Image display device
The integration of a polarizing element opposite to the output diffraction element in AR glasses blocks stray light, addressing the issue of unintended visibility and improving image privacy and clarity in AR glasses.
Patent Information
- Application Number
- JP2021561361
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-11-26
- Filing Date
- 2020-11-19
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2040-11-19
AI Technical Summary
AR glasses suffer from stray light leakage in directions other than the intended observation position, making the displayed image visible to others.
Incorporation of a polarizing element positioned opposite to the output diffraction element, which blocks transmission of stray light by absorbing or reflecting polarized light selectively diffracted by the output diffraction element, and using a polarization diffraction element with a polarizing element arranged on the light guide plate.
Prevents stray light from being emitted to the outside, ensuring the image is only visible to the intended user, enhancing privacy and image clarity.
Smart Images

Figure 0007561763000011 
Figure 0007561763000012 
Figure 0007561763000013
Abstract
Description
[Technical field]
[0001] The present invention relates to an optical member that propagates light, and an image display device that uses the optical member. [Background technology]
[0002] In recent years, AR (Augmented Reality) glasses that display virtual images and various information superimposed on an actual scene as described in Patent Document 1 have been put to practical use. AR glasses are also called smart glasses, head mounted displays (HMDs), AR glasses, and the like.
[0003] As shown in Patent Document 1, as an example, AR glasses display an image displayed by a display (optical engine) by transmitting the image through one end of a light guide plate and emitting it from the other end, thereby superimposing a virtual image on the scene that the user actually sees. In AR glasses, the light from the display (projected light) is diffracted (refracted) using an input diffraction element and enters one end of the light guide plate. This allows the light to be introduced into the light guide plate at an angle, and the light is totally reflected and propagated within the light guide plate. The light propagated through the light guide plate is diffracted by an output diffraction element at the other end of the light guide plate, and is output from the light guide plate to the viewing position of the user. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] US2016 / 0231568A1 Summary of the Invention [Problem to be solved by the invention]
[0005] In AR glasses using a light guide element having such a light guide plate and a diffraction element, when light from the display is emitted to the user's observation position, there is a problem in that stray light leaks in the opposite direction to the observation position and can be seen by people other than the user.
[0006] An object of the present invention is to solve such problems of the conventional technology, and to provide an optical member and an image display device capable of suppressing stray light from being emitted to the outside. [Means for solving the problem]
[0007] In order to solve this problem, the present invention has the following configuration. [1] A light guide element including a light guide plate, an input diffraction element and an output diffraction element disposed on a main surface of the light guide plate, a polarizing element that blocks the transmission of light leaking to the opposite side to the exit side of the exit diffraction element; the output diffraction element is a polarizing diffraction element; the polarizing element is disposed on the opposite side to the exit side with respect to the exit diffraction element; The polarizing element is an optical member that is disposed at a position overlapping with the output diffraction element in the planar direction of the main surface of the light guide plate. [2] The output diffraction element is a reflective diffraction element; The optical member according to [1], wherein the polarizing element is disposed on the side of the output diffraction element opposite the light guide plate. [3] The optical member according to [1] or [2], wherein the polarizing element is spaced apart from the light-guiding element. [4] The optical member according to any one of [1] to [3], wherein the polarizing element is an elliptically polarizing plate. [5] The optical member according to any one of [1] to [4], wherein the polarizing element is a circular polarizing plate. [6] The optical member according to any one of [1] to [5], wherein the polarizing element comprises a linear polarizer and a retardation plate. [7] The optical element according to [6], wherein the retardation plate is a λ / 4 plate. [8] The optical element according to [6] or [7], wherein the retardation plate has reverse wavelength dispersion. [9] The optical member according to any one of [1] to [8], wherein the polarizing diffraction element is a liquid crystal diffraction element formed using a composition containing a liquid crystal compound and having a liquid crystal orientation pattern in which the direction of the optical axis derived from the liquid crystal compound changes while continuously rotating along at least one direction in the plane.
[10] The optical member according to [9], wherein the liquid crystal diffraction element has a region in which the direction of the optical axis of the liquid crystal compound is twisted and rotated in the thickness direction.
[11] The optical member according to [9] or
[10] , wherein the liquid crystal diffraction element has a cholesteric liquid crystal layer having a fixed cholesteric liquid crystal phase.
[12] The optical member according to any one of [1] to
[11] , wherein the period of the diffractive structure of the polarizing diffraction element is 0.1 μm or more and 10 μm or less.
[13] An optical member according to any one of [1] to
[12] , and a display element that projects an image onto the incident diffraction element of the optical member. Effect of the Invention
[0008] According to the present invention, it is possible to provide an optical member and an image display device capable of suppressing stray light from being emitted to the outside. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a top view conceptually illustrating an example of an image display device using an optical member of the present invention. [Diagram 2] FIG. 4 is a top view conceptually illustrating another example of an image display device using the optical member of the present invention. [Diagram 3] FIG. 3 is a front view conceptually showing the image display device shown in FIG. 2. [Figure 4] FIG. 3 is a side view conceptually showing the image display device shown in FIG. 2. [Diagram 5] FIG. 4 is a top view conceptually illustrating another example of an image display device using the optical member of the present invention. [Figure 6] FIG. 11 is a top view conceptually showing another example of an image display device of the present invention. [Figure 7]FIG. 2 is a plan view conceptually showing a liquid crystal layer used as a diffraction element. [Figure 8] 8 is a conceptual diagram of the liquid crystal layer shown in FIG. 7. [Figure 9] 8 is a diagram conceptually showing a cross-sectional SEM image of the liquid crystal layer shown in FIG. 7. [Figure 10] 8 is a conceptual diagram for explaining the function of the liquid crystal layer shown in FIG. 7. [Figure 11] FIG. 13 is a diagram conceptually illustrating another example of a liquid crystal layer used as a diffraction element. [Figure 12] FIG. 13 is a diagram conceptually illustrating another example of a liquid crystal layer used as a diffraction element. [Figure 13] FIG. 1 is a conceptual diagram of an example of an exposure apparatus for exposing an alignment film. [Figure 14] FIG. 13 is a diagram conceptually illustrating another example of a liquid crystal layer used in a diffraction element. [Figure 15] FIG. 15 is a plan view of the liquid crystal layer shown in FIG. [Figure 16] 15 is a conceptual diagram for explaining the function of the liquid crystal layer shown in FIG. 14. [Figure 17] 15 is a conceptual diagram for explaining the function of the liquid crystal layer shown in FIG. 14. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, the optical member and image display device of the present invention will be described in detail based on preferred embodiments shown in the accompanying drawings.
[0011] In this specification, a numerical range expressed using "to" means a range that includes the numerical values before and after "to" as the lower and upper limits. In this specification, "(meth)acrylate" is used to mean "either one or both of acrylate and methacrylate."
[0012] In this specification, visible light is electromagnetic light with wavelengths visible to the human eye, in the wavelength range of 380 to 780 nm, while non-visible light is light with wavelengths below 380 nm and above 780 nm. In addition, although not limited thereto, among visible light, light in the wavelength region of 420 to 490 nm is blue light, light in the wavelength region of 495 to 570 nm is green light, and light in the wavelength region of 620 to 750 nm is red light.
[0013] [Optical components and image display devices] The optical member of the present invention comprises: a light guide element including a light guide plate, an input diffraction element and an output diffraction element disposed on a main surface of the light guide plate; a polarizing element that blocks the transmission of light leaking to the opposite side to the exit side of the exit diffraction element; the output diffraction element is a polarizing diffraction element; the polarizing element is disposed on the opposite side to the exit side with respect to the exit diffraction element; The polarizing element is an optical member that is disposed at a position overlapping with the output diffraction element in the planar direction of the main surface of the light guide plate.
[0014] The image display device of the present invention comprises: The optical member described above; and a display element that projects an image onto the incident diffraction element of the optical member.
[0015] FIG. 1 conceptually shows an example of an image display device of the present invention that uses the optical member of the present invention.
[0016] The image display device 10 shown in Fig. 1 is used as AR glasses as a suitable example. The optical member of the present invention can be used as optical elements such as transparent screens, lighting devices (including backlights for liquid crystal displays), and sensors, in addition to AR glasses. The image display device of the present invention can also be used as an image display device that uses these optical elements.
[0017] The image display device 10 shown in Figure 1 has a display element 12, a light guide plate 16, a light guide element 14 having an input diffraction element 18 and an output diffraction element 24 arranged on the main surface of the light guide plate 16, and an optical member 13 having a polarizing element 26.
[0018] In the image display device 10 shown in Fig. 1, the incident diffraction element 18 and the exit diffraction element 24 are disposed at different positions in the planar direction of the main surface of the light guide plate 16. In the example shown in Fig. 1, the exit diffraction element 24 is disposed on the left side of the incident diffraction element 18. Note that the main surface is the maximum surface of a sheet-like object (plate-like object, film, etc.). The display element 12 is disposed at a position overlapping with the incident diffraction element 18 in the planar direction of the main surface of the light guide plate 16, facing the surface of the light guide plate 16 opposite the side on which the incident diffraction element 18 is disposed.
[0019] 1, the input diffraction element 18 and the output diffraction element 24 are reflective diffraction elements that diffract light while reflecting it, and the output diffraction element 24 is a polarizing diffraction element that selectively diffracts light in a predetermined polarization state.
[0020] In the image display device 10, the image (light corresponding to the image) displayed by the display element 12 is incident on the light guide plate 16 in a direction perpendicular to the main surface and enters the incident diffraction element 18. The light incident on the incident diffraction element 18 is diffracted by the incident diffraction element 18 and enters the light guide plate 16. At that time, the incident diffraction element 18 diffracts the light at an angle at which the light is totally reflected within the light guide plate 16, and also diffracts the light so that the diffracted light travels in a direction toward the exit diffraction element 24. In the example shown in FIG. 1, the incident diffraction element 18 diffracts the incident light toward the left in FIG. 1.
[0021] The light diffracted by the input diffraction element 18 is totally reflected and propagates within the light guide plate 16, and enters the output diffraction element 24. The output diffraction element 24 diffracts the incident light at an angle that deviates from the angle at which the light is totally reflected within the light guide plate 16. In the example shown in Fig. 1, the output diffraction element 24 diffracts the incident light toward the lower side in Fig. 1. That is, as shown in Fig. 1, the output diffraction element 24 diffracts the incident light in a direction approximately perpendicular to the main surface of the light guide plate.
[0022] The light diffracted by the output diffraction element 24 is output from the light guide plate 16 toward the user U. In this way, the image display device 10 can display the image projected by the display element 12.
[0023] Here, the optical member 13 has a polarizing element 26. In the example shown in Fig. 1, the polarizing element 26 is disposed on the opposite side of the output diffraction element 24 to the light guide plate 16 side. That is, the polarizing element 26 is disposed on the opposite side of the output diffraction element 24 from the output side. Moreover, the polarizing element 26 is disposed at a position overlapping with the output diffraction element 24 in the planar direction of the main surface of the light guide plate 16.
[0024] In the example shown in FIG. 1, the polarizing element 26 is made up of a retardation layer 27 and a linear polarizer 28.
[0025] As described above, when the image irradiated by the display element is guided by using the light guide element having the light guide plate and the diffraction element, and the image is outputted by the output diffraction element, light (stray light L) is emitted in the opposite direction to the output side by the output diffraction element. x If light leaks to the opposite side from the output side, the image can be seen by people other than the user. According to the study by the present inventors, it was found that the stray light is light in a polarized state that is selectively diffracted by the output diffraction element. In other words, the stray light is considered to be a part of the light that is guided through the light guide plate and should be diffracted by the output diffraction element toward the output side.
[0026] In contrast, the optical member of the present invention has a polarizing element disposed on the opposite side to the emission side with respect to the emission diffraction element and disposed at a position overlapping with the emission diffraction element in the planar direction of the main surface of the light guide plate.
[0027] The polarizing element is a polarizing element that absorbs or reflects the light in the polarized state selectively diffracted by the output diffraction element. By arranging such a polarizing element on the opposite side of the output diffraction element from the output side in the planar direction of the main surface of the light guide plate, where the polarizing element overlaps with the output diffraction element, it is possible to prevent the transmission of light leaking to the opposite side of the output side of the output diffraction element. This makes it possible to suppress stray light from being emitted to the outside. In addition, it is possible to suppress the image from being viewed by people other than the user due to stray light. Note that the polarizing element is preferably a polarizing element that absorbs the light in the polarized state selectively diffracted by the output diffraction element.
[0028] For example, when the light selectively diffracted by the output diffraction element is right-handed circularly polarized light, a left-handed circular polarizer that transmits left-handed circularly polarized light and absorbs (or reflects) right-handed circularly polarized light is used as the polarizing element. By arranging the left-handed circular polarizer on the opposite side to the output side of the output diffraction element and in a position overlapping with the output diffraction element in the planar direction of the main surface of the light guide plate, it is possible to absorb (or reflect) the right-handed circularly polarized light leaking to the opposite side to the output side of the output diffraction element, thereby preventing transmission.
[0029] In addition, the polarizing element absorbs or reflects light with a certain polarization state and transmits light with other polarization states. Therefore, part of the background light on the back side (opposite the exit side) of the optical member transmits through the polarizing element and reaches the user side. Therefore, the user sees the background and the image projected by the display element superimposed on each other.
[0030] As the polarizing element, a circular polarizing plate may be used when the output diffraction element selectively diffracts circularly polarized light, an elliptical polarizing plate may be used when the output diffraction element selectively diffracts elliptically polarized light, or a linear polarizing plate may be used when the output diffraction element selectively diffracts linearly polarized light. Furthermore, for example, even when the output diffraction element selectively diffracts circularly polarized light, the polarization state of the circularly polarized light may be destroyed while being guided through the light guide plate, and the light may become elliptically polarized light. Therefore, when the output diffraction element selectively diffracts circularly polarized light, an elliptically polarizing plate may be used.
[0031] Furthermore, the polarizing element may be disposed so as to overlap at least a portion of the output diffraction element when viewed from a direction perpendicular to the main surface of the light guide plate, but is preferably disposed so as to cover the entire surface as shown in FIG.
[0032] 1, the polarizing element 26 is configured to be spaced apart from the light guide element 14, but this is not limiting, and the polarizing element 26 may be in contact with the light guide element 14. From the viewpoint of the brightness of the displayed image, it is preferable that the polarizing element 26 is spaced apart from the light guide element 14. In general, the refractive index of the polarizing element 26 is higher than that of air and is close to that of the light guide element 14. Therefore, when the polarizing element 26 and the light guide element 14 are in contact with each other, when a part of the light guided in the light guide plate 16 reaches the interface with the polarizing element 26 directly before entering the output diffraction element 24, or when the light reaches the interface with the polarizing element 26 without being diffracted even after entering the output diffraction element 24, the light is not totally reflected at the interface with the polarizing element 26 and is absorbed. Therefore, the amount of light diffracted and emitted by the output diffraction element 24 is reduced, and the displayed image becomes dark. On the other hand, when the polarizing element 26 and the light guide element 14 are separated from each other, when the light not diffracted by the output diffraction element 24 reaches the interface with air, the light is totally reflected at the interface with air and guided through the light guide plate 16, and is eventually diffracted by the output diffraction element 24. Therefore, the amount of light diffracted and emitted by the output diffraction element 24 can be increased, and the displayed image can be brightened.
[0033] Here, in the example shown in FIG. 1, the light guide element of the optical member has a configuration including an incident diffraction element and an exit diffraction element, but this is not limited thereto, and the light guide element may further have an intermediate diffraction element.
[0034] 2 to 4 conceptually show another example of the image display device of the present invention using the optical member of the present invention. Fig. 2 is a top view, showing the image display device 10b as viewed from the top of the paper of Fig. 3. Fig. 3 is a front view, showing the image display device 10b as viewed from the side observed by a user U. Fig. 4 is a side view, showing the image display device 10b as viewed from the right hand side of the paper of Fig. 3.
[0035] 2 to 4 includes a display element 12, a light guide plate 16, a light guide element 14b having an input diffraction element 18, an intermediate diffraction element 20, and an output diffraction element 24 arranged on the main surface of the light guide plate 16, and an optical member 13b having a polarizing element 26. Note that the display element 12 is not shown in FIG.
[0036] 2 to 4, the entrance diffraction element 18, the intermediate diffraction element 20, and the exit diffraction element 24 are disposed at different positions in the planar direction of the main surface of the light guide plate 16. In the example shown in Fig. 3, the intermediate diffraction element 20 is disposed to the left of the entrance diffraction element 18 in Fig. 3, and the exit diffraction element 24 is disposed below the intermediate diffraction element 20 in Fig. 3. The display element 12 is disposed at a position overlapping with the incident diffraction element 18 in the planar direction of the main surface of the light guide plate 16, facing the surface of the light guide plate 16 opposite the side on which the incident diffraction element 18 is disposed.
[0037] In the image display device 10b, the image displayed by the display element 12 is incident on the light guide plate 16 in a direction perpendicular to the main surface and enters the incident diffraction element 18. The light incident on the incident diffraction element 18 is diffracted by the incident diffraction element 18 and enters the light guide plate 16. At that time, the incident diffraction element 18 diffracts the light at an angle at which the light is totally reflected within the light guide plate 16, and also diffracts the light so that the diffracted light travels in a direction toward the intermediate diffraction element 20. In the example shown in FIG. 3, the incident diffraction element 18 diffracts the incident light toward the left in FIG. 3.
[0038] The light diffracted by the input diffraction element 18 is totally reflected and propagates within the light guide plate 16, and is input to the intermediate diffraction element 20. The intermediate diffraction element 20 diffracts the light so that the traveling direction of the input light is toward the output diffraction element 24. In the example shown in Fig. 3, the intermediate diffraction element 20 diffracts the input light in the downward direction in Fig. 3.
[0039] The light diffracted by the intermediate diffraction element 20 is totally reflected and propagates within the light guide plate 16, and enters the exit diffraction element 24. The exit diffraction element 24 diffracts the incident light at an angle that deviates from the angle at which the light is totally reflected within the light guide plate 16. In the example shown in Fig. 3, the exit diffraction element 24 diffracts the incident light in a direction perpendicular to the paper surface of Fig. 3. That is, as shown in Fig. 2, the exit diffraction element 24 diffracts the incident light in a direction approximately perpendicular to the main surface of the light guide plate.
[0040] The light diffracted by the output diffraction element 24 is output from the light guide plate 16 toward the user U. In this way, the image display device 10b can display the image projected by the display element 12. Here, since the light guide element 14b has the intermediate diffraction element 20, when light is diffracted by the intermediate diffraction element 20, part of the light can be diffracted at a plurality of points of the intermediate diffraction element, thereby expanding the exit pupil.
[0041] Here, the optical member 13b has a polarizing element 26, similar to the optical member 13 shown in Fig. 1. In the example shown in Fig. 2, the polarizing element 26 is disposed on the opposite side of the output diffraction element 24 from the light guide plate 16 side. That is, the polarizing element 26 is disposed on the opposite side of the output diffraction element 24 from the output side. Moreover, the polarizing element 26 is disposed at a position overlapping with the output diffraction element 24 in the planar direction of the main surface of the light guide plate 16. As a result, the light L leaking to the opposite side to the output side of the output diffraction element 24 x It is possible to block the transmission of stray light L x It is also possible to prevent stray light from causing an image to be viewed by people other than the user.
[0042] In the example shown in FIG. 1, reflection type diffraction elements are used as the output diffraction element 24 and the input diffraction element 18, but the present invention is not limited to this, and transmission type diffraction elements may also be used.
[0043] FIG. 5 conceptually shows another example of an image display device using the optical member of the present invention. The image display device 10c shown in FIG. 5 includes a display element 12, a light guide plate 16, a light guide element 14c having an input diffraction element 18c and an output diffraction element 24c arranged on the main surface of the light guide plate 16, and an optical member 13c having a polarizing element 26.
[0044] In an image display device 10c shown in Fig. 5, an entrance diffraction element 18c and an exit diffraction element 24c are disposed at different positions in the planar direction of the main surface of the light guide plate 16. In the example shown in Fig. 5, the exit diffraction element 24c is disposed to the left of the entrance diffraction element 18c. The display element 12 is disposed facing the incident diffraction element 18 at a position overlapping the incident diffraction element 18 in the planar direction of the main surface of the light guide plate 16 .
[0045] 5, the input diffraction element 18c and the output diffraction element 24c are transmissive diffraction elements that diffract light while transmitting it, and the output diffraction element 24c is a polarizing diffraction element that selectively diffracts light in a predetermined polarization state.
[0046] In the image display device 10c, an image displayed by the display element 12 is incident on the input diffraction element 18 from a direction perpendicular to the main surface of the light guide plate 16. The input diffraction element 18c diffracts the incident light and makes it incident on the light guide plate 16. At that time, the input diffraction element 18c diffracts the light at an angle at which the light is totally reflected within the light guide plate 16, and also diffracts the light so that the diffracted light travels in a direction toward the output diffraction element 24c. In the example shown in FIG. 5, the input diffraction element 18c diffracts the incident light toward the left in FIG. 5.
[0047] The diffracted light by the input diffraction element 18c is totally reflected and propagates within the light guide plate 16, and enters the output diffraction element 24c. The output diffraction element 24c diffracts the incident light at an angle that deviates from the angle at which the light is totally reflected within the light guide plate 16. In the example shown in FIG. 5, the output diffraction element 24c diffracts the incident light toward the lower side in FIG. 5. That is, as shown in FIG. 5, the output diffraction element 24c diffracts the incident light in a direction substantially perpendicular to the main surface of the light guide plate.
[0048] The light diffracted by the output diffraction element 24c is output from the light guide plate 16 toward the user U. In this way, the image display device 10c can display the image projected by the display element 12.
[0049] Here, the optical member 13c has a polarizing element 26. In the example shown in Fig. 5, the polarizing element 26 is disposed on the side opposite to the output diffraction element 24c side of the light guide plate 16. That is, the polarizing element 26 is disposed on the side opposite to the output side with respect to the output diffraction element 24c. Moreover, the polarizing element 26 is disposed at a position overlapping with the output diffraction element 24c in the planar direction of the main surface of the light guide plate 16. As a result, the light L leaking to the opposite side to the output side of the output diffraction element 24c x It is possible to block the transmission of stray light L x It is also possible to prevent stray light from causing an image to be viewed by people other than the user.
[0050] Here, the incident diffraction element, the intermediate diffraction element, and the exit diffraction element may have a configuration having a liquid crystal layer having wavelength selectivity, as described later. That is, the incident diffraction element, the intermediate diffraction element, and the exit diffraction element may have wavelength selectivity. In this case, each diffraction element may have a configuration having one liquid crystal layer having wavelength selectivity, or may have two or more layers.
[0051] For example, the diffraction element may have two liquid crystal layers, one that selectively reflects red light and one that selectively reflects green light, or it may have three liquid crystal layers, one that selectively reflects red light, one that selectively reflects green light, and one that selectively reflects blue light.
[0052] In the case where the diffraction element has a configuration having multiple liquid crystal layers, for example, each liquid crystal layer can be configured to reflect three colors of light, namely red light, green light, and blue light, so that the light-guiding element can guide a color image. Also, for example, the diffraction element may have three liquid crystal layers with different selective reflection central wavelengths, and may be configured to reflect one or two colors selected from visible light such as red light, green light, and blue light, as well as infrared light and / or ultraviolet light, or may be configured to reflect only light other than visible light. Alternatively, the diffraction element may have two or four or more liquid crystal layers with different selective reflection central wavelengths. The diffraction element may be configured to reflect light other than visible light, such as infrared light and / or ultraviolet light, in addition to visible light, such as red light, green light, and blue light, or each liquid crystal layer may be configured to reflect light other than visible light, such as infrared light and / or ultraviolet light.
[0053] In the image display device, the optical member of the present invention may have two or more light guide elements. As an example, as conceptually shown in Fig. 6, an image display device 10d having an optical member 13e having two light guide elements 14d and 14e is illustrated. In this configuration, as an example, the optical member 13e has a light guide plate 16d, a light guide element 14d having an incident diffraction element 18d and an outgoing diffraction element 24d arranged on the main surface of the light guide plate 16d, a light guide element 14e having an incident diffraction element 18e and an outgoing diffraction element 24e arranged on the main surface of the light guide plate 16e, and a polarizing element 26e, in this order. The light guide element 14d and the light guide element 14e are arranged so that the light exit surface sides face the same direction. The polarizing element 26e is arranged on the surface side opposite to the exit side of the light guide element.
[0054] For example, in the image display device 10d, the light guide element 14d has a diffraction element that reflects green light, and the light guide element 14e has a diffraction element that reflects blue light. With this configuration, the image display device 10d can guide green light and blue light, respectively. At this time, stray light L leaking to the opposite side from the emission side by the emission diffraction elements of the light guide elements 14d and 14e is x is absorbed (or reflected) by the polarizing element 26e, thereby making it possible to prevent stray light from being emitted to the outside.
[0055] 6, the configuration has two optical members that respectively guide the green light and the blue light, but it may have three or more optical members. For example, it may have three optical members that respectively guide the red light, the green light, and the blue light.
[0056] Alternatively, the light emitting device may have a configuration having a plurality of optical members, with at least one optical member guiding light of two or more colors. For example, the light emitting device may have two optical members, with one optical member guiding two colors selected from red light, green light, and blue light, and the other optical member guiding light of the remaining color. The optical member may also be configured to guide light other than visible light (infrared or ultraviolet light).
[0057] Although not shown, the incident diffraction element, the intermediate diffraction element, and the exit diffraction element are each attached to the light guide plate by an attachment layer. In the present invention, the lamination layer can be a layer made of various known materials as long as it is a layer that can laminate objects to be laminated together. The lamination layer may be a layer made of an adhesive that has fluidity when laminated and then becomes solid, a layer made of a pressure-sensitive adhesive that is a soft solid in a gel (rubber) state when laminated and does not change its gel state afterwards, or a layer made of a material that has the characteristics of both an adhesive and a pressure-sensitive adhesive. Therefore, the lamination layer may be a known layer used for laminating sheet-like objects in optical devices and optical elements, such as an optically clear adhesive (OCA), an optically clear double-sided tape, and an ultraviolet curing resin.
[0058] Alternatively, instead of bonding with an adhesive layer, the incident diffraction element, intermediate diffraction element and exit diffraction element may be laminated with a light guide plate and held with a frame or a jig or the like to form the light guide element of the present invention.
[0059] Furthermore, the entrance diffraction element, the intermediate diffraction element and the exit diffraction element may be formed directly on the light guide plate.
[0060] Each component will be described below.
[0061] [Display element] The display element 12 displays an image (video) to be observed by the user U, and projects the image onto the incident diffraction element. Therefore, the display element 12 is disposed so that the image it projects is incident on the incident diffraction element.
[0062] In the image display device of the present invention, there is no limitation on the display element 12, and various known display elements (display devices, projectors) used in AR glasses etc. can be used. As an example of the display element 12, a display element having a display and a projection lens is exemplified.
[0063] In the image display device of the present invention, there is no limitation on the display, and for example, various known displays used in AR glasses and the like can be used. Examples of displays include liquid crystal displays (including LCOS: Liquid Crystal On Silicon, etc.), organic electroluminescence displays, and scanning displays using DLP (Digital Light Processing) and MEMS (Micro Electro Mechanical Systems) mirrors.
[0064] When the image display device is configured to display a multi-color image, a display capable of displaying a multi-color image is used. For example, as shown in FIG. 6, when a plurality of optical members are provided, a display is used that displays a multicolor image using light of a wavelength diffracted by each diffractive element of each optical member.
[0065] In the display element 12 used in the image display device of the present invention, the projection lens is also a known projection lens (collimator lens) used in AR glasses and the like.
[0066] Here, in the image display device of the present invention, the image displayed by the display element 12, that is, the light irradiated by the display element 12 is not limited, but unpolarized (natural light) or circularly polarized light is preferable. When the display element 12 irradiates circularly polarized light and the display irradiates an unpolarized image, the display element 12 preferably has a circular polarizing plate, for example, made of a linear polarizer and a λ / 4 plate. When the display irradiates a linearly polarized image, the display element 12 preferably has a λ / 4 plate, for example. The light emitted by the display element 12 may be other polarized light (for example, linearly polarized light, etc.).
[0067] [Light guide plate] In the light-guiding element 14, the light-guiding plate 16 is a known light-guiding plate that reflects and guides (propagates) light that has entered the interior. There are no limitations on the light guide plate 16, and various known light guide plates used in AR glasses, backlight units of liquid crystal displays, and the like can be used.
[0068] [Diffraction element] The incident diffraction element, the intermediate diffraction element, and the exit diffraction element can be polarized diffraction elements. In the following description, when it is not necessary to distinguish between these diffraction elements, they are collectively referred to as diffraction elements. Also, the incident diffraction element and the intermediate diffraction element can be a known diffraction element other than a polarized diffraction element.
[0069] [Polarizing Diffraction Element] A known polarizing diffraction element can be used as the polarizing diffraction element. The polarizing diffraction element is a diffraction element that controls the diffraction direction, polarization state, and diffracted light intensity of the emitted light according to the polarization state of the incident light by controlling the polarization state in a fine region. Examples of the polarizing diffraction element include a polarizing diffraction element having a diffraction structure formed using structural birefringence described in "Erez Hasman et al., Polarization dependent focusing lens by use of quantized Pancharatnm-Berry phase diffractive optics, Applied Physics Letters, Volume 82, Number 3 pp.328-330" and a polarizing diffraction element having a diffraction structure formed using a birefringent material described in Japanese Patent No. 5276847. The polarizing diffraction element is exemplified by a liquid crystal diffraction element that is formed using a composition containing a liquid crystal compound and has a liquid crystal orientation pattern in which the direction of the optical axis derived from the liquid crystal compound changes while continuously rotating along at least one direction in the plane. In addition, the liquid crystal diffraction element preferably has a cholesteric liquid crystal layer formed by fixing a cholesteric liquid crystal phase.
[0070] (Liquid crystal diffraction element A) An example of the liquid crystal diffraction element will be described with reference to FIGS. Fig. 7 is a schematic diagram showing the orientation state of liquid crystal compounds in the plane of the principal surface of the liquid crystal layer 34 of the liquid crystal diffraction element. Fig. 8 is a schematic cross-sectional view showing the state of the liquid crystal phase in a cross section perpendicular to the principal surface. In the following description, the principal surface of the liquid crystal layer 34 is the XY plane, and the cross section perpendicular to the XY plane is the XZ plane. That is, Fig. 7 corresponds to a schematic diagram of the XY plane of the liquid crystal layer 34, and Fig. 8 corresponds to a schematic diagram of the XZ plane of the liquid crystal layer 34. The liquid crystal layer shown in Figs. 7 and 8 is an example of a cholesteric liquid crystal layer in which the liquid crystal compound is cholesterically oriented. Also, it is an example in which the liquid crystal compound is a rod-shaped liquid crystal compound. The cholesteric liquid crystal layer reflects one circularly polarized light of the selective reflection wavelength and transmits light of another wavelength range and the other circularly polarized light. Therefore, a liquid crystal diffraction element having a cholesteric liquid crystal layer is a reflective liquid crystal diffraction element.
[0071] In the example shown in FIG. 8, the liquid crystal diffraction element has a support 30, an alignment film 32, and a liquid crystal layer . 8 has a support 30, an alignment film 32, and a liquid crystal layer 34, but the present invention is not limited thereto. The liquid crystal diffraction element may have only the alignment film 32 and the liquid crystal layer 34, after the support 30 is peeled off, for example, after being bonded to the light guide plate 16. Alternatively, the liquid crystal diffraction element may have only the liquid crystal layer 34, after the support 30 and the alignment film 32 are peeled off, for example, after being bonded to the light guide plate 16.
[0072] <Support> The support 30 supports an alignment film 32 and a liquid crystal layer 34 . The support 30 may be any type of sheet-like material (film, plate-like material) that can support the alignment film 32 and the liquid crystal layer . The support 30 preferably has a transmittance to the corresponding light of 50% or more, more preferably 70% or more, and even more preferably 85% or more.
[0073] There is no limitation on the thickness of the support 30, and the thickness capable of supporting the alignment film 32 and the liquid crystal layer 34 may be appropriately set depending on the application of the liquid crystal diffraction element and the material from which the support 30 is formed. The thickness of the support 30 is preferably from 1 to 2000 μm, more preferably from 3 to 500 μm, and further preferably from 5 to 250 μm.
[0074] The support 30 may be a single layer or multiple layers. Examples of the support 30 in the case of a single layer include support 30 made of glass, triacetyl cellulose (TAC), polyethylene terephthalate (PET), polycarbonate, polyvinyl chloride, acrylic, polyolefin, etc. Examples of the support 30 in the case of a multilayer include a support that includes any of the above-mentioned single-layer supports as a substrate, and another layer is provided on the surface of this substrate.
[0075] <Alignment film> In the liquid crystal diffraction element, an alignment film 32 is formed on the surface of a support 30 . The alignment film 32 is an alignment film for aligning the liquid crystal compound 40 in a predetermined liquid crystal alignment pattern when the liquid crystal layer 34 is formed. As will be described later, in the present invention, the liquid crystal layer 34 has a liquid crystal orientation pattern in which the direction of the optical axis 40A (see FIG. 7) derived from the liquid crystal compound 40 changes while continuously rotating along one direction in the plane. Therefore, the alignment film 32 is formed so that the liquid crystal layer 34 can form this liquid crystal orientation pattern. In the following description, "the orientation of the optical axis 40A rotates" will also be simply referred to as "the optical axis 40A rotates."
[0076] The alignment film 32 may be of any of various known types. Examples include rubbed films made of organic compounds such as polymers, obliquely evaporated films of inorganic compounds, films with microgrooves, and films formed by stacking LB (Langmuir-Blodgett) films made of organic compounds such as ω-tricosanoic acid, dioctadecylmethylammonium chloride, and methyl stearate using the Langmuir-Blodgett method.
[0077] The alignment film 32 formed by rubbing treatment can be formed by rubbing the surface of the polymer layer several times in a certain direction with paper or cloth. Preferred materials for use in the alignment film 32 include polyimide, polyvinyl alcohol, polymers having polymerizable groups as described in JP-A-9-152509, and materials used in forming the alignment films 32 described in JP-A-2005-97377, JP-A-2005-99228, and JP-A-2005-128503.
[0078] In a liquid crystal diffraction element, a so-called photo-alignment film, which is formed by irradiating a photo-alignable material with polarized or non-polarized light to form the alignment film 32, is preferably used as the alignment film 32. That is, in a liquid crystal diffraction element, a photo-alignment film formed by applying a photo-alignment material onto the support 30 is preferably used as the alignment film 32. The photo-alignment film can be irradiated with polarized light from a vertical direction or an oblique direction, while the photo-alignment film can be irradiated with unpolarized light from an oblique direction.
[0079] Examples of photo-alignment materials used in the alignment film that can be used in the present invention include those described in JP-A-2006-285197, JP-A-2007-76839, JP-A-2007-138138, JP-A-2007-94071, JP-A-2007-121721, JP-A-2007-140465, JP-A-2007-156439, and JP-A-2007 azo compounds described in JP-A-133184, JP-A-2009-109831, JP-A-3883848 and JP-A-4151746; aromatic ester compounds described in JP-A-2002-229039; maleimides having photo-orientable units described in JP-A-2002-265541 and JP-A-2002-317013; / or alkenyl-substituted nadimide compounds, photocrosslinkable silane derivatives described in Japanese Patent No. 4205195 and Japanese Patent No. 4205198, photocrosslinkable polyimides, photocrosslinkable polyamides and photocrosslinkable polyesters described in JP-T-2003-520878, JP-T-2004-529220 and Japanese Patent No. 4162850, and photodimerizable compounds described in JP-A-9-118717, JP-T-10-506420, JP-T-2003-505561, WO 2010 / 150748, JP-A-2013-177561 and JP-A-2014-12823, particularly cinnamate compounds, chalcone compounds and coumarin compounds, etc. are exemplified as preferred examples. Among these, azo compounds, photocrosslinkable polyimides, photocrosslinkable polyamides, photocrosslinkable polyesters, cinnamate compounds, and chalcone compounds are preferably used.
[0080] There is no limitation on the thickness of the alignment film 32, and the thickness may be appropriately set so as to obtain the necessary alignment function depending on the material from which the alignment film 32 is formed. The thickness of the alignment film 32 is preferably 0.01 to 5 μm, and more preferably 0.05 to 2 μm.
[0081] There is no limitation on the method for forming the alignment film 32, and various known methods can be used depending on the material for forming the alignment film 32. As an example, there is a method in which the alignment film 32 is applied to the surface of the support 30 and dried, and then the alignment film 32 is exposed to laser light to form an alignment pattern.
[0082] FIG. 13 conceptually shows an example of an exposure apparatus for exposing the alignment film 32 to light to form an alignment pattern. The exposure device 60 shown in Figure 13 includes a light source 64 equipped with a laser 62, a λ / 2 plate 65 that changes the polarization direction of laser light M emitted by the laser 62, a polarizing beam splitter 68 that splits the laser light M emitted by the laser 62 into two light beams MA and MB, mirrors 70A and 70B that are respectively arranged on the optical paths of the two split light beams MA and MB, and λ / 4 plates 72A and 72B. The light source 64 emits linearly polarized light P0. The λ / 4 plate 72A converts the linearly polarized light P0 (light beam MA) into right-handed circularly polarized light P R The λ / 4 plate 72B converts the linearly polarized light P0 (light beam MB) into left-handed circularly polarized light P L , respectively.
[0083] A support 30 having an alignment film 32 before an alignment pattern is formed is placed in an exposure section, and two light beams MA and MB are caused to intersect and interfere on the alignment film 32, and the alignment film 32 is exposed by being irradiated with the interference light. Due to the interference at this time, the polarization state of the light irradiated to the alignment film 32 changes periodically in the form of interference fringes, thereby obtaining an alignment film having an alignment pattern in which the alignment state changes periodically (hereinafter also referred to as a pattern alignment film). In the exposure device 60, the period of the alignment pattern can be adjusted by changing the crossing angle α of the two light beams MA and MB. That is, in the exposure device 60, in an alignment pattern in which the optical axis 40A derived from the liquid crystal compound 40 continuously rotates along one direction, the length of one period in which the optical axis 40A rotates by 180° in one direction in which the optical axis 40A rotates can be adjusted by adjusting the crossing angle α. By forming a cholesteric liquid crystal layer on the alignment film 32 having an alignment pattern in which the alignment state changes periodically, a liquid crystal layer 34 can be formed having a liquid crystal alignment pattern in which the optical axis 40A derived from the liquid crystal compound 40 rotates continuously along one direction, as described below. Moreover, by rotating the optical axes of the λ / 4 plates 72A and 72B by 90°, respectively, the rotation direction of the optical axis 40A can be reversed.
[0084] As described above, the patterned alignment film has an alignment pattern that aligns the liquid crystal compound so that the direction of the optical axis of the liquid crystal compound in the liquid crystal layer formed on the patterned alignment film changes while continuously rotating along at least one direction in the plane. If the axis along which the patterned alignment film aligns the liquid crystal compound is defined as the alignment axis, the patterned alignment film can be said to have an alignment pattern in which the direction of the alignment axis changes while continuously rotating along at least one direction in the plane. The alignment axis of the patterned alignment film can be detected by measuring the absorption anisotropy. For example, when the patterned alignment film is irradiated with linearly polarized light while rotating and the amount of light transmitted through the patterned alignment film is measured, the direction in which the amount of light is maximum or minimum is observed to change gradually along one direction in the plane.
[0085] In the present invention, the alignment film 32 is provided as a preferred embodiment, but is not an essential component. For example, by forming an alignment pattern on the support 30 by a method of subjecting the support 30 to a rubbing treatment, a method of processing the support 30 with laser light, or the like, it is possible to configure the liquid crystal layer to have a liquid crystal alignment pattern in which the direction of the optical axis 40A derived from the liquid crystal compound 40 changes while continuously rotating along at least one direction in the plane. That is, in the present invention, the support 30 may act as an alignment film.
[0086] <Liquid crystal layer> In the liquid crystal diffraction element, a liquid crystal layer 34 is formed on the surface of an alignment film 32 . As described above, the liquid crystal layer is a cholesteric liquid crystal layer having a fixed cholesteric liquid crystal phase, and has a liquid crystal orientation pattern in which the direction of the optical axis derived from the liquid crystal compound changes while continuously rotating along at least one direction in the plane.
[0087] As conceptually shown in FIG. 8, the liquid crystal layer 34 has a helical structure in which liquid crystal compounds 40 are spirally stacked, similar to a cholesteric liquid crystal layer formed by fixing a normal cholesteric liquid crystal phase, and has a structure in which liquid crystal compounds 40 spirally spirally spirally stacked at multiple pitches, with one helical pitch being one rotation (360° rotation) of the liquid crystal compounds 40.
[0088] As is well known, a cholesteric liquid crystal layer formed by fixing a cholesteric liquid crystal phase has wavelength selective reflectivity. As will be described in detail later, the selective reflection wavelength range of the cholesteric liquid crystal layer depends on the length of one pitch of the helix described above (pitch P shown in FIG. 9).
[0089] Therefore, a diffraction element having such a liquid crystal layer has wavelength selectivity and diffracts light of a specific wavelength. Therefore, the wavelength of light reflected (diffracted) by the diffraction element can be appropriately set by adjusting the helical pitch P of the liquid crystal layer to appropriately set the selective reflection wavelength range of the liquid crystal layer.
[0090] 7, in the XY plane of the liquid crystal layer 34, the liquid crystal compounds 40 are aligned along a plurality of alignment axes D parallel to each other in the XY plane, and on each alignment axis D, the direction of the optical axis 40A of the liquid crystal compounds 40 changes while continuously rotating in one direction in the plane along the alignment axis D. For the sake of explanation, it is assumed that the alignment axis D is oriented in the X direction. In addition, in the Y direction, the liquid crystal compounds 40 having the same direction of the optical axis 40A are aligned at equal intervals. Here, "the orientation of the optical axis 40A of the liquid crystal compound 40 changes while continuously rotating in one direction in the plane along the arrangement axis D" means that the angle between the optical axis 40A of the liquid crystal compound 40 and the arrangement axis D varies depending on the position along the arrangement axis D, and the angle between the optical axis 40A and the arrangement axis D gradually changes from θ to θ+180° or θ-180° along the arrangement axis D. In other words, the optical axes 40A of the multiple liquid crystal compounds 40 aligned along the arrangement axis D change while rotating at a constant angle along the arrangement axis D, as shown in FIG. The difference in angle between the optical axes 40A of the liquid crystal compounds 40 adjacent to each other in the direction of the alignment axis D is preferably 45° or less, more preferably 15° or less, and even more preferably a smaller angle. In addition, in this specification, when the liquid crystal compound 40 is a rod-shaped liquid crystal compound, the optical axis 40A of the liquid crystal compound 40 refers to the molecular long axis of the rod-shaped liquid crystal compound. On the other hand, when the liquid crystal compound 40 is a discotic liquid crystal compound, the optical axis 40A of the liquid crystal compound 40 refers to the axis parallel to the normal direction to the disc surface of the discotic liquid crystal compound.
[0091] In the liquid crystal layer 34, in the liquid crystal orientation pattern of such liquid crystal compound 40, the length (distance) over which the optical axis 40A of the liquid crystal compound 40 rotates 180° in the direction of the alignment axis D along which the optical axis 40A continuously rotates and changes in the plane is defined as the length Λ of one period of the liquid crystal orientation pattern. That is, the length Λ of one period is defined as the distance between the centers in the direction of the arrangement axis D of two liquid crystal compounds 40 that are at the same angle with respect to the direction of the arrangement axis D. Specifically, as shown in Fig. 7, the length Λ of one period is defined as the distance between the centers in the direction of the arrangement axis D of two liquid crystal compounds 40 whose directions of the arrangement axis D and the optical axes 40A coincide with each other. In the following description, this length Λ of one period is also referred to as "one period Λ". The liquid crystal alignment pattern of the liquid crystal layer 34 repeats this one period Λ in the direction of the arrangement axis D, that is, in one direction in which the direction of the optical axis 40A changes by continuously rotating.
[0092] On the other hand, the liquid crystal compound 40 forming the liquid crystal layer 34 has the same orientation of the optical axis 40A in a direction perpendicular to the direction of the alignment axis D (Y direction in Figure 7), i.e., in the Y direction perpendicular to the direction in which the optical axis 40A continuously rotates. In other words, in the liquid crystal compound 40 forming the liquid crystal layer 34, the angle between the optical axis 40A of the liquid crystal compound 40 and the direction of the alignment axis D is equal in the Y direction.
[0093] When the XZ plane of the liquid crystal layer 34 shown in Fig. 8 is observed with a SEM (scanning electron microscope), a striped pattern is observed in which the arrangement direction of the alternating bright portions 42 and dark portions 44 as shown in Fig. 9 is inclined at a predetermined angle with respect to the main surface (XY plane). In such an SEM cross section, the distance in the normal direction between adjacent bright portions 42 and 42 or between adjacent dark portions 44 and 44 corresponds to 1 / 2 pitch. That is, as shown by P in Fig. 9, two bright portions 42 and two dark portions 44 correspond to one pitch of the spiral (one winding of the spiral).
[0094] The effect of diffraction by the liquid crystal layer will now be described. In a conventional cholesteric liquid crystal layer, the helical axis derived from the cholesteric liquid crystal phase is perpendicular to the main surface (XY plane), and the reflection surface is parallel to the main surface (XY plane). In addition, the optical axis of the liquid crystal compound is not tilted with respect to the main surface (XY plane). In other words, the optical axis is parallel to the main surface (XY plane). Therefore, when the XZ plane of a conventional cholesteric liquid crystal layer is observed with an SEM, the alignment direction in which light and dark areas are alternately arranged is perpendicular to the main surface (XY plane). Since the cholesteric liquid crystal phase has specular reflectivity, for example, when light is incident on a cholesteric liquid crystal layer from the normal direction, the light is reflected in the normal direction.
[0095] In contrast, the liquid crystal layer 34 reflects the incident light with an inclination toward the direction of the arrangement axis D with respect to the specular reflection. The liquid crystal layer 34 has a liquid crystal orientation pattern in which the optical axis 40A changes while continuously rotating in the plane along the direction of the arrangement axis D (a predetermined direction). The following will be described with reference to FIG. 10.
[0096] As an example, the liquid crystal layer 34 is configured to polarize right-handed circularly polarized red light R R Therefore, when light is incident on the liquid crystal layer 34, the liquid crystal layer 34 selectively reflects right-handed circularly polarized red light R R It reflects only light and transmits all other light.
[0097] In the liquid crystal layer 34, the optical axis 40A of the liquid crystal compound 40 changes while rotating along the direction of the alignment axis D (one direction). The liquid crystal alignment pattern formed in the liquid crystal layer 34 is a periodic pattern along the alignment axis D. Therefore, the right-handed circularly polarized light R of the red light incident on the liquid crystal layer 34 is R As conceptually shown in Figure 10, the right-handed circularly polarized light R of the reflected red light is reflected (diffracted) in a direction according to the period of the liquid crystal orientation pattern. R is reflected (diffracted) in a direction inclined toward the alignment axis D direction with respect to the XY plane (the main surface of the cholesteric liquid crystal layer).
[0098] As a result, when the liquid crystal layer 34 is applied to a light guide element or the like, it can reflect (diffract) light incident from a direction perpendicular to the main surface of the light guide plate at an angle that causes total reflection within the light guide plate, and can also be used as a diffraction element that can reflect (diffract) light that is guided by total reflection within the light guide plate in a direction perpendicular to the main surface of the light guide plate.
[0099] In the liquid crystal layer 34, the direction of the arrangement axis D, which is one direction in which the optical axis 40A rotates, can be appropriately set to adjust the reflection direction (diffraction angle) of light.
[0100] When circularly polarized light of the same wavelength and rotation direction is reflected, the reflection direction of the circularly polarized light can be reversed by reversing the rotation direction of the optical axis 40A of the liquid crystal compound 40 facing the alignment axis D. For example, in Figures 7 and 8, the rotation direction of the optical axis 40A toward the array axis D is clockwise, and some circularly polarized light is reflected with an inclination toward the array axis D, but by changing this to counterclockwise, some circularly polarized light is reflected with an inclination in the opposite direction to the array axis D.
[0101] Furthermore, in liquid crystal layers having the same liquid crystal orientation pattern, the reflection direction is reversed depending on the helical rotation direction of the liquid crystal compound 40, that is, the rotation direction of the reflected circularly polarized light. For example, when the direction of rotation of the helix is right-twisted, right-handed circularly polarized light is selectively reflected, and by having a liquid crystal orientation pattern in which the optical axis 40A rotates clockwise along the direction of the array axis D, right-handed circularly polarized light is reflected at an inclination toward the direction of the array axis D. Furthermore, for example, when the direction of rotation of the helix is left twisted, left-handed circularly polarized light is selectively reflected, and a liquid crystal layer having a liquid crystal orientation pattern in which the optical axis 40A rotates clockwise along the direction of the arrangement axis D reflects left-handed circularly polarized light tilted in the direction opposite to the direction of the arrangement axis D.
[0102] In the liquid crystal layer, in the liquid crystal orientation pattern of the liquid crystal compound, the length over which the optical axis of the liquid crystal compound rotates 180° is one period Λ of the diffraction structure, and the direction in which the optical axis of the liquid crystal compound changes while rotating (the direction of the alignment axis D) is the periodic direction of the diffraction structure.
[0103] In a liquid crystal layer having a liquid crystal orientation pattern, the shorter the period Λ, the larger the angle of the reflected light with respect to the incident light. In other words, the shorter the period Λ, the more the reflected light can be reflected at a greater inclination with respect to the incident light. Therefore, the period of the liquid crystal orientation pattern in the liquid crystal layer of each diffraction element can be appropriately set according to the diffraction angle, arrangement, etc. of each diffraction element. The period (one period Λ) of the diffractive structure of these diffractive elements is preferably 0.1 μm to 10 μm, more preferably 0.1 μm to 1 μm, and even more preferably 0.1 μm to 0.8 μm, and from the viewpoint of propagating light through the light guide plate 16 by total reflection, is even more preferably equal to or less than the wavelength λ of the incident light.
[0104] In addition, the liquid crystal layer of the incident diffraction element, the liquid crystal layer of the intermediate diffraction element, and the liquid crystal layer of the exit diffraction element, which diffract light of the same wavelength, have the same rotation direction of the helical twist of the cholesteric liquid crystal phase. On the other hand, the liquid crystal layers diffracting light of the same wavelength may have the same or different rotation directions of the helical twist of the cholesteric liquid crystal phase. That is, for example, as in the example shown in FIG. 6, when there are two optical members that guide different colors, the rotation direction of the helical twist of the liquid crystal layer of the diffraction element of one optical member 13d may be the same or different from the rotation direction of the helical twist of the liquid crystal layer of the diffraction element of the other optical member 13e.
[0105] 8, the liquid crystal compound 40 is configured such that its optical axis 40A is aligned parallel to the main surface (XY surface) in the XZ surface of the liquid crystal layer 34, but is not limited thereto. For example, as shown in FIG 11, the liquid crystal compound 40 may be configured such that its optical axis 40A is aligned at an angle to the main surface (XY surface) in the XZ surface of the liquid crystal layer 34.
[0106] 11, the inclination angle (tilt angle) of the liquid crystal compound 40 with respect to the principal surface (XY plane) in the XZ plane of the liquid crystal layer 34 is uniform in the thickness direction (Z direction), but is not limited thereto. The liquid crystal layer 34 may have a region in which the tilt angle of the liquid crystal compound 40 varies in the thickness direction. For example, in the example shown in FIG. 12, the optical axis 40A of the liquid crystal compound 40 at the interface on the alignment film 32 side of the liquid crystal layer is parallel to the main surface (the pretilt angle is 0), and the tilt angle of the liquid crystal compound 40 increases with increasing distance in the thickness direction from the interface on the alignment film 32 side, and thereafter, the liquid crystal compound is oriented at a constant tilt angle up to the other interface (air interface).
[0107] In this way, the liquid crystal layer may have a configuration in which the optical axis of the liquid crystal compound has a pretilt angle at one of the upper and lower interfaces, or may have pretilt angles at both interfaces, or the pretilt angles may be different at both interfaces. When the liquid crystal compound has a tilt angle (is inclined) in this way, the effective birefringence of the liquid crystal compound increases when light is diffracted, and the diffraction efficiency can be improved.
[0108] The average angle (average tilt angle) between the optical axis 40A of the liquid crystal compound 40 and the principal surface (XY plane) is preferably 5 to 80°, more preferably 10 to 50°. The average tilt angle can be measured by observing the XZ plane of the liquid crystal layer 34 with a polarizing microscope. In particular, in the XZ plane of the liquid crystal layer 34, the optical axis 40A of the liquid crystal compound 40 is preferably tilted in the same direction with respect to the principal surface (XY plane). The tilt angle is an arithmetic average of angles between the optical axis 40A of the liquid crystal compound 40 and the principal surface measured at any five or more points in a cross section of the cholesteric liquid crystal layer observed under a polarizing microscope.
[0109] Light that is perpendicularly incident on the diffraction element (liquid crystal layer) travels obliquely within the liquid crystal layer due to the bending force acting on it. As the light travels within the liquid crystal layer, a deviation occurs from the conditions, such as the diffraction period, that are set to obtain the desired diffraction angle for perpendicular incidence, resulting in diffraction loss. When a liquid crystal compound is tilted, there exists a direction in which a higher birefringence occurs with respect to the direction in which light is diffracted, compared to when it is not tilted. In this direction, the effective extraordinary refractive index becomes larger, and therefore the birefringence, which is the difference between the extraordinary refractive index and the ordinary refractive index, becomes higher. By setting the tilt angle direction in accordance with the desired diffraction direction, it is possible to suppress deviation from the original diffraction conditions at that direction. As a result, it is believed that a higher diffraction efficiency can be obtained when using a liquid crystal compound with a tilt angle.
[0110] In addition, it is desirable to control the tilt angle by treating the interface of the liquid crystal layer. At the interface on the support side, the tilt angle of the liquid crystal compound can be controlled by performing a pretilt treatment on the alignment film. For example, when forming the alignment film, the alignment film is exposed to ultraviolet light from the front and then obliquely exposed, so that a pretilt angle can be generated in the liquid crystal compound in the liquid crystal layer formed on the alignment film. In this case, the liquid crystal compound is pretilted in the direction in which the single axis side is visible with respect to the second irradiation direction. However, since the liquid crystal compound in the direction perpendicular to the second irradiation direction does not pretilt, there are regions in the plane that are pretilted and regions that are not pretilted. This contributes to increasing the birefringence in the desired direction when diffracting light in that direction, and is therefore suitable for increasing diffraction efficiency. Furthermore, an additive that promotes the pretilt angle can be added to the liquid crystal layer or the alignment film, in which case the additive can be used as a factor for further increasing the diffraction efficiency. This additive can also be used to control the pretilt angle of the air-side interface.
[0111] Here, in the cross section of the liquid crystal layer observed by SEM, the bright and dark areas derived from the cholesteric liquid crystal phase are inclined with respect to the main surface. When the in-plane retardation Re of the liquid crystal layer is measured from the normal direction and the direction inclined with respect to the normal, it is preferable that the direction in which the in-plane retardation Re is minimum is inclined with respect to the normal direction in either the slow axis plane or the fast axis plane. Specifically, it is preferable that the absolute value of the measurement angle between the normal line and the direction in which the in-plane retardation Re is minimum is 5° or more. In other words, it is preferable that the liquid crystal compound of the liquid crystal layer is inclined with respect to the main surface, and the inclination direction approximately coincides with the bright and dark areas of the liquid crystal layer. The normal direction is a direction perpendicular to the main surface. The liquid crystal layer having such a configuration can diffract circularly polarized light with higher diffraction efficiency than a liquid crystal layer in which the liquid crystal compound is parallel to the main surface.
[0112] In a configuration in which the liquid crystal compound of the liquid crystal layer is tilted with respect to the main surface and the tilt direction is approximately the same as the light and dark areas, the light and dark areas corresponding to the reflecting surface are aligned with the optical axis of the liquid crystal compound. Therefore, the effect of the liquid crystal compound on the reflection (diffraction) of light is increased, and the diffraction efficiency can be improved. As a result, the amount of reflected light relative to the incident light can be further improved.
[0113] In the fast axis plane or slow axis plane of the liquid crystal layer, the absolute value of the optical axis tilt angle of the liquid crystal layer is preferably 5° or more, more preferably 15° or more, and even more preferably 20° or more. By setting the absolute value of the optical axis tilt angle to 15° or more, it is possible to more suitably match the directions of the liquid crystal compounds with the light and dark areas, which is preferable in terms of improving the diffraction efficiency.
[0114] <<Method of forming liquid crystal layer>> The liquid crystal layer can be formed by fixing a liquid crystal phase in a layer shape, in which liquid crystal compounds are aligned in a predetermined orientation state. For example, in the case of a cholesteric liquid crystal layer, the liquid crystal layer can be formed by fixing a cholesteric liquid crystal phase in a layer shape. The structure with the fixed liquid crystal phase may be any structure in which the orientation of the liquid crystal compound in the liquid crystal phase is maintained, and typically, a structure is preferred in which a polymerizable liquid crystal compound is brought into a predetermined liquid crystal phase orientation state, and then polymerized and hardened by ultraviolet light irradiation, heating, etc. to form a layer with no fluidity, and at the same time, the structure is changed to a state in which the orientation form does not change due to an external field or external force. In the structure in which the liquid crystal phase is fixed, it is sufficient that the optical properties of the liquid crystal phase are maintained, and the liquid crystal compound 40 does not need to exhibit liquid crystallinity in the liquid crystal layer. For example, the polymerizable liquid crystal compound may be polymerized by a curing reaction and lose its liquid crystallinity.
[0115] An example of a material used to form the liquid crystal layer is a liquid crystal composition containing a liquid crystal compound, which is preferably a polymerizable liquid crystal compound. The liquid crystal composition used to form the liquid crystal layer may further contain a surfactant and a chiral agent.
[0116] --Polymerizable liquid crystal compound-- The polymerizable liquid crystal compound may be a rod-shaped liquid crystal compound or a discotic liquid crystal compound. Examples of rod-shaped polymerizable liquid crystal compounds include rod-shaped nematic liquid crystal compounds.As rod-shaped nematic liquid crystal compounds, azomethines, azoxys, cyanobiphenyls, cyanophenyl esters, benzoates, cyclohexane carboxylic acid phenyl esters, cyanophenylcyclohexanes, cyano-substituted phenylpyrimidines, alkoxy-substituted phenylpyrimidines, phenyldioxanes, tolanes, and alkenylcyclohexylbenzonitriles are preferably used.Not only low molecular weight liquid crystal compounds but also high molecular weight liquid crystal compounds can be used.
[0117] The polymerizable liquid crystal compound is obtained by introducing a polymerizable group into a liquid crystal compound. Examples of the polymerizable group include an unsaturated polymerizable group, an epoxy group, and an aziridinyl group, and an unsaturated polymerizable group is preferable, and an ethylenically unsaturated polymerizable group is more preferable. The polymerizable group can be introduced into the molecule of the liquid crystal compound by various methods. The number of polymerizable groups that the polymerizable liquid crystal compound has is preferably 1 to 6, more preferably 1 to 3. Examples of the polymerizable liquid crystal compound include compounds described in Makromol.Chem., Vol. 190, p. 2255 (1989), Advanced Materials, Vol. 5, p. 107 (1993), U.S. Pat. No. 4,683,327, U.S. Pat. No. 5,622,648, U.S. Pat. No. 5,770,107, International Publication No. 95 / 22586, International Publication No. 95 / 24455, International Publication No. 97 / 00600, International Publication No. 98 / 23580, International Publication No. 98 / 52905, JP-A-1-272551, JP-A-6-16616, JP-A-7-110469, JP-A-11-80081, and JP-A-2001-328973. Two or more polymerizable liquid crystal compounds may be used in combination. The alignment temperature can be lowered by using two or more kinds of polymerizable liquid crystal compounds in combination.
[0118] As other polymerizable liquid crystal compounds, a cyclic organopolysiloxane compound having a cholesteric phase as disclosed in JP-A-57-165480 can be used. As the above-mentioned polymer liquid crystal compounds, a polymer having a mesogen group exhibiting liquid crystal property introduced into the main chain, the side chain, or both the main chain and the side chain, a polymer cholesteric liquid crystal having a cholesteryl group introduced into the side chain, a liquid crystal polymer as disclosed in JP-A-9-133810, and a liquid crystal polymer as disclosed in JP-A-11-293252 can be used.
[0119] --Discoid Liquid Crystal Compounds-- As the discotic liquid crystal compound, for example, those described in JP-A-2007-108732 and JP-A-2010-244038 can be preferably used.
[0120] Furthermore, the amount of the polymerizable liquid crystal compound added in the liquid crystal composition is preferably 75 to 99.9 mass %, more preferably 80 to 99 mass %, and even more preferably 85 to 90 mass %, based on the solid content mass (mass excluding the solvent) of the liquid crystal composition.
[0121] --Surfactant-- The liquid crystal composition used in forming the liquid crystal layer may contain a surfactant. The surfactant is preferably a compound that can function as an alignment control agent that contributes to the alignment of the cholesteric liquid crystal phase stably or quickly. Examples of the surfactant include silicone surfactants and fluorine surfactants, and fluorine surfactants are preferred.
[0122] Specific examples of surfactants include the compounds described in paragraphs
[0082] to
[0090] of JP-A-2014-119605, the compounds described in paragraphs
[0031] to
[0034] of JP-A-2012-203237, the compounds exemplified in paragraphs
[0092] and
[0093] of JP-A-2005-99248, the compounds exemplified in paragraphs
[0076] to
[0078] and paragraphs
[0082] to
[0085] of JP-A-2002-129162, and the fluorine (meth)acrylate polymers described in paragraphs
[0018] to
[0043] of JP-A-2007-272185, etc. The surfactant may be used alone or in combination of two or more kinds. As the fluorine-based surfactant, the compounds described in paragraphs
[0082] to
[0090] of JP2014-119605A are preferred.
[0123] The amount of the surfactant added in the liquid crystal composition is preferably 0.01 to 10% by mass, more preferably 0.01 to 5% by mass, and further preferably 0.02 to 1% by mass, based on the total mass of the liquid crystal compound.
[0124] --Chiral agents (optically active compounds)-- Chiral agents have the function of inducing a helical structure in the cholesteric liquid crystal phase. Chiral agents can be selected according to the purpose, since the twist direction or pitch of the helix induced varies depending on the compound. The chiral agent is not particularly limited, and known compounds (for example, those described in Liquid Crystal Device Handbook, Chapter 3, Section 4-3, Chiral Agents for TN (twisted nematic) and STN (Super Twisted Nematic), p. 199, edited by the 142nd Committee of the Japan Society for the Promotion of Science, 1989), isosorbide, and isomannide derivatives can be used. Although the chiral agent generally contains an asymmetric carbon atom, an axially asymmetric compound or a planarly asymmetric compound that does not contain an asymmetric carbon atom can also be used as the chiral agent. Examples of the axially asymmetric compound or the planarly asymmetric compound include binaphthyl, helicene, paracyclophane, and derivatives thereof. The chiral agent may have a polymerizable group. When both the chiral agent and the liquid crystal compound have a polymerizable group, a polymer having a repeating unit derived from the polymerizable liquid crystal compound and a repeating unit derived from the chiral agent can be formed by a polymerization reaction between the polymerizable chiral agent and the polymerizable liquid crystal compound. In this embodiment, the polymerizable group of the polymerizable chiral agent is preferably the same type of group as the polymerizable group of the polymerizable liquid crystal compound. Therefore, the polymerizable group of the chiral agent is also preferably an unsaturated polymerizable group, an epoxy group, or an aziridinyl group, more preferably an unsaturated polymerizable group, and even more preferably an ethylenically unsaturated polymerizable group. The chiral agent may also be a liquid crystal compound.
[0125] When the chiral agent has a photoisomerizable group, it is preferable because a pattern of a desired reflection wavelength corresponding to the emission wavelength can be formed by irradiating a photomask with actinic rays or the like after coating and alignment. As the photoisomerizable group, an isomerization site of a compound exhibiting photochromic properties, an azo group, an azoxy group, or a cinnamoyl group is preferable. Specific compounds that can be used include those described in JP-A-2002-80478, JP-A-2002-80851, JP-A-2002-179668, JP-A-2002-179669, JP-A-2002-179670, JP-A-2002-179681, JP-A-2002-179682, JP-A-2002-338575, JP-A-2002-338668, JP-A-2003-313189, and JP-A-2003-313292.
[0126] The content of the chiral dopant in the liquid crystal composition is preferably 0.01 to 200 mol %, more preferably 1 to 30 mol %, based on the molar amount of the liquid crystal compound.
[0127] --Polymerization initiator-- When the liquid crystal composition contains a polymerizable compound, it preferably contains a polymerization initiator. In an embodiment in which the polymerization reaction is caused to proceed by ultraviolet irradiation, the polymerization initiator used is preferably a photopolymerization initiator capable of initiating the polymerization reaction by ultraviolet irradiation. Examples of the photopolymerization initiator include α-carbonyl compounds (described in U.S. Pat. Nos. 2,367,661 and 2,367,670), acyloin ethers (described in U.S. Pat. No. 2,448,828), α-hydrocarbon-substituted aromatic acyloin compounds (described in U.S. Pat. No. 2,722,512), polynuclear quinone compounds (described in U.S. Pat. Nos. 3,046,127 and 2,951,758), combinations of triarylimidazole dimers and p-aminophenyl ketones (described in U.S. Pat. No. 3,549,367), acridine and phenazine compounds (described in JP-A-60-105,667 and U.S. Pat. No. 4,239,850), and oxadiazole compounds (described in U.S. Pat. No. 4,212,970). The content of the photopolymerization initiator in the liquid crystal composition is preferably 0.1 to 20% by mass, and more preferably 0.5 to 12% by mass, based on the content of the liquid crystal compound.
[0128] --Crosslinking agent-- The liquid crystal composition may contain a crosslinking agent in order to improve the film strength and durability after curing. As the crosslinking agent, those which are cured by ultraviolet light, heat, moisture, etc. can be suitably used. The crosslinking agent is not particularly limited and can be appropriately selected according to the purpose. For example, polyfunctional acrylate compounds such as trimethylolpropane tri(meth)acrylate and pentaerythritol tri(meth)acrylate; epoxy compounds such as glycidyl (meth)acrylate and ethylene glycol diglycidyl ether; aziridine compounds such as 2,2-bishydroxymethylbutanol-tris[3-(1-aziridinyl)propionate] and 4,4-bis(ethyleneiminocarbonylamino)diphenylmethane; isocyanate compounds such as hexamethylene diisocyanate and biuret type isocyanate; polyoxazoline compounds having an oxazoline group in the side chain; and alkoxysilane compounds such as vinyltrimethoxysilane and N-(2-aminoethyl)3-aminopropyltrimethoxysilane. In addition, a known catalyst can be used according to the reactivity of the crosslinking agent, which can improve productivity in addition to improving film strength and durability. These may be used alone or in combination of two or more. The content of the crosslinking agent is preferably 3 to 20% by mass, more preferably 5 to 15% by mass, based on the solid content of the liquid crystal composition. When the content of the crosslinking agent is within the above range, the effect of improving the crosslinking density is easily obtained, and the stability of the liquid crystal phase is further improved.
[0129] --Other additives-- If necessary, a polymerization inhibitor, an antioxidant, an ultraviolet absorber, a light stabilizer, a colorant, metal oxide fine particles, etc. may be added to the liquid crystal composition within a range that does not deteriorate the optical performance, etc.
[0130] The liquid crystal composition is preferably used in the form of a liquid when forming a liquid crystal layer. The liquid crystal composition may contain a solvent. The solvent is not limited and can be appropriately selected depending on the purpose, but an organic solvent is preferable. The organic solvent is not limited and can be appropriately selected according to the purpose, and examples thereof include ketones, alkyl halides, amides, sulfoxides, heterocyclic compounds, hydrocarbons, esters, and ethers. These may be used alone or in combination of two or more. Among these, ketones are preferred when considering the burden on the environment.
[0131] When forming a liquid crystal layer, it is preferable to apply a liquid crystal composition to the surface on which the liquid crystal layer is to be formed, align the liquid crystal compound in a desired liquid crystal phase state, and then harden the liquid crystal compound to form a liquid crystal layer. That is, when forming a cholesteric liquid crystal layer on the alignment film 32, it is preferable to apply a liquid crystal composition to the alignment film 32, align the liquid crystal compound in a cholesteric liquid crystal phase state, and then harden the liquid crystal compound to form a liquid crystal layer in which the cholesteric liquid crystal phase is fixed. The liquid crystal composition can be applied by any known method capable of uniformly applying a liquid to a sheet-like material, such as printing methods including ink-jet printing and scroll printing, as well as spin coating, bar coating and spray coating.
[0132] The applied liquid crystal composition is dried and / or heated as necessary, and then cured to form a liquid crystal layer. In this drying and / or heating process, the liquid crystal compound in the liquid crystal composition may be aligned in a cholesteric liquid crystal phase. When heating is performed, the heating temperature is preferably 200° C. or less, more preferably 130° C. or less.
[0133] The aligned liquid crystal compound is further polymerized as necessary. The polymerization may be either thermal polymerization or photopolymerization by light irradiation, but photopolymerization is preferred. The light irradiation is preferably performed using ultraviolet light. The irradiation energy is 20 mJ / cm. 2 ~50J / cm 2 is preferable, and 50 to 1500 mJ / cm 2 In order to promote the photopolymerization reaction, the light irradiation may be performed under heating conditions or in a nitrogen atmosphere. The wavelength of the ultraviolet light to be irradiated is preferably 250 to 430 nm.
[0134] There is no restriction on the thickness of the liquid crystal layer, and the thickness that provides the required light reflectance can be set appropriately depending on the application of the diffraction element, the light reflectance required for the liquid crystal layer, and the material from which the liquid crystal layer is formed, etc.
[0135] (Liquid crystal diffraction element B) In the above examples, a liquid crystal layer in which a liquid crystal compound is cholesterically oriented is used as the liquid crystal diffraction element, but various types of liquid crystal diffraction elements can be used for the liquid crystal diffraction element used in the present invention as long as they have a liquid crystal orientation pattern in which the optical axis 40A derived from the liquid crystal compound 40 rotates continuously along at least one direction in the plane. In the present invention, a liquid crystal diffraction element can be used that has a liquid crystal orientation pattern that is continuously rotated along at least one direction in the plane, and in which the liquid crystal compound does not form a cholesteric liquid crystal phase in the thickness direction. Note that the liquid crystal diffraction element may have a configuration in which the liquid crystal compound is twisted and rotated in the thickness direction to such an extent that it does not form a cholesteric liquid crystal phase.
[0136] Another example of the liquid crystal diffraction element will be described with reference to FIGS. 14 and 15. FIG. The liquid crystal diffraction element shown in FIGS. 14 and 15 has a support 30, an alignment film 32, and a liquid crystal layer . Like the liquid crystal layer 34, the liquid crystal layer 36 of the liquid crystal diffraction element shown in Fig. 15 has a liquid crystal orientation pattern in which the optical axis 40A of the liquid crystal compound 40 rotates continuously along the direction of the arrangement axis D. Note that Fig. 15 also shows only the liquid crystal compound on the surface of the alignment film 32, like Fig. 7 described above. 14, the liquid crystal compound 40 forming the liquid crystal layer 36 is not helically twisted in the thickness direction, and the optical axis 40A is located at the same position in the plane direction. Such a liquid crystal layer can be formed by not adding a chiral agent to the liquid crystal composition in the formation of the liquid crystal layer described above.
[0137] As described above, the liquid crystal layer 36 has a liquid crystal alignment pattern in which the direction of the optical axis 40A derived from the liquid crystal compound 40 changes while continuously rotating in the direction of the alignment axis D, i.e., the direction indicated by the arrow D, within the plane. On the other hand, the liquid crystal compounds 40 forming the liquid crystal layer 36 are arranged at equal intervals in the Y direction perpendicular to the direction of the arrangement axis D, i.e., in the Y direction perpendicular to the one direction in which the optical axis 40A continuously rotates, with the liquid crystal compounds 40 having the same orientation of the optical axis 40A being aligned. In other words, in the liquid crystal compounds 40 forming the liquid crystal layer 36, the angles between the optical axes 40A and the alignment axis D direction are equal to each other among the liquid crystal compounds 40 aligned in the Y direction.
[0138] In the liquid crystal layer 36, the liquid crystal compounds aligned in the Y direction have the same angle between their optical axes 40A and the alignment axis D (one direction in which the optical axes of the liquid crystal compounds 40 rotate). A region in which the liquid crystal compounds 40, whose optical axes 40A and the alignment axis D form the same angle, are arranged in the Y direction, is referred to as Region R. In this case, the value of the in-plane retardation (Re) in each region R is preferably half the wavelength, i.e., λ / 2. These in-plane retardations are calculated by the product of the refractive index difference Δn associated with the refractive index anisotropy of the region R and the thickness of the optically anisotropic layer. Here, the refractive index difference associated with the refractive index anisotropy of the region R in the optically anisotropic layer is a refractive index difference defined by the difference between the refractive index in the direction of the slow axis in the plane of the region R and the refractive index in the direction perpendicular to the direction of the slow axis. That is, the refractive index difference Δn associated with the refractive index anisotropy of the region R is equal to the difference between the refractive index of the liquid crystal compound 40 in the direction of the optical axis 40A and the refractive index of the liquid crystal compound 40 in the direction perpendicular to the optical axis 40A in the plane of the region R. That is, the refractive index difference Δn is equal to the refractive index difference of the liquid crystal compound 40.
[0139] When circularly polarized light enters such a liquid crystal layer 36, the light is refracted and the direction of the circular polarization is changed. This effect is conceptually shown in Figures 16 and 17. In the liquid crystal layer 36, the product of the refractive index difference of the liquid crystal compound and the thickness of the optically anisotropic layer is assumed to be λ / 2. As shown in Figure 16, when the product of the refractive index difference of the liquid crystal compound in the liquid crystal layer 36 and the thickness of the optically anisotropic layer is λ / 2, when incident light L1 that is left-handed circularly polarized light is incident on the liquid crystal layer 36, the incident light L1 is given a phase difference of 180° by passing through the liquid crystal layer 36, and the transmitted light L2 is converted into right-handed circularly polarized light. In addition, since the liquid crystal orientation pattern formed in the liquid crystal layer 36 is a periodic pattern in the direction of the array axis D, the transmitted light L2 travels in a direction different from that of the incident light L1. In this way, the left-handed circularly polarized incident light L1 is converted into right-handed circularly polarized transmitted light L2 that is tilted at a certain angle in the direction of the array axis D with respect to the incident direction.
[0140] On the other hand, as shown in Figure 17, when the product of the refractive index difference of the liquid crystal compound in the liquid crystal layer 36 and the thickness of the optically anisotropic layer is λ / 2, when right-handed circularly polarized incident light L4 is incident on the liquid crystal layer 36, the incident light L4 is given a phase difference of 180° by passing through the liquid crystal layer 36 and is converted into left-handed circularly polarized transmitted light L5. Furthermore, since the liquid crystal orientation pattern formed in the liquid crystal layer 36 is a periodic pattern in the direction of the array axis D, the transmitted light L5 travels in a direction different from that of the incident light L4. At this time, the transmitted light L5 travels in a direction different from that of the transmitted light L2, that is, in the opposite direction to the direction of the arrow X with respect to the incident direction. In this way, the incident light L4 is converted into the transmitted light L5 of left-handed circular polarization tilted at a certain angle in the opposite direction to the array axis D with respect to the incident direction.
[0141] Like the liquid crystal layer 34, the liquid crystal layer 36 can adjust the angles of refraction of the transmitted light L2 and L5 by changing one period Λ of the formed liquid crystal orientation pattern. Specifically, the shorter the period Λ of the liquid crystal orientation pattern of the liquid crystal layer 36, the stronger the interference between the lights that have passed through adjacent liquid crystal compounds 40, and therefore the greater the refraction of the transmitted light L2 and L5. In addition, by reversing the direction of rotation of the optical axis 40A of the liquid crystal compound 40, which rotates along the arrangement axis D1, the direction of refraction of the transmitted light can be reversed. That is, in the examples shown in Figures 14 to 17, the direction of rotation of the optical axis 40A facing the arrangement axis D is clockwise, but by changing this rotation direction to counterclockwise, the direction of refraction of the transmitted light can be reversed.
[0142] From the viewpoint of diffraction efficiency, even when using such a liquid crystal diffraction element that transmits and diffracts incident light, it is preferable to use a liquid crystal diffraction element having a region where the liquid crystal compound is twisted and rotated (the twist angle is less than 360°). In particular, when diffracting light at an angle that causes total reflection within the light guide plate, from the viewpoint of diffraction efficiency, a liquid crystal diffraction element having a region where the liquid crystal compound is twisted and rotated can be suitably used. Also, from the viewpoint of diffraction efficiency, it is preferable to stack and use liquid crystal diffraction elements having different angles by which the liquid crystal compound is twisted and rotated, or to stack and use liquid crystal diffraction elements having different directions by which the liquid crystal compound is twisted and rotated.
[0143] Moreover, such a liquid crystal diffraction element having a region in which the liquid crystal compound is not cholesterically oriented but is twisted and rotated (the twist angle is less than 360°) can also be used as a reflective diffraction element. In such a liquid crystal diffraction element, diffracted light is reflected at the interface of the liquid crystal diffraction element and emitted from the light incident side, and the light is diffracted while being reflected, so that the liquid crystal diffraction element can also function as a reflective diffraction element.
[0144] In the light guide element of the present invention, different types of diffraction elements may be combined as the diffraction elements. For example, a transmission type liquid crystal diffraction element may be used as the incident diffraction element, and reflective type liquid crystal diffraction elements may be used as the intermediate diffraction element and the exit diffraction element.
[0145] [Polarizing element] The polarizing element is a polarizing element that absorbs or reflects at least a part of the light in the polarized state selectively diffracted by the output diffraction element. Therefore, the polarized light that the polarizing element absorbs or reflects is appropriately set according to the configuration of the output diffraction element. As the polarizing element, a conventionally known circular polarizing plate, an elliptical polarizing plate, a linear polarizing plate, or the like is used.
[0146] The circular polarizing plate or the elliptical polarizing plate may be a combination of a retardation plate and a linear polarizer. For example, in the case of a circular polarizing plate, a λ / 4 plate is used as the retardation plate, and the retardation plate is laminated so that the slow axis of the λ / 4 plate and the absorption axis of the linear polarizer are at 45°.
[0147] The retardation plate preferably has reverse wavelength dispersion, which allows the retardation layer to handle light with a wide wavelength range. Note that reverse wavelength dispersion means that the absolute value of the retardation increases with increasing wavelength, and normal dispersion means that the absolute value of the retardation increases with decreasing wavelength.
[0148] The optical member and image display device of the present invention may use a diffractive optics method for enlarging the exit pupil in order to improve visibility. Specifically, an optical method using a plurality of diffractive elements (diffractive elements), i.e., a diffractive optical method with inner coupling, intermediate and outer coupling diffractive elements, can be used. This method is described in detail in JP-A-2008-546020.
[0149] The light-guiding element and image display device of the present invention have been described in detail above, but the present invention is not limited to the above-mentioned examples, and various improvements and modifications may of course be made within the scope of the present invention without departing from the gist of the present invention. EXAMPLES
[0150] The features of the present invention will be described in more detail below with reference to examples. The materials, reagents, amounts used, amounts of substances, ratios, processing contents, processing procedures, etc. shown in the following examples can be appropriately changed without departing from the spirit of the present invention. Therefore, the scope of the present invention should not be interpreted as being limited by the specific examples shown below.
[0151] [Example 1-1] <Fabrication of incident diffraction element B> (Formation of alignment film) A glass substrate was prepared as a support. The following coating solution for forming an alignment film was applied to the support by spin coating. The support on which the coating solution for forming an alignment film was formed was dried on a hot plate at 60° C. for 60 seconds to form an alignment film.
[0152] Coating solution for forming alignment film ---------------------------------------------------------------------------------- 1.00 parts by weight of the following photoalignment material Water 16.00 parts by mass Butoxyethanol 42.00 parts by weight Propylene glycol monomethyl ether 42.00 parts by mass ----------------------------------------------------------------------------------
[0153] -Material for photo alignment- [ka]
[0154] (Exposure of alignment film) The alignment film was exposed using the exposure apparatus shown in FIG. 13 to form an alignment film P-1 having an alignment pattern. The exposure device used was a laser that emitted a laser beam with a wavelength of 325 nm. The exposure dose by the interference light was 1000 mJ / cm 2 The period of the orientation pattern formed by the interference of the two laser beams (the length of the optical axis rotating 180°) was controlled by changing the crossing angle (crossing angle α) of the two beams.
[0155] (Formation of liquid crystal layer) The following composition A-1 was prepared as a liquid crystal composition for forming the incident diffraction element B. This composition A-1 is a liquid crystal composition that forms a cholesteric liquid crystal layer (cholesteric liquid crystal phase) that reflects right-handed circularly polarized light. Composition A-1 ------------------------------------------------------------------ Rod-shaped liquid crystal compound L-1 100.00 parts by mass Polymerization initiator (BASF, Irgacure (registered trademark) 907) 3.00 parts by mass Photosensitizer (KAYACURE DETX-S, Nippon Kayaku) 1.00 parts by mass Chiral agent Ch-1 6.10 parts by mass Methyl ethyl ketone 204.00 parts by mass ------------------------------------------------------------------
[0156] Rod-shaped liquid crystal compound L-1 [ka]
[0157] Chiral Agent Ch-1 [ka]
[0158] The above composition A-1 was applied onto the alignment film P-1, and the coating film was heated to 80° C. on a hot plate. Thereafter, ultraviolet rays having a wavelength of 365 nm were irradiated at 300 mJ / cm 2 using a high-pressure mercury lamp in a nitrogen atmosphere at 80° C. 2 The coating film was irradiated with light at a dose of 100 nm to fix the orientation of the liquid crystal compound, thereby forming a liquid crystal layer of the incident diffraction element B.
[0159] When the cross section of the coating layer was examined with a scanning electron microscope (SEM), the number of pitches in the normal direction (thickness direction) to the main surface was 8. In addition, the pitch P of the inclined surfaces of the bright and dark areas to the main surface was 0.31 μm. The bright and dark areas referred to here are the bright and dark areas derived from the cholesteric liquid crystal phase that can be seen when the cross section of the cholesteric liquid crystal layer is observed with a SEM.
[0160] It was confirmed by a polarizing microscope that the liquid crystal layer of incident diffraction element B had a periodic alignment surface as shown in Fig. 7. When the cross section of the coating layer was examined by SEM, it was found that in the liquid crystal alignment pattern of the liquid crystal layer of incident diffraction element B, one period Λ in which the optical axis of the liquid crystal compound rotates by 180° was 0.32 μm.
[0161] (Fabrication of output diffraction element B) The output diffraction element B was fabricated in the same manner as the input diffraction element B, except that the film thickness was adjusted.
[0162] The pitch number of the liquid crystal layer was 2 pitches.
[0163] (Fabrication of λ / 4 plate) (Formation of alignment film) An alignment film was formed in the same manner as in Example 1.
[0164] (Exposure of alignment film) The obtained alignment film P-Q1 was irradiated with polarized ultraviolet light (50 mJ / cm 2 The alignment film P-Q1 was exposed to light by a high-pressure mercury lamp.
[0165] (Formation of λ / 4 plate) As a liquid crystal composition forming λ / 4, the following composition C-1 was prepared. Composition C-1 ---------------------------------------------------------------------------------- Liquid crystal compound L-2 42.00 parts by mass Liquid crystal compound L-3 42.00 parts by mass Liquid crystal compound L-4 16.00 parts by mass Polymerization initiator PI-1 0.50 parts by mass Leveling agent G-1 0.20 parts by weight Methyl ethyl ketone 176.00 parts by mass Cyclopentanone 44.00 parts by mass ----------------------------------------------------------------------------------
[0166] -Liquid crystal compound L-2- [ka]
[0167] -Liquid crystal compound L-3- [ka]
[0168] -Liquid crystal compound L-4- [ka]
[0169] -Polymerization initiator PI-1- [ka]
[0170] -Leveling agent G-1- [ka]
[0171] As the λ / 4 plate, a layer made of a reverse dispersion liquid crystal compound was formed. The λ / 4 plate was formed by applying the above composition C-1 onto the alignment film P-Q1. The applied coating was heated to 70° C. on a hot plate, then cooled to 65° C., and then irradiated with 500 mJ / cm2 ultraviolet light having a wavelength of 365 nm using a high-pressure mercury lamp in a nitrogen atmosphere. 2 The coating film was irradiated with an irradiation dose of 1000 nm to fix the alignment of the liquid crystal compound. This resulted in a λ / 4 plate, whose Re(530) was 133 nm.
[0172] (Fabrication of polarizing element) The λ / 4 plate and a linear polarizer prepared above were attached to each other with an adhesive layer while adjusting the direction, to prepare a circular polarizing plate, which was used as a polarizing element.
[0173] (Fabrication of light guide element) The light guide plate used was 60 mm x 70 mm in size, 1 mm in thickness, and made of glass. The input diffraction element B was cut to a size of 6 mm in diameter and used. The output diffraction element B was cut to a size of 20 mm x 25 mm and used. When cutting out each diffraction element, the cutting direction and the periodic direction of the diffraction structure were adjusted so that the periodic direction of the diffraction structure would be in a predetermined direction when each diffraction element was placed on the light guide plate.
[0174] Each of the produced diffraction elements was attached to one main surface of the light guide plate using an adhesive. The diffraction elements were arranged as shown in Fig. 1. The entrance diffraction element B and the exit diffraction element B were arranged 8 mm apart in the left-right direction. In this manner, a light guide element was produced.
[0175] (Production of optical components) A polarizing element was disposed at a distance from the produced light guide element on the opposite side to the light guide plate side from the position where the light guide element overlapped with the output diffraction element in the planar direction, to produce an optical member. The polarizing element was cut to a size of 20 mm x 25 mm and used. The distance between the light guide element and the polarizing element was 2 mm.
[0176] [Example 1-2] An optical member was produced in the same manner as in Example 1-1, except that the polarizing element was disposed so as to be in contact with the light guide element.
[0177] [Examples 1-3] An optical member was produced in the same manner as in Example 1-1, except that a linear polarizer was used as the polarizing element.
[0178] [Comparative Example 1] An optical member was produced in the same manner as in Example 1-1, except that no polarizing element was provided.
[0179] [Examples 2-1 to 2-3, Comparative Example 2] Except for using the following input diffraction element G instead of input diffraction element B, and using the following output diffraction element G instead of output diffraction element B, optical members were produced in the same manner as in Examples 1-1 to 1-3 and Comparative Example 1.
[0180] (Fabrication of incident diffraction element G) Incident diffraction element G was prepared in the same manner as incident diffraction element B, except that in exposing the alignment film, the crossing angle (crossing angle α) of the two lights was changed to vary one period of the alignment pattern formed on the alignment film, the amount of chiral agent in the composition forming the liquid crystal layer was changed to 5.27 parts by mass, and the film thickness was adjusted.
[0181] The number of pitches in the thickness direction of the liquid crystal layer of the incident diffraction element G was 8 pitches, and in the liquid crystal alignment pattern, one period Λ in which the optical axis of the liquid crystal compound rotated by 180° was 0.39 μm. The pitch P of the liquid crystal layer was 0.36 μm.
[0182] (Fabrication of output diffraction element G) The exit diffraction element G was fabricated in the same manner as the entrance diffraction element G, except that the film thickness was adjusted.
[0183] The pitch number of the liquid crystal layer was 2 pitches.
[0184] [Examples 3-1 to 3-3, Comparative Example 3] Except for using the following input diffraction element R instead of input diffraction element B and the following output diffraction element R instead of output diffraction element B, optical members were produced in the same manner as in Examples 1-1 to 1-3 and Comparative Example 1.
[0185] (Fabrication of incident diffraction element R) Incident diffraction element R was prepared in the same manner as incident diffraction element B, except that in exposing the alignment film, the crossing angle (crossing angle α) of the two lights was changed to vary one period of the alignment pattern formed on the alignment film, the amount of chiral agent in the composition forming the liquid crystal layer was changed to 4.42 parts by mass, and the film thickness was adjusted.
[0186] The number of pitches in the thickness direction of the liquid crystal layer of the incident diffraction element R was 8 pitches, and in the liquid crystal alignment pattern, one period Λ in which the optical axis of the liquid crystal compound rotated by 180° was 0.45 μm. The pitch P of the liquid crystal layer was 0.43 μm.
[0187] (Fabrication of output diffraction element R) The output diffraction element R was fabricated in the same manner as the input diffraction element R, except that the film thickness was adjusted.
[0188] The pitch number of the liquid crystal layer was 2 pitches.
[0189] [Example 4-1] (Fabrication of intermediate diffraction element B) Intermediate diffraction element B was produced in the same manner as incident diffraction element B, except that in the exposure of the alignment film, the amount of chiral agent in the composition forming the liquid crystal layer was changed to 5.57 parts by mass and the film thickness was adjusted.
[0190] The number of pitches in the thickness direction of the liquid crystal layer of the intermediate diffraction element B was 2, and the pitch P of the liquid crystal layer was 0.34 μm. In the liquid crystal alignment pattern, one period Λ in which the optical axis of the liquid crystal compound rotates by 180° was 0.23 μm.
[0191] (Fabrication of light guide element) The light guide plate used was 60 mm x 70 mm in size, 1 mm in thickness, and made of glass. The input diffraction element B was cut to a size of 6 mm in diameter. The intermediate diffraction element B was cut to a size of 15 mm (maximum) × 25 mm. The output diffraction element B was cut to a size of 20 mm × 25 mm. When cutting out each diffraction element, the cutting direction and the periodic direction of the diffraction structure were adjusted so that the periodic direction of the diffraction structure would be in a predetermined direction when each diffraction element was placed on the light guide plate.
[0192] Each of the produced diffraction elements was attached to one main surface of the light guide plate using an adhesive. The diffraction elements were arranged as shown in Fig. 3. The intermediate diffraction element B and the incident diffraction element B were arranged 1 mm apart in the left-right direction. The exit diffraction element B and the intermediate diffraction element B were arranged 8 mm apart in the up-down direction. In this manner, a light guide element was produced.
[0193] (Production of optical components) A polarizing element was disposed at a distance from the produced light guide element on the opposite side to the light guide plate side from the position where the light guide element overlapped with the output diffraction element in the planar direction, to produce an optical member. The polarizing element was cut to a size of 20 mm x 25 mm and used. The distance between the light guide element and the polarizing element was 2 mm.
[0194] [Example 4-2] An optical member was produced in the same manner as in Example 4-1, except that the polarizing element was disposed so as to be in contact with the light guide element.
[0195] [Example 4-3] An optical member was produced in the same manner as in Example 4-1, except that a linear polarizer was used as the polarizing element.
[0196] [Comparative Example 4] An optical member was produced in the same manner as in Example 4-1, except that no polarizing element was provided.
[0197] [Examples 5-1 to 5-3, Comparative Example 5] Optical elements were prepared in the same manner as in Examples 4-1 to 4-3 and Comparative Example 4, except that incident diffraction element G was used instead of incident diffraction element B, intermediate diffraction element G described below was used instead of intermediate diffraction element B, and exit diffraction element G was used instead of exit diffraction element B.
[0198] (Fabrication of intermediate diffraction element G) Intermediate diffraction element G was prepared in the same manner as incident diffraction element G, except that in exposing the alignment film, the crossing angle (crossing angle α) of the two lights was changed to vary one period of the alignment pattern formed on the alignment film, the amount of chiral agent in the composition forming the liquid crystal layer was changed to 4.64 parts by mass, and the film thickness was adjusted.
[0199] The number of pitches in the thickness direction of the liquid crystal layer was 2, and in the liquid crystal alignment pattern, one period Λ in which the optical axis of the liquid crystal compound rotated by 180° was 0.28 μm. The pitch P of the liquid crystal layer was 0.41 μm.
[0200] [Examples 6-1 to 6-3, Comparative Example 6] Optical members were prepared in the same manner as in Examples 4-1 to 4-3 and Comparative Example 4, except that incident diffraction element R was used instead of incident diffraction element B, intermediate diffraction element R described below was used instead of intermediate diffraction element B, and exit diffraction element R was used instead of exit diffraction element B.
[0201] (Fabrication of intermediate diffraction element R) Intermediate diffraction element R was prepared in the same manner as incident diffraction element R, except that in exposing the alignment film, the crossing angle (crossing angle α) of the two lights was changed to vary one period of the alignment pattern formed on the alignment film, the amount of chiral agent in the composition forming the liquid crystal layer was changed to 3.94 parts by mass, and the film thickness was adjusted.
[0202] The number of pitches in the thickness direction of the liquid crystal layer was 2, and in the liquid crystal alignment pattern, one period Λ in which the optical axis of the liquid crystal compound rotated by 180° was 0.32 μm. The pitch P of the liquid crystal layer was 0.48 μm.
[0203] [evaluation] The fabricated light guide elements were evaluated for stray light and brightness of displayed images by the following method. Examples 1-1 to 1-3, 4-1 to 4-3 and Comparative Examples 1 and 4 were evaluated using light with a wavelength of 450 nm. Examples 2-1 to 2-3, 5-1 to 5-3 and Comparative Examples 2 and 5 were evaluated using light with a wavelength of 532 nm. Examples 3-1 to 3-3, 6-1 to 6-3 and Comparative Examples 3 and 6 were evaluated using light with a wavelength of 635 nm.
[0204] (stray light) A projection display was prepared by combining a projection light source and a convex lens with LCOS (Liquid crystal on silicon). The projection display was arranged so that it projected an image toward the incident diffraction element, creating an image display device. A circular polarizer was placed between the projection display and the incident diffraction element, and a right-handed circularly polarized image was projected onto the incident diffraction element. Each projection display was designed to project an image of a color (wavelength) corresponding to the corresponding incident diffraction element. An image was displayed using the produced image display device, and stray light was evaluated according to the following criteria. A: Stray light was generated insignificantly. B: Stray light was slightly visible, but within the acceptable range. C: Stray light was visible and noticeable
[0205] (Brightness of displayed image) The light emitted from the light source was passed through a linear polarizer and a λ / 4 plate to obtain circularly polarized light. This light was made incident on the input diffraction element of the light guide element, and the amount of light emitted from the output diffraction element was measured with a power meter. The measurement points were 10 mm from the top end of the output diffraction element, the center position on the left and right, and the position ±6 mm to the left and right from the center. In addition, when the normal direction to the main surface of the light guide plate was set to 0°, the incident angle of the light to the input diffraction element was changed from 0° to 20° in 10° increments. A pinhole was placed so that the effective aperture of the power meter was 2 mmΦ, and the amount of light was measured so that the output light was transmitted through the center of the pinhole, and the evaluation was performed using the average light amount of the measured values at each position and each incident angle. A: Light intensity is 80% or more of the corresponding comparison example. B: Light intensity is less than 80% of the corresponding comparative example. The results are shown in Tables 1 and 2 below.
[0206] [Table 1]
[0207] [Table 2]
[0208] It can be seen from Tables 1 and 2 that Examples 1-1 to 6-3 of the present invention are able to suppress stray light more effectively than the corresponding Comparative Examples.
[0209] Furthermore, comparisons between Examples 1-1 and 1-2, between Examples 2-1 and 2-2, between Examples 3-1 and 3-2, between Examples 4-1 and 4-2, between Examples 5-1 and 5-2, and between Examples 6-1 and 6-2 show that arranging the polarizing element at a distance from the light-guiding element can prevent the displayed image from becoming dark. Furthermore, comparisons between Examples 1-1 and 1-3, between Examples 2-1 and 2-3, between Examples 3-1 and 3-3, between Examples 4-1 and 4-3, between Examples 5-1 and 5-3, and between Examples 6-1 and 6-3 show that stray light can be more effectively suppressed by using a circular polarizing plate consisting of a retardation layer and a linear polarizer as the polarizing element. From the above results, the effects of the present invention are clear. [Industrial Applicability]
[0210] The present invention can be suitably used in various optical devices that utilize light guidance, such as AR glasses. [Explanation of symbols]
[0211] 10, 10b~10d Image display device 12 Display element 14, 14a to 14e Light guide element 16, 16d~16e light guide plate 18, 18c-18e Incident diffraction element 20 Intermediate Diffraction Element 24, 24c to 24e Output diffraction element 30 Support 32 Alignment film 34, 36 Liquid crystal layer 40 Liquid crystal compounds 40A optical axis 42 Akabe 44 Dark part 60 Exposure Equipment 62 Laser 64 Light source 65 λ / 2 plate 68 Polarizing Beam Splitter 70A, 70B Mirror 72A,72B λ / 4 board R R Red right-handed circularly polarized light M Laser light MA,MB rays P O Linearly polarized P R Right circular polarization P L Left circular polarization α intersection angle Q Absolute Phase E,E1,E2 Equiphase surface U user D Array axis Λ 1 period Pitch
Claims
1. a light guide element including a light guide plate, an input diffraction element and an output diffraction element disposed on a main surface of the light guide plate; a display element for projecting an image onto the incident diffraction element; a polarizing element that blocks transmission of light that is irradiated by the display element, is diffracted by the input diffraction element, is input to the light guide plate, is guided through the light guide plate, and reaches the output diffraction element, the polarizing element preventing transmission of light that leaks to an opposite side to the output side of the output diffraction element; the output diffraction element is a polarizing diffraction element, the polarizing element is disposed on the opposite side to the exit side with respect to the exit diffraction element, the polarizing element is disposed at a position overlapping with the output diffraction element in a planar direction of a main surface of the light guide plate, the polarizing element absorbs or reflects light of one polarization state and transmits light of the other polarization state; the output diffraction element is a reflective diffraction element, The image display device, wherein the polarizing element is disposed on a side of the output diffraction element opposite to a side of the light guide plate.
2. a light guide element including a light guide plate, an input diffraction element and an output diffraction element disposed on a main surface of the light guide plate; a display element for projecting an image onto the incident diffraction element; a polarizing element that blocks transmission of light that is irradiated by the display element, is diffracted by the input diffraction element, is input to the light guide plate, is guided through the light guide plate, and reaches the output diffraction element, the polarizing element preventing transmission of light that leaks to an opposite side to the output side of the output diffraction element; the output diffraction element is a polarizing diffraction element, the polarizing element is disposed on the opposite side to the exit side with respect to the exit diffraction element, the polarizing element is disposed at a position overlapping with the output diffraction element in a planar direction of a main surface of the light guide plate, the polarizing element absorbs or reflects light in a polarized state selectively diffracted by the output diffraction element, the output diffraction element is a reflective diffraction element, The image display device, wherein the polarizing element is disposed on a side of the output diffraction element opposite to a side of the light guide plate.
3. The image display device according to claim 1 , wherein the polarizing element is spaced apart from the light guide element.
4. 4. The image display device according to claim 1, wherein the polarizing element is an elliptically polarizing plate.
5. 5. The image display device according to claim 1, wherein the polarizing element is a circular polarizing plate.
6. 6. The image display device according to claim 1, wherein the polarizing element comprises a linear polarizer and a retardation plate.
7. 7. The image display device according to claim 6, wherein the retardation plate is a λ / 4 plate.
8. 8. The image display device according to claim 6, wherein the retardation plate has reverse wavelength dispersion.
9. The image display device according to any one of claims 1 to 8, wherein the polarizing diffraction element is a liquid crystal diffraction element formed using a composition containing a liquid crystal compound and having a liquid crystal orientation pattern in which the direction of the optical axis derived from the liquid crystal compound changes while continuously rotating along at least one direction in a plane.
10. 10. The image display device according to claim 9, wherein the liquid crystal diffraction element has a region in which the direction of the optical axis of the liquid crystal compound is twisted and rotated in the thickness direction.
11. 11. The image display device according to claim 9, wherein the liquid crystal diffraction element has a cholesteric liquid crystal layer formed by fixing a cholesteric liquid crystal phase.
12. 12. The image display device according to claim 1, wherein the period of the diffraction structure of the polarizing diffraction element is 0.1 μm or more and 10 μm or less.
Citation Information
Patent Citations
Waveguide
US20160231568A1
Waveguides with extended field of view
US20170299864A1
Reflective structure, device, and manufacturing method for reflective structure
WO2016194961A1
Method and system for display device with integrated polarizer
WO2018152233A1
Augmented reality display with waveguide configured to capture images of eye and / or environment
WO2019060741A1