Elevator rope and its manufacturing method

The elevator rope design addresses shape loss in high-strength fiber yarns by using a steel core and steel wire layers to maintain shape, ensuring low ellipticity and improved durability.

JP7551767B2Active Publication Date: 2024-09-17MITSUBISHI ELECTRIC CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2022556757
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-14
Publication Date
2024-09-17
Estimated Expiration
2040-10-14

AI Technical Summary

Technical Problem

High-strength fiber yarns used in elevator ropes tend to lose their shape when loosely twisted, leading to ellipticity issues that can shorten the rope's lifespan, especially in high-lift elevators with large diameters and lengths.

Method used

The elevator rope design includes a steel core surrounded by a fiber layer made of high-strength synthetic fibers, with additional steel wire layers wound around, using the steel core to maintain shape and reduce ellipticity.

Benefits of technology

This design allows for easy production of elevator ropes with low ellipticity, reducing weight and potentially eliminating the need for weight-compensating ropes, while enhancing durability and traction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007551767000015
    Figure 0007551767000015
  • Figure 0007551767000009
    Figure 0007551767000009
  • Figure 0007551767000007
    Figure 0007551767000007
Patent Text Reader

Abstract

Provided is an elevator rope for suspending a car of an elevator, the elevator rope comprising: a steel core composed of steel strands formed by twisting a plurality of steel wires, or a single steel wire; a first fiber layer composed of high-strength synthetic fibers disposed on the outer circumference of the steel core; and a first steel wire layer obtained by winding, multiple times, steel strands formed by twisting a plurality of steel wires, or a single steel wire, on the outer circumference of the first fiber layer. According to this elevator rope, an elevator rope that includes high-strength synthetic fibers and has low ellipticity can be easily manufactured.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an elevator rope for suspending a car in an elevator and a method for manufacturing the same. [Background technology]

[0002] As buildings become taller, elevators are becoming higher. In elevators with high lifts, the diameter and length of the elevator ropes used become larger, so that lightweight, high-strength ropes are required. Therefore, a method of using lightweight, strong, high-strength synthetic fibers as the core of elevator ropes is known.

[0003] Patent Document 1 discloses a method for manufacturing an elevator rope by placing a fiber core made of high-strength synthetic fiber in the center and winding a steel strand around the outer periphery of the fiber core. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] International Publication No. 2017 / 064808 Summary of the Invention [Problem to be solved by the invention]

[0005] In the manufacture of a fiber core made of high-strength synthetic fibers, a large number of high-strength fiber yarns, each of which is made by bundling a number of high-strength synthetic fibers having a diameter of several to several tens of μm, are arranged and bundled or twisted together to form a fiber core, so that the overall cross-sectional shape of the fiber core is circular. In this case, the high-strength fiber yarns are intentionally twisted a little loosely so that the fiber core can sufficiently bear the tensile load applied to the elevator rope during elevator operation. However, since the high-strength fiber yarns are thin and soft, they tend to lose their shape when twisted loosely, and it is not easy to make a circular core material, and they may end up becoming elliptical. If the ellipticity of the core material is high, the ellipticity of the rope in which a steel strand is wound around the outer periphery of the core material will also be high, and if the ellipticity is high, the life of the rope may be shortened.

[0006] Therefore, an object of the present disclosure is to provide an elevator rope having a structure that allows for easy production of an elevator rope containing high-strength synthetic fibers and having low ovality, and a method for producing the same. [Means for solving the problem]

[0007] The elevator rope according to the present disclosure comprises a steel core made of a steel strand formed by twisting together a plurality of steel wires or a single steel wire, a first fiber layer made of high-strength synthetic fibers arranged on the outer periphery of the steel core, and a first steel wire layer made by winding a plurality of steel strands formed by twisting together a plurality of steel wires or a single steel wire around the outer periphery of the first fiber layer.

[0008] The manufacturing method for an elevator rope according to the present disclosure includes the steps of arranging a plurality of fiber bundles made of high-strength synthetic fibers around the outer periphery of a steel core made of a steel strand formed by twisting a plurality of steel wires together or a single steel wire to form a first fiber layer, and winding a plurality of the steel strand formed by twisting a plurality of steel wires together or a single steel wire around the outer periphery of the first fiber layer to form a first steel wire layer. Effect of the Invention

[0009] According to the elevator rope and manufacturing method thereof according to the present disclosure, an elevator rope containing high-strength synthetic fibers and having low ovality can be easily manufactured. [Brief description of the drawings]

[0010] [Figure 1] 1 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a first embodiment. [Diagram 2] FIG. 2 is a side view showing a state in which each layer of the elevator rope according to the first embodiment has been cut open in order. [Diagram 3] 4 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a modified example of the first embodiment. FIG. [Figure 4] FIG. 11 is a side view showing a state in which each layer of the elevator rope according to the first modified example of the first embodiment has been cut open in order. [Diagram 5] FIG. 11 is a side view showing a state in which each layer of an elevator rope according to a second modified example of the first embodiment has been cut open in order. [Figure 6] FIG. 6 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a second embodiment. [Figure 7] 13 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a modified example of the second embodiment. FIG. [Figure 8] FIG. 11 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a third embodiment. [Figure 9] FIG. 13 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a first modified example of the third embodiment. [Figure 10] FIG. 13 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a second modified example of the third embodiment. [Figure 11] FIG. 11 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a fourth embodiment. [Figure 12] FIG. 13 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a modified example of the fourth embodiment. [Figure 13] FIG. 13 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a fifth embodiment. [Figure 14] FIG. 13 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a modified example of the fifth embodiment. [Figure 15] FIG. 13 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a sixth embodiment. [Figure 16] FIG. 23 is a cross-sectional view perpendicular to the longitudinal direction of an elevator rope according to a modified example of the sixth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] [First embodiment] Hereinafter, an elevator rope 100 according to a first embodiment will be described. Fig. 1 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 100. Fig. 2 is a side view showing the state in which each layer of the elevator rope 100 has been cut open in order.

[0012] 1 and 2, an elevator rope 100 has a steel core 11 and a first fiber layer 12 made of high-strength synthetic fibers arranged on the outer periphery of the steel core 11. Also, a first steel wire layer 13 is formed by winding a plurality of first steel strands 13n around the outer periphery of the first fiber layer 12.

[0013] The steel core 11 is made of a steel strand formed by twisting together a number of steel wires. The steel core 11 is made of a core wire 11a and six side wires 11b wound around the outer periphery of the core wire 11a. Both the core wire 11a and the side wires 11b are made of steel wires.

[0014] The first fiber layer 12 is a layer made of high-strength synthetic fibers arranged on the outer periphery of the steel core 11. The first fiber layer 12 is formed by twisting together a plurality of fiber bundles, each of which is made of high-strength synthetic fibers. Examples of high-strength synthetic fibers include carbon fibers, glass fibers, polyparaphenylenebenzoxazole (PBO) fibers, aramid fibers, polyarylate fibers, and basalt fibers. Each fiber bundle may be integrated by being solidified with a resin such as an epoxy resin or a urethane resin, or may be coated with a resin.

[0015] The first steel wire layer 13 is formed by winding a plurality of first steel strands 13n, each of which is made by twisting a plurality of steel wires, around the outer periphery of the first fiber layer 12. In the example shown in FIG. 1, eight first steel strands 13n are wound around the outer periphery of the first fiber layer 12. Each first steel strand 13n has a core wire 13a, nine first side wires 13b wound around the outer periphery of the core wire 13a, and nine second side wires 13c wound around the outer periphery of the core wire 13a. The core wire 13a, the first side wires 13b, and the second side wires 13c are all made of steel wires. In the first embodiment, the first steel wire layer 13 is located in the outermost layer of the elevator rope 100 and is exposed to the outside.

[0016] When manufacturing the elevator rope 100, first, a plurality of fiber bundles made of high-strength synthetic fibers are arranged on the outer periphery of the steel core 11 made of a steel strand twisted together with a plurality of steel wires to form the first fiber layer 12. Specifically, the plurality of fiber bundles are twisted together along the outer periphery of the steel core 11 to form the first fiber layer 12. At this time, the plurality of fiber bundles are twisted together a little loosely so that the first fiber layer 12 can sufficiently bear the tensile load applied to the elevator rope. However, since the steel core 11 is used as the core material, the shape is not easily distorted when twisted together, and the first fiber layer 12 is easily formed. Then, a plurality of first steel strands 13n made of twisted together with a plurality of steel wires are wound around the outer periphery of the first fiber layer 12 to form the first steel wire layer 13.

[0017] As described above, the elevator rope 100 includes the steel core 11, the first fiber layer 12 made of high-strength synthetic fibers arranged around the outer periphery of the steel core 11, and the first steel wire layer 13 formed by winding a plurality of steel strands around the outer periphery of the first fiber layer 12. This makes it possible to easily form the first fiber layer 12 using the steel core 11 as a core material, and to easily manufacture an elevator rope containing high-strength synthetic fibers and having low ellipticity.

[0018] Furthermore, the higher the elevator rises and falls, the more preferable it is to provide the elevator with a rope (or chain) for weight compensation. However, since elevator rope 100 contains high-strength synthetic fibers, it can be made lighter, and therefore the number or mass of the rope (or chain) for weight compensation can be further reduced or completely eliminated.

[0019] In the above first embodiment, the first fiber layer 12 is described as being made by twisting a plurality of fiber bundles around the outer periphery of the steel core 11. However, instead of this, the first fiber layer 12 may be made by knitting a plurality of fiber bundles together, or may be made by arranging a plurality of fiber bundles approximately in parallel and bundling them together.

[0020] In the first embodiment, the structure of the constituent strands constituting the steel core 11 (such as the number and arrangement of steel wires) may be changed as appropriate. The number of first steel strands 13n constituting the first steel wire layer 13 and the structure of each first steel strand 13n (such as the number and arrangement of steel wires) may also be changed as appropriate.

[0021] [First Modification of the First Embodiment] Hereinafter, an elevator rope 101 which is a first modified example of the first embodiment will be described. Fig. 3 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 101. Fig. 4 is a side view showing the state in which each layer of the elevator rope 101 has been cut open in order.

[0022] As shown in Figs. 3 and 4, the elevator rope 101 differs from the first embodiment in that it has a resin coating layer 18 as the outermost layer. That is, in the elevator rope 100 according to the first embodiment, the first steel wire layer 13 is exposed to the outside as the outermost layer of the elevator rope 100. In contrast, in the elevator rope 101 according to this modification, the outer periphery of the first steel wire layer 13 is coated with the coating layer 18. This improves the abrasion resistance and durability of the elevator rope 101. The coating layer 18 is inserted between the adjacent first steel strands 13n. As a material for the coating layer 18, a resin having a sufficient friction coefficient, such as an elastomer resin or polyurethane, is used to ensure traction ability between the sheave.

[0023] Furthermore, the higher the elevator rises and falls, the more preferable it is to provide the elevator with a rope (or chain) for weight compensation, but the elevator rope 101 can be made lighter by including high-strength synthetic fibers, and the improved coefficient of friction between the rope and the sheave suppresses slippage between the rope and the sheave, enabling stable power transmission. As a result, the number or mass of the rope (or chain) for weight compensation can be further reduced or completely eliminated.

[0024] [Second Modification of the First Embodiment] Hereinafter, an elevator rope 102 which is a second modified example of the first embodiment will be described. Fig. 5 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 102. The elevator rope 102 differs from the first embodiment in that it has a buffer layer made of resin between the steel core 11 and the first fiber layer 12, and between the first fiber layer 12 and the first steel wire layer 13. In the following explanation, the difference will be explained, and explanations of the same configuration as the first embodiment will be omitted.

[0025] As shown in Fig. 5, the elevator rope 102 has a first buffer layer 19a made of resin between the steel core 11 and the first fiber layer 12. This can suppress wear of the first fiber layer 12 caused by direct contact between the steel core 11 and the first fiber layer 12. In addition, a second buffer layer 19b made of resin is provided between the first fiber layer 12 and the first steel wire layer 13. This can suppress wear of the first fiber layer 12 caused by direct contact between the first fiber layer 12 and the first steel wire layer 13. The first buffer layer 19a and the second buffer layer 19b are made of a resin having wear resistance and low friction, such as polyethylene or polypropylene.

[0026] In the second modified example of the first embodiment, a case is described in which a buffer layer made of resin is provided between the steel core 11 and the first fiber layer 12 and between the first fiber layer 12 and the first steel wire layer 13. However, instead of this, a buffer layer may be provided only in one of these locations. This makes it possible to suppress wear of the first fiber layer 12 at the location where the buffer layer is provided. In other words, it is sufficient to provide a buffer layer in at least one location between the steel core 11 and the first fiber layer 12 and between the first fiber layer 12 and the first steel wire layer 13.

[0027] [Second embodiment] An elevator rope 200 according to the second embodiment will be described below. Fig. 6 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 200. The elevator rope 200 differs from that of the first embodiment in that the steel core 21 is made of a single steel wire. In contrast, in the first embodiment, the steel core 11 is made of a steel strand in which a plurality of steel wires are twisted together. Other points are the same as those of the first embodiment, so a description thereof will be omitted here.

[0028] In addition, in this second embodiment, a buffer layer may be provided at least in one location between the steel core 21 and the first fiber layer 12 and between the first fiber layer 12 and the first steel wire layer 13.

[0029] [Modification of the second embodiment] An elevator rope 201 which is a modified example of the second embodiment will be described below. FIG. 7 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 201. As shown in FIG. 7, the elevator rope 201 differs from the second embodiment in that it has a resin coating layer 28 as the outermost layer. That is, in the elevator rope 200 according to the second embodiment, the first steel wire layer 13 is exposed to the outside as the outermost layer of the elevator rope 200. In contrast, in the elevator rope 201 according to this modified example, the outer periphery of the first steel wire layer 13 is coated with the coating layer 28. This improves the abrasion resistance and durability of the elevator rope 201.

[0030] The covering layer 28 is inserted between the adjacent first steel strands 13n. The material of the covering layer 28 is a resin having a sufficient coefficient of friction, such as an elastomer resin or polyurethane, in order to ensure traction capacity with the sheave.

[0031] [Third embodiment] Hereinafter, an elevator rope 300 according to the third embodiment will be described. Fig. 8 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 300.

[0032] As shown in Fig. 8, an elevator rope 300 has a steel core 31 and a first fiber layer 32 made of high-strength synthetic fibers arranged around the steel core 31. The rope also has a first steel wire layer 33 formed by winding a plurality of first steel strands 33n around the first fiber layer 32. The rope also has a second fiber layer 34 made of high-strength synthetic fibers arranged around the first steel wire layer 33. The rope also has a second steel wire layer 35 formed by winding a plurality of second steel strands 35n around the second fiber layer 34.

[0033] The steel core 31 is made of a steel strand formed by twisting together a number of steel wires. The steel core 31 is made of a core wire and six side wires wound around the core wire. Both the core wire and the side wires are made of steel wires.

[0034] The first fiber layer 32 is a layer made of high-strength synthetic fibers arranged on the outer periphery of the steel core 31. The first fiber layer 32 is formed by twisting together a plurality of fiber bundles, each of which is made of high-strength synthetic fibers. Examples of high-strength synthetic fibers include carbon fibers, glass fibers, polyparaphenylenebenzoxazole (PBO) fibers, aramid fibers, polyarylate fibers, and basalt fibers. Each fiber bundle may be integrated by being solidified with a resin such as an epoxy resin or a urethane resin, or may be coated with a resin.

[0035] The first steel wire layer 33 is formed by winding a plurality of first steel strands 33n, each of which is made by twisting a plurality of steel wires, around the outer periphery of the first fiber layer 32. In the example shown in Fig. 8, twelve first steel strands 33n are wound around the outer periphery of the first fiber layer 32. Each first steel strand 33n is made of a core wire and six side wires wound around the outer periphery of the core wire. Both the core wire and the side wires are made of steel wire.

[0036] The second fiber layer 34 is a layer made of high-strength synthetic fibers arranged on the outer periphery of the first steel wire layer 33. The second fiber layer 34 is formed by twisting together a plurality of fiber bundles, each of which is made of high-strength synthetic fibers. Examples of high-strength synthetic fibers include carbon fibers, glass fibers, polyparaphenylenebenzoxazole (PBO) fibers, aramid fibers, polyarylate fibers, and basalt fibers. Each fiber bundle may be integrated by being solidified with a resin such as an epoxy resin or a urethane resin, or may be coated with a resin.

[0037] The second steel wire layer 35 is formed by winding a plurality of second steel strands 35n, each of which is made by twisting a plurality of steel wires, around the outer periphery of the second fiber layer 34. In the example shown in FIG. 8, twelve second steel strands 35n are wound around the outer periphery of the second fiber layer 34. Each second steel strand 35n has a core wire, nine first side wires wound around the outer periphery of the core wire, and nine second side wires wound around the outer periphery of the first side wires. The core wire, the first side wires, and the second side wires are all made of steel wires. In the third embodiment, the second steel wire layer 35 is located in the outermost layer of the elevator rope 300 and is exposed to the outside.

[0038] When manufacturing the elevator rope 300, first, a plurality of fiber bundles made of high-strength synthetic fibers are arranged on the outer periphery of the steel core 31 made of a steel strand twisted together with a plurality of steel wires to form the first fiber layer 32. Specifically, the plurality of fiber bundles are twisted together along the outer periphery of the steel core 31 to form the first fiber layer 32. At this time, the plurality of fiber bundles are twisted together a little loosely so that the first fiber layer 32 can sufficiently bear the tensile load applied to the elevator rope. However, since the steel core 31 is used as the core material, the shape is not easily distorted when twisted together, and the first fiber layer 32 is easily formed. After that, a plurality of first steel strands 33n made of twisted together with a plurality of steel wires are wound around the outer periphery of the first fiber layer 32 to form the first steel wire layer 33.

[0039] Then, a plurality of fiber bundles made of high-strength synthetic fibers are arranged on the outer periphery of the first steel wire layer 33. To form the second fiber layer 34, a plurality of fiber bundles are twisted together along the outer circumferential surface of the first steel wire layer 33 to form the second fiber layer 34. Thereafter, a plurality of second steel strands 35n formed by twisting together a plurality of steel wires are wound around the outer periphery of the second fiber layer 34 to form the second steel wire layer 35.

[0040] As described above, the elevator rope 300 includes the steel core 31, the first fiber layer 32 made of high-strength synthetic fibers arranged around the steel core 31, and the first steel wire layer 33 made of a plurality of steel strands wound around the first fiber layer 32. This allows the first fiber layer 32 to be easily formed using the steel core 31 as a core material, and an elevator rope containing high-strength synthetic fibers and having low ellipticity can be easily manufactured. The elevator rope 300 further includes the second fiber layer 34 made of high-strength synthetic fibers arranged around the first steel wire layer 33, and the second steel wire layer 35 made of a plurality of steel strands wound around the second fiber layer 34. That is, two fiber layers are provided. This allows the amount of high-strength synthetic fibers used to be increased, thereby realizing weight reduction.

[0041] Furthermore, the higher the elevator's lift height, the more preferable it is to provide the elevator with a weight compensation rope (or chain); however, elevator rope 300, which contains a greater amount of high-strength synthetic fibers due to its multiple fiber layers, is lighter than conventional elevator ropes, and the number or mass of weight compensation ropes (or chains) can be further reduced or completely eliminated.

[0042] In the above third embodiment, the first fiber layer 32 and the second fiber layer 34 are described as being formed by twisting a plurality of fiber bundles around the outer periphery of the steel core 31. Alternatively, however, the first fiber layer 32 and the second fiber layer 34 may be formed by knitting a plurality of fiber bundles together, or by arranging a plurality of fiber bundles approximately in parallel and bundling them together.

[0043] In the third embodiment, the structure of the constituent strands constituting the steel core 31 (such as the number and arrangement of steel wires) may be changed as appropriate. The number of first steel strands 33n constituting the first steel wire layer 33 and the structure of each first steel strand 33n (such as the number and arrangement of steel wires) may also be changed as appropriate. The number of second steel strands 35n constituting the second steel wire layer 35 and the structure of each second steel strand 35n (such as the number and arrangement of steel wires) may also be changed as appropriate.

[0044] In the third embodiment, a buffer layer made of resin may be provided at least in one of the following locations: between the steel core 31 and the first fiber layer 32, between the first fiber layer 32 and the first steel wire layer 33, between the first steel wire layer 33 and the second fiber layer 34, and between the second fiber layer 34 and the second steel wire layer 35. This makes it possible to suppress wear of the first fiber layer 32 or the second fiber layer 34 in the locations where the buffer layer is provided. In this case, the material for the buffer layer may be a resin having wear resistance and low friction, such as polyethylene or polypropylene.

[0045] [First Modification of the Third Embodiment] An elevator rope 301 which is a modified example of the third embodiment will be described below. FIG. 9 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of elevator rope 301. As shown in FIG. 9, elevator rope 301 differs from the third embodiment in that elevator rope 301 has a resin coating layer 38 as the outermost layer. That is, in elevator rope 300 according to the third embodiment, second steel wire layer 35 is exposed to the outside as the outermost layer of elevator rope 300. In contrast, in elevator rope 301 according to this modified example, the outer periphery of second steel wire layer 35 is coated with coating layer 38. This improves the abrasion resistance and durability of elevator rope 301.

[0046] The covering layer 38 is inserted between the adjacent second steel strands 35n. The material of the covering layer 38 is a resin having a sufficient coefficient of friction, such as an elastomer resin or polyurethane, in order to ensure traction capacity with the sheave.

[0047] Furthermore, the higher the elevator's lift height, the more preferable it is to provide the elevator with a rope (or chain) for weight compensation, but elevator rope 301, which contains a greater amount of high-strength synthetic fiber through multiple fiber layers, can be made lighter than conventional elevator ropes, and the improved friction coefficient with the sheave can suppress slippage between the sheave and ensure stable power transmission. As a result, the number or mass of weight compensation ropes (or chains) can be further reduced or completely eliminated.

[0048] [Second Modification of the Third Embodiment] An elevator rope 302, which is a modified example of the third embodiment, will be described below. FIG. 10 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 302. As shown in FIG. 10, the elevator rope 302 differs from the third embodiment in that it has a resin coating 39 that coats each of the first steel strands 33n of the first steel wire layer 33, but there is no substantial difference in other respects. This makes it possible to suppress wear of the first fiber layer 32 caused by direct contact between the first fiber layer 32 and the first steel wire layer 33. In addition, it is possible to suppress wear of the second fiber layer 34 caused by direct contact between the first steel wire layer 33 and the second fiber layer 34. The material of the coating 49 is a resin having wear resistance and low friction, such as polyethylene or polypropylene.

[0049] [Fourth embodiment] An elevator rope 400 according to the fourth embodiment will be described below. Fig. 11 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 400. The elevator rope 400 differs from that of the third embodiment in that the steel core 41 is made of a single steel wire. In contrast, in the third embodiment, the steel core 31 is made of a steel strand in which a plurality of steel wires are twisted together. Since the other points are the same as those of the third embodiment, the description will be omitted here.

[0050] [Modification of the fourth embodiment] An elevator rope 401 which is a modified example of the fourth embodiment will be described below. FIG. 12 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 401. As shown in FIG. 12, the elevator rope 401 differs from the fourth embodiment in that it has a resin coating layer 48 as the outermost layer. That is, in the elevator rope 400 according to the fourth embodiment, the second steel wire layer 35 is exposed to the outside as the outermost layer of the elevator rope 400. In contrast, in the elevator rope 401 according to this modified example, the outer periphery of the second steel wire layer 35 is coated with the coating layer 48. This improves the abrasion resistance and durability of the elevator rope 401.

[0051] The covering layer 48 is inserted between the adjacent second steel strands 35n. The material of the covering layer 48 is a resin having a sufficient coefficient of friction, such as an elastomer resin or polyurethane, in order to ensure traction capacity with the sheave.

[0052] [Fifth embodiment] Hereinafter, an elevator rope 500 according to the fifth embodiment will be described. Fig. 13 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 500.

[0053] As shown in Fig. 13, an elevator rope 500 has a steel core 51, a first fiber layer 52 made of high-strength synthetic fibers arranged around the steel core 51, and a first steel wire layer 53 formed by winding a plurality of first steel strands 53n around the first fiber layer 52. The rope also has a second fiber layer 54 made of high-strength synthetic fibers arranged around the first steel wire layer 53, and a second steel wire layer 55 formed by winding a plurality of second steel strands 55n around the second fiber layer 54. The rope also has a third fiber layer 56 made of high-strength synthetic fibers arranged around the second steel wire layer 55, and a third steel wire layer 57 formed by winding a plurality of third steel strands 57n around the third fiber layer 56.

[0054] The steel core 51 is made of a steel strand formed by twisting together a number of steel wires. The steel core 51 is made of a core wire and six side wires wound around the core wire. Both the core wire and the side wires are made of steel wires.

[0055] The first fiber layer 52 is a layer made of high-strength synthetic fibers arranged on the outer periphery of the steel core 51. The first fiber layer 52 is formed by twisting together a plurality of fiber bundles, each of which is made of high-strength synthetic fibers. Examples of high-strength synthetic fibers include carbon fibers, glass fibers, polyparaphenylenebenzoxazole (PBO) fibers, aramid fibers, polyarylate fibers, and basalt fibers. Each fiber bundle may be integrated by being solidified with a resin such as an epoxy resin or a urethane resin, or may be coated with a resin.

[0056] The first steel wire layer 53 is formed by winding a plurality of first steel strands 53n, each of which is made by twisting a plurality of steel wires together, around the outer periphery of the first fiber layer 52. In the example shown in Fig. 13, twelve first steel strands 53n are wound around the outer periphery of the first fiber layer 52. Each first steel strand 53n is made of a core wire and six side wires wound around the outer periphery of the core wire. Both the core wire and the side wires are made of steel wire.

[0057] The second fiber layer 54 is a layer made of high-strength synthetic fibers arranged on the outer periphery of the first steel wire layer 53. The second fiber layer 54 is formed by twisting together a plurality of fiber bundles, each of which is made of high-strength synthetic fibers. Examples of high-strength synthetic fibers include carbon fibers, glass fibers, polyparaphenylenebenzoxazole (PBO) fibers, aramid fibers, polyarylate fibers, and basalt fibers. Each fiber bundle may be integrated by being solidified with a resin such as an epoxy resin or a urethane resin, or may be coated with a resin.

[0058] The second steel wire layer 55 is formed by winding a plurality of second steel strands 55n, which are formed by twisting a plurality of steel wires together, around the outer periphery of the second fiber layer 54. In the example shown in Fig. 13, 20 second steel strands 55n are wound around the outer periphery of the second fiber layer 54. Each second steel strand 55n has a core wire, nine first side wires wound around the outer periphery of the core wire, and nine second side wires wound around the outer periphery of the first side wires. The core wire, the first side wires, and the second side wires are all made of steel wires.

[0059] The third fiber layer 56 is a layer made of high-strength synthetic fibers arranged on the outer periphery of the second steel wire layer 55. The third fiber layer 56 is formed by twisting together a plurality of fiber bundles, each of which is made of high-strength synthetic fibers. Examples of high-strength synthetic fibers include carbon fibers, glass fibers, polyparaphenylenebenzoxazole (PBO) fibers, aramid fibers, polyarylate fibers, and basalt fibers. Each fiber bundle may be integrated by being solidified with a resin such as an epoxy resin or a urethane resin, or may be coated with a resin.

[0060] The third steel wire layer 57 is formed by winding a plurality of third steel strands 57n, each of which is made by twisting a plurality of steel wires, around the outer periphery of the third fiber layer 56. In the example shown in FIG. 13, 15 third steel strands 57n are wound around the outer periphery of the third fiber layer 56. Each third steel strand 57n has a core wire, nine first side wires wound around the outer periphery of the core wire, and nine second side wires wound around the outer periphery of the first side wires. The core wire, the first side wires, and the second side wires are all made of steel wires. In the fifth embodiment, the third steel wire layer 57 is located in the outermost layer of the elevator rope 500 and is exposed to the outside.

[0061] When manufacturing the elevator rope 500, first, a plurality of fiber bundles made of high-strength synthetic fibers are arranged around the outer periphery of a steel core 51 made of a steel strand formed by twisting together a plurality of steel wires. To form the first fiber layer 52, a plurality of fiber bundles are twisted together along the outer circumferential surface of the steel core 51 to form the first fiber layer 52. At this time, the plurality of fiber bundles are twisted together somewhat loosely so that the first fiber layer 52 can sufficiently bear the tensile load applied to the elevator rope, but since the steel core 51 is used as the core material, the shape is not easily distorted when twisted together, and the first fiber layer 52 is easily formed. After that, a plurality of first steel strands 53n formed by twisting together a plurality of steel wires are wound around the outer circumferential surface of the first fiber layer 52 to form the first steel wire layer 53.

[0062] Thereafter, a plurality of fiber bundles made of high-strength synthetic fibers are arranged around the outer periphery of the first steel wire layer 53 to form the second fiber layer 54. Specifically, the plurality of fiber bundles are twisted together along the outer periphery of the first steel wire layer 53 to form the second fiber layer 54. In addition, a plurality of second steel strands 55n formed by twisting together a plurality of steel wires are wound around the outer periphery of the second fiber layer 54 to form the second steel wire layer 55.

[0063] Thereafter, a plurality of fiber bundles made of high-strength synthetic fibers are arranged on the outer periphery of the second steel wire layer 55 to form a third fiber layer 56. Specifically, the plurality of fiber bundles are twisted together along the outer periphery of the second steel wire layer 55 to form the third fiber layer 56. In addition, a plurality of third steel strands 57n formed by twisting together a plurality of steel wires are wound around the outer periphery of the third fiber layer 56 to form the third steel wire layer 57.

[0064] As described above, the elevator rope 500 includes a steel core 51, a first fiber layer 52 made of high-strength synthetic fibers arranged around the steel core 51, and a first steel wire layer 53 formed by winding a plurality of steel strands around the first fiber layer 52. This allows the first fiber layer 52 to be easily formed using the steel core 51 as a core material, and allows an elevator rope containing high-strength synthetic fibers to be easily manufactured. The elevator rope 500 further includes a second fiber layer 54 made of high-strength synthetic fibers arranged around the first steel wire layer 53, and a second steel wire layer 55 formed by winding a plurality of steel strands around the second fiber layer 54. The elevator rope 500 further includes a third fiber layer 56 made of high-strength synthetic fibers arranged around the second steel wire layer 55, and a third steel wire layer 57 formed by winding a plurality of steel strands around the third fiber layer 56. In other words, there are three fiber layers, which allows for a greater amount of high-strength synthetic fiber to be used, resulting in a lighter weight.

[0065] Furthermore, the higher the elevator's lift height, the more preferable it is to provide the elevator with a weight compensation rope (or chain). However, elevator rope 500, which contains a greater amount of high-strength synthetic fibers due to its multiple fiber layers, is lighter than conventional elevator ropes, and the number or mass of weight compensation ropes (or chains) can be further reduced or completely eliminated.

[0066] In the above fifth embodiment, the first fiber layer 52 and the second fiber layer 54 are described as being formed by twisting a plurality of fiber bundles around the outer periphery of the steel core 51. However, instead of this, the first fiber layer 52 and the second fiber layer 54 may be formed by knitting a plurality of fiber bundles together, or by arranging a plurality of fiber bundles approximately in parallel and bundling them together.

[0067] In the above fifth embodiment, the structure of the constituent strands constituting the steel core 51 (such as the number and arrangement of steel wires) may be changed as appropriate. The number of first steel strands 53n constituting the first steel wire layer 53 and the structure of each first steel strand 53n (such as the number and arrangement of steel wires) may also be changed as appropriate. The number of second steel strands 55n constituting the second steel wire layer 55 and the structure of each second steel strand 55n (such as the number and arrangement of steel wires) may also be changed as appropriate. The number of third steel strands 57n constituting the third steel wire layer 57 and the structure of each third steel strand 57n (such as the number and arrangement of steel wires) may also be changed as appropriate.

[0068] In the fifth embodiment, a buffer layer made of resin may be provided between the first fiber layer 52 and the first steel wire layer 53. This can suppress wear of the first fiber layer 52 caused by direct contact between the first fiber layer 52 and the first steel wire layer 53. For the same reason, a buffer layer made of resin may also be provided between the first steel wire layer 53 and the second fiber layer 54, and between the second fiber layer 54 and the second steel wire layer 55. A buffer layer made of resin may also be provided between the second steel wire layer 55 and the third fiber layer 56, and between the third fiber layer 56 and the third steel wire layer 57. The material of the buffer layer may be a resin having wear resistance and low friction, such as polyethylene or polypropylene.

[0069] In the fifth embodiment, a buffer layer made of resin may be provided at least in one of the following locations: between the steel core 51 and the first fiber layer 52, between the first fiber layer 52 and the first steel wire layer 53, between the first steel wire layer 53 and the second fiber layer 54, between the second fiber layer 54 and the second steel wire layer 55, between the second steel wire layer 55 and the third fiber layer 56, and between the third fiber layer 56 and the third steel wire layer 57. This can suppress wear of the first fiber layer 52, the second fiber layer 54, or the third fiber layer 56 in the locations where the buffer layer is provided. In this case, the material of the buffer layer can be a resin having wear resistance and low friction, such as polyethylene or polypropylene.

[0070] [Modification of the fifth embodiment] An elevator rope 501 which is a modification of the fifth embodiment will be described below. FIG. 14 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 501. As shown in FIG. 14, the elevator rope 501 differs from the fifth embodiment in that it has a resin coating layer 58 as the outermost layer. That is, in the elevator rope 500 according to the fifth embodiment, the third steel wire layer 57 is exposed to the outside as the outermost layer of the elevator rope 500. In contrast, in the elevator rope 501 according to this modification, the outer periphery of the third steel wire layer 57 is coated with the coating layer 58. This improves the abrasion resistance and durability of the elevator rope 501.

[0071] The covering layer 58 is inserted between the adjacent third steel strands 57n. The material of the covering layer 58 is a resin having a sufficient coefficient of friction, such as an elastomer resin or polyurethane, in order to ensure traction capacity with the sheave.

[0072] [Sixth embodiment] An elevator rope 600 according to the sixth embodiment will be described below. Fig. 15 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 600. The elevator rope 600 differs from the fifth embodiment in that the steel core 61 is made of a single steel wire. In contrast, in the fifth embodiment, the steel core 51 is made of a steel strand in which a plurality of steel wires are twisted together. Since the other points are the same as those in the fifth embodiment, the description will be omitted here.

[0073] [Modification of the sixth embodiment] An elevator rope 601 which is a modified example of the sixth embodiment will be described below. FIG. 16 is a cross-sectional view showing a cross section perpendicular to the longitudinal direction of the elevator rope 601. As shown in FIG. 16, the elevator rope 601 differs from the sixth embodiment in that it has a resin coating layer 68 as the outermost layer. That is, in the elevator rope 600 according to the sixth embodiment, the third steel wire layer 57 is exposed to the outside as the outermost layer of the elevator rope 600. In contrast, in the elevator rope 601 according to this modified example, the outer periphery of the third steel wire layer 57 is coated with the coating layer 68. This improves the abrasion resistance and durability of the elevator rope 601.

[0074] The covering layer 68 is inserted between the adjacent third steel strands 57n. The material of the covering layer 68 is a resin having a sufficient coefficient of friction, such as an elastomer resin or polyurethane, in order to ensure traction capacity with the sheave.

[0075] In the above embodiment, the case where the fiber layer is one, two or three layers has been described, but the number of fiber layers can be appropriately increased according to the degree of increase in the diameter of the elevator rope. In that case, it is preferable to provide a steel wire layer on the outer periphery of each fiber layer. [Explanation of symbols]

[0076] 11, 21, 31, 41, 51, 61 steel core 11a, 13a core wire 11b Lateral line 13b First Lateral Line 13c Second lateral line 12, 32, 52 First fiber layer 13, 33, 53 First wire layer 13n, 33n, 53n 1st steel strand 18, 28, 38, 48, 58, 68 coating layer 19a First buffer layer 19b Second buffer layer 34, 54 Second fiber layer 35, 55 Second steel wire layer 35n, 55n Second Steel Strand 39 Covering 56 Third fiber layer 57 Third wire layer 57n Third Steel Strand 100,101,200,201,300,301,400,401,500,501,600,601 Elevator rope

Claims

1. A steel core made of a steel strand formed by twisting together a plurality of steel wires or a single steel wire; a first fiber layer made of high strength synthetic fibers arranged on an outer periphery of the steel core; A first steel wire layer is formed by winding a plurality of steel strands or a single steel wire around the outer periphery of the first fiber layer; a second fiber layer made of high strength synthetic fiber arranged on an outer periphery of the first steel wire layer; A second steel wire layer is formed by winding a plurality of steel strands or a single steel wire around the outer periphery of the second fiber layer. An elevator rope comprising:

2. 2. The elevator rope according to claim 1, further comprising a buffer layer made of resin at least in one location between the first steel wire layer and the second fiber layer and between the second fiber layer and the second steel wire layer.

3. a third fiber layer made of high strength synthetic fiber arranged on an outer periphery of the second steel wire layer; a third steel wire layer formed by winding a plurality of steel strands or a single steel wire around the outer periphery of the third fiber layer; The elevator rope according to claim 1 or 2, further comprising:

4. 4. The elevator rope according to claim 3, further comprising a buffer layer made of resin at least in one location between the second steel wire layer and the third fiber layer and between the third fiber layer and the third steel wire layer.

5. 5. The elevator rope according to claim 1, further comprising a resin coating layer as an outermost layer.

6. A step of forming a first fiber layer by arranging a plurality of fiber bundles made of high-strength synthetic fibers on an outer periphery of a steel strand made of a plurality of twisted steel wires or a steel core made of a single steel wire; A step of winding a plurality of steel strands or a single steel wire around the outer periphery of the first fiber layer to form a first steel wire layer; forming a second fiber layer by arranging a plurality of fiber bundles made of high strength synthetic fibers on an outer periphery of the first steel wire layer; a step of winding a plurality of steel strands or a single steel wire around the outer periphery of the second fiber layer to form a second steel wire layer; A method for manufacturing an elevator rope comprising the steps of:

7. forming a third fiber layer by arranging a plurality of fiber bundles made of high strength synthetic fibers on an outer periphery of the second steel wire layer; a step of winding a plurality of steel strands or a single steel wire around the outer periphery of the third fiber layer to form a third steel wire layer; The method for manufacturing an elevator rope according to claim 6, further comprising:

8. The method for producing an elevator rope according to claim 6 or 7, further comprising a step of forming a coating layer by coating the rope with a coating body made of a resin as an outermost layer.

Citation Information

Patent Citations

  • Main rope for rope type elevator

    JP2002060162A

  • Elevator driving mechanism

    JP2003292270A

  • Elevator device and wire rope for elevator

    JP2011046462A

  • Coated wire rope

    WO2004055263A1

  • Elevator rope and manufacturing method therefor

    WO2017064808A1