System and method for manufacturing a shrouded impeller
By employing rings to maintain a consistent gap between the shroud and vanes during manufacturing, the impeller balance and compressor efficiency are improved, addressing the issue of unbalanced impellers and porosity in traditional methods.
Patent Information
- Application Number
- JP2022508908
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-08-12
- Filing Date
- 2020-08-12
- Publication Date
- 2024-09-18
- Estimated Expiration
- 2040-08-12
AI Technical Summary
Impellers in compressors often become unbalanced and inefficient due to improper centering of the shroud during metal bonding processes, leading to increased porosity and reduced efficiency.
The use of rings extending from the inner surface of the shroud to maintain a consistent gap between the shroud and vanes during the manufacturing process, ensuring proper alignment and balance by forming an interference or friction fit with the vane tips.
This method enhances impeller balance, reduces porosity, and increases compressor efficiency by maintaining a consistent gap, thereby reducing maintenance requirements and fluid resistance.
Smart Images

Figure 0007553186000004 
Figure 0007553186000005 
Figure 0007553186000003
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to U.S. Non-provisional Patent Application No. 16 / 947,680, filed August 12, 2020, and U.S. Provisional Patent Application No. 62 / 885,907, filed August 13, 2019, the disclosures of which are incorporated herein by reference in their entireties.
[0002] The field of the disclosure relates generally to impellers for compressors and the like, and more particularly to systems and methods for enabling more reliable manufacturing of impellers, such as by brazing. [Background technology]
[0003] A typical centrifugal compressor includes a compressor housing and an impeller located within the compressor housing. The impeller includes a hub, blades attached to the hub, and a shroud attached to the blades on the opposite side of the hub. The blades are typically cast with the hub, and the shroud is typically attached to the blades using a metal joining process, such as a brazing process, a welding process, a soldering process, and / or any other metal joining process. However, if the shroud is not centered on the blades and the hub during the metal joining process, the impeller will be unbalanced, reducing the efficiency of the impeller and the compressor. In addition, an unbalanced impeller will also continue to increase porosity, which also reduces the efficiency of the impeller and the compressor.
[0004] This Background section is intended to introduce the reader to various aspects of art that may be related to various aspects of the present disclosure, which are described and / or claimed below. This discussion is believed to be helpful in providing the reader with background information to facilitate a better understanding of the various aspects of the present disclosure. Accordingly, it should be understood that these statements are to be read in this light, and not as admissions of prior art. Summary of the Invention
[0005] In one aspect, a method of manufacturing an impeller includes attaching a plurality of blades to a hub. The impeller includes the blades, the hub, and a shroud. The blades each include a tip, and the shroud includes an inner surface and at least one ring extending from the inner surface. The method also includes applying a brazing compound to the tips of the blades and the inner surface of the shroud. The method further includes inserting the blades and the hub into the shroud such that the tips of the blades are pressed against the ring. The ring and tips of the blades form an interference fit between the ring and the tips of the blades that maintains a consistent gap between the shroud and the blades during manufacturing of the impeller. The method also includes attaching the blades to the shroud using a brazing process.
[0006] In another aspect, a compressor includes a compressor housing and an impeller disposed within the compressor housing. The impeller includes a hub including a hub surface, a plurality of vanes extending from the hub surface, and a shroud. The shroud includes an inner surface attached to the vanes and at least one ring extending from the inner surface. The ring is configured to engage the vanes when the vanes and hub are inserted into the shroud and to maintain a consistent gap between the shroud and the vanes during manufacture of the impeller.
[0007] In yet another aspect, an impeller includes a hub including a hub surface, a plurality of vanes extending from the hub surface, and a shroud. The shroud includes an inner surface attached to the vanes and at least one ring extending from the inner surface. The ring is configured to engage the vanes when the vanes and hub are inserted into the shroud and to maintain a consistent gap between the shroud and the vanes during manufacture of the impeller.
[0008] Various refinements exist in the features mentioned with respect to the above-mentioned aspects. Further features may also be incorporated into the above-mentioned aspects. These refinements and further features may exist individually or in any combination. For example, various features discussed below with respect to any of the illustrated embodiments may be incorporated into any of the above-mentioned aspects, alone or in any combination. [Brief description of the drawings]
[0009] [Figure 1] FIG. 2 is a schematic cross-sectional view of a compressor. [Diagram 2] FIG. 2 is a perspective view of the impeller illustrated in FIG. 1 with the shroud removed for clarity. [Diagram 3] FIG. 3 is a cross-sectional view of the impeller illustrated in FIGS. 1 and 2. [Figure 4] FIG. 4 is a perspective view of a shroud for use with the impeller illustrated in FIGS. 1-3. [Diagram 5] FIG. 5 is a perspective view of a portion of the inner surface of the shroud illustrated in FIG. 4. [Figure 6] 5 is another perspective view of a portion of the inner surface of the shroud illustrated in FIG. 4. [Figure 7] FIG. 7 is a cross-sectional view of the impeller illustrated in FIGS. [Figure 8] FIG. 8 is a flow diagram of a method of manufacturing the impeller illustrated in Figures 1 to 7. Corresponding reference characters indicate corresponding parts throughout the drawings. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] FIG. 1 is a schematic cross-sectional view of a compressor 100 illustrated as a single-stage centrifugal compressor. Non-limiting examples of centrifugal compressors include single-stage centrifugal compressors, two-stage centrifugal compressors, and multi-stage centrifugal compressors. In alternative embodiments, the compressor 100 may include any type of compressor including an impeller. The compressor 100 generally includes a compressor housing 102 that defines at least one enclosed cavity in which compression is accomplished. The compressor 100 includes an inlet 110 for introducing fluid into the compressor housing 102, an outlet 106 for discharging fluid from the compressor housing, and an impeller 200 for adding kinetic energy to the fluid. The kinetic energy imparted to the fluid by the impeller 200 is converted to increased pressure (i.e., compression). The impeller 200 is connected to a drive shaft (not shown) that is operably connected to a motor (not shown). The motor rotates the impeller 200 at a selected rotational speed to compress the fluid to a preselected pressure that exits the outlet 106. Any suitable motor may be operably connected to the compressor 100, including, but not limited to, an electric motor. The fluid may include any fluid that enables the compressor 100 to operate as described herein, including, but not limited to, air, refrigerant, and / or other fluids.
[0011] FIG. 2 is a perspective view of the impeller 200 illustrated in FIG. 1 with the shroud 206 removed for clarity. FIG. 3 is a cross-sectional view of the impeller 200 illustrated in FIGS. 1 and 2. In this embodiment, the impeller 200 is configured to compress a fluid flow for the compressor 100 and for a cooling system in which the compressor 100 is incorporated, such as an HVAC system. The impeller 200 includes a plurality of blades 202 coupled between a hub 204 and a shroud 206. For example, the impeller 200 includes fourteen blades 202. Each blade 202 includes a tip 207 extending along a length of the blade that defines an outer diameter 209 of the blade. Alternatively, the blades 202 may have any suitable blade shape, such as airfoil blades, backward-curved blades, forward-curved blades, vertical blades, and / or radial blades, that enable the impeller 200 to operate as described herein. Further, the impeller 200 may include any number of vanes 202 that enable the operation described herein. In addition, as shown in FIG. 2, the vanes 202 are spirally wound around the hub surface 216 such that each vane forms a helical or helical ramp around the hub surface 216. In alternative embodiments, the vanes 202 may have any orientation relative to the hub surface 216 that enables the impeller 200 to operate as described herein. For example, the vanes 202 may be attached to the hub surface 216 such that the vanes are oriented parallel to the central axis 208.
[0012] The hub 204 and shroud 206 in this embodiment are coaxial and configured to rotate about a central axis 208. The vanes 202 are coupled to the hub 204 and / or shroud 206 such that the vanes, hub, and shroud define a fluid flow path 210. The vanes 202, hub 204, and shroud 206 define an inlet 212 and an outlet 214. During rotation, the vanes 202 are configured to draw in fluid through the inlet 212 along the central axis 208 and expel the fluid radially outward through the outlet 214 defined between adjacent vanes 202, hub 204, and shroud 206. When the impeller 200 is operating, fluid enters through the inlet 212 and is redirected outward from the central axis 208 by the hub 204. 2, the hub surface 216 of the hub 204 includes a bell-shaped profile that redirects fluid radially outward from the central axis 208. The vanes 202 are configured to draw fluid through an inlet 212 and into a fluid passage 210 where the fluid passes between the vanes. The fluid passage 210 pushes the fluid outward through an outlet 214 due to centrifugal forces generated by the rotating vanes 202. More specifically, adjacent vanes 202, hub 204, and shroud 206 define a fluid passage 210 configured to accelerate the fluid through the fluid passage 210 such that the outlet 214 discharges the fluid in a direction generally perpendicular to the central axis 208.
[0013] 1 and 3, the shroud 206 also includes a bell-shaped profile that complements the bell-shaped profile of the hub surface 216. More specifically, the inner surface 218 and the outer surface 220 also include a bell-shaped profile that complements the bell-shaped profile of the hub surface 216. Due to the bell-shaped profiles of the hub surface 216, the inner surface 218, and the outer surface 220, the hub surface, the inner surface, and the outer surface are oriented generally parallel to the central axis 208 proximate the inlet 212 and generally perpendicular to the central axis proximate the outlet 214. That is, proximate the inlet 212, the inner surface 218 and the hub surface 216 are oriented such that the inner surface surrounds the hub surface, and proximate the outlet 214, the inner surface and the hub surface are oriented such that the inner surface is axially offset from the hub surface along the central axis 208. Additionally, proximate the inlet 212, the vanes 202 are oriented such that an inner surface 218 surrounds the vanes. The orientation of the inner surface 218 relative to the vanes 202 and hub surface 216 allows the inner surface to maintain the position of the shroud 206 relative to the vanes and hub 204 during the manufacturing process.
[0014] FIG. 4 is a perspective view of the shroud 206 illustrated in FIGS. 1-3. FIG. 5 is a perspective view of a portion of the inner surface 218 of the shroud 206 proximate the inlet 212. FIG. 6 is a perspective view of a portion of the inner surface 218 proximate the outlet 214. FIG. 7 is a cross-sectional view of a portion of the impeller 200. The shroud 206 includes at least one protrusion 502 and 504 extending from the inner surface 218 of the shroud. The protrusions 502 and 504 in this embodiment are ring-shaped. In an alternative embodiment, the protrusions 502 and 504 may have any shape that enables the impeller 200 to operate as described herein. In this embodiment, the shroud 206 includes a first ring 502 located proximate the inlet 212 and a second ring 504 located proximate the outlet 214. In an alternative embodiment, the shroud 206 includes only the first ring 502. In another alternative embodiment, the shroud 206 includes only the second ring 504 .
[0015] Each of the rings 502 and 504 is a rounded bump including an apex 506, a first edge 508, and a second edge 510. In alternative embodiments, the rings 502 and 504 may have any shape that enables the rings 502 and 504 to operate as described herein. The height 514 of the rings 502 and 504 is measured from the inner surface 218 to the apex 506. In this embodiment, the height 514 is approximately 0.001 inches. (0.0254mm) From about 0.006 inches (0.1524 mm) , or approximately 0.005 inches (0.127mm) However, the height 514 may be any length that enables the rings 502 and 504 to operate as described herein. The first ring 502 defines an inner diameter 518 within the shroud 206. As discussed in more detail below, the height 514 of the rings 502 and 504 enables the inner surface 218 and the ring to hold the position of the shroud 206 relative to the vanes 202 and hub 204 during the manufacturing process and to maintain a consistent gap 516 between the shroud 206 and the vanes 202.
[0016] In this example, the vanes 202 and hub 204 are made as a single unit prior to attaching the shroud 206 to the vanes. Specifically, the vanes 202 and hub 204 are made as a single unit using a casting or machining process, and the shroud 206 is attached to the vanes using a metallurgical joining process. Alternatively, the vanes 202 and hub 204 are made separately from one another, and the vanes are attached to the hub using a metallurgical joining process, such as, but not limited to, a brazing process, a welding process, a soldering process, and / or any other metallurgical joining process. The shroud 206 is then attached to the vanes 202 using a metallurgical joining process, such as, but not limited to, a brazing process, a welding process, a soldering process, and / or any other metallurgical joining process. In one embodiment, the shroud 206 is then attached to the vanes 202 using a brazing process.
[0017] To join the shroud 206 to the vanes 202, the position of the shroud relative to the vanes is fixed or maintained during the brazing process by the rings 502 and 504. Specifically, the vanes 202 and hub 204 are inserted into the shroud 206 such that the vane tips 207 are pressed against the rings 502 and 504. More specifically, as the vanes 202 are inserted into the inlet 212, the vane tips 207 engage the first ring 502 such that the first ring presses against the vane tips and maintains a consistent gap 516 between the shroud 206 and the vanes during the brazing process.
[0018] The first ring 502 engages the tip 207 of the vane 202 such that the first ring holds the vane and hub 204 in place by friction between the first ring 502 and the vane tip. For example, the first ring 502 and the vane tip 207 form an interference or friction fit that holds the vane and hub 204 in place by friction between the first ring 502 and the vane tip. As used herein, an interference or friction fit is a fit between two parts where the exterior dimensions of one part slightly exceed the interior dimensions of the part that must fit. In this embodiment, the vane tip 207 also includes a bell-shaped profile that complements the bell-shaped profile of the inner surface 218. However, the bell-shaped profile of the vane tip 207 does not include a notch to accommodate the first ring 502. As such, the height 514 of the first ring 502 causes the outer diameter 209 of the vane 202 to exceed the inner diameter 518 of the first ring such that the first ring is pressed against the tip 207 of the vane. Thus, the height 514 of the first ring 502 allows the first ring to form an interference or friction fit with the vane 202 such that the first ring maintains a consistent gap 516 between the shroud 206 and the vane during the brazing process, and maintains the position of the shroud relative to the vane and hub 204 during the brazing process.
[0019] Additionally, as the vanes 202 are inserted into the shroud 206, the tips 207 of the vanes proximate the outlet 214 rest against the second ring 504 such that the second ring 504 maintains the vanes and hub 204 in place during the brazing process. The height 514 of the second ring 504 causes the second ring 504 to rest against the tips 207 of the vanes 202, forming a consistent gap 516 between the vane tips and the shroud 206. Thus, the height 514 of the second ring 504 maintains a consistent gap 516 between the shroud 206 and the vanes 202 during the brazing process, maintaining the position of the shroud relative to the vanes and hub 204.
[0020] The heights 514 of the first ring 502 and the second ring 504 are selected to maintain a consistent gap 516 between the shroud 206 and the vanes 202. As shown in FIG. 7 , the consistent gap 516 defines a consistent gap width 520. In this embodiment, the metallurgical joining process determines the value of the consistent gap width 520. For example, in this embodiment, the brazing process requires a predetermined gap between the shroud 206 and the vanes 202 to properly join the hub 204 and the vanes to the shroud. In this embodiment, the consistent gap width 520 is approximately 0.001 inches. (0.0254mm) From about 0.006 inches (0.1524 mm) . Because the value of the consistent gap width 520 is determined by the brazing process, the consistent gap width 520 is not scaled to fit the size of the impeller 200. The consistent gap width 520 remains the same for all impeller 200 sizes for the brazing process. In alternative embodiments, the consistent gap width 520 may be any value that allows a metallurgical joining process to attach the shroud 206 and vanes 202 to the hub 204 and vanes 202. Additionally, in alternative embodiments, the consistent gap width 520 may be scaled to fit the size of the impeller 200.
[0021] In this embodiment, the brazing process is a dip brazing process. In an alternative embodiment, the brazing process is any other type of brazing process, including but not limited to a torch brazing process, a furnace brazing process, a silver brazing process, a braze welding process, a vacuum brazing process, and / or any other brazing process. The impeller 200 is suitably made of aluminum, which may form undesirable oxides with oxygen in the air during the brazing process. The dip brazing process reduces the formation of oxides by preventing air from contacting the areas of the impeller 200 that are being joined. Specifically, the impeller 200 is immersed in a bath of molten salt, which prevents air from contacting the areas of the impeller that are being joined during the dip brazing process.
[0022] FIG. 8 is a flow diagram of a method 800 for manufacturing the impeller 200. In this embodiment, the method 800 is a dip brazing process. The method 800 includes the step of joining and / or forming (802) the vanes 202 and the hub 204. As mentioned above, the vanes 202 and the hub 204 may be made as a single unit using a casting process, or may be made separately and then attached to each other using a metal joining process, such as, but not limited to, a brazing process, a welding process, a soldering process, and / or any other metal joining process. Once the vanes 202 and the hub 204 are joined together, the vanes are ready for the dip brazing process. Specifically, the method 800 includes the step of applying (804) a brazing compound or filler metal to the tip 207 and / or the inner surface 218 of the vanes 202. The brazing compound may be any mixture or compound that enables the method 800 to join the shroud 206 to the vanes 202.
[0023] Once the vanes 202 and hub 204 are joined together and a brazing compound is applied to the tips 207 and / or inner surface 218 of the vanes 202, the vanes and hub 204 are inserted (806) into the shroud 206. Specifically, the vanes 202 and hub 204 are inserted (806) such that the tips 207 of the vanes engage the rings 502 and 504, forming an interference fit between the rings and the vane tips, maintaining the position of the vanes and hub 204 relative to the shroud 206, and further maintaining a consistent gap 516 between the shroud and the vanes. Thus, the rings 502 and 504 maintain the position of the vanes 202 and hub 204 relative to the shroud 206, and maintaining a consistent gap 516 between the shroud and the vanes.
[0024] The method 800 also includes preheating (808) the assembled vanes 202, hub 204, and shroud 206 in a furnace (not shown). More specifically, the assembled vanes 202, hub 204, and shroud 206 are heated to a temperature of about 1,000° F. to about 1,100° F. to ensure a uniform temperature throughout the assembly during the dip brazing process. The assembled vanes 202, hub 204, and shroud 206 are then immersed or submerged (810) in a bath of molten salt (not shown). The molten salt acts as a solvent in contact with the brazing compound, melting the brazing compound and allowing it to flow by capillary action to the interface between the inner surface 218 and the tip 207 of the vanes 202. The molten salt may include at least one salt of beryllium, magnesium, calcium, strontium, sodium, potassium, and barium. The molten salt may also include any salt that enables a dip brazing process to join the vanes 202 and the shroud 206. The method 800 further includes removing (812) the formed impeller 200 from the molten salt bath and cleaning and / or quenching (814) the impeller 200.
[0025] The rings 502 and 504 maintain the position of the vanes 202 and hub 204 relative to the shroud 206 during method 800 and maintain a consistent gap 516 between the shroud 206 and the vanes 202. Specifically, the tips 207 of the vanes 202 engage the rings 502 and 504, forming an interference fit between the rings and the vane tips, maintaining the position of the vanes and hub 204 relative to the shroud 206 and further maintaining a consistent gap 516 between the shroud and the vanes. Thus, the rings 502 and 504 maintain the position of the vanes 202 and hub 204 relative to the shroud 206 during the preheating (808), soaking (810), and removing (812) processes, allowing the impeller 200 to be brazed together in method 800.
[0026] The described impeller includes at least one ring extending from an inner surface of the shroud to maintain a consistent gap between the shroud and the blades during manufacturing of the impeller. The consistent gap improves balance of the impeller and increases efficiency of a compressor including the impeller. An example impeller includes a hub, a plurality of blades, and a shroud. The shroud includes at least one ring to maintain a position of the shroud relative to the blades and hub during a metal bonding process. The inclusion of the ring allows a consistent gap between the blades and the shroud to be maintained throughout the metal bonding process. More specifically, the blades and hub are inserted into the shroud prior to initiation of the metal bonding process. The ring is placed on the inner surface of the shroud and the tips of the blades are pressed against the ring to form an interference or friction fit that maintains a consistent gap between the blades and the shroud throughout the metal bonding process. The consistent gap improves balance of the impeller and increases efficiency of a compressor including the impeller, and may further reduce maintenance requirements of the compressor. Additionally, the consistent gap can also reduce the porosity of the brazed joints of the impeller, which reduces resistance and friction to the fluid channeled through the impeller, increasing compressor efficiency and reducing compressor maintenance requirements. Thus, the ring increases compressor efficiency and reduces compressor maintenance requirements.
[0027] The exemplary system and method achieve better results compared to conventional systems and methods. For example, unlike known impellers that include a hub, a plurality of blades, and a shroud, the shroud of the described exemplary impeller includes at least one ring to maintain the position of the shroud relative to the blades and hub during the metal bonding process described above. The inclusion of the ring allows a consistent gap between the blades and the shroud to be maintained throughout the metal bonding process. More specifically, the blades and hub are inserted into the shroud prior to the initiation of the metal bonding process. The ring is placed on the inner surface of the shroud and the tips of the blades are pressed against the ring to form an interference or friction fit that maintains a consistent gap between the blades and the shroud throughout the metal bonding process. The consistent gap improves the balance of the impeller, which increases the efficiency of a compressor that includes the impeller, and further reduces the maintenance requirements of the compressor. Additionally, the consistent gap also reduces the porosity of the impeller brazed joint, which reduces the resistance and friction of the fluid channeled through the impeller, increasing the efficiency of the compressor and reducing the maintenance requirements of the compressor. The rings therefore increase the efficiency of the compressor and reduce the maintenance requirements of the compressor.
[0028] Exemplary embodiments of the impeller and methods of assembling the disclosed impeller are described in detail above. The systems and methods are not limited to the specific embodiments described herein, and rather, the components of the systems and methods may be used independently and separately from other components described herein. For example, the impellers described herein may be used in compressors other than HVAC compressors, such as turbocharger compressors.
[0029] When introducing elements of the present disclosure or one or more embodiments thereof, the articles "a," "an," "the," and "said" are intended to mean that there are one or more of the elements. The terms "comprising," "including," "containing," and "having" are inclusive and intended to mean that there may be additional elements other than the listed elements. The use of specific orientation terms (e.g., "top," "bottom," "side," etc.) is done for convenience of description and does not require any particular orientation of the items being described.
[0030] Because various changes may be made in the above structures and methods without departing from the scope of the present disclosure, it is intended that all matter contained in the above description and shown in the accompanying drawing or drawings shall be interpreted as illustrative and not in a limiting sense.
Claims
1. 1. A method of manufacturing a compressor impeller including a plurality of blades, a hub, and a shroud, wherein the blades each include a tip, and the shroud includes an inner surface and a first ring and a second ring each extending from the inner surface, the method comprising: attaching the vanes to the hub; applying a brazing compound to the tips of the blades or to an inner surface of the shroud, or both; inserting the vanes and the hub into the shroud such that the tips of the vanes are pressed against at least one of the first ring and the second ring to form an interference fit between at least one of the first ring and the second ring and the tips of the vanes that maintains a consistent gap between the shroud and the vanes during a brazing process; attaching the vanes to the shroud at the consistent gap using the brazing process; The method includes:
2. The method of claim 1 , wherein the position of the shroud relative to the vanes is fixed by at least one of the first ring and the second ring during the brazing process.
3. 2. The method of claim 1, wherein the step of inserting the vanes and the hub into the shroud such that tips of the vanes press against at least one of the first ring and the second ring comprises inserting the vanes and the hub into an inlet of the shroud such that tips of the vanes press against at least one of the first ring and the second ring.
4. The method of claim 1 , wherein the first ring is positioned proximate an inlet of the shroud and the second ring is positioned proximate an outlet of the shroud.
5. 5. The method of claim 4, wherein the step of inserting the vanes and the hub into the shroud so that tips of the vanes press against at least one of the first ring and the second ring comprises inserting the vanes and the hub into the shroud so that tips of the vanes proximate the inlet press against the first ring.
6. 5. The method of claim 4, wherein the step of inserting the vane and the hub into the shroud so that a tip of the vane is pressed against at least one of the first ring and the second ring comprises inserting the vane and the hub into the shroud so that a tip of the vane proximate the outlet rests against the second ring and so that the second ring maintains the vane and the hub in a predetermined position during the brazing process.
7. The method of claim 1 , wherein the step of attaching the vane to the shroud at the consistent gap using a brazing process comprises attaching the vane to the shroud at the consistent gap using a dip brazing process.
8. The method of claim 1 , wherein the first ring and the second ring each include a rounded bump including an apex, a first edge, and a second edge.
9. The method of claim 8 , wherein the first ring and the second ring each define a height between the inner surface and the apex.
10. The method of claim 9 , wherein the height is between 0.0254 millimeters and 0.1524 millimeters.
11. The method of claim 1 , wherein the consistent gap defines a consistent gap width.
12. The method of claim 11 , wherein the consistent gap width is between 0.0254 millimeters and 0.1524 millimeters.
Citation Information
Patent Citations
Method for manufacturing impeller, and impeller
JP2010174652A
Method for manufacturing impeller
JP2012102678A
Systems and methods for manufacturing a shrouded impeller
US9091277B1