Insulating Rope

The insulating rope with periodically formed bumps on its jacket addresses the issue of water-induced dielectric strength loss by ensuring effective rainwater runoff, thereby maintaining insulation performance in wet conditions.

JP7560122B2Active Publication Date: 2024-10-02TAKAGI INDUSTRIAL CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021102577
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-06-21
Publication Date
2024-10-02
Estimated Expiration
2041-06-21

AI Technical Summary

Technical Problem

Insulating ropes used outdoors for power transmission lines lose dielectric strength due to water accumulation on the outer sheath during rain, leading to reduced insulation performance.

Method used

The insulating rope features a core wire covered by a jacket with periodically formed bumps or knob members along its length, designed to disrupt the water chain and maintain dielectric strength by facilitating rainwater runoff.

Benefits of technology

The bumps effectively prevent water accumulation, reducing leakage current and maintaining dielectric strength during rainfall, enhancing the rope's performance in wet conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007560122000001
    Figure 0007560122000001
  • Figure 0007560122000002
    Figure 0007560122000002
  • Figure 0007560122000003
    Figure 0007560122000003
Patent Text Reader

Abstract

To provide an insulating rope which can maintain dielectric strength even during rainfall time.SOLUTION: An insulating rope AA includes: a core wire 10; and an insulating outer cover 20 which covers an outer periphery of the core wire 10. In the insulating rope AA, a plurality of cobs 31 which have enlarged rope diameters are provided at intervals along a longitudinal direction. Each of the cobs 31 may be formed of a thickness increased section of the outer cover 20. Each of the cobs 31 may be formed of a cob member fitted into the outer periphery of the outer cover 20. The insulating rope can maintain insulating strength even during rainfall time because rain water running on an outside surface of the insulating rope AA falls from the cobs 31 and can cut continuous portions of water.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an insulating rod. P More specifically, the present invention relates to an insulating rope having insulating properties. P About 。 [Background technology]

[0002] For example, insulated ropes are used in power line re-laying work to support an electric wire to be re-layed while keeping nearby power lines live (Patent Document 1). Insulated ropes are required to have high insulation properties because they may come into contact with live wires or be exposed to induced voltages. For this reason, insulated ropes are composed of a rope core made of braided non-conductive fibers and an outer sheath whose outer periphery is covered with insulating resin. The outer sheath itself has insulating properties and also has waterproof properties that prevent rainwater from penetrating the rope core. Since the outer sheath prevents rainwater from penetrating the rope core, it is possible to prevent a decrease in insulating properties due to the rope core becoming wet. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 63-211392 Summary of the Invention [Problem to be solved by the invention]

[0004] However, when an insulated rope is exposed to rain, water accumulates on the surface of the outer sheath, causing a decrease in dielectric strength. Therefore, insulated ropes that are used outdoors for long periods of time, particularly near live parts, are required to be able to maintain their dielectric strength even when it rains.

[0005] In view of the above circumstances, the present invention provides an insulating rope capable of maintaining its dielectric strength even during rainfall. P The purpose is to provide 。 [Means for solving the problem]

[0006] Books The insulated rope of the present invention comprises a core wire, an insulating outer sheath covering the outer periphery of the core wire, a plurality of knob members fitted to the outer periphery of the outer cover at intervals along the longitudinal direction; Equipped with The bump member is a separate member from the outer cover. It is characterized by: Effect of the Invention

[0007] Books To the invention According Rainwater running along the outer surface of the insulating rope falls off the bumps, breaking the water chain, allowing the rope to maintain its dielectric strength even during rainfall. 。 [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a side view of an insulating rope according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a longitudinal sectional view of the insulating rope. [Diagram 3] 3 is a cross-sectional view taken along line III-III in FIG. 1. [Figure 4] Figure (A) is an explanatory diagram of an insulated rope without knobs exposed to rain. Figure (B) is an explanatory diagram of an insulated rope with knobs exposed to rain. [Diagram 5] FIG. [Figure 6] FIG. 6 is a side view of an insulating rope according to a second embodiment of the present invention. [Figure 7] 1 is a photograph of an insulating rope produced as an example. [Figure 8] FIG. 2 is a side view of a water injection insulation performance test device. [Figure 9] Figure (A) is a photograph of an insulated rope without a knob when water is poured in. Figure (B) is a photograph of an insulated rope with a knob when water is poured in. [Figure 10] 1 is a graph showing measurement results of leakage current. [Figure 11] 1 is a graph showing measurement results of a flashover voltage. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Next, an embodiment of the present invention will be described with reference to the drawings. [First embodiment] As shown in Fig. 1, the insulated rope AA according to the first embodiment of the present invention comprises a core wire 10 and an outer sheath 20 covering the outer periphery of the core wire 10. The core wire 10 comprises a rope core 11 and a braided tube 12 covering the outer periphery of the rope core 11. The core wire 10 does not have to have the braided tube 12. In other words, the core wire 10 may be composed of only the rope core 11. Furthermore, the core wire 10 may include other wire materials, etc.

[0010] The rope core 11 is made by braiding non-conductive fibers into a rope shape. Although not particularly limited, aramid fibers, polyarylate fibers, ultra-high molecular weight polyethylene fibers, etc. can be used as the non-conductive fibers constituting the rope core 11. There is no particular limit to the way the fibers of the rope core 11 are braided.

[0011] The braided tube 12 is made by weaving non-conductive fibers into a tube shape so as to cover the outer periphery of the rope core 11. Although not particularly limited, polyester fibers, vinylon fibers, etc. can be used as the non-conductive fibers constituting the braided tube 12. There is no particular limit to the way in which the fibers of the braided tube 12 are woven.

[0012] The outer cover 20 is made of an insulating material and has insulating properties. Although not particularly limited, examples of the material used for the outer cover 20 include insulating resins such as polyurethane and polyvinyl chloride (PVC).

[0013] The insulated rope AA is provided with a plurality of bumps 31 with an enlarged rope diameter spaced apart along the longitudinal direction. The portion of the insulated rope AA where the rope diameter is not enlarged, i.e., the portion other than the bumps 31, is called the smooth portion 32. As shown in Fig. 3, the bumps 31 only need to have a larger diameter than the smooth portion 32. The shape of the bumps 31 is not particularly limited. The bumps 31 may be shaped like a sphere overall, or like a disk.

[0014] As shown in Fig. 4(A), when a conventional insulated rope 100 without a knob is exposed to rain, water W is formed on the outer surface of the insulated rope 100. When a voltage is applied to the insulated rope 100 in this state, a relatively large leakage current flows, making the rope susceptible to dielectric breakdown. Thus, the dielectric strength of the insulated rope 100 decreases during rainfall.

[0015] In contrast, as shown in Fig. 4(B), when the insulated rope AA of this embodiment is exposed to rain, the rainwater running along the outer surface falls off the bumps 31, breaking the chain of water. As a result, even when a voltage is applied to the insulated rope 100, the leakage current is small and insulation breakdown is unlikely to occur. In addition, the bumps 31 create irregularities on the outer surface of the insulated rope AA, which increases the creepage distance. As a result, the dielectric strength can be maintained even during rainfall.

[0016] From the viewpoint of breaking the chain of water, it is preferable that the diameter of the bumps 31 is large. Specifically, the diameter of the bumps 31 is preferably 1.5 times or more, and more preferably 2 times or more, the diameter of the smooth portion 32. Alternatively, the difference between the diameter of the bumps 31 and the diameter of the smooth portion 32 is preferably 2 mm or more, and more preferably 4 mm or more. In this way, rainwater can easily drop off the bumps 31, making it easier to break the chain of water.

[0017] On the other hand, if the diameter of the bump 31 is too large, the workability (ease of use) of the rope decreases. From the viewpoint of maintaining the workability of the rope, the diameter of the bump 31 is preferably 3 times or less than the diameter of the smooth portion 32, and more preferably 2.5 times or less. Alternatively, the difference between the diameter of the bump 31 and the diameter of the smooth portion 32 is preferably 9 mm or less, and more preferably 6 mm or less. In this way, the workability of the insulated rope AA can be maintained.

[0018] The diameters of the multiple bumps 31 on the insulated rope AA may all be the same or may be different. The diameter of the smooth portion 32 is selected according to the intended use of the insulated rope AA. The diameter of the smooth portion 32 is, for example, 3 to 10 mm.

[0019] From the viewpoint of breaking up the water chain into small segments, it is preferable that the interval between two adjacent bumps 31 (the distance between the centers of bumps 31) is narrow. Specifically, the interval between bumps 31 is preferably 100 mm or less, and more preferably 50 mm or less. In this way, the portion where water chains are connected becomes short, and the dielectric strength can be maintained even during rainfall.

[0020] On the other hand, if the intervals between the bumps 31 are too narrow, the workability as a rope decreases. From the viewpoint of maintaining the workability as a rope, the intervals between the bumps 31 are preferably 10 mm or more, and more preferably 20 mm or more. In this way, the workability of the insulated rope AA can be maintained. The intervals between the bumps 31 may be equal or unequal.

[0021] 2, insulated rope AA of this embodiment has an outer sheath 20 whose thickness is not constant along the longitudinal direction, but has portions (thickened portions) where the thickness is increased at intervals. These thickened portions of the outer sheath 20 form bumps 31. The diameter of the core wire 10 is constant along the longitudinal direction.

[0022] Generally, the outer covering of an insulating rope is formed by extrusion molding. More specifically, the core wire is passed through a crosshead die of an extruder to form an insulating outer covering that covers the outer circumference of the core wire. Here, the thickness of the outer covering can be adjusted by the speed of the core wire as it passes through the die. Increasing the speed of the core wire makes the outer covering thinner, and decreasing the speed of the core wire makes the outer covering thicker.

[0023] In this embodiment, the speed at which the core wire 10 passes through the die is periodically slowed down. In other words, the speed of the core wire 10 is changed so as to alternate between high and low speeds. This makes it possible to form the jacket 20 having a plurality of thickened portions spaced apart along the longitudinal direction. In this manner, the jacket 20 having the humps 31 can be continuously formed by the extrusion molding machine. This makes it possible to efficiently manufacture the insulated rope AA that can maintain its dielectric strength even during rainfall.

[0024] Such an extrusion molding method can be realized, for example, by a jacket forming apparatus XX shown in FIG. The jacket forming device XX has an extruder 40. The extruder 40 is a general extruder used for covering a core wire. The extruder 40 has an extruder 41 that melts and extrudes a resin material, and a die 42 attached to the outlet of the extruder 41. A die suitable for covering a core wire, such as a crosshead die, is selected as the die 42.

[0025] The jacket forming device XX has a pay-out device 51 and a winding device 52. The pay-out device 51 pays out the wound core wire 10 and supplies it to the die 42. When the core wire 10 is passed through the die 42, the resin material is molded into the jacket 20 that covers the outer periphery of the core wire 10. The molded product (the insulated rope AA in this embodiment) discharged from the die 42 is wound by the winding device 52.

[0026] The jacket forming device XX further has a passing speed adjusting unit 60. The passing speed adjusting unit 60 may be configured to periodically slow down the passing speed of the core wire 10 through the die 42. For example, the passing speed adjusting unit 60 includes a guide 61 that guides the core wire 10, and a guide driving unit 62 that vibrates the guide 61.

[0027] The guide 61 is located between the payout device 51 and the die 42, and guides the core wire 10. The guide 61 is composed of, for example, two rollers that sandwich the core wire 10, and a base that supports the two rollers.

[0028] The guide driving unit 62 vibrates the guide 61 in a direction perpendicular to the transport direction of the core wire 10. The guide driving unit 62 is composed of, for example, a piston-crank mechanism and a motor. When the core wire 10 is transported horizontally, the guide 61 may be vibrated vertically. Note that "vibrating in a direction perpendicular to the transport direction of the core wire" means that the vibration direction has a component perpendicular to the transport direction of the core wire. The vibration direction may have a component in the transport direction of the core wire. In other words, the vibration may be in a direction oblique to the transport direction of the core wire.

[0029] As shown by the solid line in FIG. 5, the transport path where the core wire 10 becomes straight is defined as the reference path. When the guide 61 moves outward from this state, the transport path of the core wire 10 bulges outward as shown by the dashed line. This transport path is defined as the roundabout path. The roundabout path is longer than the reference path. The unwinding device 51 and the winding device 52 transport the core wire 10 at a constant speed. However, as the guide 61 moves outward, the transport path of the core wire 10 becomes longer. The core wire 10 and the insulating rope AA stretch to compensate for the increased length of the transport path. This slows down the transport speed of the core wire 10 when it passes through the die 42. Conversely, when the guide 61 returns from the outside to its original position, the transport path of the core wire 10 becomes shorter, and the transport speed of the core wire 10 when it passes through the die 42 becomes faster. In this way, by vibrating the guide 61, the passing speed of the core wire 10 through the die 42 periodically slows down.

[0030] As described above, the transport speed of the core wire 10 can be changed with a simple configuration including the guide 61 and the guide drive unit 62. This makes it possible to reduce the equipment cost of the jacket forming device XX.

[0031] By periodically slowing down the passing speed of the core wire 10 through the die 42, it is possible to continuously form the jacket 20 having thickened portions spaced apart along the longitudinal direction. In other words, since the bumps 31 can be continuously formed, the production efficiency of the jacket 20 having the bumps 31 is high.

[0032] The diameter and interval of the bumps 31 can be adjusted by the transport speed of the unwinding device 51 and the winding device 52 and the vibration period of the guide 61.

[0033] The use of the sheath forming device XX is not limited to the manufacture of an insulated rope AA. The sheath forming device XX is used to form a sheath having nubs regardless of size or spacing. The sheath forming device XX can be used, for example, to form slight irregularities on the outer surface of a rope that are suitable for increasing gripping power. In addition, the core wire forming the sheath is not limited to a fiber rope. The core wire may be a wire rope, an electric wire, an optical fiber, or the like. The material of the sheath is also not limited to insulating resin.

[0034] Second Embodiment Next, an insulating rope BB according to a second embodiment of the present invention will be described. As shown in Fig. 6, the insulated rope BB has a core wire 10 and an outer sheath 20. The core wire 10 has a constant diameter along the longitudinal direction. The outer sheath 20 has a constant thickness along the longitudinal direction. In other words, the portion consisting of the core wire 10 and the outer sheath 20 has the same structure as a conventional insulated rope.

[0035] A bump member 33 is fitted to the outer periphery of the outer jacket 20. The bump member 33 is made of, for example, two divided parts, and is fitted to the outer periphery of the outer jacket 20 by combining the two parts with the outer jacket 20 in between. The bump member 33 is made of an insulating resin such as nylon, polyethylene, or polyvinyl chloride (PVC). The shape of the bump member 33 is not particularly limited. The bump member 33 may be ring-shaped, cylindrical, or barrel-shaped.

[0036] A plurality of knob members 33 are provided at intervals along the longitudinal direction of the insulated rope BB. The knob members 33 form the bumps 31. When the insulated rope BB is exposed to rain, rainwater running along the outer surface falls off the bumps 31, breaking the chain of water. Therefore, the dielectric strength can be maintained even during rainfall. EXAMPLES

[0037] Next, an embodiment will be described. (Making insulating rope) An insulated rope with the structure shown in Figure 1 was created. Aramid fiber braided into a rope shape was used as the rope core. Polyester fiber was braided to cover the outer circumference of the rope core, creating a braided tube. The diameter of the core wire consisting of the rope core and the braided tube is 3 mm.

[0038] An outer sheath was formed around the core wire using an outer sheath forming device with the configuration shown in Figure 5. Polyurethane was used as the material for the outer sheath. A photograph of the produced insulated rope is shown in Figure 7. The diameter of the bumps of the insulated rope is 8.8 mm or 9.8 mm. The diameter of the smooth part is 4.4 mm. Therefore, the diameter of the bumps is 2.0 to 2.2 times the diameter of the smooth part, and the difference between the diameter of the bumps and the diameter of the smooth part is 4.4 to 5.4 mm. In addition, the spacing between the bumps is 14.4 mm or 16.4 mm.

[0039] (Water injection insulation performance test) A water injection insulation performance test was conducted on an insulated rope using the test equipment shown in FIG. The insulating rope under test was stretched diagonally and showered with rainfall equivalent to 3mm / min. Two electrodes were placed at a distance from each other on the insulating rope and an AC voltage was applied between the electrodes. The current (leakage current) that flowed through the insulating rope was measured with an ammeter.

[0040] The test subjects were an insulated rope with a knob as shown in Figure 7, and an insulated rope with a conventional configuration without a knob. The diameter of the insulated rope with a conventional configuration is 4.4 mm. The materials of the rope core, braided tube, and outer sheath are the same as those of the insulated rope with a knob.

[0041] Figure 9(A) shows a photograph of an insulated rope without a knot when water is poured into it. It can be seen that the water forms a continuous line along the outer surface of the insulated rope. Figure 9(B) shows a photograph of an insulated rope with a knot when water is poured into it. It can be seen that the water running along the outer surface of the insulated rope falls off the knot and the water line is broken.

[0042] Leakage current The electrodes on the insulated rope were spaced 30 cm apart, and an AC voltage of 50 kV was applied to measure the leakage current. The results are shown in Figure 10. For an insulated rope without knobs, the leakage current was 6 to 9 mA. In contrast, for an insulated rope with knobs, the leakage current was 0.1 mA on average, with a maximum of 0.5 mA. This confirmed that adding knobs to an insulated rope can reduce the leakage current to 1 / 12 or less.

[0043] Voltage resistance The electrodes on the insulated rope were spaced 25cm apart, and the applied AC voltage was increased to measure the flashover voltage when a spark discharge occurred. The results are shown in Figure 11. In dry conditions, the flashover voltage of the insulated rope without a knot was 104.3 kV, and the flashover voltage of the insulated rope with a knot was 107.3 kV. In dry conditions, there is no significant difference in flashover voltage depending on whether or not there is a knot.

[0044] When water is poured into the insulated rope, the flashover voltage of the insulated rope without a knob drops to 45.5 kV. On the other hand, the flashover voltage of the insulated rope with a knob does not drop much and remains at 94.6 kV. This confirms that adding a knob to an insulated rope can increase the flashover voltage when water is poured into it by 2.1 times.

[0045] From the above, it was found that the insulated rope with knobs has superior dielectric strength during rainfall compared to the insulated rope without knobs. [Industrial Applicability]

[0046] The insulating rope of the present invention is used in applications that require insulating performance. Since it can maintain its dielectric strength even in the rain, it is particularly suitable for use outdoors for long periods of time near live electrical parts. For example, it can be used as a rope for marking divisions or danger signs near live electrical parts. [Explanation of symbols]

[0047] AA, BB insulated rope 10 core wire 11 Rope core 12 Braided Tube 20 Outer cover 31 Cobb 32 Smooth section 33 Cob material XX Enveloping device 40 Extrusion molding machine 41 Extruder 42 Die 51 Payout device 52 Winding device 60 Passage speed adjustment section 61 Guide 62 Guide drive unit

Claims

[Claim 1] A core wire, An insulating outer sheath that covers the outer periphery of the core wire; a plurality of knob members fitted to the outer periphery of the outer cover at intervals along the longitudinal direction; The bump member is a separate member from the outer cover. An insulating rope characterized by:

Citation Information

Patent Citations

  • JP1974027553A

  • JP1974033962A

  • JP1974095669U

  • JP1974105861A

  • JP1975151690A