Ceramic device and method for manufacturing same
The ceramic device with a substrate composed of A x B y C 1-x-v Ti 1-y+w O 3 *(Mn 2 P 2 O 7 ) z *D u addresses ESD sensitivity and size reduction challenges, achieving reliable and cost-effective miniaturized capacitors with improved electrical properties.
Patent Information
- Application Number
- JP2021566081
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-05-08
- Filing Date
- 2020-04-24
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2040-04-24
AI Technical Summary
Conventional ceramic materials used in miniaturizing capacitors face issues with increased sensitivity to electrostatic discharge (ESD), which can render them unusable, and reducing size negatively impacts electrical properties.
A ceramic device with a ceramic substrate composed of a specific formula A x B y C 1-x-v Ti 1-y+w O 3 *(Mn 2 P 2 O 7 ) z *D u, where A, B, and C are doping metals, and D is an additive manganese pyrophosphate, allowing for a lower sintering temperature and improved electrical properties, including ESD resistance.
The solution enables the production of smaller capacitors with enhanced ESD resistance and reduced costs due to the use of nickel-containing internal electrodes, maintaining high reliability and compactness.
Smart Images

Figure 0007561143000002 
Figure 0007561143000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a ceramic device including a ceramic substrate having a ceramic material. The present invention also relates to a method of making the ceramic device.
[0002] Ceramic devices are widely used components in electronic devices. With the increasing demand for miniaturization and effective power of electronic devices, there is a need to provide smaller ceramic devices. However, the reduction in size of ceramic devices using conventional ceramic materials can have a detrimental effect on the electrical properties of the ceramic devices in particular. Therefore, miniaturization of capacitors using conventional ceramic materials can increase the sensitivity of the capacitor to electrostatic discharge (ESD), for example, which may render the capacitor unusable.
[0003] The German translation of the international application 11 2012 000 669 gives a first example of a ceramic element according to the prior art so far.
[0004] The German translation of the international application 11 2012 000 669 describes a laminated semiconducting ceramic capacitor with varistor function and a method for its manufacture, in particular a grain boundary insulating semiconducting ceramic based on SrTiO3 used for the varistor function, and also discloses an embodiment in which a dopant is added to the corresponding semiconducting ceramic, the dopant being selected primarily from lanthanum, neodymium, niobium and tantalum.
[0005] French Patent Publication No. 2 799 301 describes a second example of a ceramic element according to the previous prior art.
[0006] French Patent Publication No. 2 799 301 describes a nonlinear resistor that can be used to protect the power grid against overvoltages and a method for its manufacture, and discloses that the nonlinear resistor has zinc oxide as its main component, that the nonlinear resistor is provided with a high resistance layer on its side, and that the nonlinear resistor may be doped with manganese pyrophosphate. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] German translation of international application No. 11 2012 000 669 [Patent Document 2] French Patent Publication No. 2 799 301 Summary of the Invention [Problem to be solved by the invention]
[0008] In view of the above, it is an object of the present invention to provide a ceramic device including a ceramic substrate based on an improved ceramic material. It is also an object of the present invention to provide a method for producing the ceramic device. [Means for solving the problem]
[0009] The solution of the invention to achieve the above object is a ceramic device as defined in claim 1. For further embodiments of the ceramic device and for the method of manufacturing the ceramic device, please refer to the other claims.
[0010] A ceramic device is provided having a ceramic substrate, the ceramic substrate comprising a ceramic material as a main component, the ceramic material being represented by the general formula A x B y C 1-x-v Ti 1-y+w O3* (Mn2P2O7) z *D uIn the general formula, A is a first doping selected from the group of first metals consisting of neodymium, praseodymium, cerium and lanthanum. B is a second doping selected from the group of second metals consisting of niobium, tantalum and vanadium. C is a main component of the base ceramic material, which is selected from the group of third metals consisting of calcium, strontium and barium. D is an additive containing at least one first compound, which contains a fourth metal selected from the group of fourth metals consisting of aluminum, nickel and iron. x is the amount ratio of A, y is the amount ratio of B, v is the amount ratio of vacancies in A, w is the amount ratio of excess titanium, z is the amount ratio of Mn2P2O7, and u is the amount ratio of D. With respect to the amount ratio, 0.0≦x<0.1, 0.0≦y<0.1, 0≦v<1.5*x, 0≦w<0.05, 0.01≦z<0.1 The relationship 0≦u<0.05 applies.
[0011] Hereinafter, base ceramic material will refer to a base compound represented by the general formula CTiO3, where C is the major component of the base ceramic material, which is selected from the group of third metals.
[0012] Also, hereinafter, a first doping refers to a first metal occupying atomic positions of a third metal in the lattice of the base ceramic material.
[0013] Also, hereinafter, a second doping will refer to a second metal occupying an atomic site of titanium in the lattice of the base ceramic material.
[0014] In one embodiment of the ceramic material, the ceramic material includes a base ceramic material including a first doping and a second doping, at least one additive, and manganese pyrophosphate having a composition formula of Mn2P2O7.
[0015] The values of the percentages of the amount of the first doping, the second doping, and the additive may all be zero. In other words, the ceramic material may include only one of the first doping, the second doping, and the additive in addition to the base ceramic material. The ceramic material may also include only the first doping and the additive, or the second doping and the additive, as a complement to the base ceramic material. Furthermore, the ceramic material may only include the base ceramic material including the first doping and the second doping. In this case, the ceramic material does not include any additive. In all the above embodiments, the percentage of manganese pyrophosphate included in the ceramic material is greater than zero. In other words, the ceramic material always includes manganese pyrophosphate.
[0016] Also, the first doping may include at least two first metals, the second doping may include at least two second metals, and the main component of the base ceramic material may include at least two third metals.
[0017] The additive may also include at least one first compound and a second compound, each of which includes one fourth metal. Among them, the fourth metal included in the first compound is different from the fourth metal included in the second compound. That is, the first compound includes a fourth metal different from that of the second compound. As the first compound and the second compound, a metal oxide including at least one fourth metal may be used.
[0018] The ceramic material preferably has any of the combinations of components shown in Table 1 below.
[0019] [Table 1]
[0020] In Table 1, B1 represents a second metal and B2 represents another second metal, which are contained in the second doping B, where the coefficients y1 and y2 are the proportions of the second metals B1 and B2, respectively, in the second doping B. The sum of the coefficients y1 and y2 is the proportion y of the amount of the second doping in the ceramic material.
[0021] Additionally, C1 represents a third metal, C2 represents another third metal, and C3 represents yet another third metal, which are contained in the main component C of the substrate material. The values of C1, C2, and C3 represent the percentage amounts of the corresponding third metals in the main component C, where the sum of the values of C1, C2, and C3 is 1.
[0022] Additionally, D1 represents a fourth metal and D2 represents another fourth metal, which are contained in additive D. The sum of coefficients u1 and u2 is the fraction u of the amount of additive contained in the ceramic material.
[0023] It should be noted that the quantity ratios of the components of the ceramic material may vary in the range of up to 10% in accordance with the examples 1 to 7 listed in Table 1. Thus, the quantity ratio of the first doping x in Example 1 is not limited to, for example, its value of 0.02. To be precise, x may have all values in the range of 0.018 to 0.022. Similarly, the other values of the corresponding quantity ratios listed in Table 1 may also all vary in the range of up to 10%. The advantageous quantity ratios vary in the range of up to 5% of the values listed in the table. This means that in the case of the quantity ratio x of the first doping in Example 1, it can take all values in the range of 0.019 to 0.021.
[0024] The ceramic substrate of the ceramic device may also have a plurality of ceramic layers, which may be the same or different, and internal electrodes disposed between the ceramic layers, where the internal electrodes include nickel as a major component.
[0025] The ceramic device may also be configured as a capacitor. In particular, the ceramic device may be configured as a multilayer capacitor. The multilayer capacitor includes a ceramic substrate having a plurality of ceramic layers and internal electrodes provided between the ceramic layers. The internal electrodes preferably include nickel.
[0026] Due to the manganese pyrophosphate contained in the ceramic material, a densely sintered ceramic substrate can be obtained at a relatively low sintering temperature of 1200° C. or less. Hereinafter, a densely sintered ceramic substrate refers to a substrate with a sintered density of 90% or more.
[0027] The inventors explain the positive effect of manganese pyrophosphate, namely that it melts congruently under reducing conditions already at temperatures below 1100°C. Congruent melting means that manganese pyrophosphate becomes completely liquid at the so-called melting point, but does not decompose. As a result, the molten manganese pyrophosphate is distributed homogeneously in the ceramic body, which results in a very homogeneous and highly compacted ceramic body.
[0028] The use of manganese pyrophosphate to lower the sintering temperature inhibits grain growth during sintering of the ceramic, improving the electrical and mechanical properties of the ceramic substrate.
[0029] Lowering the sintering temperature also allows the use of nickel-containing internal electrodes, because they do not melt at low sintering temperatures, and nickel has a lower cost than traditional internal electrode metals such as gold, silver, and palladium, which helps keep the overall cost of ceramic elements at a low level.
[0030] Ceramic materials can be the main component of a ceramic substrate that is part of a capacitor, particularly a multilayer capacitor, which can reduce the size of the capacitor and provide a multilayer capacitor with ESD resistance and Ni-containing internal electrodes, making the multilayer capacitor more reliable and less expensive.
[0031] Construction types 0603 and below shall be considered small capacitor sizes. Additionally, ESD-resistant capacitors shall be defined as those with construction types 0603 and below, capacitances less than 10nF, and ESD voltages greater than 8kV. ESD-resistant capacitors preferably have capacitances of 1nF and ESD voltages greater than 20kV. ESD voltage is the voltage that can be applied without damaging the element. The higher the ESD voltage, the higher the voltage that can be applied without damaging the element.
[0032] The present invention also relates to a method for manufacturing a ceramic device, said method comprising the steps of: providing a base ceramic material having a general formula of CTiO3, where C is a major component of the base ceramic material, the major component including a third metal selected from a group of third metals consisting of calcium, strontium, and barium; Adding an additive containing Mn2P2O7, a first dopant comprising a first metal, and / or a second dopant comprising a second metal, and / or a compound containing Ti, and / or at least one first compound comprising a fourth metal to the ceramic material and mixing to obtain a mixture, wherein the first metal is selected from a first group of metals consisting of neodymium, praseodymium, cerium and lanthanum, the second metal is selected from a second group of metals consisting of niobium, tantalum and vanadium, the third metal is selected from a third group of metals consisting of calcium, strontium and barium, and the fourth metal is selected from a fourth group of metals consisting of aluminum, nickel and iron; grinding the mixture to obtain a powder of the mixture; producing a ceramic green sheet from the powder of the mixture; forming an internal electrode on the ceramic green sheet; laminating the ceramic green sheets to obtain a green sheet laminate; A step of compressing the green sheet laminate to obtain a compressed green sheet laminate; Singulating the pressed green sheet laminate to obtain raw materials for singulated elements; decarbonizing the singulated element to obtain a decarbonized element; sintering the decarburized element to obtain a sintered element; annealing the sintered element to obtain a ceramic substrate; Coating the exterior surface of the ceramic substrate with a metal coating and sintering to obtain a ceramic device.
[0033] Hereinafter, a material that includes at least one first metal shall be considered a first dopant, the first metal being a component of the first dopant.
[0034] Hereinafter, a material comprising at least one second metal shall be considered as a second dopant, said second metal being a component of the second doping.
[0035] As the first dopant, at least one oxide of a first metal may be used, where the first metal is selected from the first group of metals.
[0036] As the second dopant, at least one oxide of a second metal may be used, where the second metal is selected from the group of second metals.
[0037] A first and / or second dopant may also be added to the base ceramic material. Here, the first dopant includes at least two first metals, and the second dopant includes at least two second metals. In other words, the first dopant includes at least one component that contains at least two different first metals. The first dopant may preferably include a first component and a second component. Here, the first component includes a first metal that is different from the first metal included in the second component. The second dopant is similar to the first dopant, except that it includes a second metal instead of the first metal.
[0038] The primary component of the base ceramic material may further include at least two third metals.
[0039] Also, an additive may be added to the base ceramic material, the additive comprising at least aluminum and nickel. In other words, the additive may comprise a first compound comprising at least aluminum and nickel. The additive may preferably comprise a first compound and a second compound, where the first compound comprises nickel and the second compound comprises aluminum, or vice versa.
[0040] Alternatively, a metal-containing slurry containing nickel may be used to form the internal electrodes.
[0041] The laminate of the decarburized green sheets may be sintered at a temperature of 1200 to 1250° C. for a holding time of 1 to 5 hours. It is preferable to sinter the laminate of the decarburized green sheets at 1200° C., 1250° C., or a temperature therebetween for 4 hours.
[0042] In a preferred embodiment of the method for manufacturing the ceramic device, the stack of decarburized green sheets may be sintered in a reducing atmosphere, which hereinafter refers to an atmosphere that prevents oxidation of the ceramic material and the nickel-containing internal electrodes, particularly by oxygen in the air.
[0043] The sintered elements can also be reoxidized by annealing in air. For example, in a capacitor, this step can set the electrical properties of the capacitor, such as its ESD resistance.
[0044] The ceramic substrate may also be coated with a passivation layer made of glass, which protects the ceramic substrate from external influences such as humidity and temperature changes.
[0045] The present invention will now be described in detail based on embodiments with reference to the accompanying drawings. [Brief description of the drawings]
[0046] [Figure 1] FIG. 1 shows a ceramic device having a ceramic substrate.
[0047] The drawings and the dimensional ratios therein are not drawn to scale. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0048] FIG. 1 shows a ceramic device having a ceramic substrate 1 with an internal electrode 2 disposed therein and two metal coatings 3 attached to two opposing outer faces 1′ of the ceramic substrate 1. The ceramic substrate 1 also has a passivation layer 4 formed from glass. The ceramic device is configured as a multilayer capacitor. The ceramic substrate is made of a material having the formula La0,2Ba0, 194 Sr0, 776 Ti1O3* (Mn2P2O7) 0.01 Since the ceramic material includes a ceramic material represented by the formula:
[0049] In one embodiment, a ceramic substrate is manufactured by providing a base ceramic material represented by the formula Ba0.2Sr0.8TiO3. Lanthanum oxide as a first dopant, titanium oxide as a titanium-containing compound, and manganese pyrophosphate are added to the base ceramic material. The total amount ratio of the base ceramic material, the first dopant, the titanium-containing compound, and the manganese pyrophosphate is 100 mol%. Thus, the amount ratio value of the base compound is 97 mol%, the amount ratio value of the first dopant is 1 mol%, the amount ratio value of the titanium-containing compound is 1.5 mol%, and the amount ratio value of the manganese pyrophosphate is 0.5 mol%. Then, the base compound, the first dopant, the titanium-containing compound, and the manganese pyrophosphate are mixed and ground to obtain a powder of the mixture.
[0050] The powder of this mixture is used to produce ceramic green sheets, on which internal electrodes are formed by a metal-containing paste containing nickel. In a next step, the flat pressed ceramic green sheets are stacked into a green sheet laminate and pressed to obtain a pressed green sheet laminate. The pressed green sheet laminate is then singulated, after which the singulated elements are decarburized at 600° C. and sintered in a reducing atmosphere at 1250° C. for 4 hours to obtain the ceramic substrate 1. In another step, the two opposing outer faces 1′ of the ceramic substrate 1 are coated with a metal coating 3. Finally, the ceramic substrate 1 is coated with a passivation layer 4 made of glass.
[0051] The present invention is not limited to the above examples. The ceramic material may have a combination of components corresponding to Examples 2 to 7 in Fig. 1, but may have a specific combination of components different from the combination of components in Examples 1 to 7 in Fig. 1. Here, Examples 1 to 7 are preferred. Furthermore, the application of the ceramic material is not limited to a capacitor. [Explanation of symbols]
[0052] 1. Ceramic substrate 1´ External surface 2 Internal electrode 3 Outer metal layer 4 Passivation Layer
Claims
1. A ceramic device having a ceramic substrate (1), the ceramic substrate comprising a ceramic material as a main component, the ceramic material having a general formula of: x B y C 1-x-v Ti 1-y+w O 3 * (Mn 2 P 2 O 7 ) z *D u where A is a first doping selected from the group of first metals consisting of neodymium, praseodymium, cerium and lanthanum; B is a second doping selected from the group of second metals consisting of niobium, tantalum and vanadium; C is a major component of the base ceramic material, said major component being selected from the group of third metals consisting of calcium, strontium and barium; and D is an additive comprising at least one first compound, said first compound comprising a fourth metal selected from the group of fourth metals consisting of aluminum, nickel and iron; x is the ratio of the amount of A, y is the ratio of the amount of B, v is the ratio of the amount of vacancies of A, w is the ratio of the amount of excess titanium, z is the ratio of the amount of Mn 2 P 2 O 7 is the proportion of the amount of D; 0.0≦x<0.1, 0.0≦y<0.1, 0≦v<1.5*x, 0≦w<0.05, 0.01≦z<0.1, A ceramic device having a ceramic substrate (1) to which the relationship 0≦u<0.05 applies.
2. The first doping comprises at least two first metals, and / or the second doping comprises at least two second metals, and / or the main component of the base ceramic material comprises at least two third metals. The ceramic device of claim 1 .
3. The additive includes at least one first compound and a second compound, the first compound and the second compound each including a fourth metal, and the fourth metal included in the first compound is different from the fourth metal included in the second compound. The ceramic device according to claim 1 or 2.
4. The ceramic substrate (1) has a plurality of ceramic layers and internal electrodes (2) provided between the ceramic layers. The ceramic device according to any one of claims 1 to 3.
5. A ceramic device as described in claim 4, wherein the internal electrode (2) contains nickel as its main component.
6. It is a capacitor, The ceramic device according to any one of claims 1 to 5.
7. 7. The ceramic device of claim 6, wherein the capacitor has a type 0603 or smaller construction.
8. The ceramic device according to claim 6 or 7, wherein the capacitor has a capacitance of 10 nF or less.
9. The ceramic device according to claim 6 , wherein the capacitor has an ESD voltage of more than 8 kV.
10. 10. The ceramic device according to any one of claims 6 to 9, further comprising a passivation layer (4) on the ceramic body (1).
11. 11. The ceramic device according to any one of the preceding claims, wherein the ceramic substrate is provided with a passivation layer (4) made of glass.
12. The ceramic substrate (1) has a sintered density of 90% or more. A ceramic device according to any one of claims 1 to 11.
13. A method for producing a ceramic device according to any one of claims 4 to 12, comprising the steps of: General formula CTiO 3 It is expressed as providing a base ceramic material, wherein C is a major component of said base ceramic material, said major component comprising a third metal selected from a group of third metals consisting of calcium, strontium and barium; The ceramic material may further comprise Mn 2 P 2 adding and mixing an additive comprising O7, a first dopant comprising a first metal, and / or a second dopant comprising a second metal, and / or a compound containing Ti, and / or said at least one first compound comprising a fourth metal, to obtain a mixture, wherein the first metal is selected from a first group of metals consisting of neodymium, praseodymium, cerium and lanthanum, the second metal is selected from a second group of metals consisting of niobium, tantalum and vanadium, the third metal is selected from a third group of metals consisting of calcium, strontium and barium, and the fourth metal is selected from a fourth group of metals consisting of aluminum, nickel and iron; grinding the mixture to obtain a powder of the mixture; producing a ceramic green sheet from the powder of the mixture; forming the internal electrodes (2) on the ceramic green sheets; laminating the ceramic green sheets to obtain a green sheet laminate; a step of compressing the green sheet laminate to obtain a compressed green sheet laminate; Singulating the pressed green sheet laminate to obtain raw materials for singulated elements; decarbonizing the singulated elements to obtain decarbonized elements; sintering the decarbonized element to obtain a sintered element; annealing the sintered element to obtain a ceramic substrate; and coating an exterior surface of the ceramic substrate with a metal coating and sintering the metal coating to obtain a ceramic device.
14. The main component of the base ceramic material includes at least two third metals. The method of claim 13.
15. The first dopant comprises at least two first metals and / or the second dopant comprises at least two second metals.
15. The method according to claim 13 or 14.
16. Add an additive containing at least aluminum and nickel 16. The method according to any one of claims 13 to 15.
17. The internal electrodes (2) are formed using a metal-containing slurry containing nickel.
17. The method according to any one of claims 13 to 16.
18. The laminate of the decarburized green sheets is sintered at a temperature of 1200 to 1250° C. for a holding time of 1 to 5 hours.
18. The method according to any one of claims 13 to 17.
19. The decarburized green sheet laminate is sintered in a reducing atmosphere.
19. The method according to any one of claims 13 to 18.
20. The ceramic substrate (1) is coated with a passivation layer (4) made of glass.
20. The method according to any one of claims 13 to 19.
21. 21. The method of any one of claims 13 to 20, wherein the annealing is performed in air.
Citation Information
Patent Citations
Voltage non-linear resistor for over voltage protective device, has sintered compact and high resistant layer containing mullite, orthoaluminum phosphate, ferrite and iron oxide
FR2799301A1
Ceramic capacitor and its manufacture
JP1995272973A
Multilayer ceramic chip capacitor
JP2000124058A
Method for manufacturing dielectric slurry and method for manufacturing laminated ceramic electronic part
JP2012072033A
WO112012000669