Method for sealing an electrolytic cell and sealed electrolytic cell - Patents.com
Adhesive bonding with a state-changing encapsulant simplifies assembly and reduces space requirements in electrolytic cells, addressing assembly complexity and space limitations in existing bipolar electrolyzers.
Patent Information
- Application Number
- JP2024534085
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-08
- Filing Date
- 2022-12-06
- Publication Date
- 2024-11-28
- Estimated Expiration
- 2042-12-06
AI Technical Summary
Existing bipolar electrolyzers face challenges in assembly complexity and space requirements due to the need for precise positioning of multiple components and structural elements for sealing, which limits cell volume and increases operational stress.
A method involving adhesive bonding using an encapsulant that transforms from a liquid to a solid state to create a seal between cell elements, eliminating the need for external structural elements and allowing for simplified assembly and reduced space requirements.
This approach simplifies assembly, reduces space needs, and allows for thinner electrolytic cells with improved space utilization and reduced mechanical stress, while maintaining electrical insulation and sealing efficacy.
Smart Images

Figure 2024544224000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for sealing an electrolysis cell according to the preamble of claim 1 and to a sealed electrolysis cell according to the preamble of claim 7. [Background technology]
[0002] Bipolar electrolysers for large-scale production (i.e., megawatt range) of hydrogen and / or chlorine can be classified into two main design categories: filter press designs and single element designs.
[0003] In conventional filter press electrolysers, a stack of electrolytic cells is formed in a cell rack by stacking multiple elements with sheet separators and gaskets between adjacent elements and compressing the entire stack to seal all the electrolytic cells at once. In a filter press design electrolyser, each cell element forms an anode half-cell of one electrolytic cell and a cathode half-cell of an adjacent electrolytic cell in the stack. The sealing force for all the cells is provided by tie rods that extend along the stack.
[0004] In electrolytic cells of single element design, each electrolytic cell is a separately sealed unit. Each electrolytic cell comprises two cell elements in the form of half shells, which are bolted together at the rim areas of the two cell elements with a separator and a gasket interposed therebetween. Each cell element thus forms one half cell of the electrolytic cell, the half cells being separated by a separator. The sealing force for sealing the electrolytic cell is provided by a number of bolts distributed circumferentially along the rim areas of the cell elements.
[0005] In both design options, the separator can be an ion exchange membrane or a porous diaphragm, depending on the intended purpose of the electrolytic cell. Furthermore, in both design options, short circuits between the two cell elements forming each electrolytic cell should be reliably prevented, so that in addition to the gasket, at least one layer of an electrically insulating material is usually interposed in the rim area before sealing.
[0006] US Patent Application Publication No. 2011 / 0259735 shows examples of filter press and single element designs for bipolar electrolysers.
[0007] Known types of bipolar electrolysers have the disadvantage that they require a great deal of assembly effort to seal the cells. In filter press electrolysers, the sealing force for all cells is provided by the same set of tie rods, but sealing the cell stack is complicated and time-consuming because all separators, gaskets and insulating layers need to be accurately positioned at once. Single element electrolysers require a large number of bolted connections for each element to safely prevent leakage during operation. Furthermore, the spatial requirements of the structural elements necessary to provide the sealing force reduce the space available for the cell volume, and especially in single element designs, conventional sealing arrangements set a lower limit for the thickness of each element. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] US Patent Application Publication No. 2011 / 0259735 Summary of the Invention [Problem to be solved by the invention]
[0009] It is an object of the present invention to provide a method for sealing an electrolysis cell and a sealed electrolysis cell that requires less assembly effort and has reduced space requirements for the sealing arrangement. [Means for solving the problem]
[0010] This object is achieved by a method for sealing an electrolysis cell according to the features of claim 1 and by a sealed electrolysis cell having the features of claim 7.
[0011] Provided herein is a method for sealing an electrolysis cell comprising an anode half-cell and a cathode half-cell formed by at least two cell elements and a sheet-like separator separating the half-cells from each other, the method comprising: Providing two cell elements and a sheet-like separator; interposing a separator between the two cell elements and interposing a layer of encapsulant between each face of the separator and the two cell elements in the rim region of each of the cell elements; - sealing the electrolysis cell, wherein a force is applied to the cell elements to compress the rim area. Includes.
[0012] According to the invention, the sealant is an electrically insulating material, and during the sealing step, the state of the sealant is changed from a liquid state to a solid state to create an adhesive bond between the cell elements and the interposed separator by the sealant, the force being relaxed after the sealant has solidified.
[0013] Sealing the electrolysis cell with adhesive bonding of the cell elements simplifies the assembly of the cell, since it is no longer necessary to place and fasten bolts. Furthermore, due to the electrically insulating properties of the adhesive, a separate insulating layer can be dispensed with. The method according to the invention is particularly well suited for the automated manufacture of electrolysis cells. In addition, since the sealing force according to the invention is provided by the adhesive bond between the sealant and the cell elements, it is possible to assemble filter press type electrolysers cell by cell. Thus, an external force compressing the stack to seal the cell is no longer required. Furthermore, since external structural elements are no longer required to maintain the sealing force, the space requirements of the sealing arrangement according to the invention are particularly low, allowing a further reduction in the thickness of the cell.
[0014] In some embodiments, the sealant is a chemically curable or solvent-based adhesive. Chemically curable and solvent-based adhesives have the advantage of being a particularly strong adhesive bond that can withstand high temperatures and / or harsh chemicals. When using an adhesive as the sealant, the layer of sealant is preferably interposed by applying the adhesive in a viscous liquid state to the rim areas of both cell elements.
[0015] In another embodiment, the sealing material is a thermoplastic material and the step of sealing the electrolysis cell comprises: - inputting energy into the encapsulant to cause the encapsulant to enter a thermoplastic state; bonding the cell elements and the interposed separator while the encapsulant is in a thermoplastic state; - Reducing the temperature of the encapsulant to solidify the encapsulant; Includes.
[0016] Thermoplastic materials have the advantage that they offer the possibility of opening and resealing the electrolytic cell in an easy and non-destructive way: for maintenance, e.g. replacing the separator, the rim area can be heated until the thermoplastic material is again in a thermoplastic state and the cell elements can be separated.
[0017] If a thermoplastic material is used as the sealant, the adhesive bond can be created in a two-step process, where a layer of sealant is first bonded to the cell element, and then the two layers of sealant are bonded to each other and to the separator in a sealing step. The first bond can, for example, already be present when the two cell elements are provided, i.e. the cell elements are provided with a coating of thermoplastic material in their rim area. Alternatively, the first bond can be created during the step of interposing the sealant or during the sealing step.
[0018] Thermoplastic materials can be brought into a thermoplastic state by different types of energy supply. In the simplest case, the energy is input by heating the rim area. Another possible way of inputting energy is the thermal welding of a layer of sealing material by ultrasound.
[0019] Particularly preferred for sealing the electrolysis cell are thermoplastic materials containing polypropylene (PP), in particular atactic polypropylene (PP-R), and / or polyvinyl chloride (PVC).
[0020] Preferably, the sealing step further comprises folding the rim regions of the cell elements backwards towards one side. By folding both rim regions backwards towards the same side, for example by 120°-180°, a mechanical interlocking of the cell elements is achieved which further supports sealing of the cell. In particular, the folds are advantageous in electrolysis cells operated at elevated internal pressures, since the folds provide pressure relief to the adhesive bond by shape locking.
[0021] In a preferred embodiment, the cell elements are made of metal sheets having a thickness of 0.8 mm or less. Preferred metals are nickel and / or titanium. With the sealing concept according to the invention, it is even conceivable to manufacture electrolysis cells from metal foils having a thickness of 0.2 mm or less.
[0022] The problem is further solved by a sealed electrolysis cell comprising an anode half-cell and a cathode half-cell formed by at least two cell elements and a sheet-like separator separating the half-cells from each other. The cell elements each have a rim region and are attached to each other at their rim regions in an electrically insulating and sealed manner, with a layer of sealant interposed between each face of the separator and the two cell elements. According to the invention, the sealant is a solidified liquid material that forms an adhesive bond between the cell elements and provides electrical insulation and sealing of the cell elements.
[0023] The main advantage of the sealed electrolysis cell of the invention is that the sealing force is provided by adhesive bonding, and external structural elements for maintaining the sealing force can be omitted. Thus, electrolyzers using this type of electrolysis cell can use the available space more efficiently and allow the cell to operate under lower mechanical stress. Furthermore, the sealing structure no longer limits the possibilities for designing electrolysis cells with reduced thickness.
[0024] In certain embodiments, the encapsulant is a chemically cured adhesive or a dry, solvent-based adhesive.
[0025] In another embodiment, the encapsulant is a thermoplastic material, particularly preferably containing polypropylene (PP) and / or polyvinyl chloride (PVC).
[0026] In a preferred embodiment, the edges of the sheet separator are embedded in the solidified sealing material. Thus, the risk of leakage due to the capillary effect of the separator can also be avoided. This is particularly advantageous when a porous membrane is used as the separator, since it is known that the porous membrane causes leakage problems due to capillary forces when the porous membrane extends between the rim regions of the cell elements to the outside of the cell.
[0027] Additionally, the rim regions of the cell elements are preferably folded back towards one side to provide a mechanical form of lock between the cell elements.
[0028] The cell elements are preferably made of metal sheet having a thickness of less than or equal to 0.8 mm, in particular less than or equal to 0.2 mm. Preferred metals are nickel and / or titanium.
[0029] In particular, the present invention relates to electrolytic cells of industrial scale. Thus, the separator of the electrolytic cell according to the invention is preferably 0.5 m 2 ~4m 2 Furthermore, the electrolytic cell preferably has an area of at least 3 kA / m 2 The current density is configured as follows:
[0030] Further advantages of the present invention will be described below with reference to the embodiments illustrated in the accompanying drawings. [Brief description of the drawings]
[0031] [Figure 1] 1 shows a schematic flow diagram illustrating the method of the present invention for sealing an electrolysis cell. [Figure 2A] 1A-1D show schematic diagrams of the different stages in the fabrication of a sealed electrolysis cell of the single element type according to the invention; [Figure 2B] 3A-3D diagrammatically illustrate different stages in the fabrication of a sealed electrolysis cell of the single element type according to the invention; [Figure 2C] 10A-10C show schematic diagrams of yet another stage in the fabrication of a sealed electrolysis cell of the single element type according to the present invention; [Figure 3A] 1A-1D show schematic diagrams of the different stages in the fabrication of a sealed electrolysis cell of the filter press type according to the invention; [Figure 3B] 3A-3D diagrammatically illustrate different stages in the fabrication of a sealed electrolysis cell of the filter press type according to the invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0032] In the drawings, like parts are identified with the same reference characters throughout and therefore are generally described and referenced only once.
[0033] In Fig. 1, a flow diagram of a method 100 for sealing an electrolysis cell is shown, illustrating the sequence of steps in an abstract manner. Fig. 2A shows the electrolysis cell before the sealing step of the method, and Fig. 2B shows one embodiment of the sealed electrolysis cell 1. Fig. 2C shows a different embodiment of the sealed electrolysis cell 1 having a folded back rim region. The method steps are described below with reference to Fig. 1 and Figs. 2A-2C.
[0034] According to the method of the invention in step 110, two cell elements 4, 5 and a sheet-like separator 6 are provided. In step 120, the separator 6 is interposed between the two cell elements 4, 5 and layers of sealing material 7, 8 are interposed between each face of the separator 6 and the two cell elements 4, 5 in the rim regions 9, 10 of each of the cell elements 4, 5. Figure 2A shows the electrolysis cell in the assembled state after step 120.
[0035] In step 130, the electrolysis cell 1 is sealed, in which a force F is applied to the cell elements 4, 5 to compress the rim regions 9, 10. The sealants 7, 8 are electrically insulating materials, and during the sealing step 130, the state of the sealants 7, 8 is changed from a liquid state to a solid state to create an adhesive bond between the cell elements 4, 5 and the interposed separator 6 by the sealants 7, 8. The force F is relaxed after the sealants 7, 8 have solidified. Figure 2B shows the sealed electrolysis cell 1 after step 130.
[0036] The sealing materials 7 and 8 may be a chemically curable adhesive or a solvent-based adhesive.
[0037] In the method shown in Fig. 1, the sealing material 7, 8 is a thermoplastic material. Thus, the step 130 of sealing the electrolysis cell 1 further comprises a step 140 of inputting energy into the rim regions 9, 10 to bring the sealing material 7, 8 into a thermoplastic state, a step 150 of bonding the cell elements 4, 5 and the interposed separator 6 while the sealing material 7, 8 is in a thermoplastic state, and a step 160 of reducing the temperature of the sealing material 7, 8 to solidify the sealing material 7, 8. Preferably, the sealing material 7, 8 contains polypropylene (PP) and / or polyvinyl chloride (PVC).
[0038] For example, energy may be input by heating the rim regions 9, 10 to a temperature at which the encapsulant is in its thermoplastic state. Reducing the temperature of the encapsulant 7, 8 may be accomplished, for example, by stabilizing the temperature to ambient temperature or by active cooling of the rim regions 9, 10.
[0039] Preferably, as shown in Figure 1, the sealing step 130 further includes folding 170 the rim regions 9, 10 of the cell elements 4, 5 backward against one side of the separator. The folding 170 can be performed either after the sealing material has solidified or before. In particular, when using a chemically curable or solvent-based adhesive, the folding 170 is preferably performed before the adhesive has solidified. Figure 2C shows one embodiment of the sealed cell 1 after the folding step 170.
[0040] A sealed electrolysis cell 1 produced according to the method of the present invention is shown in Figure 2B. The sealed electrolysis cell 1 comprises an anode half-cell 2 and a cathode half-cell 3 formed by at least two cell elements 4, 5, and a sheet-like separator 6 separating the half-cells 2, 3 from each other.
[0041] The anode half-cell 2 and the cathode half-cell 3 each contain an anode and a cathode (not shown), which may be integrally joined to the respective cell elements 4, 5 or may be constructed as separate components.
[0042] The cell elements 4, 5 each have a rim region 9, 10 and are attached to one another at the rim regions 9, 10 in an electrically insulating and sealed manner with layers of sealant 7, 8 interposed between each side of the separator 6 and the two cell elements 4, 5. The sealants 7, 8 of the sealed cell 1 are solidified liquid materials that form an adhesive bond between the cell elements 4, 5 and provide electrical insulation and sealing of the cell elements 4, 5.
[0043] The solidified encapsulant may be a chemically cured adhesive or a dried solvent-based adhesive. Alternatively, the encapsulant may be a thermoplastic material. In particular, the encapsulant may contain polypropylene (PP) and / or polyvinyl chloride (PVC).
[0044] As shown in Figure 2B, the edges 11 of the sheet separator 6 are preferably embedded in the solidified encapsulant, and thus the sheet separator 6 is trapped in a form-fitting manner within the adhesive bond between the cell elements 4, 5, rather than extending outside the cell through the rim regions 9, 10.
[0045] The cell elements 4, 5 are preferably made of metal sheets having a thickness of 0.8 mm or less. In particular, it is conceivable for the cell elements to be made of metal foils having a thickness of 0.1 mm or less. Preferred metals are nickel and titanium.
[0046] The electrolytic cell 1 is preferably configured for alkaline water electrolysis or chlor-alkali electrolysis.
[0047] Figure 2C shows an embodiment of a sealed electrolysis cell 11 in which the rim regions 9, 10 of the cell elements 4, 5 are folded back towards one side. Thus, in all other respects, the description of the embodiment shown in Figure 2A is applicable to the embodiment shown in Figure 2B.
[0048] The embodiment of Figures 2B and 2C relates to an electrolysis cell 1 of single element design. The electrolysis cells 1 are constructed as separate units and can be electrically connected in series by abutting the back faces of the cell elements 4, 5 against adjacent cells. This allows a stack of electrolysis cells 1 to be built and a power supply provided on the outside of the outermost cell of the stack.
[0049] 3A and 3B show an embodiment of a filter press type method and sealed cell 1. Each cell element 4, 5 provides an anode half-cell 2 and a cathode half-cell 3 of an adjacent cell. Multiple cell elements 4, 5 can be sealed one to the other with one separator 6 each to a stack of filter press type electrolysis cells 1.
[0050] Therefore, in all other respects, the description of the embodiment shown in Figures 2A and 2B is applicable to the embodiment shown in Figures 3A and 3B. [Explanation of symbols]
[0051] 1 Electrolysis cell 2 Anode half cell 3 Cathode half cell 4, 5 Cell elements 6 Separator 7, 8 Encapsulating material 9, 10 Rim area 11 Edge of separator 100 Method for sealing an electrolytic cell 110 Providing cell elements and separators 120 Interpose separators and sealants between cell elements 130 Sealing the electrolytic cell 140 Entering energy into the rim area 150 Combine cell elements with separators 160 Reduces temperature in the rim area 170 Folding Rim Area F Compression force
Claims
1. A method for sealing an electrolytic cell (1) comprising an anode half-cell (2) and a cathode half-cell (3) formed by at least two cell elements (4, 5) and a sheet-like separator (6) separating the half-cells (2, 3) from one another, the method (100) comprising the steps of: providing (110) said two cell elements (4, 5) and said sheet-like separator (6); a step (120) of interposing the separator (6) between the two cell elements (4, 5) and a layer of sealing material (7, 8) between each face of the separator (6) and the two cell elements (4, 5) in the rim regions (9, 10) of each of the cell elements (4, 5); a step (130) of sealing the electrolysis cell (1), wherein a force (F) is applied to the cell elements (4, 5) to compress the rim areas (9, 10); A method comprising: characterised in that the sealing material (7, 8) is an electrically insulating material, and during the sealing step (130) the state of the sealing material (7, 8) is changed from a liquid state to a solid state, creating an adhesive bond between the cell elements (4, 5) and the interposed separator (6) by the sealing material (7, 8), and the force (F) is relieved when the sealing material (7, 8) solidifies. method.
2. 2. The method according to claim 1, characterized in that the sealing material (7, 8) is a chemically curable adhesive or a solvent-based adhesive.
3. The sealing material (7, 8) is a thermoplastic material, and the step of sealing (130) the electrolysis cell (1) comprises: - inputting energy into the sealing material (7, 8) to bring the sealing material (7, 8) into a thermoplastic state (140); - bonding (150) said cell elements (4, 5) and said interposed separator (6) while said sealing material (7, 8) is in said thermoplastic state; - reducing the temperature of the sealing material (7, 8) to solidify the sealing material (7, 8) (160); The method of claim 1 , comprising:
4. 4. The method of claim 3, wherein the energy is input by heating or ultrasound.
5. 5. Method according to claim 3 or 4, characterized in that the sealing material (7, 8) contains polypropylene (PP) and / or polyvinyl chloride (PVC).
6. The sealing step (130) comprises: Folding (170) the rim regions (9, 10) of the cell elements (4, 5) backwards towards one side.
6. The method according to claim 1, further comprising:
7. 7. Method according to any one of claims 1 to 6, characterized in that the cell elements (4, 5) are made of metal sheet having a thickness of less than or equal to 0.8 mm, in particular less than or equal to 0.2 mm.
8. A sealed electrolysis cell (1) comprising an anode half-cell (2) and a cathode half-cell (3) formed by at least two cell elements (4, 5) and a sheet-like separator (6) separating the half-cells (2, 3) from one another, the cell elements (4, 5) each having a rim region (9, 10) and attached to one another in an electrically insulating and sealed manner at the rim regions (9, 10) with layers of sealant (7, 8) interposed between each face of the separator (6) and the two cell elements (4, 5), characterized in that the sealant (7, 8) is a solidified liquid material which forms an adhesive bond between the cell elements (4, 5) and provides electrical insulation and sealing of the cell elements (4, 5).
9. 9. The sealed electrolysis cell according to claim 8, characterized in that the sealing material (7, 8) is a chemically cured adhesive or a dry, solvent-based adhesive.
10. 9. The sealed electrolysis cell according to claim 8, characterized in that the sealing material (7, 8) is a thermoplastic material.
11. 11. The sealed electrolysis cell according to claim 10, characterized in that the sealing material (7, 8) contains polypropylene (PP) and / or polyvinyl chloride (PVC).
12. 12. The sealed electrolysis cell according to any one of claims 8 to 11, characterized in that the edge (11) of the sheet-like separator (6) is embedded in the solidified sealing material (7, 8).
13. 13. The sealed electrolysis cell according to any one of claims 8 to 12, characterized in that the rim areas (9, 10) of the cell elements (4, 5) are folded backwards towards one side.
14. 14. The sealed electrolysis cell according to any one of claims 8 to 13, characterized in that the cell elements (4, 5) are made of metal sheets having a thickness of 0.8 mm or less, in particular 0.2 mm or less.
Citation Information
Patent Citations
Gasket and electrolyser
CN105121710A
Ion exchange membrane unit for electrolytic cell
JP1986117294A
New sealant for electrochemical battery component
JP2005347256A
Manufacturing method of cell of fuel cell and manufacturing equipment of the same
JP2007157438A
Integrated membrane electrode assembly and method of making same
JP2007504614A
Cited By
Electrolytic cell and electrolytic cell having a cell casing made from metal foil
JP2024546700A
Electrolytic cell and electrolytic bath having a cell casing made from metal foil
JP7821286B2