Thermal and electromagnetic generation and switching of chirality in ferroelectrics.

By transitioning nanostructured ferroelectrics through a high-temperature state and applying an electromagnetic field during cooling, the method achieves controllable and switchable chirality, addressing the challenge of producing tunable chiral nanomaterials with reduced field requirements and enabling efficient switching.

JP7562160B2Active Publication Date: 2024-10-07TERRA QUANTUM AG
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2022138984
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-09-29
Filing Date
2022-09-01
Publication Date
2024-10-07
Estimated Expiration
2042-09-01

AI Technical Summary

Technical Problem

The challenge lies in producing chiral nanomaterials with tunable and switchable chirality, as existing methods often result in racemic mixtures, complicating industrial manufacture and requiring complex post-production sorting or synthesis processes.

Method used

A method involving nanostructured ferroelectrics that undergo a high-temperature state transition, followed by cooling under an electromagnetic field, allows for the controlled switching and tuning of chirality, enabling controllable, switchable, and reconfigurable polarization states.

Benefits of technology

This approach reduces the required electromagnetic field strength for reliable switching and enables reversible, repeatable switching between different polarization states, facilitating applications in storage and sensing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007562160000003
    Figure 0007562160000003
  • Figure 0007562160000004
    Figure 0007562160000004
  • Figure 0007562160000005
    Figure 0007562160000005
Patent Text Reader

Abstract

To provide a method and an apparatus for reversibly switching the chirality of a single nanostructure multiple times.SOLUTION: Nanostructured ferroelectric 300 provides a high temperature state and a low temperature ferroelectric state. The low temperature ferroelectric state has polarization states from a plurality of polarization states. The plurality of polarization states includes at least a first chiral polarization state having a first chirality and a second chiral polarization state having a second chirality different from the first chirality. A method for producing the nanostructured ferroelectric having a predetermined chirality comprises: selecting a predetermined chirality from the first chirality and the second chirality and selecting an electromagnetic field according to the predetermined chirality so that the nanostructured ferroelectric in a high temperature state is provided; and applying an electromagnetic field to the nanostructured ferroelectric in the high temperature state and cooling the nanostructured ferroelectric from the high temperature state to a low temperature ferroelectric state while applying the electromagnetic field so that the nanostructured ferroelectric establishes a polarized state having the predetermined chirality.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to techniques for creating and switching the chirality of a polarization field in nanostructured ferroelectrics. [Background technology]

[0002] Chirality or handedness, introduced by Lord Kelvin in 1894, is a fundamental property that describes objects that lack mirror symmetry. The prototypical example of a chiral object is the human hand. The left hand is a non-superimposable mirror image of the right hand. The two hands do not match no matter how they are oriented. Mathematically, an object is chiral (or said to have chirality) if it cannot be mapped onto its mirror image by any combination of rotations and translations. Chirality distinguishes between left-handed and right-handed modifications of chiral objects, also called enantiomers. Molecular chirality is a major concept in stereochemistry and biochemistry, given that a wide variety of organic substances, such as glucose, cellulose, and DNA molecules, are non-mirror symmetric. Chiral molecules are molecules that have a non-superimposable mirror image.

[0003] Chirality is the focus of modern materials science because chiral materials have excellent laser manipulation capabilities such as chiral sensing, optical activity, negative refractive index rotation, and circular dichroism. Due to these capabilities, chiral materials find diverse applications in optoelectronics and plasmonics. However, the fabrication of chiral nanomaterials with tunable and switchable chirality, i.e., the design of nanoscale inorganic and hybrid objects with controllable and configurable chirality, remains a challenge. Some examples of new generation chiral nanomaterials include chiral metal particles and nanocrystals, DNA-assembled plasmonic nanostructures, core-shell plasmonic spheres, and chiral plasmonic particles assembled on scaffolds. The problem that arises is that chiral nanomaterials are usually fabricated as racemic mixtures of left-handed and right-handed particles, which vanishes the average chiral response. However, for practical applications, systems with monochirality are highly desirable.

[0004] One way to achieve monochiral nanomaterials is to employ enantioselective synthesis. An alternative approach is to filter or sort nanomaterials according to their chirality after production. Both approaches substantially complicate the industrial production of nanoparticles.

[0005] Possible ways to address these issues are reviewed in Luk'yanchuk et al., "Hopfions emerge in ferroelectrics," Nat. Commun. 11, 2433 (2020) and Tikhonov et al., "Controllable skyrmion chirality in ferroelectrics," Sci. Rep. 10, 8657 (2020). Summary of the Invention [Problem to be solved by the invention]

[0006] In view of the high technological demands, methods are being sought to create monochiral systems and to make the chirality of these systems switchable and tunable. Corresponding techniques make it possible to fabricate nanostructures with desired chirality, and most importantly, with controllable chirality. Control can include switching, tuning, configuring, and reconfiguring chirality. In particular, there is a need for methods to reversibly switch the chirality of a single nanostructure multiple times, both after and independently of the nanostructure's fabrication. [Means for solving the problem]

[0007] This object is achieved by a method according to claim 1. Claim 14 relates to an apparatus for producing nanostructured ferroelectrics with a polarization state of predetermined chirality. The dependent claims relate to preferred embodiments.

[0008] Materials composed of chiral molecules have found widespread applications in fields ranging from nonlinear optics and spintronics to biology and medicine. However, chirality is usually an immutable, intrinsic property of a given material that cannot be easily and freely altered. This disclosure presents methods that allow one to configure, switch, and tune the chirality of nanostructured ferroelectrics to ensure their widespread use in a variety of applications.

[0009] In a first aspect, a nanostructured ferroelectric is adapted to provide a high temperature state and a low temperature ferroelectric state. In the low temperature ferroelectric state, the nanostructured ferroelectric has a polarization state from a plurality of polarization states. The plurality of polarization states includes at least a first chiral polarization state having a first chirality and a second chiral polarization state having a second chirality different from the first chirality. A method for producing a nanostructured ferroelectric with a predetermined chirality includes selecting a predetermined chirality from the first chirality and the second chirality, selecting an electromagnetic field according to the predetermined chirality, providing a nanostructured ferroelectric in a high temperature state, applying the electromagnetic field to the nanostructured ferroelectric in the high temperature state, and cooling the nanostructured ferroelectric from the high temperature state to the low temperature ferroelectric state while applying the electromagnetic field to establish a polarization state of the nanostructured ferroelectric with the predetermined chirality.

[0010] The polarization state of the nanostructured ferroelectric provides a switchable chirality. The switchable chiral polarization structure can be applied, for example, to storage and sensing applications, particularly using polarization-dependent optical control and / or readout. This temperature change protocol takes the nanostructure through a transition between the ferroelectric state and the high-temperature state, and the energy barrier between polarization states with different chiralities is reduced. Thus, the method can reliably drive the nanostructured ferroelectric into a polarization state with a predetermined chirality using an electromagnetic field selected according to the predetermined chirality.

[0011] Thus, the method can provide controllable chirality of the polarization state of the nanostructured ferroelectric. The controllable chirality may include tunable, switchable, and / or reconfigurable chirality. In particular, the controllable chirality may be tunable, switchable, and / or reconfigurable multiple times and / or independent of the initial fabrication of the nanostructured ferroelectric.

[0012] Compared to methods without heat treatment, the disclosed method reduces the magnitude of the electromagnetic field required for reliable switching.

[0013] The nanostructured ferroelectric may comprise lead titanate, lead zirconate titanate, zirconium oxide, hafnium zirconium oxide or hafnium oxide, particularly doped hafnium oxide, for example doped with silicon.

[0014] The nanostructured ferroelectric may include a multiferroic material.

[0015] According to some embodiments, any polarization state included in the plurality of polarization states has either a first chirality or a second chirality.

[0016] According to an embodiment, the first extension dimension of the nanostructured ferroelectric material along the first direction is at most 1000 nm, in particular at most 200 nm, at most 100 nm or at most 80 nm.

[0017] The second extension dimension of the nanostructured ferroelectric material along the second direction may be at most 1000 nm, in particular at most 200 nm, at most 100 nm, or at most 80 nm. In particular, the second direction may be perpendicular to the first direction.

[0018] The third extension dimension of the nanostructured ferroelectric material along the third direction may be at most 1000 nm, in particular at most 200 nm, at most 100 nm, or at most 80 nm. In particular, the third direction may be perpendicular to the first direction and / or the second direction.

[0019] The nanostructured ferroelectric may be a layer and the first extension dimension may correspond to the thickness of the layer.

[0020] The nanostructured ferroelectric may have a prismatic shape and the first extension dimension may correspond to the height of the prismatic column.

[0021] The nanostructured ferroelectric may have a rod shape. The first extension dimension, the second extension dimension, or the third extension dimension may correspond to a height of a prism. The first extension dimension, the second extension dimension, or the third extension dimension may correspond to a width of the rod. The first extension dimension, the second extension dimension, or the third extension dimension may correspond to a length of the rod.

[0022] In some embodiments, the nanostructured ferroelectric may have a shape of a disk. The first or second dimension may correspond to a diameter of the disk. The first or second dimension may correspond to a height of the disk.

[0023] The prism may be a rectangular prism and the second extended dimension may correspond to the length of a side of a rectangular base of the rectangular prism.

[0024] In some embodiments, the nanostructured ferroelectric may have a spherical shape and the first extended dimension may correspond to a diameter of the sphere.

[0025] In other embodiments, the nanostructured ferroelectric may have a pyramidal shape and the first extended dimension may correspond to a side length of the pyramid.

[0026] The high temperature state may be a paraelectric state.

[0027] At elevated temperatures, the nanostructured ferroelectric may have an achiral polarization state.

[0028] Cooling may include cooling the nanostructured ferroelectric from a temperature above the Curie temperature of the nanostructured ferroelectric to a temperature below the Curie temperature of the nanostructured ferroelectric.

[0029] The low temperature state may correspond to a room temperature state of the nanostructured ferroelectric.

[0030] Applying the electromagnetic field may include irradiating the nanostructured ferroelectric with electromagnetic waves.

[0031] Electromagnetic waves may include microwave, terahertz, infrared, visible light, ultraviolet, or x-ray radiation.

[0032] The central wavelength of the electromagnetic radiation may be at least 190 nm, in particular at least 250 nm, in particular at least 370 nm, in particular at least 700 nm.

[0033] The central wavelength of the electromagnetic wave may be at most 3000 nm, in particular at most 1400 nm, at most 1100 nm or at most 980 nm.

[0034] The central wavelength may correspond to a weighted average of all the wavelengths of the electromagnetic wave.

[0035] The electromagnetic wave may in particular be a pulsed electromagnetic wave having a pulse duration of at most 1 ns, in particular at most 300 ps, ​​at most 100 ps, ​​at most 40 ps, ​​at most 10 ps or at most 2 ps.

[0036] According to an embodiment, the energy per pulse and area of ​​the pulsed electromagnetic wave in the nanostructured ferroelectric is 100 mJ / cm 2 Not exceeding 70 mJ / cm 2 or not exceeding 40 mJ / cm 2 not exceed.

[0037] Providing the nanostructured ferroelectric material at an elevated temperature may include heating the nanostructured ferroelectric material using electromagnetic waves.

[0038] The electromagnetic wave may be elliptically polarized. The chirality of the elliptically polarized electromagnetic wave may correspond to a predetermined chirality.

[0039] The electromagnetic wave may be circularly polarized. The chirality of the circularly polarized electromagnetic wave may correspond to a predetermined chirality.

[0040] The elliptically or circularly polarized electromagnetic radiation can provide a stimulus that makes a first chiral polarization state having a first chirality more energetically favorable than a second chiral polarization state having a second chirality, thereby increasing the probability that the nanostructured ferroelectric will develop the first chiral polarization state upon cooling to the low temperature ferroelectric phase.

[0041] The method may further comprise supporting the nanostructured ferroelectric by a substrate, particularly while applying the electromagnetic field and / or while cooling the nanostructured ferroelectric.

[0042] The substrate may be in direct contact with the nanostructured ferroelectric and may be adapted to induce stress or strain in the nanostructured ferroelectric. In particular embodiments, the nanostructured ferroelectric comprises lead titanate and / or lead zirconate titanate and / or the substrate comprises strontium titanate.

[0043] The substrate can induce strain or stress in the nanostructured ferroelectric, which can be used to tune the chiral ground state(s) of the nanostructured ferroelectric.

[0044] In some embodiments, the substrate may be adapted to absorb heat from the nanostructured ferroelectric during a process step that cools the nanostructured ferroelectric.

[0045] The substrate may be adapted to absorb energy from the electromagnetic waves and provide the energy to the nanostructured ferroelectric material during a process step that provides the nanostructured ferroelectric material at elevated temperatures.

[0046] In some embodiments, the substrate may be adapted to induce electromagnetic waves, and in particular to reflect electromagnetic waves towards the nanostructured ferroelectric.

[0047] The nanostructured ferroelectric may be a ferroelectric layer disposed on a substrate.

[0048] At least one additional layer, in particular at least one additional layer that is not ferroelectric, may be disposed on the nanostructured ferroelectric.

[0049] A second nanostructured ferroelectric may be disposed on the at least one additional layer. The second nanostructured ferroelectric may be a second ferroelectric layer.

[0050] In some embodiments, an interlayer, particularly a dielectric interlayer, for example a non-ferroelectric dielectric interlayer, may be disposed between the substrate and the ferroelectric layer.

[0051] The ferroelectric layer may be included in a stacked multi-layer structure including multiple ferroelectric layers and multiple additional layers, in particular the additional layers may not be ferroelectric.

[0052] In some embodiments, the stacked multi-layer structure may include alternating ferroelectric layers and additional layers.

[0053] The substrate may be adapted to transfer heat to the nanostructured ferroelectric during a process step that provides the nanostructured ferroelectric at a high temperature.

[0054] The nanostructured ferroelectric may be surrounded by a solid or liquid matrix while the nanostructured ferroelectric is cooled.

[0055] In some embodiments, the solid or liquid matrix can be adapted to absorb heat from the nanostructured ferroelectric material during a process step that cools the nanostructured ferroelectric material.

[0056] The solid or liquid matrix may be adapted to be transparent to electromagnetic waves.

[0057] The solid or liquid matrix may be adapted to transfer heat to the nanostructured ferroelectric material during a process step that provides the nanostructured ferroelectric material at elevated temperatures.

[0058] The electromagnetic field may be a non-uniform electromagnetic field.

[0059] The method may further include applying a non-uniform electromagnetic field to the nanostructured ferroelectric during and / or after cooling of the nanostructured ferroelectric from the high temperature state to the low temperature ferroelectric state to transport the nanostructured ferroelectric to a location associated with a predetermined chirality.

[0060] Applying a non-uniform electromagnetic field may include focusing an electromagnetic wave at a focal point located at or near the nanostructured ferroelectric material.

[0061] The method may further include lifting the nanostructured ferroelectric from the surface using a non-uniform electromagnetic field.

[0062] In some embodiments, the method can further include applying a non-uniform electromagnetic field to a second nanostructured ferroelectric material having a chirality different from the predetermined chirality to transport the second nanostructured ferroelectric material to a second location different from the location associated with the predetermined chirality.

[0063] In particular, the method can include simultaneously applying a non-uniform electromagnetic field to the nanostructured ferroelectric and the second nanostructured ferroelectric to separate the nanostructured ferroelectric and the second nanostructured ferroelectric.

[0064] The substrate may be electrically conductive, and application of a non-uniform electromagnetic field may induce plasmonic excitations in the substrate, particularly at the surface of the substrate, which may be adapted to separate the nanostructured ferroelectric and a second nanostructured ferroelectric having a chirality different from the given chirality according to the chirality of their polarization states.

[0065] Applying a non-uniform electromagnetic field may include using optical tweezers.

[0066] In some embodiments, applying a non-uniform electromagnetic field may include using plasmonic tweezers, particularly plasmonic tweezers having a plasmonic trap stiffness in the range of 0.1-5 fN / (μm W), or in the range of 0.1-1 fN / (μm W).

[0067] The non-uniform electric field can have a field polarization, and the method can further include selecting the field polarization in accordance with the predetermined chirality. The field polarization can be linear, elliptical or circular.

[0068] Selecting the field polarization may include selecting the handedness of circular or elliptical polarization, or selecting the direction of linear polarization.

[0069] Applying the electromagnetic field may include applying a voltage to electrodes disposed on opposite sides of the nanostructured ferroelectric.

[0070] The electrodes may be disposed on opposite sides of a plurality of nanostructured ferroelectrics including the nanostructured ferroelectric material. In particular, the plurality of nanostructured ferroelectrics may be a racemic mixture of nanostructured ferroelectrics.

[0071] According to an embodiment, exactly one nanostructured ferroelectric is disposed between the electrodes.

[0072] According to some embodiments, at least one of the electrodes has a first electrode extension dimension along a first direction of at most 1000 nm, in particular at most 200 nm, at most 100 nm, or at most 80 nm.

[0073] According to an embodiment, at least one of the electrodes has a second electrode extension dimension along a second direction of at most 1000 nm, in particular at most 200 nm, at most 100 nm, or at most 80 nm, which may be different from the first direction, in particular perpendicular to the second direction.

[0074] At least one of the electrodes may be a tip, in particular a conductive tip, in particular a tip adapted to provide a scanning tunnelling microscope tip or a conductive atomic force microscope tip.

[0075] According to an embodiment, the absolute value of the electric field does not exceed 100 kV / cm, in particular does not exceed 10 kV / cm.

[0076] At least one of the electrodes may have a chiral shape.

[0077] In some examples, chiral molecules can be adsorbed on at least one of the electrodes proximate the nanostructured ferroelectric. In particular, the chiral molecules can be nanotubes, such as carbon nanotubes.

[0078] At least one of the electrodes may be a chiral distorted tip, in particular a chiral distorted conductive tip, such as a chiral distorted scanning tunnelling microscope tip or a conductive atomic force microscope tip.

[0079] Chiral molecules on the tip, or chiral distortion of the tip, can provide a chiral electric field that can act as a stimulus to drive the nanostructured ferroelectrics into a polarization state of predetermined chirality upon cooling.

[0080] Providing a nanostructured ferroelectric in a high temperature state may further include providing a nanostructured ferroelectric having a first chirality in a low temperature ferroelectric state and heating the nanostructured ferroelectric to a high temperature state. The predetermined chirality may be a second chirality.

[0081] Methods according to the present disclosure can provide reversible and repeatable switching between different polarization states.

[0082] Heating the nanostructured ferroelectric material to a high temperature condition may include using a resistive heater.

[0083] The resistive heater may be in direct contact with the nanostructured ferroelectric, or with the substrate supporting the nanostructured ferroelectric, or with the solid or liquid matrix surrounding the nanostructured ferroelectric.

[0084] Heating the nanostructured ferroelectric material to an elevated temperature condition may include using a microwave heater.

[0085] Heating the nanostructured ferroelectric to a high temperature condition may use energy absorbed from electromagnetic radiation. Energy can be absorbed from electromagnetic radiation by the nanostructured ferroelectric.

[0086] Alternatively or additionally, energy may be absorbed from the electromagnetic waves by a substrate supporting the nanostructured ferroelectric or by a solid or liquid matrix surrounding the nanostructured ferroelectric, and the method may further include transferring energy to the nanostructured ferroelectric by a substrate supporting the nanostructured ferroelectric or by a solid or liquid matrix surrounding the nanostructured ferroelectric.

[0087] In a second aspect, an apparatus for generating a nanostructured ferroelectric material having a predetermined chirality comprises a holding element, a heating element, a field application element, and a cooling element. The holding element is adapted to receive the nanostructured ferroelectric material. The heating element heats the nanostructured ferroelectric material to a high temperature state. The field application element is adapted to apply an electromagnetic field to the nanostructured ferroelectric material while the nanostructured ferroelectric material is in the high temperature state. The cooling element is adapted to cool the nanostructured ferroelectric material to a low temperature ferroelectric state having a polarization state with a predetermined chirality while applying the electromagnetic field to the nanostructured ferroelectric material with the field application element.

[0088] The nanostructured ferroelectric may be characterised by one or all of the features described above in the context of the method according to the first aspect.

[0089] The holding element may comprise a substrate, in particular a conductive substrate, adapted to support the nanostructured ferroelectric material. The cooling element may comprise a substrate.

[0090] In particular, the substrate may be adapted to absorb heat from the nanostructured ferroelectric and / or the substrate may be adapted to be in direct thermal contact with the nanostructured ferroelectric.

[0091] Alternatively or additionally, the retaining element may comprise a solid or liquid matrix adapted to surround the nanostructured ferroelectric material. The cooling element may comprise a solid or liquid matrix.

[0092] In particular, the solid or liquid matrix may be adapted to absorb heat from the nanostructured ferroelectric material and / or the solid or liquid matrix may be adapted to be in direct thermal contact with the nanostructured ferroelectric material.

[0093] The heating element may comprise a resistive heater, in particular a resistive heater in direct thermal contact with the holding element and / or a resistive heater adapted for direct thermal contact with the nanostructured ferroelectric material.

[0094] The field application element may include electrodes disposed on opposite sides of the nanostructured ferroelectric.

[0095] The electrode may be characterised by one or all of the features described above in the context of the electrode of the method according to the first aspect.

[0096] The apparatus may further comprise a monitoring element adapted to monitor the polarization state of the nanostructured ferroelectric, in particular adapted to monitor the helicity of the polarization state of the nanostructured ferroelectric or the chirality of the polarization state of the nanostructured ferroelectric.

[0097] The monitoring element may include a device adapted to determine the polarization of the probe electromagnetic wave, in particular a polarimeter for the probe electromagnetic wave. The monitoring element may further comprise a probe light source adapted to generate a probe electromagnetic wave, direct the probe electromagnetic wave towards the nanostructured ferroelectric, and direct the probe electromagnetic wave after reflection from or transmission through the nanostructured ferroelectric towards a device adapted to determine the polarization of the probe electromagnetic wave.

[0098] The apparatus may further comprise a radiation source adapted to generate electromagnetic waves and irradiate the nanostructured ferroelectric with the electromagnetic waves.

[0099] The radiation source wave can provide a heating element and / or an electric field application element. The electromagnetic wave can include or be microwave, terahertz, infrared, or visible light radiation.

[0100] The radiation source may be included in optical tweezers. The optical tweezers may be adapted to transport the nanostructured ferroelectric to a location associated with the predetermined chirality. Alternatively or additionally, the optical tweezers may be adapted to separate the nanostructured ferroelectric from a second nanostructured ferroelectric having a chirality different from the predetermined chirality.

[0101] The radiation source may be included in the plasmonic tweezers. The plasmonic tweezers may be adapted to irradiate a conductive substrate of the nanostructured ferroelectric to induce plasmonic excitations in the conductive substrate. The plasmonic excitations in the conductive substrate may be adapted to separate the nanostructured ferroelectric and a second nanostructured ferroelectric having a chirality different from the given chirality. Alternatively or additionally, the plasmonic excitations in the conductive substrate may be adapted to generate a plasmonic trap. The plasmonic trap may be adapted to separate the nanostructured ferroelectric and the second nanostructured ferroelectric.

[0102] The electromagnetic wave may be adapted to provide a probing electromagnetic wave.

[0103] The apparatus may further comprise focusing optics for focusing the electromagnetic wave onto the nanostructured ferroelectric. In particular, the focusing optics may comprise a lens or a microscope objective.

[0104] The focusing optics and the radiation source may be adapted to generate a non-uniform electromagnetic field at a receiving element, particularly a receiving element adapted to receive the nanostructured ferroelectric material, the non-uniform electromagnetic field may be adapted to transport the nanostructured ferroelectric material to a location related to the polarization state of the nanostructured ferroelectric material, particularly a location related to the chirality of the polarization state of the nanostructured ferroelectric material.

[0105] The focusing optics and radiation source can provide optical tweezers adapted to move the nanostructured ferroelectric according to its polarization state, and in particular according to the chirality of its polarization state.

[0106] In some embodiments, the retaining element may include a conductive substrate.

[0107] The radiation source and focusing optics may be adapted to induce plasmonic excitations in the conductive substrate, in particular at the surface of the conductive substrate.

[0108] The focusing optics, radiation source, and conductive substrate can provide plasmonic tweezers adapted to move the nanostructured ferroelectric according to its polarization state, in particular plasmonic tweezers having a plasmonic trap stiffness in the range of 0.1-5 fN / (μm W), or in the range of 0.1-1 fN / (μm W). [Brief description of the drawings]

[0109] The techniques of the present disclosure and their associated advantages will become most apparent from a description of exemplary embodiments taken in conjunction with the accompanying drawings. [Figure 1a] FIG. 1 shows examples of left-handed and right-handed enantiomers of hand shapes. [Figure 1b]FIG. 1 shows examples of left-handed and right-handed enantiomers in the form of a helix. [Diagram 2] FIG. 2 is a diagram showing a chiral domain wall of a ferroelectric material. [Figure 3a] FIG. 1 illustrates a nanostructured ferroelectric in the form of a thin ferroelectric film with chiral polarization states that include skyrmions. [Figure 3b] FIG. 1 shows a nanostructured ferroelectric in the form of a multilayer structure having a thin ferroelectric film with a chiral polarization state involving a vortex. [Figure 4] FIG. 1 shows the potential energy surface of a nanostructured ferroelectric. [Diagram 5] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in nanostructured ferroelectrics, according to one embodiment. [Figure 6a] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 6b] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 7a] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 7b] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 8] FIG. 1 shows a nanostructured ferroelectric in the form of a nanodot having chiral polarization structures associated with domain walls. [Figure 9a] FIG. 1 shows a nanostructured ferroelectric in the form of nanoparticles having chiral polarization structures without domain walls. [Figure 9b] FIG. 1 shows nanostructured ferroelectrics in the form of nanodots with different chiral polarization structures without domain walls. [Figure 10a] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 10b]FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 11a] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 11b] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 12a] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 12b] FIG. 1 illustrates a method and apparatus for producing a predetermined chirality in a nanostructured ferroelectric according to another embodiment. [Figure 13] FIG. 1 illustrates a method and apparatus for generating predetermined chirality in nanostructured ferroelectrics using enantioselective transport, according to one embodiment. [Figure 14] FIG. 1 illustrates a method and apparatus for generating predetermined chirality in nanostructured ferroelectrics using enantioselective transport, according to another embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0110] The techniques of the present disclosure will now be described with reference to several different embodiments from the field of materials science. Although some features are described with respect to only some of these embodiments, those skilled in the art will understand that these embodiments may be combined, and thus, these features may generally be present in some or all of the described embodiments.

[0111] Figures 1a and 1b show two examples of chiral structures: human hands 104L, 104R in 1a and helices 106L, 106R in 1b. Both hands 104L, 104R and helices 106L, 106R exist as two different enantiomers. The enantiomers are mirror images of each other with respect to the mirror plane 100. The mirror images 104R, 106R differ from the prototypes 104L, 106L in their sense of rotation 102R, or chirality, respectively. In this context, the enantiomers with a counterclockwise sense of rotation 102R are referred to as right-handed enantiomers 104R, 106R, and the enantiomers with a clockwise sense of rotation 102L are referred to as left-handed enantiomers 104L, 106L.

[0112] FIG. 2 shows a chiral ferroelectric domain wall 200L, 200R between two ferroelectric domains 202U, 202D. Ferroelectrics are characterized by remnant polarizations 204U, 204D. The long-range electric fields associated with the polarizations 204U, 204D are energetically costly. Therefore, bulk ferroelectrics typically exhibit domain walls 200L, 200R that reduce the long-range fields and associated energies.

[0113] In the vicinity of the domain walls 200L, 200R, the polarizations 204U, 204D are typically oriented parallel to the surfaces defined by the domain walls 200L, 200R. It has long been believed that across the domain walls, the polarization maintains its orientation and changes its value only, for example from negative to positive with respect to an axis parallel to the polarization 204U (Ising domain walls). However, recent experiments have found ferroelectric domain walls 200L, 200R in which the polarizations 204U, 204D rotate around the surface normal 208 of the domain walls 200L, 200R, as shown in FIG. 2. This type of domain wall is referred to as a Bloch domain wall 200L, 200R. The sense of rotation 102L, 102R can be clockwise 102L or counterclockwise 102R, resulting in a left-handed Bloch domain wall 200L or a right-handed Bloch domain wall 200R. The Bloch domain wall 202L, 202R is chiral and is not superimposable upon itself upon specular reflection and / or spatial rotation transformation.

[0114] In bulk ferroelectrics, the ferroelectric domains and domain walls form in random locations with random orientations. However, in many practical applications, controlled orientation and placement may be preferred. To this end, the ferroelectric is nanostructured along at least one direction.

[0115] In the context of the present disclosure, a nanostructured ferroelectric may be understood as having an extension dimension along at least one direction that is confined to the nanoscale, e.g., 1 μm or less. Such ferroelectrics are sometimes referred to as nanoconfined.

[0116] An example is a thin layer that is confined along a direction perpendicular to the layer.

[0117] 3a shows a thin ferroelectric layer 300 on a substrate 302. As a result of the nanostructure geometry, the polarization 304 is preferably oriented within (in-plane) or perpendicular (out-of-plane) to the thin ferroelectric layer 300. The choice of the material providing the ferroelectric material of the thin ferroelectric layer 300 and its environment (e.g., substrate 302) provides control over the orientation of the polarization 304.

[0118] The choice of ferroelectric material of the thin ferroelectric layer 300, its environment, e.g., the choice of material providing the substrate, and the growth conditions are also used to control the topology of the domain walls 306. In general, the thin ferroelectric layer may include chiral (e.g., Ising) and achiral domain walls, such as the Bloch domain walls discussed in the context of FIG.

[0119] For layers containing various types of chiral and achiral domain walls, the chirality is determined by helicity

number

number

[0120] 3a shows a thin ferroelectric layer 300 of lead titanate (PbTiO3) deposited to a thickness of 50 nm on a dielectric strontium titanate (SrTiO3) substrate 302. The lattice mismatch induces strain in the ferroelectric layer 300. The thin ferroelectric layer 300 develops an out-of-plane orientation of polarization 304.

[0121] The ferroelectric thin layers were grown using pulsed laser deposition, although physical vapor deposition techniques, atomic layer deposition or molecular beam epitaxy may alternatively be applied. Details of the growth conditions can be found in Das et al., "Local negative permittivity and topological phase transition in polar skyrmions," Nat. Mater. 20, 194 (2021).

[0122] The growth conditions of the ferroelectric layer 300 in Figure 3a are optimized for polarization 304 to form a chiral polarization state due to skyrmions 308. Skyrmions can be viewed as Bloch domain walls similar to one of the Bloch domain walls 200L, 200R described above in the context of Figure 2.

[0123] However, the skyrmion 308 has a curvature that results in a self-closed structure 308. Depending on the chirality of the underlying Bloch domain wall, the skyrmion 308 can be left-handed or right-handed. Figure 3a shows a skyrmion 308 with a counterclockwise sense of rotation 102R, i.e., a right-handed skyrmion 308. The regular arrangement of skyrmions 308 shown in Figure 3a is sometimes referred to as a chiral bubble domain or a cylindrical domain.

[0124] FIG. 3b shows a multilayer structure 312 including an alternating sequence of thin ferroelectric layers 300a, 300b, 300c and paraelectric layers 302a, 303b. For example, the multilayer structure may be formed from alternating layers of ferroelectric lead titanate and dielectric strontium titanate, each having a thickness of 9-10 nm, as described in detail in Yadav et al., Observation of polar vortices in oxide superlattices, Nature 530, 198 (2016). The same growth techniques as described in the context of the thin ferroelectric layer 300 of FIG. 3a are applied to form the ferroelectric layers.

[0125] The multilayer structure 312 of Fig. 3b includes three thin ferroelectric layers 300a, 300b, 300c and two paraelectric layers 302a, 302b, but this is merely an example and the number of layers can generally be freely adapted to the requirements of the application. For example, in optical applications, the number of ferroelectric layers can be increased to at least 10, or at least 50, or at least 100, to produce a multilayer structure 312 with enhanced thickness and optical activity. In contrast, in storage applications, a single ferroelectric layer can be used to minimize the amount of polarization material and maximize switching speed.

[0126] The polarization of the thin ferroelectric layers 300a, 300b, 300c of the multilayer structure 312 forms a-core vortices 314L, 314R. The a-core vortices 314L, 314R in each of the thin ferroelectric layers 300a, 300b, 300c typically alternately swirl in opposite directions. Chirality of the vortices 314L, 314R appears when the vortices have a-core structure and the polarization escapes along the vortex axis in a third spatial direction, forming a helical chiral texture. A dashed line 316 separates the region with the left-handed vortex 314L from the region with the right-handed vortex 314R.

[0127] Any of the chiral structures of the nanostructured ferroelectric, such as the Bloch domain walls 200L, 200R, skyrmions 308, or vortices 314L, 314R, can be either right-handed or left-handed, and the polarization states associated with both chiralities are typically energetically degenerate. As a result, when the nanostructured ferroelectric is cooled from a paraelectric high-temperature state to a ferroelectric room-temperature state, both chiralities can be formed with equal probability. The equal probability of both handednesses being formed can be understood as a direct consequence of the energy degeneracy of the two states. However, the situation can change when an appropriate external stimulus is applied, as will now be explained in more detail below with reference to FIG. 4.

[0128] Figure 4 shows the energy E of the polarization states of nanostructured ferroelectrics as a function of their chirality χ. Figure 4 shows the potential energy landscape of the high temperature paraelectric state 402 (dashed line), the potential energy landscape of the ferroelectric state in the absence of an external stimulus 404, and the potential energy landscapes of the ferroelectric states in the presence of two different external stimuli 404L, 404R.

[0129] Upon cooling through the Curie temperature in the absence of an external stimulus, the polarization state may have an equal probability of transitioning from the paraelectric state potential energy surface 402 to an energy minimum in the ferroelectric state potential energy surface 404 associated with left-handed chirality L and right-handed chirality R. However, by applying an appropriate stimulus, the energy degeneracy of the minima associated with the two chiralities L, R can be lifted. One handedness or chirality may be preferred by the ferroelectric. In FIG. 4, this is reflected in the lower energy of the minimum associated with left-handed chirality L in the potential energy landscape 404L in the presence of an external stimulus.

[0130] The modified external stimulus may result in a potential energy landscape 404R with a lower energy minimum for right-handed chirality R. Thus, if the ferroelectric is cooled from the high-temperature paraelectric state 402 to the low-temperature ferroelectric state in the presence of either of the two stimuli, the ferroelectric may achieve a state of the corresponding energy minimum of the potential energy surface 404L, 404R with the prescribed chirality L, R.

[0131] The stimulus may include electromagnetic radiation, an electric field, a mechanical force, a structural or chemical stimulus. One aspect of the present disclosure relates to the design of a suitable stimulus, as well as methods and devices for applying the stimulus.

[0132] Fig. 5 shows a light-assisted method and apparatus for producing a desired chirality and switching the chirality of a nanostructured ferroelectric according to a first embodiment. According to the embodiment of Fig. 5, the chirality of a thin ferroelectric layer 300 on a substrate 302, which may be similar to the thin ferroelectric layer 300 on the substrate 302 of Fig. 3a, is controlled. However, the method can also be applied to other nanostructured ferroelectrics, for example multi-layer structures such as the multi-layer structure 312 of Fig. 3b.

[0133] The device includes a resistive heater 502 in thermal contact with the substrate 302. Upon application of a supply voltage to the heater 502, the temperature of the heater 502, the substrate 302 and the thin ferroelectric layer 300 increases until the temperature of the ferroelectric layer 300 approaches or exceeds the Curie temperature of the ferroelectric material contained therein, e.g., 400° C. for BaTiO3 or 500° C. for PbTiO3. Upon heating, the ferroelectric material may undergo a phase transition from a room temperature ferroelectric phase to a high temperature paraelectric phase.

[0134] The power supplied to the heater 502 is then reduced and the thin ferroelectric layer 300 is cooled from the paraelectric high temperature phase to a temperature well below the Curie temperature of the ferroelectric material contained in the thin ferroelectric layer 300. Radiative heat transfer from the surface of the thin ferroelectric layer 300 to the environment typically provides sufficient heat transfer for cooling. On the other hand, for a thicker layer 300 and / or substrate 302, the substrate 302 may be coupled to a cooling device, such as a Peltier element, to remove heat from the thin ferroelectric layer 300 more quickly.

[0135] Upon cooling below the Curie temperature, the paraelectric phase may become unstable and a breaking of the symmetry of the local polarization may occur, resulting in the local formation of remnant polarization 304 in the thin ferroelectric layer 300. The thin ferroelectric layer 300 may achieve a polarization structure with an out-of-plane polarization 304, as shown in FIG. 5 and FIG. 3a. To minimize the energy associated with the out-of-plane polarization 304, skyrmions 308 may further be formed surrounding a small region (core) of opposite polarization. Skyrmions 308 may be right-handed or left-handed. As explained in the context of FIG. 4 for any nanostructured ferroelectric, skyrmions 308 of either handedness or chirality may have equal energy and therefore equal probability of forming during cooling in the absence of an external stimulus.

[0136] According to the embodiment shown in Fig. 5, a laser 504 irradiates the thin ferroelectric layer 300 with light or near infrared radiation 506 having a circular polarization 508. Thus, the laser provides an external stimulus that breaks the energy degeneracy between the polarization states 304 of the left-handed skyrmions 308 and the right-handed skyrmions. Depending on the handedness of the circular polarization 508 or the chirality of the light or near infrared radiation 506, the polarization states of the left-handed skyrmions 308 or the right-handed skyrmions 308 are at a global energy minimum and are formed during cooling. The emitted light or near infrared radiation 506 is applied while cooling the thin ferroelectric layer 300 from a high temperature paraelectric state to a temperature well below the Curie temperature. When the nanostructured ferroelectric 300 is cooled, its polarization state can achieve a global minimum on the potential energy surface 504L, 504R with left-handed or right-handed chirality, the chirality being controlled via the helicity of the light or near-infrared radiation 506. In this way, polarization states with left-handed or right-handed skyrmions 308 can be prepared in a controlled manner. By repeating the process steps of heating, applying light or near-infrared radiation 506 of selected helicity, and cooling, the chirality-controlled polarization states can be repeatedly rewritten.

[0137] The embodiment shown in FIG. 5 uses a laser 504 as a source of optical or near infrared radiation 506, more specifically a Ti:sapphire amplifier system emitting laser pulses in the wavelength range of 700-1200 nm at a repetition rate of 1 kHz. The emitted laser pulses can be frequency doubled, tripled or quadrupled. The laser pulses may also be provided by a laser amplifier using a doped fiber. The excitation laser fluence is set to 40-70 mJcm to avoid damage to the nanostructured ferroelectric 300. -2 According to alternative embodiments, terahertz radiation emitted from a quantum cascade laser, microwave radiation from a magnetron, or X-ray radiation from an X-ray tube or synchrotron may be applied.

[0138] According to the embodiment shown in Figure 5, the energy for heating the nanostructured ferroelectric 300 is supplied primarily by a resistive heater 502. Alternatively, a laser 504, or alternative radiation source 504 as described above, may provide most of the energy for heating, or all of it and the resistive heater may be omitted. The energy from the laser or radiation source 504 may be absorbed directly by the nanostructured ferroelectric 300, or may be absorbed by the substrate and subsequently transferred by the substrate 302 towards the nanostructured ferroelectric 300.

[0139] The apparatus 500 of FIG. 5 comprises an additional laser 510 acting as a probe light source emitting a probe light 512. A part of the probe light 512 is reflected from the surface of the thin ferroelectric layer 300, and another part of the probe light 512 is transmitted through the thin ferroelectric layer 300 and is reflected from the substrate 302 before being transmitted through the thin ferroelectric layer 300 again. The polarization of the reflected and / or transmitted probe light 512 can be analyzed using a rotating polarizer 514 acting as a polarimeter together with a photodetector (not shown). Measuring the polarization of the reflected and / or transmitted probe light 512 may make it possible to monitor the polarization, in particular the chirality, of the nanostructured ferroelectric. Instead of using an additional laser 510 as a probe light source, a part of the light or near infrared radiation 506 from the laser 504 may be used to monitor the polarization state.

[0140] Fig. 6a shows a method and apparatus for producing a desired chirality of nanostructured ferroelectrics according to a second embodiment. The apparatus comprises a heater 502, which may be similar to the heater 502 described in the context of the embodiment of Fig. 5. In addition, a counter electrode 602 is provided on the side of the thin ferroelectric layer 300 opposite the substrate 302. When a power supply is applied to the heater 502, the thin ferroelectric layer 300 may be heated to a temperature close to or above the Curie temperature of the ferroelectric material contained in the thin ferroelectric layer 300. During the subsequent cooling of the thin ferroelectric layer 300, a voltage U is applied between the substrate 302 and the counter electrode 602 to generate an electric field 604 through the thin ferroelectric layer 300. The electric field 604 may lift the energy degeneracy between the local minima of the potential energy surface 404 of the thin ferroelectric layer 300. The amplitude of the electric field 604 may be up to 10 kV / cm, or even up to 100 kV / cm, depending on the ferroelectric material and its thickness. Depending on the sign of the voltage U or the direction of the electric field 604, a potential energy surface 404L with a global minimum for the left-handed chirality L of the thin ferroelectric layer or a potential energy surface 404R with a global minimum for the right-handed chirality R of the thin ferroelectric layer can be generated. Thus, by cooling the thin ferroelectric layer 300 in the presence of the electric field 604, a ferroelectric layer 300 with skyrmions 308 of controlled chirality, either left-handed or right-handed, can be prepared.

[0141] Figure 6b shows an embodiment similar to that of figure 6a. However, instead of a single counter electrode, a top electrode 602 and a bottom electrode 606 are provided. A voltage U is applied between the top electrode 602 and the bottom electrode 606, generating an electric field 604. In this way, the electric field 604 can be applied to the nanostructured ferroelectrics 300a, 300b, 300c in the absence of a conductive substrate.

[0142] FIG. 7 shows a method and apparatus for generating a desired chirality and switching the chirality of a nanostructured ferroelectric 300 according to a third embodiment. This embodiment is similar to that described in the context of FIG. 6a. However, a conductive atomic force microscope tip 602' is used as a counter electrode to achieve a strong and localized electric field 604'. This may provide two advantages. First, due to the tip enhancement of the electric field 604', a reduced voltage U' is sufficient to provide an electric field 604' large enough to reliably control the chirality of the polarization state 304 of the thin ferroelectric layer 300. Second, the electric field 604' is spatially confined on the nanometer scale, thus making it possible to write chiral structures 308 with nanometer-sized dimensions into the thin ferroelectric layer 300. This is particularly attractive for (optical) metamaterial generation or storage applications.

[0143] FIG. 7b shows an embodiment similar to that of FIG. 7a, with the difference that the conductive atomic force microscope tip 602″ is chiral and therefore generates a chiral electric field 604″. The right-handed chiral electric field 604″ in FIG. 7b further reduces the energy 404R of the right-handed chiral polarization state of the skyrmion 308 in the thin ferroelectric layer 300, thus assisting in the formation of the right-handed skyrmion 308 when the thin ferroelectric layer 300 is cooled to the ferroelectric phase. The conductive atomic force microscope tip 602″ can be fabricated, for example, by growing or etching the tip 602′ with an overall chiral shape or by applying a torque to the initially achiral tip 602′, prior to use in a scanning probe microscope. Alternatively, the conductive atomic force microscope tip 602″ may have a broadly achiral shape and a chiral molecule, such as a chiral carbon nanotube, may be adsorbed at the very tip, for example by picking it up in the scanning process of the scanning probe microscope. Reservoirs of left-handed and right-handed chiral molecules may be provided in different regions on the substrate 302, and the chirality of the tip 604'' may be altered by picking up chiral molecules from the corresponding regions.

[0144] FIG. 8 shows a cylindrical nanodot 800 hosting a skyrmion 308 on a substrate 302. The skyrmion 308 may be depicted as a curved self-closed domain wall 306, as previously described in the context of FIG. 3a. The rotational orientation 102R of the skyrmion 308 in FIG. 8 is right-handed. Compared to the ferroelectric in the thin ferroelectric film 300, the ferroelectric in the nanodot 800 experiences additional confinement along both directions parallel to the substrate 302, the thin ferroelectric film 300, and / or the surface of the nanodot 800. The additional confinement may improve control over the formation, location, and rotational orientation of the skyrmion 308, while control via the environment, particularly via the choice of substrate 302, is still possible.

[0145] The nanodots 800 are 60 nm in diameter and 30 nm in height. The nanodots can be fabricated by depositing bismuth ferrite on strontium titanate on a porous anodic alumina scaffold, as described in detail in Li et al., "High-density array of ferroelectric nanodots with robust and reversibly switchable topological domain states," Sci. Adv. 3, e1700919 (2017). Alternatively, the nanodots 800 can be fabricated by first depositing a continuous film of ferroelectric material on a flat substrate, followed by structuring the continuous film using lithography (e.g., photolithography, electron beam lithography, ion beam lithography, x-ray lithography) and etching techniques (e.g., wet etching, ion beam etching, reactive ion etching). The nanodots 800 in FIG. 8 are cylindrical, i.e., prisms with a circular base. Lithographic fabrication techniques can be used to fabricate nanodots with prismatic shapes and a wide range of base shapes, providing the option to optimize the shape and size of the nanodot 800 according to the requirements of a particular application. For example, the base may be rectangular and highly elongated (nanorods), square, triangular, or elliptical. The methods and apparatus for producing desired chirality in nanostructured ferroelectrics according to the present disclosure are applicable to nanodots having any of these shapes.

[0146] 9a and 9b show nanoparticles 900a, 900b. Within the context of the present disclosure, nanodots 800 may have a polarization structure with chirality that depends on the presence of domain walls 306, while nanoparticles 900a, 900b may have a polarization state with chirality even in the absence of domain walls.

[0147] The nanoparticles 900a, 900b shown in Figures 9a and 9b are spherical and have a diameter of 30 nm. The nanoparticles may be made using solvothermal and hydrothermal methods. Alternatively, the nanoparticles 900a, 900b may be produced using sol-gel synthesis, peroxo-oxalate complexation, non-isothermal decomposition, or by any combination of these techniques. The size and shape can be adjusted by the selection of the ferroelectric material and preparation conditions. For example, faceted, generally approximately spherical, pyramidal, cubic, rectangular, icosahedral, or dodecahedral shapes may be achieved. The nanoparticles may also have one of the shapes described in connection with the nanodots 800.

[0148] 9a and 9b show two examples of nanoparticles 900a, 900b with polarization states 304 exhibiting chirality. The polarization states of the nanoparticles 900a, 900b may depend on the preparation conditions and / or previous treatment with an external stimulus such as an external electric field. The preparation conditions and external field treatment may be adjusted to achieve, for example, a vortex state, a hopfion, or a skyrmion state. Details are given in Luk'yanchuk et al. "Hopfions emerge in ferroelectrics," Nat. Commun. 11, 2433 (2020)).

[0149] The methods and apparatus for generating desired chirality in nanostructured ferroelectrics described in Figures 4, 5, 6a, 6b, 7a and 7b can also be applied to nanodots 800 and nanoparticles 900a, 900b as nanostructured ferroelectrics for generating desired chirality. The disclosures related to Figures 10a, 10b, 11a, 11b, 12a and 12b refer to the corresponding parts of the disclosures above, and similar components will not be described again. Only aspects of the methods and apparatus related to their specific application to nanodots 800 and nanoparticles 900a, 900b are pointed out.

[0150] Figure 10a shows a light-assisted method and apparatus 500' for generating a desired chirality and switching the chirality of nanodots 800 or nanoparticles 900a, 900b, similar to the embodiment described in the context of Figure 5 for a thin ferroelectric film. Although a nanodot 800 having a cylindrical shape is shown in Figure 10a, the method can be applied to any of the nanodots 800 or nanoparticles 900a, 900b described above in connection with Figures 8, 9a and 9b.

[0151] FIG. 10b shows an embodiment similar to that of FIG. 10a. In this embodiment, the nanodots 800 or nanoparticles 900a, 900b are embedded in a solid or liquid matrix 302′, rather than being supported on a substrate 302. Surrounding the nanodots 800 or nanoparticles 900a, 900b by the solid or liquid matrix 302′ provides a very efficient path for carrying heat away from the nanodots 800 or nanoparticles 900a, 900b, and thus allows them to be cooled effectively. Thus, the material forming the solid or liquid matrix 302′ can be selected to provide an optimized thermal conductivity. According to an embodiment, a portion of the light or near infrared radiation 506 from the laser 504 can be used for the polarimeter 514 to monitor the polarization state of the nanodots 800 or nanoparticles 900a, 900b. However, an additional probe light source may be provided, for example, to illuminate the nanodots 800 or nanoparticles 900a, 900b along a direction perpendicular to the direction of the light or near infrared radiation 506.

[0152] Figures 11a and 11b show an embodiment similar to that of Figure 6b. An upper electrode 602 and a lower electrode 606 are arranged on opposite sides of a nanodot 800 or nanoparticle 900a, 900b. By applying a voltage U between the electrodes 602, 606, an electric field 604 is generated which can act as a stimulus to generate a polarization state with a desired chirality while cooling the nanodot 800 or nanoparticle 900a, 900b. In Figure 11b, the voltage -U applied between the upper electrode 602 and the lower electrode 606 is reversed compared to the voltage U applied in Figure 11a, resulting in a reversal of the chirality of the polarization state of the nanodot 800 or nanoparticle 900a, 900b.

[0153] According to one embodiment, the bottom electrode 606 is provided by a conductive substrate.

[0154] According to one embodiment, the nanodots 800 or nanoparticles 900a, 900b can be deposited on the bottom electrode from a suspension or solution by dip coating or spin coating. The concentration of the nanodots 800 or nanoparticles 900a, 900b in the suspension or solution can be selected to control the density of deposited nanodots 800 or nanoparticles 900a, 900b per area on the bottom electrode 606. In particular, the concentration can be selected to achieve a density low enough to have a single nanodot 800 or nanoparticle 900a, 900b in the electric field 604, if required by the application. Other applications may require a larger number of nanodots 800 or nanoparticles 900a, 900b in the field, which can be easily achieved by applying a suspension or solution with a high concentration of nanodots 800 or nanoparticles 900a. A top electrode can be deposited on top of the deposited nanodots 800 or nanoparticles 900a, 900b. Prior to depositing the top electrode, a matrix, in particular a dielectric matrix, may be deposited around the nanodots 800 or nanoparticles 900a, 900b, in particular to provide a propagation path for electromagnetic radiation to heat the nanodots 800 or nanoparticles 900a, 900b. The matrix may be optimized to enhance thermal conductivity to facilitate cooling of the nanodots 800 or nanoparticles 900a, 900b.

[0155] In an alternative embodiment, the electrodes 602, 606 may be arranged in a single plane, for example as a finger structure on a surface. The nanodots 800 or nanoparticles 900a, 900b may be deposited between the electrodes 602, 606 from a suspension or solution. The density of the deposited nanodots 800 or nanoparticles 900a, 900b may be controlled by the concentration of the suspension or solution, as described above. Either or both of the electrodes 602, 606 may also function as a resistive heater to heat the nanodots 800 or nanoparticles 900a, 900b.

[0156] Figure 12a shows an embodiment similar to that of Figure 7a. Using the tip 602' as a top electrode, an electric field 604' can be selectively applied to individual nanodots 800 or nanoparticles 900a, 900b of a plurality of nanodots 800 or nanoparticles 900a, 900b present on the substrate 302.

[0157] Figure 12b shows an embodiment similar to that of Figure 7b. Using a chiral tip 602'' as a top electrode, an electric field 604' can be selectively applied to individual nanodots 800 or nanoparticles 900a, 900b of a plurality of nanodots 800 or nanoparticles 900a, 900b present on a substrate 302.

[0158] 13 illustrates an embodiment using enantioselective transport of nanodots 800 or nanoparticles 900a, 900b from a collection 1304 of nanodots 800 or nanoparticles 900a, 900b. The collection 1304 can include both left-handed nanodots or nanoparticles 1304L and right-handed nanodots or nanoparticles 1304R. The optical tweezers 1300 consist of a light source (not shown) for generating light or near-infrared radiation 506 having circular polarization 508 and a microscope objective lens 1302 for tightly focusing the light or near-infrared radiation 506. The tight focusing can generate a gradient of the light or near-infrared radiation 506, resulting in a force on the nanodots 800 or nanoparticles 900a, 900b of the collection 1304. The force on the nanodots 800 or nanoparticles 900a, 900b may depend on the chirality of the nanodots 800 or nanoparticles 900a, 900b and the circular polarization 508 of the light or near infrared radiation 506. The circular polarization 508 may be selected to selectively transport nanodots 800 or nanoparticles 900a, 900b of a preselected chirality. In the example shown in Figure 13, the light or near infrared radiation 506 with right-handed circular polarization 508 transports only nanodots 800 or nanoparticles 1304R of the set 1304 with right-handed chirality.

[0159] In the method according to the embodiment of FIG. 13, light or near infrared radiation 506 heats the collection 1304 of nanodots 800 or nanoparticles 900a, 900b to a paraelectric state. Alternatively or additionally, the collection 1304 may be heated using a resistive heater 502 in thermal contact with the substrate 302. The heating power can then be reduced and the collection 1304 can be cooled. The selected circular polarization 508 may determine the resulting chirality of the polarization state of the nanodots 800 or nanoparticles 900a, 900b. Once the nanodots 800 or nanoparticles 900a, 900b have cooled to a ferroelectric state and achieved a preselected chirality, enantioselective transport can be applied to move the nanodots 800 or nanoparticles 900a, 900b of a given chirality to a target destination location or remove the nanodots 800 or nanoparticles 900a, 900b of the opposite chirality. In this way, the chirality purity of the nanodots 800 or collection 1304 of nanoparticles 900a, 900b can be further improved.

[0160] Figure 14 shows another embodiment using enantioselective transport of nanodots 800 or nanoparticles 900a, 900b from a collection 1304 of nanodots 800 or nanoparticles 900a, 900b. This embodiment is similar to that of Figure 13. However, instead of optical tweezers 1300, plasmonic tweezers 1400 are applied. Thus, light or near-infrared radiation 506 with linear polarization 508' is focused onto the conductive substrate 302 using a microscope objective lens 1302. The linear polarization or near-infrared radiation 506 can induce plasmonic excitations in the conductive substrate 302, which can exert a force on the collection 1304 of nanodots 800 or nanoparticles 900a, 900b. Typical plasmonic trap stiffness can vary from 0.1 to 1 and 5 fN / (μm×mW). The forces experienced by nanodot 800 or nanoparticle 900a may be different for left-handed nanodot or nanoparticle 1304L and right-handed nanodot or nanoparticle 1304R. Thus, left-handed nanodot or nanoparticle 1304L and right-handed nanodot or nanoparticle 1304R may be transported to different regions on surface 302 and thereby separated.

[0161] The description of the embodiments and drawings only serves to illustrate the techniques of the present disclosure and the advantages associated therewith, and should not be construed as meaning any limitation. The scope of the present disclosure should be determined from the appended claims.

Claims

1. A method for producing a nanostructured ferroelectric material (300, 300a, 300b, 300c, 800, 900a, 900b) having a predetermined chirality, comprising the steps of: the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) is adapted to provide a high temperature state and a low temperature ferroelectric state and adapted to provide a remanent polarization, a first extension dimension of the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) along a first direction is up to 1000 nm; In the low temperature ferroelectric state, the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) has a polarization state from a plurality of polarization states; The plurality of polarization states includes at least a first chiral polarization state having a first chirality (102R) and a second chiral polarization state having a second chirality (102L) different from the first chirality (102R); The method comprises: selecting the predetermined chirality from the first chirality (102R) and the second chirality (102L); selecting an electromagnetic field (506, 604, 604', 604'') according to said predetermined chirality; providing said nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) at said elevated temperature; applying said electromagnetic field (506, 604, 604', 604'') to said nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) at said elevated temperature; cooling the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) from the high temperature state to the low temperature ferroelectric state while applying the electromagnetic field (506, 604, 604', 604'') to establish the polarization state of the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) having the predetermined chirality; A method comprising:

2. The method of claim 1, wherein the first extension dimension is up to 100 nm.

3. The method of claim 1 , wherein the high temperature state is a paraelectric or ferroelectric state at high temperature.

4. The method of claim 1 , wherein the low temperature ferroelectric state corresponds to a room temperature state of the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b).

5. The method of claim 1 , wherein applying the electromagnetic field (506) comprises irradiating the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) with an electromagnetic wave (506).

6. 6. The method of claim 5, wherein the electromagnetic wave (506) is elliptically polarized, and a chirality (508) of the elliptically polarized electromagnetic wave (506) corresponds to the predetermined chirality.

7. The method of claim 1, further comprising supporting the nanostructured ferroelectric material (300, 300a, 300b, 300c, 800, 900a, 900b) by a substrate (302) while applying the electromagnetic field (506, 604, 604', 604'').

8. 2. The method of claim 1, wherein the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) is surrounded by a solid or liquid matrix (302') while the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) is cooled.

9. During and / or after cooling the nanostructured ferroelectrics (300, 300a, 300b, 300c, 800, 900a, 900b) from the high temperature state to the low temperature ferroelectric state, 2. The method of claim 1, further comprising applying a non-uniform electromagnetic field to the nanostructured ferroelectric material (300, 300a, 300b, 300c, 800, 900a, 900b) to transport the nanostructured ferroelectric material (300, 300a, 300b, 300c, 800, 900a, 900b) to a position associated with the predetermined chirality.

10. 10. The method of claim 9, wherein the inhomogeneous electromagnetic field (506, 604, 604', 604'') has a field polarization (508, 508'), the method further comprising selecting the field polarization (508, 508') according to the predetermined chirality.

11. 2. The method of claim 1, wherein applying the electromagnetic field (604, 604', 604'') comprises applying a voltage (U, -U) to electrodes (602, 602', 602'', 606) disposed on opposite sides of the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b).

12. The method of claim 11 , wherein at least one of the electrodes (602″) has a chiral shape that provides a chiral electromagnetic field (604″) as the electromagnetic field (604″).

13. Providing the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) in the high temperature state, providing the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) in the low temperature ferroelectric state and having the first chirality (102R); heating said nanostructured ferroelectrics (300, 300a, 300b, 300c, 800, 900a, 900b) to said elevated temperature state; The method of any one of claims 1 to 12, wherein the predetermined chirality is the second chirality (102L).

14. The method of claim 1, wherein the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) comprises lead titanate, lead zirconate titanate, zirconium oxide, hafnium zirconium oxide, hafnium oxide, or silicon doped hafnium oxide.

15. An apparatus for producing a nanostructured ferroelectric material (300, 300a, 300b, 300c, 800, 900a, 900b) having a predetermined chirality, comprising: a holding element (302, 302') adapted to receive said nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b); a heating element (502, 504) adapted to heat the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) to a high temperature state; a field application element (504, 602, 602', 602'', 606) adapted to apply an electromagnetic field (506, 604, 604', 604'') to the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) while the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) is in the high temperature state; a cooling element adapted to cool the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) to a low temperature ferroelectric state having a polarization state with the predetermined chirality while applying the electromagnetic field (506, 604, 604', 604'') to the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) using the field application element; Equipped with 1. A device comprising: a nanostructured ferroelectric material (300, 300a, 300b, 300c, 800, 900a, 900b) adapted to provide a remanent polarization, and a first extension dimension of the nanostructured ferroelectric material (300, 300a, 300b, 300c, 800, 900a, 900b) along a first direction is up to 1000 nm.

16. a radiation source (504) adapted to generate an electromagnetic wave (506) and further adapted to irradiate the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) with the electromagnetic wave (506); 16. The apparatus of claim 15, wherein the radiation source (504) is included in optical tweezers adapted to transport the nanostructured ferroelectric to a position associated with the predetermined chirality and / or to separate the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) from a second nanostructured ferroelectric having a chirality different from the predetermined chirality.

17. The device of claim 15 or 16, wherein the nanostructured ferroelectric (300, 300a, 300b, 300c, 800, 900a, 900b) comprises lead titanate, lead zirconate titanate, zirconium oxide, hafnium zirconium oxide, hafnium oxide, or silicon doped hafnium oxide.

Citation Information

Patent Citations

  • Insulation material and manufacturing method therefor

    JP2014078560A

  • Integrated metal complex

    JP2015072427A

  • Chirality detection device, chirality detection method, separation device, separation method, and chiral substance device

    WO2020230893A1