Glass plate manufacturing method and transfer mold
The method of using a transfer mold with movable pins to form glass plates with curved shapes addresses the inefficiency of multiple prototypes by enabling reusable prototypes and fixed pin positions, enhancing manufacturing efficiency and reducing costs.
Patent Information
- Application Number
- JP2021061398
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-31
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2041-03-31
AI Technical Summary
Existing methods for manufacturing glass plates with curved shapes require multiple prototypes to adjust the position of pins in pin groups, leading to increased production costs and inefficiencies.
A method involving a transfer mold with independently movable pins that are fixed in position, allowing separation from a prototype while maintaining alignment, and a process to bend glass plates along these pins, reducing the need for multiple master molds.
This approach allows for the reuse of prototypes, decreases the number of required master molds, and improves manufacturing efficiency by fixing pin positions, thereby reducing production costs and time.
Smart Images

Figure 0007559653000004 
Figure 0007559653000005 
Figure 0007559653000006
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a glass plate and a transfer mold. [Background technology]
[0002] The bending apparatus described in Patent Document 1 includes a heater, a first pin group, a first guide plate, a first movable plate, and a first movement mechanism. The heater heats the forming plate. The first pin group includes three or more first pins that contact a first main surface of the forming plate. The first guide plate supports the three or more first pins in parallel with each other and supports the three or more first pins independently and freely moveable in their respective longitudinal directions. The first movable plate is disposed on the opposite side of the forming plate with respect to the first guide plate. A first forming die having a first curved surface that contacts the first pin group is attached to the first movable plate. The first movement mechanism moves the first movable plate relative to the first guide plate in the longitudinal direction of the first pins. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2020 / 080305 Summary of the Invention [Problem to be solved by the invention]
[0004] In Patent Document 1, the lower end of each first pin is pushed up by the upward curved surface of a first mold, and the position of each first pin is adjusted to a desired position. In this state, a glass sheet is placed on the group of first pins, and the glass sheet is bent along the upper ends of each first pin.
[0005] For example, when multiple glass sheets are placed on different pin groups to bend each glass sheet, a master mold for adjusting the position of each pin in each pin group must be prepared for each pin group, which results in a large number of master molds.
[0006] One aspect of the present disclosure provides a technique for reducing the number of masters used to adjust the positions of each pin that constitutes a pin group. [Means for solving the problem]
[0007] A method for manufacturing a glass plate according to an embodiment of the present disclosure is a method for manufacturing a glass plate having a curved surface shape, and includes the following steps (A) to (E). (A) A first transfer mold is prepared having a first pin group including three or more first pins that are independently movable in the longitudinal direction and parallel to each other. (B) A tip of each of the first pins is brought into contact with a curved surface of a first master mold, and the position of each of the first pins is adjusted and fixed. (C) While the position of each of the first pins is kept fixed, each of the first pins is separated from the first master mold. (D) The glass plate is placed on the first transfer mold with the tip of each of the fixed first pins facing upward. (E) The glass plate is heated, and the glass plate is bent along the tip of each of the fixed first pins.
[0008] A transfer mold according to one embodiment of the present disclosure is a transfer mold used for manufacturing a glass plate having a curved surface shape. The transfer mold includes a pin group including three or more pins that are independently movable in the longitudinal direction and parallel to each other, and a position of each of the pins. of and a fixing device for fixing the same. Effect of the Invention
[0009] According to one aspect of the present disclosure, the position of each pin constituting a pin group is fixed. The pins can be separated from the master while keeping the position of each pin fixed, and the master can be reused. Therefore, the number of masters can be reduced. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a flowchart showing a method for manufacturing a glass plate according to one embodiment. [Diagram 2] FIG. 2 is a perspective view showing an example of the first transfer mold. [Diagram 3] FIG. 3 is a top view of the first transfer mold of FIG. [Figure 4] FIG. 4 is a cross-sectional view taken along line IV-IV in FIG. [Diagram 5] FIG. 5 is a cross-sectional view showing an example of step S102 in FIG. [Figure 6] FIG. 6 is a cross-sectional view showing an example of step S104 in FIG. [Figure 7] FIG. 7 is a cross-sectional view showing an example of step S105 in FIG. [Figure 8] FIG. 8 is a cross-sectional view showing an example of the second transfer mold. [Figure 9] FIG. 9 is a cross-sectional view showing a modification of step S103 in FIG. [Figure 10] FIG. 10 is a cross-sectional view showing a modification of step S104 in FIG. [Figure 11] FIG. 11 is a cross-sectional view showing a modification of step S105 in FIG. [Figure 12] FIG. 12 is a cross-sectional view showing a modified example of the fixing device. [Figure 13] FIG. 13(A) is a transmission image of the glass plate obtained in Example 1, FIG. 13(B) is a transmission image of the glass plate obtained in Example 2, FIG. 13(C) is a transmission image of the glass plate obtained in Example 3, FIG. 13(D) is a transmission image of the glass plate obtained in Example 4, FIG. 13(E) is a transmission image of the glass plate obtained in Example 5, and FIG. 13(F) is a transmission image of the glass plate obtained in Example 6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, an embodiment of the present disclosure will be described with reference to the drawings. In each drawing, the same or corresponding configurations are denoted by the same reference numerals, and description thereof may be omitted. In each drawing, the X-axis direction, the Y-axis direction, and the Z-axis direction are perpendicular to each other, the X-axis direction and the Y-axis direction are horizontal directions, and the Z-axis direction is a vertical direction. The positive Z-axis direction is a vertically upward direction, and the negative Z-axis direction is a vertically downward direction.
[0012] A method for manufacturing a glass plate according to one embodiment will be described with reference to Fig. 1. As shown in Fig. 1, the method for manufacturing a glass plate includes steps S101 to S104. Step S101 includes preparing a first transfer mold 1. The first transfer mold 1 includes, for example, a first pin group 2 and a first fixing tool 3, as shown in Figs. 2 to 4.
[0013] The first pin group 2 includes three or more first pins 21 that are independently movable in the longitudinal direction and parallel to one another. The first fixing device 3 movably fixes the position of each of the first pins 21. The position of each of the first pins 21 can be adjusted, making it possible to form glass sheets 9 (see FIG. 6) with various curved shapes. It is also possible to measure the deviation between the curved shape of the glass sheet 9 and a target curved shape, and finely adjust the position of each of the first pins 21 so as to reduce the deviation.
[0014] The thickness of the glass plate 9 is preferably 0.2 mm or more, more preferably 0.8 mm or more, and even more preferably 1 mm or more. The thickness of the glass plate 9 is preferably 5 mm or less, more preferably 3 mm or less, and even more preferably 2 mm or less. The radius of curvature of the glass plate 9 is preferably 50 mm or more, more preferably 100 mm or more, and even more preferably 200 mm or more. The radius of curvature of the glass plate 9 is, for example, 10,000 mm or less.
[0015] Each of the first pins 21 is arranged parallel to the Z-axis direction, for example. The longitudinal direction of each of the first pins 21 is, for example, the Z-axis direction. When viewed from the longitudinal direction of each of the first pins 21, the multiple first pins 21 are arranged in a staggered manner as shown in Fig. 3, but may also be arranged in a matrix.
[0016] When viewed in the longitudinal direction of each first pin 21, the tip of each first pin 21 (for example, first head 26) is circular, but may be polygonal (for example, triangular, rectangular, or hexagonal). In the latter case, the tips of adjacent first pins 21 can be stably pressed against each other. On the other hand, in the former case, a gap can be formed between adjacent first pins 21, the heat capacity of the first pin group 2 can be reduced, and the temperature of the first pin group 2 can be raised in a short time.
[0017] As shown in Fig. 4, the tip of each first pin 21 includes an upwardly convex dome-shaped curved surface 22, which supports the glass sheet 9 from below. Compared to a case in which the glass sheet 9 is supported by a corner 24 between the curved surface 22 and the side surface 23 of the first pin 21, local stress concentration on the glass sheet 9 can be suppressed. The curved surface 22 is, for example, hemispherical, and the radius of curvature is determined taking into consideration the radius of curvature of the glass sheet 9, etc. The dome-shaped curved surface 22 may be an upwardly convex double curved surface, or may be aspherical.
[0018] The first fixing device 3 movably fixes the position of each first pin 21 in the Z-axis direction. The first fixing device 3 includes, for example, a first outer frame 31 and a first movable key 32. The first outer frame 31 surrounds the first pin group 2. The first movable key 32 protrudes inward from the first outer frame 31 as shown in Fig. 5, and presses adjacent first pins 21 against each other.
[0019] The first outer frame 31 is, for example, a rectangular frame. The first movable key 32 protrudes from one of two opposing side walls of the first outer frame 31 toward the other side wall, and presses adjacent first pins 21 together. Although not shown, the first outer frame 31 may be a circular frame or an elliptical frame, and the shape of the frame is not particularly limited.
[0020] The first movable key 32 is movable in, for example, the X-axis direction. By moving the first movable key 32 in the positive direction of the X-axis, the worker or the work robot moves the first pins 21 together in the positive direction of the X-axis and presses adjacent first pins 21 together. As a result, the position of each first pin 21 in the Z-axis direction can be fixed.
[0021] Furthermore, the worker or the working robot moves the first movable key 32 in the negative direction of the X-axis to release the fixed position of each of the first pins 21 in the Z-axis direction. The position of each of the first pins 21 in the Z-axis direction can be adjusted, and glass sheets 9 with various curved shapes can be formed.
[0022] The first fixing device 3 may further include a first screw 33 that presses the first pin 21 via the first movable key 32. In this case, the first outer frame 31 includes a first screw hole 34 into which the first screw 33 is screwed. The first screw 33 is, for example, a set screw.
[0023] By rotating the first screw 33, the worker or the working robot can move the first movable key 32 and press adjacent first pins 21 together. If the rotation of the first screw 33 is stopped in this state, the first screw 33 continues to press the first movable key 32. This makes it possible to prevent the first movable key 32 from being pushed back by a reaction force.
[0024] Although not shown, the first fixing device 3 may further include a first cylinder instead of the first screw 33. The first cylinder has a cylinder tube, a piston that moves inside the cylinder tube, and a rod that moves together with the piston. The first cylinder presses the first pin 21 via the first movable key 32 by air pressure, hydraulic pressure, or the like.
[0025] The first fastener 3 may include a first arrangement plate 36 in which a plurality of first arrangement holes 35 are formed, through which the first pins 21 are inserted one by one. The first arrangement plate 36 is fixed to the first outer frame 31, for example, by bolts (not shown). The plurality of first arrangement holes 35 are arranged in a staggered manner, similar to the plurality of first pins 21, but may also be arranged in a matrix. The horizontal positions of the first pins 21 can be regulated by the horizontal positions (X-axis direction positions and Y-axis direction positions) of the first arrangement holes 35, and the first pins 21 can be arranged in a desired pattern.
[0026] The first pin 21 may include a first intermediate shaft 25 inserted into the first arrangement hole 35, a first head 26 removably attached to one longitudinal end of the first intermediate shaft 25, and a first flange 27 provided on the other longitudinal end of the first intermediate shaft 25. The first pin 21 is provided with the first head 26 facing the glass plate 9.
[0027] The first head 26 includes an upwardly convex dome-shaped curved surface 22, and supports the glass sheet 9 from below with the curved surface 22. Adjacent first heads 26 are pressed against each other at their side surfaces 23. The first heads 26 are removable, so that they can be replaced if damaged.
[0028] For example, the first head 26 includes a screw hole 28 on a surface facing away from the curved surface 22. The first intermediate shaft 25 includes a threaded shaft that is screwed into the screw hole 28. In this way, the first head 26 is removably attached to the first intermediate shaft 25.
[0029] The first head 26 and the first flange 27 prevent the first intermediate shaft 25 from slipping out of the first alignment hole 35. The diameter of each of the first head 26 and the first flange 27 is larger than the diameter of the first alignment hole 35.
[0030] The first head 26 may further include a hollow hole 29 continuing to the screw hole 28. That is, the first head 26 may have a hollow structure. The heat capacity of the first head 26 can be reduced, and the temperature rise time of the first head 26 can be shortened.
[0031] As will be described in detail later, the first transfer mold 1 is heated from the outside together with the glass plate 9. If the temperature rise rate is fast, the temperatures of the first outer frame 31 and the first movable key 32 may become higher than the temperature of the first pin 21 inside them during the temperature rise.
[0032] Therefore, the first outer frame 31 and the first movable key 32 may be formed of a material with a lower average linear expansion coefficient than the first pins 21. This makes it possible to restrict the first outer frame 31 and the like from expanding beyond the first pin group 2 during the temperature rise, and to restrict the force pressing adjacent first pins 21 together from loosening. The average linear expansion coefficient is the average value of the linear expansion coefficients from room temperature (e.g., 20°C) to the forming temperature of the glass plate 9.
[0033] However, if the temperature rise rate is slow, the first outer frame 31, the first movable key 32, and the first pin group 2 inside them will reach approximately the same temperature. Therefore, the first outer frame 31, the first movable key 32, and the first pins 21 may be made of the same material.
[0034] The first pin 21, the first outer frame 31, or the first movable key 32 is formed of a metal (for example, stainless steel, heat-resistant steel, or cemented carbide), a ceramic (for example, silicon carbide, silicon nitride, or quartz), carbon, or the like.
[0035] The stainless steel may be either martensitic or austenitic. The average linear expansion coefficient of martensitic stainless steel is smaller than that of austenitic stainless steel. The cemented carbide may be, for example, tungsten carbide.
[0036] The first pin 21, the first outer frame 31, or the first movable key 32 may include a base material and a coating film formed on the base material, or may be formed of a plurality of materials. The coating film may cover at least a part of the base material. The coating film may be a metal film, a ceramic film, a carbon film, or the like.
[0037] 5, step S102 includes abutting the tip of each of the first pins 21 against the curved surface 41 of the first mold 4, adjusting the Z-axis direction position of each of the first pins 21, and fixing the same. In this embodiment, the Z-axis direction position of each of the first pins 21 is fixed by the first fixing tool 3, but it may be fixed by welding or the like.
[0038] If the Z-axis direction position of each first pin 21 is fixed by the first fixing tool 3 or by welding, the first transfer mold 1 and the first original mold 4 can be separated before placing the glass plate 9 on the first transfer mold 1, and the separated first original mold 4 can be reused. Therefore, for example, when placing multiple glass plates 9 on different first transfer molds 1 and bending each glass plate 9, the number of first original molds 4 can be reduced.
[0039] Unlike the first transfer mold 1, the first mold 4 is not heated. Therefore, the first mold 4 can be made of a material with lower heat resistance than the first transfer mold 1, and can be manufactured at low cost and in a short period of time. The first mold 4 is manufactured, for example, by a 3D printer, and a resin is used as the material. The first mold 4 may be manufactured by cutting or injection molding. The material of the first mold 4 is not limited to resin, and may be carbon or metal (for example, stainless steel or aluminum).
[0040] The curved surface 41 of the first mold 4 may be a single curved surface or a double curved surface. A single curved surface is a cylindrical surface, etc., and has a constant cross-sectional shape in a predetermined direction. On the other hand, a double curved surface has a curved cross-sectional shape in both a cross section perpendicular to the X-axis direction and a cross section perpendicular to the Y-axis direction.
[0041] Step S103 includes separating each of the first pins 21 from the first mold 4 while fixing the position of each of the first pins 21 in the Z-axis direction. The separated first mold 4 can be reused. Therefore, for example, when multiple glass sheets 9 are placed on different first transfer molds 1 and each glass sheet 9 is bent and shaped, the number of first molds 4 can be reduced.
[0042] 6, step S104 includes placing the glass plate 9 on the first transfer mold 1 with the tips (e.g., first heads 26) of the first pins 21 fixed in step S102 facing upward. The first transfer mold 1 is a lower mold that supports the glass plate 9 from below.
[0043] Step S104 may include laying a heat-resistant cloth 5 between the first transfer mold 1 and the glass plate 9. The heat-resistant cloth 5 is, for example, a nonwoven fabric containing stainless steel fibers or silica fibers. By laying the heat-resistant cloth 5, it is possible to prevent the first pins 21 from leaving marks on the glass plate 9.
[0044] The heat-resistant cloth 5 has a thickness of 0.3 mm to 1.5 mm and a surface density of 100 g / m 2 ~1400g / m 2and the air permeability is 20cc / (cm 2 sec)~200cc / (cm 2 ·sec). Air permeability is measured in accordance with the Japanese Industrial Standard JIS R3240:2013.
[0045] If the heat-resistant cloth 5 has the above-mentioned physical properties, heat transfer between the first pin 21 and the glass plate 9 can be suppressed, thermal stress in the glass plate 9 can be alleviated, and wrinkles in the heat-resistant cloth 5 can be suppressed when the glass plate 9 is bent into a complex curved shape.
[0046] The thickness of the heat-resistant fabric 5 is preferably 0.5 mm to 1.0 mm. The surface density of the heat-resistant fabric 5 is preferably 500 g / m 2 ~1000g / m 2 The air permeability of the heat-resistant fabric 5 is preferably 20 cc / (cm 2 sec)~160cc / (cm 2 sec).
[0047] 7, step S105 includes heating the glass sheet 9 and bending the glass sheet 9 along the tips of the first pins 21 fixed in step S102. The pitch P (not shown) between the center lines of adjacent first pins 21 fixed in step S102 is 5 mm to 30 mm. In this embodiment, the pitch P is equal to the diameter of the first pins 21, but may be larger than the diameter of the first pins 21 as described later.
[0048] If the pitch P is 5 mm or more, the thickness of the first pins 21 is sufficiently large, and deformation of the first pins 21 can be suppressed. On the other hand, if the pitch P is 30 mm or less, local sagging of the glass plate 9 between adjacent first pins 21 can be suppressed. The pitch P is preferably 5 mm to 20 mm.
[0049] Step S105 includes placing the first transfer mold 1 with the glass plate 9 placed on it in a heating furnace, and heating the glass plate 9. The heating furnace may be of a batch type or a continuous type. The heating furnace may be equipped with a conveyor for transporting the first transfer mold 1, or may be of a continuous transport type. A continuous transport type heating furnace is divided into a plurality of zones along the transport path. The glass plate 9 is heated while being transported together with the first transfer mold 1.
[0050] Step S105 may include heating the glass sheet 9 to a preset forming temperature. The forming temperature may be, for example, 10 8 Pa s~10 12 The temperature range is set to correspond to the viscosity range of 10 Pa·s. 8 If the viscosity of the glass is 10 Pa·s or more, it is possible to prevent the first pins 21 from leaving marks on the glass plate 9. 12 If the viscosity of the glass is less than 10 Pa·s, the glass sheet 9 can be bent. 8.5 dPa·s~10 11.5 dPa·s.
[0051] Step S105 includes bending the glass sheet 9 by, for example, the weight of the glass sheet 9. Unlike the case where the upper surface of the glass sheet 9 is pressed by a press machine or the like, it is possible to prevent the glass sheet 9 from being left with contact marks from the press machine.
[0052] Step S105 may include bending the glass sheet 9 using the weight of the glass sheet 9 and air pressure. For example, by blowing compressed air onto the periphery of the glass sheet 9, the periphery of the glass sheet 9 can be bent reliably.
[0053] In this embodiment, a press machine is not used in step S105, but a press machine may be used. The press machine is provided, for example, in one zone of a continuous conveying heating furnace. The press machine presses an upper mold placed above the glass sheet 9 downward, and the glass sheet 9 is sandwiched between the upper mold and the first transfer mold 1 to perform press molding. The upper mold is attached to the press machine, but may be placed on the glass sheet 9 and conveyed together with the glass sheet 9. In the latter case, the upper mold may be a second transfer mold 6 described later.
[0054] Next, a second transfer mold 6 and a method for manufacturing a glass plate using the second transfer mold 6 will be described with reference to Figs. 8 to 11. The second transfer mold 6 is used in combination with the first transfer mold 1. In this case, step S101 includes preparing the second transfer mold 6. The second transfer mold 6 is configured similarly to the first transfer mold 1, and includes, for example, a second pin group 7 and a second fixing tool 8, as shown in Fig. 8.
[0055] The second pin group 7 includes three or more second pins 71 that are independently movable in the longitudinal direction and parallel to one another. The second fixing device 8 movably fixes the position of each second pin 71. The position of each second pin 71 can be adjusted, allowing glass sheets 9 of various curved shapes to be formed. It is also possible to measure the deviation between the curved shape of the glass sheet 9 and a target curved shape, and finely adjust the position of each second pin 71 so as to reduce the deviation.
[0056] Each second pin 71 is arranged parallel to, for example, the Z-axis direction. The longitudinal direction of each second pin 71 is, for example, the Z-axis direction. When viewed from the longitudinal direction of each second pin 71, the multiple second pins 71 are arranged in a staggered pattern, but may also be arranged in a matrix.
[0057] 8, the tip of each second pin 71 includes a downwardly convex dome-shaped curved surface 72, and the curved surface 72 presses the glass plate 9 from above. Compared to the case where the glass plate 9 is pressed by the corner 74 between the curved surface 72 and the side surface 73 of the second pin 71, local stress concentration on the glass plate 9 can be suppressed.
[0058] The second fixing device 8 movably fixes the position of each second pin 71 in the Z axis direction. The second fixing device 8 includes, for example, a second outer frame 81 and a second movable key 82. The second outer frame 81 surrounds the second pin group 7. The second movable key 82 protrudes inward from the second outer frame 81 as shown in Fig. 9, and presses adjacent second pins 71 against each other.
[0059] The second fixing device 8 may further include a second screw 83 that presses the second pin 71 via the second movable key 82. In this case, the second outer frame 81 includes a second screw hole 84 into which the second screw 83 is screwed. The second screw 83 is, for example, a set screw.
[0060] Although not shown, the second fixing device 8 may further include a second cylinder instead of the second screw 83. The second cylinder has a cylinder tube, a piston that moves inside the cylinder tube, and a rod that moves together with the piston. The second cylinder presses the second pin 71 via the second movable key 82 by air pressure, hydraulic pressure, or the like.
[0061] The second fastener 8 may include a second arrangement plate 86 in which a plurality of second arrangement holes 85 are formed, through which the second pins 71 are inserted one by one. The second arrangement plate 86 is fixed to the second outer frame 81 by, for example, bolts (not shown). The plurality of second arrangement holes 85 are arranged in the same manner as the plurality of second pins 71.
[0062] The second pin 71 may include a second intermediate shaft 75 inserted into the second arrangement hole 85, a second head 76 removably attached to one longitudinal end of the second intermediate shaft 75, and a second flange 77 provided on the other longitudinal end of the second intermediate shaft 75. The second pin 71 is provided with the second head 76 facing the glass plate 9.
[0063] The second head 76 includes a downwardly convex dome-shaped curved surface 72, and presses the glass plate 9 from above with the curved surface 72. Adjacent second heads 76 are pressed against each other with their side surfaces 73. The second heads 76 are removable, so that they can be replaced if damaged.
[0064] For example, the second head 76 includes a screw hole 78 on a surface facing away from the curved surface 72. The second intermediate shaft 75 includes a threaded shaft that is screwed into the screw hole 78. In this way, the second head 76 is removably attached to the second intermediate shaft 75.
[0065] The second head 76 and the second flange 77 prevent the second intermediate shaft 75 from slipping out of the second alignment hole 85. The diameter of each of the second head 76 and the second flange 77 is larger than the diameter of the second alignment hole 85.
[0066] The second head 76 may further include a hollow hole 79 continuing to the screw hole 78. That is, the second head 76 may have a hollow structure. The heat capacity of the second head 76 can be reduced, and the temperature rise time of the second head 76 can be shortened.
[0067] The second outer frame 81 and the second movable key 82 may be formed of a material having a lower average linear expansion coefficient than the second pin 71. However, the second outer frame 81 and the second movable key 82, and the second pin 71 may be formed of the same material.
[0068] The second pin 71, the second outer frame 81, or the second movable key 82 is formed of a metal (for example, stainless steel, heat-resistant steel, or cemented carbide), a ceramic (for example, silicon carbide, silicon nitride, or quartz), carbon, or the like.
[0069] The second pin 71, the second outer frame 81, or the second movable key 82 may include a base material and a coating film formed on the base material, or may be formed of a plurality of materials. The coating film may cover at least a portion of the base material.
[0070] 9, step S102 includes abutting the tip of each second pin 71 against the curved surface 41A of the second mold 4A, and adjusting and fixing the Z-axis position of each second pin 71. In this embodiment, the Z-axis position of each second pin 71 is fixed by the second fixture 8, but it may also be fixed by welding or the like.
[0071] If the Z-axis direction position of each second pin 71 is fixed by the second fixing tool 8 or by welding, the second transfer mold 6 and the second original mold 4A can be separated before placing the second transfer mold 6 on the glass plate 9, and the separated second original mold 4A can be reused. Therefore, for example, when placing different second transfer molds 6 on multiple glass plates 9 to bend and shape each glass plate 9, the number of second original molds 4A can be reduced.
[0072] Unlike the second transfer mold 6, the second mold 4A is not heated. Therefore, the second mold 4A can be made of a material with lower heat resistance than the second transfer mold 6, and can be manufactured at low cost and in a short period of time. The second mold 4A is manufactured, for example, by a 3D printer, and a resin is used as the material. The second mold 4A may be manufactured by cutting or injection molding. The material of the second mold 4A is not limited to resin, and may be carbon or metal (for example, stainless steel or aluminum).
[0073] The curved surface 41A of the second mold 4A may be a single curved surface or a double curved surface. The curved surface 41A of the second mold 4A may have a different radius of curvature from the curved surface 41 of the first mold 4. More specifically, the curved surface 41A of the second mold 4A may have a smaller radius of curvature than the curved surface 41 of the first mold 4.
[0074] Step S103 includes separating each of the second pins 71 from the second master 4A while fixing the Z-axis position of each of the second pins 71. The separated second master 4A can be reused. Therefore, for example, when placing different second transfer dies 6 on a plurality of glass plates 9 to bend and shape each glass plate 9, the number of second master dies 4A can be reduced.
[0075] 10, step S104 includes placing the second transfer mold 6 on the glass plate 9 with the tips (e.g., second heads 76) of the second pins 71 fixed in step S102 facing downward. The second transfer mold 6 is an upper mold that presses the glass plate 9 from above.
[0076] Step S104 may include laying a heat-resistant cloth 5A between the second transfer mold 6 and the glass plate 9. The heat-resistant cloth 5A has the same configuration as the heat-resistant cloth 5. Laying the heat-resistant cloth 5A can prevent the second pins 71 from leaving marks on the glass plate 9. Note that the heat-resistant cloth 5A may also be laid on the glass plate 9 when the glass plate 9 is press-molded with an upper mold attached to a press machine.
[0077] The second fixing device 8 may include a mounting plate 87 for attaching the heat-resistant cloth 5A to the second outer frame 81. The heat-resistant cloth 5A can be stretched along the tips of the second pins 71 fixed in step S102.
[0078] The mounting plate 87 is fixed to the second outer frame 81, and the heat-resistant cloth 5A is attached to the mounting plate 87 by a plurality of bolts 88 or the like. Each bolt 88 is inserted into a through hole in the heat-resistant cloth 5A and screwed into a bolt hole in the mounting plate 87.
[0079] It should be noted that the first fixing tool 3 does not include a mounting plate for attaching the heat-resistant cloth 5 to the first outer frame 31, but may include one. In the latter case, when the second transfer mold 6 presses the glass plate 9 from above, the heat-resistant cloth 5 laid under the glass plate 9 is bent along the tips of the first pins 21 fixed in step S102. Note that before the second transfer mold 6 is placed on the glass plate 9, the heat-resistant cloth 5 laid under the glass plate 9 is stretched flat by the mounting plate.
[0080] Step S104 may include guiding the second transfer die 6 in the vertical direction relative to the first transfer die 1 by inserting a guide rod 11 fixed to the first transfer die 1 into a guide hole 61 fixed to the second transfer die 6. This makes it possible to suppress tilting of the second transfer die 6.
[0081] Three or more guide rods 11 are provided, each of which is set up vertically. A guide hole 61 is provided for each guide rod 11. The arrangement of the guide rods 11 and the guide holes 61 may be reversed. In other words, the guide rods 11 may be fixed to the second transfer mold 6, and the guide holes 61 may be fixed to the first transfer mold 1.
[0082] 11, step S105 includes heating the glass sheet 9 and bending the glass sheet 9 along the tips of the second pins 71 fixed in step S102. The weight of the second transfer mold 6 can press the glass sheet 9, and the entire glass sheet 9 can be reliably bent.
[0083] Next, a modified example of the first fixing device 3 will be described with reference to Fig. 12. In the first fixing device 3 of the above embodiment, adjacent first pins 21 are pressed together by a first outer frame 31 and a first movable key 32, fixing the Z-axis direction position of each of the first pins 21. In contrast, in the first fixing device 3 of this modified example, a first arrangement plate 36 and a movable plate 37 fix the Z-axis direction position of each of the first pins 21.
[0084] Similar to the first arrangement plate 36, the movable plate 37 is formed with a plurality of insertion holes 38 through which the first pins 21 are inserted one by one. The plurality of insertion holes 38 are arranged similarly to the plurality of first pins 21. By moving the movable plate 37 in a direction perpendicular to the longitudinal direction of each of the first pins 21, each of the first pins 21 can be sandwiched between the first arrangement plate 36 and the movable plate 37, and the Z-axis direction position of each of the first pins 21 can be fixed. The second fixture 8 may also be configured similarly to the first fixture 3 of this modified example. EXAMPLES
[0085] Next, experimental data will be described. In Examples 1 to 6, bending of a glass sheet was performed under the same conditions except for the conditions shown in Table 1. The glass sheet was soda lime glass. The glass sheet before bending had an X-axis dimension of 300 mm, a Y-axis dimension of 200 mm, and a Z-axis dimension (thickness) of 1.8 mm. The target curved surface of the lower surface of the glass sheet after bending was a single curved surface. The single curved surface had a cross-sectional shape perpendicular to the Y-axis direction with a curvature radius of 900 mm, and a cross-sectional shape perpendicular to the X-axis direction was linear. Examples 1 to 6 are all working examples. Table 1 shows the main conditions and the results.
[0086] [Table 1] In Table 1, when the transfer mold is only the lower mold, it means that the glass plate was bent using only the weight of the glass plate, and when the transfer mold is both upper and lower molds, it means that the glass plate was bent using the weight of the upper mold and the weight of the glass plate. In Table 1, when the transfer mold is both upper and lower molds and there is heat-resistant cloth, it means that the heat-resistant cloth was placed between the upper and lower molds and the glass plate. η is the viscosity (dPa s) equivalent to the forming temperature. The heating rate was set so that it took 4 hours to reach the forming temperature from room temperature. The forming time is the time the glass plate was heated at the forming temperature.
[0087] In Table 1, Ra is the arithmetic mean roughness as defined in the Japanese Industrial Standard JIS B0601:2013, and Wa is the arithmetic mean waviness as defined in the Japanese Industrial Standard JIS B0601:2013. Ra and Wa were measured using a non-contact three-dimensional measuring device (NH-3MAS) manufactured by Mitaka Koki Co., Ltd. The measurement pitch was 0.4 μm, and the measurement range was 5000 μm. Ra was calculated by setting the cutoff value to 0.08 mm. Wa was calculated by setting the cutoff value to 0.8 mm.
[0088] The pin marks were evaluated using Ra. The smaller the Ra, the smaller the pin mark and the better the pin mark evaluation. A pin mark evaluation of "◯" indicates that Ra is 0 μm or more and less than 0.002 μm. A pin mark evaluation of "△" indicates that Ra is 0.002 μm to 0.006 μm. A pin mark evaluation of "×" indicates that Ra is more than 0.006 μm.
[0089] Waviness was evaluated using Wa. The smaller Wa is, the smaller the waviness and the better the waviness evaluation. A waviness evaluation of "◯" indicates that Wa is 0 μm or more and less than 0.0003 μm. A waviness evaluation of "△" indicates that Wa is 0.0003 μm to 0.001 μm. A waviness evaluation of "×" indicates that Wa is more than 0.001 μm.
[0090] In Table 1, the PV (Peak to Valley) value is the maximum height difference between the deviation of the actual curved surface and the target curved surface, and was measured using a three-dimensional measuring device ATOS (model number: ATOS Triple scan III) manufactured by GOM.
[0091] Shape error was evaluated using PV value. The smaller the PV value, the smaller the shape error and the better the shape error evaluation. A shape error evaluation of "◯" indicates that the PV value is between 0mm and 0.5mm. A shape error evaluation of "△" indicates that the PV value is between 0.5mm and 1.5mm. A shape error evaluation of "×" indicates that the PV value is over 1.5mm. A PV value of 1.5mm or less ensures the design of the curved glass. A PV value of 0.5mm or less can improve the fit of the curved glass for automotive use with the vehicle body.
[0092] The transmission images of the glass plates obtained in Examples 1 to 6 are shown in Fig. 13. The transmission images of the glass plates were obtained by placing a light source on the opposite side of the screen with the glass plate as a reference, and capturing an image reflected on the screen. The transmission images shown in Fig. 13 have been binarized. The black areas in the transmission images represent pin marks.
[0093] From the results of Examples 1 and 2, it can be seen that by placing a heat-resistant cloth between the glass plate and the transfer mold, pin marks and waviness can be reduced, but shape error increases. The reason for the large shape error is that the heat-resistant cloth prevents the glass plate from deforming due to its own weight. A nonwoven fabric made of stainless steel fibers was used as the heat-resistant cloth.
[0094] Furthermore, from the results of Examples 1 and 3, it can be seen that even when a heat-resistant cloth is placed between the glass plate and the transfer mold, if both the upper and lower molds are used as the transfer mold, the glass plate can be pressed by the weight of the upper mold, the entire glass plate can be bent reliably, and shape error can be reduced.
[0095] Furthermore, it can be seen from the results of Examples 3 to 5 that pin marks and waviness can be reduced by lowering the molding temperature. It can also be seen that even if the molding temperature is lowered, the deterioration of shape error can be prevented by pressing the glass sheet with the weight of the upper mold.
[0096] Table 2 shows the relationship between pin pitch and PV value when a glass plate is heated at 620°C for 1200 seconds. The relationship shown in Table 2 was obtained by viscoelastic analysis using commercially available analysis software (ABAQUS). The physical properties of the glass used in the viscoelastic analysis are shown in Table 3.
[0097] [Table 2]
[0098] [Table 3] The physical properties shown in Table 3 are those of soda-lime glass. In Table 2, the PV value is the maximum height difference between the actual curved surface after bending and the target curved surface. The target curved surface was a double curved surface. The cross-sectional shape perpendicular to the Y-axis direction of the double curved surface was a curved shape with a radius of curvature of 900 mm, and the cross-sectional shape perpendicular to the X-axis direction was a curved shape with a radius of curvature of 2000 mm. The glass sheet before bending had an X-axis dimension of 82 mm, a Y-axis dimension of 43 mm, and a Z-axis dimension (thickness) of 1.8 mm. The pin tip surface was a hemisphere with a radius of 3 mm. The presence or absence of heat-resistant cloth was set to "none."
[0099] From Table 2, we can see that to keep the PV value at 1.5 mm or less, the pin pitch should be 30 mm or less, and to keep the PV value at 0.5 mm or less, the pin pitch should be 20 mm or less.
[0100] The manufacturing method of the glass plate and the transfer mold according to the present disclosure have been described above, but the present disclosure is not limited to the above-mentioned embodiments. Various changes, modifications, substitutions, additions, deletions, and combinations are possible within the scope of the claims. These naturally fall within the technical scope of the present disclosure. [Explanation of symbols]
[0101] 1. First transcription type 2 First pin group 21 1st pin 3 First fixture
Claims
1. A method for producing a glass sheet having a curved surface, comprising the steps of: preparing a first transfer mold including a first pin group including three or more first pins that are independently movable in a longitudinal direction and parallel to each other; abutting a tip of each of the first pins against a curved surface of a first mold, and adjusting and fixing a position of each of the first pins; Separating each of the first pins from the first mold while fixing the position of each of the first pins; placing the glass plate on the first transfer mold with the tips of the fixed first pins facing upward; heating the glass sheet and bending the glass sheet along the tips of the fixed first pins; A method for producing a glass sheet, comprising:
2. The method for manufacturing a glass sheet according to claim 1 , wherein the glass sheet is bent by its own weight.
3. The method for manufacturing a glass sheet according to claim 1 , wherein the glass sheet is bent by its own weight and air pressure.
4. The method for manufacturing a glass plate according to claim 1 , wherein an upper mold disposed above the glass plate is pressed downward by a press machine, and the glass plate is sandwiched between the upper mold and the first transfer mold to perform press molding.
5. preparing a second transfer mold including a second pin group including three or more second pins that are independently movable in a longitudinal direction and parallel to each other; abutting a tip of each of the second pins against a curved surface of a second mold, adjusting and fixing a position of each of the second pins; Separating each of the second pins from the second mold while fixing the position of each of the second pins; placing the second transfer mold on the glass plate with the tips of the fixed second pins facing downward; bending the glass sheet along the tips of the fixed second pins; The method for producing a glass sheet according to claim 1 , comprising:
6. a guide rod is fixed to one of the first transfer die and the second transfer die, and a guide hole is fixed to the other of the first transfer die and the second transfer die; The method for manufacturing a glass sheet according to claim 5 , further comprising: guiding the second transfer mold in a vertical direction relative to the first transfer mold by inserting the guide rod into the guide hole.
7. The method for manufacturing a glass plate according to any one of claims 1 to 5, wherein the tip of each of the first pins includes an upwardly convex dome-shaped curved surface, and the curved surface supports the glass plate.
8. 8. The method for manufacturing a glass plate according to claim 1, wherein a pitch between center lines of the fixed adjacent first pins is 5 mm to 30 mm.
9. The method for manufacturing a glass plate according to any one of claims 1 to 8, further comprising laying a heat-resistant cloth between the first pin group and the glass plate.
10. The heat-resistant fabric has a thickness of 0.3 mm to 1.0 mm and a surface density of 100 g / m 2 ~1400g / m 2 and the air permeability is 20 cc / (cm 2 ・sec)~200cc / (cm 2 10. The method for producing a glass plate according to claim 9, wherein the heating time is 100 min.
11. When bending the glass sheet, the glass sheet is heated at a preset forming temperature, The molding temperature is 10 8 Pa.s to 10 12 The method for producing a glass plate according to any one of claims 1 to 10, wherein the temperature range is set within a range corresponding to a viscosity range of Pa·s.
12. A transfer mold used in the manufacture of a glass plate having a curved surface shape, A pin group including three or more pins that are independently movable in a longitudinal direction and parallel to each other; and a fixture for fixing the position of each of the pins.
13. The transfer mold according to claim 12 , wherein the fixing device includes an outer frame that surrounds the group of pins, and a movable key that protrudes inward from the outer frame and presses adjacent pins together.
14. The fastener further includes a screw that presses the pin through the movable key; The transfer mold according to claim 13 , wherein the outer frame includes a screw hole into which the screw is screwed.
15. The transfer mold according to claim 13 , wherein the fixture further comprises a cylinder that presses the pin through the movable key.
16. The transfer mold according to any one of claims 13 to 15, wherein the fixing device includes a mounting plate for attaching a heat-resistant cloth to the outer frame.
17. The transfer mold according to any one of claims 12 to 16, wherein the fixing device includes an arrangement plate having a plurality of insertion holes formed therein, through which the pins are inserted one by one.
18. The transfer mold according to claim 17, wherein the pin includes an intermediate shaft inserted into the insertion hole, a head removably attached to one longitudinal end of the intermediate shaft, and a flange provided on the other longitudinal end of the intermediate shaft, with the head facing the glass plate.
19. The transfer mold according to any one of claims 12 to 18, wherein the pin has a hollow structure.
20. The transfer mold according to any one of claims 12 to 19, wherein a tip of each of the pins includes a dome-shaped curved surface and supports the glass plate with the curved surface.
21. The transfer mold according to any one of claims 12 to 20, wherein a pitch between center lines of adjacent pins is 5 mm to 30 mm in a state in which the pins are fixed by the fixing device.
Citation Information
Patent Citations
Apparatus and method for capturing, deforming and positioning thin glass panes
JP2020511389A
Glass forming mold of adjustable shape
WO2016141041A1
Bending device and bending method
WO2020080305A1