Conversion of plastic waste to hydrocarbons using transition metal oxides.
The steam cracking process using transition metal oxides in a non-highest oxidation state and a dual fluidized bed system addresses energy and safety issues, enhancing monomer selectivity and efficiency in polymer recycling.
Patent Information
- Application Number
- JP2024527512
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-12
- Filing Date
- 2022-11-09
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2042-11-09
AI Technical Summary
Existing steam cracking processes for polymers, particularly polyolefins, face challenges with high energy requirements, safety concerns, and low selectivity to monomer production, especially due to intramolecular H atom transfer leading to undesirable by-products.
A steam cracking process using a hydrogen control material comprising transition metals or their oxides in a non-highest oxidation state, which prevents intramolecular H atom migration by hydrogenating free radicals, combined with a dual fluidized bed system for continuous operation and hydrogen recycling.
Achieves low energy consumption, high safety standards, and high selectivity to monomers like ethylene and propylene, while avoiding undesirable by-products, through simultaneous hydrogenation and steam cracking in a fluidized bed reactor.
Smart Images

Figure 2024544916000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the field of polymer recycling, in particular the recycling of polymers into their monomeric fraction. Even more specifically, the present invention relates to the recycling of polymers by steam cracking. [Background technology]
[0002] The use of fluidized bed technology to break down plastic waste into chemicals has been thoroughly investigated since the 1970s, as outlined, for example, in US Pat. No. 3,985,820. Much effort has been directed towards the production of oils and other heavier chemicals as a means of plastic waste treatment. However, these methods suffer from the drawback of not being able to directly access the monomer portion of the polymer. However, access to such technology would be desirable, as it would completely close the cycle of polymer recycling.
[0003] Recent developments have therefore also targeted the recovery of monomers, especially olefins, from plastic waste, with varying degrees of success. WO 2020 / 169888 outlines a method in which plastic waste is vaporized in the presence of sand and Ca-containing species to produce hydrocarbons, especially olefins. However, besides the olefin fraction, a significant fraction of heavy compounds is still produced. The advantage of these methods is the lack of multifunctional catalysts that are very sensitive to the various contaminants present in the waste stream. However, the product distribution of such methods is generally controlled by the peak cracking temperature. These methods are therefore purely thermally controlled. Moreover, a higher selectivity to the monomer portion in the process output is generally achieved using higher temperatures (i.e., higher severity), making the process energetically unfavourable.
[0004] Therefore, polymer cracking processes have been developed using catalytically active fluidized bed materials that interact with the radical pool in the reaction zone and cause a change in the product distribution. Steam cracking of long-chain saturated hydrocarbons proceeds via a free radical reaction mechanism. The initial hydrocarbon chain undergoes random scission by the cleavage of the C-C bond forming two free radicals. [ka]
[0005] In this first step, primary radicals are formed, which can undergo intramolecular H-atom transfer (backbiting) to give rise to more stable secondary or tertiary radicals. [ka]
[0006] Thus, the initial distribution of hydrogen atoms along the carbon chain is altered by intramolecular H-atom transfer. Further reactions of these radicals form unstable free radicals with H / C ≠ 2, such as the methyl free radical. These unstable free radicals can in turn detach H atoms from surrounding molecules and free radicals, known as intermolecular H-atom transfer. Intermolecular H-atom transfer can further disrupt the distribution of H atoms and cause the detachment of H atoms from stable molecules such as ethylene. [ka]
[0007] H-atom transfer results in the formation of products with H / C ratios varying from 0 to 4. Thus, the products obtained from steam cracking of naphtha-like hydrocarbons, such as polyethylene, can be divided into two groups: 1. H / C=2 (same as the H / C ratio of the initial polyethylene molecule) 2. H / C≠2 (formed due to H atom transfer)
[0008] The products belonging to each category are shown in Table 1. [Table 1]
[0009] In the absence of H-atom transfer, the products of steam cracking are expected to have the same H / C ratio as the feed. Polymers such as poly(methyl methacrylate) (PMMA) and polystyrene (PS) maintain their molecular structure as well as their H / C ratio when steam cracked. Random scission of PMMA and PS molecules leads to the formation of tertiary free radicals, which are relatively more stable than primary free radicals. In addition, the functional group -COOCH 3 and -C 6 H 5 The presence of provides steric hindrance and prevents the loss of H atoms on the hydrocarbon chain.
[0010] Thus, H-atom transfer is important in the steam cracking of polymeric (e.g. polyolefin) hydrocarbons, as it prevents the production of light monomers (e.g. olefins: ethylene and propylene) and contributes to the production of less valuable hydrocarbons (methane, carbon oxides, aromatics, etc.). This is particularly relevant since H-atom transfer during steam cracking of polyolefins is unavoidable due to the lack of tertiary carbon atoms and hence steric hindrance along the polymer chain.
[0011] As a solution, the prior art offers a hydrocracking process. During the hydrocracking process, the cracked hydrocarbon molecules are immediately hydrogenated under high hydrogen partial pressure. The catalysts used in such processes are bifunctional catalysts with cracking and hydrogenation functions. The hydrogenation function works on the principle of absorbing hydrogen under very high pressure (higher than 200 bar) to activate the catalyst. The adsorption of hydrogen atoms on the surface of platinum (hydrocracking catalyst) is shown in Figure 1. Without the adsorption of hydrogen atoms under high pressure, the hydrogen molecule behaves chemically inert due to its high bond dissociation energy (436 kJ / mol).
[0012] However, compared to the steam cracking processes described above, hydrocracking processes have the disadvantage that they require significantly higher pressures to operate, which leads to the usual disadvantages of higher energy consumption, higher demands on the equipment used and potential explosion hazards. [Prior art documents] [Patent documents]
[0013] [Patent Document 1] U.S. Pat. No. 3,985,820 [Patent Document 2] International Publication No. 2020 / 169888 Summary of the Invention [Problem to be solved by the invention]
[0014] It is therefore an object of the present invention to find a process for steam cracking polymers, in particular polyolefins, which has low energy requirements, high safety standards and high selectivity to the monomeric portion of the polymer, in particular to the olefins. It is a further object of the present invention to provide such a steam cracking process which can be carried out continuously. [Means for solving the problem]
[0015] Surprisingly, the above objectives are: a) contacting plastic waste with steam and a hydrogen control material comprising at least one transition metal and / or an oxide thereof, wherein said transition metal is not in its highest oxidation state, thereby producing a mixture of gaseous hydrocarbons and a mixture of condensed hydrocarbons, and oxidizing said hydrogen control material to an oxidized hydrogen control material; and x) A step of extracting the mixture of hydrocarbons in gaseous form. It has been found that this can be achieved by a method for producing a mixture of hydrocarbons from plastic waste, comprising: [Brief description of the drawings]
[0016] [Figure 1] FIG. 1 is a schematic diagram of hydrogen activation by a hydrocracking catalyst. [Diagram 2] Figure 2 is a schematic diagram of hydrogen activation from water molecules by transition metals. [Diagram 3] FIG. 3 is a schematic diagram of the hydrogenation and recycling mechanism of the hydrogen control material of the present invention. [Figure 4] FIG. 4 is a schematic diagram of a typical dual fluidized bed (DFB) system configuration. [Diagram 5] FIG. 5 is a schematic diagram of the configuration of a dual fluidized bed system of the present invention. [Figure 6] FIG. 6 is a schematic diagram of the reactor set-up used in the comparative and inventive examples. [Figure 7] Figure 7 shows the hydrogen concentration profile during oxidation of reduced bauxite in steam at 800 °C. [Figure 8] FIG. 8 is a diagram showing the yield of light olefins in a comparison between a comparative example (CE) and an example of the present invention (IE). [Figure 9] Figure 9 is a backscattered electron micrograph of 2Fe / Al2O3 particles. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] The present invention relates to a method of contacting steam with plastic waste and a hydrogen control material comprising at least one transition metal and / or its oxide that is not in its highest oxidation state.
[0018] Thereby, hydrogen control materials help prevent intramolecular H-atom migration that leads to the formation of secondary or tertiary free radicals, thereby causing the generation of other undesirable by-products of the desired monomer portion of the polymer.
[0019] As a hydrogen control material, any transition metal and / or its oxide can be used as long as the transition metal is not in its highest oxidation state. In other words, the transition metal is the material that can convert H 2 O to H 2 Preferably, the transition metal of the hydrogen control material is selected from the list consisting of Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu and Zn. In general, however, the selection of the hydrogen control material depends on the minimum process temperature. For example, of all transition metals, Cr, Mn, Zn and Fe can be oxidized with steam (at least 1 bar pressure) at temperatures above 100°C, preferably in the range of 500-1200°C, more preferably in the range of 700-1000°C, most preferably in the range of 700-900°C. Thus, more preferably, the transition metal of the hydrogen control material is selected from the list consisting of Cr, Mn, Zn and Fe. Most preferably, the transition metal of the hydrogen control material is Fe.
[0020] The hydrogen control material is preferably an oxide of a transition metal. Preferably, the transition metal has the second highest oxidation state. Most preferably, the transition metal has the lowest oxidation state.
[0021] In a specific embodiment, the hydrogen control material comprises a non-oxidized transition metal, such as iron in the zero oxidation state.
[0022] In another specific embodiment, the hydrogen control material comprises a transition metal oxide such as iron(II) oxide and / or iron(III) oxide, particularly iron(III) oxide. More specifically, the hydrogen control material comprises iron(III) oxide (i.e., Fe 2 O 3 ).
[0023] In a further specific embodiment, the hydrogen control material is reduced bauxite or Al, preferably coated (at least partially) with iron (III) oxide in an amount equivalent to 2 wt. % atomic iron. 2 O 3 ("2Fe / Al 2 O 3 " ) particles.
[0024] To carry out the reactions described below, it is specifically necessary that the hydrogen control material be in direct contact with the steam.
[0025] Without being bound by theory, it is believed that transition metals that are not in their highest oxidation state split water molecules into hydrogen and oxygen: [ka]
[0026] Since water molecules react on the transition metal surface, the hydrogen generated on the metal surface can be likened to hydrogen adsorbed on a hydrocracking catalyst (Figure 1). Figure 2 shows the decomposition of water molecules on the transition metal surface.
[0027] Thus, when used in steam cracking of hydrocarbons, hydrogen control materials hydrogenate the generated free radicals simultaneously with the mechanism of decomposition of polymer chains. The H atoms required for hydrogenation are provided by the decomposition of water molecules on the surface of such hydrogen control materials, while the oxygen atoms of the water molecules oxidize the transition metals (e.g., M to MeO).
[0028] The hydrogen oxide control material is preferably recycled to the process after reduction with a suitable reducing agent. Such reducing agent is preferably selected from the list consisting of carbon monoxide, methane and hydrogen. Such a recycling process is depicted in FIG. 3.
[0029] Plastic waste generally may comprise a polymer backbone composed of uninterrupted CC chains. Thus, plastic waste preferably comprises polymers such as polyolefins and halogenated polymers such as PVC, PTFE, etc. More preferably, plastic waste comprises polyolefins such as polyolefins. Plastic waste may comprise one or more polyolefins selected from polyethylene homopolymers, polyethylene copolymers, polypropylene homopolymers, and polypropylene copolymers. Most preferably, plastic waste comprises polyethylene. It is preferred that plastic waste is substantially free of additives such as fillers, antioxidants, and common additives.
[0030] The mixture of hydrocarbons preferably comprises a monomer that can be used to polymerize one of the polymers in the plastic waste, more preferably the mixture of hydrocarbons comprises at least one of ethene, propene, butene.
[0031] The temperature of step a) of the method of the present invention depends on the transition metal of the hydrogen control material used. In general, the method of the present invention can usually be carried out at room temperature. Nevertheless, higher temperatures increase the reaction rate. Therefore, preferably, step a) of the method of the present invention is carried out at a temperature higher than 500° C. More preferably, step a) of the method of the present invention is carried out at a temperature of 700° C. or higher. Typically, step a) of the method of the present invention is carried out at a temperature of 1000° C. or lower.
[0032] Preferably, step a) of the process of the invention is carried out at atmospheric or reduced pressure. More preferably, step a) of the process of the invention is carried out at a pressure at which steam can exist in a subcritical state at the temperature used in said process step a).
[0033] Preferably, step a) of the method of the invention is carried out as a fluidized bed process, the steam forming part of the carrier gas and at least the hydrogen control material forming part of the fluidized bed material. It is essential to the invention that the hydrogen control material is in contact with the steam and the plastic waste. The hydrogen control material can therefore be located anywhere in the fluidized bed material, but it must be ensured that it is at least partially in direct contact with the steam and the plastic waste. Preferably, in such a case, at least a part of the hydrogen control material is located on at least a part of the surface of the fluidized bed material. This is necessary to allow the steam and the plastic waste to come into contact with said hydrogen control material. Preferably, more than 50% of the surface of the fluidized bed material is covered by the hydrogen control material, more preferably more than 80% of the surface of the fluidized bed material is covered by the hydrogen control material. Preferably, the remaining part of the fluidized bed material is chemically inert to the hydrogen activation reaction. More preferably, the remaining part of the fluidized bed material is capable of transferring heat. Even more preferably, the remaining part of the fluidized bed material is a metal oxide satisfying the two aforementioned properties. Thus, even more preferably, such a metal oxide is SiO 2 , Al 2 O 3 and MgO. Most preferably, the fluidized bed material is reduced bauxite.
[0034] In one embodiment, step a) of the process is carried out as a fluidized bed process, the fluidized bed material being SiO 2 , Al 2 O 3 and MgO, the particles being at least partially coated with a hydrogen control material.
[0035] In another embodiment, step a) of the process is carried out as a fluidized bed process, the fluidized bed material being SiO 2 , Al 2 O 3and MgO, wherein the particles are at least partially coated with at least one transition metal, wherein the transition metal is not in its highest oxidation state, and the transition metal is selected from the list consisting of Cr, Mn, Zn, and Fe.
[0036] In another embodiment, step a) of the process is carried out as a fluidized bed process, the fluidized bed material being SiO 2 , Al 2 O 3 and MgO, the particles being at least partially coated with iron(III) oxide.
[0037] In a specific embodiment, step a) of the process is carried out as a fluidized bed process, the fluidized bed material being Al 2 O 3 wherein the particles are at least partially coated with iron(III) oxide.
[0038] In another specific embodiment, step a) of the process is carried out as a fluidized bed process, the fluidized bed material comprising particles of reduced bauxite.
[0039] As mentioned above, the hydrogen control material needs to be reduced again after the decomposition and hydrogenation reactions have taken place. Therefore, in order to be able to carry out the method continuously, the hydrogen control material also needs to be continuously reduced and reintroduced into step a). This can be done by any means known to those skilled in the art. A preferred method for achieving this purpose is described below.
[0040] The process of the invention, in which step a) is preferably carried out as a fluidized bed process, is modified in that the fluidized bed material, including the hydrogen control material, is continuously or batchwise removed from the fluidized bed without interfering with the operation of the fluidization process. This can be achieved by any means known to those skilled in the art. Preferably, it is achieved by a non-mechanical valve called a loop seal (LS). The loop seal allows the transport of the fluidized bed material without exchanging gas between the two reactors. Usually, these loop seals are fluidized to prevent agglomeration of the hot fluidized bed material. In steam cracking processes, the fluidization of the loop seal is usually performed with steam.
[0041] The removed fluidized bed material contains a certain amount of hydrogen oxide control material since it has already been used to promote the steam cracking and hydrogenation reactions. Thus, after being removed from the fluidized bed, the steam used to fluidize the loop seal is at least partially replaced by a reducing agent, which reduces the hydrogen oxide control material back to hydrogen control material. Preferably, the reducing agent is selected from the list consisting of carbon monoxide, methane, and hydrogen. After the reduction step, the fluidized bed material containing the hydrogen control material is reintroduced into the fluidized bed of step a).
[0042] Thus, the method of the present invention preferably comprises the steps of: b) removing at least a portion of the hydrogen oxide control material from the fluidized bed of step a); d) reducing the hydrogen oxide control material with a reducing agent, thereby forming a hydrogen control material; e) reintroducing the hydrogen control material into step a). Further includes:
[0043] Even more preferably, the reduction step of the hydrogen oxide control material is combined with a heat supply step, which is usually necessary in industry to keep the heat high in the steam cracking reactor. The steam cracking reaction is an endothermic reaction and requires a continuous supply of heat energy. This is provided by heating the reactor or by introducing hot material into the reactor. Such a configuration is defined as a dual fluidized bed (DFB) system. The most common industrial process that can be likened to such a DFB system is the fluidized catalytic cracking (FCC) process. The hot fluidized bed material is recirculated between two interconnected fluidized beds: the combustor and the steam cracker (Figure 4). The overall reaction on the combustor side is exothermic, whereas on the cracker side the reaction is endothermic. The heat generated on the combustor side is transported by the fluidized bed material to the cracker side to meet the endothermic heat demand. This kind of configuration allows the production of two separate gas streams, namely the flue gas from the combustor and the product gas from the cracker.
[0044] In a DFB system, the fluidized bed material is continuously circulated between two interconnected fluidized beds (Figure 4). The fluidized bed material is fully oxidized in the combustor (in the presence of air) and partially reduced in the cracker (in the presence of a hydrocarbon feed). The partially reduced fluidized bed material leaves the cracker along with the unreacted solids and enters the combustor, where the unreacted solids are oxidized along with the fluidized bed material.
[0045] Also in the DFB system, the two fluidized beds are preferably interconnected by a non-mechanical valve called a loop seal (LS). The loop seal allows the transport of the fluidized bed material between the two reactors without exchanging gas. Usually, these loop seals are fluidized to prevent agglomeration of the hot fluidized bed material. Such a configuration is shown in FIG. 5. The system is modified according to the previously described embodiment: after being removed from the fluidized bed of the steam cracker, the steam used to fluidize the loop seal (LS2) is at least partially replaced by a reducing agent, which reduces the oxidized hydrogen control material back to the hydrogen control material. Preferably, the reducing agent is selected from the list consisting of carbon monoxide, methane and hydrogen. After the reduction step, the hydrogen control material is reintroduced into the fluidized bed of step a).
[0046] Therefore, even more preferably, the method of the invention comprises: b) removing at least a portion of the hydrogen oxide control material and at least a portion of the condensed hydrocarbon mixture from said fluidized bed of step a); c) oxidizing the condensed hydrocarbon mixture, thereby forming a flue gas and a heated hydrogen oxide control material; d) reducing the heated hydrogen oxide control material with a reducing agent, thereby forming a hydrogen control material; e) reintroducing the hydrogen control material into step a). Further includes:
[0047] Preferably, step c) of the process of the invention is carried out at a temperature between 500 and 1200° C., preferably between 700 and 1000° C., most preferably between 800 and 900° C. Likewise, preferably, step c) of the process of the invention is carried out at a pressure below atmospheric pressure, preferably above −0.5 bar(g), preferably in the range of −0.8 to −2 kPa.
[0048] Also preferably, step d) of the process of the invention is carried out at a temperature between 500 and 1200° C., preferably between 700 and 1000° C., most preferably between 800 and 900° C. Likewise preferably, step d) of the process of the invention is carried out at a pressure below atmospheric pressure, preferably above −0.5 bar(g), preferably in the range of −0.8 to −2 kPa.
[0049] Preferably, movement of the hydrogen control material in the method of the preferred embodiment is accomplished by movement of a fluidized bed material containing the hydrogen control material. EXAMPLES
[0050] [Measurement method] Fluidized bed material analysis Al 2 O 3 To confirm the presence of Fe in the particles, SEM-EDS was performed. Figure 9 shows the Al coated with iron(III) oxide. 2 O 3 The backscattered electron (BSE) signal from a cross-section of a particle is shown, where the weight percent of atomic iron is the weight percent of the coated Al 2 O 3 2% based on the total weight of the particle. The BSE contrast is caused by differences in average atomic weight; i.e. the brightness of a pixel increases as the atomic weight of the element being scanned increases. Thus the epoxy, which is made of light elements, appears black and the particles appear lighter in color. Since Fe is heavier than Al, the relative Fe content of the particles can be determined from the BSE contrast; lighter particles contain relatively more Fe.
[0051] Devolatization gas analysis The sampled gas is 2 , CO, CO 2 , and C.H. 4 Analyze for concentration (vol %) with a SICK GMS 820 permanent gas analyzer. Continuously monitor these gases to determine total devolatization time and ensure that no volatile gases remain after 120 seconds of sampling time.
[0052] Comprehensive Gas Analysis The remainder of the sampled gas is passed through a coil condenser maintained at -5°C for comprehensive analysis of other devolatilized species. The gas exiting the coil condenser is collected in a 0.5 L Tedlar gas bag. The gas bags collected during each experiment are analyzed with an Agilent 490 Micro GC system to determine the composition. The Agilent micro-GC is equipped with four different columns with a TCD detector for each column. An overview of the gases measured in the micro GC system is given in Table 2.
[0053] [Table 2]
[0054] 〔material〕 The PE pellets used in this study have a bulk density of 945 kg / m 3 , pellet size 2.5 mm, supplied by Borealis AB. Fluidized bed materials with different iron oxide contents were investigated for their hydrogenation capabilities. The chemical composition of the fluidized bed materials used in this study is listed in Table 3 (wt % based on the total weight of the material).
[0055] [Table 3]
[0056] Bauxite is obtained directly from natural ores, whereas Al 2 O 3 is a synthetic material obtained from Sigma Aldrich. 2 O 3 Al 2 O 3 to iron nitrate nonahydrate (Fe(NO 3 ) 3 9H 2 The AlO solution is prepared by the following reaction: 2 O 3 Fe on the surface 2 O 3 is formed: [ka]
[0057] 2Fe / Al 2 O 3 The material is sintered at 700°C. Therefore, most of the iron (Fe) is 2 O 3 Since the iron is in the form of 2Fe / Al, it can be assumed that the oxidation state is +3, i.e., iron(III) oxide. 2 O 3 " refers herein to Al coated with iron(III) oxide. 2 O 3 The weight percent of atomic iron is defined as the weight percent of the coated Al 2 O 3 2% based on the total weight of the particles.
[0058] Reactor Setup The experimental setup used for the comparative and inventive examples is shown in Figure 6. The main reactor is a stainless steel tube with an inner diameter (ID) of 88.9 mm and a height of 1305 mm. It is a bubbling fluidized bed reactor, similar to a cracker in a DFB system. The fluidizing gas is fed from the bottom of the reactor through a wind box and a distribution plate. The fluidizing gas is fed separately and mixed homogeneously in the wind box before entering the reactor through the gas distribution plate. The flow rate of the fluidizing gas is controlled by a mass flow controller (MFC).
[0059] The reactor is externally heated by an electric oven. The temperature along the height of the reactor is continuously measured and recorded by thermocouples at the rear of the reactor. The fluidized bed material is charged from the top of the reactor before turning on the reactor oven. A split stream of gas exiting the reactor is sampled through one of the gas sampling ports: h1-h5.
[0060] The gas sampling probe is inserted into the reactor through one of the ports, and the remaining ports are sealed to prevent the fluidized bed material from entering the ports. The height of the ports is selected according to the height of the fluidized bed. The probe is heated to 350 °C with an electric heating band to prevent condensation of hydrocarbons and vapors. The sampled gas is split into two parts, one of which is passed through the gas conditioning system and the other through the coil condenser.
[0061] The gas conditioning system includes an isopropanol wash of the sampled gas, which is then dried with silica gel beads and glass wool. The gas conditioning system is immersed in a water bath as shown in Figure 6. The cold, dried gas is analyzed with a SICK GMS 820 permanent gas analyzer. The coil condenser used in this study is a 4.5 m long PTFE tubing coil maintained at -5°C. The sampled gas is collected through the coil condenser into a 0.5 L Tedlar gas bag.
[0062] Comparative Example 1 g of PE pellets per batch is directly charged into the hot fluidized bed. The experimental conditions and procedures for each set are summarized in Tables 4 and 5, respectively.
[0063] Helium is used as one of the fluidizing gases during the devolatization and char combustion stages of each experiment. A known volume of helium is used as a tracer gas to determine the volume of gas produced during devolatization and char combustion.
[0064] Prior to the introduction of each batch of PE pellets, the fluidized bed material is exposed to an oxidizing environment at the same reaction temperature. Oxidation of the fluidized bed material is accomplished by fluidizing the bed material with air, as described in the previous section.
[0065] The slipstream of gas leaving the reactor was sampled from sampling port h5, and O 2 The O concentration (volume %) leaving the fluidized bed is continuously analyzed. 2 The concentration of O 2Complete oxidation is considered when the concentration corresponds to 20.9 vol%. To simulate the conditions in the DFB system, the fluidized bed material is fully oxidized before each batch of experiments, and the fluidized bed material enters the cracker after being fully oxidized in the combustor.
[0066] The conditions used in the comparative examples are shown in Tables 4 and 5.
[0067] [Table 4]
[0068] [Table 5]
[0069] During the steam cracking of polyethylene, a portion of the sampled gas was 2 , CO, CO 2 , and C.H. 4 The concentration (volume %) is analyzed by a continuous gas analyzer. These gases are continuously monitored to determine the total time of devolatization and to ensure that no volatile gases remain after the sampling time of 120 seconds.
[0070] Micro GC analysis was performed to analyze the full spectrum of products in the resulting product gas.
[0071] [Example of the invention] The simultaneous hydrogenation of the hydrocarbon species produced from the steam cracking of polyethylene is achieved by the decomposition of water molecules on the surface of a fluidized bed material containing reduced transition metals. To reduce the iron oxides present in the fluidized bed material, the fluidized bed material is treated with CO and N 2 Fluidization is performed using a mixture of CO and CO leaving the reactor. 2 CO / N 2 The mixed gas is used to fluidize the bed material, and the iron oxide content of the bed material decreases according to the following formula: [ka]
[0072] The fluidization gas was then changed to 100% N to purge the reactor and create an inert environment. 2 for 2 minutes. After the CO concentration reaches 0%, steam is added to the bed as a fluidizing gas. The steam added to the reactor is converted to hydrogen by the bed material according to the following reaction: [ka]
[0073] The polyethylene pellets are directly charged into the fluidized bed immediately after adding steam to the reactor. This ensures that the steam cracking and hydrogen generation reactions occur simultaneously. The concentration profile of hydrogen produced during the process using bauxite as the fluidized bed material is shown in Figure 7. The reaction time marked "PE feed" in Figure 7 is the time when the polyethylene pellets were fed into the fluidized bed. The experimental procedure is shown in Tables 4 and 6.
[0074] [Table 6]
[0075] 〔result〕 Bauxite and 2Fe / Al 2 O 3 The yields of gaseous products obtained for comparative and inventive examples of steam cracking of polyethylene in the presence of are shown in Table 7.
[0076] [Table 7]
[0077] The yield of light olefins ethylene and propylene is significantly increased when using transition metals that are not in their highest oxidation state, i.e., reduced. A comparison of the yield of light olefins from both hydrogen control materials is shown in Figure 8. It is clear from the results that the hydrogen generated by the decomposition of water molecules on the surface of the reduced transition metal interferes with the free radical pool generated during the steam cracking of polyethylene. Since this example was carried out at normal pressure, it could be shown that high selectivity to the light monomer portion of the polymer in the steam cracking process is possible at low pressure.
[0078] In addition, bauxite contains Fe 2 O 3 Al 2 O 3 Al is not only located on the surface of the particles. 2 O 3 The 2Fe / Al alloy is uniformly distributed throughout the material as individual particles. 2 O 3 Well then, Al 2 O 3 On its surface, Fe 2 O 3 FIG. 9 shows the 2Fe / Al 2 O 3 The scanning electron microscope (SEM) images of the 2Fe / Al alloys. Hydrogen donation works well with both fluidized bed materials. However, the 2Fe / Al alloys 2 O 3 The difference in olefin yield is significantly larger in the
Claims
1. a) contacting plastic waste with steam and a hydrogen control material comprising at least one transition metal and / or its oxide, wherein said transition metal is not in its highest oxidation state, thereby forming a mixture of gaseous hydrocarbons and a mixture of condensed hydrocarbons, and oxidizing said hydrogen control material to an oxidized hydrogen control material; x) removing the mixture of hydrocarbons in gaseous form; 1. A method for producing a mixture of hydrocarbons from plastic waste, comprising:
2. 2. The method of claim 1, wherein the transition metal is selected from the list consisting of Cr, Mn, Zn and Fe, preferably the transition metal is Fe.
3. The method of claim 1 , wherein the hydrogen control material comprises iron (II) oxide and / or iron (III) oxide, in particular iron (III) oxide.
4. The hydrogen control material is preferably reduced bauxite or Al coated with iron (III) oxide in an amount equivalent to 2 wt. % atomic iron. 2 O 3 Particles (“2Fe / Al 2 O 3 The method according to any one of claims 1 to 3, wherein the compound is selected from the group consisting of 1) 1-3).
5. The method according to any one of claims 1 to 4, wherein the plastic waste comprises one or more polyolefins.
6. 6. The method of claim 5, wherein the polyolefin is selected from polyethylene homo- or copolymer, polypropylene homo- or copolymer.
7. The method according to any of the preceding claims, wherein step a) is carried out at a temperature above 500°C, preferably at a temperature of 700°C or higher.
8. The process according to any one of claims 1 to 7, wherein step a) is carried out at normal pressure.
9. A method according to any of the preceding claims, wherein step a) is carried out as a fluidised bed process, said steam forming part of the carrier gas and at least said hydrogen control material forming part of the fluidised bed.
10. b) removing at least a portion of the hydrogen oxide control material and at least a portion of the condensed hydrocarbon mixture from the fluidized bed of step a); c) oxidizing the condensed hydrocarbon mixture, thereby forming a flue gas and a heated, oxidized hydrogen control material; d) reducing the heated and oxidized hydrogen control material with a reducing agent, thereby forming said hydrogen control material; e) reintroducing the hydrogen control material into step a). The method of claim 8 further comprising:
11. 10. The method of claim 9, wherein the reducing agent is selected from the list consisting of carbon monoxide, methane, and hydrogen.
12. The method according to any of claims 8 to 10, wherein step c) is carried out at a temperature of 500 to 1200°C.
13. The method according to any one of claims 8 to 11, wherein step c) is carried out at subatmospheric pressure.
14. The method according to any of claims 8 to 12, wherein step d) is carried out at a temperature of 500 to 1200°C.
15. The method according to any one of claims 8 to 13, wherein step d) is carried out at subatmospheric pressure.
16. The process according to any of claims 8 to 14, wherein step c) is carried out as a fluidized bed process.
Citation Information
Patent Citations
Thermal decomposition of plastics, and device and dechlorinating agent used therefor
JP1999140460A
Iron oxide-based catalyst for decomposing organic waste, its manufacturing method and treating method of organic waste
JP2001129405A
Method for treating waste plastics
JP2001323308A
Method for producing light oil from waste plastic containing phthalate-based polyester and / or polyvinyl chloride
JP3170290B2
Cracking process
US3985820A