Simulation method, simulation device, film forming device, article manufacturing method, and program

The simulation method and device address the challenges of uniform film thickness and air bubbles in curable compositions by predicting and adjusting droplet behavior, enhancing film formation efficiency and reducing defects.

JP7555750B2Active Publication Date: 2024-09-25CANON KK
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2020128506
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-07-29
Publication Date
2024-09-25
Estimated Expiration
2040-07-29

AI Technical Summary

Technical Problem

Existing film forming technologies face challenges in achieving uniform thickness and preventing air bubbles in curable compositions, requiring extensive trial and error for optimal mold pressing conditions, which is time-consuming and costly.

Method used

A simulation method and device that predict the behavior of curable compositions during film formation by simulating the interaction between droplets and a mold, detecting abnormalities such as air bubbles, and adjusting droplet arrangements to minimize defects.

Benefits of technology

Enables efficient detection and prevention of abnormalities in film formation, reducing defects and simplifying the setup process by providing real-time visualization and adjustment of droplet patterns.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555750000006
    Figure 0007555750000006
  • Figure 0007555750000007
    Figure 0007555750000007
  • Figure 0007555750000008
    Figure 0007555750000008
Patent Text Reader

Abstract

To provide a technique advantageous in detecting an abnormality in a behavior of a curable composition in a process of forming a film of the curable composition.SOLUTION: Provided is a simulation method of predicting a behavior of a curable composition in a process of bringing a plurality of droplets of the curable composition arranged on a first member into contact with a second member and forming a film of the curable composition in a space between the first member and the second member. The simulation method includes: for each of the plurality of droplets of the curable composition, a first step of obtaining, on the basis of whether the droplet merges with an adjacent droplet, an evaluation value for evaluating a relationship regarding a degree of merging with the adjacent droplet; and a second step of displaying, together with information indicating a state of the droplet corresponding to the evaluation value, the evaluation value obtained in the first step.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a simulation method, a simulation device, a film forming device, an article manufacturing method, and a program. [Background technology]

[0002] There is a film-forming technique in which a curable composition is placed on a substrate, the curable composition is brought into contact with a mold, and the curable composition is cured to form a film made of the curable composition on the substrate. Such a film-forming technique is applied to an imprinting technique or a planarization technique. In the imprinting technique, a mold having a pattern is used, and the curable composition on the substrate is brought into contact with the pattern of the mold, and the curable composition is cured, thereby transferring the pattern of the mold to the curable composition on the substrate. In the planarization technique, a mold having a flat surface is used, and the curable composition on the substrate is brought into contact with the flat surface, and the curable composition is cured to form a film having a flat upper surface.

[0003] The curable composition is placed in the form of droplets on the substrate, and then the mold is pressed against the droplets of the curable composition. As a result, the droplets of the curable composition on the substrate spread to form a film of the curable composition. At this time, it is important to form a film of the curable composition with a uniform thickness and to ensure that no air bubbles remain in the film. In order to achieve this, the arrangement of the droplets of the curable composition and the method and conditions for pressing the mold against the curable composition are adjusted. To achieve such adjustments by trial and error using an apparatus, it requires a huge amount of time and money. Therefore, there is a need for the development of a simulator that supports such adjustments.

[0004] Patent Document 1 discloses a simulation method for predicting the wetting, spreading and coalescence (joining of droplets) of multiple droplets arranged on a pattern formation surface, and a method for generating a droplet arrangement pattern using the simulation method. Patent Document 1 also discloses calculating the droplet height distribution for the generated droplet arrangement pattern, and adjusting the droplet arrangement so that the droplet height distribution falls within a predetermined range.

[0005] On the other hand, in the imprint process, it is necessary to grasp the amount of air bubbles trapped between the droplets of the curable composition, because in a location where there are many air bubbles trapped between the droplets of the curable composition, the droplets do not spread even after the pressing of the mold is completed, and defects (abnormalities) due to unfilled portions occur.

[0006] However, the amount of gas bubbles trapped between droplets of the curable composition is determined by a complex of actions including the action between the mold and the droplets, the bonding between droplets, etc. Therefore, the amount of gas trapped between droplets cannot be kept below a predetermined amount by simply adjusting the arrangement of the droplets so that the height distribution of the droplets of the curable composition falls within a predetermined range. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Patent No. 5599356 Summary of the Invention [Problem to be solved by the invention]

[0008] The present invention has been made in consideration of such problems in the conventional technology, and an exemplary object of the present invention is to provide a technique that is advantageous for detecting abnormalities in the behavior of a curable composition in a process for forming a film of the curable composition. [Means for solving the problem]

[0009] In order to achieve the above object, a simulation method according to one aspect of the present invention is a simulation method for predicting behavior of a curable composition in a process of contacting a plurality of droplets of the curable composition disposed on a first member with a second member to form a film of the curable composition in a space between the first member and the second member, the simulation method comprising the steps of: ,next Regarding the degree of adhesion with the contacting droplet Joint information is information A first step for obtaining Met The above The bonding information and the plurality of Droplets spread Status information and of and a second step of displaying both.

[0010] Further objects or other aspects of the present invention will become apparent from the following description of the embodiments with reference to the accompanying drawings. Effect of the Invention

[0011] According to the present invention, for example, a technique that is advantageous for detecting abnormal behavior of a curable composition during a process for forming a film of the curable composition can be provided. [Brief description of the drawings]

[0012] [Figure 1] 1 is a schematic diagram showing a configuration of a film forming apparatus and a simulation apparatus according to an embodiment of the present invention. [Diagram 2] 4 is a flowchart for explaining a simulation method in the first embodiment. [Diagram 3] FIG. 1 illustrates the concept of droplet elements of a curable composition. [Figure 4] 11A and 11B are diagrams illustrating a process for determining whether adjacent droplet elements are joined. [Diagram 5] FIG. 2 is a diagram showing an example of calculation of the behavior of droplets of a curable composition using the simulation device shown in FIG. [Figure 6] FIG. 1 shows a droplet element of a hardenable composition defined by 18 angles. [Figure 7] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 8] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 9] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 10] 10 is a flowchart for explaining a simulation method in the second embodiment. [Figure 11] FIG. 2 is a diagram for explaining a link structure. [Figure 12] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 13] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 14] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 15] 13 is a flowchart for explaining a simulation method in the third embodiment. [Figure 16] 11 is a diagram for explaining a determination of the presence or absence of a closed region. FIG. [Figure 17] 11 is a diagram for explaining a determination of the presence or absence of a closed region. FIG. [Figure 18] 11A and 11B are diagrams for explaining a method for calculating the amount of bubbles contained in a closed region. [Figure 19] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 20] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 21] FIG. 1 is a diagram for explaining a method for detecting an abnormality in the behavior of a curable composition. [Figure 22] FIG. 4 is a diagram showing an example of an image displayed on a display. [Figure 23] 1A to 1C are diagrams for explaining a method for manufacturing an article. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, the embodiments will be described in detail with reference to the attached drawings. Note that the following embodiments do not limit the invention according to the claims. Although the embodiments describe a number of features, not all of these features are essential to the invention, and the features may be combined in any manner. Furthermore, in the attached drawings, the same reference numbers are used for the same or similar configurations, and duplicated descriptions are omitted.

[0014] FIG. 1 is a schematic diagram showing the configuration of a film-forming apparatus IMP and a simulation apparatus 1 in an embodiment of the present invention. The film-forming apparatus IMP brings multiple droplets of the curable composition IM arranged on a substrate S into contact with a mold M, and executes a process of forming a film of the curable composition IM in the space between the substrate S and the mold M. The film-forming apparatus IMP may be configured, for example, as an imprint apparatus or as a flattening apparatus. Here, the substrate S and the mold M are interchangeable, and a film of the curable composition IM may be formed in the space between the mold M and the substrate S by bringing multiple droplets of the curable composition IM arranged on the mold M into contact with the substrate S. Therefore, in general, the film-forming apparatus IMP is an apparatus that brings multiple droplets of the curable composition IM arranged on a first member into contact with a second member, and executes a process of forming a film of the curable composition IM in the space between the first member and the second member. In this embodiment, the first member will be described as the substrate S and the second member as the mold M, but the first member may be the mold M and the second member may be the substrate S. In this case, the substrate S and the mold M in the following description may be interchanged.

[0015] In the imprinting apparatus, a mold M having a pattern is used to transfer the pattern of the mold M to the curable composition IM on the substrate S. In the imprinting apparatus, a mold M having a pattern region PR in which a pattern is provided is used. In the imprinting apparatus, the curable composition IM on the substrate S is brought into contact with the pattern region PR of the mold M as an imprinting process, the curable composition IM is filled in the space between the region of the substrate S where the pattern is to be formed and the mold M, and then the curable composition IM is cured. As a result, the pattern of the pattern region PR of the mold M is transferred to the curable composition IM on the substrate S. In the imprinting apparatus, for example, a pattern made of a cured product of the curable composition IM is formed in each of a plurality of shot regions of the substrate S.

[0016] In the planarization apparatus, a mold M having a flat surface is used for the planarization process, and the curable composition IM on the substrate S is brought into contact with the flat surface of the mold M, and the curable composition IM is cured to form a film having a flat upper surface. When the planarization apparatus uses a mold M having dimensions (size) that cover the entire area of ​​the substrate S, a film made of the cured product of the curable composition IM is formed over the entire area of ​​the substrate S.

[0017] As the curable composition, a material that is cured by applying energy for curing is used. As the energy for curing, electromagnetic waves, heat, etc. are used. The electromagnetic waves include, for example, light having a wavelength selected from the range of 10 nm to 1 mm, specifically, infrared rays, visible light, ultraviolet rays, etc. Thus, the curable composition is a composition that is cured by irradiation with light or heating. The photocurable composition that is cured by irradiation with light contains at least a polymerizable compound and a photopolymerization initiator, and may further contain a non-polymerizable compound or a solvent as necessary. The non-polymerizable compound is at least one selected from the group consisting of a sensitizer, a hydrogen donor, an internal mold release agent, a surfactant, an antioxidant, a polymer component, etc. The viscosity of the curable composition (viscosity at 25°C) is, for example, 1 mPa·s to 100 mPa·s.

[0018] The substrate may be made of, for example, glass, ceramics, metal, semiconductor, or resin. If necessary, a member made of a material different from that of the substrate may be provided on the surface of the substrate. The substrate may be made of, for example, a silicon wafer, a compound semiconductor wafer, or quartz glass.

[0019] In this specification and the accompanying drawings, directions are shown in an XYZ coordinate system in which the direction parallel to the surface of the substrate S is the XY plane. The directions parallel to the X-axis, Y-axis, and Z-axis in the XYZ coordinate system are the X direction, the Y direction, and the Z direction, respectively, and the rotation around the X-axis, the Y axis, and the Z axis are θX, θY, and θZ, respectively. Control or drive regarding the X-axis, Y-axis, and Z-axis means control or drive regarding the direction parallel to the X-axis, the direction parallel to the Y axis, and the direction parallel to the Z axis, respectively. Furthermore, control or drive regarding the θX-axis, θY-axis, and θZ-axis means control or drive regarding the rotation around an axis parallel to the X-axis, the rotation around an axis parallel to the Y axis, and the rotation around an axis parallel to the Z axis, respectively. Furthermore, the position is information specified based on the coordinates of the X-axis, the Y-axis, and the Z axis, and the orientation is information specified by the values ​​of the θX-axis, the θY-axis, and the θZ axis. Positioning means controlling the position and / or orientation.

[0020] The film forming apparatus IMP has a substrate holding part SH that holds a substrate S, a substrate driving mechanism SD that drives the substrate holding part SH to move the substrate S, and a base SB that supports the substrate driving mechanism SD. The film forming apparatus IMP also has a mold holding part MH that holds a mold M, and a mold driving mechanism MD that drives the mold holding part MH to move the mold M.

[0021] The substrate driving mechanism SD and the mold driving mechanism MD constitute a relative movement mechanism that moves at least one of the substrate S and the mold M so that the relative positions of the substrate S and the mold M are adjusted. The adjustment of the relative positions of the substrate S and the mold M by the relative movement mechanism includes driving for contact between the curable composition IM on the substrate S and the mold M, and driving for separation of the mold M from the cured curable composition IM on the substrate S. The adjustment of the relative positions of the substrate S and the mold M by the relative movement mechanism also includes alignment of the substrate S and the mold M. The substrate driving mechanism SD is configured to drive the substrate S about a plurality of axes (e.g., three axes of the X axis, the Y axis, and the θZ axis, preferably six axes of the X axis, the Y axis, the Z axis, the θX axis, the θY axis, and the θZ axis). The mold driving mechanism MD is configured to drive the mold M about a plurality of axes (e.g., three axes of the Z axis, the θX axis, and the θY axis, preferably six axes of the X axis, the Y axis, the Z axis, the θX axis, the θY axis, and the θZ axis).

[0022] The film forming apparatus IMP has a curing unit CU for curing the curable composition IM filled in the space between the substrate S and the mold M. The curing unit CU cures the curable composition IM on the substrate S, for example, by applying energy for curing to the curable composition IM via the mold M.

[0023] The film forming apparatus IMP has a transparent member TR for forming a space SP on the back side (opposite the surface facing the substrate S) of the mold M. The transparent member TR is made of a material that transmits the curing energy from the curing unit CU, and makes it possible to apply the curing energy to the curable composition IM on the substrate S.

[0024] The film forming apparatus IMP has a pressure control unit PC that controls the pressure in the space SP to control the deformation of the mold M in the Z-axis direction. For example, the pressure control unit PC makes the pressure in the space SP higher than atmospheric pressure, whereby the mold M is deformed into a convex shape toward the substrate S.

[0025] The film-forming apparatus IMP has a dispenser DSP for placing, supplying, or distributing the curable composition IM on the substrate S. However, the substrate S on which the curable composition IM has been placed by another device may be supplied (carried in) to the film-forming apparatus IMP. In this case, the film-forming apparatus IMP does not need to have the dispenser DSP.

[0026] The film forming apparatus IMP may have an alignment scope AS for measuring the positional deviation (alignment error) between the substrate S (or the shot area of ​​the substrate S) and the mold M.

[0027] The simulation device 1 executes calculations to predict the behavior of the curable composition IM in a process executed in the film forming device IMP. Specifically, the simulation device 1 executes calculations to predict the behavior of the curable composition IM in a process of bringing multiple droplets of the curable composition IM arranged on a substrate S into contact with a mold M to form a film of the curable composition IM in a space between the substrate S and the mold M.

[0028] The simulation device 1 is configured, for example, by incorporating a simulation program 21 into a general-purpose or dedicated computer. The simulation device 1 may also be configured by a PLD (abbreviation for Programmable Logic Device) such as an FPGA (abbreviation for Field Programmable Gate Array) or an ASIC (abbreviation for Application Specific Integrated Circuit).

[0029] In this embodiment, the simulation device 1 is configured by storing a simulation program 21 in the memory 20 of a computer having a processor 10, a memory 20, a display 30, and an input device 40. The memory 20 may be a semiconductor memory, a disk such as a hard disk, or another form of memory. The simulation program 21 may be stored in a computer-readable memory medium, or may be provided to the simulation device 1 via a communication facility such as a telecommunication line.

[0030] The simulation method and the simulation device of the present invention relate to a process for forming a film of a curable composition in a space between a substrate and a mold, for example, a simulation of the behavior of the curable composition in an imprint process. Specifically, the simulation method and the simulation device of the present invention simulate the spread of droplets, including the interaction between droplets of the curable composition on the substrate, to predict and visually display the spread of the droplets at any time. In addition, the simulation method and the simulation device of the present invention detect and visually display an abnormality (abnormality in the spread of the droplets) caused by air bubbles trapped between the droplets from the joining state of the droplets of the curable composition on the substrate and its change. This makes it possible to visually confirm the behavior (state) of the spread of the droplets of the curable composition on the substrate, and to grasp the abnormality in the spread of the droplets in advance, and to suppress defects due to non-filling by adjusting the arrangement of the droplets based on such information.

[0031] Hereinafter, a simulation method executed by the simulation device 1 in each embodiment will be specifically described.

[0032] First Embodiment 2 is a flowchart for explaining the simulation method in the first embodiment. The simulation method includes steps S001, S002, S003, S004, S005, S006, S007, S008, and S009. The simulation device 1 may be understood as a collection of hardware elements that execute each step of the simulation method in the first embodiment.

[0033] S001 is a step of setting conditions (simulation conditions) necessary for the simulation. S002 is a step of setting the initial state of the curable composition IM based on the simulation conditions set in S001. S001 and S002 may be understood as a single combined step, for example, a preparation step. S003 is a step of calculating the movement of the mold M to update (calculate) the position of the mold M (the distance between the substrate S and the mold M). S004 is a step of calculating the behavior (flow of the droplets) of the droplets spread by the mold M for each of the multiple droplets of the curable composition IM based on the position of the mold M updated in S003. S005 is a step of judging whether adjacent droplets (liquid particles) of the multiple droplets of the curable composition IM have joined together based on the behavior of the droplets calculated in S004. S006 is a step of calculating joining information for each of the multiple droplets of the curable composition IM based on whether adjacent droplets have joined together as judged in S004. S007 is a step of judging whether or not there is an abnormality in the behavior of the curable composition IM at that time based on the bonding information calculated in S006 and the time-series changes (i.e., detecting an abnormality in the behavior of the curable composition IM). S008 is a step of judging whether or not the time in the calculation (simulation) has reached the end time. If the time in the calculation has not reached the end time, the time is advanced to the next time and the process proceeds to S003. On the other hand, if the time in the calculation has reached the end time, the process proceeds to S009. S009 is a step of displaying at least one of the bonding information calculated in S006 and abnormality information indicating whether or not there is an abnormality in the behavior of the curable composition judged in S007, together with information indicating the state of the multiple droplets of the curable composition IM (the behavior of the curable composition IM).

[0034] Hereinafter, each step of the simulation method in the first embodiment will be described in detail.

[0035] In S001, various patterns are set as conditions necessary for the simulation. The parameters include the arrangement of droplets of the curable composition IM on the substrate S, the volume of each droplet, the physical properties of the curable composition IM, information on the unevenness of the surface of the mold M (for example, information on the pattern of the pattern region PR), information on the unevenness of the surface of the substrate S, etc. The parameters also include a time profile of the force applied to the mold M by the mold driving unit MD, a profile of the pressure applied to the space SP (mold M) by the pressure control unit PC, etc.

[0036] In S002, the initial state of each of the droplets of the curable composition IM (the state of the droplet when the simulation is started) is set. The initial state includes the outline (shape) and height of each droplet of the curable composition IM placed on the substrate S when the droplet spreads out. The initial state can also be calculated by assuming a static equilibrium state using the physical property values ​​of the curable composition IM. In addition to the physical property values ​​of the curable composition IM, the elapsed time since the droplet of the curable composition IM was placed on the substrate S is input, and a general fluid simulation is performed to calculate the initial state from the dynamic wetting and spreading behavior.

[0037] In the simulation method of this embodiment, each droplet of the curable composition IM is modeled as a droplet element DRP as shown in Fig. 3. Fig. 3 is a diagram showing the concept of the droplet element DRP of the curable composition IM. Referring to Fig. 3, the i-th droplet element in the calculation domain is represented as a DRP i Hereinafter, the subscript i represents the number of the droplet element DRP.

[0038] First, a representative point is set inside the droplet element of the curable composition IM. The coordinates of the representative point are Ci(x0,y0). The representative point of the droplet element of the curable composition IM may be the center of gravity of the droplet, or may be a point (position) different from the center of gravity of the droplet, but it is necessary to set it inside the outline of the droplet. In addition, the distance from the representative point of the droplet element of the curable composition IM to a point on the outline (outer periphery) of the droplet element at an angle θ (the angle between the line connecting the representative point and the point on the droplet outline and the reference line) is expressed as a radius r(θ). The radius r(θ) has a different value for each angle θ. Here, information indicating whether each point on the outline of the droplet element is joined (penetrated) to an adjacent droplet element is also stored. The position (radius r(θ)) of the point on the outline that is joined to the adjacent droplet element is fixed at that time. The region of angle θ where the radius r(θ) is fixed in this way is called a fixed region FIX, as shown by the diagonal lines in FIG. 3. i On the other hand, the region of angle θ where radius r(θ) is not fixed is called the free region FRE, as shown by the solid line in Figure 3. i In the initial state of the droplet of the curable composition IM, all angles θ belong to the free region.

[0039] When the simulation method of the present embodiment is implemented as an actual program, it is considered that the angle θ is divided into a finite number of angles and handled (i.e., a finite number of points are set on the droplet's contour to define the droplet's contour). FIG. 6 is a diagram showing a droplet element of a curable composition IM defined (divided) by 18 angles θ (θ1 to θ20). In this case, the angle θ may be set by equally dividing 360 degrees, or an arbitrary angle may be set. When determining the contour between adjacent points on the contour represented by a finite number of angles, any interpolation may be applied. For example, adjacent points on the contour may be connected by a line, or higher-order interpolation may be applied.

[0040] In S003, the movement of the mold M is calculated, and the position of the mold M is updated. The movement of the mold M is calculated by a dynamic calculation that takes into consideration the force generated when the droplets of the curable composition IM or the liquid film formed by bonding liquid particles is crushed, the force caused by the flow of gas in the space SP between the mold M and the substrate S, the load applied to the mold M, the effect of the elastic deformation of the mold M, and the like.

[0041] In S004, the behavior of the droplet element DRP spread by the mold M is calculated. S004 includes a step of determining whether the droplet element DRP is in contact with the mold M. The droplet element DRP obtained in S002 i Height h drp,i and the droplet element DRP i The distance h between the mold M and the substrate S at the representative point (x0, y0) of i If the following formula (1) is satisfied, the droplet element DRP i It is determined that has come into contact with type M.

[0042]

number

[0043] On the other hand, if equation (1) is not satisfied, at the current time in the calculation, the droplet element DRP i is determined to be not in contact with the mold M. In this case, the droplet element DRP i No calculation of the behavior of

[0044] Droplet element DRP determined to have come into contact with type M i The behavior of the droplet being pushed out by the movement of the mold M is calculated for each droplet element DRP. In this process, the volume of the droplet of the hardenable composition IM is conserved (maintained). Therefore, i Volume V i and the distance h at the droplet element position at the current time i Using and, the droplet element DRP at the current time i Area S new can be expressed by the following equation (2).

[0045]

number

[0046] In S005, it is determined whether adjacent droplet elements have joined together. In S004, as a result of calculating the contour of the droplet elements, it occurs that a point on the contour at an angle θ belonging to the free region FRE enters the interior (inside the contour) of an adjacent droplet element. In this case, the radius r(θ) at the angle θ is fixed (i.e., the distance from the representative point to the point on the contour corresponding to the joined portion of the droplets is fixed). In other words, the angle θ is included in the fixed region FIX, and at the subsequent time, the spread (flow) of the droplet elements of the curable composition IM does not occur in the direction of the angle θ. In S005, it is determined whether the droplets have joined together for all pairs of adjacent droplet elements as described above.

[0047] 4, a process for determining whether adjacent droplet elements are joined, i.e., whether a point on the droplet outline is located inside the outline of an adjacent droplet, will be described. First, a droplet element DRP i Focusing on the droplet element DRP i Free area FRE i Consider a point P on the contour with an angular orientation belonging to the droplet element DRP i The droplet element adjacent to the droplet element DRP j Let P and the droplet element DRP j Representative point C of j (Center) and the line segment PC j Find the length of the line segment PC j The angle θ between the droplet element and the reference line j Calculate the angle θ j Droplet element DRP in j Radius QC j Find the length of QC j Length of and line segment PC j Compare the length of the radius QC j The length of the line segment PC j If the length of the droplet element DRP is longer than i A point P on the contour of the adjacent droplet element DRP jOn the other hand, the radius QC j The length of the line segment PC j If the length of the droplet element DRP is shorter than i A point P on the contour of the adjacent droplet element DRP j In FIG. 4, the droplet element DRP i A point P on the contour of the adjacent droplet element DRP j In the figure, the droplet element DRP is largely inserted into the droplet element DRP, but this is to emphasize the feature of this embodiment. In the actual calculation, the time interval is set to be sufficiently small, so that the droplet element DRP is inserted into the droplet element DRP. i A point P on the contour of the adjacent droplet element DRP j The amount of penetration into the interior of the mold can be made negligible.

[0048] Fig. 5 is a diagram showing an example of calculation of the behavior (spread) of droplets of the curable composition IM by the simulation device 1 implementing the simulation method of this embodiment. The distance between the mold M and the substrate S is closer to the center of Fig. 5, and becomes greater the further away from the center of Fig. 5. Referring to Fig. 5, it can be seen that the complex joining of droplets can be expressed according to the arrangement of the droplets of the curable composition IM on the substrate S.

[0049] In S006, the joining information is calculated using the result of the determination of whether adjacent droplet elements have joined. The joining information means an evaluation value that evaluates the relationship regarding the degree of joining with adjacent droplets. For example, in this embodiment, the joining information is information indicating how much of the contour of each droplet of the curable composition IM is in contact with the contour of other droplets. Specifically, the joining information is the ratio of the portion determined to be in contact with other droplets to the contour length of the droplet of the curable composition IM, that is, the ratio of the portion in contact with the contour of the adjacent droplet out of the entire circumference of the droplet contour. In this case, the contour of the droplet of the curable composition IM may be divided by multiple angles, and the ratio of the angle determined to be in contact with other droplets may be used as the joining information.

[0050] With reference to FIG. 6, the ratio of the joining with adjacent droplets to the contour length of the droplet of the curable composition IM, that is, an overview of the joining information in this embodiment, will be described. In FIG. 6, 601 indicates the contour of a droplet element of interest, and 602 indicates the contour of a droplet element adjacent to the droplet element of interest. The contour 601 of the droplet element of interest is sampled at a plurality of points 603, and it is determined whether each of the plurality of points 603 is in contact with an adjacent droplet element 602. For example, among the plurality of points 603, point 604 is determined to be in contact with an adjacent droplet element 602. Finally, the ratio of points 604 in contact with adjacent droplet elements 602 to the total number of points 603 sampled on the contour 601 of the droplet element of interest is set as the joining information.

[0051] The bonding information thus obtained is displayed on the display 30 in S009 together with information showing the state (spread state) of the droplets of the curable composition IM relative to the bonding information. Fig. 7 is a diagram showing an example of an image including the bonding information displayed on the display 30 in S009. In Fig. 7, the droplet element DRP arranged in the shot region ST of the substrate S is i In this embodiment, the droplet element DRP i For each of the droplet elements DRP, the droplet element DRP is calculated according to the ratio of joining with adjacent droplets to the droplet contour length. i The color in the area has been changed.

[0052] Consider a case where the mold M is deformed into a convex shape toward the substrate S when the mold M is brought into contact with the curable composition IM on the substrate S. In this case, the droplet element DRP disposed in the center of the shot area ST i Droplet elements DRP arranged outside the shot area ST i Towards the droplet element DRP i Therefore, the droplet element DRP arranged at the center of the shot area ST is pushed out. i is a droplet element DRP arranged outside the shot area ST i In comparison with the droplet element DRP, the rate of joining with adjacent droplets tends to be higher. iFor each droplet, the droplet element DRP is calculated according to the proportion of adjacent droplets that join together. i The droplet element DRP has a high rate of joining with adjacent droplets. i The areas are displayed in darker colors. Specifically, the colors within those areas are displayed in lighter colors in the order of droplet element DRP1, droplet element DRP2, and droplet element DRP3, that is, in the order of increasing distance from the center of the shot area ST. Also, when a droplet element is not in contact with adjacent droplets, such as droplet element DRP4, the color of that area is displayed in white. i and the droplet element DRP i By displaying the outlines of the droplets in different colors (making them distinguishable), the boundaries between adjacent droplets can also be confirmed.

[0053] In this embodiment, the case where the brightness of the droplet area corresponding to the joining information is changed according to the size of the joining information has been described, but the present invention is not limited to this. For example, the hue of the droplet area corresponding to the joining information may be changed according to the size of the joining information. In addition, by displaying a legend that corresponds to the color representing the size of the joining information and the size relationship of the joining information indicated by the color (in this embodiment, the rate of joining with adjacent droplets), the joining information can also be grasped numerically. This allows the contact state of the droplets, which is the spreading state of the droplets, to be visually grasped for each of the multiple droplets of the curable composition IM.

[0054] In S007, the presence or absence of an abnormality in the behavior of the curable composition IM at that time is determined based on the bonding information calculated in S006 and the time-series changes (i.e., an abnormality in the behavior of the curable composition IM is detected). Usually, when the contact between the curable composition IM on the substrate S and the mold M progresses, the droplet element DRP arranged near the center of the shot region ST i The proportion of droplets joining adjacent droplets increases from the center of the shot area ST, and gradually spreads to the periphery of the shot area ST. On the other hand, when an abnormality occurs in the behavior of the curable composition IM, the droplet element DRP arranged near the center of the shot area ST i Among the surrounding droplet elements DRP iCompared to droplet element DRP, the rate at which droplets join with adjacent droplets is small. i exists.

[0055] 8 is a diagram showing an example of an image including bonding information displayed on the display 30 in S009 when an abnormality occurs in the behavior of the curable composition IM. In FIG. 8, a droplet element DRP arranged in a shot region ST of the substrate S is i In this embodiment, the droplet element DRP i For each of the droplet elements DRP, the droplet element DRP is calculated according to the ratio of joining with adjacent droplets to the droplet contour length. i In Fig. 8, the droplet element DRP has a high rate of joining with adjacent droplets. i The areas with a darker hue are shown in the figure.

[0056] Normally, the droplet element DRP placed near the center of the shot area ST i is a droplet element DRP located away from the center of the shot area ST i In comparison, the rate at which droplets join with adjacent droplets is high, and the area is displayed in a darker color. However, in Fig. 8, the area of ​​droplet element DRP1 arranged near the center of shot area ST is displayed in a lighter color than the areas of the surrounding droplet elements. Specifically, the area of ​​droplet element DRP2 arranged further outside of shot area ST than droplet element DRP1 is displayed in a lighter color than the area of ​​droplet element DRP1, indicating that an abnormality has occurred in the behavior of droplet element DRP2.

[0057] An example of a method for detecting an abnormality in the behavior of the curable composition IM will be described below. This method is a method for searching for droplets that have a part of their outline that is not joined to adjacent droplets and are surrounded by droplets whose outlines are entirely joined to adjacent droplets, and detecting such droplets as droplets in which an abnormality has occurred. Specifically, a droplet that is less likely to join to adjacent droplets than surrounding droplets is detected as a droplet in which an abnormality has occurred. In this embodiment, the presence or absence of an abnormality is determined (an abnormality is detected) by following the steps (1), (2), and (3). Note that the joining information of a droplet in a state where the entire outline is not joined to an adjacent droplet is set to 0, the joining information of a droplet in a state where the entire outline is joined to an adjacent droplet is set to 1, and the joining information of a droplet in a state where a part of the outline is joined to an adjacent droplet is set to between 0 and 1.

[0058] (1) From all droplets, extract droplets that have a contour portion that is not joined to adjacent droplets, i.e., droplets with joining information other than 1, and classify these droplets as droplet group DG1 (for example, droplet element DRP1 shown in Figure 8).

[0059] (2) From all droplets contained in droplet group DG1, droplets having representative points within a range of a preset distance D from a representative point of the droplets contained in droplet group DG1 are extracted, and these droplets are set as droplet group DG2 (for example, droplet element DRP2 shown in Fig. 8). In Fig. 8, 801 indicates the range of distance D from droplet element DRP1, that is, the droplet extraction range.

[0060] (3) When all droplets in each droplet group DG2 have edges that are all joined to each other (joining information is 1) with respect to all droplets in droplet group DG1, it is determined to be abnormal. Also, when droplets in each droplet group DG2 have greater joining information than droplets in droplet group DG1, it is determined to be abnormal.

[0061] The abnormality in the behavior of the curable composition IM detected in this manner is displayed on the display 30 in S009 as abnormality information indicating the presence or absence of behavior of the curable composition IM together with information indicating the state (spread state) of the droplets of the curable composition IM. Fig. 9 is a diagram showing an example of an image including abnormality information displayed on the display 30 in S009. In Fig. 9, each droplet element DRP shown in Fig. 8 i An abnormality is judged for each droplet element DRP1, and the area of ​​the droplet element DRP1 judged to be abnormal is displayed in black. Moreover, the droplet element DRP1 judged to be abnormal is displayed in a different color from the droplet element judged to be normal (not judged to be abnormal), for example, the droplet element DRP2. In this way, by displaying the droplets judged to be abnormal and the droplets judged to be normal in different colors (distinguishing them), the presence or absence of an abnormality can be visually grasped. Moreover, the droplets judged to be abnormal and the droplets judged to be normal may be displayed in different display modes, for example, the droplets judged to be abnormal may be made to blink and the droplets judged to be normal may not be made to blink.

[0062] The calculation steps including S003, S004, S005, S006, and S007 are performed for a plurality of preset times. The plurality of times are arbitrarily set within a period from the time when the mold M starts to descend from the initial position to the time when the mold M comes into contact with a plurality of droplets, the plurality of droplets spread while being crushed, the plurality of droplets bond to each other, and finally form a single film, and the curable composition is cured. The plurality of times are typically set at regular time intervals.

[0063] In S008, it is determined whether the time in the calculation has reached the end time. As described above, if the time in the calculation has not reached the end time, the time is advanced to the next time and the process proceeds to S003, and if the time in the calculation has reached the end time, the process proceeds to S009. In one example, in S008, the current time is advanced by a specified time increment to become the new time. Then, if the new time has reached the end time, the process proceeds to S009.

[0064] In S009, as described above, at least one of the images shown in Fig. 7, Fig. 8, and Fig. 9 is displayed on the display 30. In S009, for example, in response to a user request, the images shown in Fig. 7, Fig. 8, and Fig. 9 may be displayed while being switched between, or some or all of the images shown in Fig. 7, Fig. 8, and Fig. 9 may be displayed.

[0065] According to this embodiment, it is possible to visually determine and recognize the behavior of multiple droplets of the curable composition IM arranged on the substrate S, particularly the presence or absence of an abnormality in the spread of the droplets. Therefore, it is possible to provide a technique that is advantageous for detecting abnormalities in the behavior of the curable composition IM in a process of forming a film of the curable composition IM in the film forming apparatus IMP. In addition, by repeatedly adjusting the droplet arrangement pattern of the curable composition IM using the simulation method of this embodiment and the results thereof, it is possible to easily set the conditions of the process while reducing abnormalities in the process of forming a film of the curable composition IM.

[0066] <Second embodiment> 10 is a flowchart for explaining the simulation method in the second embodiment. The simulation method includes steps S101, S102, S103, S104, S105, S106, S107, S108, and S109. The simulation device 1 may be understood as a collection of hardware elements that execute each step of the simulation method in the second embodiment.

[0067] S101 is a step of setting conditions (simulation conditions) required for the simulation. S102 is a step of generating a link structure that connects adjacent droplets based on the droplet arrangement information of the curable composition IM set in S101. S101 and S102 may be understood as a single combined step, for example, a preparation step. S103 is a step of calculating the movement of the mold M and updating the position of the mold M. S104 is a step of calculating the behavior of the droplets spread by the mold M for each of the multiple droplets of the curable composition IM based on the position of the mold M updated in S103. S105 is a step of judging whether each link of the link structure generated in S102 is closed, that is, whether the link is open or closed. S106 is a step of calculating the joining information for each of the multiple droplets of the curable composition IM based on whether each link of the link structure judged in S105 is closed. S107 is a step of judging whether or not there is an abnormality in the behavior of the curable composition IM at that time based on the bonding information calculated in S106 and the time-series changes (i.e., detecting an abnormality in the behavior of the curable composition IM). S108 is a step of judging whether or not the time in the calculation (simulation) has reached the end time. If the time in the calculation has not reached the end time, the time is advanced to the next time and the process proceeds to S103. On the other hand, if the time in the calculation has reached the end time, the process proceeds to S109. S109 is a step of displaying at least one of the bonding information calculated in S106 and abnormality information indicating whether or not there is an abnormality in the behavior of the curable composition judged in S107, together with information indicating the state of the multiple droplets of the curable composition IM (the behavior of the curable composition IM).

[0068] Hereinafter, each step of the simulation method in the second embodiment will be described in detail, except that S101, S103, and S104 are similar to S001, S003, and S004 shown in FIG.

[0069] In S102, a link structure that connects adjacent droplets is generated based on the droplet arrangement information of the curable composition IM. The link structure will be described with reference to FIG. 11. Each droplet of the curable composition IM is modeled as a droplet element DRP as shown in FIG. 11. Referring to FIG. 11, a node ND is generated at a representative point C of the droplet element DRP, and a link is generated by connecting adjacent nodes. Specifically, a link is generated between nodes generated in droplet elements present in the vicinity of a location where droplets of the curable composition IM are joined, and is defined as a line segment connecting both nodes. In addition, when two droplet elements that constitute a link are joined, such a link is called a closed link LNC, and when two droplet elements that constitute a link are not joined, such a link is called an open link LNO. In addition, when a link is expressed without distinguishing between a closed link and an open link, it is written as a link LN. In addition, links are generated so that they always intersect at nodes and do not intersect at other parts (i.e., links are generated only for adjacent droplet elements). As a generation method for generating such a link structure, for example, a method using Delaunay division is available.

[0070] In S105, the open / closed state of all the links LN is determined. In this embodiment, in each link LN, if the droplet elements constituting the link LN are not joined to each other, the link LN is determined to be an open link LNO, and if the droplet elements constituting the link LN are joined to each other, the link LN is determined to be a closed link LNC. To determine whether adjacent droplet elements are joined, as described with reference to FIG. 4, a process for determining whether a point on the droplet outline is located inside the outline of an adjacent droplet may be used. Specifically, as shown in FIG. 4, a radius QC j Length of and line segment PC j Compare the length of the radius QC j The length of the line segment PC j If the length of the link LN is longer than the radius QC j Length of and line segment PC j Compare the length of the radius QCj The length of the line segment PC j If the length is shorter than the length of the link LN, it is determined that the link LN is open.

[0071] In S106, the joining information is calculated using the result of the determination of whether the link LN is open or closed. The joining information means an evaluation value that evaluates the relationship regarding the degree of joining with adjacent droplets. For example, in this embodiment, the joining information is information indicating how many links of the links of each droplet of the curable composition IM are closed. Specifically, the joining information is the ratio of closed links LNC among the links LN generated for the droplet element DRP.

[0072] The bonding information thus obtained is displayed on the display 30 in S109 together with information showing the state (spread state) of the droplets of the curable composition IM relative to the bonding information. Fig. 12 is a diagram showing an example of an image including the bonding information displayed on the display 30 in S109. In Fig. 12, the droplet element DRP arranged in the shot region ST of the substrate S is i In Fig. 12, the droplet element DRP i For each of the droplet elements DRP i Among the links LN having the nodes, the closed links LNC are indicated by solid lines, and the open links LNO are indicated by dashed lines. In this embodiment, i For each of the droplet elements DRP, depending on the percentage of closed links LNC i The color in the area has been changed.

[0073] Consider a case where the mold M is deformed into a convex shape toward the substrate S when the mold M is brought into contact with the curable composition IM on the substrate S. In this case, the droplet element DRP disposed in the center of the shot area ST i Droplet elements DRP arranged outside the shot area ST i Towards the droplet element DRP i Therefore, the droplet element DRP arranged at the center of the shot area ST is pushed out. i is a droplet element DRP arranged outside the shot area STi In Fig. 12, the ratio of the droplet element DRP i For each, depending on the percentage of closed links LNC, the droplet element DRP i The intensity of the droplets in the area of ​​the LNC droplets is changed by changing the ratio of the closed link LNC to the droplet element DRP. i The areas are displayed in darker colors. Specifically, the areas are displayed in lighter colors in the order of droplet element DRP1, droplet element DRP2, and droplet element DRP3, that is, in the order of increasing distance from the center of the shot area ST. Also, when a droplet element is not in contact with adjacent droplets, such as droplet element DRP4, that is, when the ratio of closed links LNC is zero, the color of that area is displayed in white. i and the droplet element DRP i By displaying the outlines of the droplets in different colors (making them distinguishable), the boundaries between adjacent droplets can also be confirmed.

[0074] In this embodiment, the case where the brightness of the droplet area corresponding to the joining information is changed according to the size of the joining information has been described, but the present invention is not limited to this. For example, the hue of the droplet area corresponding to the joining information may be changed according to the size of the joining information. In addition, by displaying a legend that associates the color representing the size of the joining information with the size relationship of the joining information indicated by the color (in this embodiment, the ratio of closed links LNC), the joining information can also be grasped numerically. This makes it possible to visually grasp the contact state of the droplets, which is the spreading state of the droplets, for each of the multiple droplets of the curable composition IM. In addition, in FIG. 12, the closed links LNC are shown by solid lines and the open links LNO are shown by dashed lines, so that the presence or absence of joining between the droplets can be visually grasped.

[0075] In S107, the presence or absence of an abnormality in the behavior of the curable composition IM at that time is determined based on the bonding information calculated in S106 and the time-series changes (i.e., an abnormality in the behavior of the curable composition IM is detected). Usually, when the contact between the curable composition IM on the substrate S and the mold M progresses, the droplet element DRP arranged near the center of the shot region ST iThe ratio of the closed links LNC increases from the center of the shot area ST, and gradually spreads to the periphery of the shot area ST. On the other hand, when an abnormality occurs in the behavior of the curable composition IM, the droplet element DRP i Among the surrounding droplet elements DRP i Compared to the droplet element DRP, the proportion of closed links LNC is small. i exists.

[0076] 13 is a diagram showing an example of an image including bonding information displayed on the display 30 in S009 when an abnormality occurs in the behavior of the curable composition IM. In FIG. 13, a droplet element DRP arranged in a shot region ST of the substrate S is i In this embodiment, the droplet element DRP i For each of the droplet elements DRP, depending on the percentage of closed links LNC i In Fig. 13, the droplet element DRP with a high ratio of closed links LNC is colored differently. i The areas with a darker hue are shown in the figure.

[0077] Normally, the droplet element DRP placed near the center of the shot area ST i is a droplet element DRP located away from the center of the shot area ST i 13, the ratio of closed links LNC is high, and the area is displayed in a darker color. However, in Fig. 13, the area of ​​droplet element DRP1 arranged near the center of shot area ST is displayed in a lighter color than the areas of the surrounding droplet elements. Specifically, the area of ​​droplet element DRP2 arranged further outside of shot area ST than droplet element DRP1 is displayed in a lighter color than the area of ​​droplet element DRP1, and it can be seen that an abnormality has occurred in the behavior of droplet element DRP2.

[0078] An example of a method for detecting abnormalities in the behavior of the curable composition IM will be described below. This method searches for droplets that include an open link LNO in a link LN surrounded by droplets whose links LN are all closed links LNC, and detects such droplets as droplets in which an abnormality has occurred. In this embodiment, the presence or absence of an abnormality is determined (an abnormality is detected) by following the steps (1), (2), and (3) below. Note that the joining information of a droplet whose links LN are all open links LNO is 0, the joining information of a droplet whose links LN are all closed links LNC is 1, and the joining information of a droplet whose links LN are partly closed links LNC is between 0 and 1 depending on the proportion of closed links LNC.

[0079] (1) From all droplets, droplets including an open link LNO, that is, droplets whose joining information is other than 1, are extracted, and these droplets are set as a droplet group DG1 (for example, the droplet element DRP1 shown in FIG. 13).

[0080] (2) From all droplets contained in droplet group DG1, droplets having representative points within a range of a preset distance D from a representative point of the droplets contained in droplet group DG1 are extracted, and these droplets are set as droplet group DG2 (for example, droplet element DRP2 shown in FIG. 13). In FIG. 13, 1301 indicates the range of distance D from droplet element DRP1, that is, the droplet extraction range.

[0081] (3) When all links LN having all droplets included in each droplet group DG2 as nodes are closed links LNC (joining information is 1), it is determined to be abnormal. Also, when droplets included in each droplet group DG2 have greater joining information than droplets included in the droplet group DG1, it is determined to be abnormal.

[0082] The abnormality in the behavior of the curable composition IM detected in this manner is displayed on the display 30 in S109 as abnormality information indicating the presence or absence of behavior of the curable composition IM together with information indicating the state (spread state) of the droplets of the curable composition IM. Fig. 14 is a diagram showing an example of an image including abnormality information displayed on the display 30 in S109. In Fig. 14, each droplet element DRP shown in Fig. 13 is iThe droplet element DRP1 determined to be abnormal is displayed in black. The droplet element DRP1 determined to be abnormal is displayed in a different color from the droplet element determined to be normal (not determined to be abnormal), for example, the droplet element DRP2. In this way, the droplets determined to be abnormal and the droplets determined to be normal are displayed in different colors (distinguishing them), so that the presence or absence of an abnormality can be visually grasped. The droplets determined to be abnormal and the droplets determined to be normal may be displayed in different display modes, for example, the droplets determined to be abnormal may be made to blink and the droplets determined to be normal may not be made to blink. In addition, in FIG. 14, the closed link LNC is shown by a solid line and the open link LNO is shown by a dashed line, so that the presence or absence of a bond between the droplets at the location where an abnormality occurs can be visually grasped.

[0083] The calculation steps including S103, S104, S105, S106, and S107 are performed for a plurality of preset times. The plurality of times are arbitrarily set within a period from the time when the mold M starts to descend from the initial position to the time when the mold M comes into contact with a plurality of droplets, the plurality of droplets spread while being crushed, the plurality of droplets bond to each other, and finally form a film, and the curable composition is cured. The plurality of times are typically set at regular time intervals.

[0084] In S108, it is determined whether the time in the calculation has reached the end time. As described above, if the time in the calculation has not reached the end time, the time is advanced to the next time and the process proceeds to S103, and if the time in the calculation has reached the end time, the process proceeds to S109. In one example, in S108, the current time is advanced by a specified time increment to become the new time. Then, if the new time has reached the end time, the process proceeds to S109.

[0085] In S109, as described above, at least one of the images shown in Fig. 12, 13, and 14 is displayed on the display 30. In S109, for example, in response to a user request, the images shown in Fig. 12, 13, and 14 may be displayed while being switched between, or some or all of the images shown in Fig. 12, 13, and 14 may be displayed.

[0086] According to this embodiment, it is possible to visually determine and recognize the behavior of multiple droplets of the curable composition IM arranged on the substrate S, particularly the presence or absence of an abnormality in the spread of the droplets. Therefore, it is possible to provide a technique that is advantageous for detecting abnormalities in the behavior of the curable composition IM in a process of forming a film of the curable composition IM in the film forming apparatus IMP. In addition, by repeatedly adjusting the droplet arrangement pattern of the curable composition IM using the simulation method of this embodiment and the results thereof, it is possible to easily set the conditions of the process while reducing abnormalities in the process of forming a film of the curable composition IM.

[0087] <Third embodiment> 15 is a flowchart for explaining the simulation method in the third embodiment. The simulation method includes steps S201, S202, S203, S204, S205, S206, S207, S208, S209, and S210. The simulation device 1 may be understood as a collection of hardware elements that execute each step of the simulation method in the third embodiment.

[0088] S201 is a step of setting conditions (simulation conditions) required for the simulation. S202 is a step of generating a link structure that connects adjacent droplets based on the droplet arrangement information of the curable composition IM set in S201. S201 and S202 may be understood as one combined step, for example, a preparation step. S203 is a step of calculating the movement of the mold M and updating the position of the mold M. S204 is a step of calculating the behavior of the droplets spread by the mold M for each of the multiple droplets of the curable composition IM based on the position of the mold M updated in S203. S205 is a step of judging whether each link of the link structure generated in S202 is closed, that is, whether the link is open or closed. S206 is a step of judging the presence or absence of a closed region formed by adjacent droplets when the spread droplets are joined together. S207 is a step of calculating joining information for each of the multiple droplets of the curable composition IM based on the results of the judgments in S205 and S206. S208 is a step of judging whether or not there is an abnormality in the behavior of the curable composition IM at that time based on the bonding information calculated in S207 and the time-series changes (i.e., detecting an abnormality in the behavior of the curable composition IM). S209 is a step of judging whether or not the time in the calculation (simulation) has reached the end time. If the time in the calculation has not reached the end time, the time is advanced to the next time and the process proceeds to S203. On the other hand, if the time in the calculation has reached the end time, the process proceeds to S210. S210 is a step of displaying at least one of the bonding information calculated in S207 and abnormality information indicating whether or not there is an abnormality in the behavior of the curable composition judged in S208, together with information indicating the state of the multiple droplets of the curable composition IM (the behavior of the curable composition IM).

[0089] Each step of the simulation method in the third embodiment will be described in detail below. However, since S201, S202, S203, S204, and S205 are similar to S101, S102, S103, S104, and S105 shown in Fig. 10, detailed description thereof will be omitted here. Also, each droplet of the curable composition IM is modeled as a droplet element DRP.

[0090] In S206, the presence or absence of a closed region formed by adjacent droplets is determined. The presence or absence of a closed region is determined by referring to whether each link of the link structure determined in S205 is closed, and by determining whether adjacent closed links are connected to each other to form a closed figure (loop).

[0091] The determination of the presence or absence of a closed region will be specifically described with reference to Figures 16(a) and 16(b). Figure 16(a) shows the spread state of the droplet elements at a certain time, and Figure 16(b) shows the spread state of the droplet elements after a certain time has passed since the state shown in Figure 16(a). In Figures 16(a) and 16(b), links LN connect adjacent droplet elements generated in S202.

[0092] At the time shown in FIG. 16(a), the link connecting the representative point C1 of the droplet element DRP1 and the representative point C3 of the droplet element DRP3 is an open link LNO 13 Similarly, the link connecting the representative point C2 of the droplet element DRP2 and the representative point C3 of the droplet element DRP3 is determined to be an open link LNO 23 Similarly, the link connecting the representative point C1 of the droplet element DRP1 and the representative point C2 of the droplet element DRP2 is determined to be an open link LNO 12 After a certain time has passed, these links are determined to be closed links LNC 13 , L.N.C. 23 and LNC 12 (That is, the liquid drop element DRP1, the liquid drop element DRP2, and the liquid drop element DRP3 are joined together.) As shown in Fig. 16(b), when a closed link LNC exists, the presence or absence of a closed region is determined.

[0093] Next, a method for determining whether or not a closed region exists will be described. First, based on the result of the determination of whether the link is open or closed, a closed link in the region of interest is selected as a starting point from among the links that have transitioned from an open link to a closed link. Next, for the starting closed link, it is determined whether an adjacent link is a closed link, and if the adjacent link is a closed link, this adjacent closed link is selected as a starting point. Then, using the adjacent closed link as a starting point, it is determined whether the adjacent link is a closed link. By repeating this process, if a closed figure is formed by the links selected as closed links, it is determined that a closed region exists. Note that when selecting adjacent closed links, if there are multiple adjacent closed links, a closed region can be appropriately extracted by continuing to select a closed link that forms a maximum (or minimum) angle between the starting closed link and the adjacent closed link.

[0094] A method for determining whether or not there is a closed region will be described in detail with reference to FIG. 16(b). First, a closed link LNC 12 Select the link LNC as the starting link. 12 Among the nodes (droplet elements DRP1 and DRP3) that make up the droplet element DRP1, one of the nodes is focused on, and a closed link is searched for among the adjacent links starting from the focused node. Here, for the node of the droplet element DRP1, the closed link LNC 14 and LNC 13 are candidates. 14 is a closed link corresponding to the link connecting the representative point C1 of the droplet element DRP1 and the representative point C4 of the droplet element DRP4. Next, the closed link LNC 12 and close link LNC 14 The angle θ between 14 and the closed link LNC 12 and close link LNC 13 The angle θ between 13 The closed link with the larger angle is selected as the next starting closed link. 13 is the angle θ 14 Since it is larger than, the next closed link is the closed link LNC 13By repeating this process, the closed link LNC 23 When selecting an adjacent closed link starting from the already selected link LNC 12 is selected again, it is determined that a closed region is formed. Fig. 17 shows a closed region formed by five droplet elements DRP1, DRP2, DRP3, DRP4, and DRP5. In Fig. 17 as well, by repeating the selection of adjacent closed links, it is possible to determine the presence or absence of a closed region formed by more droplet elements, as in Fig. 16.

[0095] In S207, the joining information is calculated using the result of the determination of whether the link LN is open or closed and the result of the determination of the presence or absence of a closed region in S106. The joining information means an evaluation value that evaluates the relationship regarding the degree of joining with adjacent droplets. In this embodiment, the joining information is the amount of bubbles contained in the closed region formed by multiple adjacent closed links.

[0096] 18(a) and 18(b) are diagrams for explaining a method for calculating the amount of air bubbles contained in a closed region. In this embodiment, the amount V of air bubbles contained in the closed region formed by the droplet elements DRP1, DRP2, and DRP3 is used as the joining information. bub Fig. 18(a) shows the state of the substrate S as viewed from above, and Fig. 18(b) shows the state of the substrate S as viewed from the side along a line 1801 shown in Fig. 18(a).

[0097] First, as shown in FIG. 18(a), the bubble area S bub The bubble area Sbub is calculated by the following formula (3): close and the area S of the droplet elements DRP1, DRP2, and DRP3 included in the closed region. drp It is calculated as the difference between

[0098]

number

[0099] Referring to FIG. 18(b), the amount of bubbles V bub is the amount of air bubbles sandwiched between the mold M and the substrate S, and is calculated by the following formula (4): Here, h is the distance (height) between the mold M and the substrate S.

[0100]

number

[0101] In the formula (4), the amount of bubbles contained in the closed region is calculated as the volume of the bubbles, but this is not limited to this. For example, the amount of gas contained in the closed region can be calculated by multiplying the number of molecules of gas contained in the bubbles, n, by the following formula (5): bub where R is the gas constant and T is the temperature.

[0102]

number

[0103] In this way, the number of gas molecules contained in the bubble is calculated as an amount proportional to the product of the gas pressure in the bubble and the volume of the bubble. The gas pressure can be calculated, for example, as the force that the bubble receives when the mold M is pressed against it.

[0104] The bonding information thus obtained is displayed on the display 30 in S210 together with information showing the state (spread state) of the droplets of the curable composition IM relative to the bonding information. Fig. 19 is a diagram showing an example of an image including the bonding information displayed on the display 30 in S210. In Fig. 19, the droplet element DRP arranged in the shot region ST of the substrate S is i For the distribution of the air bubbles, the amount of air bubbles calculated from formula (4) or formula (5) is displayed as joining information. Specifically, the amount of air bubbles is displayed by a bubble chart display in which the size of a circle 1901 is changed according to the amount (size) of air bubbles. For example, as shown in FIG. 20, iis displayed, and the size of the circle 2001 representing the amount of bubbles contained in the closed region is changed according to the amount of bubbles. This allows the amount (distribution state) of bubbles contained in the closed region to be visually grasped.

[0105] In this embodiment, the case where the size of the circle representing the air bubbles is changed according to the amount (size) of the air bubbles has been described, but the present invention is not limited to this. For example, the hue of the closed space area corresponding to the amount of the air bubbles may be changed according to the amount of the air bubbles.

[0106] In S208, the presence or absence of an abnormality in the behavior of the curable composition IM at that time is determined based on the bonding information calculated in S207 and the time-series changes (that is, an abnormality in the behavior of the curable composition IM is detected).

[0107] An example of a method for detecting abnormality in the behavior of the curable composition IM will be described below. In this embodiment, the presence or absence of an abnormality is determined (the abnormality is detected) by following the steps (1) and (2).

[0108] (1) A graph relating to the amount of bubbles contained in a closed region is generated as shown in Fig. 21. In Fig. 21, the vertical axis represents the amount of bubbles contained in a closed region, and the horizontal axis represents the number of closed regions containing bubbles.

[0109] (2) In the graph shown in FIG. 21, a threshold value is set for the amount of bubbles, and bubbles having an amount of bubbles larger than the threshold value are determined to be abnormal. Then, droplets that form a closed space containing abnormal bubbles are determined to be abnormal. The threshold value is set according to the filling time for filling the mold M with the curable composition IM. For example, when the filling time is long, a large amount of bubbles is absorbed during the filling period, so a large threshold value is set. On the other hand, when the filling time is short, a small amount of bubbles is absorbed during the filling period, so a small threshold value is set.

[0110] The amount of bubbles determined to be abnormal in this manner is displayed on the display 30 in S210 as abnormality information indicating the presence or absence of behavior of the curable composition IM. FIG. 22 is a diagram showing an example of an image including abnormality information displayed on the display 30 in S210. In FIG. 22, only bubbles determined to be abnormal are displayed as circles whose size is changed according to the amount of bubbles. This allows only bubbles determined to be abnormal to be visually confirmed, so that each droplet element DRP i It is possible to easily grasp the location of an abnormality in the liquid droplets. In this embodiment, only the bubbles determined to be abnormal are displayed, but it is preferable to display them together with information showing the state (spread state) of the droplets of the curable composition IM. This makes it possible to visually grasp the location (droplet element) where an abnormality has occurred. In addition, the bubbles determined to be abnormal may be made to blink in order to distinguish them from the other bubbles.

[0111] The calculation steps including S203, S204, S205, S206, S207, and S208 are executed for a plurality of preset times. The plurality of times are arbitrarily set within a period from the time when the mold M starts to descend from the initial position to the time when the mold M comes into contact with a plurality of droplets, the plurality of droplets spread while being crushed, the plurality of droplets bond to each other, and finally form one film, and the curable composition is cured. The plurality of times are typically set at regular time intervals.

[0112] In S209, it is determined whether the time in the calculation has reached the end time. As described above, if the time in the calculation has not reached the end time, the time is advanced to the next time and the process proceeds to S203, and if the time in the calculation has reached the end time, the process proceeds to S210. In one example, in S209, the current time is advanced by a specified time increment to become the new time. Then, if the new time has reached the end time, the process proceeds to S210.

[0113] In S210, as described above, at least one of the images shown in Fig. 19, Fig. 20, and Fig. 22 is displayed on the display 30. In S210, for example, in response to a user request, the images shown in Fig. 19, Fig. 20, and Fig. 22 may be displayed while being switched between, or some or all of the images shown in Fig. 19, Fig. 20, and Fig. 22 may be displayed.

[0114] According to this embodiment, it is possible to visually determine and recognize the behavior of multiple droplets of the curable composition IM arranged on the substrate S, particularly the presence or absence of an abnormality in the spread of the droplets. Therefore, it is possible to provide a technique that is advantageous for detecting abnormalities in the behavior of the curable composition IM in a process of forming a film of the curable composition IM in the film forming apparatus IMP. In addition, by repeatedly adjusting the droplet arrangement pattern of the curable composition IM using the simulation method of this embodiment and the results thereof, it is possible to easily set the conditions of the process while reducing abnormalities in the process of forming a film of the curable composition IM.

[0115] The present invention can also be realized by a process in which a program for implementing one or more of the functions of the above-described embodiments is supplied to a system or device via a network or a storage medium, and one or more processors in a computer of the system or device read and execute the program. The present invention can also be realized by a circuit (e.g., ASIC) for implementing one or more of the functions.

[0116] The film forming apparatus IMP, in which the simulation apparatus 1 is incorporated, controls the process of contacting a curable composition placed on a first member with a second member to form a film of the curable composition on the first member, based on a prediction by the simulation apparatus 1 of the behavior of the curable composition.

[0117] The article manufacturing method of the embodiment includes a step of determining conditions for a process in which a curable composition arranged on a first member is brought into contact with a second member while repeating the above-mentioned simulation method to form a film of the curable composition on the first member, and a step of carrying out the process according to the determined conditions. Up to this point, the embodiment has been described in terms of a configuration in which a mold has a pattern, but the present invention can also be applied to a configuration in which a substrate has a pattern.

[0118] A more specific example of a method for manufacturing an article is shown in Fig. 23. As shown in Fig. 23(a), a substrate such as a silicon wafer having a workpiece such as an insulator formed on its surface is prepared, and then an imprint material (curable composition) is applied to the surface of the workpiece by an inkjet method or the like. Here, a state in which the imprint material in the form of multiple droplets is applied onto the substrate is shown.

[0119] As shown in Fig. 23(b), the imprinting mold is placed so that the side on which the concave-convex pattern is formed faces the imprinting material on the substrate. As shown in Fig. 23(c), the substrate on which the imprinting material has been applied is brought into contact with the mold, and pressure is applied. The imprinting material fills the gap between the mold and the workpiece. When light is irradiated through the mold in this state as hardening energy, the imprinting material hardens.

[0120] As shown in Fig. 23(d), after the imprint material is cured, the mold and the substrate are separated, and a pattern of the cured product of the imprint material is formed on the substrate. In this cured product pattern, the recesses of the mold correspond to the protrusions of the cured product, and the protrusions of the mold correspond to the recesses of the cured product, i.e., the recessed and protruding patterns of the mold are transferred to the imprint material.

[0121] As shown in Fig. 23(e), when etching is performed using the pattern of the cured material as an etching-resistant mask, the portions of the surface of the workpiece where there is no cured material or where only a thin portion remains are removed, forming grooves. As shown in Fig. 23(f), when the pattern of the cured material is removed, an article having grooves formed on the surface of the workpiece can be obtained. Here, the pattern of the cured material is removed, but it may also be used as an interlayer insulating film included in a semiconductor element, i.e., a component of an article, without being removed after processing.

[0122] The invention is not limited to the above-described embodiments, and various modifications and variations are possible without departing from the spirit and scope of the invention. Accordingly, the following claims are appended to apprise the public of the scope of the invention. [Explanation of symbols]

[0123] 1: Simulation device 10: Processor 20: Memory 21: Simulation program 30: Display 40: Input device

Claims

1. A simulation method for predicting behavior of a curable composition in a process of contacting a plurality of droplets of the curable composition disposed on a first member with a second member to form a film of the curable composition in a space between the first member and the second member, comprising: A first step of determining bonding information for each of a plurality of droplets of the curable composition, the bonding information being information regarding the degree of bonding between adjacent droplets; a second step of displaying the joining information obtained in the first step and information indicating a spreading state of the plurality of droplets; A simulation method comprising the steps of:

2. The simulation method according to claim 1, characterized in that in the first step, the joining information is obtained by determining, for each of the multiple droplets of the curable composition, the proportion of the portion of the entire circumference of the droplet that is in contact with the contour of an adjacent droplet.

3. The method further includes a step of determining that each of the droplets of the curable composition is a node, and that for each of the links generated by connecting the nodes, a link to which droplets constituting the link are joined is a closed link; The simulation method according to claim 1 , wherein in the first step, a ratio of the closed links among the links of each of the droplets of the curable composition is calculated as the joining information for each of the multiple droplets of the curable composition.

4. 4. The simulation method according to claim 2, wherein in the second step, the ratio obtained in the first step is displayed in color.

5. The method further includes a step of determining that each of the droplets of the curable composition is a node, and that for each of the links generated by connecting the nodes, a link to which droplets constituting the link are joined is a closed link; 2. The simulation method according to claim 1, wherein in the first step, an amount of air bubbles contained in a closed region formed by a plurality of the closed links adjacent to each other is obtained as the joining information.

6. 6. The simulation method according to claim 5, wherein in the second step, the amount of air bubbles obtained in the first step is displayed by a size of a circle.

7. The simulation method according to any one of claims 1 to 6, further comprising a third step of determining whether or not there is an abnormality in the behavior of the curable composition during the treatment based on the bonding information obtained in the first step.

8. The simulation method according to claim 7, further comprising a fourth step of displaying both information indicating the presence or absence of an abnormality in the behavior of the curable composition in the processing determined in the third step and information indicating the spreading state of the multiple droplets of the curable composition.

9. The simulation method according to claim 8, characterized in that in the third step, when it is determined that there is an abnormality in the behavior of the curable composition during the processing, a droplet in which the abnormality is occurring is identified among the multiple droplets of the curable composition.

10. The simulation method according to claim 9, further comprising a fifth step of displaying the droplets in which the abnormality has occurred identified in the third step in a manner that makes them distinguishable from droplets in which the abnormality has not occurred.

11. The simulation method according to claim 10, characterized in that, in the fifth step, droplets in which the abnormality identified in the third step has occurred and droplets in which the abnormality has not occurred are displayed in different colors.

12. 11. The simulation method according to claim 10, wherein in the fifth step, the droplet in which the abnormality has occurred and which has been identified in the third step is caused to blink.

13. A simulation device for predicting behavior of a curable composition in a process of contacting a plurality of droplets of the curable composition disposed on a first member with a second member to form a film of the curable composition in a space between the first member and the second member, the simulation device comprising: a processor that determines, for each of the plurality of droplets of the curable composition, bonding information that is information regarding the degree of bonding with adjacent droplets, and displays, on a display, the bonding information and information indicating a spreading state of the plurality of droplets; A simulation device comprising:

14. A film forming apparatus incorporating the simulation apparatus according to claim 13, A first holding portion that holds the first member; A second holding portion that holds the second member; a drive unit that drives at least one of the first holding unit and the second holding unit; A control unit that controls the drive unit, the control unit controls driving of the drive unit to adjust the relative positions of the first member and the second member, and performs a process of bringing a plurality of droplets of the curable composition into contact with the second member based on a prediction by the simulation device of a behavior of the curable composition placed on the first member, and forming a film of the curable composition in a space between the first member and the second member. A film forming apparatus comprising:

15. determining conditions for a process in which a plurality of droplets of a curable composition disposed on a first member are brought into contact with a second member while repeating the simulation method according to any one of claims 1 to 12, and a film of the curable composition is formed in a space between the first member and the second member; executing the process according to the condition; A method for producing an article, comprising:

16. A program for causing a computer to execute the simulation method according to any one of claims 1 to 12.

Citation Information

Patent Citations

  • Additive for alkanol amineetolu oil fatty acid coal flotation method

    JP1980099356A

  • Imprint lithography method and apparatus

    JP2010183076A

  • Defect inspection device and image display method

    JP2011038947A

  • Simulation method, program, recording medium recording program, creation method of droplet arrangement pattern using recording medium, nanoimprint method, manufacturing method of patterned substrate and ink jet device

    JP2012212833A

  • Device and method for surface inspection

    JP2014211440A