Temperature control mold, resin container manufacturing device and manufacturing method

The temperature adjustment mold with an axially extending rod and annular protrusions addresses the issue of axial temperature control in hot parison blow molding, enhancing wall thickness distribution and reducing shrinkage and deformation in resin containers.

JP7554902B2Active Publication Date: 2024-09-20NISSEI ASB MASCH CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023502443
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-02-25
Filing Date
2022-02-22
Publication Date
2024-09-20
Estimated Expiration
2042-02-22

AI Technical Summary

Technical Problem

Conventional temperature adjustment methods for hot parison blow molding fail to provide adequate temperature control in the axial direction, leading to difficulties in improving wall thickness distribution and controlling shrinkage and deformation of resin containers.

Method used

A temperature adjustment mold with a rod portion that extends axially and features annular protrusions to contact the preform's inner surface, allowing for localized temperature adjustment in the axial direction while restricting radial contraction, using a protrusion to adjust the temperature at predetermined portions.

Benefits of technology

Enables localized temperature control in the axial direction, improving wall thickness distribution and reducing shrinkage and deformation of resin containers during the blow molding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007554902000007
    Figure 0007554902000007
  • Figure 0007554902000001
    Figure 0007554902000001
  • Figure 0007554902000004
    Figure 0007554902000004
Patent Text Reader

Abstract

[Problem] Provided is a temperature adjustment mold capable of locally adjusting the temperature, from the inside of a preform in the axial direction while controlling contraction deformation of the preform. [Solution] This temperature adjustment mold for adjusting the temperature of a resin preform which has been obtained by injection molding and has a bottomed shape is inserted into the inside of the preform and comprises a rod part extending in the axial direction of the preform. The rod part has an annular protrusion that protrudes in the radial direction of the rod part and makes contact with the inner peripheral surface of the preform. The rod part makes contact with the bottom part of the preform and controls axial contraction of the preform. The protrusion controls radial contraction of the preform and also propagates heat between the rod part and the preform to adjust the temperature at a predetermined part in the axial direction of the preform.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a temperature adjusting mold, and an apparatus and method for manufacturing a resin container. [Background technology]

[0002] A hot parison type blow molding machine has been known as one of the conventional manufacturing devices for resin containers. The hot parison type blow molding machine is configured to blow mold a resin container by utilizing the heat retained during injection molding of a preform, and is advantageous in that it can manufacture a variety of resin containers with excellent aesthetic appearance compared to the cold parison type.

[0003] Generally, the preform immediately after injection molding does not have a temperature distribution suitable for forming a container, so in the hot parison blow molding cycle, a temperature adjustment process of the preform is performed between the injection molding process and the blow molding process in order to suppress temperature deviation of the preform or to give the preform a desired temperature distribution suitable for forming a container.

[0004] In this type of temperature adjustment process, the preform is molded to match the internal shape of the preform. temperature adjustment The rod mold is inserted inside the preform and the inner peripheral surface of the preform is temperature adjustment Temperature control may be performed by placing a rod mold in close contact. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent No. 3330677 [Patent Document 2] Patent No. 3255485 Summary of the Invention [Problem to be solved by the invention]

[0006] Conventional temperature adjustmentThe rod type is not suitable for temperature control by applying a temperature difference in the axial direction because it is in close contact with the inner peripheral surface of the preform, and therefore, for example, it is difficult to locally cool the area corresponding to the thin-walled part of the container from inside the preform while restricting the shrinkage deformation of the preform and improving the thickness distribution of the container. [Means for solving the problem]

[0007] One aspect of the present invention is a temperature control mold for controlling the temperature of an injection-molded resin preform having a bottom. The temperature control mold includes a rod portion that is inserted into the interior of the preform and extends in the axial direction of the preform. The rod portion has an annular protrusion that protrudes in the radial direction of the rod portion and contacts the inner peripheral surface of the preform. The rod portion contacts the bottom of the preform to restrict contraction of the preform in the axial direction. The protrusion restricts contraction of the preform in the radial direction, and also conducts heat between the rod portion and the preform to adjust the temperature at a predetermined location in the axial direction of the preform. Moreover, the position of the protrusion in the axial direction is adjustable. Effect of the Invention

[0008] According to one aspect of the present invention, it is possible to locally adjust the temperature in the axial direction from inside the preform while restricting shrinkage and deformation of the preform. [Brief description of the drawings]

[0009] [Figure 1] 1 is a diagram showing a schematic configuration of a blow molding device according to an embodiment of the present invention; [Diagram 2] FIG. 4 is a vertical cross-sectional view showing a configuration example of a temperature adjustment unit. [Diagram 3] 4 is a cross-sectional view of the temperature adjusting portion near a protrusion. FIG. [Figure 4] FIG. 3 is a diagram showing a modification of FIG. 2. [Diagram 5] FIG. 5 is a diagram showing a modification of FIG. [Figure 6] FIG. 3 is a diagram showing another modified example of FIG. 2. [Figure 7]1 is a flow chart showing steps of a blow molding method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the embodiments, in order to make the description easier to understand, structures and elements other than the main parts of the present invention will be described in a simplified or omitted manner. In addition, in the drawings, the same elements are given the same reference numerals. Note that the shapes, dimensions, etc. of each element shown in the drawings are shown only for illustrative purposes, and do not represent the actual shapes, dimensions, etc.

[0011] 1 is a diagram showing a schematic configuration of a blow molding apparatus 20 according to the present embodiment. The blow molding apparatus 20 according to the present embodiment is an apparatus of the hot parison type (also called one-stage type) that blow molds a container by utilizing the heat (internal heat) retained during injection molding without cooling the preform 10 to room temperature.

[0012] The blow molding apparatus 20 includes an injection molding section 21, a temperature adjustment section 22, a blow molding section 23, a removal section 24, and a conveying mechanism 26. The injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24 are disposed at positions rotated a predetermined angle (e.g., 90 degrees) around the conveying mechanism 26.

[0013] (Transport mechanism 26) The conveying mechanism 26 includes a transfer plate 28 (not shown in FIG. 1) that moves so as to rotate around an axis perpendicular to the plane of the drawing in FIG. 1. At least one neck mold 27 (not shown in FIG. 1) that holds the neck of the preform 10 or a resin container (hereinafter simply referred to as a container) is arranged at each predetermined angle on the transfer plate 28. The conveying mechanism 26 conveys the preform 10 (or the container) whose neck is held by the neck mold 27 to the injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24 in this order by moving the transfer plate 28 by 90 degrees at a time. The conveying mechanism 26 further includes a lifting mechanism (vertical mold opening / closing mechanism) and a mold opening mechanism for the neck mold 27, and performs an operation of lifting and lowering the transfer plate 28 and an operation related to mold closing and mold opening (mold release) in the injection molding section 21, etc.

[0014] (Injection molding section 21) The injection molding section 21 includes an injection cavity mold and an injection core mold, both of which are not shown, and manufactures the preform 10 shown in Fig. 2. An injection device 25 that supplies a resin material, which is a raw material of the preform 10, is connected to the injection molding section 21.

[0015] In the injection molding section 21, the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26 are closed to form a mold space having a preform shape. Then, a resin material is poured from an injection device 25 into the mold space having the preform shape, whereby the preform 10 is manufactured in the injection molding section 21. For example, the overall shape of the preform 10 is a cylindrical shape with one end open and the other end closed at a bottom. A neck is formed at the end of the open side of the preform 10.

[0016] The material of the container and the preform 10 is a thermoplastic synthetic resin, and can be appropriately selected according to the application of the container. Specific types of materials include, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexane dimethylene terephthalate), Tritan (Tritan (registered trademark): a copolyester manufactured by Eastman Chemical Co.), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyethersulfone), PPSU (polyphenylsulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: acrylic), PLA (polylactic acid), and the like.

[0017] Incidentally, even when the injection molding section 21 is opened, the neck mold 27 of the transport mechanism 26 is not opened, but continues to hold and transport the preforms 10. The number of preforms 10 simultaneously molded in the injection molding section 21 (i.e., the number of containers that can be simultaneously molded by the blow molding device 20) can be set appropriately.

[0018] (Temperature adjustment section 22) Temperature adjustment section 22 equalizes the temperature of preform 10 manufactured in injection molding section 21 and removes temperature deviations, and adjusts the temperature of preform 10 to a temperature suitable for blow molding (for example, about 90°C to 105°C) and a temperature distribution suitable for the container shape to be molded. Temperature adjustment section 22 also has the function of cooling preform 10 in a high temperature state after injection molding.

[0019] 2 is a vertical cross-sectional view showing a configuration example of the temperature adjustment unit 22. The temperature adjustment unit 22 includes a cavity mold (temperature adjustment pot mold, heating pot mold) 31 capable of accommodating the preform 10, and a temperature adjustment rod 32 which is a mold member inserted inside the preform.

[0020] Cavity mold 31 has a space for adjusting temperature, which has approximately the same shape as the outer shape of preform 10 produced in injection molding section 21. Cavity mold 31 is divided into at least three in the axial direction of preform 10, and includes upper mold 31a, middle mold 31b, and lower mold 31c.

[0021] The upper die 31a is a die facing (opposing) the outer circumferential surface near the neck of the preform 10. The middle die 31b is a die facing the outer circumferential surface of the body of the preform 10. The lower die 31c is a die facing the outer circumferential surface of the bottom of the preform 10. The bottom surface of the upper die 31a and the top surface of the middle die 31b, as well as the bottom surface of the middle die 31b and the top surface of the lower die 31c, are engaged with each other in a spigot structure, for example, with a heat insulating member sandwiched between them.

[0022] The upper mold 31a, the middle mold 31b, and the lower mold 31c of the cavity mold 31 are each fitted with a heating member (not shown) such as a band heater (ring-shaped heater) or a rod-shaped heater. The upper mold 31a, the middle mold 31b, and the lower mold 31c are each kept at a predetermined temperature by the heating member. The temperature of the preform 10 is adjusted by heating the outer periphery of the preform 10 with heat from the cavity mold 31. The body of the heated preform 10 shrinks and deforms toward the inner diameter side and the neck side. The temperature distribution in the axial direction of the preform 10 can also be changed by changing the temperature of the heating members of the upper mold 31a, the middle mold 31b, and the lower mold 31c.

[0023] The temperature adjustment rod 32 is an example of a rod portion (rod member) and is configured to be movable axially (up and down in the figure) relative to the neck mold 27 that holds the preform 10 in the temperature adjustment unit 22. Fig. 2 shows a state in which the temperature adjustment rod 32 has been moved (lowered) downward in the figure by a rod drive mechanism (not shown) and inserted into the neck mold 27 and the preform 10.

[0024] The diameter of the temperature adjustment rod 32 is set to a dimension smaller than the inner diameter of the preform 10. In addition, the tip of the temperature adjustment rod 32 inserted inside the preform 10 contacts the bottom of the preform 10. The axial length of the temperature adjustment rod 32 is set to a length that assumes the amount of shrinkage of the preform 10 from when it is carried out from the injection molding section 21 until the temperature adjustment rod 32 is inserted. Thereby, the temperature adjustment rod 32 has the function of maintaining the axial length of the preform 10 at a predetermined dimension during temperature adjustment and restricting excessive shrinkage of the preform 10.

[0025] In addition, a flow path (not shown) through which a temperature adjustment medium flows along the axial direction is formed inside the temperature adjustment rod 32. Therefore, the temperature adjustment rod 32 is maintained at a predetermined temperature by the temperature adjustment medium flowing inside. In this embodiment, temperature adjustment Although a case will be described in which the rod 32 is set at a temperature lower than the preform 10 and the preform 10 is cooled by the temperature adjustment rod 32, it is also possible to heat the preform 10 by the temperature adjustment rod 32.

[0026] Moreover, the temperature adjustment rod 32 has an annular protrusion 33 that protrudes radially outward. Fig. 3 is a cross-sectional view of the vicinity of the protrusion of the temperature adjustment part 22. Note that in Fig. 3 as well, the flow path inside the temperature adjustment rod 32 is omitted from illustration. The protrusion 33 shown in Figures 2 and 3 is detachable from the temperature adjustment rod 32 and is composed of a pair of half-ring bodies 34 made of a material with good thermal conductivity. The half-ring body 34 has an annular large-diameter part (protrusion 33) on the outer periphery, and the mounting position can be adjusted in the axial direction of the temperature adjustment rod 32. The pair of half-ring bodies 34 (protrusions 33) are fixed by fixing means (not shown). temperature adjustment It is fixed to the rod 32 .

[0027] The protrusions 33 have the function of contacting a specific portion of the preform 10 in the axial direction from the inside and adjusting the temperature of the specific portion. At the portion of the inside of the preform 10 that comes into contact with the protrusions 33, heat is conducted between the temperature adjustment rod 32 via the protrusions 33. On the other hand, at the portion of the inside of the preform 10 that does not come into contact with the protrusions 33, the heat of the temperature adjustment rod 32 is not easily conducted because air is present between the temperature adjustment rod 32 and the preform 10. Therefore, it is possible to adjust the temperature distribution in the axial direction of the preform 10 at the position of the protrusions 33.

[0028] Furthermore, as described above, the protrusions 33 come into contact with the inner circumference of the preform 10, so that the preform 10 is less likely to shrink toward the inner diameter side of the protrusions 33. Therefore, the protrusions 33 also function to maintain the radial dimension of the preform 10 during temperature adjustment and to restrict excessive shrinkage of the preform 10.

[0029] In addition, the outer diameter of the protrusion 33 is appropriately set in consideration of the temperature adjustment time by the protrusion 33 according to the shrinkage amount of the preform 10. When the outer diameter of the protrusion 33 is increased, the shrinking preform 10 and the protrusion 33 come into contact relatively early, and the temperature adjustment time by contact with the protrusion 33 becomes longer. On the other hand, when the outer diameter of the protrusion 33 is decreased, the contact between the shrinking preform 10 and the protrusion 33 becomes slower than when the outer diameter of the protrusion 33 is large, and the above-mentioned temperature adjustment time becomes shorter. Therefore, by adjusting the outer diameter of the protrusion 33, the contact time between the predetermined part of the preform 10 and the protrusion 33 changes, and it is possible to adjust the temperature adjustment time for the predetermined part of the preform 10. The above adjustment can be performed, for example, by preparing multiple types of half-split ring bodies 34 with different outer diameters of the protrusion 33 and appropriately replacing the half-split ring bodies 34 according to the specifications such as the container shape to be manufactured and the material of the preform 10.

[0030] 2 shows an example in which the protrusion 33 is disposed at the axial middle portion of the temperature adjustment rod 32, and cools the corresponding portion of the preform 10 that forms the shoulder of the container. By locally cooling the portion of the preform 10 that corresponds to the shoulder of the container and reducing the retained heat, the thickness of the shoulder of the container can be increased during blow molding, and the thickness distribution of the container can be improved.

[0031] Fig. 4 is a modified example of Fig. 2, and shows an example in which the vicinity of the boundary between the neck mold 27 and the upper mold 31a (corresponding area under the neck of the preform 10) is cooled by a protrusion 33. In Fig. 4, as in the example of Fig. 2, the protrusion 33 is formed of a pair of half-split ring bodies 34. According to the example of Fig. 4, by locally cooling the area under the neck to reduce the fluidity of the resin in that area, it is possible to suppress the generation of burrs in the gap between the neck mold 27 and the upper mold 31a or between the neck mold 27 and the upper surface of the blow mold.

[0032] Fig. 5 is a modified example of Fig. 4, and shows an example in which a protrusion 33 is integrally formed with a temperature adjustment rod 32 at a position below the neck. The example of Fig. 5 can also achieve the same effect as that of Fig. 4.

[0033] Fig. 6 shows another modified example of Fig. 2, in which an annular contact ring 35 constituting the protrusion 33 and a cylindrical spacer 36 are placed over the temperature adjustment rod 32. Note that the structure and function of the cavity mold 31 in Fig. 6 are similar to those in Figs. 2 to 5, and therefore a duplicated description will be omitted.

[0034] The inner diameters of the annular contact ring 35 and the cylindrical spacer 36 are each set to a dimension that allows the temperature adjustment rod 32 to be inserted therethrough. At least one contact ring 35 and at least one (more preferably two or more) spacers 36 are inserted into the temperature adjustment rod 32 and are arranged concentrically on the outer periphery of the rod body 32b of the temperature adjustment rod 32. Note that FIG. 6 shows an example in which two each of the contact rings 35 and spacers 36 are attached to the temperature adjustment rod 32.

[0035] The outer diameter of the contact ring 35 is set to be larger than the outer diameter of the spacer 36. The contact ring 35 attached to the temperature control rod 32 protrudes outward from the spacer 36 and comes into contact with the inside of the preform 10, and dissipates heat from the preform 10. temperature adjustment The heat is conducted to the rod 32. Therefore, the contact ring 35 fulfills the function of the protrusion 33 that contacts a specific portion of the preform 10 in the axial direction from the inside and adjusts (cools) the temperature of the specific portion.

[0036] The spacer 36 is attached to the temperature adjustment rod 32 to position the contact ring 35 in the axial direction. The spacer 36 does not come into contact with the preform 10, and serves to form an air layer between the spacer 36 and the inner periphery of the preform 10. In this manner, the temperature distribution in the axial direction of the preform 10 can be adjusted by the position of the contact ring 35.

[0037] The temperature adjustment rod 32 also has a tip piece 32a. The tip piece 32a has a larger diameter than the rod body 32b, and is detachable from the tip of the rod body 32b. The contact ring 35 and the spacer 36 are inserted into the rod body 32b with the tip piece 32a removed. The tip piece 32a is attached to the tip of the rod body 32b after the contact ring 35 and the spacer 36 are inserted into the rod body 32b, and prevents the contact ring 35 and the spacer 36 from coming off. More specifically, temperature adjustment After the stepped portion at the lower end (tip) of the rod 32 is accommodated in the recess at the upper end of the tip piece 32a, temperature adjustment A locking pin (not shown) is inserted into the through holes formed in the rod 32 and the tip piece, respectively, to prevent the contact ring 35 and the spacer 36 from coming off. The spacer 36 and the tip piece 32a hold the contact ring 35 (projection 33) together. temperature adjustment It functions as a fixing means for fixing to the rod 32.

[0038] The example of Fig. 6 can also provide the same effect as that of Fig. 2. In the example of Fig. 6, the outer diameter and number of contact rings 35 and the axial position of contact rings 36 defined by spacers 36 can be changed as appropriate by replacing contact rings 35 and spacers 36.

[0039] (Blow molding section 23) Returning to FIG. 1, the blow molding section 23 performs stretch blow molding on the preform 10 whose temperature has been adjusted in the temperature adjustment section 22, to manufacture a container. The blow molding section 23 includes a blow cavity mold, which is a pair of split molds corresponding to the shape of the container, a bottom mold, a stretching rod, and an air introduction member (blow core mold, neither of which are shown). The blow molding section 23 blow molds the preform 10 while stretching it. This allows the preform 10 to be shaped into the shape of the blow cavity mold to manufacture a container.

[0040] (Removal part 24) The removal section 24 is configured to release the neck of the container manufactured in the blow molding section 23 from the neck mold 27 and remove the container to the outside of the blow molding apparatus 20.

[0041] (Explanation of the blow molding method) Next, a blow molding method using the blow molding apparatus 20 of this embodiment will be described. 7 is a flow chart showing the steps of the blow molding method. In this embodiment, a mold adjustment step (S100) is carried out before each of the steps (S101 to S104) of the blow molding method, which will be described later, is carried out.

[0042] (Step S100: Mold adjustment process) The mold adjustment step is a step of adjusting the position of the protrusion 33 of the temperature adjustment rod 32 according to the shape of the container to be formed, etc. As an example, the following operations are performed in the mold adjustment step.

[0043] First, the blow molding device 20 is test-operated to obtain information on the container shape before adjustment. Next, based on the information on the container shape, the axial position of the protrusion 33 of the temperature adjustment rod 32 is adjusted. At this time, the temperature adjustment time by the temperature adjustment rod 32 may be changed by changing the outer diameter of the protrusion 33 by changing parts or the like.

[0044] For example, when there is a thin-walled portion in the axial direction of the container, the worker adjusts the position of the protrusion 33 of the temperature adjustment rod 32 so that the portion of the preform 10 corresponding to the thin-walled portion of the container comes into contact with the protrusion 33. As a result, the portion of the preform 10 corresponding to the thin-walled portion of the container comes into contact with the protrusion 33 and is locally cooled, improving the thickness distribution of the container after adjustment. Also, for example, if burrs occur under the neck of the container, the worker adjusts the temperature adjustment rod 32 so that the protrusion 33 is located near the boundary between the neck mold 27 and the upper mold 31a (corresponding to the area under the neck of the preform 10). This locally cools the area under the neck of the preform 10, suppressing the occurrence of burrs under the neck of the container.

[0045] Once the above mold adjustment process is completed, the following steps of the blow molding cycle are carried out.

[0046] (Step S101: Injection molding process) In step S101, in the injection molding section 21, resin is injected from the injection device 25 into a preform-shaped mold space formed by the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26, and the preform 10 is manufactured.

[0047] In step S101, when the injection molding of the preform 10 is completed, the injection molding section 21 is opened and the preform 10 is released from the injection cavity mold and the injection core mold. Next, the transfer plate 28 of the transfer mechanism 26 moves so as to rotate by a predetermined angle, and the preform 10 held by the neck mold 27 is transferred to the temperature adjustment section 22.

[0048] (Step S102: Temperature adjustment process) Next, in the temperature adjusting section 22, temperature adjustment is performed to bring the temperature of the preform 10 close to a temperature suitable for the final blow.

[0049] In the temperature adjustment step, the transfer plate 28 is lowered so that the preform 10 held by the neck mold 27 is accommodated in the cavity mold 31. In addition, the temperature adjustment rod 32 is inserted into the preform 10 by being lowered.

[0050] In the temperature adjustment section 22, the preform 10 is heated from the outside in a non-contact manner by the cavity mold 31. This adjusts the temperature of the preform 10 so that it does not fall below a temperature suitable for blow molding, and also reduces temperature deviations that occur during injection molding. In addition, the inner circumferential surface of the preform 10 comes into contact with the protrusions of the temperature adjustment rod 32 due to contraction of the preform 10, so that a specified portion of the preform 10 is locally cooled.

[0051] After the temperature adjustment step, the transfer plate 28 of the conveying mechanism 26 moves so as to rotate by a predetermined angle, and the preform 10 after temperature adjustment held by the neck mold 27 is conveyed to the blow molding section 23 .

[0052] (Step S103: Blow molding process) Next, in the blow molding section 23, the container is blow molded. First, the blow cavity mold is closed to accommodate the preform 10 in the mold space, and the air introduction member (blow core) is lowered to bring the air introduction member into contact with the neck of the preform 10. Then, the stretch rod (vertical axis stretching member) is lowered to hold the bottom of the preform 10 from the inside, and while performing vertical axis stretching as necessary, blow air is supplied from the air introduction member to horizontally stretch the preform 10. As a result, the preform 10 is shaped by expanding so as to fit closely into the mold space of the blow cavity mold, and is blow molded into a container. Note that the bottom mold waits at a lower position where it does not come into contact with the bottom of the preform 10 before the blow cavity mold is closed, and quickly rises to the molding position before or after the mold is closed.

[0053] (Step S104: container removal process) When the blow molding is completed, the blow cavity mold and the bottom mold are opened, so that the container can be removed from the blow molding section 23. Next, the transfer plate 28 of the conveying mechanism 26 moves so as to rotate a predetermined angle, and the container is conveyed to the removal section 24. In the removal section 24, the neck of the container is released from the neck mold 27, and the container is removed to the outside of the blow molding apparatus 20.

[0054] This completes the series of steps in the blow molding cycle. Thereafter, the transfer plate 28 of the conveying mechanism 26 is moved so as to rotate by a predetermined angle, and the above steps S101 to S104 are repeated. When the blow molding apparatus 20 is in operation, four sets of containers are produced in parallel, with a time difference between each step.

[0055] The effects of this embodiment will be described below. The temperature adjustment rod 32 of this embodiment has an annular protrusion 33 that protrudes in the radial direction and comes into contact with the inner peripheral surface of the preform 10. The protrusion 33 conducts heat between the temperature adjustment rod 32 and the preform 10. As a result, in this embodiment, it is possible to adjust the temperature by cooling a specific portion of the preform 10 in the axial direction from the inside with the protrusion 33, and it is possible to improve the wall thickness distribution of the blow-molded container.

[0056] Furthermore, the tip of the temperature adjustment rod 32 comes into contact with the bottom of the preform 10 to restrict axial contraction of the preform 10. The protrusion 33 comes into contact with the inner peripheral surface of the preform 10 to restrict radial contraction of the preform 10. This suppresses variation in the shape of the preform 10 during temperature adjustment, making it easy to provide an appropriate temperature distribution to the preform 10 in each blow molding cycle.

[0057] Furthermore, the protrusion 33 in this embodiment is provided on the half-split ring body 34 or the contact ring 35 which is detachable from the temperature adjustment rod 32, and the axial position can be adjusted. This makes it possible to easily adjust the position where the temperature of the preform 10 is adjusted according to the specifications of the container, etc. In addition, the radial protrusion amount of the protrusion 33 can be changed by replacing the half ring body 34 or the contact ring 35. This changes the timing at which the protrusion 33 comes into contact with the shrinking preform 10, and thereby makes it possible to adjust the temperature adjustment time by the protrusion 33.

[0058] Here, when the material of the preform 10 is polyethylene (PE) or high density polyethylene (HDPE), the thermal shrinkage rate is higher than that of PET, etc., and the preform 10 is easily deformed by shrinkage during temperature adjustment. Moreover, it is known that these materials do not have strain hardening characteristics compared to PET, etc., and it is difficult to adjust the wall thickness during blow molding. The strain hardening characteristic is a characteristic in which the weakest part of the preform (usually the hottest part) first reaches the yield point during the blow process, and then the weak part begins to stretch, increasing its strength through molecular orientation until the wall thickness becomes uniform. Therefore, when blow molding a PE or HDPE preform, it is very important to appropriately adjust the temperature before blowing while suppressing the shrinkage deformation of the preform. According to this embodiment, it is easy to adjust the temperature of the preform suitable for molding a PE or HDPE container.

[0059] The present invention is not limited to the above-described embodiment, and various improvements and design changes may be made without departing from the spirit of the present invention. For example, in the above embodiment, a plurality of protrusions 33 may be provided in the axial direction of the temperature adjustment rod 32 .

[0060] In addition, the embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0061] Reference Signs List 10: preform, 20: blow molding device, 21: injection molding section, 22: temperature adjustment section, 23: blow molding section, 31: cavity mold, 32: temperature adjustment rod, 33: protrusion, 34: half ring body

Claims

1. A temperature control mold for controlling the temperature of an injection-molded resin preform having a bottom, A rod portion is inserted into the preform and extends in an axial direction of the preform, The rod portion has an annular protrusion portion that protrudes in a radial direction of the rod portion and contacts an inner peripheral surface of the preform, the rod portion contacts a bottom portion of the preform to restrict axial contraction of the preform; the protrusion portion restricts radial contraction of the preform and conducts heat between the rod portion and the preform to adjust the temperature at a predetermined portion of the preform in the axial direction; The position of the protrusion in the axial direction is adjustable. Mold for temperature adjustment.

2. The protrusion is detachable from the rod. The temperature regulating mold according to claim 1 .

3. The preform is further provided with a cavity mold for accommodating the preform and heating the preform from its outer periphery. The temperature regulating mold according to claim 1 or 2.

4. an injection molding unit that injection molds a resin preform having a bottom; A temperature adjusting unit that adjusts a temperature distribution in an axial direction of the preform containing the heat retained during injection molding by using the temperature adjusting mold according to any one of claims 1 to 3; a blow molding section for producing a resin container by blow molding the temperature-controlled preform; A resin container manufacturing apparatus comprising:

5. An injection molding process of injection molding a resin preform having a bottom; a temperature adjustment step of adjusting an axial temperature distribution of the preform containing the heat retained during injection molding using the temperature adjustment mold according to any one of claims 1 to 3; a blow molding step of producing a resin container by blow molding the temperature-controlled preform; A method for producing a resin container having the above structure.

Citation Information

Patent Citations

  • JP1973074562A

  • Shinchofukikomiseikeiyoparisonnokanetsuhoho

    JP1976077661A

  • Molding method for deformed hollow container

    JP1990086424A

  • Method and device for molding

    JP1994344427A

  • blow molding machine

    JP3255485B2