Method and mold for providing a MEMS device including pyramidal protrusions

The method addresses the challenge of producing sharp, single-tip MEMS devices by using a sacrificial layer and isotropic etching, achieving efficient and cost-effective manufacturing with precise tip control.

JP7554208B2Active Publication Date: 2024-09-19SMARTTIP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021560709
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-04-12
Filing Date
2020-04-07
Publication Date
2024-09-19
Estimated Expiration
2040-04-07

AI Technical Summary

Technical Problem

Existing methods for manufacturing MEMS devices with pyramidal protrusions result in tips with two or more planes, leading to a less sharp tip geometry, which is less suitable for scanning applications, and involve time-consuming etching processes that increase manufacturing costs.

Method used

A method involving a mold with a sacrificial layer and isotropic etching to create MEMS devices with a single tip, using a polycrystalline silicon sacrificial layer and anisotropic etching to form a pyramidal tip with three wall sections, allowing for rapid production of sharp tips.

Benefits of technology

Enables the reliable and rapid manufacture of MEMS devices with sharp, single-tip protrusions, reducing manufacturing time and costs by avoiding the need to completely etch the silicon substrate, while allowing for precise control over tip shape and material properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007554208000012
    Figure 0007554208000012
  • Figure 0007554208000004
    Figure 0007554208000004
  • Figure 0007554208000009
    Figure 0007554208000009
Patent Text Reader

Abstract

A method and mold for providing a MEMS device including pyramidal protrusions is provided. [Solution] A method for providing a MEMS device, such as an AFM probe, including triangular pyramidal protrusions is performed using multiple MEMS method steps. To enable reliable, rapid, and large-scale manufacturing of such MEMS devices including three-sided protrusions with a relatively small half-cone angle and a single tip, a mold is used. The mold includes a sacrificial layer on top of a base substrate. The method for providing the MEMS device includes: providing a layer of protrusion material in an area on a first side of the mold that includes the pits; patterning the layer of protrusion material into a desired shape; and isotropically etching the sacrificial layer of the mold with an isotropic etchant that can etch the sacrificial layer to enable separation of the MEMS device from at least the base substrate of the mold. [Representative diagram] Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for providing a MEMS device including triangular pyramidal protrusions using a number of MEMS method steps. [Background technology]

[0002] In the art, methods are known for manufacturing MEMS devices that include protrusions. A typical example of this is a probe, for example a probe used for scanning. Nowadays, such probes are manufactured using a substrate <100> It is mass produced using silicon wafers and anisotropic etching.

[0003] Generally, two methods can be recognized for producing pyramidal tips: 1) Silicon chip manufacturing, whereby chips are produced by silicon etching. 2) Tip molding, a well-known nanofabrication method for producing very sharp tips, such as those used in scanning probe microscopy (SPM) field emitters, vacuum electronics, or tunneling-based devices. Tip molding consists of etching a pyramidal pit into a sacrificial substrate (typically silicon), depositing the desired thin film material onto the mold, further processing the deposited material to define other features such as a cantilever arm, and then removing the sacrificial substrate to reveal the pyramidal tip. The most common mold geometries are: <100> This is a pyramid (square pyramid) obtained by anisotropically etching a silicon wafer.

[0004] Chip molding technology has several advantages: 1) The tip material can be selected depending on the application. The material can be harder / more wear resistant than silicon. The tip material may also have different dielectric properties than silicon. The tip material can be, for example, silicon nitride, diamond, metal or polymer. 2) The cantilever properties can be better controlled: they can be smaller and / or softer cantilevers with more precisely defined stiffness (because the thickness of the shaped probes can be more easily controlled by deposition than by etching). 3) Any active components are easily integrated into the MEMS device (probe). Examples of such active components are heaters, sensors and actuators.

[0005] A drawback of the known method is that the resulting protrusion, in the shape of a pyramid containing four planes, has not one tip, but two tips (each formed by three planes) or one ridge. In other words, the pyramidal tip is not as sharp as it would be if there was only one tip. This is because the pyramidal tip has three <111> In the paper “Advances in Manufacturing of Molded Tips for Scanning Probe Microscopy” (

[2012] N. Moldovan et al in JOURNAL OF MICROELECTROMECHANICAL SYSTEMS, VOL. 21, NO. 2, APRIL 2012) which discloses the fabrication of three-sided tips by etching a Si(311) wafer to form pits defined by planes, the tips are called wedges. The tips produced using this method have a relatively large cone angle, making them less suitable for scanning purposes such as AFM probes. This problem is discussed in “Advanced Micromachining Schemed for Scanning Probe Tips” (PhD Thesis Rolf Vermeer

[2016] ) and in the paper “Fabrication of novel AFM probe with High-Aspect-Ratio Ultra-Sharp Three-Face Silicon Nitride Tips” (R. Vermeer et al in 14TH IEEE INTERNATIONAL CONFERENCE ON NANOTECHNOLOGY, IEEE, 18 August 2014, pages 229-233, XP032690978, 001: 10.11 09 / NANO.2014.6967957), which is aimed at the fabrication of triangular pyramidal tips for probes. <111> It discloses the use of silicon. This process uses dry etching to remove the substrate, which adversely affects the cost and speed of production. Summary of the Invention [Problem to be solved by the invention]

[0006] It is an object of the present invention to provide a method that allows for reliable and rapid large scale manufacture of MEMS devices that include a three-sided protrusion, the protrusion having a relatively small half-cone angle and a single tip. [Means for solving the problem]

[0007] To this end, the method according to the preamble uses a mold, said mold comprising: - defining a first side and a second side; - a base substrate, at a first side of the mold, a surface of the base substrate defining a major plane parallel to the first side, the major plane being a monocrystalline silicon <111> Defining a plane; - in a first aspect of the mold, a sacrificial layer on top of a base substrate, said sacrificial layer being selected from polycrystalline silicon and amorphous silicon; - a pit on a first side of the mold, said pit comprising: - extending through the sacrificial layer [page 3 lines 18-19 of this application as filed] into the base substrate; and - <111> includes three wall portions parallel to the crystal plane, each of the three wall portions intersecting the other two wall portions; and - including the apex of the bottom part of the pit; A method for providing a MEMS device includes: - providing a layer of protruding material in a region on a first side of the mould extending from a first subregion outside the pits to a second subregion including the apex of the pits; - patterning a layer of protruding material into a desired shape; and isotropically etching a sacrificial layer of the mold with an isotropic etchant capable of etching the sacrificial layer to separate the MEMS device from at least a base substrate of the mold; The present invention is characterized by comprising:

[0008] Thus, MEMS devices including protrusions with sharp tips can be produced.The base substrate can be used to conveniently produce a large number of MEMS devices including protrusions.

[0009] Another advantage of the method is that the device can be obtained without dissolving the entire silicon substrate, which can be achieved by: <111> Given that it is oriented silicon, this takes some time.

[0010] A typical method includes further steps for final processing of the MEMS device.

[0011] The pit extends from the first through the sacrificial layer to the base substrate.

[0012] A method for fabricating a mass storage device including a probe is known from US 2006 / 003493 A1, in which the probe comprises a cantilever having a first end region operatively connected to a substrate and a second end region rotated in an orientation opposite the first end region, where a tip is arranged on the second end region, the tip pointing in a direction opposite the first end region.

[0013] A method for producing sharp tips is known from US Patent No. 8701211 B2: the tips are formed by depositing on one or more moulds formed in a sacrificial crystalline semiconductor substrate with exposed {311} faces, which are etched by a crystal etchant to form three-sided, one or more trihedral or pyramidal moulds or one or more indentations.

[0014] According to an advantageous embodiment, the mould is prepared by subjecting an intermediate product to a number of method steps to form the mould, the intermediate product being: - defining a first side and a second side; and - a base substrate, the surface of the base substrate defining a main plane parallel to the first side of the intermediate product, the main plane being a monocrystalline silicon <111> Define a plane; The method steps include: - in a first aspect, providing a sacrificial layer of a first material on an intermediate base substrate, said first material being non-monocrystalline silicon; - providing the sacrificial layer of the intermediate product with a masking layer of a second material different from the first material; - providing the intermediate product with a blind hole extending from a first side into the base substrate; - The intermediate product is a silicon substrate layer <111> anisotropically etching the silicon using an etchant capable of etching the sacrificial layer in any direction parallel to the major surface at least as fast as the rate of anisotropic etching of the crystal planes, so as to form a pit including three pyramidal wall portions; - removing the masking layer of the second material; - providing a molding layer in the pit of the intermediate product, the molding layer forming the apex of the pit with three wall portions to form a mould. Includes.

[0015] Low Pressure Chemical Vapor Deposition (LPCVD) can be used to deposit a layer of polysilicon as a sacrificial layer. <111> It is isotropically etched by anisotropic etchants such as TMAH or KOH to etch silicon substrates.

[0016] Providing the shaped layer in the pits may include depositing the shaped layer or growing the shaped layer.

[0017] Typically, the masking layer is removed prior to the step of providing a shaping layer.

[0018] To form the blind holes, openings, typically circular openings, can be made in the masking layer. The blind holes are then made by directional etching of the multilayer stack (e.g. silicon oxide, polycrystalline silicon and monocrystalline silicon), for example in combination with reactive ion etching (RIE) and deep reactive ion etching (DRIE) to obtain blind holes with walls perpendicular to the main plane. The depth of the blind holes will later determine the height of the protrusions.

[0019] If the shaping layer is not removed when separating the MEMS device from the substrate, this step is performed to result in a MEMS device that includes a projection having a single tip.

[0020] This is a very time consuming process since the molding layer is generally relatively thin (e.g. 1 um) and has a large exposed surface area. <111> This can be accomplished relatively quickly compared to the removal of substrate in the Vermeer method (mentioned above), which requires etching along a planar surface.

[0021] In the case of silicon oxide as the molding layer, it is conveniently removed by wet etching, with a suitable etchant being buffered hydrofluoric acid (BHF).

[0022] According to an advantageous embodiment, the step of providing a shaped layer comprises growing the shaped layer.

[0023] This helps to define the tip of the final projection very sharply.

[0024] The molding layer may include silicon oxide, which is a silicon-based sacrificial layer and <111> Easily grown from silicon.

[0025] According to an advantageous embodiment, the step of subjecting the intermediate product to anisotropic etching of silicon using an etchant capable of etching the sacrificial layer in any direction parallel to the main plane, in order to form pits, comprises: <111> The method includes etching at a rate that is greater than the rate of anisotropic etching of the silicon substrate layer.

[0026] The pits formed include a tip bottom portion that extends beyond (out of) the plane defined by the pyramidal tip wall portions, in other words, a relatively wide tip bottom portion is formed, which is favorable in terms of tip strength.

[0027] According to an advantageous embodiment, after separation of the MEMS device and the mould, the moulding layer is removed by etching.

[0028] Because the shaping layer is generally relatively thin (eg, 1 um) and has a large surface area exposed, this can be accomplished relatively quickly compared to the removal of (111) in the Vermeer method (supra).

[0029] In the case of silicon oxide as the molding layer, it is conveniently removed by wet etching, the preferred etchant being buffered hydrofluoric acid (BHF).

[0030] According to an advantageous embodiment, the masking layer is selected from i) silicon nitride, and ii) silicon oxide.

[0031] Preferably, the molding layer is silicon oxide and the protrusion material is silicon nitride.Such a masking layer can be easily removed by buffered HF (BHF), leaving behind the sacrificial layer and the silicon substrate.

[0032] According to an advantageous embodiment, the layer of protruding material comprises a material selected from i) silicon nitride, and ii) diamond.

[0033] These are hard materials that are excellent for making sharp, wear-resistant projections.

[0034] According to an advantageous embodiment, the layer of projection material is formed as a stack of sub-layers, and the method includes providing a first sub-layer of a first projection material, followed by providing a second sub-layer of a second projection material different from the first projection material.

[0035] Therefore, the properties of the protrusions can be tailored to the specific requirements for the MEMS device. The first sub-layer may for example be diamond to provide a wear-resistant layer. The first sub-layer may also be metal to provide a conductive layer.

[0036] The second material may be, for example, silicon nitride to provide the tip and cantilever of the MEMS probe with desired mechanical properties not available from the first material.

[0037] According to an advantageous embodiment, the MEMS device is a probe.

[0038] This is a very important application area for the method of the present invention: the sharp tip of the protrusion allows for more accurate measurements.

[0039] Finally, the invention relates to a mould for manufacturing a MEMS device; The mold is - defining a first side and a second side; - a base substrate, at a first side of the mold, a surface of the base substrate defining a major plane parallel to the first side, the major plane being a monocrystalline silicon <111> Defining a plane; In a first aspect of the present invention, the method includes the steps of: providing a sacrificial layer on a base substrate; and the sacrificial layer is selected from polycrystalline silicon and amorphous silicon; and - a pit on a first side of the mold, said pit comprising: - extending through the sacrificial layer into the base substrate; and - <111> includes three wall portions parallel to the crystal plane, each of the three wall portions intersecting the other two wall portions; and - Includes the apex of the bottom part of the pit.

[0040] Such moulds are very useful in the method according to the invention. Generally, a wafer may contain multiple moulds and be used in the method according to the invention.

[0041] The pit extends from the first through the sacrificial layer and into the base substrate.

[0042] According to an advantageous embodiment, the sacrificial layer is at least partially covered by a shaping layer, which forms the apex of the pit.

[0043] Thus, the shape of the chip to be formed can be controlled to a greater extent than is possible with just the sacrificial layer alone, and / or the sacrificial layer can be more selective with respect to separation speed and the molding layer can be selected to better control the shape of the chip.

[0044] The present invention will now be described with reference to the drawings. [Brief description of the drawings]

[0045] [Figure 1] A cross-sectional view of a MEMS device (probe) is shown. [Figure 2A] A method for producing the probe of FIG. 1 is shown. [Figure 2B] A method for producing the probe of FIG. 1 is shown. [Figure 2C] A method for producing the probe of FIG. 1 is shown. [Figure 2D] A method for producing the probe of FIG. 1 is shown. [Figure 2E] A method for producing the probe of FIG. 1 is shown. [Figure 2F] A method for producing the probe of FIG. 1 is shown. [Figure 2G] A method for producing the probe of FIG. 1 is shown. [Figure 2H] A method for producing the probe of FIG. 1 is shown. [Figure 2I] A method for producing the probe of FIG. 1 is shown. [Figure 2J]A method for producing the probe of FIG. 1 is shown. [Figure 2K] A method for producing the probe of FIG. 1 is shown. [Figure 2L] A method for producing the probe of FIG. 1 is shown. [Figure 2M] A method for producing the probe of FIG. 1 is shown. [Figure 2N] A method for producing the probe of FIG. 1 is shown. [Diagram 3] FIG. 2C is a scanning electron microscope photograph of the tip mold portion of the tip mold of FIG. 2F. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0046] FIG. 1 shows a cross-sectional view of a MEMS device 100, where the probe 100 includes a probe body 110, a cantilever beam 120 with a proximal end 121 and a distal end 122, and a tip unit 130 at the distal end portion.

[0047] The tip unit 130 includes a tip base 131 and a pyramidal tip 132 with a tip 133. The pyramidal tip 132 is a tetrahedral tip 132, i.e., it has three sides that meet at the tip 133. The half-cone angle is 20°.

[0048] The method according to the invention will now be explained using Figures 2A to 2N, where each figure shows steps both in top view and in cross section. The method steps illustrate the manufacture of the probe 100 of Figure 1.

[0049] The manufacturing process begins with <111> A silicon wafer 210 (FIG. 2A) is used to start with the fabrication of a mold 200. Until the mold 200 is completed, the mold half-finished product is called an intermediate product 200′. The wafer 210 includes a first major side 211 and a second major side 212.

[0050] A 1 um thick polycrystalline silicon (polysilicon) sacrificial layer 220 is deposited on the wafer 210 using low pressure chemical vapor deposition (LPCVD) (FIG. 2B).

[0051] Generally, when the thickness of the polysilicon layer is selected, the way in which the shaping layer is deposited must be taken into consideration. If the shaping layer (silicon oxide) is thermally grown, the polysilicon layer will be consumed during the thermal oxidation process. The polysilicon layer must be thick enough so that after thermal oxidation, a part of the polysilicon layer remains on the wafer. A practical approach is to start with 1 um of polysilicon, and after growing a silicon oxide layer about 1 um thick by thermal oxidation, about 500 nm of polysilicon remains on the wafer. This remaining layer is then used as a sacrificial layer for the MEMS probe release.

[0052] A masking layer 230 is then deposited (FIG. 2C). This layer serves to protect the polysilicon layer during the later anisotropic wet etching of silicon. In this embodiment, silicon oxide is used as a masking layer grown on the polysilicon sacrificial layer 220 using high temperature thermal oxidation (wet oxidation at 1000° C. for 15 minutes, resulting in a SiO 2 layer of about 150 nm). An alternative method is to use LPCVD deposition to deposit the SiO 2 . Another option is to use silicon nitride as a masking layer. Both silicon oxide and silicon nitride are stable masking materials with respect to the chemical etchants used later in the anisotropic etching of silicon (e.g. with KOH or TMAH).

[0053] After patterning the circular opening by standard lithography techniques (not shown), a cylindrical hole 235 is created by directional etching of the multi-layer stack using a combination of reactive ion etching (RIE) and deep reactive ion etching (DRIE) (FIG. 2D). The dimensions of the cylindrical pit 235 (and the thickness of the shaping layer 240, described below) are what determine the height of the tip unit 130 (from the cantilever 120 to the tip 133). The base of the cylindrical pit 235 is what determines the side length of the equilateral triangle at the base of the triangle of the pyramidal tip 132. During the anisotropic etching of the silicon of the pit 235, the triangular side of the pyramidal tip 132 is the furthest. <111> It is determined when a plane is reached. When this occurs on all three sides, an equilateral triangle is formed on the chip bottom surface 131. That means that the shape of the pit 235 does not have to be perfectly cylindrical to get an equilateral triangle. <111> The angles between the planes are determined by the crystal structure of the single crystal silicon substrate. <111> The flat surface is also etched with the anisotropic etchant (albeit much slower than the otherwise rapid etching of the flat surface), so the final length of the base side of the triangle is determined not only by the initial shape of the cylindrical pit, but also by the anisotropic etch time.

[0054] After directional etching of the cylindrical pits 235, the wafer was immersed in potassium hydroxide (KOH). KOH etches polysilicon topically, i.e., with the same etch rate in all directions. On the other hand, the substrate layer 110 <111> Silicon is etched anisotopically, in which case: <111> The planar surfaces are etched much slower than other crystal planes. In this way, a tetrahedral chip unit mold 250 is formed (FIG. 2E).

[0055] The bottom portion of the chip unit mold 250 is a tetrahedral portion 250' with very smooth walls. This bottom portion of the tetrahedral is an equilateral triangle.

[0056] Polysilicon sacrificial layer <111> The simultaneous etching of silicon makes the top portion of the chip unit mold 250 wider because the etch rate of polysilicon is so fast that the etch rate of the (111) crystal plane cannot keep up with the etching rate of the substrate from the first side. <111> This is because it allows etching of silicon.

[0057] Other anisotropic etchants of silicon may be used to form the mold (eg, TMAH).

[0058] The silicon oxide of the masking layer 230 that protected the polysilicon layer 220 during the KOH etch is removed using concentrated HF (50% HF), leaving the polysilicon and <111> The silicon substrate is left behind.

[0059] A silicon oxide molding layer 240 is then provided conformally (i.e. having the same thickness whether on horizontal or inclined surface parts) by deposition, by growth or by both (FIG. 2G). The silicon oxide layer can be deposited by LPCVD (silicon oxide deposited from tetraethyl orthosilicate, so-called TEOS deposition) or grown by thermal oxidation. A combination of TEOS deposition and thermal oxidation can also be used. More information on molding can be found in Vermeer's PhD thesis (see chapter 3.3 above). The silicon oxide layer needs to be thick enough to completely fill the bottom of the bottom tip unit mold part 250' and to form the tip unit mold apex 251', thereby making it possible to obtain a sharp AFM tip 132. The mold 200 is now ready for the manufacture of MEMS devices.

[0060] After the mold 200 containing the tip unit mold 250 with sharp pits is produced, a structural layer 260 of protruding material is deposited (FIG. 2H), in this embodiment silicon nitride deposited by LPCVD to a thickness of 600 nm.

[0061] The structural layer is patterned (FIG. 2I) to create the cantilever beam 120 and the cantilever base 271 using standard contact lithography in combination with RIE.

[0062] After patterning, the silicon wafer is bonded to a pre-diced glass wafer 280 by anodic bonding (FIG. 2J).

[0063] The MEMS device now needs to be separated (ie, released) from the substrate of mold 200 .

[0064] To this end, the sacrificial polysilicon layer 220 beneath the cantilever 120 and the cantilever base 271 is removed using a wet chemical etch (25% by weight TMAH at 90° C. in this embodiment), which also etches the silicon base substrate around the tip unit 130. In this way, the entire probe is released from the substrate - i.e. most of the mold 200 is removed (FIG. 2K) - without the need to completely etch the substrate. This saves time, especially since, whether by wet or dry etching, <111> Silicon of this orientation etches slowly: to completely dissolve a 500um thick (100) silicon wafer - as is done during the fabrication of a MEMS device with a square pyramidal chip - requires approximately 8 hours of wet etching. <111> Complete removal of the silicon wafer material would take 100 times longer, and therefore on the order of 800 hours.

[0065] The released MEMS devices are still connected together because the glass substrate is not perfectly diced in some directions (not shown), as is known per se in the art, and the edges of the silicon wafer are still connected to the glass substrate (not shown), because no sacrificial silicon layer was deposited there during the manufacture of mold 200.

[0066] After release of the MEMS device from mold 200, the silicon oxide molding layer 240 is removed using buffered HF (BHF) (FIG. 2L).

[0067] In this embodiment, the MEMS probe is metallized by deposition of a metal layer 290 (we use a Ti / Au bilayer as the reflective coating. The Ti layer is an adhesion layer with a thickness of 10 nm. The gold reflective layer is 50 nm thick.) This metal layer 290 serves as a reflective layer on the cantilever beam 120 for AFM imaging.

[0068] Alternatively, such a reflective layer can be deposited earlier in the process (on top of the silicon nitride structural layer 260) by devoting more processing steps to patterning. In either case, a stack of sublayers is formed.

[0069] It is also possible to deposit a sublayer earlier in the process, for example as a first sublayer on top of shaping layer 240. This would be done, for example, if it were desired to provide a projection with a tip that is coated with a material different from the structural material of the cantilever, for example if it were desirable to have a tip that is coated with diamond.

[0070] The MEMS device 100 is now ready for use and can be removed by dicing. To reduce the risk of the cantilever breaking, a known technique is used to apply a sticky foil (UV dicing foil) to the first main side. The MEMS probes are removed by removing the foil. In this way, all MEMS probes are transferred to the foil. The stickiness of the UV foil is reduced by exposing it to UV light. After exposure, the individual MEMS probes can be collected from the foil using tweezers.

[0071] 3 is a scanning electron microscope photograph of the chip unit mold portion 250' of the chip unit mold 250 after removal of the masking layer by KOH etching (FIG. 2F), as viewed from the first major side 211 towards the second major side 212. At the center are the three chip unit mold portions 250' that define the chip unit mold portion 250'. <111> There is a flat surface and around it is a wider, uppermost portion of the chip unit mold 250. At the first major side 211, the wider, uppermost portion of the chip unit mold 250 has a (substantially) circular periphery.

Claims

1. A method of providing a MEMS device (100) including triangular pyramidal protrusions using a number of MEMS method steps; A mold (200) is used, said mold (200) comprising: - defining a first side (211) and a second side (212); - a base substrate, at said first side (211) of said mould, a surface of said base substrate defining a main plane parallel to said first side (211), said main plane defining a <111> plane of monocrystalline silicon; - at said first side of said mold (200), comprising a sacrificial layer (220) on top of said base substrate, said sacrificial layer (220) being selected from polycrystalline silicon and amorphous silicon; - said first side (211) of said mould (200) comprises a pit (235), said pit (235) comprising: - extending through the sacrificial layer (220) into the base substrate; and - comprises three wall portions parallel to the <111> crystal planes, each of the three wall portions intersecting the other two wall portions; and - including the apex (251') of the bottom part of said pit (235); The method of providing the MEMS device (100) comprises: providing a layer of projection material on said first side (211) of said mould (200) in an area extending from a first subarea outside said pits (235) to a second subarea including said apex (251') of said pits (235); - patterning said layer of protruding material into a desired shape; and isotropically etching said sacrificial layer (220) of said mold by an isotropic etchant capable of etching said sacrificial layer (220) in order to separate said MEMS device (100) from at least said base substrate of said mold (200); A method comprising:

2. The mould is prepared by subjecting an intermediate product (200') to a number of method steps to form a mould, the intermediate product (200') comprising: - defining a first side (211) and a second side (212); and - a base substrate, said surface of said base substrate defining a main plane parallel to said first side (211) of said intermediate product (200'), said main plane defining a <111> plane of monocrystalline silicon; The method steps include: providing said base substrate of said intermediate product (200') at said first side (211) with a sacrificial layer (220) of a first material, said first material being non-monocrystalline silicon; providing said sacrificial layer (220) of said intermediate product (200') with a masking layer (230) of a second material different from said first material; - providing said intermediate product (200') with a blind hole (235) extending from said first side (211) into said base substrate; - subjecting said intermediate product (200') to anisotropic etching of said silicon using an etchant capable of etching said sacrificial layer (220) in any direction parallel to said main surface at least as fast as the rate of anisotropic etching of said <111> crystallographic planes of said silicon substrate layer (110), so as to form a pit (235) comprising three pyramidal wall portions; - removing said masking layer (230) of said second material, providing a molding layer (240) in said pit (235) of said intermediate product (200'), said molding layer (240) forming an apex (251') of said pit (235) bounded by said three wall portions to form said mould; The method of claim 1 , comprising:

3. The method of claim 2 , wherein the step of providing the shaped layer (240) comprises growing the shaped layer (240).

4. 4. The method of claim 2 or 3, wherein the step of subjecting the intermediate product (200') to anisotropic etching of the silicon using an etchant capable of etching the sacrificial layer (220) in any direction parallel to the major surface comprises etching at a rate that exceeds a rate of anisotropic etching of the <111> silicon substrate layer (110) to form the pits (235).

5. The method according to any one of claims 2 to 4, wherein after separation of the MEMS device (100) and the mould (200), the shaping layer (240) is removed by etching.

6. The method of any one of claims 2 to 5, wherein the masking layer (230) is selected from i) silicon nitride, and ii) silicon oxide.

7. A method according to any preceding claim, wherein the layer of protrusion material comprises a material selected from i) silicon nitride, and ii) diamond.

8. 8. The method of claim 1, wherein the layer of protrusion material is formed as a stack of sub-layers, the method comprising providing a first sub-layer of a first protrusion material, followed by providing a second sub-layer of a second protrusion material different from the first protrusion material.

9. The method of any one of claims 1 to 8, wherein the MEMS device (100) is a probe (100).

10. A mold (200) for manufacturing a MEMS device, comprising: The mold (200) is - defining a first side (211) and a second side (212); - a base substrate, at said first side (211) of said mould (200), said base substrate comprising a surface defining a main plane parallel to said first side (211), said main plane defining a <111> plane of monocrystalline silicon; the first side of the mold (200) comprises a sacrificial layer (220) on top of the base substrate, the sacrificial layer (220) being selected from polycrystalline silicon and amorphous silicon; and - said first side (211) of said mould (200) comprises a pit (235), said pit (235) comprising: - extending through the sacrificial layer (220) into the base substrate; and - comprises three wall portions parallel to the <111> crystal planes, each of the three wall portions intersecting the other two wall portions; and a mould (200), characterised in that it includes an apex (251') of the bottom part of said pit (235).

11. 11. The mold (200) of claim 10, wherein the sacrificial layer (220) is at least partially covered by a molding layer (240), the molding layer (240) forming the apexes (251') of the pits (235).

Citation Information

Patent Citations

  • Cantilever incorporating film type displacement sensor

    JP1995035540A

  • Semiconductor device and method of manufacturing the same

    JP2011038780A

  • A method for fabricating three-dimensional nanostructures having nanosubstructures, and a method for fabricating insulating pyramids with metal tips, pyramids with nanoapertures, and pyramids with horizontal and / or vertical nanowires that can be obtained by this method.

    JP2011511270A

  • Nucleation control of diamond films by microlithographic patterning

    US5242711A