Optical fiber connection components and optical fiber connection structure
The optical fiber connection component with a glass plate and liquid crystal polymer resin ferrule addresses heat resistance and alignment issues, ensuring precise and low-loss connections to optical integrated circuits.
Patent Information
- Application Number
- JP2021555978
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-11-14
- Filing Date
- 2020-10-30
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2040-10-30
AI Technical Summary
Existing optical fiber connectors face challenges in heat resistance and high-definition arrangement, with materials like liquid crystal polymer being difficult to mold for high hole forming accuracy, and resin materials blocking UV adhesion for optical integrated circuits.
An optical fiber connection component comprising a glass plate with coaxial through holes and a resin ferrule made of liquid crystal polymer, which maintains high precision and heat resistance, allowing UV adhesion and reducing thermal deformation for precise optical fiber alignment.
The solution provides improved heat resistance and high-definition optical fiber arrangement with reduced thermal deformation, enabling low-loss connections and compatibility with UV-adhesive optical integrated circuits.
Smart Images

Figure 0007559766000004 
Figure 0007559766000005 
Figure 0007559766000006
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an optical fiber connecting component and an optical fiber connecting structure.
[0002] This application claims priority to Japanese Application No. 2019-206145, filed on November 14, 2019, and incorporates by reference all of the contents of said Japanese application. [Background technology]
[0003] Patent Document 1 discloses an optical connector including an optical fiber, a ferrule having a flat ferrule end face facing the mating optical connector and holding the optical fiber, and a spacer provided on the ferrule end face to define the distance between the ferrule end face and the mating optical connector. According to the optical connector of Patent Document 1, the spacer provides a gap between the optical connectors, making it easy to clean the ferrule end face, and even when multiple optical fibers are connected at the same time, no large force is required for connection, making alignment work easy.
[0004] Patent Document 2 discloses a multi-core optical connector having multiple optical fiber insertion holes, and suggests that, in addition to polyimide resins, liquid crystal polymers and polyphenylene sulfide (PPS) can be used as the resin material for forming the multi-core optical connector.
[0005] Patent Document 3 discloses an optical path changing element made of resin, which has a structure for bending and fixing a fiber while positioning the fiber. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] International Publication No. 2017 / 073408 [Patent Document 2] Japanese Patent Publication No. 2004-117616 [Patent Document 3] Japanese Patent Publication No. 2007-147859 Summary of the Invention [Means for solving the problem]
[0007] An optical fiber connection part according to one aspect of the present disclosure includes: a glass plate having a plurality of first through holes; a resin ferrule fixed to the glass plate and having a plurality of second through holes coaxial with each of the plurality of first through holes; A plurality of optical fibers including glass fibers and a coating resin covering the glass fibers; the glass fibers exposed from the tips of the optical fibers are held in the first through holes and the second through holes, The material constituting the resin ferrule has a flexural modulus of elasticity of 5 GPa or more at 200°C. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is an external perspective view showing an optical fiber connecting component according to the present disclosure. [Diagram 2] FIG. 2 is an exploded perspective view of the optical fiber connecting part of FIG. [Diagram 3] FIG. 3 is a diagram showing the surface of a multi-hole glass plate included in the optical fiber connecting part of FIG. [Figure 4] 4 is a cross-sectional view of the optical fiber connecting part of FIG. 1 taken along line IV-IV. [Diagram 5] FIG. 5 is a conceptual diagram for explaining a glass fiber disposed between a glass plate and a resin ferrule in the optical fiber connecting part of FIG. [Figure 6] FIG. 6 is a graph showing deformations caused by heat treatment of the resin ferrule according to the example and the resin ferrule according to the comparative example. [Figure 7] FIG. 7 is a graph showing deformation of a multi-hole glass plate when an optical fiber connecting component using a resin ferrule according to an embodiment is heat-treated. [Figure 8] FIG. 8 is a front view of an optical fiber connecting part according to a first modified example. [Figure 9] FIG. 9 is a diagram showing an optical fiber connecting part according to a second modified example. [Figure 10] FIG. 10 is a schematic cross-sectional view showing a glass plate body included in the optical fiber connecting part of FIG. [Figure 11] FIG. 11 is a diagram showing an optical fiber connecting part according to a third modified example. [Figure 12] FIG. 12 is a conceptual diagram showing an optical fiber connecting part according to a fourth modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] [Problem that this disclosure aims to solve] In the optical connector of Patent Document 1, the ferrule made of a resin material has a structure having a plurality of holes, which allows two-dimensional arrangement of optical fibers, but there is room for improvement in heat resistance.
[0010] Patent Document 2 suggests using a liquid crystal polymer with excellent heat resistance as an optical connector material. Compared to PPS, which is generally used in optical connectors, liquid crystal polymer has high molding anisotropy, so it is difficult to manufacture ferrules for optical connectors, which require high hole-forming accuracy, using only liquid crystal polymer.
[0011] In Patent Document 3, the optical path changing element is formed from a resin element body in the shape of a block with an L-shaped cross section. If the positioning structure at the tip of the fiber is made of a resin material, it cannot transmit ultraviolet light, and therefore it is not possible to bond and fix the optical path changing element to an optical integrated circuit (Silicon-Photonic Integrated Circuit: Si-PIC) formed on Si such as silicon photonics using a UV adhesive.
[0012] An object of the present disclosure is to provide an optical fiber connecting component and an optical fiber connecting structure that have improved heat resistance and enable highly precise arrangement of optical fibers.
[0013] [Effects of this disclosure] According to the present disclosure, it is possible to provide an optical fiber connecting component that has improved heat resistance and enables highly precise arrangement of optical fibers.
[0014] [Description of the embodiments of the present disclosure] An overview of an embodiment of the present disclosure will be described. The optical fiber connection component of the present disclosure comprises: (1) a glass plate having a plurality of first through holes; a resin ferrule fixed to the glass plate and having a plurality of second through holes coaxial with each of the plurality of first through holes; A plurality of optical fibers including glass fibers and a coating resin covering the glass fibers; the glass fibers exposed from the tips of the optical fibers are held in the first through holes and the second through holes, The material constituting the resin ferrule has a flexural modulus of 5 GPa or more at 200° C. Here, “coaxial” refers to a positional relationship in which the central axes of the objects coincide with each other.
[0015] According to the above configuration, the optical fiber connection part as a whole has heat resistance, and the first through hole can be formed in the glass plate with high precision, so that it is possible to realize high-precision positioning that enables connection of, for example, a single-mode optical fiber. In addition, the glass plate that fixes the glass fiber is transparent to ultraviolet light, so that it is possible to use a UV adhesive when connecting the optical fiber connection part to an optical integrated circuit such as a Si-PIC.
[0016] (2) An example of such a material is a liquid crystal polymer.
[0017] By using a liquid crystal polymer as the resin material constituting the resin ferrule, the bending modulus of elasticity of the resin ferrule can be made 5 GPa or more at 200°C.
[0018] (3) It is preferable that the thermal shrinkage rate of the material when heated from room temperature to a temperature of 200° C. or higher is 0.5% or less.
[0019] When the thermal deformation of the glass plate is large, the inclination of the optical fibers to be connected may change, which may cause optical loss. In contrast, according to the above configuration, since a resin ferrule with a small thermal shrinkage rate is used, it is possible to suppress the deformation of the glass plate caused by the deformation of the resin ferrule. As a result, when multiple optical fibers fixed to the optical fiber connecting part are connected to multiple optical fibers fixed to another optical fiber connecting part, it is possible to suppress the occurrence of optical loss caused by the inclination of the optical fibers to be connected.
[0020] (4) It is preferable that the variation (standard deviation) in the inclination of the optical fibers held in the first through holes and the second through holes is 0.5 degrees or less.
[0021] By keeping the variation in the inclination of the parallel optical fibers within the above range, it is possible to suppress the occurrence of directional misalignment between the optical axis of the glass fiber and the optical axis of the connected fiber, thereby achieving a low-loss connection to the connected fiber (e.g., a Si-PIC chip).
[0022] (5) It is preferable that the PV value (difference between the maximum and minimum values) of the surface of the glass plate when the glass plate is heat-treated at 200° C. or higher is 5 μm or less.
[0023] By controlling the thermal deformation of the glass plate within the above range, the occurrence of optical loss can be suppressed.
[0024] (6) The plurality of first through holes may be arranged two-dimensionally in one cross section of the glass plate.
[0025] According to the above configuration, more optical fibers can be mounted than in the case where a conventional V-groove substrate is used, and the fiber mounting density is improved.
[0026] (7) It is preferable that the glass fiber protrudes from the end face of the glass plate by 50 nm to 1 μm.
[0027] According to the above configuration, the glass fiber can be connected to a counterpart fiber via PC (Physical Contact) connection.
[0028] (8) The glass plate has a first guide hole, The resin ferrule may have a second guide hole that is coaxial with the first guide hole.
[0029] According to the above configuration, by using the first guide hole and the second guide hole, it is easy to position the first through hole of the glass plate and the second through hole of the resin ferrule.
[0030] (9) The outer diameter of the glass fiber is preferably 100 μm or less.
[0031] According to the above-mentioned configuration, it is possible to reduce the distortion when the optical fiber is bent and fixed in the resin ferrule. This makes it possible to provide an optical fiber connection component that is small in overall height and space-saving. In addition, it is possible to suppress the tensile distortion and compressive distortion when the glass fiber is bent, which contributes to preventing breakage of the glass fiber.
[0032] (10) Each of the plurality of optical fibers may be a multi-core optical fiber having a plurality of cores and a cladding covering the plurality of cores as the glass fiber.
[0033] According to the above configuration, an optical fiber connecting component having a high core density can be realized.
[0034] The optical fiber connection structure of the present disclosure includes: (11) An optical fiber connection structure in which a first optical fiber connection part, which is the optical fiber connection part according to any one of items (1) to (10), is connected to a second optical fiber connection part in which a plurality of optical fibers are fixed so as to match the arrangement of the plurality of optical fibers in the first optical fiber connection part, a first end face of the first optical fiber connecting part and a second end face of the second optical fiber connecting part are surfaces inclined with respect to optical axes of the optical fibers, A gap of 30 μm or less is formed between the first end face and the second end face.
[0035] According to the above-mentioned configuration, good optical connection is possible, and additional processing for making the glass fiber protrude from the end face of the glass plate is not required.
[0036] (12) The second optical fiber connection part is an optical fiber connection part according to any one of items (1) to (10), At least one of the first optical fiber connecting part and the second optical fiber connecting part may have a spacer configured to form the gap on an end surface of the glass plate.
[0037] (13) The second optical fiber connection component is configured by mounting the optical fibers in a resin ferrule, The second optical fiber connecting component may have an end face provided with a spacer configured to form the gap.
[0038] (14) The second optical fiber connection part is an optical fiber connection part according to any one of items (1) to (10), or a part configured by mounting the plurality of optical fibers on a resin ferrule, The adapter of the optical fiber connection structure may include a spacer configured to form the gap.
[0039] The spacer for providing a gap between the first end surface and the second end surface is preferably provided in the configuration of any one of the above items (12) to (14).
[0040] [Details of the embodiment of the present disclosure] Hereinafter, an embodiment of the present disclosure will be described with reference to the drawings. For convenience of explanation, the description of the members having the same reference numbers as those already described in the description of the present embodiment will be omitted. For convenience of explanation, the dimensions of each member shown in the drawings may differ from the actual dimensions of each member.
[0041] In addition, in the description of this embodiment, in order to facilitate understanding of this embodiment, the X-axis, Y-axis, and Z-axis that are perpendicular to each other will be mentioned as appropriate. Note that these directions are relative directions set in the optical fiber connecting part 1 shown in Fig. 1. Therefore, the X-axis, Y-axis, and Z-axis also rotate as the optical fiber connecting part 1 rotates.
[0042] First embodiment An optical fiber connecting part 1 according to the first embodiment will be described below with reference to Figs. 1 to 5. Fig. 1 is an external perspective view showing the optical fiber connecting part 1. Fig. 2 is an exploded perspective view of the optical fiber connecting part 1 of Fig. 1. Fig. 3 is a view showing a surface of a glass plate included in the optical fiber connecting part 1 of Fig. 1. Fig. 4 is a cross-sectional view of the optical fiber connecting part 1 of Fig. 1 taken along line IV-IV. Fig. 5 is a conceptual diagram for explaining a glass fiber arranged between a glass plate and a resin ferrule in the optical fiber connecting part 1 of Fig. 1 in relation to Fig. 4. The optical fiber connecting part 1 is used to optically connect an electronic board including an optical integrated circuit chip or the like to an on-premises wiring (or an external transmission line).
[0043] 1, the optical fiber connecting part 1 has an optical fiber 10 and an optical fiber 10a arranged next to the optical fiber 10. Each of the optical fibers 10, 10a has, for example, a bent portion (bent portion 13) in the middle, and one end of the optical fiber 10, 10a is fixed to an electronic board via a fiber fixing part 20, and the other end of the optical fiber 10, 10a is connected to the on-premises wiring via a connector (not shown).
[0044] As shown in Fig. 2, the optical fiber 10, 10a has a plurality of glass fibers 11 arranged along the Y direction shown in the figure. The glass fiber 11 has a core made of silica-based glass and a cladding covering the core. The outer diameter of the glass fiber 11 is, for example, 100 µm or less. The optical fiber 10, 10a may be a single-core optical fiber including a glass fiber having a single core and a cladding covering the single core, or may be a multi-core optical fiber including a glass fiber having multiple cores and a cladding covering the multiple cores collectively.
[0045] An individual coating resin layer 12 is applied to the outside of the glass fiber 11. In addition, behind the bent portion 13 of the glass fiber 11 (in the positive direction of X in the figure), the periphery of the individual coating resin layer 12 is covered with a collective coating resin layer . In addition, the glass fiber 11 is preferably a low bending loss fiber so that it can accommodate flexible bending shapes. To obtain a low bending loss fiber, a fiber having a high refractive index core structure or a refractive index structure called a trench structure that strengthens the confinement of light in the core is preferably used. The composition of the glass fiber 11 can be created by adding a dopant to appropriately control the refractive index using SiO2 glass. The core may be made of, for example, SiO2 glass doped with GeO2, or SiO2 glass co-doped with GeO2 and F. The cladding may be made of pure SiO2 glass or SiO2 glass doped with fluorine. This makes it possible to obtain an optical fiber that is economical and has good shape controllability.
[0046] In order to increase the strength of the optical fiber, a method of carbon-coating the outer periphery of the glass fiber 11 and a method of applying compressive strain to the outer periphery of the glass fiber 11 by adjusting the thermal history during drawing can be suitably combined. The bent optical fiber 10, 10a shown in Fig. 1 may be heated and bent in advance. In this case, the glass fiber 11 at the bent portion 13 is exposed before heating. As a heating means, a burner, a CO2 laser, an arc discharge, a heater, etc. can be used.
[0047] The CO2 laser has advantageous characteristics for precise control of curvature distribution, since the irradiation intensity, irradiation range, and irradiation time can be easily adjusted. At around 10 μm, which is the typical wavelength of the CO2 laser, glass is opaque, so it is thought that the irradiation energy of the CO2 laser is absorbed by the surface layer of the glass fiber 11 and is transmitted by re-radiation and thermal conduction. If the power of the CO2 laser is too high, the surface temperature of the glass fiber 11 will rise sharply to a temperature at which the glass evaporates, and the shape will no longer be able to be maintained. For this reason, the irradiation power of the CO2 laser should be set so that the glass on the surface of the glass fiber 11 does not evaporate and the cross section of the heated glass fiber 11 remains in contact with the working point (10 4 The cooling rate of the glass fiber 11 when bent by a CO2 laser is adjusted appropriately so that the temperature can be increased to 10 4 It is desirable to cool it slowly at a rate of 0.1 °C / s or less to remove distortion.
[0048] The fiber fixing component 20 is composed of a multi-hole glass plate 21 (an example of a glass plate) and a multi-hole resin ferrule 31 (an example of a resin ferrule). As shown in Fig. 2, the multi-hole glass plate 21 has a glass plate body 22 having, for example, a rectangular parallelepiped shape. The glass plate body 22 is transparent to ultraviolet light. A rectangular front surface 23 of the glass plate body 22 is disposed opposite a rear surface 34 of the multi-hole resin ferrule 31. A rectangular rear surface 24 of the glass plate body 22 is disposed opposite an electronic board.
[0049] The thickness between the front surface 23 and the back surface 24 of the glass plate body 22 (the length in the illustrated Z direction) is thin, for example, about 1 mm, and the glass plate body 22 has a plurality of first through holes 25 penetrating the front surface 23 and the back surface 24. As shown in Fig. 3, the plurality of first through holes 25 are arranged two-dimensionally, for example, along the width direction (the illustrated Y direction) and length direction (the illustrated X direction) of the glass plate body 22. In the first through holes 25, the glass fibers 11 are held.
[0050] The first through-hole 25 can be formed by, for example, a process combining photolithography and dry etching such as reactive ion etching (RIE) or a hole-making technique using a laser. For example, the positional accuracy of the first through-hole 25 is desirably ±1 μm or less. Note that the above-mentioned technique is not limited to the above-mentioned technique as long as the position of the first through-hole 25 has an error of 1 μm or less from a predetermined design position and the inner diameter of the first through-hole 25 can be ±1 μm or less from a predetermined diameter. In this example, an example in which the glass plate body 22 has a plurality of first through-holes 25 has been described, but the number of first through-holes may be one.
[0051] The glass plate body 22 has guide holes 26 near both ends as viewed in the Y direction in the drawing. As indicated by dashed lines in Fig. 2, the multiple-hole resin ferrule 31 has guide holes 37 at positions corresponding to the guide holes 26 of the glass plate body 22. By inserting the guide pins 45 through the guide holes 26 of the glass plate body 22 and the guide holes 37 of the multiple-hole resin ferrule 31, respectively, the first through hole 25 and the second through hole 38 of the multiple-hole resin ferrule 31, which will be described in Fig. 4, can be easily aligned in a coaxial relationship.
[0052] The guide pins 45 may be pulled out from the multiple-hole glass plate 21 and the multiple-hole resin ferrule 31 after the multiple-hole glass plate 21 and the multiple-hole resin ferrule 31 are fixed together. If the guide pins 45 are left in place rather than pulled out, the multiple-hole glass plate 21 may be damaged if there is a large difference between the thermal expansion coefficient of the multiple-hole glass plate 21 and the thermal expansion coefficient of the multiple-hole resin ferrule 31.
[0053] As shown in Fig. 1, the multiple-hole resin ferrule 31 has a ferrule body 32 that is substantially L-shaped in side view, and is placed on the multiple-hole glass plate 21. As shown in Fig. 2, the ferrule body 32 has a front surface 33 on which the optical fiber 10a can be placed, and a back surface 34 that is disposed opposite the front surface 23 of the glass plate body 22 at one end side of the front surface 33. A front wall surface 35 that faces the bent portion 13 of the optical fibers 10, 10a is provided at one end of the front surface 33 of the ferrule body 32. In addition, the ferrule body 32 has side wall surfaces 36 on the sides of the front surface 33 that face the side ends of the optical fibers 10, 10a, respectively.
[0054] 4, the thickness from the front surface 33 to the back surface 34 of the ferrule body 32 (the length in the illustrated Z direction) is greater than the thickness (1 mm) from the front surface 23 to the back surface 24 of the glass plate body 22. The ferrule body 32 has a plurality of second through holes 38 penetrating the front surface 33 and the back surface 34. The second through holes 38, like the first through holes 25, are two-dimensionally arranged along the width direction (the illustrated Y direction) and length direction (the illustrated X direction) of the ferrule body 32. In each of the second through holes 38, like each of the first through holes 25, a glass fiber 11 is held.
[0055] The second through hole 38 has a fiber holding hole 39 in which the individual coating resin layer 12 of the optical fiber can be loosely fitted, near the surface 33 of the ferrule body 32. The outer diameters of the first through hole 25 and the second through hole 38 are larger than the outer diameter of the glass fiber 11 exposed from the tip of the optical fiber.
[0056] In this embodiment, an example of a multi-hole resin ferrule 31 having a substantially L-shaped ferrule body 32 has been described, but various shapes can be adopted for the portion other than the back surface 34 disposed opposite the front surface 23 of the glass plate body 22. The multi-hole resin ferrule is not limited to a shape applicable to a bent optical fiber shown in Fig. 1, for example, and may have a shape applicable to a straight, unbent optical fiber.
[0057] As shown in Fig. 4, the ferrule body 32 has a protrusion 40 protruding toward the glass plate body 22 at the outer periphery of the back surface 34. The protrusion 40 is fixed in contact with the front surface 23 of the multiple-hole glass plate 21, so that the opening of the first through hole 25 located on the front surface 23 of the multiple-hole glass plate 21 and the opening of the second through hole 38 located on the back surface 34 of the multiple-hole resin ferrule 31 are separated by a predetermined distance (indicated by H in Fig. 4). For example, an air layer 42 exists in the area around the glass fiber 11 located between the front surface 23 of the multiple-hole glass plate 21 and the back surface 34 of the multiple-hole resin ferrule 31 and between adjacent glass fibers 11, except for the area around the glass fiber 11. The area between adjacent glass fibers 11, except for the area around the glass fiber 11, may be filled with a resin having a Young's modulus of 100 MPa or less.
[0058] However, if the front surface of the multi-hole glass plate and the back surface of the multi-hole resin ferrule are brought into contact with no gaps, the difference in thermal expansion coefficient between the multi-hole glass plate and the multi-hole resin ferrule may cause shear forces to be applied to the glass fiber as the temperature changes, resulting in the glass fiber breaking. In contrast, in this embodiment, the front surface 23 of the multi-hole glass plate 21 and the back surface 34 of the multi-hole resin ferrule 31 are spaced apart by a predetermined distance H, so that the glass fiber 11 has a margin for bending. Therefore, as shown in FIG. 5, even if the positions of the first through hole 25 of the multi-hole glass plate 21 and the second through hole 38 of the multi-hole resin ferrule 31 corresponding to the first through hole 25 are misaligned due to temperature changes, shear force is unlikely to be applied to the glass fiber 11. Therefore, breakage of the glass fiber 11 between the first through hole 25 and the second through hole 38 can be prevented. In addition, since the outer diameters of the first through hole 25 and the second through hole 38 are larger than the outer diameter of the glass fiber 11, contact between the first through hole 25 and the second through hole 38 and the glass fiber 11 can be easily avoided even if there is a temperature change in the range of -40°C to 85°C at which the optical fiber connecting part 1 is normally used, which also contributes to preventing breakage of the glass fiber 11.
[0059] The first through hole 25 provided in the glass plate body 22 has a straight portion 25a for holding the glass fiber 11 and a tapered portion 25b whose diameter increases toward the front surface 23 of the glass plate body 22. Similarly, the second through hole 38 provided in the ferrule body 32 has a straight portion 38a for holding the glass fiber 11 and a tapered portion 38b whose diameter increases toward the back surface 34 of the ferrule body 32. By providing the tapered portions 25b and 38b in this manner, as shown in FIG. 5, the distance between the opening of the first through hole 25 and the opening of the second through hole 38 becomes larger by the tapered portions 25b and 38b than the distance H from the front surface 23 of the glass plate body 22 to the back surface 34 of the ferrule body 32. Therefore, the shear force applied to the glass fiber 11 can be further reduced.
[0060] For example, a liquid crystal polymer is preferably used as the resin material constituting the multi-hole resin ferrule 31. Examples of the liquid crystal polymer include the following. (1) A polycondensate of ethylene terephthalate and parahydroxybenzoic acid, [ka] (2) Polycondensates of phenol and phthalic acid (e.g., 4,4-dihydroxybiphenol and terephthalic acid) with parahydroxybenzoic acid, [ka] (3) Polyarylates, for example polycondensates of 2,6-hydroxynaphthoic acid and parahydroxybenzoic acid; [ka] In order to improve the anisotropy and low weld strength of the liquid crystal polymer, it is desirable to knead an inorganic filler into the polymer. As the inorganic filler, a spherical or fibrous glass filler can be preferably used.
[0061] Since the liquid crystal polymer has a glass transition point of 90° C. or higher, it does not denature in the temperature range of −40° C. to +85° C. where the optical fiber connecting part 1 is normally used, and has high durability against humidity. In addition, by using the above-mentioned liquid crystal polymer as the resin material of the multiple-hole resin ferrule 31, the bending elastic modulus of the multiple-hole resin ferrule 31 can achieve 5 GPa or more at 200° C., and more preferably 5 GPa or more at 260° C.
[0062] Liquid crystal polymer has good fluidity and is relatively easy to mold. The multi-hole resin ferrule 31 using liquid crystal polymer can be molded into various shapes, so it can easily meet the requirements for the optical fiber connection part 1, such as changing the optical path direction and reducing the height of the optical fiber connection part 1.
[0063] Fig. 6 is a graph showing deformation of a multi-hole resin ferrule according to an embodiment made of liquid crystal polymer (LCP) and a multi-hole resin ferrule according to a comparative example made of a conventional material, polyphenylene sulfide (PPS), when each is heat treated for 5 minutes at 260°C. Fig. 6 shows a graph of the unevenness of the end faces of the resin ferrules according to the embodiment and the comparative example.
[0064] As shown in Figure 6, in the comparative example using PPS, the unevenness of the end face of the multiple-hole resin ferrule was 12 μm or more in terms of PV (Peak-Valley) value. PPS, which is an existing resin ferrule material, has a glass transition point of around 90°C, so it undergoes large deformation after heat treatment. If a multiple-hole glass plate is attached to such a resin material that is subject to large thermal deformation and then heat treatment is performed, the multiple-hole glass plate after heat treatment will also be subject to large deformation.
[0065] On the other hand, in the embodiment using the liquid crystal polymer, the unevenness of the end face of the multi-hole resin ferrule was 5 μm or less in terms of PV value. It was confirmed that by using the liquid crystal polymer with excellent heat resistance as the resin ferrule material, the thermal deformation can be significantly suppressed compared to PPS even when heat treatment is performed at 260°C, which is a general reflow temperature. Specifically, by using the liquid crystal polymer, it is possible to suppress the thermal shrinkage rate of the multi-hole resin ferrule to 0.5% or less when heated from room temperature (for example, 20°C) to a temperature of 200°C or higher, preferably from room temperature to a temperature of 260°C or higher.
[0066] Fig. 7 is a graph showing the deformation of the multi-hole glass plate when an optical fiber connection part including a multi-hole resin ferrule using a liquid crystal polymer according to the embodiment and a multi-hole glass plate is heat-treated for 5 minutes at 260° C. As shown in Fig. 7, the unevenness of the end face of the multi-hole glass plate after heat treatment is about 0.5 μm in PV value, and a deformation amount of 5 μm in PV value, which is sufficiently permissible to ensure the positional accuracy of the fiber, and preferably 1 μm in PV value, was achieved.
[0067] As described above, the optical fiber connection part 1 according to the present embodiment includes the multi-hole glass plate 21 having a plurality of first through holes 25, the multi-hole resin ferrule 31 fixed to the multi-hole glass plate 21 and having a plurality of second through holes 38 coaxial with each of the first through holes 25, and a plurality of optical fibers 10, 10a including the glass fiber 11 held in the first through hole 25 and the second through hole 38. The multi-hole resin ferrule 31 is made of a resin material having a bending modulus of 5 GPa or more at 200°C. In order to realize a bending modulus of 5 GPa or more at 200°C, a liquid crystal polymer is used as the resin material constituting the multi-hole resin ferrule 31. This can improve the heat resistance of the optical fiber connection part 1 as a whole. In addition, the use of the multi-hole resin ferrule 31 capable of having a flexible shape makes it possible to protect the optical fibers 10, 10a and fix the bending shape.
[0068] Furthermore, since the positioning structure for the optical integrated circuit is formed by the multi-hole glass plate 21, the position and diameter of the long through-holes can be formed with high precision. Therefore, the first through-holes 25 can be arranged two-dimensionally in the multi-hole glass plate 21, and an optical fiber connecting component 1 with high channel density can be obtained. Specifically, when the area of the multi-hole glass plate 21 is S and the number of mounted fibers is n, n / S is 10 / mm 2 It is possible to obtain an optical fiber connecting component 1 with a high channel density exceeding 1000 sq.m. In addition, as described above, since the multi-hole glass plate 21 is transparent to ultraviolet light, the multi-hole glass plate 21 can be fixed to an electronic substrate, for example, an optical integrated circuit such as a Si-PIC, by using a UV adhesive.
[0069] However, if the thermal deformation of the multi-hole glass plate is large, optical loss may occur in the connection between the glass fiber and the silicon photonics chip (SiPH chip) in the optical fiber connection part. The deformation of the multi-hole glass plate is a significant problem, especially when realizing optical fiber connection parts with 100 or more channels, which requires the size of the multi-hole glass plate to be large. However, the thermal deformation of the multi-hole glass plate is not caused by the glass plate itself, but is mainly caused by the thermal deformation of the multi-hole resin ferrule. In contrast, the optical fiber connection part 1 according to the present embodiment uses a multiple-hole resin ferrule 31 made of a liquid crystal polymer, which is a resin material whose thermal shrinkage is 0.5% or less when heated from room temperature to 200°C or higher, preferably from room temperature to 260°C or higher. Therefore, compared with the existing multiple-hole resin ferrule using PPS, thermal deformation can be significantly suppressed. By suppressing the thermal deformation of the multiple-hole resin ferrule 31, the deformation amount of the multiple-hole glass plate 21 after heat treatment is also suppressed to 5 μm or less in PV value, preferably 1 μm or less. Therefore, the directional deviation between the optical axis of the glass fiber 11 and the optical axis of the connected fiber, i.e., the coupling angle difference between the channels, can be maintained at a substantially negligible level.
[0070] According to this embodiment, the deformation amount of the multi-hole glass plate 21 after the heat treatment is small, so that the variation in the inclination (angle variation) of the glass fiber 11 fixed to the multi-hole glass plate 21 is 0.5 degrees or less. This reduces the difference in the coupling angle between the glass fiber 11 and the SiPh chip, and suppresses the occurrence of optical loss. This prevents the decrease in the coupling efficiency between the grating coupler, which is generally used as a surface coupling method for the SiPh chip, and the optical fiber 10, 10a.
[0071] In this embodiment, the optical fiber 10, 10a may be a multi-core optical fiber having a glass fiber 11 having multiple cores and a cladding covering the multiple cores. By applying the multi-core optical fiber, it is possible to cope with a configuration requiring high-density light input / output of more than 100 channels from one Si-PIC, for example.
[0072] (First Modification) FIG. 8 is a front view of an optical fiber connecting part 1A according to a first modification. As in the optical fiber connecting part 1A shown in FIG. 8, the glass fiber 11 held in the first through hole 25 of the multi-hole glass plate 21 may protrude from the back surface 24 of the multi-hole glass plate 21. In this case, the protruding amount of the glass fiber 11 from the back surface 24 of the multi-hole glass plate 21 is, for example, about 50 nm to 1 μm. In this way, the glass fiber 11 protrudes from the back surface 24 of the multi-hole glass plate 21, so that the end face of the glass fiber 11 can be connected to the glass fiber protruding from the optical connector of the connection partner side by PC (Physical Contact). However, since the multi-hole glass plate 21 used in this embodiment has a composition substantially the same as that of the glass fiber 11, it is difficult to make the glass fiber 11 protrude from the multi-hole glass plate 21 in a normal polishing process used in a conventional resin ferrule. Therefore, in order to make the glass fiber 11 protrude, additional processing such as laser processing or etching processing of the back surface 24 of the multi-hole glass plate 21 is required.
[0073] (Second Modification) In the above first embodiment, an example has been described in which the first through holes 25 extend in a direction perpendicular to the rear surface 24 (and the front surface 23) of the glass plate body 22 (the Z direction in the figure), but the present invention is not limited to this example. Fig. 9 is a conceptual diagram showing an optical fiber connecting part according to a second modified example. Fig. 9 shows an optical fiber connecting part 1B and an optical fiber connecting part 1C which is a connecting partner of the optical fiber connecting part 1B. For the purpose of explanation, Fig. 9 shows a cross-sectional view of only glass plate bodies 22B and 22C and a portion of the glass fiber 11 held by the glass plate bodies 22B and 22C.
[0074] In the optical fiber connecting part 1B shown in FIG. 9, the back surface 24B (an example of a first end surface) of the multi-hole glass plate 21B is an inclined surface that is not perpendicular to the optical axis of the glass fiber 11. Specifically, it is preferable that the angle θ between the optical axis of the glass fiber 11 and the back surface 24B of the multi-hole glass plate 21B is 75 degrees or more and 85 degrees or less. For example, as shown in FIG. 10, the multi-hole glass plate 21B has the straight portion 25a of the first through hole 25 inclined at a certain angle with respect to a line perpendicular to the back surface 24B of the glass plate main body 22B. Specifically, it is preferable that the angle φ between the line perpendicular to the back surface 24B of the glass plate main body 22B and the straight portion 25a of the first through hole 25 is 8 degrees.
[0075] Similar to the optical fiber connecting part 1B, a back surface 24C (an example of a second end surface) of a multi-hole glass plate 21C provided in the connecting counterpart optical fiber connecting part 1C is an inclined surface that is not perpendicular to the optical axis of the glass fiber 11. The optical fiber connecting part 1C is a part having the same configuration as the optical fiber connecting part 1B, and both optical fiber connecting parts 1B and 1C are fixed to each other in a state in which the back surface 24B of the multi-hole glass plate 21B of the optical fiber connecting part 1B and the back surface 24C of the multi-hole glass plate 21C of the optical fiber connecting part 1C are parallel to each other.
[0076] In addition, in order to provide a gap between the back surface 24B of the optical fiber connecting part 1B and the back surface 24C of the optical fiber connecting part 1C, as shown in FIG. 9, the back surface 24B of one of the optical fiber connecting parts 1B, 1C, has a spacer 50. When the optical fiber connecting part 1B and the optical fiber connecting part 1C are fixed, the gap formed between the end face of the glass fiber 11 of the optical fiber connecting part 1B and the end face of the glass fiber 11 of the optical fiber connecting part 1C is determined by the film thickness of the spacer 50. The film thickness of the spacer 50 is, for example, 30 μm or less, preferably 20 μm or less. In this way, the glass fiber 11 of the optical fiber connecting part 1B and the glass fiber 11 of the optical fiber connecting part 1C are arranged opposite each other through the gap formed between the optical fiber connecting parts 1B and 1C, so that the glass fibers 11 are optically connected to each other.
[0077] Like the glass plate body 22B of the multiple-hole glass plate 21B, the spacer 50 is preferably heat resistant. Therefore, the spacer 50 can be formed by, for example, fusing a thin film made of liquid crystal polymer or Teflon (registered trademark) onto the glass plate body 22B. Alternatively, the spacer 50 can be formed by selectively etching a portion of the multiple-hole glass plate 21B including the glass fiber 11 to make it partially concave.
[0078] As described above, the optical fiber connecting parts 1B, 1C according to the second modification are configured such that the rear surfaces 24B, 24C of the multi-hole glass plates 21B, 21C are inclined surfaces that are not perpendicular to the optical axis of the glass fiber 11, and the rear surface 24B of the optical fiber connecting part 1B and the rear surface 24C of the optical fiber connecting part 1C are close to each other with a gap of 30 μm or less between them. This allows the glass fibers 11 to be optically connected to each other without PC connection, and allows low-loss connection while suppressing Fresnel reflection loss. Note that the inclination angle of the rear surfaces 24B, 24C of the glass plate bodies 22B, 22C varies depending on the type of optical fiber used, but when a general single-mode optical fiber is used, θ=82°, and the distance of the gap between the optical fiber connecting parts 1B, 1C, i.e., the height of the spacer 50, is 20 μm, the insertion loss of the optical fiber is 0.5 dB or less, and the reflection loss is 40 dB or more (reflectance 0.0001 or less).
[0079] (Third Modification) In the second modification shown in Fig. 9, an example was described in which a spacer 50 is provided on the glass plate body 22B of one of the optical fiber connecting parts 1B, 1C, which is composed of a multi-hole glass plate and a multi-hole resin ferrule, but this is not limited to the example. Fig. 11 is a conceptual diagram showing an optical fiber connecting part according to a third modification. Fig. 11 shows an optical fiber connecting part 1D and an optical connector 100, which is a connecting partner of the optical fiber connecting part 1D.
[0080] As in the optical fiber connecting parts 1B and 1C of the second modification, the rear surface 24D of the multi-hole glass plate 21D (glass plate body 22D) of the optical fiber connecting part 1D of the third modification is an inclined surface that is not perpendicular to the optical axis of the glass fiber 11. An optical connector 100 using an existing resin ferrule 102 is used as a connection partner of the optical fiber connecting part 1D. Specifically, the optical connector 100 is configured by fixing an optical fiber with a resin ferrule 102 made of, for example, PPS. The tip of the glass fiber 11 protrudes from the end face of the resin ferrule 102 by about 5 μm to 10 μm. The end face 104 of the resin ferrule 102 has a spacer 106. In this way, by providing the spacer 106 on the end face 104 of the resin ferrule 102 of the optical connector 100, which is the connection partner of the optical fiber connecting part 1D, additional processing is not required for the optical fiber connecting part 1D configured of the multi-hole glass plate 21D and the multi-hole resin ferrule 31 made of liquid crystal polymer. With this configuration, a gap can be provided between the end face of the glass fiber 11 of the optical fiber connection part 1D and the end face of the glass fiber of the optical connector 100, allowing the glass fibers to be brought into close proximity to each other, thereby achieving the same effect as the second modified example.
[0081] (Fourth Modification) Fig. 12 is a conceptual diagram showing an optical fiber connecting part according to a fourth modified example. Fig. 12 shows an optical fiber connecting part 1E, an optical fiber connecting part 1F which is a connecting partner of the optical fiber connecting part 1E, and an adapter 60 which holds the optical fiber connecting parts 1E and 1F in a connected state.
[0082] As with the optical fiber connecting parts 1B and 1C of the second modification, the rear surfaces 24E and 24F of the multi-hole glass plates 21E and 21F of the optical fiber connecting parts 1E and 1F of the fourth modification are inclined surfaces that are not perpendicular to the optical axis of the glass fiber 11. The adapter 60 that holds the optical fiber connecting parts 1E and 1F has an opening 61 through which the optical fiber connecting parts 1E and the optical fiber connecting parts 1F are inserted from both sides, and the inside of the opening 61 has a spacer 62 that protrudes inward at the center. In this way, by providing the spacer 62 in the adapter 60 that holds the optical fiber connecting parts 1E and 1F, additional processing of the optical fiber connecting parts 1E and 1F is not required. Even with this configuration, a gap can be provided between the end face of the glass fiber 11 of the optical fiber connecting part 1E and the end face of the glass fiber 11 of the optical fiber connecting part 1F of the connecting partner, so that the glass fibers 11 can be brought close to each other, and the same effect as the second modification can be achieved.
[0083] Although the embodiment of the present disclosure has been described above, it goes without saying that the technical scope of the present invention should not be interpreted as being limited by the description of the present embodiment. This embodiment is merely an example, and it will be understood by those skilled in the art that various modifications of the embodiment are possible within the scope of the invention described in the claims. Thus, the technical scope of the present invention should be determined based on the scope of the invention described in the claims and its equivalents. For example, the material constituting the resin ferrule does not have to be a liquid crystal polymer, but may have the physical property values described in the claims. [Explanation of symbols]
[0084] 1,1A,1B,1C,1D,1E,1F Optical fiber connection parts 10,10a optical fiber 11 Glass Fiber 12 Individually coated resin layer 13 Bend 14 Bulk coating resin layer 20 Fiber Fixing Parts 21, 21B, 21C, 21D, 21E, 21F Multi-hole glass plate (example of glass plate) 22, 22B, 22C, 22D Glass plate body 23,33 surface 24,24B,24C,24D,24E,24F,34 Back side 25 First through hole 25a, 38a straight section 25b, 38b Tapered section 26,37 Guide hole 31 Multi-hole resin ferrule (an example of the resin ferrule 102) 32 Ferrule body 35 (Ferrule body 32) front wall surface 36 (of the ferrule body 32) side wall surface 38 Second through hole 39 Fiber holding hole 40 Protrusion 42 Air Layer 45 Guide pin 50,62,106 Spacer 60 Adapter 61 Opening 100 Optical Connector 102 Resin ferrule 104 (of the resin ferrule 102) end face
Claims
1. a glass plate having a plurality of first through holes; a resin ferrule fixed to the glass plate and having a plurality of second through holes coaxial with each of the plurality of first through holes; A plurality of optical fibers including glass fibers and a coating resin covering the glass fibers; the glass fibers exposed from the tips of the optical fibers are held in the first through holes and the second through holes, The flexural modulus of the material constituting the resin ferrule is 5 GPa or more at 200° C., An optical fiber connection component, wherein each first through hole has a first tapered portion that expands in diameter toward a first surface of the glass plate, and each second through hole has a second tapered portion that expands in diameter toward a second surface of the resin ferrule that faces the first surface.
2. The optical fiber connection component according to claim 1 , wherein the material is a liquid crystal polymer.
3. 3. The optical fiber connecting component according to claim 1, wherein the material has a thermal shrinkage rate of 0.5% or less when heated from room temperature to a temperature of 200[deg.] C. or more.
4. 4. The optical fiber connecting component according to claim 1, wherein the variation in inclination of the optical fibers held in the first through holes and the second through holes is 0.5 degrees or less.
5. 5. The optical fiber connection part according to claim 1, wherein the P-V value of the surface of the glass plate when the glass plate is heat-treated at 200° C. or higher is 5 μm or less.
6. The optical fiber connecting component according to claim 1 , wherein the plurality of first through holes are arranged two-dimensionally in one cross section of the glass plate.
7. 7. The optical fiber connecting component according to claim 1, wherein the glass fiber protrudes from the end face of the glass plate by 50 nm to 1 μm.
8. the glass plate has a first guide hole; 8. The optical fiber connecting component according to claim 1, wherein the resin ferrule has a second guide hole coaxial with the first guide hole.
9. 9. The optical fiber connecting part according to claim 1, wherein an outer diameter of the glass fiber is 100 [mu]m or less.
10. 10. The optical fiber connecting part according to claim 1, wherein each of the plurality of optical fibers is a multi-core optical fiber having a plurality of cores and a cladding covering the plurality of cores as the glass fiber.
11. An optical fiber connection structure in which a first optical fiber connection part, which is the optical fiber connection part according to any one of claims 1 to 10, is connected to a second optical fiber connection part to which a plurality of optical fibers are fixed so as to match the arrangement of the plurality of optical fibers in the first optical fiber connection part, a first end face of the first optical fiber connecting part and a second end face of the second optical fiber connecting part are surfaces inclined with respect to optical axes of the optical fibers, An optical fiber connection structure, wherein a gap of 30 μm or less is formed between the first end face and the second end face.
12. The second optical fiber connecting part is an optical fiber connecting part according to any one of claims 1 to 10, The optical fiber connection structure according to claim 11, further comprising a spacer configured to form the gap on an end surface of the glass plate of at least one of the first optical fiber connection part and the second optical fiber connection part.
13. the second optical fiber connection component is configured by mounting the plurality of optical fibers in a resin ferrule, The optical fiber connection structure according to claim 11 , further comprising a spacer configured to form the gap on an end face of the second optical fiber connection component.
14. The second optical fiber connection part is an optical fiber connection part according to any one of claims 1 to 10, or a part configured by mounting the plurality of optical fibers on a resin ferrule, The optical fiber connection structure according to claim 11, further comprising a spacer configured to form the gap within an adapter of the optical fiber connection structure.
Citation Information
Patent Citations
Plastic ferrule for optical connector and its production
JP1998293232A
Ferrule, and method for manufacturing ferrule
JP2004038005A
Optical connector molding die
JP2004117616A
Method for manufacturing optical fiber assembly and optical fiber assembly
JP2004258193A
Optical path converting element
JP2007147859A