Method, planarization system, and method for manufacturing an article - Patents.com

The method of using fluid pressure differentials and mechanical forces to separate the superstrate from the substrate addresses irregular topography challenges, enhancing planarization uniformity and efficiency in semiconductor manufacturing.

JP7555967B2Active Publication Date: 2024-09-25CANON KK
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021568423
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-08-15
Filing Date
2020-07-17
Publication Date
2024-09-25
Estimated Expiration
2040-07-17

AI Technical Summary

Technical Problem

Existing planarization techniques in semiconductor manufacturing face challenges in achieving uniformity and efficiency due to irregular substrate topography, leading to issues such as non-uniform layer deposition and difficulty in separating the superstrate from the substrate.

Method used

A method involving the use of fluid pressure differentials and mechanical forces to initiate and propagate cracks at the edge of the substrate-superstrate interface, combined with a multi-zone superstrate chuck design to control curvature and facilitate separation, minimizing defects and non-uniformity.

Benefits of technology

Enhances the planarization process by reducing non-filling defects and ensuring uniformity of the planarization layer, while allowing for efficient separation of the superstrate, thereby improving overall substrate processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555967000002
    Figure 0007555967000002
  • Figure 0007555967000003
    Figure 0007555967000003
  • Figure 0007555967000004
    Figure 0007555967000004
Patent Text Reader

Abstract

A method is provided that includes generating at least one crack at a point on an edge of at least a substrate and superstrate stack, propagating the crack around a periphery, and moving the superstrate relative to the substrate to complete separation of the superstrate from the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to substrate processing, and more particularly, to planarizing surfaces in semiconductor manufacturing. [Background technology]

[0002] Planarization techniques are useful in manufacturing semiconductor devices. For example, the process for creating semiconductor devices involves repeated addition and removal of material to and from a substrate. This process can produce a layered substrate with irregular height variations (i.e., topography), and as more layers are added, the substrate height variations can increase. The height variations negatively impact the ability to add additional layers to the layered substrate. Apart from this, the semiconductor substrate (e.g., silicon wafer) itself is not always perfectly flat and can contain initial surface height variations (i.e., topography). One way to address this issue is to planarize the substrate between deposition steps. Various lithographic patterning methods benefit from patterning on a planar surface. In ArFi laser-based lithography, planarization improves depth of focus (DOF), critical dimension (CD), and critical dimension uniformity. In extreme ultraviolet lithography (EUV), planarization improves feature placement and DOF. In nanoimprint lithography (NIL), planarization improves feature filling and CD control after pattern transfer.

[0003] Planarization techniques, sometimes referred to as inkjet-based adaptive planarization (IAP), involve dispensing a variable drop pattern of a polymerizable material between a substrate and a superstrate, where the drop pattern varies depending on the substrate topography. The superstrate is then contacted with the polymerizable material, after which the material is polymerized on the substrate and the superstrate is removed. Improvements in planarization techniques, including IAP techniques, are desired, for example, to improve full-wafer processing and semiconductor device manufacturing. Summary of the Invention

[0004] A method is provided that includes generating at least one crack at a point on an edge of a stack of at least a substrate and a superstrate, propagating the crack along a perimeter, and moving the superstrate relative to the substrate to complete separation of the superstrate from the substrate. The method may further include introducing a positive fluid pressure between the substrate and the superstrate at the point on the edge to generate the crack. The positive fluid pressure may include a flow of clean dry air, helium, or nitrogen. The method may further include holding the superstrate on a superstrate chuck with a negative fluid pressure, and applying a high flow of negative fluid pressure to a peripheral zone on the superstrate to propagate the crack along the edge of the stack.

[0005] The positive fluid pressure is continuously introduced to the separated portion while a high flow of the negative fluid pressure is applied to the peripheral zone on the superstrate. The superstrate may be moved away from the substrate with a superstrate chuck. The method may further include applying a negative fluid pressure to a central zone on the superstrate to complete the separation of the superstrate from the substrate with a superstrate chuck. The method may further include applying a force to the point on an edge of the superstrate to generate the crack. Other cracks may be generated by applying a positive fluid pressure between the substrate and the superstrate at other points on the edge of the stack. The force may be applied by introducing a positive fluid pressure or mechanical contact.

[0006] The method may further include laminating the substrate and the superstrate such that the superstrate includes an overhanging edge portion and applying a force to the overhanging edge portion to create a crack. Another edge portion of the superstrate may be aligned with a notch in an edge portion of the substrate and a force is applied to the other edge portion to create another crack between the substrate and the superstrate.

[0007] A chucking system is also provided, the system including a superstraight chuck configured to hold a superstraight with a negative fluid pressure, and a force source configured to apply a force to a point on an edge of the superstraight stacked with a substrate to generate a crack between the substrate and the superstraight at the point of the edge. The superstraight chuck includes a pattern of lands, one of the lands located near the edge of the superstraight chuck being recessed below another land located on an inner portion of the superstraight chuck to allow the superstraight to deflect toward the superstraight chuck while generating the crack. The chucking system may further include a substrate chuck configured to hold the substrate with a negative fluid pressure. The substrate chuck includes a pattern of lands, one of the lands located near the edge of the substrate chuck being recessed below another land located on an inner portion of the substrate chuck to allow the substrate to deflect toward the substrate while generating the crack.

[0008] The force source may include a mechanism for generating a lateral mechanical force or a source of positive fluid pressure directed toward the edge of the superstrate. The substrate may include a notch disposed at its edge, and the force source may include a source of negative fluid pressure applied to the superstrate through the notch. The chucking system may further include a source of negative fluid pressure for applying the negative fluid pressure to the superstrate through the superstrate chuck. The superstrate chuck is configured to hold the superstrate such that the superstrate includes an overhanging portion. The force source is configured to apply a force to the overhanging portion of the superstrate to initiate the crack.

[0009] A method of manufacturing an article is provided that includes forming a cured material deposited between a substrate and a superstrate, generating at least one crack at a point at an edge between the substrate and the superstrate, propagating the crack circumferentially, and separating the superstrate from the cured material.

[0010] These and other objects, features, and advantages of the present disclosure will become apparent from a reading of the following detailed description of illustrative embodiments thereof in conjunction with the accompanying drawings and the appended claims. [Brief description of the drawings]

[0011] So that the features and advantages of the present invention may be understood in detail, a more particular description of the embodiments of the present invention may be made by reference to the embodiments illustrated in the accompanying drawings. It should be noted, however, that the accompanying drawings only illustrate typical embodiments of the present invention and therefore should not be considered as limiting the scope of the present invention, since the invention may admit of other equally effective embodiments.

[0012] [Figure 1] FIG. 1 is a diagram showing a planarization system;

[0013] [Figure 2A] Figure 2a shows the planarization process; [Figure 2B] Figure 2b shows the planarization process; [Figure 2C] Figure 2c shows the planarization process;

[0014] [Figure 3A] FIG. 3a shows a multi-zone straight chuck in one embodiment; [Figure 3B] FIG. 3b shows a multi-zone straight chuck in one embodiment;

[0015] [Figure 4A] FIG. 4a shows the operation of the superstrate chuck to form a layer on a substrate; [Figure 4B] FIG. 4b shows the operation of the superstrate chuck to form a layer on the substrate; [Figure 4C] FIG. 4c shows the operation of the superstrate chuck to form a layer on the substrate; [Figure 4D] FIG. 4d shows the operation of the superstrate chuck to form a layer on the substrate; [Figure 4E] FIG. 4e shows the operation of the superstrate chuck to form a layer on the substrate;

[0016] [Diagram 5] FIG. 5 is a flow chart of the planarization process shown in FIGS. 4a to 4e;

[0017] [Figure 6A] FIG. 6a shows a separation crack initiating at the edge of a substrate and superstrate stack in one embodiment; [Figure 6B] Figure 6b shows the alignment of the retractable pin with the substrate notch to initiate such a separation crack;

[0018] [Figure 6C] FIG. 6b shows a separation crack initiating at the edge of the substrate and superstrate stack in another embodiment;

[0019] [Figure 7A] Figure 7a shows a top view of a substrate and superstrate stack as a separation crack initiates and propagates around the stack; [Figure 7B] Figure 7b shows a top view of the substrate and superstrate stack as a separation crack initiates and propagates around the stack; [Figure 7C] Figure 7c shows a top view of the substrate and superstrate stack as a separation crack initiates and propagates around the stack;

[0020] [Figure 8] FIG. 8 shows the separated substrate and superstrate;

[0021] [Figure 9] FIG. 9 is a flow chart of the separation process shown in FIGS. 7 and 8 ;

[0022] [Figure 10] FIG. 10 shows a separation crack initiating at the edge of a substrate and superstrate stack in a further embodiment;

[0023] [Figure 11A] FIG. 11a shows a multi-zone superstrate chuck in another embodiment with improved zone sealing; [Figure 11B] FIG. 11b shows a multi-zone superstrate chuck in another embodiment with improved zone sealing;

[0024] [Figure 12]FIG. 12 shows an expanded view of an exemplary trench structure within a zone of the superstrate chuck of FIGS. 11a and 11b.

[0025] Throughout the drawings, the same reference numerals and characters, unless otherwise stated, are used to denote like features, elements, components or portions of the illustrated embodiments. Moreover, while the present disclosure will be described in detail with reference to the drawings, it is done so in connection with illustrative exemplary embodiments. It is intended that changes and modifications can be made to the exemplary embodiments described without departing from the true scope and spirit of the subject disclosure as defined by the appended claims. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0026] Flattening System 1 shows a system for planarization. Planarization system 100 is used to planarize a film on a substrate 102. Substrate 102 may be coupled to a substrate chuck 104. Substrate chuck 104 may be, but is not limited to, a vacuum chuck, a pin-type chuck, a groove-type chuck, an electrostatic chuck, an electromagnetic chuck, etc.

[0027] The substrate 102 and the substrate chuck 104 may be further supported by a substrate positioning stage 106. The substrate positioning stage 106 may provide translational and / or rotational motion along one or more of the x-, y-, z-, θ-, ψ, and φ-axes. The substrate positioning stage 106, the substrate 102, and the substrate chuck 104 may also be positioned on a base (not shown). The substrate positioning stage may be part of a positioning system.

[0028] Spaced apart from the substrate 102 is a superstrate 108 having a working surface 112 facing the substrate 102. The superstrate 108 may be formed from materials including, but not limited to, fused silica, quartz, silicon, organic polymers, siloxane polymers, borosilicate glass, fluorocarbon polymers, metals, hardened sapphire, and the like. In one embodiment, the superstrate is readily transparent to UV light. The surface 112 is generally the same area size as the surface of the substrate 108 or slightly smaller.

[0029] The superstraight 108 may be coupled to or held by a superstraight chuck 118. The superstraight chuck 118 may be, but is not limited to, a vacuum chuck, a pin-type chuck, a groove-type chuck, an electrostatic chuck, an electromagnetic chuck, and / or other similar chuck types. The superstraight chuck 118 may be configured to apply a stress, pressure, and / or strain to the superstraight 108 that varies across the superstraight 108. In one embodiment, the superstraight chuck is also readily transparent to UV light. The superstraight chuck 118 may include a system, such as a zone-based vacuum chuck, an actuator array, a pressure bladder, or the like, that can apply a pressure differential to the backside of the superstraight 108 to bend and deform the template. In one embodiment, the superstraight chuck 118 includes a zone-based vacuum chuck that can apply a pressure differential to the backside of the superstraight to bend and deform the superstraight as described in further detail herein.

[0030] The superstraight chuck 118 may be coupled to a planarizing head 120 that is part of a positioning system. The planarizing head 120 may be movably coupled to the bridge. The planarizing head 120 may include one or more actuators, such as a voice coil motor, a piezoelectric motor, a linear motor, a nut and screw motor, etc., configured to move the superstraight chuck 118 relative to the substrate 102 in at least the z-axis direction, and potentially in other directions (e.g., x-, y-, θ-, ψ-, φ-axes).

[0031] The planarization system 100 may further include a fluid dispenser 122. The fluid dispenser 122 may also be movably coupled to the bridge. In one embodiment, the fluid dispenser 122 and the planarization head 120 share one or more of all positioning components. In an alternative embodiment, the fluid dispenser 122 and the planarization head move independently of one another. The fluid dispenser 122 may be used to deposit droplets of a liquid formable material 124 (e.g., a photocurable polymerizable material) onto the substrate 102, with the volume of the deposited material varying across an area of ​​the substrate 102 based at least in part on its topographical profile. Different fluid dispensers 122 may use different techniques to dispense the formable material 124. If the formable material 124 is jettable, an inkjet type dispenser may be used to dispense the formable material. For example, thermal inkjet, microelectromechanical systems (MEMS)-based inkjet, valve jet, and piezoelectric inkjet are common technologies for dispensing jettable liquids.

[0032] The planarization system 100 may further include a curing system including a radiation source 126 that directs actinic energy, such as UV radiation, along an exposure path 128. The planarization head 120 and substrate positioner 106 may be configured to position the superstrate 108 and the substrate 102 in overlap with the exposure path 128. The radiation source 126 delivers actinic energy along the exposure path 128 after the superstrate 108 contacts the moldable material 124. FIG. 1 illustrates the exposure path 128 when the superstrate 108 is not in contact with the moldable material 124. This is done for illustrative purposes so that the relative positions of the individual components can be easily identified. Those skilled in the art will appreciate that the exposure path 128 does not substantially change when the top plate 108 contacts the moldable material 124.

[0033] The planarization system 100 may further include a camera 136 positioned to view the extension of the moldable material 124 as the superstrate 108 contacts the moldable material 124 during the planarization process. FIG. 1 shows an optical axis 138 of the image field of the field camera. As shown in FIG. 1, the planarization system 100 may include one or more optical elements (dichroic mirrors, beam combiners, prisms, lenses, mirrors, etc.) that combine the actinic radiation with the light detected by the camera 136. The camera 136 may include one or more of a CCD, a sensor array, a line camera, and a photodetector configured to collect light at wavelengths indicative of a contrast between areas under the superstrate 108 that contact the formable material 124 and areas under the superstrate 108 that do not contact the formable material 124. The camera 136 may be configured to provide an image of the extension of the moldable material 124 under the superstrate 108 and / or the separation of the superstrate 108 from the hardened moldable material 124. The camera 136 may also be configured to measure the changing interference patterns as the formable material 124 spreads across the gap between the surface 112 and the substrate surface.

[0034] The planarization system 100 may be coordinated, controlled, and / or directed by one or more processors 140 (controllers) in communication with one or more components and / or subsystems, such as the substrate chuck 104, the substrate positioning stage 106, the superstrate chuck 118, the planarization head 120, the fluid dispenser 122, the radiation source 126, and / or the camera 136. The processor 140 may operate based on instructions in a computer-readable program stored in a non-transitory computer memory 142. The processor 140 may be or include one or more of a CPU, MPU, GPU, ASIC, FPGA, DSP, and general-purpose computer. The processor 140 may be a general-purpose controller or a general-purpose computing device configured to be a controller. Examples of non-transitory computer readable memory include, but are not limited to, RAM, ROM, CDs, DVDs, Blu-Ray, hard drives, network attached storage (NAS), intranet connected non-transitory computer readable storage devices, and internet connected non-transitory computer readable storage devices.

[0035] During operation, the planarizing head 120, the substrate position stage 106, or both vary the distance between the superstrate 118 and the substrate 102 to define a desired space (a bounded physical extent in three dimensions) to be filled with the moldable material 124. For example, the planarizing head 120 is moved toward the substrate and applies a force to the superstrate 108 such that the superstrate contacts and spreads the droplet of moldable material 124, as described in further detail herein.

[0036] Planarization Process The planarization process includes the steps shown generally in Figures 2a-c. As shown in Figure 2a, moldable material 124 is dispensed in the form of droplets onto substrate 102. As previously mentioned, the substrate surface has some topography that may be known based on previous process operations or may be measured using a profilometer, AFM, SEM, or an optical surface profiler based on optical interference effects such as the Zygo NewView 8200. The local volume density of the deposited moldable material 124 varies according to the substrate topography. The superstrate 108 is then positioned in contact with moldable material 124.

[0037] FIG. 2b illustrates a post-contact step after the superstrate 108 has fully contacted the moldable material 124, but before the polymerization process begins. As the superstrate 108 contacts the moldable material 124, the droplets merge to form a film 144 of moldable material that fills the space between the superstrate 108 and the substrate 102. Preferably, the filling process occurs uniformly without air or gas bubbles being trapped between the superstrate 108 and the substrate 102 to minimize non-fill defects. The polymerization process or curing of the moldable material 124 may be initiated with actinic radiation (e.g., UV radiation). For example, the radiation source 126 of FIG. 1 may provide actinic radiation that cures, solidifies, and / or crosslinks the film 144 of formable material, defining a hardened planarization layer 146 on the substrate 102. Alternatively, the curing of the film 144 of moldable material may be initiated by using heat, pressure, a chemical reaction, other types of radiation, or any combination thereof. Once cured, a planarization layer 146 is formed and the superstrate 108 may be separated therefrom. Figure 2c shows the cured planarization layer 146 on the substrate 102 after separation of the superstrate 108. The substrate and cured layer may then undergo additional known steps and processes for device (article) fabrication including, for example, patterning, curing, oxidation, layering, deposition, doping, planarization, etching, removal of moldable material, dicing, bonding, and packaging. The substrate may be processed to fabricate multiple articles (devices).

[0038] Spreading, filling and curing of planarization material between the superstrate and the substrate One scheme for minimizing the entrapment of air or gas bubbles between the superstrate 108 and the substrate as the formable material droplets spread, merge, and fill the gap between the superstrate and the substrate is to position the superstrate so that it makes initial contact with the formable material at the center of the substrate, makes further contact, and then proceeds radially from the center to the periphery. This requires deflection or bowing of the superstrate or substrate or both to create a curvature profile within the superstrate. However, given that the superstrate 108 is typically of the same or similar areal dimensions as the substrate 102, a useful overall superstrate bowed curvature profile requires both a large vertical deflection of the superstrate and a concomitant vertical motion by the superstrate chuck and planarization assembly. Such large vertical deflections and motions may be undesirable for control, precision, and system design considerations. Such a superstrate profile can be obtained, for example, by applying back pressure to an interior region of the superstrate. However, doing so still requires a peripheral retention region to keep the superstrate retained on the superstrate chuck. If both the superstrate and the peripheral edge of the substrate are chucked flat while the droplet of moldable material spreads and merges, there will be no superstrate curvature profile available in this flat chuck region. This can impair the spreading and merging of the droplet, which can also result in non-fill defects in that region. Additionally, once the spreading and filling of the moldable material is complete, the resulting stack of the superstrate chuck, chucked superstrate, moldable material, substrate, and substrate chuck can become an over-constrained system. This can cause a non-uniform planarization profile of the resulting layer of planarization film.That is, in such an overconstrained system, any flatness errors or variations from the superstrate chuck, including front and back surface flatness, can be transferred to the superstrate and affect the layer uniformity of the planarizing film.

[0039] To solve the above problems, in one embodiment, a multi-zone superstraight chuck 118 is provided, as shown in Figures 3a and 3b. The superstraight chuck 118 includes a central zone 301 and a series of ring zones 303 around the central zone 301. The ring zones 303 may be defined into a peripheral ring zone 303b around the edge, periphery, or periphery of the superstraight chuck 118 and a plurality of inner ring zones 303a located between the central zone 301 and the peripheral ring zone 303b. The plurality of ring zones 303 may be defined by a series of lands 307 protruding from a surface of the superstraight chuck 118. As shown in Figures 3a and 3b, the lands 307 may be formed around the central zone 301. Each of the ring zones 303 is formed with at least one port 305 to connect through the superstrate chuck 118 and allow a pressure source to apply positive or negative pressure, e.g., a vacuum, to the superstrate held thereby.

[0040] FIG. 3b shows a side cross-sectional view of the superstraight chuck 118. Each of the lands 307 protrudes from the surface of the superstraight chuck 118 having a height. The lands 307 include a peripheral land 307b surrounding the peripheral ring zone 303b and a series of inner lands 307a between the central zone 301 and the peripheral ring zone 303b. As shown in FIG. 3b, the inner lands 307a have substantially the same height, but the height of the peripheral land 307b is less than the height of the inner land 307a. The central zone 301 of the superstraight chuck 118 may be in the shape of a circular cavity such that a pressure source (not shown) can apply air or gas pressure through associated channels 308 and ports 305 to deflect the central portion of the retained superstraight. Similarly, a vacuum pressure may be applied to the central zone 301 through the same channels and ports. The central zone 301 of the superstraight chuck 118 may be aligned with the central portion of the retained superstraight. Similarly, the peripheral ring zone 303a may be aligned with the outer periphery or edge of the held superstrate. The peripheral ring zone 303 is similarly provided with respective channels 308 and ports 305 for application of pressure or vacuum.

[0041] 4a-4e, a process for contacting, spreading, and merging the deposited droplets of moldable material 124 is shown. As shown in FIG. 4a, before contacting the superstraight 108 with the moldable material 124, a positive pressure (indicated by arrow P) is applied to the central zone 301 of the superstraight chuck 118 through port 305 to deflect the central portion of the superstraight 108 toward the moldable material 124. The pressure P is applied to the central zone 301 to control the initial deflection within a predetermined range and maintain a predetermined curvature of the superstraight 108, as shown in FIG. 4a. Meanwhile, a negative pressure, preferably a vacuum (indicated by arrow V), is applied to the superstraight 108 through port 305 in the ring zone 303 to hold the superstraight 108 together with the superstraight chuck 118. The superstraight 108 is then brought into initial contact with the droplets of moldable material 124, as shown in FIG. 4b.

[0042] The deflection of the superstrate 108 is then expanded radially outward from the central portion by sequentially releasing the vacuum (V) from the inner ring zones 303a proximal to the central zone 301. In this manner, the droplets of moldable material are contacted, spread, and merge to form a film layer having a fluid front end that advances radially outward as the superstrate contacts and conforms to the substrate. As the vacuum is sequentially released from the inner ring zones 303a, the pressure P applied through the central zone 301 is maintained at a desired value. Also, pressure P may be applied to the superstrate 108 through the channels 308 and ports 305 in the inner ring zones 303a where the vacuum was released. In the embodiment shown in FIG. 4c, the vacuum is sequentially released from the three inner rings 303a closest to the inner zone 301, and pressure P is sequentially applied as the vacuum is sequentially released. The flattening head may be moved downward during this sequential vacuum release and pressurization.

[0043] The deflection of the superstrate 108 is then sequentially expanded further radially while the vacuum V applied through the peripheral ring zone 303b is maintained until the vacuum is released from all the inner ring zones 303a. For each of the inner ring zones 303a, a pressure P is also applied as the vacuum is released. As shown in FIG. 4d, when the vacuum is released from all the inner ring zones 303a, the superstrate 108 is deflected to conform to the substrate 102, except for the peripheral edge of the substrate 108, which remains held by the superstrate chuck 118 via the vacuum V applied through the peripheral zone 303b. Thus, the edge of the superstrate 108 remains in a deflected, curved state due to the eventual spreading and merging of the droplets of moldable material dispensed on the peripheral edge of the substrate 102. Additionally, the peripheral land 307b, which is lower than the inner land 307a, facilitates the maintenance of such a curve.

[0044] Then, in FIG. 4e, the vacuum V applied through the peripheral ring zone 303b is released to completely release the superstraight 108 from the superstraight chuck 118. This provides several advantages. First, by releasing the periphery of the superstraight 108 from the peripheral ring zone 303b that was held in a curved state, the spreading and merging of the remaining moldable material droplets can be completed in the same center-to-periphery radial manner, thus continuing to minimize air or gas entrapment and resulting non-fill defects. Specifically, the peripheral land 307b, which is recessed relative to the inner land 307a, allows the superstraight 108 to maintain the desired curvature prior to release. Second, by completely releasing the superstraight 108 from the superstraight chuck 118, any over-constraint of the superstraight 108 due to the chucking conditions is removed, thereby reducing localized non-uniform flattening that may occur due to such constraint conditions. Third, the release of the superstrate 108 from the superstrate chuck 118 eliminates the transfer of any chuck non-flatness errors or variations to the superstrate 108, thereby reducing local non-uniform planarization variations.

[0045] Once the superstrate 108 is released, curing energy is applied to cure the moldable material to form a planarizing layer. As previously described, the curing source may be a light beam to cure the moldable material 124. In one embodiment, the size of the light beam may be adjusted or controlled with reference to the diameter of the superstrate. The light beam may also be controlled to be incident on the substrate at a predetermined angle. During curing, the lateral position (i.e., in the XY plane) of the substrate 102 relative to the curing source may be adjusted. After the curing process, the superstrate 108 is re-held by the superstrate chuck 118, after which the superstrate 108 is separated from the substrate as further described herein.

[0046] FIG. 5 shows a flow chart of the planarization process described as shown in FIG. 3 and FIG. 4. In step S501, a droplet 124 of moldable material is dispensed onto the substrate 102. A central zone of the superstraight 108 is deflected toward the droplet 124 of moldable material in step S502. The deflected superstraight 108 is then advanced by the superstraight chuck 118 into contact with the moldable material 124 in step S503. The deflection of the superstraight 108 is extended from the central zone toward the outer periphery of the superstraight 108 in step S504. The superstraight chuck 118 then stops applying force to hold the superstraight 108, for example, by a vacuum applied to the outer periphery of the superstraight 108, and the superstraight 108 is released (i.e., dechucked) from the superstraight chuck 118 in step S506. The moldable material 124 is cured in step S507. After curing, the superstrate 108 is re-held by the superstrate chuck 118 to separate the superstrate 108 from the cured moldable material 146 .

[0047] For example, when using a UV light curable material as the moldable material 124, it is desirable for the superstrate chuck 118 to be transparent with high UV light transmission for UV curing (e.g., as well as high light transmission for imaging by the camera 136, as shown in FIG. 1). As mentioned above, the air supply channels 308 and ports 305, the zones 303, and the lands 307 are integrated into the superstrate as shown in FIGS. 3 and 4. These structures can cause problems for UV curing. In particular, the UV transmission in the areas under the channels 308 and the lands 307 can be significantly reduced compared to areas without such features, resulting in under-curing or uneven curing of the moldable material. This phenomenon is sometimes referred to as the "shadow effect." The shadow effect is especially important at the edges of the lands 307. Furthermore, when the superstrate 100 is chucked to the lands 307, a thin air gap exists because the two surfaces are not in optical contact with each other. This type of thin gap can completely block the UV. This phenomenon is known as the "thin film effect" between the land and the superstrate.

[0048] One solution to the "shadow effect" described above involves moving the stack of superstrate and substrate on the wafer stage in x, y and / or θ coordinates after dechucking (i.e., releasing) the superstrate from the superstrate chuck. By moving the wafer stage in this manner during UV exposure, areas of the superstrate and substrate that would have remained under the channels, ports, and lands can be periodically moved to areas under the superstrate chuck where no chuck features are present. The required relative motion can be estimated from equation (1) below: JPEG0007555967000001.jpg17166 Here, I m is the desired average intensity over the range of motion, and I h is the high intensity (i.e., the maximum or "max" intensity) over the featureless regions of the chuck, and I lis the intensity at the feature of interest (i.e., the lowest or "low" intensity), and w h I m is the estimated range of motion to achieve l is the target feature width (e.g., width of a land, port, or channel). For example, assuming 100% UV transmission in feature-free areas, the desired I m Assume that w is 90% of that value, and i = 1 mm, from equation (1), the desired range of relative motion w h = 8.0 mm. Alternatively, the UV source can be moved by tilting or tilting it with respect to the superstraight chuck to change the angle of the UV light incident on the superstraight chuck, which can also reduce shadow effects near the feature of interest. The "pellicle effect" can be avoided by a relative movement in the z-axis direction to create a sufficient gap between the superstraight and the superstraight chuck, for example by dechucking the superstraight and moving the wafer stage in the z-direction away from the superstraight chuck. The various solutions above can be applied individually or in combination to improve the uniformity of the total UV dose in a particular area and minimize shadow and pellicle effects. In various embodiments, the applied UV light beam can be smaller, the same size, or larger than the substrate or superstraight. In one embodiment, the applied UV light beam can be moved by the above relative movement w while continuing to expose the entirety of the substrate to UV light. h The substrate may be larger than the substrate by a size that accommodates the

[0049] Separation of the superstrate from the cured planarization film layer Once the moldable material has cured and a layer of planarization film has been formed, it is necessary to remove or peel the superstrate from the formed layer. However, when the superstrate and substrate have the same or similar areal dimensions, it is difficult to initiate and propagate a separation crack between the superstrate and the formed layer as needed to completely separate the superstrate from the formed layer. This problem can be solved by the structure and method shown in Figures 6-8. As shown in Figures 6a and 6b, the substrate chuck 604 includes a retractable pin 606 located at the periphery of the chuck that can be aligned with a notch 608 on the substrate 102. Such notches (e.g., wafer notches) are common on semiconductor wafers for the purpose of orienting the wafer during processing and handling. In operation, the retractable pin 606 is positioned in alignment with a notch 608 located on the substrate 102. To initiate separation, the pin 606 moves upward through the notch 608 and contacts a point 610 on the edge of the superstrate 108, as shown in Figure 6a. The force applied by the pin 606 is sufficient to initiate a separation crack 601 between the superstraight 108 and the stiffening layer 146 on the substrate 102. Once the crack 601 is created, the application of vacuum pressure through the port 305 of the superstraight chuck 118 causes the edge of the superstraight 108 to deflect toward the superstraight chuck 118. This is facilitated by the land 307b of the superstraight chuck 118 being shorter than the adjacent land 307a, which provides space for the edge of the superstraight 108 to deflect away from the substrate 102 toward the superstraight chuck 118. The force applied to create the crack 601 can depend on the geometry and physical conditions of the superstraight, the layer of planarizing film, and the substrate. Alternatively, the crack 601 may be created by introducing a positive pressure between the substrate 102 and the superstraight 108, as shown in FIG. 6c. Here, the substrate chuck 614 includes a nozzle 616 connected to a positive fluid pressure source (not shown). Activation of nozzle 616 generates a positive fluid pressure P Iis delivered through nozzle 616 to a point 610 at the edge of superstrate 118 with sufficient force to initiate separation crack 601. The positive fluid pressure may include a flow of clean dry air, helium, or nitrogen. During the generation of crack 601, superstrate 102 is held within superstrate chuck 118 and substrate 102 is held by substrate chuck 104.

[0050] 7-8 show the progression of separation. FIG. 7a shows a top-down view in which the superstrate 118 is in full contact (as indicated by the shaded area) with the layer formed on the substrate. In FIG. 7b, a separation crack 601 is initiated as described above. Once the crack 601 is initiated, a negative pressure or high vacuum flow is applied to the outer ring zone 303b of the superstrate chuck 118 to engage the edge of the superstrate 108 and propagate the separation crack 601 around the outer zone ring 303b. This propagation proceeds circumferentially in both directions from the notch 608, as indicated by arrows C. To aid in the propagation of the crack 601 around the outer ring zone 303b, additional lateral air flow (not shown) may be provided between the substrate 102 and the superstrate 108 as the crack propagation proceeds. FIG. 7c shows the crack 601 propagated completely around the outer ring zone 303b.

[0051] Once the separation crack has propagated completely around the outer ring zone, an upward motion can be applied along the Z-axis direction of the superstrate 108 to complete the separation of the superstrate 108 from the stiffening layer on the substrate. FIG. 8 shows the superstrate 108 fully separated from the substrate 102. In completing the separation, significant upward motion of the superstrate 108 relative to the substrate 102 can induce shear stresses in the remaining contact areas between the superstrate 108 and the substrate 102. Alternatively, the Z-direction motion can be stopped at an earlier desired location and the separation can proceed and concluded through continued application of vacuum pressure to the inner and / or central ring zones. Such shear stresses can be minimized by applying a vacuum to one or more of the inner ring zone 303a and / or central zone 301 during continued separation.

[0052] FIG. 9 shows a flow chart of the separation process described and shown in FIG. 7 and FIG. 8. In step S901, a separation crack is initiated between the superstrate 108 and the stiffening layer. Then, in step S902, the separation crack is propagated around the periphery of the superstrate 108. In step S903, the remainder of the superstrate is separated from the stiffening layer. In the above-mentioned embodiment, the separation of the superstrate 108 and the substrate 102 includes the steps of generating a crack by mechanical force such as a push pin or air pressure, applying a vacuum pressure to the outer zone to propagate the crack and hold the superstrate 108 tightly, moving the superstrate 108 upward in the Z direction and away from the substrate 102 with a safe force sufficient to avoid the superstrate dechucking upward, and applying a vacuum to the center of the superstrate 108 during the upward Z direction movement to complete the separation. Alternatively, or in combination with the Z-motion scheme described above, separation propagation can be influenced by the continuous application of in-plane (or lateral) flow at high pressure from one or more sides of the substrate (not shown).

[0053] In the embodiment of FIG. 6, crack initiation is initiated by an upward force applied through the wafer notch 608 by either a mechanical pin 606 (FIG. 6a) or a fluid nozzle 616 (FIG. 6b). FIG. 10 illustrates a further embodiment of a substrate chuck configured to initiate a separation crack. Here, the substrate chuck 624 includes a separate retractable pin 626 that can initiate a separation crack when the superstrate 108 and the substrate are non-concentrically positioned. This non-concentric positioning results in a portion 628 of the superstrate 108 overhanging the substrate 102. The crack 602 can be generated by applying a force to the overhanging portion 110 via movement of the pin 626. Alternatively, the overhanging portion 608 can be obtained by using a superstrate that is slightly larger than the substrate. In this manner, the superstrate 108 can still be concentrically positioned with the substrate 102. In either case, the substrate chuck 624 may further include mechanical pins or nozzles spaced apart from the pins 626, such as in the embodiment of FIG. 6 a or 6 b, or otherwise, to generate multiple points around the periphery of the superstrate for initiating a separation crack.

[0054] Super Straight Chuck As mentioned above, the superstrate 108 is preferably held or supported by a superstrate chuck 118 that applies a pressure or vacuum (negative pressure) to the volume between the superstrate and the chucking surface in a ring zone 303 defined by lands 307 extending from the chucking surface. Apart from the outermost land 307a, the inner lands 307b preferably have the same height so that the gap depth between adjacent inner lands 307b remains constant. The land height (i.e., gap depth) is typically kept very small, for example, on the order of about tens of microns to thousands of microns, for reasons such as minimizing limitations in gas fill or exhaust response time, land stiffness characteristics, and thermal effects such as expansion or contraction. In operation, when a vacuum is applied to the ring zone to hold the superstrate against the lands of the zone, a vacuum seal is created at the superstrate-land interface. However, if sufficient force or pressure is applied to the superstrate in the opposite direction to the chucking vacuum, the substrate may be lifted off the lands of the chuck. At certain gaps between the superstrate and the lands, the vacuum seal may break or leak, causing the vacuum pressure in the zone to drop or even become zero. The superstrate may then become unintentionally dechucked from the chuck. Furthermore, even if the superstrate does not become dechucked, vacuum leakage may disrupt the level of control required, for example, when sequentially releasing the vacuum pressure in adjacent ring zones in the process of Figures 4 and 5. Such leakage in the outer lands may also negatively impact the controlled retention of the desired outer edge curvature of the superstrate in the process of Figures 4-5. Similarly, leakage in the outer lands may impede the initiation and propagation of separation cracks in the process of Figures 7-9.

[0055] To combat such undesirable leakage, a superstraight chuck 1118 is provided incorporating a trench structure 1109, as shown in Figures 11a and 11b. Similar to the superstraight chuck 1118, the superstraight chuck 1118 also includes a plurality of lands 307 that may be defined into a series of inner lands 307a and peripheral lands 307b that protrude from a surface 1119 of the superstraight chuck 1118. As shown in Figures 11b and 12, the surface 1119 is a holding or retaining surface for holding or retaining the superstraight 108. A series of inner zones 303a are defined by the lands 307a. In at least one of the ring zones 303, a trench 1109 is formed recessed from the surface of the chuck 1118. The trenches may be concentric and may be located between corresponding lands of the ring zones. The trenches 1109a formed in the inner ring zones 303a are positioned at locations distal to the center of the chuck 1118 relative to the width of the associated inner ring zone. In contrast, the trenches 1109b formed in the peripheral ring zones 303b are positioned in regions proximate to the center of the substrate chuck 1118 relative to the width of the outer ring zone. That is, the trenches 1109a formed in the inner ring zones 303a are formed at the outer diameter of the corresponding inner ring zone 303a, while the trenches 1109b formed in the peripheral ring zones 303b are formed at the inner diameter of the peripheral zone 303b.

[0056] In operation, the trench 1109 acts as a buffer that provides a uniform source of high vacuum pressure that continues to act on the superstrates even if there are gaps between the superstrates at the lands distal to the trench. In this way, the sequential outward radial release of vacuum and the application of positive pressure to the central zone and adjacent ring zones can proceed in a controlled manner. That is, the applied vacuum pressure in a given ring zone can be maintained even if a positive pressure is applied to the adjacent inner zone by an amount that can deflect the superstrates enough to create gaps at the distal lands. In other words, the presence of the trench 1109 allows for some leakage without disrupting the intended process. Similarly, the trench 1109b located in the peripheral ring zone with the smaller outer land height operates to maintain adequate vacuum pressure in the outer ring zone even if there are small gaps in the outer lands. This allows the periphery of the superstrate to be maintained at a desired curvature, even with some leakage, for both the eventual spreading and merging of the deposited droplets of moldable material (see FIG. 4d) and for the initiation and propagation of separation cracks (see FIG. 6).

[0057] FIG. 12 is an enlarged cross-sectional view of an exemplary trench structure 1109b. The particular trench dimensions and relative location within the ring zone required to achieve the desired vacuum buffering performance depend on the land height and ring zone width of the superstrate chuck. In the example shown in FIG. 12, trench 1109b is located within ring zone 303b and is recessed from the chuck surface. In this example, outer land 307b has a height h1 that is lower than the height h2 of inner land 307a. In typical use, the land height difference can range from about 5 microns to about 50 microns. Ring zone 303b has a width d. Trench 1109b is positioned such that a first edge is a distance d1 from land 307b and a second edge is a distance d2 from land 307a. Trench 1109b has a depth h3 and a width d3. In this embodiment, the relationship of these parameters satisfies the following condition: h1 <h2 h3>10h2 d3<0.5d d1>d2+d3 The port 305 connecting the trench 1109b to a pressure source (not shown) intersects the trench or is otherwise located within the trench. If the port does not intersect the trench, the required high pressure cannot be maintained and the trench is ineffective. In the above embodiment, the outer land h1 is where leakage is expected to occur. For the inner ring trench 1109b, the land heights can be the same, i.e., h1=h2. In this case, the distance d1 is measured from the designated land (i.e., h1 or h2) where leakage is expected. For example, in the embodiment of Figures 11a and 11b, the inner ring zones 303a include trenches 1109a located closer to their respective ring zone outer lands (as measured radially from the chuck center) to mitigate against leakage at the inner lands during sequential vacuum release and subsequent pressurization of the ring zones as described in the process associated with Figures 4-5.

[0058] Further modifications and alternative embodiments of various aspects will be apparent to those skilled in the art in view of this description. Accordingly, this description should be interpreted as illustrative only. It should be understood that the forms shown and described herein should be interpreted as example embodiments. Elements and materials may be substituted for those illustrated and described herein, parts and processes may be reversed, and certain features may be utilized independently, all as would be apparent to those skilled in the art after having the benefit of this description.

Claims

1. A process for initiating separation of the superstrate and the hardening layer by applying an external force by mechanical contact to a portion of the outer periphery of the superstrate at a position outside the edge of the substrate, the superstrate and the hardening layer being separated from each other at a portion of the outer periphery of the surface where the superstrate and the hardening layer are in contact with each other; a step of expanding a separation region where the superstrate and the hardened layer are separated from the partial region along an outer periphery of a surface where the superstrate and the hardened layer contact each other; starting relative movement between the substrate and the superstrate in a direction away from the substrate while expanding the separation region along the outer periphery to complete separation of the superstrate and the hardened layer; The method includes:

2. holding the superstraight in a superstraight chuck; applying a negative fluid pressure to a peripheral zone of the superstrate chuck to deflect a peripheral region of the superstrate in the step of widening the separation region; The method of claim 1 , comprising:

3. The method of claim 2 , further comprising continuing to introduce a positive fluid pressure to the portion of the area where the superstrate and the stiffening layer are separated while applying the negative fluid pressure to the peripheral zone.

4. 10. The method of claim 1, further comprising applying a negative fluid pressure to a central zone of a superstrate chuck holding said superstrate to complete separation of said superstrate and said stiffening layer.

5. The method described in claim 1, wherein a pin moves from the substrate side to the superstrate side to apply an external force to the superstrate by mechanical contact.

6. laminating the substrate and the superstrate such that the superstrate includes an overhanging edge portion relative to the substrate; applying a force to the overhanging edge portion to generate the separation region in the portion of the area; The method of claim 1 further comprising:

7. aligning a position where the external force is applied to the superstrate with a notch in the substrate; applying the external force to the location of the superstrate through the notch; The method of claim 1 , comprising:

8. A superstraight chuck for holding the superstraight; a substrate chuck for holding the substrate; a force supply source configured to apply an external force to a portion of an outer periphery of the superstrate at a position outside an edge of the substrate by mechanical contact with the stack including the substrate and the superstrate and a hardening layer sandwiched therebetween, thereby initiating separation of the superstrate and the hardening layer at a portion of an outer periphery of a surface where the superstrate and the hardening layer contact each other; A planarization system comprising:

9. 9. The planarization system of claim 8, wherein the superstraight chuck includes a pattern of lands, one of the lands located near an edge of the superstraight chuck being recessed below another of the lands located on an interior portion of the superstraight chuck to allow the superstraight to flex toward the superstraight chuck.

10. 9. The planarization system of claim 8, wherein the substrate chuck includes a pattern of lands, one of the lands located at an edge of the substrate chuck being recessed below another of the lands located at an interior portion of the substrate chuck to allow the substrate to bend toward the substrate chuck.

11. The planarization system of claim 8 , wherein the force source comprises a mechanism that generates a mechanical pushing force in a direction from the substrate side to the superstrate side of the stack.

12. The planarization system of claim 8 , wherein the substrate includes a notch disposed on an edge thereof, and the force source applies the external force to the superstrate through the notch.

13. 10. The planarization system of claim 8, wherein the force source includes a pin that applies an external force to the superstrate through mechanical contact, the pin moving from the substrate side to the superstrate side to apply the external force to the superstrate through mechanical contact.

14. the superstrate chuck is configured to hold the superstrate relative to the substrate such that the superstrate includes an overhang; the force source is configured to apply a force to the overhanging portion of the superstrate to create a separation region in the portion of the region. The planarization system of claim 8 .

15. forming a stiffening layer between the substrate and the superstrate; completing separation of the superstrate and the stiffening layer using the method of any one of claims 1 to 7; manufacturing an article by processing the cured layer; A method for manufacturing an article comprising the steps of:

Citation Information

Patent Citations

  • Method and device for manufacture photoelectric conversion device

    JP2000164905A

  • Method for peeling stamper for optical disk and apparatus therefor

    JP2000348392A

  • Separating method of compound member, manufacturing method of thin film and separating device of compound member

    JP2001230393A

  • Imprint method and imprint apparatus implementing the same