Electrode manufacturing apparatus

The method addresses uneven coating in electrode manufacturing by employing granules and controlled electrostatic fields to achieve uniform application, improving efficiency and reducing solvent use.

JP7559698B2Active Publication Date: 2024-10-02TOYOTA JIDOSHA KK
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2021120372
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-07-21
Publication Date
2024-10-02
Estimated Expiration
2041-07-21

AI Technical Summary

Technical Problem

Existing electrode manufacturing methods using electrostatic coating face issues with uneven coating due to varying adhesion forces between electrode material and magnetic particles, leading to coating inconsistencies and yield loss.

Method used

A method involving the use of granules containing active material powder and a binder, transported without magnetic force, utilizing two stages of electrostatic coating: one in a direction intersecting the vertical axis and another in the vertical axis, with controlled electric fields to ensure uniform application onto a base material.

Benefits of technology

This approach reduces coating unevenness and yield loss by ensuring consistent adhesion of granules to the base material, enhancing the manufacturing process efficiency and reducing solvent use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007559698000001
    Figure 0007559698000001
  • Figure 0007559698000002
    Figure 0007559698000002
  • Figure 0007559698000003
    Figure 0007559698000003
Patent Text Reader

Abstract

To reduce the unevenness of coating.SOLUTION: An electrode manufacturing method includes steps (a) to (f). A step (a) prepares a granule that includes active material powder and a binder. A step (b) supplies the granule to the surface of a roll. A step (c) charges the granule with electricity. A step (d) conveys the granule from a first region to a second region by rotation of the roll. A step (e) forms a first electric field between the second region and a third region and whereby causes the granule to fly from the second region toward the third region. A step (f) forms a second electric field between the third region and a substrate and whereby causes the granule to fly from the third region toward the substrate. The second region is at a lower position than the first region in the vertical direction. The third region is separate from the second region in a direction that crosses the vertical direction. The substrate is at a lower position than the third region in the vertical direction. An active material layer is formed as the granule adheres to the substrate.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an electrode manufacturing method and an electrode manufacturing apparatus. [Background technology]

[0002] JP 2020-149862 A discloses a method for manufacturing an electrode sheet. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-149862 A Summary of the Invention [Problem to be solved by the invention]

[0004] The electrode includes a substrate and an active material layer. The active material layer can be formed by applying a powder (electrode material) to the surface of the substrate.

[0005] A method for manufacturing electrodes by electrostatic coating has been proposed. Electrostatic coating is expected to form an active material layer with a homogeneous composition. Furthermore, in order to increase productivity, electrostatic coating can be performed by a roll-to-roll method.

[0006] To apply the roll-to-roll method to electrostatic coating, for example, a magnet roll can be used. That is, the powder is attracted to the surface of the magnet roll by magnetic force. The substrate is supported by a backup roll. An electric field is formed in the gap between the magnet roll and the backup roll. Electrostatic force acts on the powder in the electric field. The electric field strength is adjusted so that the electrostatic force overcomes the magnetic force. The electrostatic force causes the powder to detach from the magnet roll. The powder flies toward the substrate. The powder adheres to the substrate. This can form an active material layer, i.e. an electrode can be produced. Electrodes can be produced continuously by rotating the roll.

[0007] When the electrode material does not have magnetic properties, a magnetic carrier (magnetic particles) can be used. That is, the electrode material is mixed with the magnetic particles, so that the electrode material adheres to the magnetic particles. The magnetic particles are attracted to the magnet roll by magnetic force. This allows the electrode material to be supported by the magnet roll.

[0008] However, the adhesive strength between the electrode material and the magnetic particles tends to vary widely. If the adhesive strength is too strong, the electrode material may not separate from the magnetic particles even when electrostatic force acts on it. This can result in uneven coating.

[0009] An object of the present disclosure is to reduce painting unevenness. [Means for solving the problem]

[0010] The technical configuration and effects of the present disclosure will be described below. However, the mechanism of action in this specification includes assumptions. The mechanism of action does not limit the technical scope of the present disclosure.

[0011] 1. A method for producing an electrode includes the following steps (a) to (f). (a) Granules containing an active material powder and a binder are prepared. (b) The granules are fed onto the surface of the roll. (c) The granules are electrically charged. (d) Rotation of the roll transports the granules from the first region to the second region. (e) A first electric field is formed between the second region and the third region, thereby causing the granules to fly from the second region toward the third region. (f) A second electric field is formed between the third region and the substrate, thereby causing the granules to fly from the third region toward the substrate. In the vertical direction, the second region is located lower than the first region. In a direction intersecting the vertical direction, the third region is separated from the second region. In the vertical direction, the substrate is located lower than the third region. The active material layer is formed by the granules adhering to the substrate.

[0012] When transporting powder (electrode material) without relying on magnetic force, it is difficult to transport the powder in a direction against gravity. This is because the powder may fall from the roll due to gravity. Therefore, when transporting powder without relying on magnetic force, the powder is transported from a high position to a low position in the vertical direction.

[0013] FIG. 1 is a conceptual diagram showing an electrode manufacturing apparatus in a first embodiment. In the first embodiment, powder is transported from a high position to a low position in the vertical direction (Z-axis direction). Furthermore, in the first embodiment, electrostatic coating (flying of powder) is performed vertically downward.

[0014] The backup roll 212 is adjacent to the supply roll 211 in the vertical direction. The backup roll 212 is located lower than the supply roll 211. The supply roll 211 transports the powder 1 to the gap between the supply roll 211 and the backup roll 212. The backup roll 212 transports the substrate 13 to the gap between the supply roll 211 and the backup roll 212. Electrostatic coating is performed in the gap between the supply roll 211 and the backup roll 212. However, before the powder 1 reaches the gap between the supply roll 211 and the backup roll 212, the powder 1 may fall from the supply roll 211 due to gravity. Therefore, in the first reference embodiment, it is considered that coating unevenness and yield loss occur.

[0015] 2 is a conceptual diagram showing an electrode manufacturing apparatus in the second reference embodiment. In the second reference embodiment, the powder is also transported from a high position to a low position in the vertical direction (Z-axis direction). Furthermore, in the second reference embodiment, electrostatic coating (flying of the powder) is performed in the horizontal direction (X-axis direction).

[0016] The supply roll 221 transports the powder 1. The powder 1 is transported within a range where it is unlikely to fall due to gravity. The backup roll 222 is adjacent to the supply roll 221 in the horizontal direction. Electrostatic coating is performed in the gap between the supply roll 221 and the backup roll 222. However, some of the powder 1 that reaches the substrate 13 may not adhere to the substrate 13 and may fall due to gravity. Therefore, it is considered that coating unevenness and yield loss may occur even in the second reference embodiment.

[0017] FIG. 3 is a conceptual diagram showing an electrode manufacturing apparatus in this embodiment. The paint in this disclosure is granules 11. The granules 11 can be prepared by granulating powder. The granules 11 can also be called "granules." Ordinary powders have low fluidity and tend to easily cause particle aggregation during transportation. When particle aggregation occurs, the particles tend to be difficult to fly even when electrostatic force acts. The granules 11 can have a higher fluidity than the powder. It is expected that the granules 11 will be easily flown by electrostatic force.

[0018] In the present disclosure, two-stage electrostatic coating (flying of powder) is performed. The first roll 110 transports the granules 11. The granules 11 are transported from the first region R1 to the second region R2. The granules 11 are transported within a range where they are unlikely to fall due to gravity. Therefore, the falling of the granules 11 due to gravity before electrostatic coating can be reduced. In other words, the yield loss can be reduced.

[0019] 4 is a conceptual diagram showing electrostatic painting in this embodiment. In a direction intersecting the vertical direction, the third region R3 is separated from the second region R2. A first electrostatic painting is performed in a direction intersecting the vertical direction. That is, a first electric field E1 is formed between the second region R2 and the third region R3, and a first electrostatic force F1 acts on the granules 11. The first electrostatic force F1 causes the granules 11 to fly from the second region R2 toward the third region R3.

[0020] Furthermore, a second electrostatic coating is performed in the vertical direction. That is, a second electric field E2 is formed between the third region R3 and the substrate 13, and a second electrostatic force F2 acts on the granules 11 that have moved to the third region R3. The second electrostatic force F2 causes the granules 11 to fly from the third region R3 toward the substrate 13. In addition to the second electrostatic force F2, gravity F3 also acts on the flying granules 11. This is because the substrate 13 is located lower than the third region R3 in the vertical direction. It is expected that the resultant force of the second electrostatic force F2 and gravity F3 acts on the flying granules 11, so that the granules 11 will adhere firmly to the substrate 13. Due to the synergistic effect of the above actions, the present disclosure is expected to reduce uneven coating.

[0021] 2. The granules may have a solid content of, for example, 70 to 100% by mass.

[0022] "Solid content" refers to the mass fraction of components other than the solvent with respect to the entire mixture. Granules are prepared by granulating active material powder and binder. Granules may be in a dry state. Granules may be in a wet state. That is, granules may contain a solvent (liquid). However, granules are different from slurries (particle dispersions). In granules, the solvent forms droplets. In granules, the solvent (liquid) is dispersed in powder (solid). On the other hand, in slurries, the solvent is the dispersion medium. In slurries, powder (solid) is dispersed in the solvent (liquid). The slurry may have a solid content of, for example, 60% or less.

[0023] Conventionally, electrodes are generally manufactured by coating a slurry. However, in conventional methods, a large amount of solvent may be used. In the present disclosure, the amount of solvent used may be reduced. By reducing the amount of solvent, for example, reduction in manufacturing costs and environmental load is expected.

[0024] 3. The granules may have a D50 of, for example, 100-200 μm.

[0025] By the granules having a D50 of 100 to 200 μm, for example, the granules are expected to exhibit suitable flowability.

[0026] 4. The granules may have an angle of repose of, for example, 50° or less.

[0027] The angle of repose is an index of the fluidity of powder or granular material. The smaller the angle of repose, the higher the fluidity of the powder or granular material is considered to be. The angle of repose can become smaller due to the granulation of the powder. Granules having an angle of repose of 50° or less are expected to reduce unevenness in painting, for example.

[0028] 5. The first electric field has a first electric field strength. The second electric field has a second electric field strength. For example, the second electric field strength may be lower than the first electric field strength.

[0029] The first electric field intensity can adjust the first electrostatic force. The second electric field intensity can adjust the second electrostatic force. In the second electrostatic coating, gravity acts on the granules in addition to the second electrostatic force. Therefore, for example, the second electric field intensity may be set lower than the first electric field intensity.

[0030] 6. (d) above may include, for example, spreading the granules evenly on the surface of a roll.

[0031] By spreading the granules evenly on the surface of the roll, the variation in the amount of granules supplied can be reduced, which is expected to reduce unevenness in the coating, for example.

[0032] 7. The method for producing an electrode may further include, for example, the following (g) etc. (g) At least one of pressure and heat is applied to the active material layer to fix the active material layer to the substrate.

[0033] As a result of the above (g), for example, the peel strength of the active material layer is expected to be improved.

[0034] 8. The electrode manufacturing apparatus manufactures an electrode by adhering granules containing an active material powder and a binder to a substrate. The electrode manufacturing apparatus includes a first roll, an intermediate plate, a second roll, and an electric field forming device. The intermediate plate is spaced apart from the first roll in a direction intersecting the vertical direction. In the vertical direction, the second roll is located lower than the first roll and the intermediate plate. The electric field forming device is configured to form a first electric field between the first roll and the intermediate plate, and to form a second electric field between the intermediate plate and the second roll. The first roll is configured to transport the granules into the first electric field. The second roll is configured to transport the substrate into the second electric field.

[0035] In the electrode manufacturing apparatus of the above item 8, the granules can arrive at the substrate by flying through the first electric field and the second electric field in sequence. In other words, the electrode manufacturing method of the above item 1 can be carried out.

[0036] 9. The electrode manufacturing apparatus may further include, for example, a third roll. The electrode manufacturing apparatus may be configured such that the granules are spread evenly in the gap between the first roll and the third roll before the granules reach the first electric field.

[0037] The electrode manufacturing apparatus described in 9. above can be used to carry out the electrode manufacturing method described in 6. above. [Brief description of the drawings]

[0038] [Figure 1] FIG. 1 is a conceptual diagram showing an electrode manufacturing apparatus in the first embodiment. [Diagram 2] FIG. 2 is a conceptual diagram showing an electrode manufacturing apparatus in the second reference embodiment. [Diagram 3] FIG. 3 is a conceptual diagram showing an electrode manufacturing apparatus in this embodiment. [Figure 4] FIG. 4 is a conceptual diagram showing electrostatic painting in this embodiment. [Diagram 5] FIG. 5 is a schematic flow chart of a method for producing an electrode in this embodiment. [Figure 6]FIG. 6 is a conceptual diagram showing an example of an electrode. [Figure 7] FIG. 7 is a set of photographs showing the results of the first and second production examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0039] <Definitions of terms, etc.> Hereinafter, an embodiment of the present disclosure (which may be abbreviated as "the present embodiment" in this specification) and an example of the present disclosure (which may be abbreviated as "the present embodiment" in this specification) will be described. However, the present embodiment and the example do not limit the technical scope of the present disclosure.

[0040] In this specification, the words "comprise," "include," "have," and variations thereof (e.g., "consisting of") are open-ended. The open-ended form may or may not include additional elements in addition to the required elements. The word "consisting of" is closed-ended. However, even in a closed form, additional elements that are normally associated impurities or unrelated to the disclosed technology are not excluded. The word "consisting essentially of..." is semi-closed. In a semi-closed form, the addition of elements that do not substantially affect the basic and novel characteristics of the disclosed technology is permitted.

[0041] In this specification, the expressions "may" and "can" are used in the permissive sense of "have the potential to" rather than in the obligatory sense of "must".

[0042] In this specification, elements expressed in the singular include the plural unless otherwise specified. For example, a "particle" can mean not only a "single particle" but also a "group of particles."

[0043] In the methods described herein, the order of execution of multiple steps, operations, and the like is not limited to the order described unless otherwise specified. For example, multiple steps may proceed simultaneously. For example, multiple steps may be performed one after the other.

[0044] In this specification, geometric terms (e.g., "parallel," "orthogonal," etc.) should not be interpreted in a strict sense. For example, "parallel" may deviate slightly from the strict meaning of "parallel." In this specification, geometric terms may include, for example, tolerances, errors, etc. in design, work, manufacturing, etc. The dimensional relationships in each figure may not match the actual dimensional relationships. In order to facilitate understanding of the disclosed technology, the dimensional relationships (length, width, thickness, etc.) in each figure may be changed. Furthermore, some configurations may be omitted.

[0045] In this specification, the term "direction intersecting the vertical direction" refers to any direction that is not parallel to the vertical direction. The direction intersecting the vertical direction includes, for example, a direction perpendicular to the vertical direction (i.e., a horizontal direction). The direction intersecting the vertical direction may be perpendicular to the rotation axis of each roll.

[0046] In this specification, a numerical range such as "70 to 100%" includes an upper limit and a lower limit unless otherwise specified. That is, "70 to 100%" indicates a numerical range of "70% or more and 100% or less". In addition, a numerical value arbitrarily selected from within the numerical range may be set as a new upper limit or lower limit. For example, a new numerical range may be set by arbitrarily combining a numerical value within the numerical range with a numerical value described in another part, table, figure, etc. of this specification.

[0047] In this specification, all numerical values ​​are modified by the term "about". The term "about" may mean, for example, ±5%, ±3%, ±1%, etc. All numerical values ​​are approximations that may vary depending on the application of the disclosed technology. All numerical values ​​are expressed in significant figures. Measurements may be average values ​​of multiple measurements. The number of measurements may be three or more, five or more, or ten or more. Measurements may be rounded off based on the number of significant figures. Measurements may include errors associated with, for example, the detection limits of the measurement device.

[0048] In this specification, "D50 of 100 μm or more" refers to the particle size at which the cumulative frequency from the smaller particle size reaches 50% in the particle size distribution based on mass (number). The particle size distribution based on mass can be measured in accordance with "JIS Z 8815 General rules for sieving test method".

[0049] In this specification, "D50 less than 100 μm" refers to a particle size at which the cumulative frequency from the smaller particle size reaches 50% in a volume-based particle size distribution. The volume-based particle size distribution can be measured by a laser diffraction particle size distribution measuring device.

[0050] In this specification, the "angle of repose" refers to the angle between the horizontal plane and the slope of a cone (pile of powder) formed when powder falls naturally onto a horizontal plane. The angle of repose can be measured using a powder property evaluation device "Powder Tester" manufactured by Hosokawa Micron Corporation or an equivalent device.

[0051] In this specification, when a compound is expressed by a stoichiometric composition formula such as "LiCoO2", the stoichiometric composition formula is merely a representative example. The composition ratio may be non-stoichiometric. For example, when lithium cobalt oxide is expressed as "LiCoO2", unless otherwise specified, the lithium cobalt oxide is not limited to the composition ratio of "Li / Co / O=1 / 1 / 2" and may contain Li, Co and O in any composition ratio. Furthermore, doping, substitution, etc. with trace elements may be allowed.

[0052] In this specification, the "melting point" refers to the peak top temperature of the melting peak (endothermic peak) in a DSC (Differential Scanning Calorimetry) curve. The DSC curve can be measured in accordance with "JIS K 7121 Method for Measuring Transition Temperature of Plastics." "Near the melting point" can refer to, for example, a range of the melting point ±20°C.

[0053] <Electrode manufacturing equipment> 3 is a conceptual diagram showing an electrode manufacturing apparatus in this embodiment. Hereinafter, the "electrode manufacturing apparatus in this embodiment" may be abbreviated as "the present manufacturing apparatus." The present manufacturing apparatus 100 manufactures an electrode 10 by adhering granules 11 to a substrate 13.

[0054] The present manufacturing apparatus 100 includes a first roll 110, an intermediate plate 140, a second roll 120, and an electric field forming device 150. The present manufacturing apparatus 100 may further include, for example, a hopper 160, a third roll 130, and the like.

[0055] The manufacturing apparatus 100 may further include, for example, a control device (not shown) etc. The control device may limit the operation of each element.

[0056] The present manufacturing apparatus 100 may further include, for example, a fixing device (not shown) and the like. The fixing device can apply at least one of heat and pressure to the active material layer 12. The fixing device may include, for example, a pair of heat rolls and the like.

[0057] In Figure 3, the axes of rotation of each roll may be substantially parallel, and the curved arrows on each roll indicate the direction of rotation of the roll.

[0058] Electric field generating device 4 is a conceptual diagram showing electrostatic painting in this embodiment. The electric field forming device 150 includes a first power source 151 and a second power source 152. Each of the first power source 151 and the second power source 152 may include, for example, a high-voltage power source device. The first power source 151 and the second power source 152 may be independent of each other, for example. The first power source 151 and the second power source 152 may be integrated, for example.

[0059] The first power source 151 applies a DC voltage (potential difference) between the first roll 110 and the relay plate 140. That is, the first power source 151 forms a first electric field E1 between the first roll 110 and the relay plate 140. The second power source 152 applies a DC voltage between the relay plate 140 and the second roll 120. That is, the second power source 152 forms a second electric field E2 between the relay plate 140 and the second roll 120.

[0060] In the present manufacturing apparatus 100, the granules 11 fly sequentially through the first electric field E1 and the second electric field E2, so that the granules 11 can arrive at the substrate 13. The granules 11 adhere to the substrate 13, so that the active material layer 12 can be formed.

[0061] "hopper" The granules 11 may be filled, for example, in a hopper 160 (see FIG. 3). The hopper 160 includes a rotary feeder 161. The rotary feeder 161 may deliver the granules 11, for example, at a constant flow rate.

[0062] <<First Roll>> The first roll 110 is conductive. The first roll 110 may be made of, for example, a metal. The entire first roll 110 may be conductive. A part of the first roll 110 may be conductive. For example, a part in contact with the granules 11 may be conductive. For example, a surface layer of the first roll 110 may be conductive. The first roll 110 is electrically connected to a first power source 151.

[0063] The first roll 110 may also be referred to as a "supply roll", for example. The first roll 110 receives the granules 11 from the hopper 160 in the first region R1. The first roll 110 rotates to transport the granules 11 in the circumferential direction. The granules 11 are transported from the first region R1 to the second region R2.

[0064] In the vertical direction, the second region R2 is located lower than the first region R1. The second region R2 is formed in a gap between the first roll 110 and the relay plate 140. A first electric field E1 is formed between the first roll 110 and the relay plate 140. That is, the first roll 110 transports the granules 11 into the first electric field E1.

[0065] The first region R1 may be, for example, arc-shaped. For example, a "clock position" may be set with the rotation axis of the first roll 110 as the center. The 6 o'clock direction and the 12 o'clock direction at the clock position are parallel to the vertical direction (Z-axis direction). The 3 o'clock direction and the 9 o'clock direction at the clock position are parallel to the horizontal direction (X-axis direction). The first region R1 may be formed, for example, between the 11 o'clock direction and the 1 o'clock direction. The first region R1 may be formed, for example, between the 12 o'clock direction and the 1 o'clock direction. The central angle of the sector formed by both ends of the first region R1 and the center (rotation axis) of the first roll 110 may be, for example, 1 to 45°.

[0066] The second region R2 faces the relay plate 140. The range of the second region R2 can be adjusted, for example, by the size, shape, etc. of the relay plate 140. The second region R2 may be, for example, arc-shaped. The second region R2 may be formed, for example, between the 2 o'clock direction and the 4 o'clock direction. The second region R2 may be formed, for example, between the 2 o'clock direction and the 3 o'clock direction. This is expected to reduce, for example, the falling of the granules 11 (yield loss). The central angle of the sector formed by both ends of the second region R2 and the center of the first roll 110 may be, for example, 1 to 45°.

[0067] "Third Roll" The third roll 130 is disposed between the hopper 160 and the relay plate 140 (see FIG. 3). The third roll 130 faces the first roll 110. The third roll 130 may also be referred to as a "squeegee", for example. The granules 11 are spread evenly in the gap between the first roll 110 and the third roll 130. This may reduce, for example, the variation in the supply amount of the granules 11.

[0068] The diameter of the third roll 130 may be smaller than the diameter of the first roll 110, for example. The rotation direction of the third roll 130 may be opposite to the rotation direction of the first roll 110, for example. By rotating the third roll 130 in the opposite direction to the rotation direction of the first roll 110, the variation in the supply amount of the granules 11 (the thickness of the granule layer) may be reduced. Note that a squeegee in a form other than a roll may be used. For example, a blade-type squeegee or the like may be used.

[0069] Relay Board The relay board 140 is conductive. The relay board 140 may be made of, for example, metal. The entire relay board 140 may be conductive. A part of the relay board 140 may be conductive. For example, the surface layer of the relay board 140 may be conductive. The relay board 140 is electrically connected to a first power source 151. The relay board 140 is also electrically connected to a second power source 152 (see FIGS. 3 and 4).

[0070] The relay plate 140 is spaced apart from the first roll 110 in a direction intersecting the vertical direction. The relay plate 140 may be spaced apart from the first roll 110 in the horizontal direction. The gap between the relay plate 140 and the first roll 110 may be, for example, 10 to 50 times the D50 of the granules 11. This gap indicates the shortest distance between the relay plate 140 and the first roll 110. The gap between the relay plate 140 and the first roll 110 may be, for example, 1 to 10 mm, or 2 to 6 mm.

[0071] The relay board 140 includes a third region R3 (see FIG. 4). The third region R3 is separated from the second region R2 in a direction intersecting the vertical direction. The third region R3 may be separated from the second region R2 in the horizontal direction.

[0072] The relay plate 140 may have any shape. The relay plate 140 may be, for example, flat or curved. In the relay plate 140, the surface that receives the granules 11 may be, for example, spherical or parabolic. For example, the cross section (FIGS. 3 and 4) parallel to the thickness direction of the relay plate 140 may be curved or bent vertically downward. In the first electrostatic coating, the granules 11 may arrive at the relay plate 140 from multiple directions. For example, by the relay plate 140 being curved, the position where the granules 11 adhere to the substrate 13 in the second electrostatic coating may be stabilized. This is expected to reduce, for example, uneven coating.

[0073] The relay plate 140 may also be referred to as, for example, an "opposing plate." The relay plate 140 includes a first opposing surface 141 and a second opposing surface 142 (see FIG. 4). The first opposing surface 141 faces the first roll 110. The first opposing surface 141 may extend along the vertical direction. The second opposing surface 142 faces the second roll 120 (substrate 13). The second opposing surface 142 may extend in a direction intersecting the vertical direction.

[0074] The second opposing surface 142 may be continuous with the first opposing surface 141. The second opposing surface 142 may be separated from the first opposing surface 141. The second opposing surface 142 may be integrated with the first opposing surface 141 and indistinguishable from it. For example, a part of the second opposing surface 142 may overlap with the first opposing surface 141. For example, the entire second opposing surface 142 may overlap with the first opposing surface 141. The second opposing surface 142 may be substantially the same as the first opposing surface 141. For example, when the relay plate 140 is flat, the second opposing surface 142 may be substantially the same as the first opposing surface 141.

[0075] <<Second Roll>> The second roll 120 is conductive. The second roll 120 may be made of, for example, a metal. The entire second roll 120 may be conductive. A part of the second roll 120 may be conductive. For example, a part in contact with the base material 13 may be conductive. For example, a surface layer of the second roll 120 may be conductive. The second roll is electrically connected to the second power source 152. The second roll 120 may be grounded.

[0076] In the vertical direction, the second roll 120 is located lower than the first roll 110 and the relay plate 140 (see FIG. 3). The second roll 120 may be disposed, for example, directly below the first roll 110. The second roll 120 may be disposed, for example, directly below the relay plate 140. The diameter of the second roll 120 may be larger than the diameter of the first roll 110, for example.

[0077] The gap between the second roll 120 and the relay plate 140 may be, for example, 20 to 100 times the D50 of the granules 11. This gap indicates the shortest distance between the second roll 120 and the relay plate 140. The gap between the second roll 120 and the relay plate 140 may be, for example, 2 to 20 mm, or 6 to 10 mm.

[0078] The second roll 120 may also be referred to as a "backup roll", for example. The second roll 120 supports the substrate 13. The substrate 13 is transported by the rotation of the second roll 120. The second roll 120 transports the substrate 13 into the second electric field E2. In the vertical direction, the substrate 13 is located lower than the third region R3 (see FIG. 4).

[0079] <Electrode manufacturing method> FIG. 5 is a schematic flow chart of the manufacturing method of an electrode in this embodiment. Hereinafter, "the manufacturing method of an electrode in this embodiment" is abbreviated as "the manufacturing method". The manufacturing method includes "(a) preparation of granules", "(b) supply", "(c) charging", "(d) roll transport", "(e) first electrostatic coating", and "(f) second electrostatic coating". The manufacturing method may further include "(g) fixing" after "(f) second electrostatic coating", for example. The manufacturing apparatus 100 described above may execute "(b) supply" to "(g) fixing", for example.

[0080] In this manufacturing method, for example, an electrode for a lithium ion battery can be manufactured. However, the lithium ion battery is only one example. This manufacturing method can be applied to any battery system. In this manufacturing method, at least one of a positive electrode and a negative electrode can be manufactured.

[0081] (a) Preparation of Granules This manufacturing method includes preparing granules 11 containing an active material powder and a binder. The granules 11 are, so to speak, precursors of the active material layer 12. The granules 11 can be prepared by granulating a powder. The granules 11 contain an active material powder and a binder. That is, the granules 11 can be prepared by granulating a mixed powder of the active material powder and the binder. The mixed powder can further contain an optional component (such as a conductive material). For example, the granules 11 can be prepared by dry granulation, or the granules 11 can be prepared by wet granulation. In this manufacturing method, any dry granulator or wet granulator can be used.

[0082] The granule 11 is an aggregate of composite particles. One composite particle contains one or more active material particles. One composite particle may contain two or more active material particles. One composite particle may contain an aggregate of active material particles.

[0083] The composite particles may have any shape, for example, pellets, spheres, flakes, columns, irregular shapes, etc.

[0084] Granule 11 may have a D50 of, for example, 50 to 500 μm. Granule 11 may have a D50 of, for example, 100 to 200 μm. When granule 11 has a D50 of 100 to 200 μm, for example, granule 11 is expected to exhibit suitable fluidity.

[0085] Granulation is expected to improve fluidity. The active material powder (before granulation) may have an angle of repose of, for example, more than 50°. Granules 11 (after granulation) may have an angle of repose of, for example, 50° or less. When granules 11 have an angle of repose of 50° or less, for example, coating unevenness is expected to be reduced. Granules 11 may have an angle of repose of, for example, 45° or less. Granules 11 may have an angle of repose of, for example, 30° or more.

[0086] <Active material powder> The active material powder includes active material particles. The active material powder is an aggregate of active material particles. The active material powder may have a D50 of, for example, 1 to 30 μm, may have a D50 of 1 to 20 μm, or may have a D50 of 1 to 10 μm.

[0087] The active material particles cause an electrode reaction. The active material particles may contain any component. The active material particles may contain, for example, a positive electrode active material. The active material particles may contain, for example, at least one selected from the group consisting of LiCoO2, LiNiO2, LiMnO2, LiMn2O4, Li(NiCoMn)O2, Li(NiCoAl)O2, and LiFePO4. For example, "(NiCoMn)" in "Li(NiCoMn)O2" indicates that the sum of the composition ratios in parentheses is 1. As long as the sum is 1, the amount of each component is arbitrary. Li(NiCoMn)O2 is, for example, Li(Ni 1 / 3 Co 1 / 3 Mn 1 / 3 )O2, Li(Ni 0.5 Co 0.2 Mn 0.3 )O2, Li(Ni 0.8 Co 0.1 Mn 0.1 ) O2, etc.

[0088] The active material particles may include, for example, a negative electrode active material, such as graphite, soft carbon, hard carbon, silicon, silicon oxide, a silicon-based alloy, tin, tin oxide, a tin-based alloy, and Li4Ti5O 12 may contain at least one selected from the group consisting of:

[0089] <Binder> The binder may be in powder form. The binder binds solid materials together in the active material layer 12. The amount of the binder may be, for example, 0.1 to 10 parts by mass with respect to 100 parts by mass of the active material powder. The binder may contain any component. The binder may contain at least one selected from the group consisting of, for example, polyvinylidene fluoride (PVdF), polytetrafluoroethylene (PTFE), vinylidene fluoride-hexafluoropropylene copolymer (PVdF-HFP), styrene butadiene rubber (SBR), carboxymethyl cellulose (CMC), polyimide (PI), polyamideimide (PAI), and polyacrylic acid (PAA).

[0090] <Optional ingredients> The granules 11 may further include, for example, a conductive material. The conductive material may be in powder form. The conductive material may form an electronic conduction path in the active material layer 12. The amount of the conductive material may be, for example, 0.1 to 10 parts by mass with respect to 100 parts by mass of the active material powder. The conductive material may include any component. The conductive material may include, for example, conductive carbon particles, conductive carbon fibers, etc. The conductive material may include, for example, at least one selected from the group consisting of carbon black, vapor-grown carbon fibers, carbon nanotubes, and graphene flakes. The carbon black may include, for example, at least one selected from the group consisting of acetylene black, furnace black, channel black, and thermal black.

[0091] The granules 11 may further contain, for example, a solvent. The solvent is liquid. The solvent may be dispersed in the granules 11 in the form of droplets. For example, the binder may absorb the solvent and swell. The solvent may contain any component. For example, the solvent may contain at least one selected from the group consisting of water, N-methyl-2-pyrrolidone (NMP), and butyl butyrate. The granules 11 may have, for example, a solid content rate of 70 to 100%, a solid content rate of 80 to 100%, or a solid content rate of 90 to 100%.

[0092] The granules 11 may further include, for example, a solid electrolyte. That is, in this manufacturing method, an electrode 10 for an all-solid-state battery may also be manufactured. The solid electrolyte may be in a powder form. The solid electrolyte may form an ion conduction path in the active material layer 12. The solid electrolyte may include any component. The solid electrolyte may include, for example, at least one selected from the group consisting of Li2S-P2S5, LiI-Li2S-P2S5, LiBr-Li2S-P2S5, and LiI-LiBr-Li2S-P2S5.

[0093] 《(b) Supply》 The manufacturing method includes feeding granules 11 onto a surface of a first roll 110 (see FIG. 3). For example, the granules 11 may be loaded into a hopper 160. A rotary feeder 161 may deliver the granules 11 to a first region R1, for example at a constant flow rate.

[0094] (c) Electric Charge This manufacturing method includes charging the granules 11. In Fig. 5, "(c) Charging" is illustrated between "(b) Supply" and "(d) Roll Conveyance" for convenience. However, "(c) Charging" may be performed at any timing between "(a) Preparation of Granules" and "(e) First Electrostatic Coating". For example, "(c) Charging" and "(d) Roll Conveyance" may be performed simultaneously.

[0095] For example, the first power source 151 may supply an electric charge (electrons) to the first roll 110. For example, the first roll 110 may inject an electric charge into the granules 11 (see FIG. 3). This may cause the granules 11 to become negatively charged.

[0096] (d) Roll transport The method includes conveying granules 11 from a first region R1 to a second region R2 by rotation of a first roll 110 (see FIG. 3). The second region R2 is vertically lower than the first region R1. The second region R2 is located within a first electric field E1 (see FIG. 4).

[0097] Before the granules 11 reach the first electric field E1 (second region R2), the granules 11 may be spread evenly on the surface of the first roll 110. For example, the granules 11 may be spread evenly in the gap between the first roll 110 and the third roll 130. This is expected to stabilize the amount of granules 11 supplied to the first electric field E1.

[0098] (e) First electrostatic coating The manufacturing method includes forming a first electric field E1 between the second region R2 and the third region R3, thereby causing the granules 11 to fly from the second region R2 toward the third region R3 (see FIG. 4).

[0099] For example, the first power source 151 may apply a DC voltage between the first roll 110 and the relay plate 140. This may form a first electric field E1 between the second region R2 and the third region R3. A first electrostatic force F1 may act on the granules 11 supplied to the second region R2. The first electrostatic force F1 may cause the granules 11 to detach from the first roll 110 and fly toward the relay plate 140.

[0100] (f) Second electrostatic coating This manufacturing method includes forming a second electric field E2 between the third region R3 and the substrate 13, thereby causing the granules 11 to fly from the third region R3 toward the substrate 13 (see FIG. 4). The granules 11 that arrive at the substrate 13 may adhere to the substrate 13. This allows the active material layer 12 to be formed. That is, the electrode 10 may be manufactured.

[0101] For example, the second power source 152 may apply a DC voltage between the relay plate 140 and the second roll 120. This may form a second electric field E2 between the third region R3 and the substrate 13. A second electrostatic force F2 may act on the granules 11 attached to the relay plate 140. Furthermore, gravity F3 may also act on the granules 11. Due to the combined force of the second electrostatic force F2 and gravity F3, the granules 11 may detach from the relay plate 140 and fly toward the substrate 13. It is expected that the combined force of the second electrostatic force F2 and gravity F3 will cause the granules 11 to firmly adhere to the substrate 13.

[0102] <Base material> The substrate 13 may be, for example, in the form of a sheet. The substrate 13 may be, for example, in the form of a strip. The substrate 13 is conductive. The substrate 13 may be a current collector. The substrate 13 may include, for example, a metal foil. The substrate 13 may include, for example, at least one selected from the group consisting of an aluminum (Al) foil, an Al alloy foil, a copper (Cu) foil, a Cu alloy foil, a nickel (Ni) foil, a Ni alloy foil, a titanium (Ti) foil, and a Ti alloy foil. The substrate 13 may have a thickness of, for example, 5 to 50 μm, or 5 to 20 μm.

[0103] <Field strength> The electrostatic force can be adjusted by the electric field strength. The first electric field E1 has a first electric field strength. The second electric field E2 has a second electric field strength. In the first electric field E1, a first electrostatic force F1 acts on the granules 11. In the second electric field E2, in addition to the second electrostatic force F2, a gravitational force F3 acts on the granules 11. Thus, for example, the second electric field strength may be lower than the first electric field strength.

[0104] The first electric field strength is obtained by dividing the DC voltage applied between the first roll 110 and the relay plate 140 by the gap (shortest distance) between the first roll 110 and the relay plate 140. If the first electric field strength is excessively low, the granules 11 may not fly. If the first electric field strength is excessively high, the impact of the granules 11 colliding with the relay plate 140 may be excessively large. The granules 11 may bounce off the relay plate 140 due to the reaction of the collision. The first electric field strength may be, for example, 75,000 to 300,000 V / m, or 100,000 to 200,000 V / m.

[0105] The second electric field strength is obtained by dividing the DC voltage applied between the relay plate 140 and the second roll 120 by the gap (shortest distance) between the relay plate 140 and the second roll 120. If the second electric field strength is excessively low, the granules 11 may not adhere to the substrate 13. If the second electric field strength is excessively high, the impact of the granules 11 colliding with the substrate 13 may be excessively large. The granules 11 may bounce off the substrate 13 due to the recoil of the collision. The second electric field strength may be, for example, 37500 to 150000 V / m or 50000 to 100000 V / m.

[0106] (g) Fixation The present production method may include applying at least one of pressure and heat to active material layer 12 to fix active material layer 12 to substrate 13. Fixing active material layer 12 is expected to improve the peel strength of active material layer 12, for example.

[0107] Pressure and heat may be applied separately. Pressure and heat may be applied substantially simultaneously. For example, the active material layer 12 may be compressed by a heat roll, a heat plate, or the like. The heating temperature of the active material layer 12 may be, for example, a temperature near the melting point of the binder. The softening, melting, and resolidification of the binder are expected to improve the fixing power. The heating temperature may be, for example, 80 to 200°C, 120 to 200°C, or 140 to 180°C.

[0108] The pressure can be adjusted according to, for example, the target thickness and the target density of active material layer 12. For example, a pressure of 50 to 200 MPa may be applied to active material layer 12.

[0109] "others" In this manner, the electrode 10 can be manufactured. When the active material layer 12 (granules 11) contains a solvent, the electrode 10 may be dried. The electrode may be cut into a predetermined planar shape in accordance with the battery design.

[0110] <Electrode> FIG. 6 is a conceptual diagram showing an example of an electrode. The electrode 10 may be a positive electrode or a negative electrode. The electrode 10 may have any outer shape according to the battery design. The electrode 10 may be, for example, strip-shaped. The electrode 10 includes a substrate 13 and an active material layer 12. The active material layer 12 is disposed on the surface of the substrate 13. The active material layer 12 may be disposed on only one surface of the substrate 13. The active material layer 12 may be disposed on both the front and back surfaces of the substrate 13.

[0111] The active material layer 12 may have any thickness. For example, the active material layer 12 may have a thickness of 10 to 500 μm, or may have a thickness of 50 to 200 μm. When the electrode 10 is a positive electrode, the active material layer 12 has a thickness of, for example, 2 to 4 g / cm 3 When the electrode 10 is a negative electrode, the active material layer 12 may have a density of, for example, 1 to 2 g / cm. 3 The density of active material layer 12 refers to the "apparent density." The apparent density is determined by dividing the mass of active material layer 12 by the apparent volume of active material layer 12. The apparent volume includes the void volume.

[0112] The active material layer 12 may contain, for example, by mass fraction, 1 to 10% of a binder, 0 to 10% of a conductive material, and the remainder being active material powder. The active material powder may contain a positive electrode active material or a negative electrode active material. EXAMPLES

[0113] <Electrode manufacturing> The present embodiment will be described below. In the first manufacturing example, a positive electrode was manufactured. In the second manufacturing example, a negative electrode was manufactured.

[0114] 《First manufacturing example》 The following materials were prepared: Active material powder: Li(NiCoMn)O2 Conductive material: Acetylene black Binder: PVdF Substrate 13: Aluminum foil (thickness 12 μm)

[0115] A mixing device, "High Speed ​​Mixer" manufactured by EarthTechnica, was prepared. The active material powder, conductive material, and binder were put into the mixing tank of the mixing device. The material mixing ratio was "active material powder / conductive material / binder = 90 / 5 / 5 (mass ratio)". The rotation speed of the stirring blade was set to 4500 rpm. The materials were mixed for one minute. In this way, a mixed powder was prepared. The mixed powder had an angle of repose of 59.6°.

[0116] A dry granulator was prepared. The mixed powder was granulated by the dry granulator. Thus, granules 11 were prepared. Each of the composite particles constituting granules 11 was formed into a flake shape. Granules 11 were sized using a 16-mesh wire screen. Granules 11 after sizing had a D50 of 100 to 200 μm. Granules 11 after sizing had an angle of repose of 42.1°.

[0117] The electrode manufacturing equipment shown in Figures 4 and 5 was prepared. The settings of each part were as follows: First electric field E1: First roll 110 (-1200V), relay plate 140 (-600V) Gap between the first roll 110 and the relay plate 140: 4 mm First electric field strength: 150000V / m

[0118] Second electric field E2: relay plate 140 (-600V), second roll 120 (0V, GND) Gap between relay plate 140 and second roll 120: 8 mm Second electric field strength: 75000V / m

[0119] Granules 11 were supplied from a hopper 160 to the surface of the first roll 110. The granules 11 were charged by receiving an electric charge from the first roll 110. The granules 11 were transported from the first region R1 to the second region R2 by the rotation of the first roll 110. The granules 11 were attached to the substrate 13 by flying successively through the first electric field E1 and the second electric field E2. In this way, an active material layer 12 was formed. That is, an electrode 10 was produced. The active material layer 12 had a planar size of 60 mm × 200 mm.

[0120] Electrode 10 was sandwiched between two heat plates (flat plates). The temperature of the heat plates was 160° C. A load of 15 tf was applied to active material layer 12 by the heat plates for 30 seconds. As a result, active material layer 12 was fixed to substrate 13.

[0121] 《Second manufacturing example》 The following materials were prepared: Active material powder: amorphous coated graphite Binder: PVdF Substrate 13: Cu foil (thickness 8 μm)

[0122] In the amorphous coated graphite, the surface of each graphite particle was coated with an amorphous carbon material. A mixing device "High Speed ​​Mixer" manufactured by EarthTechnica Corporation was prepared. An active material powder and a binder were put into the mixing tank of the mixing device. The material blend ratio was "active material powder / binder = 97.5 / 2.5 (mass ratio)". The rotation speed of the stirring blade was set to 4500 rpm. The materials were mixed for one minute. In this way, a mixed powder was prepared. The mixed powder had an angle of repose of 49.7°.

[0123] The mixed powder was granulated by a dry granulator. Thus, granules 11 were prepared. Each of the composite particles constituting granules 11 was formed into a flake shape. The granules 11 were sized using a 16-mesh wire screen. The granules 11 after sizing had a D50 of 100 to 200 μm. The granules 11 after sizing had an angle of repose of 44.3°. Except for these, the electrode 10 was manufactured in the same manner as in the first manufacturing example.

[0124] <Manufacturing results> FIG. 7 is a photograph showing the results of the first and second manufacturing examples. In both the first and second manufacturing examples, no coating unevenness was observed on the active material layer 12. In addition, in both the first and second manufacturing examples, the entire amount of the granules 11 added was used to form the active material layer 12. In other words, no substantial yield loss occurred.

[0125] The present embodiment and the present embodiment are illustrative in all respects. The present embodiment and the present embodiment are not restrictive. The technical scope of the present disclosure includes all modifications within the meaning and scope equivalent to the description of the claims. For example, it is also intended from the beginning that any configuration may be extracted from the present embodiment and the present embodiment, and that they may be arbitrarily combined. [Explanation of symbols]

[0126] 1 powder, 10 electrode, 11 granules, 12 active material layer, 13 substrate, 100 electrode manufacturing apparatus, 110 first roll, 120 second roll, 130 third roll, 140 relay plate, 141 first opposing surface, 142 second opposing surface, 150 electric field forming apparatus, 151 first power source, 152 second power source, 160 hopper, 161 rotary feeder, 211, 221 supply roll, 212, 222 backup roll, E1 first electric field, E2 second electric field, F1 first electrostatic force, F2 second electrostatic force, F3 gravity, R1 first region, R2 second region, R3 third region.

Claims

1. An electrode manufacturing apparatus for manufacturing an electrode by adhering granules containing an active material powder and a binder to a substrate, comprising: A first roll; A relay board, A second roll; An electric field forming device; Including, The relay plate is spaced from the first roll in a direction intersecting a vertical direction, In the vertical direction, the second roll is located lower than the first roll and the relay plate, the electric field forming device is configured to form a first electric field between the first roll and the relay plate, and to form a second electric field between the relay plate and the second roll; the first roll is configured to convey the granules into the first electric field; the second roll is configured to transport the substrate into the second electric field; Electrode manufacturing equipment.

2. Further comprising a third roll, Before the granules reach the first electric field, The granules are spread evenly in the gap between the first roll and the third roll. The electrode manufacturing apparatus according to claim 1 .

Citation Information

Patent Citations

  • Method of manufacturing electrode for electrochemical element, electrode for electrochemical element, and electrochemical element

    JP2011049231A

  • Powder coating device, and powder coating method