Assembled paper container and film pasting machine

The assembly-type paper container with protrusions on the resin film and a specialized molding machine addresses the sealing issues by ensuring complete coverage of the gap between the container body and flange, effectively preventing leakage.

JP7558974B2Active Publication Date: 2024-10-01TOKAN KOGYO CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2021566812
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-12-25
Filing Date
2020-09-01
Publication Date
2024-10-01
Estimated Expiration
2040-09-01

AI Technical Summary

Technical Problem

Existing assembly-type paper containers face challenges in completely sealing the gap between the container body and the flange portion due to the thin resin film and top seal, leading to potential leakage or oozing of contents.

Method used

The assembly-type paper container design incorporates a resin film with protrusions above the gap, which is folded into multiple layers and covered by a top seal, and a film adhesion molding machine that forms these protrusions during the manufacturing process.

Benefits of technology

This design effectively seals the gap, preventing leakage or oozing of contents by ensuring the top seal covers the entire surface, including the gap, thereby enhancing the container's sealing capabilities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007558974000001
    Figure 0007558974000001
  • Figure 0007558974000002
    Figure 0007558974000002
  • Figure 0007558974000003
    Figure 0007558974000003
Patent Text Reader

Abstract

[Problem] To provide a flat-pack paper container whereby leakage of contained matter or the seepage of contained matter from a container section of a container main body is suppressed. [Solution] A flat-pack paper container (1) that includes: a container main body (11) having a container section (12); and resin film (3). The container main body (11) has: a floor surface (121); a plurality of side surfaces (122); and a flange section (13) that is connected to the plurality of side surfaces (122) and, after assembly, is flush with a top surface (131). The top surface (131) has gaps (22) extending from the container section (12) towards the outside of the container main body (11). The resin film (3) covers the top surface (131) and has protruding sections (31) above the gaps (22) that traverse the gaps (22).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] An embodiment of the present invention relates to a prefabricated paper container and a film attachment and forming machine. [Background technology]

[0002] There is known a prefabricated paper container in which a tray-shaped container body having a flange at the upper end is assembled from blank sheets made of paper whose main material is paper. Some prefabricated paper containers have a thermoplastic resin film having resin properties attached to the inner surface of the container body and the upper surface of the flange (Patent Document 1 and Patent Document 2). Prefabricated paper containers with a resin film are mainly used as trays or bowls for storing food, etc., because they have resin properties.

[0003] Furthermore, compared to plastic containers, the prefabricated paper container is an environmentally friendly product, for example, because it can suppress the generation of secondary microplastics in the environment. Furthermore, the resin film can be peeled off from the container body, and the resin film and the container body, i.e., the paper, can be separated, and the resin film and the container body can be recycled separately. Due to these advantages, it is expected that the prefabricated paper container can be used as a packaging container for food and the like and a storage container for food and the like by applying, for example, Modified Atmosphere Packaging (MAP). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 6-293334 [Patent Document 2] JP 2019-172339 A Summary of the Invention [Problem to be solved by the invention]

[0005] In the container body of a prefabricated paper container, a gap is formed on the upper surface of the flange portion due to the close proximity of the end faces of the blank sheets. Currently, it is difficult to completely fill this gap even if the inner surface of the container body and the upper surface of the flange portion are covered with a resin film. The resin film is thin. When a resin film is attached to a prefabricated paper container, for example, by vacuum pressure, the resin film is sucked into the gap. It is difficult to fill the gap with the resin film alone.

[0006] Packaging methods have been developed that replace the air in the storage section of the container body with a food gas suitable for packaging food (e.g., MAP). When this packaging method is applied to a prefabricated paper container with a resin film, a top seal is attached to the resin film on the upper surface of the flange section. However, the top seal is also thin. For this reason, even if the top seal is attached to the resin film, a cavity is created along the gap between the upper surface of the resin film and the lower surface of the top seal. It is difficult to completely seal the cavity even with the top seal. Moreover, both ends of the cavity are open. The storage section of the container body is connected to the outside of the container body through the cavity.

[0007] For the reasons described above, even if the storage section of an assembled paper container with a resin film is covered with a top seal, there is a possibility that the contents may leak or seep out of the storage section through the cavity.

[0008] An embodiment of the present invention provides an assembly-type paper container that can prevent the contents from leaking or seeping out of the storage portion of the container body, and a film bonding and molding machine that can manufacture this assembly-type paper container. [Means for solving the problem]

[0009] A first aspect of the present invention provides an assembly-type paper container that is assembled from blank sheets whose main material is paper, and that includes a container body having a storage section, and a resin film covering the inner surface of the storage section, wherein the container body has a bottom surface, a plurality of side surfaces rising from the bottom surface, a flange portion that is connected to the plurality of side surfaces and has a flush upper surface after assembly, and a top seal that is attached to the resin film on the upper surface of the flange portion and covers the storage section, and a gap is formed on the upper surface of the flange portion, the gap being generated when the end surfaces of the blank sheets are close to each other, the resin film covers the upper surface of the flange portion, and has a protrusion above the gap that crosses the gap and is configured so that the resin film is convex, and the top seal is attached to the protrusion above the upper surface of the flange portion. Contact While crossing the gap, the adhesive is attached to the resin film. Ta It is characterized by:

[0012] The first aspect of this invention 2 In the first aspect, the assembled paper container according to the present invention is Manufacturing The film is characterized in that it is folded into three or more layers at least within the gap.

[0013] The first aspect of this invention 3 The film attachment molding machine according to the present invention is a resin Manufacturing A film application forming machine that applies a film to a prefabricated paper container with a flange portion, the film application forming machine comprising a lower die on which the prefabricated paper container is placed, and a film application forming machine provided on the lower die for applying the resin film through the prefabricated paper container placed on the lower die. Manufacturing The film is sucked, and the resin Manufacturing A bonding section that bonds a film to the assembly-type paper container and a resin layer that faces the lower mold and is disposed between the lower mold and the bonding section. Manufacturing An upper mold in which the film is sandwiched, and a resin film is inserted into the upper mold. Manufacturing a flange pressing portion for pressing the film; and a resin film on the flange portion. ManufacturingThe projection forming area of ​​the film is sucked, and the projection that is convex with respect to the flange portion is pressed against the resin. Manufacturing and a molding section for molding the film.

[0014] The first aspect of this invention 4 The film attachment forming machine according to the present invention is 3 In one aspect, the suction direction of the molding portion is opposite to the suction direction of the adhesive portion.

[0015] The first aspect of this invention 5 The film attachment forming machine according to the present invention is 3 Mode or number 4 In the aspect The adhering section adheres the resin film on which the protrusions are formed by the molding section to the assembly-type paper container. It is characterized by: Effect of the Invention

[0016] First to third aspects 2 The assembled paper container according to the embodiment has a flange portion having an upper surface covered. Made of resin The film has a protrusion above the gap that crosses the gap. This allows the top seal to be attached above the gap. Made of resin The film can be attached so as to close the cavity that is open at both ends. 2 According to the assembly-type paper container relating to this aspect, it is possible to provide a assembly-type paper container that can prevent the contained contents from leaking or seeping out from the containing portion of the container body.

[0017] No. 3 Mode ~ No. 5 The film attachment molding machine according to the embodiment is a resin film arranged on a flange portion. Manufacturing The film is sucked and the protruding parts that are convex with respect to the flange are filled with resin. Manufacturing The film is molded by a molding section. 3 Mode ~ No. 5 According to the film attachment forming machine according to the embodiment, the first to third embodiments 2 A film bonding and forming machine capable of manufacturing the assembled paper container according to the embodiment can be provided. [Brief description of the drawings]

[0018] [Figure 1] Fig. 1(a) is a plan view showing an example of a prefabricated paper container according to one embodiment. Fig. 1(b) is a side view showing an example of a prefabricated paper container according to one embodiment. Fig. 1(c) is a perspective view showing an example of a prefabricated paper container according to one embodiment. [Diagram 2] FIG. 2 is a plan view showing an example of a blank sheet. [Diagram 3] 3(a) to 3(d) are schematic cross-sectional views showing examples of the protrusions. [Figure 4] FIG. 4 is a plan view showing an example in which a storage section is covered with a top seal. [Diagram 5] 5(a) to 5(d) are schematic cross-sectional views showing how the top seal is attached to the resin film. [Figure 6] 6(a) to 6(d) are schematic cross-sectional views showing how the top seal is attached to the resin film. [Figure 7] 7(a) and 7(b) are schematic cross-sectional views showing an example of a film application forming machine. [Figure 8] 8(a) and 8(b) are schematic cross-sectional views showing how the protrusions are formed. [Figure 9] FIG. 9 is a schematic block diagram showing an example of a film adhering system. [Figure 10] 10(a) and 10(b) are schematic cross-sectional views showing an example of a protrusion according to a first modified example. [Figure 11] 11(a) and 11(b) are schematic cross-sectional views showing an example of a protrusion according to a second modified example. [Figure 12] 12(a) and 12(b) are schematic cross-sectional views showing an example of a protrusion according to a third modified example. [Figure 13] 13(a) and 13(b) are schematic cross-sectional views showing an example of a protrusion according to a fourth modified example. [Figure 14] 14(a) and 14(b) are schematic cross-sectional views showing an example of a protrusion according to a fifth modified example. [Figure 15] 15(a) and 15(b) are schematic cross-sectional views showing an example of a protrusion according to a sixth modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the respective drawings, common parts are given common reference numerals and duplicated explanations will be omitted.

[0020] (Assembled paper container) Fig. 1(a) is a plan view showing an example of a prefabricated paper container according to one embodiment. Fig. 1(b) is a side view showing an example of a prefabricated paper container according to one embodiment. Fig. 1(c) is a perspective view showing an example of a prefabricated paper container according to one embodiment. Fig. 2 is a plan view showing an example of a blank sheet.

[0021] The prefabricated paper container 1 shown in Figures 1(a) to 1(c) is assembled from a blank sheet 2 shown in Figure 2. The blank sheet 2 is mainly made of paper. In Figure 2, dotted lines indicate "valley folds" and dashed lines indicate "mountain folds". The valley folds and mountain folds are, for example, perforations, half cuts, or rules. Furthermore, thick solid lines indicate "slits". The prefabricated paper container 1 is obtained by performing "valley folds" and "mountain folds" on the blank sheet 2.

[0022] The collapsible paper container 1 includes a container body 11 and Made of resin The container body 11 includes a storage section 12 and a flange section 13. The container body 11 has a bottom surface 121 and a plurality of side surfaces 122 rising from the bottom surface 121. The storage section 12 is composed of the bottom surface 121 and the plurality of side surfaces 122. In this embodiment, there are eight side surfaces 122. Three or more side surfaces 122 can constitute the storage section 12. Three or more side surfaces 122 may be sufficient.

[0023] The flange portion 13 is connected outwardly from the storage portion 12 to the upper ends of the respective side surfaces 122. The flange portion 13 has an upper surface 131. The upper surface 131 of the flange portion 13 becomes flush after assembly. The upper surface 131 of the flange portion 13 has a gap 22. The gap 22 is generated on the upper surface 131 as a result of the end surfaces 21 of the blank sheets 2 coming close to each other after assembly. The gap 22 extends from the storage portion 12 toward the outside of the container body 11. In this embodiment, an example is shown in which the gap 22 is generated at the four corners of the flange portion 13.

[0024] resin Manufacturing The film 3 covers the inner surface of the housing portion 12, the inner surface of the side surface 122, and the upper surface 131 of the flange portion 13. Manufacturing The film 3 is selected to have, for example, watertightness and gas diffusion properties. Manufacturing An example of the film 3 is a film made of a thermoplastic resin. Manufacturing The film 3 has a protrusion 31 above the gap 22. The protrusion 31 crosses the gap 22. In this embodiment, there are four gaps 22. There are also four protrusions 31. The four protrusions 31 are provided above each of the four gaps 22. A plurality of protrusions 31 may be provided for each gap 22. The shape of the protrusions 31 may be any shape, such as a semicircular shape, a rectangular shape, a triangular shape, etc., when viewed from a cross section along IIIB-IIIB in FIG. 1(a).

[0025] Figures 3(a) to 3(d) are schematic cross-sectional views showing an example of a protrusion. The cross section shown in Figure 3(a) is taken along line IIIA-IIIA in Figure 1(a). The cross section shown in Figure 3(b) is taken along line IIIB-IIIB in Figure 1(a). The cross section shown in Figure 3(c) is taken along line IIIC-IIIC in Figure 1(a). The cross section shown in Figure 3(d) is taken along line IIID-IIID in Figure 1(a).

[0026] As shown in FIG. 3(a) to FIG. 3(d), Manufacturing The film 3 falls into the gap 22. However, the protrusion 31 protrudes upward from the flange portion 13 above the gap 22.

[0027] The protrusion 31 can be molded from a resin. Manufacturing Examples of the film 3 include polyolefins such as polyethylene (PE) and polypropylene (PP), polyesters such as polyvinyl chloride and polyethylene terephthalate (PET), ethylene-vinyl acetate copolymers (EVA), ethylene-acrylic acid copolymers, polyamides, polyvinylidene chloride, polystyrene, polycarbonate, polybutene, and polyvinyl alcohol. Manufacturing The film 3 may be a single film made of any of the above materials, or may be a film made of a mixture of two or more of the above materials. Manufacturing The film 3 may be a single-layer film or a laminated film having a plurality of layers laminated together.

[0028] FIG. 4 is a plan view showing an example in which the storage section is covered with a top seal.

[0029] As shown in Fig. 4, the collapsible paper container 1 can package and store food and the like by covering the storage section 12 with the top seal 4. The top seal 4 is a resin seal on the upper surface 131 of the flange section 13. Manufacturing The top seal 4 is attached to the film 3. As a result, the top seal 4 covers the storage portion 12. In this embodiment, the top seal 4 crosses the gap 22 above the upper surface 131 of the flange portion 13, crushing the protrusion 31 while applying the resin Manufacturing The top seal 4 is attached to the film 3. Manufacturing When attaching the top seal 4 to the film 3, the top seal 4 is pressed by a pressing machine (e.g., a seal head) of a pressing machine. The pressing machine presses the top seal 4 in an area shown as pressing area 32. In this embodiment, the protrusion 31 is designed so that the entire protrusion 31 fits within the width of the pressing area 32. This allows the protrusion 31 to be reliably crushed by the pressing machine.

[0030] <Top seal attachment: Example> 5(a) to 5(d) show, as a reference example of the present invention, an example in which the protrusions 31 are not formed.

[0031] Figures 5(a) to 5(d) show the top seal made of resin. Manufacturing 5(a) to 5(d) are schematic cross-sectional views showing a state in which the adhesive is attached to a film.The cross sections shown in each of Fig. 5(a) to Fig. 5(d) correspond to the cross section shown in Fig. 3(b).

[0032] As shown in FIG. 5(a), the resin Manufacturing The film 3 is placed on the upper surface 131 of the flange portion 13 .

[0033] Next, as shown in FIG. 5(b), the resin is Manufacturing The film 3 is sucked through the container body 11. The container body 11 is mainly made of paper. Manufacturing The film 3 is adhered to the flange portion 13. At this time, the resin Manufacturing The film 3 is sucked into the gap 22 and falls into the gap 22 .

[0034] Next, as shown in FIG. 5(c), Manufacturing A heated top seal 4 is placed on the film 3 .

[0035] Next, as shown in FIG. 5(d), the heated top seal 4 is pressed by a pressing machine to form a resin Manufacturing The resin is then heat-pressed onto the upper surface 33 of the film 3. Manufacturing Since the film 3 is pressed into the gap 22, the lower surface 41 of the top seal 4 is made of resin. Manufacturing The resin does not reach the upper surface 33 of the film 3. Manufacturing A cavity 5 is formed between the upper surface 33 of the film 3 and the lower surface 41 of the top seal 4. Since both ends of the cavity 5 are open, the storage section 12 communicates with the outside of the container body 11 through the cavity 5.

[0036] Once the cavity 5 is formed, even if the storage section 12 is covered with the top seal 4, leakage or seepage of the contents from the storage section 12 occurs through the cavity 5.

[0037] <Attaching the top seal> Figures 6(a) to 6(d) show the top seal made of resin. Manufacturing 6(a) to 6(d) are schematic cross-sectional views showing how the adhesive is attached to a film.The cross sections shown in Fig. 6(a) to 6(d) correspond to the cross section shown in Fig. 3(b).

[0038] As shown in Figure 6(a), Made of resin The film 3 is placed on the upper surface 131 of the flange portion 13 .

[0039] Next, as shown in FIG. 6(b), the resin is Manufacturing The film 3 is sucked through the prefabricated paper container 1. Manufacturing The film 3 is adhered to the upper surface 131 of the flange portion 13. In this embodiment, the resin Manufacturing The film 3 is sucked into the gap 22 and falls into the gap 22. However, the protrusion 31 is pushed upward from the gap 22 into the resin on the upper surface 131 of the flange portion 13. Manufacturing It remains protruding beyond the upper surface 33 of the film 3. An example of the formation of the protrusions 31 will be described later.

[0040] Next, as shown in FIG. 6(c), Manufacturing A heated top seal 4 is placed on the film 3 .

[0041] Next, as shown in FIG. 6(d), the heated top seal 4 is pressed by a pressing machine. The top seal 4 is made of resin. Manufacturing The resin is thermally bonded to the upper surface 33 of the film 3. Manufacturing The upper surface of the film 3 contacts the lower surface 41 of the top seal 4 .

[0042] Furthermore, in the process of thermocompression bonding, the protrusion 31 is crushed by the top seal 4 being pressed by a pressing machine. Since the protrusion 31 crosses the gap 22, the protrusion 31 is crushed across the gap 22. A part of the protrusion 31 is crushed by the resin Manufacturing6(b), the protrusion 31 has one first corner 31a above the gap 22 that crosses the gap 22. The cross section of the protrusion 31 along the gap 22 is triangular. The slope 312 of the triangle is formed by the resin as the protrusion 31 is crushed. Manufacturing This becomes the upper surface 33 of the film 3. Manufacturing The upper surface of the film 3 crosses the gap 22 and comes into contact with the lower surface 41 of the top seal 4 .

[0043] According to this embodiment, the top seal 4 is also formed of resin above the gap 22. Manufacturing That is, the top seal 4 can be thermally pressed onto the upper surface 33 of the film 3 above the gap 22. Manufacturing The film 3 can be attached to the upper surface thereof so as to block the cavity 5 .

[0044] In addition, the protrusion 31 is crushed, so that the resin Manufacturing The side walls 34 of the protrusions 31 of the film 3 are folded and overlapped in multiple layers at least in the gaps 22. For example, in the example shown in FIG. Manufacturing The film 3 is folded into three layers. Manufacturing The film 3 may be folded into three or more layers, for example in an accordion shape. Manufacturing The film 3 is folded into multiple layers at least in the gap 22, so that the top seal 4 is also formed above the gap 22 by the resin. Manufacturing It is easy to heat-press the resin onto the upper surface 33 of the film 3. Manufacturing This is because the film 3 exerts a reaction force on the top seal 4 during pressing.

[0045] 6(b), the protrusion 31 has a first corner 31a. When the protrusion 31 has the first corner 31a, there is an advantage that the protrusion 31 is more easily crushed than when the protrusion 31 does not have the corner 31a. The first corner 31a does not have to have an angular shape, and may have a gentle shape, for example, a rounded shape.

[0046] In this way, resin Manufacturing According to one embodiment in which the cavity 5 can be blocked by the film 3 and the top seal 4, an assembly-type paper container 1 can be provided that can prevent the contents from leaking or seeping out of the storage section 12 of the container body 11.

[0047] (Film pasting machine) 7(a) and 7(b) are schematic cross-sectional views showing an example of a film application forming machine.

[0048] The film attachment molding machine 600 is a new molding machine capable of manufacturing the prefabricated paper container 1 according to one embodiment. Manufacturing The film 3 is attached to the assembled paper container 1 with the flange portion 13. Furthermore, the film attachment molding machine 600 attaches the protrusion portion 31 to the film 3 by using a resin. Manufacturing Form into film 3.

[0049] As shown in FIGS. 7( a ) and 7 ( b ), the film application forming machine 600 includes a lower mold 610 , an application section 611 , an upper mold 620 , a flange pressing section 630 , and a forming section 631 .

[0050] The prefabricated paper container 1 is placed on the lower mold 610.

[0051] The adhesive part 611 is provided on the lower mold 610. The adhesive part 611 is connected to a vacuum pump 640. The adhesive part 611 applies a resin to the prefabricated paper container 1 placed on the lower mold 610 via the prefabricated paper container 1. Manufacturing Film 3 is aspirated.

[0052] The upper mold 620 faces the lower mold 610. The upper mold 620 is, for example, movable up and down. Manufacturing The film 3 is sandwiched between the lower mold 610 and the upper mold 620. The upper mold 620 presses the resin Manufacturing When the film 3 is sandwiched between the two, a nearly sealed processing space is formed. ManufacturingThe film 3 is attached to the housing portion 12 and the flange portion 13 by, for example, vacuum pressure.

[0053] The flange pressing portion 630 is housed in the upper mold 620. The flange pressing portion 630 is supported on a top plate portion 621 of the upper mold 620 by an expandable and contractible elastic member 632. An example of the elastic member 632 is a spring. The flange pressing portion 630 presses the flange portion 13 and the resin on the flange portion 13, for example, under vacuum and compressed air. Manufacturing Hold film 3.

[0054] The molding section 631 is provided on the flange pressing section 630. The molding section 631 is connected to a vacuum pump 640. The molding section 631 is configured to mold the resin on the flange section 13. Manufacturing The projection-forming region of the film 3 is suctioned. The projection-forming region is set so as to cross the gap 22. The projections 31 are formed by, for example, using a resin. Manufacturing This is performed while the film 3 is attached to the housing portion 12 and the flange portion 13. The suction direction of the molding portion 631 is opposite to the suction direction of the attachment portion 611. In this embodiment, the attachment portion 611 is made of resin Manufacturing The film 3 is sucked in the direction toward the assembled paper container 1. The forming section 631 is a resin Manufacturing The film 3 is sucked in a direction away from the prefabricated paper container 1.

[0055] 8(a) and 8(b) are schematic cross-sectional views showing how the protrusions 31 are formed.

[0056] As shown in FIG. 8(a) and FIG. 8(b), when the protrusion 31 is formed by suction, the resin Manufacturing The thickness T of the film 3 changes. For example, after suction, the resin of the protrusion 31 Manufacturing The thickness T of the film 3 is reduced. Manufacturing When the thickness T of the film 3 is thin, the protrusions 31 are easier to fold or crush than when the thickness T is thick. Manufacturing This is one of the advantages of forming the film 3 by suction.

[0057] (Example of film attachment machine operation) As shown in FIG. 7(a) and FIG. 7(b), the heated resin is poured into the upper mold 620 in a state where the upper mold 620 is separated from the lower mold 610. Manufacturing The film 3 is guided between the upper mold 620 and the lower mold 610 .

[0058] Next, the prefabricated paper container 1 is placed on the lower mold 610.

[0059] Next, the upper die 620 is lowered, and the resin is Manufacturing The film 3 is pressed. Furthermore, the flange portion 13 and the resin on the flange portion 13 are pressed by the flange pressing portion 630. Manufacturing Hold film 3.

[0060] Next, the adhesive portion 611 and the molding portion 631 are Manufacturing The film 3 is sucked. Manufacturing The film 3 is attached to each of the bottom surface 121 of the housing portion 12, the side surface 122 of the housing portion 12, and the upper surface 131 of the flange portion 13. In addition, a protrusion 31 that is convex with respect to the flange portion 13 is formed above the gap 22 on the flange portion 13.

[0061] The timing of suction by the molding part 631 may be earlier than the timing of suction by the adhering part 611. Manufacturing The protrusions 31 can be formed before the film 3 is attached to the upper surface 131 of the flange portion 13. This provides the advantage that the protrusions 31 can be easily formed.

[0062] Next, the upper mold 620 is raised. Then, the collapsible paper container 1 is Manufacturing The whole film 3 is removed from the film attachment forming machine.

[0063] In this manner, the film application and forming machine 600 makes it possible to manufacture the assembly type paper container 1.

[0064] (Film Adhesive System) FIG. 9 is a schematic block diagram showing an example of a film adhering system.

[0065] The film application system 700 includes a resin film wound around a feed roller 710. Manufacturing While the film 3 is being wound by the winding roller 720, the resin is applied to the prefabricated paper container 1 having the flange portion 13. Manufacturing Apply film 3.

[0066] As shown in FIG. 9, the film application system 700 includes a feed roller 710, a take-up roller 720, a heater 730, the film application forming machine 600, and a trimming machine 740.

[0067] The feed roller 710 is provided with a roll of resin strip. Manufacturing Film 3 is attached.

[0068] The winding roller 720 is provided with a strip of resin Manufacturing One end of the film 3 is attached to the winding roller 720. Manufacturing The film 3 is wound up. Manufacturing The film 3 advances in a feed direction W from a feed roller 710 towards a take-up roller 720 .

[0069] The heater 730 is disposed between the feed roller 710 and the take-up roller 720. The heater 730 heats a strip of resin. Manufacturing The film 3 is heated.

[0070] The film attachment forming machine 600 is disposed between the heater 730 and the take-up roller 720. The film attachment forming machine 600 is, for example, the film attachment forming machine described above.

[0071] The trimming machine 740 is disposed between the film attachment molding machine 600 and the winding roller 720. The trimming machine 740 trims a strip-shaped resin Manufacturing The assembled paper container 1 attached to the film 3 is then ManufacturingThe film 3 is trimmed. As a result, the collapsible paper container 1 is made of a strip of resin. Manufacturing Departed from film 3.

[0072] In this way, the film application system 700 includes the film application forming machine 600. Therefore, the film application system 700 can manufacture the prefabricated paper container 1. Moreover, the film application system 700 can manufacture the prefabricated paper container 1 by attaching a strip of resin Manufacturing The film 3 can be produced continuously.

[0073] (Modifications of the protrusion 31) Next, some modified examples of the protrusion 31 will be described.

[0074] <First Modification> 10(a) and 10(b) are schematic cross-sectional views showing an example of a protrusion according to Modification Example 1. The schematic cross-section shown in Fig. 10(a) shows the state before the top seal is attached, and the schematic cross-section shown in Fig. 10(b) shows the state after the top seal is attached.

[0075] As shown in Fig. 10(a) and Fig. 10(b), the protrusion 31 may have two corners, a first corner 31a and a second corner 31b, above the gap 22. The cross section of the protrusion 31 along the gap 22 is rectangular. In the first modified example, the rectangular upper surface 313 is formed by pressing the resin during the process of the protrusion 31 being crushed. Manufacturing This becomes the upper surface 33 of the film 3 .

[0076] In the first modified example, the resin Manufacturing The upper surface of the film 3 can cross the gap 22 and come into contact with the lower surface 41 of the top seal 4. Manufacturing The film 3 and the top seal 4 make it possible to close the cavity 5 .

[0077] Therefore, according to the first modified example, it is possible to provide a prefabricable paper container 1 that is capable of preventing the contained contents from leaking or seeping out from the containing section 12 of the container body 11.

[0078] <Second Modification> 11(a) and 11(b) are schematic cross-sectional views showing an example of a protrusion according to Modification 2. The schematic cross-section shown in Fig. 11(a) shows the state before the top seal is attached, and the schematic cross-section shown in Fig. 11(b) shows the state after the top seal is attached.

[0079] 11(a) and 11(b), the cross section of the protrusion 31 in the direction along the gap 22 may be trapezoidal. In the second modification, the trapezoidal upper surface 314 is formed by the resin during the process in which the protrusion 31 is crushed. Manufacturing This becomes the upper surface 33 of the film 3 .

[0080] In the second modified example as well, it is possible to provide a prefabricable paper container 1 that is capable of preventing the contained contents from leaking or seeping out from the containing section 12 of the container body 11.

[0081] <Third Modification> 12(a) and 12(b) are schematic cross-sectional views showing an example of a protrusion according to Modification Example 3. The schematic cross-section shown in Fig. 12(a) shows the state before the top seal is attached, and the schematic cross-section shown in Fig. 12(b) shows the state after the top seal is attached.

[0082] As shown in Figures 12(a) and 12(b), the cross section of the protrusion 31 in the direction along the gap 22 may have a shape of two triangles combined together. In the third modified example, the slope 315 of the first triangle and the slope 316 of the second triangle face each other, forming a so-called M shape. In the third modified example, the protrusion 31 has a first corner 31a, a second corner 31b, and a third corner 31c above the gap 22. In the third modified example, both the slope 315 of the first triangle and the slope 316 of the second triangle are pressed against each other by the resin during the process of the protrusion 31 being crushed. Manufacturing This becomes the upper surface 33 of the film 3 .

[0083] In the third modified example as well, it is possible to provide a prefabricated paper container 1 that is capable of preventing the contained contents from leaking or seeping out from the containing section 12 of the container body 11.

[0084] In the third modification, both the slope 315 of the first triangle and the slope 316 of the second triangle are made of resin. Manufacturing This forms the upper surface 33 of the film 3. Therefore, above the gap 22, the top seal 4 and the resin Manufacturing This makes it easy to increase the contact area with the upper surface 33 of the film 3. As a result, according to the third modified example, there is an additional advantage that the effect of blocking the cavity 5 can be easily improved.

[0085] <Fourth Modification> 13(a) and 13(b) are schematic cross-sectional views showing an example of a protrusion 31 according to a fourth modified example. The schematic cross-section shown in Fig. 13(a) shows the state before the top seal 4 is attached, and the schematic cross-section shown in Fig. 13(b) shows the state after the top seal 4 is attached.

[0086] As shown in Figures 13(a) and 13(b), when the cross section of the protrusion 31 in the direction along the gap 22 is M-shaped, the first triangular portion and the second triangular portion may be formed halfway up the protrusion 31.

[0087] In the fourth modified example as well, it is possible to provide a prefabricable paper container 1 that is capable of preventing the contained contents from leaking or seeping out from the containing section 12 of the container body 11.

[0088] <Fifth Modification> 14(a) and 14(b) are schematic cross-sectional views showing an example of a protrusion according to a fifth modified example.

[0089] As shown in Figures 14(a) and 14(b), for example, in the first modified example, the first corner 31a and the second corner 31b may have not only a sharp shape but also a gentle shape, for example, a rounded shape as shown in the figure. This also applies to the first corner 31a in the above embodiment (see, for example, Figure 6(b)), the first corner 31a and the second corner 31b in the second modified example (see, for example, Figure 11(a)), the first corner 31a to the third corner 31c in the third modified example (see, for example, Figure 12(a)), and the first corner 31a to the third corner 31c in the fourth modified example (see, for example, Figure 13(a)).

[0090] <Sixth Modification> 15(a) and 15(b) are schematic cross-sectional views showing an example of a protrusion according to a sixth modified example.

[0091] As shown in Figures 15(a) and 15(b), the tip surface 317 of the protrusion 31 may be rounded as a whole. For example, even if the tip surface 317 is rounded as a whole, the protrusion 31 can be crushed into, for example, a bellows shape. Therefore, in the sixth modified example, the resin Manufacturing The upper surface 33 of the film 3 can be pressed against the top seal 4 .

[0092] Although one embodiment of the present invention has been described above, the above embodiment is presented as an example and is not intended to limit the scope of the invention. In addition, the above embodiment is not the only embodiment of the present invention. The embodiment of the present invention can be implemented in various new forms other than the above embodiment. Therefore, the above embodiment can be variously omitted, replaced, and modified without departing from the gist of the present invention. Such new forms and modifications are included in the scope and gist of the present invention, and are included in the scope of the invention described in the claims and the equivalents of the invention described in the claims. [Explanation of symbols]

[0093] 1: Assembled paper container 11: Container body 12: Storage section 121: Bottom 122: Side 13: Flange part 131:Top surface 2: Blank sheet 21: End face 22: Gap 3: Resin Manufacturing film 31:Protrusion 31a: 1st corner 31b:Second corner 31c: 3rd corner 312: Triangular slope 313: Top surface of a rectangle 314: Top of trapezoid 315: Slope of the first triangle 316: Slope of the second triangle 317: Tip surface of protrusion 32: Pressed area 33:Top surface 34: Side wall 4: Top seal 41: Bottom surface 5: Cavity 600: Film pasting machine 610: Lower mold 611: Adhesive part 620: Upper mold 621: Top plate 630: Flange holding part 631: Molding section 632: Elastic member 640: Vacuum pump 700: Film application system 710: Feeding roller 720: Winding roller 730: Heating machine 740: Trimming machine T: Thickness W: Feed direction

Claims

1. A prefabricated paper container comprising a container body having a container section and a resin film covering the inner surface of the container section, the prefabricated paper container being assembled from blank sheets mainly made of paper, The container body includes: The bottom surface and A plurality of side surfaces rising from the bottom surface; a flange portion that is connected to the plurality of side surfaces and has a flush upper surface after assembly; a top seal attached to the resin film on the upper surface of the flange portion to cover the storage portion; a gap is formed on an upper surface of the flange portion, the gap being generated when end surfaces of the blank sheets are brought into close proximity with each other, the gap extending from the storage portion toward the outside of the container body; the resin film covers an upper surface of the flange portion, and has a protrusion above the gap that crosses the gap and is configured so that the resin film is convex; The top seal is attached to the resin film above the upper surface of the flange portion, across the gap while contacting the protrusion. A prefabricated paper container characterized by the above.

2. The resin film is folded in three or more layers at least in the gap. The collapsible paper container according to claim 1,

3. A film application and forming machine that applies a resin film to a flanged assembled paper container, comprising: The film attachment forming machine includes: A lower mold on which the prefabricated paper container is placed; an attachment section provided in the lower mold section, which sucks the resin film through the prefabricated paper container placed on the lower mold section and attaches the resin film to the prefabricated paper container; an upper mold that faces the lower mold and has the resin film sandwiched between the lower mold and an upper mold; a flange pressing portion that is accommodated in the upper mold and presses the flange portion and the resin film on the flange portion; a forming section provided on the flange pressing section and configured to suck a protrusion forming region of the resin film on the flange section and form a protrusion on the resin film that is convex relative to the flange section; Equipped with This film bonding and forming machine is characterized by the above.

4. The suction direction of the molding part is opposite to the suction direction of the adhesive part.

4. The film application and forming machine according to claim 3,

5. The adhering unit adheres the resin film, on which the protrusions are formed by the molding unit, to the assembly-type paper container.

5. The film application and forming machine according to claim 3 or 4,

Citation Information

Patent Citations

  • JP1975116823U

  • Air tight container blank and its forming method

    JP1992142246A

  • Package container and its blank

    JP1994293334A

  • Packaging container

    JP1996119260A

  • Paper tray and production method thereof

    JP1997254280A