating the temperature of the cleaning composition to a temperature above ambient temperature, or any other temperature effective to substantially improve the cleaning action of the cleaning composition in such applications. In one such embodiment, such a process is also commonly used in high volume assembly line operations where cleaning of articles, particularly metal parts and assemblies, must be done efficiently and quickly.

[0127] In one embodiment, the cleaning method of the present disclosure includes immersing the article to be cleaned in a liquid cleaning composition at an elevated temperature. In another embodiment, the cleaning method of the present disclosure includes immersing the article to be cleaned in a liquid cleaning composition at about the boiling point of the cleaning composition. In one such embodiment, this step removes a significant amount of the target contaminants from the article. In yet another embodiment, this step removes most of the target contaminants from the article. In one embodiment, after this step, the article is immersed in a freshly distilled cleaning composition, which is at a lower temperature than the temperature of the liquid cleaning composition in the previous immersion step. In one such embodiment, the freshly distilled cleaning composition is at about ambient or room temperature. In yet another embodiment, the method also includes a step of then contacting the article with the relatively hot vapors of the cleaning composition by exposing the article to the vapors generated from the hot / boiling cleaning composition associated with the first-mentioned immersion step. In one such embodiment, this causes the vapors of the cleaning composition to condense on the article. In a particular preferred embodiment, the distilled cleaning composition may be sprayed onto the article before the final rinse.

[0128] Many kinds and types of vapor degreasing equipment are believed to be applicable for use in connection with the present method. An example of such equipment and its operation is disclosed in U.S. Patent No. 3,085,918, which is incorporated herein by reference. The equipment disclosed herein includes a boiling sump for containing the cleaning composition, a washing sump for containing the distilled cleaning composition, a water separator, and other auxiliary equipment.

[0129] The cleaning method may also include cold cleaning, in which the contaminated article is immersed in the fluid cleaning composition of the present disclosure under ambient or room temperature conditions, or wiped with a rag or similar object impregnated with the cleaning composition under such conditions.

[0130] Another embodiment relates to a method of depositing a fluorolubricant on a surface, the method comprising: (a) combining at least one fluorolubricant with a solvent to form a lubricant-solvent combination, the solvent comprising an azeotropic or azeotrope-like composition of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether; (b) contacting the lubricant-solvent combination with the surface; and (c) evaporating the solvent from the surface to form a fluorolubricant coating on the surface.

[0131] In one embodiment of the present invention, the fluorolubricant of the present disclosure includes perfluoropolyether (PFPE) compounds or lubricants containing X-1P®, a phosphazene-containing disk lubricant. These perfluoropolyether compounds are sometimes referred to as perfluoroalkylethers (PFAE) or perfluoropolyalkylethers (PFPAE). These PFPE compounds range from simple perfluorinated ether polymers to functionalized perfluorinated ether polymers. Different types of PFPE compounds that may be useful as fluorolubricants in the present disclosure are available from several sources.

[0132] In another embodiment, fluorolubricants useful in the method of the present invention include, but are not limited to, Krytox® GLP 100, GLP 105, or GLP 160 (EI du Pont de Nemours & Co., Fluoroproducts, Wilmington, DE, 19898, USA), Fomblin® Z-Dol 2000, 2500, or 4000, Z-Tetraol, or Fomblin® AM 2001, or AM 3001 (sold by Solvay Solexis SpA, Milan, Italy), Demnum™ LR-200 or S-65 (provided by Daikin America, Inc., Osaka, Japan), X-1P® (partially fluorinated hexaphenoxycyclotriphosphazene disc lubricant available from Quixtor Technologies Corporation, a subsidiary of Dow Chemical Co, Midland, MI), and mixtures thereof.

[0133] Krytox® lubricants have the general structure F(CF(CF3)CF2O) n -CF2CF3, where n ranges from 10 to 60. Fomblin® lubricants range in molecular weight from 500 to 4000 atomic mass units and have the general formula X-CF2-O(CF2-CF2-O) p -(CF2O) q A functionalized perfluoropolyether having -CF2-X, where X is -CH2OH, CH2(O-CH2-CH2) n OH, CHOCHCH(OH)CHOH, or -CHO-CH-piperonyl. Demnum™ oils are perfluoropolyether-based oils ranging in molecular weight from 2700 to 8400 atomic mass units. In addition, new lubricants have been developed, such as those from Moresco (Thailand) Co., Ltd, which may be useful in the method of the present invention.

[0134] The fluorolubricant of the present disclosure may additionally contain additives to improve the properties of the fluorolubricant.X-1P (registered trademark), which can function as a lubricant itself, is often added to other lower-cost fluorolubricants to enhance the durability of disk drives by inactivating the Lewis acid sites on the disk surface that are involved in PFPE decomposition.Other common lubricant additives can be used in the fluorolubricant of the present invention.

[0135] The fluorolubricants of the present disclosure may further include Z-DPA (Hitachi Global Storage Technologies, San Jose, Calif.), a PFPE terminated with a dialkylamine end group. The nucleophilic end group serves the same purpose as X1P®, thus providing the same stability without any additives.

[0136] The surface on which the fluorolubricant may be deposited is any solid surface that may benefit from lubrication. Semiconductor materials such as silica disks, metal or metal oxide surfaces, vapor-deposited carbon surfaces, or glass surfaces represent the types of surfaces for which the disclosed method is useful. The method of the present invention is particularly useful for coating magnetic media such as computer drive hard disks. In the manufacture of computer disks, the surface may be a glass, or aluminum substrate, having a layer of magnetic media, which is also coated by vapor deposition of a thin (10-50 angstroms) layer of amorphous hydrogenated or nitrogenated carbon. The fluorolubricant may be deposited on the surface disk indirectly by applying the fluorolubricant to the carbon layer of the disk.

[0137] The first step of combining at least one fluorolubricant with a solvent ("fluorolubricant / solvent combination") can be performed in any suitable manner, such as by mixing in a suitable vessel, such as a beaker or other vessel that can be used as a bath for the deposition process. The fluorolubricant concentration in the azeotropic solvent can be from about 0.010 percent (w / w) to about 0.50 percent (w / w).

[0138] The step of contacting the fluoro-lubricant / solvent combination with the surface can be done in any manner appropriate for the surface based on the size and shape of the surface. The hard drive disk needs to be supported in some manner, such as a mandrel or some other support that can fit through the hole in the center of the disk. Thus, the disk is held vertically so that the plane of the disk is perpendicular to the solvent bath. The mandrel can have different shapes, including but not limited to a cylindrical rod or a V-shaped rod. The mandrel shape will determine the contact area with the disk. The mandrel can be constructed of any material strong enough to hold the disk, including but not limited to metal, metal alloy, plastic, or glass. Additionally, the disk can be supported vertically upright in a woven basket or clamped in a vertical position with one or more clamps on the outer edge. The support can be constructed of any material with the strength to hold the disk, such as metal, metal alloy, plastic, or glass. However the disk is supported, the disk will be lowered into a vessel that holds a bath of the fluoro-lubricant / solvent combination. The bath may be kept at room temperature or may be heated or cooled to a temperature ranging from about 0°C to about 50°C.

[0139] Alternatively, the disk may be supported as described above and the bath may be raised to immerse the disk. In either case, the disk may then be removed from the bath either by lowering the bath or by raising the disk. Excess fluorolubricant / solvent combination may be drained into the bath.

[0140] Either method of contacting the disk surface with the fluorolubricant / solvent combination, either by lowering the disk into the bath or by raising the bath and immersing the disk, is generally referred to as dip coating. Other methods for contacting the disk with the fluorolubricant / solvent combination, including spraying or spin coating, may be used in the present disclosure.

[0141] When the disk is removed from the bath, it has a coating of fluorolubricant and some residual solvent (unsaturated fluorinated ether) on its surface. The residual solvent is allowed to evaporate. Evaporation is usually carried out at room temperature. However, other temperatures, both above and below room temperature, may also be used in the evaporation step. Temperatures ranging from about 0° C. to about 100° C. may be used for evaporation.

[0142] The surface, or the disk if the surface is a disk, will be left with a substantially uniform or homogeneous coating of substantially solvent-free fluorolubricant after completion of the coating method. The fluorolubricant may be applied to a thickness of less than about 300 nm, and alternatively to a thickness of about 100 to about 300 nm.

[0143] Since a uniform fluorinated lubricant coating is required for proper functioning of the disk, areas of varying thickness of such fluorinated lubricant are undesirable on the surface of the disk. As more and more information is stored on the same size disk, the read / write head must get closer and closer to the disk to function properly. If irregularities due to coating thickness variations exist on the surface of the disk, the likelihood of contact between the head and these areas on the disk becomes much greater. While it is desirable to have enough fluorinated lubricant on the disk to flow into areas where it can be removed by head contact or other means, a coating that is too thick can cause "smearing," a problem associated with read / write heads picking up excess amounts of fluorinated lubricant.

[0144] One particular coating thickness irregularity observed in the industry is what is known as the "rabbit ear" effect. These irregularities are visually detected on the surface of the disk after depositing the fluorolubricant using existing solvent systems. When the disk contacts a solution of fluorolubricant in a solvent and then is removed from the solution, any points where the solution accumulates and cannot easily drain will result in droplets of solution that do not easily run off. One such droplet formation point is the contact point(s) of the mandrel or other support device with the disk. If a V-shaped mandrel is used, there are two contact points where the mandrel contacts the inner edge of the disk. If the fluorolubricant solution forms droplets at these locations that do not run off when removed from the bath, then as the solvent evaporates, areas of greater fluorolubricant thickness are formed. The two contact points with the disk create what is known as the "rabbit ear" effect, as the areas of greater fluorolubricant thickness create a pattern on the disk surface that resembles a visually detectable rabbit ear.

[0145] When dip-coating is used to deposit a fluoro-lubricant on a surface, the withdrawal speed (the speed at which the disk is removed from the bath), as well as the density and surface tension of the fluoro-lubricant, are relevant in determining the resulting film thickness of the fluoro-lubricant. Knowledge of these parameters is required to obtain the desired film thickness. Details on how these parameters affect the coating are provided in "Dip-Coating of Ultra-Thin Liquid Lubricant and its Control for Thin-Film Magnetic Hard Disks" in IEEE Transactions on Magnetics, vol. 31, no. 6, November 1995.

[0146] Although the present invention has been described with reference to one or more embodiments, it will be understood by those skilled in the art that various changes can be made without departing from the scope of the invention and that equivalents can be substituted for its elements. In addition, many modifications can be made to adapt a particular situation or material to the teachings of the invention without departing from the essential scope of the invention. Therefore, it is not intended that the invention be limited to the particular embodiment disclosed as the best mode contemplated for carrying out this invention, but the invention is intended to include all embodiments falling within the scope of the appended claims. In addition, all numerical values ​​specified in the detailed description should be interpreted as if both exact and approximate values ​​were explicitly specified. EXAMPLES

[0147] The concepts described herein are further illustrated in the following examples, which do not limit the scope of the invention as described in the claims. It should be noted that not all of the operations or examples described above in the general description are required, some of the specific operations may not be required, and one or more additional operations may be performed in addition to the operations described above. Furthermore, the order in which the operations are described is not necessarily the order in which they are performed.

[0148] In the foregoing specification, the inventive concept has been described with reference to specific embodiments. However, those skilled in the art will appreciate that various modifications and changes can be made without departing from the scope of the invention as set forth in the claims below. Accordingly, the specification is to be regarded in an illustrative rather than restrictive sense, and all such modifications are intended to be included within the scope of the invention.

[0149] Benefits, other advantages, and solutions to problems have been described above with respect to specific embodiments. However, these benefits, advantages, solutions to problems, and any features that may give rise to or make more evident any benefit, advantage, or solution are not to be construed as essential, necessary, or essential features in any or all of the claims.

[0150] It should be understood that certain features that are, for clarity, described herein in the context of separate embodiments, may also be provided in combination in a single embodiment. Conversely, for brevity, various features that are described in the context of a single embodiment may also be provided separately or in any subcombination. Further, references to values ​​stated in ranges include each and every value within that range.

[0151] Example 1 - Boiling Point Depression of PFH Using HFE-347pcF A boiling point apparatus was used to determine the azeotrope-like range of a mixture of perfluoroheptene and 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether (HFE-347pcF). The apparatus consisted of a flask equipped with a thermocouple, a heating mantle, and a condenser. A rubber septum was attached to the side neck of the flask to allow one component to be added to the flask. Initially, the flask contained 100% perfluoroheptene, and the liquid was gradually heated to reflux and the boiling point was recorded to the nearest 0.1°C. Additions of HFE-347pcF were made to the flask through the side neck in increments of approximately 1% by weight. After each addition of HFE-347pcF, the boiling point of the flask was allowed to stabilize and then recorded. HFE-347pcF was added to the perfluoroheptene mixture in the flask until a composition of approximately 50% by weight HFE-347pcF and 50% by weight perfluoroheptene was present. A similar experiment was run starting with 100% HFE-347pcF in the flask and then adding perfluoroheptene in small increments to the flask to again obtain approximately 50% HFE-347pcF and 50% perfluoroheptene. In this way, the boiling points of mixtures of 0-100% HFE-347pcF and perfluoroheptene were obtained. The results are reported in Table 4.

[0152] [Table 4]

[0153] The data show a minimum boiling point of 54.9° C. for compositions of 31.7 to 47.8 wt % PFH.

[0154] Example 2: Boiling Point Depression of PFH with Novec 7100 A boiling point apparatus was used to determine the azeotrope-like range of the mixture of perfluoroheptene and Novec 7100. The apparatus consisted of a flask equipped with a thermocouple, a heating mantle, and a condenser. A rubber septum was attached to the side neck of the flask to allow one component to be added to the flask. Initially, the flask contained 100% perfluoroheptene, the liquid was gradually heated to reflux, and the boiling point was recorded to the nearest 0.1°C. Additions of Novec 7100 were made to the flask through the side neck in increments of approximately 1% by weight. After each addition of Novec 7100, the boiling point of the flask was allowed to stabilize and then recorded. Novec 7100 was added to the perfluoroheptene mixture in the flask until a composition of approximately 50% by weight Novec 7100 and 50% by weight perfluoroheptene was present. A similar experiment was run starting with 100% Novec 7100 in the flask, then perfluoroheptene was added in small increments to the flask to again obtain approximately 50% Novec 7100 and 50% perfluoroheptene. In this way, the boiling points of mixtures of 0-100% Novec 7100 and perfluoroheptene were obtained. The results are reported in Table 5.

[0155] [Table 5]

[0156] The data show a minimum boiling point of 59.9° C. for compositions of 0.9 to 10.1 wt % PFH.

[0157] Example 3 - Boiling Point Depression of PFH with Novec 7200 A boiling point apparatus was used to determine the azeotrope-like range of the mixture of perfluoroheptene and Novec 7200. The apparatus consisted of a flask equipped with a thermocouple, a heating mantle, and a condenser. A rubber septum was attached to the side neck of the flask to allow one component to be added to the flask. Initially, the flask contained 100% Novec 7200, and the liquid was gradually heated to reflux and the boiling point was recorded to the nearest 0.1°C. Additions of perfluoroheptene were made to the flask through the side neck in increments of approximately 1% by weight. After each addition of perfluoroheptene, the boiling point of the flask was allowed to stabilize and then recorded. Perfluoroheptene was added to the Novec 7200 mixture in the flask until the composition was approximately 50% by weight perfluoroheptene and 50% by weight Novec 7200. A similar experiment was run starting with 100% perfluoroheptene in the flask and then Novec 7200 was added in small increments to the flask to again obtain approximately 50% perfluoroheptene and 50% Novec 7200. In this manner, the boiling points of mixtures of 0-100% perfluoroheptene and Novec 7200 were obtained. The results are reported in Table 6. The data show a temperature minimum at 69.9°C, indicating that an azeotrope had formed. The bubble point temperature of the mixture remained constant, indicating that the mixture is an azeotrope-like mixture over a wide composition range.

[0158] [Table 6]

[0159] The data show a minimum boiling point of 69.9° C. for compositions of 15.2-20.5 wt % PFH.

[0160] Example 4 Azeotropes or azeotrope-like mixtures have been used to remove oil from surfaces as described in the examples below.

[0161] Azeotropic compositions of perfluoroheptene and the indicated amounts of fluoroethers were prepared. A pre-weighed cover glass sample (size approximately 32×18 mm) was coated with approximately 20 mg of mineral oil using a cotton swab. The coupon was weighed and immersed in the solvent in an ultrasonic cleaner at room temperature for 1 minute. The glass was removed from the solvent, air-dried for 1 minute, and then finally weighed. The % of oil removed was calculated to indicate the cleaning effectiveness.

[0162] Table 7 shows that the azeotrope-like mixture was effective in removing oil from the coupons.

[0163] [Table 7]

[0164] Example 5 - PFPE Lubricant Solubility The solubility of Fomblin T4 PFPE lubricant from Solvay was determined gravimetrically at room temperature. A glass vial was weighed to four decimal places using a laboratory balance. A known amount of lubricant was added to the vial and the mass was recorded. Each solvent was added in known increments until the lubricant was completely dissolved. After dissolution, the total weight of the container was measured and the mass of the solvent / lubricant mixture was calculated by subtracting the weight of the empty vial. The solubility limit was calculated as the weight of the lubricant divided by the weight of the solvent / lubricant mixture and expressed as the maximum weight percent of the lubricant that is completely dissolved in a given solvent.

[0165] [Table 8]

[0166] As shown in Table 8 above, mixtures of PFH and HFE-347pcf demonstrated better lubricant solubility than the pure components.

Claims

1. An azeotrope or azeotrope-like composition comprising perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether.

2. 2. The azeotropic composition of claim 1 comprising from about 31.7 weight percent to about 47.8 weight percent perfluoroheptene and from 52.2 weight percent to about 68.3 weight percent 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether.

3. 2. The azeotrope-like composition of claim 1 comprising from about 6.1 weight percent to about 61.1 weight percent perfluoroheptene and from about 38.9 weight percent to about 93.9 weight percent 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether.

4. 2. The azeotrope-like composition of claim 1 comprising from about 16.8 weight percent to about 56 weight percent perfluoroheptene and from about 44 weight percent to about 83.2 weight percent 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether.

5. 2. The azeotrope-like composition of claim 1 comprising from about 24 weight percent to about 52 weight percent perfluoroheptene and from about 48 weight percent to about 76 weight percent 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether.

6. 2. The azeotropic composition of claim 1 comprising from about 0.9 weight percent to about 10.1 weight percent perfluoroheptene and 89.9 weight percent to about 99.1 weight percent nonafluorobutyl methyl ether.

7. 2. The azeotrope-like composition of claim 1 comprising from about 0.9 weight percent to about 40.3 weight percent perfluoroheptene and from about 59.7 weight percent to about 99.1 weight percent nonafluorobutyl methyl ether.

8. 2. The azeotrope-like composition of claim 1 comprising from about 0.9 weight percent to about 27.3 weight percent perfluoroheptene and from about 72.7 weight percent to about 99.1 weight percent nonafluorobutyl methyl ether.

9. 10. The azeotrope-like composition of claim 1 comprising from about 0.9 weight percent to about 14 weight percent perfluoroheptene and from about 86 weight percent to about 99.1 weight percent nonafluorobutyl methyl ether.

10. 2. The azeotropic composition of claim 1 comprising from about 79.5 weight percent to about 84.8 weight percent perfluoroheptene and from 15.2 weight percent to about 20.5 weight percent nonafluorobutyl ethyl ether.

11. 2. The azeotrope-like composition of claim 1 comprising from about 61.3 weight percent to about 99.7 weight percent perfluoroheptene and from about 0.3 weight percent to about 38.7 weight percent nonafluorobutyl ethyl ether.

12. 2. The azeotrope-like composition of claim 1 comprising from about 67.8 weight percent to about 93.4 weight percent perfluoroheptene and from about 6.6 weight percent to about 32.2 weight percent nonafluorobutyl ethyl ether.

13. 2. The azeotrope-like composition of claim 1 comprising from about 74.3 weight percent to about 89.5 weight percent perfluoroheptene and from about 10.5 weight percent to about 25.7 weight percent nonafluorobutyl ethyl ether.

14. 1. A method for removing residue from a surface of an article, comprising: contacting the surface with a composition comprising an azeotrope or azeotrope-like composition of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether; b. recovering said surface from said composition.

15. The method of claim 14, wherein the composition further comprises a propellant.

16. 16. The method of claim 15, wherein the propellant is comprised of air, nitrogen, carbon dioxide, 2,3,3,3-tetrafluoropropene, trans-1,3,3,3-tetrafluoropropene, 1,2,3,3,3-pentafluoropropene, difluoromethane, trifluoromethane, difluoroethane, trifluoroethane, tetrafluoroethane, pentafluoroethane, a hydrocarbon, or dimethyl ether, or a combination thereof.

17. The method of claim 14, wherein the composition further comprises at least one surfactant.

18. The method of claim 14, wherein said contacting is performed by vapor degreasing.

19. The vapor degreasing a. boiling the composition; b. exposing said article to a vapor of said composition.

20. 15. The method of claim 14, wherein said contacting is performed by wiping said surface with an object saturated with said composition.

21. 1. A method for depositing a fluorolubricant on a surface of an article, comprising the steps of: a. combining a fluorolubricant with a solvent, thereby forming a mixture, the solvent comprising an azeotrope or azeotrope-like composition of perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether; b. contacting the mixture with the surface of the article; c) evaporating the solvent from the surface of the article to form a fluorolubricant coating on the surface.

22. 22. The method of claim 21, wherein the surface comprises a semiconductor material, a magnetic medium, a metal, a metal oxide, evaporated carbon, or glass, or a combination thereof.

23. The method of claim 22 , wherein the surface comprises a magnetic medium.

24. 24. The method of claim 23, wherein the magnetic medium is a computer disk.

25. 22. The method of claim 21, wherein said contacting is performed by dipping or immersing said surface in a bath comprising said fluorolubricant and a solvent.

26. 22. The method of claim 21, wherein the contacting step is performed by spraying or spin coating the surface with the fluorolubricant and solvent.

27. The method of claim 21, wherein the concentration of fluorolubricant in the lubricant-solvent mixture is from about 0.02 weight percent to about 0.5 weight percent.

28. 22. The method of claim 21, wherein the evaporating step is carried out at a temperature of about 10°C to about 40°C.

29. 22. The method of claim 21, wherein the fluorolubricant comprises at least one perfluoropolyether.

30. 1. An immersion cooling unit comprising: an immersion cell defining an interior cavity; i) an electronic component within the internal cavity; ii) a dielectric working fluid partially filling the interior cavity; and iii) a condensing coil disposed within the interior cavity above the electronic components; the dielectric working fluid at least partially immerses the electronic components; The immersion cooling unit, wherein the dielectric working fluid comprises an azeotrope or azeotrope-like composition comprising perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether.

31. 31. The immersion cooling unit of claim 30, wherein the dielectric working fluid does not submerge the condensing coil.

32. 31. The immersion cooling unit of claim 30, wherein the operating temperature range is from 40°C to 80°C.

33. 33. The immersion cooling unit of claim 32, wherein the operating temperature range is from 50°C to 70°C.

34. The dielectric working fluid has a volume resistivity of at least 1×10 10 31. The immersion cooling unit of claim 30, wherein:

35. The dielectric working fluid has a volume resistivity of at least 1×10 11 31. The immersion cooling unit of claim 30, wherein:

36. The dielectric working fluid has a volume resistivity of at least 1×10 12 31. The immersion cooling unit of claim 30, wherein:

37. 31. The immersion cooling unit of claim 30, wherein the dielectric working fluid has a global warming potential (GWP) of less than 500.

38. 31. The immersion cooling unit of claim 30, wherein the electronic component is one of a microprocessor, a wafer used to manufacture semiconductor devices, a power control semiconductor, a power distribution switchgear, a power transformer, a circuit board, a multi-chip module, packaged and unpackaged semiconductor devices, a laser, a fuel cell, and an electrochemical cell.

39. 31. The immersion cooling unit of claim 30, wherein the dielectric working fluid comprises an azeotrope of about 31.7 weight percent to about 47.8 weight percent perfluoroheptene and 52.2 weight percent to about 68.3 weight percent 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether.

40. 31. The immersion cooling unit of claim 30, wherein the dielectric working fluid comprises an azeotrope-like mixture of about 16.8 weight percent to about 56 weight percent perfluoroheptene and about 44 weight percent to about 83.2 weight percent 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether.

41. 1. A method for cooling an electrical component, comprising: at least partially immersing an electrical component in a working fluid; and using the working fluid to transfer heat from the electrical component; The method wherein the working fluid comprises an azeotrope or azeotrope-like composition comprising perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether.

42. 42. The method of claim 41, wherein the transferring of heat occurs through pumping of the working fluid from the electrical component to be cooled to a remote heat sink.

43. 43. The method of claim 42, wherein the transferring of heat occurs through evaporation of the working fluid in contact with the electrical component to be cooled and condensation of the working fluid vapor through contact with a heat sink.

44. 1. A method of replacing a high GWP dielectric fluid in an immersion cooling system, comprising:

1. A method comprising: charging an immersion cooling system designed for use with a perfluorinated working fluid with a composition comprising an azeotrope or azeotrope-like composition comprising perfluoroheptene and a fluorinated ether selected from 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, nonafluorobutyl methyl ether, and nonafluorobutyl ethyl ether.

45. 45. The method of claim 44, wherein the electrical component-to-fluid thermal resistance of the alternative fluid is lower than or equivalent to the perfluorinated working fluid.

46. 45. The method of claim 44, wherein the electrical component-to-fluid thermal resistance of the alternative fluid is no more than 20% higher than that of the perfluorinated working fluid.

47. 45. The method of claim 44, wherein the electrical component-to-fluid thermal resistance of the alternative fluid is no more than 10% higher than that of the perfluorinated working fluid.