Ceramics

A ceramic structure with a monoclinic zirconia second layer enhances the fracture resistance of a stabilized zirconia first layer by creating compressive stress, addressing the issue of low strength in ceramics.

JP7562271B2Active Publication Date: 2024-10-07NITERRA CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020045329
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-03-16
Publication Date
2024-10-07
Estimated Expiration
2040-03-16

AI Technical Summary

Technical Problem

Ceramics made of stabilized zirconia are prone to breaking due to low strength in the first layer.

Method used

A ceramic structure comprising a first layer of stabilized or partially stabilized zirconia, a second layer of monoclinic zirconia, and optionally a third layer of an oxide, where the second layer's smaller linear expansion coefficient creates compressive stress, enhancing the fracture resistance of the first layer.

Benefits of technology

The compressive stress in the second layer prevents the first layer from fracturing, thereby increasing the ceramic's fracture toughness and preventing deformation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007562271000002
    Figure 0007562271000002
  • Figure 0007562271000001
    Figure 0007562271000001
Patent Text Reader

Abstract

To provide a ceramic that makes it difficult to break a first layer containing stabilized zirconia or partially stabilized zirconia.SOLUTION: A ceramic includes a first layer and a second layer, and in which the first layer contains stabilized zirconia or partially stabilized zirconia, and the second layer contains monoclinic zirconia.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to ceramics containing zirconia. [Background technology]

[0002] Stabilized zirconia and partially stabilized zirconia are used for various purposes such as machine parts, electrical parts, etc. Patent Document 1 discloses ceramics having a support layer (first layer) made of Ca-containing stabilized zirconia. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-113714 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, the above technique has a problem in that if the strength of the first layer made of stabilized zirconia is low, the ceramic is easily broken.

[0005] The present invention has been made to solve this problem, and has an object to provide a ceramic that can make the first layer, which contains stabilized zirconia or partially stabilized zirconia, less susceptible to fracture. [Means for solving the problem]

[0006] To this end, the ceramic of the present invention comprises a first layer and a second layer, the first layer comprising stabilized zirconia or partially stabilized zirconia, and the second layer comprising monoclinic zirconia. Effect of the Invention

[0007] According to the ceramics described in claim 1, since monoclinic zirconia has a smaller linear expansion coefficient than stabilized zirconia or partially stabilized zirconia, compressive stress remains in the second layer of the ceramics produced through a firing process due to the difference between the linear expansion coefficient of the first layer and the linear expansion coefficient of the second layer. Since the fracture toughness has little effect on the fracture strength of ceramics under compressive stress, the first layer, which is affected by the compressive stress of the second layer, can be made less susceptible to fracture.

[0008] According to the ceramics of claim 2, the thickness of the second layer is 74 μm or less, so that the compressive load of the second layer can be prevented from becoming excessive. Therefore, in addition to the effect of claim 1, damage and deformation of the second layer can be prevented.

[0009] According to the ceramics described in claim 3, a second layer is disposed between the third layer containing an oxide and the first layer, so that in addition to the effects of claim 1 or 2, the function of the third layer can be added to the ceramics. [Brief description of the drawings]

[0010] [Figure 1] FIG. 2 is a cross-sectional view of a ceramic according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, preferred embodiments of the present invention will be described with reference to the accompanying drawings. Fig. 1 is a cross-sectional view including a central axis O of a ceramic 10 in one embodiment. In this embodiment, the ceramic 10 is a cylindrical tube. Fig. 1 illustrates one side of the ceramic 10 with respect to the central axis O, and the other side of the central axis O is omitted.

[0012] The ceramic 10 includes, in that order, a first layer 11, a second layer 12, and a third layer 13. The ceramic 10 is manufactured through the steps of forming and firing the first layer 11, the second layer 12, and the third layer 13. In this embodiment, the second layer 12 is fixed to the outer periphery of the first layer 11, and the third layer 13 is fixed to the outer periphery of the second layer 12. In this embodiment, the ceramic 10 has a function of permeating oxygen in the thickness direction.

[0013] The first layer 11 includes stabilized zirconia or partially stabilized zirconia. Stabilized zirconia is zirconia in which oxides (stabilizers) such as CaO, MgO, Y2O3, Sc2O3, and Yb2O3 are dissolved in ZrO2 so that cubic crystals are stable at room temperature. Partially stabilized zirconia is zirconia in which the amount of stabilizer is reduced compared to the amount of stabilizer in stabilized zirconia, and cubic crystals and tetragonal crystals are dispersed at room temperature. Stabilized zirconia and partially stabilized zirconia function as oxygen ion conductors.

[0014] In addition to stabilized zirconia or partially stabilized zirconia, the first layer 11 may contain other oxygen ion conductors, electronic conductors, or oxides that have both oxygen ion conductivity and electronic conductivity (hereinafter referred to as "mixed conductive oxides").

[0015] Other oxygen ion conductors include, for example, ceria-based solid solutions, such as cerium-based composite oxides, such as gadolinium-doped ceria and samarium-doped ceria.

[0016] The electron conductor may be selected from oxides having a perovskite structure, oxides having a spinel crystal structure, and metal materials such as precious metals. Examples of oxides having a perovskite structure include oxides in which Sr is added to the La site in a LaMnO3 compound, composite oxides such as CaTiO3 and BaTiO3, and La 1-X M X CrO 3-Z(wherein M is an alkaline earth metal excluding Mg, 0≦X≦0.4, and Z is a value indicating that the ratio of metal elements or the amount of oxygen atoms varies.)

[0017] Examples of mixed conductive oxides include oxides having a perovskite structure in which Sr is added to the La site and Fe is added to the Ga site in a LaGaO3 compound, oxides having a perovskite structure in which Ba is added to the Sr site and Fe is added to the Co site in a SrCoO3 compound, oxides having a layered perovskite structure, oxides having a fluorite structure, oxides having an oxyapatite structure, and oxides having a melilite structure.

[0018] The first layer 11 may contain a catalyst. Examples of the catalyst include metals such as Ni, Co, and Cu, and precious metals such as Rh and Pt. The first layer 11 may be porous. When the first layer 11 is porous, the weight of the first layer 11 can be reduced compared to when the first layer 11 is dense. When the first layer 11 is porous, the mechanical strength is generally lower compared to when the first layer 11 is dense, so the effect of increasing the mechanical strength of the first layer 11 by the second layer 12 becomes significant. When the first layer 11 is porous, the porosity of the first layer 11 is, for example, 20 to 60%, preferably 30 to 50%.

[0019] The porosity of the first layer 11 can be obtained from a scanning electron microscope (SEM) image of a cross section of the ceramic 10. The porosity is a percentage obtained by dividing the sum of the areas of the pores surrounded by the first layer 11 that appear within the SEM field of view by the sum of the areas of the first layer 11 and the pores within the field of view.

[0020] The second layer 12 contains monoclinic zirconia. The monoclinic zirconia contained in the second layer 12 can be qualitatively analyzed by Raman spectroscopy. A laser Raman microscope is used to obtain a Raman scattering spectrum of a cross section of the ceramic 10, and the portion where a vibration mode specific to monoclinic crystals is recognized is the second layer 12.

[0021] The second layer 12 may contain at least one of tetragonal zirconia and cubic zirconia in addition to monoclinic zirconia. Tetragonal zirconia and cubic zirconia can also be qualitatively analyzed by Raman spectroscopy. At least a part of the elements constituting the compound of the third layer 13 may be contained in the second layer 12. However, the compositions of the first layer 11 and the second layer 12 are set so that the linear expansion coefficient of the second layer 12 from room temperature to 1000°C is smaller than the linear expansion coefficient of the first layer 11 from room temperature to 1000°C.

[0022] Since the monoclinic zirconia contained in the second layer 12 has a smaller linear expansion coefficient than the stabilized zirconia or partially stabilized zirconia contained in the first layer 11, compressive stress remains in the second layer 12 of the ceramic 10 manufactured through the molding and firing processes due to the difference between the linear expansion coefficients of the first layer 11 and the second layer 12. Since the fracture toughness has little effect on the fracture strength of the ceramic 10 under compressive stress, the first layer 11 bonded to the second layer 12 can be made less susceptible to fracture.

[0023] It is preferable to form the second layer 12 such that, in the vicinity of the interface 14 between the second layer 12 and the first layer 11, the band intensity of the monoclinic crystal appearing in the Raman scattering spectrum in the second layer 12 decreases toward the interface 14. Since the band intensity appearing in the Raman scattering spectrum is proportional to the concentration of monoclinic zirconia, by decreasing the concentration of monoclinic zirconia toward the interface 14, the difference between the linear expansion coefficient of the first layer 11 and the linear expansion coefficient of the second layer 12 can be buffered near the interface 14.

[0024] The thickness of the second layer 12 is preferably thinner than that of the first layer 11. This is to prevent the first layer 11 from being deformed by the compressive stress remaining in the second layer 12. The thickness of the second layer 12 is preferably 5 μm to 100 μm. When the thickness of the second layer 12 is in this range, the compressive load of the second layer 12 can be made appropriate, and therefore, depending on the thickness of the first layer 11, deformation or damage of the first layer 11 and the second layer 12 can be suppressed. The thickness of the first layer 11 is preferably 0.5 mm to 3 mm. This is to allow the compressive stress of the second layer 12 to affect a wide range in the thickness direction of the first layer 11.

[0025] The second layer 12 may contain a catalyst. Examples of the catalyst include metals such as Ni, Co, and Cu, and noble metals such as Rh and Pt. The second layer 12 may be porous.

[0026] The third layer 13 contains an oxide. Examples of the oxide contained in the third layer 13 include one or more selected from oxygen ion conductors such as stabilized zirconia, partially stabilized zirconia, and ceria-based solid solutions, electronic conductors, and mixed conductive oxides. The ceria-based solid solutions, electronic conductors, and mixed conductive oxides contained in the third layer 13 are the same as those described for the first layer 11. For the stabilized zirconia or partially stabilized zirconia of the third layer 13, zirconia in which a stabilizer different from the stabilizer of the stabilized zirconia or partially stabilized zirconia contained in the first layer 11 is used.

[0027] The third layer 13 can contain a catalyst. Examples of the catalyst include metals such as Ni, Co, and Cu, and precious metals such as Rh and Pt. By bonding the oxide-containing third layer 13 to the second layer 12, the function of the third layer 13 can be imparted to the ceramic 10.

[0028] The thickness of the third layer 13 is preferably thinner than that of the first layer 11. In addition, the sum of the thickness of the second layer 12 and the thickness of the third layer 13 is preferably thinner than the thickness of the first layer 11. This is because the compressive stress remaining in the second layer 12 in the presence of the third layer 13 is allowed to affect the first layer 11.

[0029] The ceramic 10 is manufactured, for example, as follows. First, a compact for the first layer 11 is prepared. The compact for the first layer 11 is made by mixing a pore-forming agent, such as synthetic resin beads or carbon powder, and a binder with a powder of a specific oxide, and then extrusion molding, press molding, or the like. The porosity of the first layer 11 is set by the particle size and amount of the pore-forming agent, etc.

[0030] Next, the paste constituting the second layer 12 is applied to the surface of the molded body of the first layer 11 and dried to form the molded body of the second layer 12. Next, the paste constituting the third layer 13 is applied to the surface of the molded body of the second layer 12 and dried to form the molded body of the third layer 13. The paste constituting the second layer 12 and the paste constituting the third layer 13 are made by mixing a vehicle with a powder of a specified oxide. The paste is applied by a printing method, a spraying method, a dip coating method, a doctor blade method, or the like. In this way, the molded bodies of the first layer 11, the second layer 12, and the third layer 13 are integrated.

[0031] Next, the compact is fired. Through the firing process, ceramic 10 is obtained in which first layer 11, second layer 12, and third layer 13 are bonded to each other. During the firing process, from when the maximum temperature is reached until the temperature returns to room temperature, compressive stress remains in second layer 12 of ceramic 10 due to the difference between the linear expansion coefficient of first layer 11 and the linear expansion coefficient of second layer 12. This makes ceramic 10 less likely to break.

[0032] The production of the molded body is not limited to extrusion molding and paste coating. It is of course possible to produce the molded body by other known methods. Examples of other methods include sheet molding, sheet lamination, press molding, etc.

[0033] The green body is not limited to one in which a green body for the second layer 12 is formed on the surface of a green body for the first layer 11, and a green body for the third layer 13 is formed on the surface of the green body for the first layer 12. For example, one in which a green body for the third layer 13 is formed on the surface of a green body for the first layer 11 can be used. In the step of firing this green body, the second layer 12 can be formed between the first layer 11 and the third layer 13 due to diffusion between the elements constituting the oxide of the first layer 11 and the elements constituting the oxide of the third layer 13. EXAMPLES

[0034] The present invention will be described in more detail with reference to examples, but the present invention is not limited to these examples.

[0035] (Preparation of test specimens) Powders of calcia-stabilized zirconia, acrylic pore former, and catalyst (Pt) were mixed with a binder, and extrusion molding was performed to obtain a plate-shaped molded body (first layer molded body) with a thickness of about 3 mm. Separately, powders of monoclinic zirconia, acrylic pore former, and catalyst (Pt) were mixed with a vehicle to obtain a paste for the second layer. This paste was printed on the entire surface of the first layer molded body. The printing thickness of the paste was varied for each molded body to obtain various molded bodies with different printing thicknesses. This molded body was fired (maximum temperature 1500°C) to obtain ceramics in which the first layer and the second layer were bonded to each other. The factors other than the thickness of the second layer when obtaining the ceramics were the same.

[0036] The obtained ceramics were cut into rectangles measuring 3 mm in width and 40 mm in length to prepare test pieces in which a first layer was laminated with a second layer. The surface of the first layer of each test piece opposite the surface to which the second layer was attached was polished to make the thickness of each test piece uniform at 2 mm. The average porosity of the first layer of each test piece was 40%.

[0037] At the center position of the length of the test piece, Raman scattering spectra were obtained at 2 μm intervals in the thickness direction from the surface of the second layer of the cut surface (side surface of the test piece) by Raman spectroscopy, and the distance M from the surface at which the vibration mode specific to the monoclinic crystal was no longer observed was measured. Since the vibration mode specific to the monoclinic crystal was observed at a position 2 μm closer to the surface than the distance M, the distance N between that position and the surface (distance N = distance M - 2 μm) was taken as the thickness of the second layer of each test piece. Five test pieces were selected for each thickness of the second layer.

[0038] (Calculation of bending strength) In accordance with JIS R1601:2008, the second layer of the test piece was placed on the supports of a support with a support distance of 30 mm, and a load was applied to one point in the center of the first layer between the supports. The maximum bending stress (three-point bending strength) when the test piece broke was calculated, and the average bending strength of five test pieces was obtained. Table 1 shows the relationship between the thickness (μm) of the second layer and the average three-point bending strength (MPa). Test piece No. 1 was made by firing (maximum temperature 1500°C) a molded body of the first layer (one with no paste printed on the surface) to a dimension of 3 mm in width, 40 mm in length, and 2 mm in thickness.

[0039] [Table 1] As shown in Table 1, it was found that test pieces No. 2 to No. 7, in which a second layer was formed with a thickness in the range of 2 to 74 μm, had a greater bending strength than test piece No. 1, in which a second layer was not formed. The second layer of the test piece was placed on the fulcrum of the support, and a load was applied to a single point in the center of the first layer between the fulcrums, so tensile stress was applied to the second layer during this bending test. It is presumed that the bending strength of the test piece increased because compressive stress remained in the second layer.

[0040] The present invention has been described above based on an embodiment, but the present invention is in no way limited to the above embodiment, and it can be easily inferred that various improvements and modifications are possible within the scope of the present invention without departing from the spirit of the present invention.

[0041] In the embodiment, the ceramic 10 is a cylindrical tube, but this is not necessarily limited to this. The ceramic 10 can be in any shape, such as a flat plate, a curved plate, or a bent tube.

[0042] In the embodiment, the ceramic 10 has a function of an oxygen permeable membrane, but the use of the ceramic 10 is not limited to this. The ceramic 10 can be used for any purpose, such as a mechanical part or an electric part. Therefore, it is possible for the first layer 11 to contain other oxides, such as alumina or mullite, instead of an ion conductor or an electron conductor.

[0043] In the embodiment, the ceramic 10 in which the first layer 11, the second layer 12, and the third layer 13 are laminated in this order has been described, but the present invention is not necessarily limited to this. It is of course possible to place a fourth layer between the first layer 11 and the second layer 12, or to laminate a fourth layer on the third layer 13. When the fourth layer is placed between the first layer 11 and the second layer 12, the third layer 13 can be omitted. The fourth layer contains an oxide. The oxide contained in the fourth layer may be the same as the oxide contained in the third layer 13.

[0044] When a fourth layer is disposed between the first layer 11 and the second layer 12, the thickness of the second layer 12 plus the thickness of the fourth layer is preferably thinner than the thickness of the first layer 11. This is to ensure that the compressive stress remaining in the second layer 12 is effective on the first layer 11 in the presence of the fourth layer.

[0045] When the fourth layer is laminated on the third layer 13, the thickness of the second layer 12 and the third layer 13 plus the thickness of the fourth layer is preferably thinner than the thickness of the first layer 11. This is to ensure that the compressive stress remaining in the second layer 12 in the presence of the third layer 13 and the fourth layer affects the first layer 11. In this case, it is of course possible for the fourth layer to be a layer containing a catalyst made of a metal such as Ni, Co, Cu, or a precious metal such as Rh or Pt. [Explanation of symbols]

[0046] 10. Ceramics 11 First Layer 12 Second Layer 13 The Third Layer

Claims

1. A ceramic including a first layer and a second layer, the first layer comprises stabilized zirconia or partially stabilized zirconia; the second layer comprises monoclinic zirconia; The first layer is a porous ceramic having a porosity of 20 to 60%.

2. 2. The ceramic according to claim 1, wherein the second layer has a thickness of 74 μm or less.

3. a third layer comprising an oxide; The ceramic according to claim 1 or 2, wherein the second layer is disposed between the first layer and the third layer.

Citation Information

Patent Citations

  • Zirconia oxygen sensor element

    JP1988210063A

  • High-strength calcined compact of zirconia and production thereof

    JP1989208367A

  • Zirconia porcelain and electrochemical cell utilizing the same

    JP1992342461A

  • ZrO2 SINTERED COMPACT AND ITS MANUFACTURING METHOD, MEMBER OF CRUSHER, AND CRUSHER

    JP2006298711A

  • Oxygen permeation membrane, method for manufacturing same, and reformer

    JP2017113714A