Crystal pulling furnace for producing single crystal silicon ingot, method and single crystal silicon ingot

The crystal pulling furnace with dual heat treatment devices addresses non-uniform BMD concentration in single crystal silicon ingots by applying tailored heat treatments, resulting in improved silicon wafer quality and yield.

JP7562846B2Active Publication Date: 2024-10-07XIAN ESWIN MATERIAL TECHNOLOGY CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023515716
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-09-30
Filing Date
2022-09-29
Publication Date
2024-10-07
Estimated Expiration
2042-09-29

AI Technical Summary

Technical Problem

The existing Czochralski method for producing single crystal silicon ingots results in non-uniform bulk microdefect (BMD) concentration due to varying nitrogen content along the ingot, affecting the quality and yield of silicon wafers.

Method used

A crystal pulling furnace with dual heat treatment devices applying different temperatures to uniformly distribute BMD concentration by melting and forming BMDs at specific regions of the ingot during the pulling process.

Benefits of technology

Achieves a monocrystalline silicon ingot with uniform BMD concentration, enhancing the quality and yield of silicon wafers by optimizing BMD distribution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007562846000001
    Figure 0007562846000001
  • Figure 0007562846000002
    Figure 0007562846000002
  • Figure 0007562846000003
    Figure 0007562846000003
Patent Text Reader

Abstract

The present invention provides a crystal pulling furnace, a method, and a single crystal silicon ingot for producing a single crystal silicon ingot. The crystal pulling furnace includes a pulling mechanism configured to pull a single crystal silicon ingot by the Czochralski method using a nitrogen-doped silicon melt, a first heat treater for heat treating the single crystal silicon ingot at a first heat treatment temperature to melt BMDs in the single crystal silicon ingot, and a second heat treater disposed above the first heat treater for heat treating the single crystal silicon ingot at a second heat treatment temperature to form BMDs in the single crystal silicon ingot. The pulling mechanism is further configured to move the single crystal silicon ingot in a crystal pulling direction to a position where its rear end is heat treated in the first heat treater and its front end is heat treated in the second heat treater.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to Chinese Patent Application No. 202111165968.6, filed in China on September 30, 2021, the entire contents of which are incorporated herein by reference.

[0002] The present application relates to the field of semiconductor silicon wafer manufacturing, and in particular to a crystal pulling furnace for producing a single crystal silicon ingot, a method, and a single crystal silicon ingot. [Background technology]

[0003] As is well known, current integrated circuits are mainly fabricated in the near-surface layer within 5 microns from the surface of a silicon wafer. Therefore, in order to introduce a defect region in the body or backside of the silicon wafer and to introduce a defect-free, impurity-free clean region of 10 to 20 microns near the surface, a technology such as intrinsic gettering or extrinsic gettering is required. In recent years, in addition to the general intrinsic gettering and extrinsic gettering technology, new oxygen annealing technology, rapid thermal processing technology and nitrogen doping technology have been developed and applied.

[0004] In the above integrated circuit, it is very advantageous to provide a silicon wafer having a denuded zone (DZ) extending from the front side into the body and a region including bulk microdefects (BMD) adjacent to the DZ and extending further into the body. The front side here refers to the surface of the silicon wafer on which electronic components are formed. The above DZ is important because, in order to form electronic components on a silicon wafer, it is required that the electronic component formation region is free of crystalline defects, otherwise it may cause failures such as circuit breaks, and by forming the electronic components in the DZ, the influence of crystalline defects can be avoided. The role of the above BMD is to have an intrinsic gettering (IG) effect on metal impurities, and by keeping the metal impurities in the silicon wafer away from the DZ, adverse effects such as an increase in leakage current due to metal impurities and deterioration of the quality of the gate oxide film can be avoided.

[0005] In the manufacture of the above-mentioned silicon wafer having the BMD region, it is very advantageous to dope the silicon wafer with nitrogen. For example, when the silicon wafer is doped with nitrogen, at high temperatures, the nitrogen atoms first bond with each other to form diatomic nitrogen, which promotes oxygen precipitation to consume a large amount of vacancies and reduce the concentration of vacancies. Since void defects are composed of vacancies, the reduction in the concentration of vacancies reduces the size of the void defects, and at a relatively low temperature, a silicon wafer with reduced void defect size is formed. In the high-temperature heat treatment of the integrated circuit manufacturing process, the void defects in the nitrogen-doped silicon single crystal are easily removed, and the yield of the integrated circuit is improved. At the same time, doping with nitrogen has a favorable effect on the BMD density distribution, such as promoting the formation of nitrogen-nucleated BMDs, allowing the BMDs to reach a certain density and functioning effectively as a gettering source for metals, making the BMD density distribution more uniform in the radial direction of the silicon wafer, and making the BMD density higher in the region adjacent to the DZ and gradually decreasing as it approaches the body of the silicon wafer.

[0006] In the related art, silicon wafers for manufacturing semiconductor electronic components such as the above-mentioned integrated circuits are mainly manufactured by slicing single crystal silicon ingots pulled by the Czochralski method. The Czochralski method involves melting polycrystalline silicon in a quartz crucible to obtain silicon melt, immersing a single crystal seed crystal in the silicon melt, and then continuously lifting the seed crystal away from the surface of the silicon melt, so that a single crystal silicon ingot grows at the phase interface during the movement. Pulling of single crystal silicon ingots by the Czochralski method is generally performed inside a crystal pulling furnace. Due to the lattice mismatch between the doping element and the silicon element, there is a segregation phenomenon in the growth process of single crystal silicon, that is, the concentration of the doping element crystallized in the single crystal silicon ingot is smaller than that in the melt (raw material), and the concentration of the doping element in the crucible continues to increase, and the concentration of the doping element in the single crystal silicon ingot also continues to increase. The segregation coefficient of nitrogen in silicon single crystal is 7×10 -4 Since the nitrogen concentration distribution is small, during the pulling of the single crystal silicon ingot, the nitrogen concentration distribution gradually increases from the front end of the crystal ingot to the rear end of the crystal ingot. As shown in Figure 1, which shows the theoretical distribution of nitrogen concentration in the nitrogen-doped single crystal along the crystal growth direction, the difference in nitrogen concentration between the front and rear ends of the nitrogen-doped single crystal is large, and accordingly, the difference in BMD concentration between the front and rear ends of the nitrogen-doped single crystal is large. Summary of the Invention [Problem to be solved by the invention]

[0007] In order to solve the above technical problems, the embodiments of the present application are expected to provide a crystal pulling furnace, a method, and a single crystal silicon ingot for producing a single crystal silicon ingot, which solves the problem that the difference in BMD content at the front and rear ends of a single crystal silicon ingot is large due to the large difference in nitrogen content from the front to rear ends of the crystal ingot during pulling of the crystal ingot, and obtains a single crystal silicon ingot with a uniform BMD concentration overall. [Means for solving the problem]

[0008] The technical means of the present application is realized as follows.

[0009] As a first aspect, an embodiment of the present application provides a crystal pulling furnace for producing a single crystal silicon ingot. The crystal pulling furnace includes a pulling mechanism configured to pull a single crystal silicon ingot by a Czochralski method using a nitrogen-doped silicon melt, a first heat treater for heat treating the single crystal silicon ingot at a first heat treatment temperature that melts BMDs of the single crystal silicon ingot, and a second heat treater disposed above the first heat treater for heat treating the single crystal silicon ingot at a second heat treatment temperature that forms BMDs in the single crystal silicon ingot. The pulling mechanism is further configured to move the single crystal silicon ingot in a crystal pulling direction to a position where a rear end of the single crystal silicon ingot is heat treated by the first heat treater and a front end of the single crystal silicon ingot is heat treated by the second heat treater.

[0010] Optionally, the first heat treatment temperature is between 950°C and 1200°C.

[0011] Optionally, the second heat treatment temperature is between 600°C and 850°C.

[0012] Optionally, the crystal pulling furnace further includes a first temperature sensor for sensing a heat treatment temperature of the first heat treatment device, a second temperature sensor for sensing a heat treatment temperature of the second heat treatment device, and a controller for controlling the first heat treatment device and the second heat treatment device to provide different heat treatment temperatures based on the temperatures sensed by the first temperature sensor and the second temperature sensor.

[0013] Optionally, the second heat treatment device includes a first segment for providing a heat treatment temperature of 600°C to 700°C aligned in the crystal pulling direction, and a second segment for providing a heat treatment temperature of 700°C to 850°C.

[0014] Optionally, the pulling mechanism is further configured to maintain the single crystal silicon ingot in a heat treated position for 2 hours.

[0015] Optionally, the crystal pulling furnace includes an upper furnace chamber having a small radial dimension and a lower furnace chamber having a large radial dimension, the first heat treatment device and the second heat treatment device are disposed in the upper furnace chamber, and a crucible and a heater for heating the crucible are provided in the lower furnace chamber.

[0016] Optionally, the total length of the first heat treater and the second heat treater along the crystal pulling direction is equal to or greater than the length of the single crystal silicon ingot, so that the entire single crystal silicon ingot can be heat treated simultaneously in the first heat treater and the second heat treater.

[0017] In a second aspect, an embodiment of the present application provides a method for producing a single crystal silicon ingot, the method including: pulling a single crystal silicon ingot by a Czochralski method using a nitrogen-doped silicon melt, moving the single crystal silicon ingot along a crystal pulling direction to a heat-treated position, heat-treating a rear end of the single crystal silicon ingot at a first heat-treatment temperature that melts BMDs of the single crystal silicon ingot, and heat-treating a front end of the single crystal silicon ingot at a second heat-treatment temperature that forms BMDs in the single crystal silicon ingot.

[0018] In a third aspect, the present embodiment provides a single crystal silicon ingot produced by the method according to the second aspect. [Brief description of the drawings]

[0019] [Figure 1] FIG. 1 is a schematic diagram of the theoretical distribution of nitrogen concentration along the crystal growth direction in a nitrogen-doped silicon single crystal in the related art. [Diagram 2] FIG. 2 is a schematic diagram of one embodiment of a typical crystal pulling furnace. [Diagram 3]FIG. 3 is a schematic diagram of a crystal pulling furnace in accordance with an embodiment of the present application, showing a single crystal silicon ingot being pulled from a silicon melt. [Figure 4] FIG. 4 is another schematic diagram of the crystal pulling furnace of FIG. 3, showing the single crystal silicon ingot completely pulled from the silicon melt and into the first heat treater and the second heat treater. [Diagram 5] FIG. 5 is a schematic diagram of a crystal pulling furnace in accordance with another embodiment of the present application. [Figure 6] FIG. 6 is a schematic diagram of a crystal pulling furnace in accordance with another embodiment of the present application. [Figure 7] FIG. 7 is a schematic diagram of a method for producing a single crystal silicon ingot in an embodiment of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, the technical solutions in the embodiments of the present application will be described clearly and completely with reference to the accompanying drawings in the embodiments of the present application.

[0021] Referring to FIG. 2, one embodiment of a general crystal pulling furnace is shown. The crystal pulling furnace 100 includes an upper furnace chamber 101 having a small radial dimension and a lower furnace chamber 102 having a large radial dimension. The lower furnace chamber 102 is provided with a crucible 200 for placing a silicon material therein. The crucible specifically includes a graphite crucible and a quartz crucible. Between the inner wall of the lower furnace chamber and the outer periphery of the crucible, a heater 300 is provided for heating the crucible and the silicon material therein to form a silicon melt S2. A pulling passage is opened at the top of the lower furnace chamber 102, which communicates with the upper furnace chamber 101 and through which a single crystal silicon ingot S3 is pulled up. In addition, a crucible rotation mechanism 400 and a crucible placement device 500 are provided in the lower furnace chamber 102. The crucible 200 is placed by the crucible placement device 500. A crucible rotation mechanism 400 for driving the crucible 200 to rotate about its own axis in a direction R is located below the crucible mounting device 500 .

[0022] When the single crystal silicon ingot S3 is pulled using the crystal pulling furnace 100, first, a high-purity polycrystalline silicon raw material is put into the crucible 200, and the crucible 200 is rotated and driven by the crucible rotating mechanism 400 while the heater 300 continues to heat the crucible 200, and the polycrystalline silicon raw material contained in the crucible is melted into a molten state, that is, into a molten silicon melt S2. Here, the heating temperature is maintained at about 1000°C. Since the gas in the furnace is usually an inert gas, unnecessary chemical reactions do not occur at the same time as the polycrystalline silicon melts. When the thermal field by the heater 300 is controlled to control the liquid surface temperature of the silicon melt S2 to the crystallization critical point, when the single crystal seed crystal S1 located above the liquid surface is pulled upward from the liquid surface along the direction P, the silicon melt S2 rises as the single crystal seed crystal S1 is pulled up, and the single crystal silicon ingot S3 is grown according to the crystallization direction of the single crystal seed crystal S1. In order to provide the silicon wafer finally produced with a high BMD density, it is possible to choose to dope the single crystal silicon ingot with nitrogen during the pulling of the single crystal silicon ingot. For example, the pulled single crystal silicon ingot and the silicon wafer cut from the single crystal silicon ingot can be doped with nitrogen by injecting nitrogen into the furnace chamber of the crystal pulling furnace 100 during pulling or by doping the silicon melt S2 in the crucible 200 with nitrogen. However, as can be seen from FIG. 1, the single crystal silicon ingot produced by the crystal pulling furnace 100 has a high N concentration at the rear end and a low N concentration at the front end, so that the BMD concentration at the front end of the single crystal silicon ingot is low and the BMD concentration at the rear end is high, resulting in a decrease in the quality and yield of the single crystal silicon ingot.

[0023] In order to solve the problem that the BMD concentration is not uniform throughout the single crystal silicon ingot, the present application provides a crystal pulling furnace 110. As shown in FIG. 3, the crystal pulling furnace 110 includes a pulling mechanism 700 configured to pull a single crystal silicon ingot S3 by the Czochralski method using a nitrogen-doped silicon melt S2, a first heat treater 610, and a second heat treater 620 disposed above the first heat treater 610. The first heat treater 610 and the second heat treater 620 are both disposed in the upper furnace chamber 101 and are vertically stacked along the crystal pulling direction P. The first heat treater 610 heat treats the single crystal silicon ingot S3 at a first heat treatment temperature that melts the BMDs of the single crystal silicon ingot S3. The second heat treater 620 heat treats the single crystal silicon ingot S3 at a second heat treatment temperature that causes BMD to form in the single crystal silicon ingot S3. The pulling mechanism 700 is further configured to move the single crystal silicon ingot S3 in the crystal pulling direction to a position where the rear end is placed in the first heat treater 610 and the front end is heat treated by the second heat treater 620.

[0024] The first heat treater 610 provides a first heat treatment temperature of 950-1200°C, providing a lower temperature region of the temperature range of 950-1200°C to the portion of the single crystal silicon ingot in the first heat treater 610. When the portion of the single crystal silicon ingot S3 with a high nitrogen content is heat treated in the lower temperature region, the BMD in this portion melts at this temperature, achieving the purpose of reducing the BMD content of this portion. The second heat treater 620 provides a second heat treatment temperature of 600-850°C, providing an upper temperature region of the temperature range of 600-700°C to the portion of the single crystal silicon ingot in the second heat treater. When the portion of the single crystal silicon ingot S3 with a low nitrogen content is heat treated in the upper temperature region, it contributes to the nucleation of BMD in this portion, achieving the purpose of increasing the BMD concentration of this portion. In this way, the parts of the single crystal silicon ingot with inconsistent BMD concentrations are subjected to corresponding heat treatments at different heat treatment temperatures, thereby avoiding the entire single crystal silicon ingot from having a non-uniform BMD concentration.

[0025] As can be seen from FIG. 1, the BMD concentration at the tip of the single crystal silicon ingot located in the upper temperature region is small. Optionally, the second heat treater includes a first segment and a second segment arranged vertically along the crystal pulling direction P. The first segment provides a heat treatment temperature of 600°C to 700°C, and the second segment provides a heat treatment temperature of 700°C to 850°C. Different heat treatment temperatures are selected for the portions of the single crystal silicon ingot S3 having different BMD concentrations by the first segment and the second segment, ensuring that the nucleation of BMD is more sufficient, and a single crystal silicon ingot S3 having a more uniform BMD concentration as a whole is obtained.

[0026] 4, the pulling mechanism 700 moves the single crystal silicon ingot S3 along the crystal pulling direction P, grows the single crystal silicon ingot S3 from a phase interface located in the lower furnace chamber 102, and moves the single crystal silicon ingot S3 to a position where it is heat-treated by the first heat treater 610 and the second heat treater 620. In order to allow the single crystal silicon ingot S3 to be heat-treated under a predetermined condition, the pulling mechanism 700 is optionally configured to hold the entire single crystal silicon ingot S3 in the first heat treater 610 and the second heat treater 620 for a required heat treatment time. As shown in FIG. 4, the single crystal silicon ingot S3 is pulled up by the pulling mechanism 700 so as to be completely positioned in the first heat treater 610 and the second heat treater 620, and the pulling mechanism 700 can hold the single crystal silicon ingot S3 in that position until a preset heat treatment time has elapsed.

[0027] In any embodiment of the present application, the heat treatment time may be 2 hours.

[0028] 5, in order to further control the accuracy of the heat treatment temperature, the crystal pulling furnace 110 further includes a first temperature sensor 801 for sensing the heat treatment temperature of the first heat treater 610, a second temperature sensor 802 for sensing the heat treatment temperature of the second heat treater 620, and a controller 900 for controlling the first heat treater 610 and the second heat treater 620 based on the heat treatment temperatures sensed by the first temperature sensor 801 and the second temperature sensor 802. The first temperature sensor 801 is installed on the side of the first heat treater 610 facing the inner chamber of the upper furnace chamber 101, and senses the temperature of the lower temperature region by a sensing probe to obtain the heat treatment temperature of the temperature region where the different portions of the single crystal silicon ingot S3 are located, and then controls the heating power of the first heat treater 610 by the controller 900 electrically connected thereto to accurately adjust the first heat treatment temperature and keep the temperature of the lower temperature region constant. The second temperature sensor 802 is arranged on the side facing the inner chamber of the upper furnace chamber 101 of the second heat treatment device 620, and its operating principle is the same as that of the first temperature sensor 801, and its description is omitted here.

[0029] In one embodiment of the present application, the crystal pulling furnace 110 is installed so that the entire single crystal silicon ingot S3 can be placed in the first heat treater and the second heat treater at the same time for heat treatment. Optionally, as shown in FIG. 6, the length H of the first heat treater 610 and the second heat treater 620 along the crystal pulling direction P is equal to or greater than the length L of the single crystal silicon ingot S3. Thus, the single crystal silicon ingot S3 can be placed completely in the first heat treater 610 and the second heat treater 620, and different portions of the single crystal silicon ingot S3 can be subjected to corresponding heat treatments at the same time.

[0030] By using the crystal pulling furnace according to the embodiment of the present application, the problem that the N concentration at the front end of the crystal ingot is much smaller than the N concentration at the rear end of the crystal ingot due to the small segregation coefficient of N when pulling a nitrogen-doped single crystal silicon ingot, resulting in non-uniform BMD concentration throughout the single crystal silicon ingot, is solved.

[0031] 7, an embodiment of the present application further provides a method for manufacturing a single crystal silicon ingot, the method including: pulling a single crystal silicon ingot by a Czochralski method using a nitrogen-doped silicon melt, moving the single crystal silicon ingot along a crystal pulling direction to a heat-treated position, heat-treating a rear end of the single crystal silicon ingot at a first heat-treatment temperature that melts BMDs of the single crystal silicon ingot, and heat-treating a front end of the single crystal silicon ingot at a second heat-treatment temperature that forms BMDs in the single crystal silicon ingot.

[0032] An embodiment of the present application further provides a single crystal silicon ingot, which is manufactured by the method for manufacturing a single crystal silicon ingot according to an embodiment of the present application.

[0033] The technical means described in the embodiments of the present application can be combined in any manner as long as there is no contradiction.

[0034] The above are only specific embodiments of the present application, but the scope of protection of the present application is not limited thereto, and any changes or replacements that a person skilled in the art can easily think of within the technical scope disclosed in the present application should be included in the scope of protection of the present application. Therefore, the scope of protection of the present application should be based on the scope of protection of the claims.

Claims

1. 1. A crystal pulling furnace for producing a single crystal silicon ingot, comprising: A pulling mechanism configured to pull a single crystal silicon ingot by the Czochralski method using a nitrogen-doped silicon melt; a first heat treatment device for heat treating the single crystal silicon ingot at a first heat treatment temperature for melting BMDs of the single crystal silicon ingot; a second heat treatment device disposed above the first heat treatment device for heat treating the single crystal silicon ingot at a second heat treatment temperature that causes BMDs to form in the single crystal silicon ingot; Including, the pulling mechanism is further configured to move the single crystal silicon ingot in a crystal pulling direction to a position where its rear end is heat-treated by the first heat treater and its front end is heat-treated by the second heat treater.

2. 2. The crystal pulling furnace according to claim 1, wherein the first heat treatment temperature is 950°C to 1200°C.

3. 2. The crystal pulling furnace according to claim 1, wherein the second heat treatment temperature is 600°C to 850°C.

4. a first temperature sensor for sensing a heat treatment temperature of the first heat treater; a second temperature sensor for sensing a heat treatment temperature of the second heat treater; a controller that controls the first heat processor and the second heat processor to provide different heat processing temperatures based on temperatures sensed by the first temperature sensor and the second temperature sensor; The crystal pulling furnace according to any one of claims 1 to 3, further comprising:

5. 5. The crystal pulling furnace according to claim 4, wherein the second heat treatment device includes a first segment for providing a heat treatment temperature of 600°C to 700°C and a second segment for providing a heat treatment temperature of 700°C to 850°C in the crystal pulling direction.

6. 10. The crystal pulling furnace of claim 1, wherein the pulling mechanism is further configured to maintain the single crystal silicon ingot in a heat treated position for two hours.

7. The furnace includes an upper furnace chamber having a small radial dimension and a lower furnace chamber having a large radial dimension, the first heat treatment device and the second heat treatment device are disposed in the upper furnace chamber; 2. The crystal pulling furnace according to claim 1, wherein a crucible and a heater for heating said crucible are provided in said lower furnace chamber.

8. 4. The crystal pulling furnace according to claim 1, wherein the total length of the first heat treater and the second heat treater along the crystal pulling direction is equal to or greater than the length of the single crystal silicon ingot so that the entire single crystal silicon ingot can be heat-treated in the first heat treater and the second heat treater simultaneously.

9. 1. A method for producing a single crystal silicon ingot, comprising: Pulling a single crystal silicon ingot by a Czochralski process using the nitrogen-doped silicon melt; moving the single crystal silicon ingot along a crystal pulling direction to a position where it is to be heat treated; heat treating a rear end portion of the single crystal silicon ingot at a first heat treatment temperature that melts BMDs of the single crystal silicon ingot; heat treating the tip portion of the single crystal silicon ingot at a second heat treatment temperature that causes BMDs to form in the single crystal silicon ingot; A method comprising:

10. 10. A single crystal silicon ingot produced by the method of claim 9.

Citation Information

Patent Citations

  • Silicon single crystal pulling-up method

    JP2002047094A

  • Method for producing wafer

    JP2005060168A

  • Silicon wafer, and method for evaluating and manufacturing the same

    JP2007207877A

  • Method for manufacturing silicon wafer

    JP2009088240A

  • Method for manufacturing single crystal with uniform distribution of micro-defects and Apparatus for implementing the same

    KR1020100091789A