Reflector, manufacturing method thereof, lens module and electronic device
A silicon-based reflector with a planar structure addresses the volume and mass issues of equilateral triangular prisms by minimizing outward angles and enhancing stress tolerance, ensuring efficient and durable periscope lens modules.
Patent Information
- Application Number
- JP2023501864
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-07-17
- Filing Date
- 2021-05-18
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2041-05-18
AI Technical Summary
The use of equilateral triangular prisms in periscope lens modules results in a relatively large volume and mass, leading to space inefficiencies and increased risk of damage due to collisions and frictional forces during assembly.
A reflector using a silicon-based substrate with a planar structure, featuring specific included angles and reflective films, reduces volume and mass, and minimizes the formation of outwardly protruding right angles, thereby reducing the risk of cracks and edge damage.
The silicon-based reflector effectively reduces the space occupied and minimizes damage risks, while maintaining high stress tolerance and flatness, facilitating efficient mass production and improving the performance of periscope lens modules.
Smart Images

Figure 0007562933000001 
Figure 0007562933000002 
Figure 0007562933000003
Abstract
Description
[Technical field]
[0001] This application claims priority to Chinese Patent Application No. 202010693017.5, entitled "Reflector, Manufacturing Method Thereof, Lens Module, and Electronic Device," filed on July 17, 2020. The Chinese patent application is incorporated herein by reference in its entirety.
[0002] The present application relates to the field of optical technology, and in particular to a reflector, a manufacturing method thereof, a lens module and an electronic device. [Background technology]
[0003] To achieve telephoto imaging, electronic devices such as mobile phones generally use a periscope lens module. The periscope lens module may include a regular triangular prism, a lens set, and a photosensitive element arranged in sequence. The included angle between the inclined surface of the regular triangular prism and the optical axis of the lens set is 45 degrees, and the inclined surface can reflect the incident light to the lens set. Then, the lens set can transmit the reflected light to the photosensitive element.
[0004] However, both the volume and mass of a regular triangular prism are relatively large, resulting in a lens module with a relatively large volume and a relatively large mass. Summary of the Invention
[0005] The present application provides a reflector, a manufacturing method thereof, a lens module and an electronic device, which can solve the technical problem in the related art that the use of a regular triangular prism as a reflector leads to a relatively large volume and a relatively large mass of the lens module.
[0006] According to one embodiment, a reflector is provided. The reflector includes a silicon-based substrate and a first reflective film. The silicon-based substrate has a first surface and a second surface, a first side surface and a second side surface, which are opposite to each other. The first side surface is connected to both the first surface and the second side surface, and the second side surface is connected to the second surface. The first reflective film is located on the first surface. An included angle between the first side surface and the first surface is greater than a first angle threshold, and an included angle between the second side surface and the first side surface is greater than a second angle threshold. The included angle between the second side surface and the second surface is an obtuse angle.
[0007] The reflector provided in the present application uses a silicon-based substrate having a planar structure as a substrate, which can effectively reduce the volume and mass of the reflector when compared with a regular triangular prism. In addition, the included angle between the second side and the second surface of the silicon-based substrate is designed as an obtuse angle to ensure that no right angle protruding outward is formed between the second side and the second surface after the reflector is tilted and arranged. Therefore, the space occupied when the reflector applied to the periscope lens module can be reduced, and further the risk of cracking or edge damage of the side edge of the silicon-based substrate caused by collision or friction force during assembly of the reflector can be effectively reduced.
[0008] Optionally, the included angle between the second side and the first surface is 45 degrees. When the reflector is applied to a periscope lens module, the included angle between the first reflective film and the optical axis of the lens set is usually 45 degrees. Therefore, the included angle between the second side and the first surface is also designed to be 45 degrees, which can ensure that the second side of the silicon-based substrate is parallel to the optical axis of the lens set, thereby ensuring that no outward protruding angle is formed between the second side and the second surface, and further reducing the risk of side edge cracking or edge breakage of the silicon-based substrate.
[0009] Optionally, the reflector further includes a second reflective film located on the second surface, and the material of the second reflective film may be the same as that of the first reflective film.
[0010] The first surface and the second surface of the silicon-based substrate are coated with a reflective film of the same material, so that the two kinds of stresses generated by the thin-film coating process can offset each other, which can further reduce the deformation of the silicon-based substrate generated during the thin-film coating, thereby ensuring the quality of the tuned reflector.
[0011] Optionally, the material of the silicon-based substrate is single-crystal silicon with a target crystal orientation. Because the Young's modulus of single-crystal silicon with different crystal orientations is different, by forming the silicon-based substrate using single-crystal silicon with the same crystal orientation, the consistency of the overall Young's modulus of the silicon-based substrate can be guaranteed. Furthermore, the relatively high consistency of the stress resistance performance of the silicon-based substrate can be guaranteed, so that the reflector made by using the silicon-based substrate has better flatness.
[0012] Optionally, the target crystal orientation is (111). Because single crystal silicon with (111) crystal orientation has a high Young's modulus and better stress resistance, a silicon-based substrate made of single crystal silicon with (111) crystal orientation can further ensure the flatness of the manufactured reflector.
[0013] Optionally, the first reflective film may be an insulating film or a metal film. The material of the metal film may include at least one of aluminum, gold, and silver. The material of the insulating film may be a non-metallic compound.
[0014] Optionally, the height of the first side is equal to 0, and the height direction of the first side is perpendicular to the first surface. To further reduce the total thickness of the silicon-based substrate, the height of the first side is designed to be 0, thereby reducing the volume and mass of the reflector.
[0015] According to another aspect, a method for manufacturing a reflector is provided. In the method, a first reflective material film layer is first formed on a first surface of a silicon wafer, and then the silicon wafer and the first reflective material film layer are processed to obtain at least one reflector. Each reflector includes a silicon base substrate obtained by processing the silicon wafer, and a first reflective film obtained by processing the first reflective material film layer. The silicon base substrate has a first surface and a second surface facing each other, a first side surface and a second side surface. The first side surface is connected to both the first surface and the second side surface, and the second side surface is connected to the second surface. The first reflective film is located on the first surface. The included angle between the first side surface and the first surface is greater than a first angle threshold, and the included angle between the second side surface and the first side surface is greater than a second angle threshold. The included angle between the second side surface and the second surface is an obtuse angle.
[0016] In the manufacturing method provided herein, a silicon wafer and a first reflective material film layer can be processed to obtain a plurality of reflectors. In this way, mass production of reflectors can be realized, which effectively improves reflector adjustment efficiency and reduces reflector adjustment costs. In addition, the performance consistency of the adjusted reflectors can be guaranteed.
[0017] Optionally, the process of processing the silicon wafer and the first reflective material film layer may include first cutting a second surface of the silicon wafer by using a first cutting blade to form a second side of the reflector, where a cutting depth of the first cutting blade is smaller than a thickness of the silicon wafer, and the second surface and the first surface are two opposite surfaces of the silicon wafer, and then continuing cutting the silicon wafer by using a second cutting blade to cut the first reflective material film layer to form the first side of the reflector and the first reflective film of the reflector.
[0018] The above mechanical cutting method is relatively simple and effective. In addition, different shapes of the first cutting blade may be selected to form the second side with different inclination angles, which helps to meet the design requirements of different reflectors.
[0019] Optionally, processing the silicon wafer and the first reflective material film layer may include first processing the first reflective material film layer and the silicon wafer starting from a side of the first reflective material film layer facing away from the silicon wafer to form a first side of the reflector and a first reflective film of the reflector, and then cutting a second side of the silicon wafer by using a first cutting blade to form a second side of the reflector, where the second side and the first side are two opposing side surfaces of the silicon wafer.
[0020] In the present application, alternatively, the first reflective material film layer and the first side of the silicon wafer may be processed first, and then the second side of the silicon wafer is processed.
[0021] Optionally, the process of processing the first reflective material film layer and the silicon wafer starting from a side of the first reflective material film layer facing away from the silicon wafer may include etching the first reflective material film layer and the silicon wafer starting from the side of the first reflective material film layer facing away from the silicon wafer, or cutting the first reflective material film layer and the silicon wafer starting from the side of the first reflective material film layer facing away from the silicon wafer by using a second cutting blade.
[0022] In the method provided in the present application, the first reflective material film layer and the first surface of the silicon wafer can be processed by using different processes to form the first side surface of the reflector and the first reflective film of the reflector. This manufacturing method has relatively high flexibility. By processing the first reflective material film layer through etching, the first reflective material film layer can be prevented from cracking, and the reliability of the etching is relatively high.
[0023] Optionally, before processing the first reflective material film layer and the silicon wafer starting from the side of the first reflective material film layer facing away from the silicon wafer, an alignment mark may first be formed on the second side of the silicon wafer, and then the alignment mark may be used as a reference for processing the first reflective material film layer and the silicon wafer starting from the side of the first reflective material film layer facing away from the silicon wafer, and the alignment mark may be used as a reference for cutting the second side of the silicon wafer by using a first cutting blade.
[0024] To ensure that the silicon wafer can be effectively separated after two processing steps to obtain multiple reflectors, alignment marks are first formed on the second side of the silicon wafer, so that the alignment marks can be used as a reference for subsequently processing the first and second sides of the silicon wafer in sequence.
[0025] Optionally, the method further includes using the same material as that of the first reflective material layer to form a second reflective material layer on a second side of the silicon wafer, and processing the second reflective material layer to obtain a second reflective film in the reflector, the second reflective film being located on a second surface of the silicon-based substrate.
[0026] A reflective material film layer made of the same material is formed on the first side and the second side of the silicon wafer, so that two kinds of stresses generated by the thin film coating process can cancel each other out, thereby further reducing the deformation of the silicon wafer generated during the thin film coating, thereby ensuring the flatness of the adjusted reflector.
[0027] Yet another aspect provides a lens module, the lens module including the reflector provided in the previous aspect, a lens set, and a light-sensitive element, the lens set being located between the reflector and the light-sensitive element, a first reflective film in the reflector being closer to the lens set than the silicon-based substrate, and the first reflective film being configured to reflect incident light to the lens set.
[0028] Optionally, the included angle between the second side and the first surface of the silicon-based substrate is equal to the included angle between the first reflective film and the optical axis of the lens set. In this way, it may be ensured that the second side of the silicon-based substrate is parallel to the optical axis of the lens set, which ensures that no outward protruding angle is formed between the second side and the second surface, further reducing the risk of side edge cracking or edge breakage of the silicon-based substrate.
[0029] Optionally, the included angle between the first reflective film and the optical axis of the lens set is 45 degrees.
[0030] Yet another aspect provides an electronic device including a housing and a lens module disposed within the housing as provided in the previous aspect.
[0031] In summary, the embodiments of the present application provide a reflector, its manufacturing method, a lens module, and an electronic device. The reflector uses a silicon-based substrate having a planar structure as a substrate, which can effectively reduce the volume and mass of the reflector when compared with a regular triangular prism. In addition, the included angle between the second side and the second surface of the silicon-based substrate is designed as an obtuse angle to ensure that no right angle protruding outward is formed between the second side and the second surface after the reflector is tilted and arranged. Therefore, the space occupied when the reflector applied to the periscope lens module can be reduced, and further, the risk of cracking or edge breakage of the side edge of the silicon-based substrate caused by collision or friction force during assembly of the reflector can be effectively reduced. In addition, since the Young's modulus of the silicon-based substrate is relatively high, the coating of the surface of the silicon-based substrate with the reflective film does not cause a relatively large deformation of the silicon-based substrate, which can ensure a relatively high quality of the adjusted reflector. [Brief description of the drawings]
[0032] [Figure 1] FIG. 2 is a schematic diagram of a structure of a reflector according to an embodiment of the present application.
[0033] [Diagram 2] FIG. 2 is a schematic diagram of a partial structure of a periscope lens module according to an embodiment of the present application.
[0034] [Diagram 3] FIG. 13 is a schematic diagram of a partial structure of another periscope lens module.
[0035] [Figure 4] FIG. 1 is a schematic diagram of the amount of deformation when optical glass is used as the base.
[0036] [Diagram 5] FIG. 1 is a schematic diagram of a structure of a silicon-based substrate according to an embodiment of the present application.
[0037] [Figure 6] FIG. 2 is a schematic diagram of the deformation amount when a silicon-based substrate with a (100) crystal orientation is used as the base according to one embodiment of the present application.
[0038] [Figure 7] FIG. 2 is a schematic diagram of the deformation amount when a silicon-based substrate with a (111) crystal orientation is used as the base according to one embodiment of the present application.
[0039] [Figure 8] FIG. 2 is a schematic diagram of another reflector structure according to an embodiment of the present application;
[0040] [Figure 9] FIG. 2 is a schematic diagram of the deformation amount when a silicon-based substrate with a (111) crystal orientation is used as a base and both of the two surfaces of the silicon-based substrate are coated with a reflective film.
[0041] [Figure 10] FIG. 13 is a schematic diagram of yet another reflector structure according to an embodiment of the present application.
[0042] [Figure 11] FIG. 13 is a schematic diagram of yet another reflector structure according to an embodiment of the present application.
[0043] [Figure 12] 1 is a flow chart of a method for manufacturing a reflector according to an embodiment of the present application.
[0044] [Figure 13] 4 is a flow chart of another method for manufacturing a reflector according to an embodiment of the present application.
[0045] [Figure 14] 1 is a schematic diagram of a manufacturing process for a reflector according to an embodiment of the present application.
[0046] [Figure 15] FIG. 2 is a schematic diagram of a first cutting blade according to an embodiment of the present application.
[0047] [Figure 16] FIG. 2 is a cross-sectional view of a second cutting blade according to an embodiment of the present application.
[0048] [Figure 17] 13 is a flow chart of yet another method of manufacturing a reflector according to an embodiment of the present application.
[0049] [Figure 18] 4A-4C are schematic diagrams of another manufacturing process for a reflector according to an embodiment of the present application.
[0050] [Figure 19] 13 is a flow chart of yet another method of manufacturing a reflector according to an embodiment of the present application.
[0051] [Figure 20] FIG. 2 is a schematic diagram of a structure of a periscope lens module according to an embodiment of the present application.
[0052] [Figure 21] FIG. 1 is a schematic diagram of a structure of an electronic device according to an embodiment of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0053] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, a reflector, a manufacturing method thereof, a lens module and an electronic device provided in embodiments of the present application will be described in detail with reference to the accompanying drawings.
[0054] An embodiment of the present application provides a reflector. The reflector is made of a silicon-based substrate with a planar structure to solve the problem of the large volume and mass of the triangular prism in the related art. Figure 1 is a schematic diagram of the structure of the reflector according to an embodiment of the present application. As shown in Figure 1, the reflector 10 includes a silicon-based substrate 101 and a first reflective film 102.
[0055] The silicon base substrate 101 has a first surface 1a and a second surface 1b, a first side surface 1c and a second side surface 1d that are opposite to each other. The first side surface 1c is connected to both the first surface 1a and the second side surface 1d, and the second side surface 1d is connected to the second surface 1b. The fact that the first surface 1a and the second surface 1b are opposite to each other means that the first surface 1a is parallel to the second surface 1b or that the first surface 1a is approximately parallel to the second surface 1b.
[0056] The first reflective film 102 is located on the first surface 1a, and the included angle α between the first side surface 1c and the first surface 1a is greater than a first angle threshold. The included angle β between the second side surface 1d and the first side surface 1c is greater than a second angle threshold. The included angle γ between the second side surface 1d and the second surface 1b is an obtuse angle. That is, the silicon base substrate 101 has a second side surface that is inclined with respect to the surface of the silicon base substrate 101.
[0057] The first angle threshold may be an acute angle close to 90°, and the second angle threshold may be an acute angle close to 90° or an obtuse angle. In addition, the first angle threshold may be equal to the second angle threshold or may not be equal to the second angle threshold. For example, the first angle threshold may be 80° or 85°, and the second angle threshold may be 90°. In other words, both the included angle α between the first side surface 1c and the first surface 1a and the included angle β between the second side surface 1d and the first side surface 1c are relatively large angles. For example, the included angle α may be a right angle or an acute angle close to a right angle, and the included angle β may be a right angle or an obtuse angle. In order to ensure the yield of the reflector by effectively reducing the risk of cracks or edge breakage caused due to collision or frictional forces during packaging of the reflector, both the included angle α between the first side 1c and the first surface 1a and the included angle β between the second side 1d and the first side 1c are designed to be relatively large angles.
[0058] The reflector 10 provided in this embodiment of the present application can be applied to a periscope lens module. FIG. 2 is a schematic diagram of a partial structure of a periscope lens module according to an embodiment of the present application. As shown in FIG. 2, in a periscope lens module, the reflector 10 needs to be arranged at an angle, so that the included angle between the first reflective film 102 in the reflector 10 and the optical axis (parallel to the transmission direction of the emitted light in FIG. 2) of the lens set 20 in the periscope lens module is an acute angle. For example, the included angle is 45°. Since the included angle γ between the second side surface 1d and the second surface 1b of the silicon base substrate 101 in the reflector 10 is an obtuse angle, when the reflector 10 is arranged at an angle, the second side surface 1d may be parallel or approximately parallel to the optical axis of the lens set 20.
[0059] 3, when the second side 1d of the silicon-based substrate 101 is designed to be perpendicular to the second surface 1b, the right angle formed between the second side 1d of the silicon-based substrate 101 and the second surface 1b after the reflector 10 is placed at an angle occupies a relatively large space, and cracks or edge breaks at the right angle are easily generated due to collision or frictional force during assembly of the reflector 10.
[0060] Based on the above analysis, it can be seen that in the reflector 10 provided in this embodiment of the present application, the included angle γ between the second side 1d and the second surface 1b of the silicon-based substrate 101 is designed as an obtuse angle, so as to ensure that no outwardly protruding right angle is formed between the second side 1d and the second surface 1b after the reflector 10 is placed at an angle. Thus, the space occupied by the reflector 10 can be reduced, and further, the risk of side edge cracks or edge breakage of the silicon-based substrate 101 caused by collision or frictional force during assembly of the reflector 10 can be effectively reduced.
[0061] Optionally, in this embodiment of the present application, when the reflector 10 is applied to a periscope lens module, after the reflector 10 is arranged at an angle, as shown in Fig. 2, the included angle between the first reflective film 102 and the optical axis of the lens set 20 is θ. To enable the second side 1d of the silicon-based substrate 101 to be parallel to the optical axis of the lens set 20, the included angle δ between the second side 1d of the silicon-based substrate 101 and the first surface 1a can be designed as an angle equal to the included angle θ. Alternatively, it can be understood that the included angle γ between the second side 1d of the silicon-based substrate 101 and the second surface 1b is designed as an angle complementary to the included angle θ.
[0062] For example, assuming that the included angle θ between the first reflective film 102 and the optical axis of the lens set 20 is 45°, the included angle δ between the second side surface 1d and the first surface 1a of the silicon-based substrate 101 may be 45°, and the included angle γ between the second side surface 1d and the second surface 1b of the silicon-based substrate 101 may be 135°.
[0063] The included angle δ between the second side 1d and the first surface 1a of the silicon-based substrate 101 is designed as an angle equal to the included angle θ, so that when the reflector 10 is applied to a periscope lens module, the second side 1d of the silicon-based substrate 101 may be parallel to the optical axis of the lens set 20. Therefore, no outward protruding angle is formed between the second side 1d and the second surface 1b, which can ensure that the risk of side edge cracking or edge breakage of the silicon-based substrate 101 is further reduced.
[0064] Related art usually uses a solution of coating optical glass with a reflective film to adjust the reflector, however, because the Young's modulus of optical glass is relatively small, generally 70 gigapascals (GPa), the concave surface on the optical glass needs to be ground and polished first before the optical glass is coated to offset the deformation of the optical glass caused by the stress generated during the coating of the reflective film.
[0065] In this embodiment of the present application, the material of the silicon-based substrate 101 may be single crystal silicon. The Young's modulus of single crystal silicon is about 169 GPa, which is much higher than that of optical glass. Therefore, for the same stress caused by the thin film coating, the deformation amount of the silicon-based substrate 101 is smaller. For example, FIG. 4 is a schematic diagram of the deformation amount when optical glass is used as the base. Please refer to the reference numbers in FIG. 5. The horizontal axis in FIG. 4 represents the distance from the center point A of the base measured in microns (μm), and the vertical axis represents the deformation amount (also called warpage displacement) of the base measured in μm. It can be seen from FIG. 4 that when optical glass is used as the base of the reflector, the stress generated during the adjustment of the reflective film causes a deformation of 0.52 μm at the corner of the optical glass. FIG. 6 is a schematic diagram of the deformation amount when a silicon-based substrate with a crystal orientation of (100) is used as the base. As shown in Figure 6, when a silicon-based substrate with a (100) crystal orientation is used as the base of the reflector, the stress with the same value generated during the preparation of the reflective film will cause a deformation of 0.24 μm at the corner of the silicon-based substrate. Compared with that of optical glass, the deformation amount is reduced by 2.2 times.
[0066] Because the Young's modulus of the silicon-based substrate is relatively high, the stress generated during the preparation of the reflective film causes a relatively small amount of deformation of the silicon-based substrate. Therefore, it is no longer necessary to use the method of grinding and polishing the concave surface in advance to offset the deformation caused by the stress. Therefore, this can effectively reduce the complexity of the reflector manufacturing process, reduce the manufacturing cost, and improve the yield of this process.
[0067] Optionally, the material of the silicon-based substrate 101 may be single-crystal silicon with a target crystal orientation. That is, the crystal orientation of the single-crystal silicon used by the silicon-based substrate 101 is consistent. Because the Young's modulus of single-crystal silicon with different crystal orientations is different, the consistency of the overall Young's modulus of the silicon-based substrate 101 can be guaranteed by forming the silicon-based substrate 101 using single-crystal silicon with the same crystal orientation. In addition, the relatively high consistency of the stress resistance performance of the silicon-based substrate 101 can be guaranteed, and as a result, the reflector 10 made by using the silicon-based substrate 101 will have better flatness.
[0068] In this embodiment of the present application, the crystal orientation of the single crystal silicon used by the silicon-based substrate 101 may be (111). Single crystal silicon with a crystal orientation of (111) may be expressed as single crystal silicon (111). The Young's modulus of single crystal silicon (111) is 188 GPa, which is greater than that of single crystal silicon (100) which is 169 GPa. Therefore, single crystal silicon (111) has better stress resistance than single crystal silicon (100). For example, FIG. 7 is a schematic diagram of the deformation amount when a silicon-based substrate with a crystal orientation of (111) is used as a base. It can be seen through the comparison between FIG. 6 and FIG. 7 that when the same coating stress is generated, the deformation of the silicon-based substrate 101 using single crystal silicon (100) is 0.24 μm, while the deformation of the silicon-based substrate 101 using single crystal silicon (111) is only 0.2 μm. The deformation amount is reduced by 18%.
[0069] From this, it can be seen that by using a silicon-based substrate 101 made by using single crystal silicon (111), the flatness of the manufactured reflector 10 can be further guaranteed.
[0070] Optionally, as shown in FIG. 8 , the reflector 10 provided in this embodiment of the present application further includes a second reflective film 103 located on the second surface 1b, and the material of the second reflective film 103 may be the same as that of the first reflective film 102.
[0071] The first surface 1a and the second surface 1b of the silicon-based substrate 101 are coated with a reflective film of the same material, so that the two kinds of stresses generated by the thin-film coating process are offset with each other, which can further reduce the deformation of the silicon-based substrate 101 generated during the thin-film coating. For example, FIG. 9 is a schematic diagram of the deformation amount when a silicon-based substrate with a crystal orientation of (111) is used as a base and both of the two surfaces of the silicon-based substrate are coated with a reflective film. It can be seen through the comparison between FIG. 7 and FIG. 9 that when only the first surface 1a of the silicon-based substrate 101 is coated, the deformation of the silicon-based substrate 101 is about 0.2 μm. When both the first surface 1a and the second surface 1b of the silicon-based substrate 101 are coated, the deformation of the silicon-based substrate 101 can be reduced to 0.09 μm. The deformation amount is reduced by 2.2 times, which significantly improves the deformation resistance effect of the silicon-based substrate 101.
[0072] Optionally, in this embodiment of the present application, the first reflective film 102 in the reflector 10 may be an insulating film or a metal film. The material of the metal film may include at least one of aluminum, gold and silver. The material of the insulating film may be a non-metallic compound.
[0073] Of course, in addition to insulating films and metal films, the first reflective film 102 may alternatively be made of other materials, provided that the first reflective film can effectively reflect light.
[0074] In this embodiment of the present application, the height h1 of the first side 1c of the silicon-based substrate 101 may be smaller than the height h2 of the second side 1d, as shown in Figure 8. Both the height directions of the first side 1c and the second side 1d are perpendicular to the first surface of the silicon-based substrate 101.
[0075] Optionally, as shown in Fig. 10, the height h1 of the first side 1c of the silicon-based substrate 101 may be 0. That is, the silicon-based substrate 101 may not include the first side 1c, but may only include the second side 1d. In this way, the thickness of the silicon-based substrate 101 can be effectively reduced, thereby reducing the volume and mass of the reflector 10.
[0076] Optionally, as shown in FIG. 5, the first surface 1a of the silicon-based substrate 101 may be rectangular, for example, square. Thus, the silicon-based substrate 101 may not include four first side surfaces 1c and four second side surfaces 1d. The included angles of the first side surfaces 1c and the first surface 1a may be equal to each other or may not be equal to each other. The included angles between the second side surfaces 1d and the second surface 1b (not shown in FIG. 5) may be equal to each other or may not be equal to each other.
[0077] In this embodiment of the present application, to ensure the symmetry of the overall structure of the reflector 10, the included angles of the first side 1c and the first surface 1a of the silicon-based substrate 101 may be equal to each other, for example, all of them are 90°. In addition, the included angles between the second side 1d and the second surface 1b may also be equal to each other, for example, all of them are 135°.
[0078] Fig. 11 is a schematic diagram of yet another reflector structure according to an embodiment of the present application. As shown in Fig. 11, a first reflective film 102 can cover a first surface 1a. Specifically, the shape of the first reflective film 102 is the same as that of the first surface 1a, and the size of the first reflective film 102 is also the same as that of the first surface 1a.
[0079] In addition, the embodiment of the present application provides a reflector. The reflector uses a silicon-based substrate having a planar structure as a substrate, which can effectively reduce the volume and mass of the reflector when compared with a regular triangular prism. In addition, the included angle between the second side and the second surface of the silicon-based substrate is designed as an obtuse angle to ensure that no right angle protruding outward is formed between the second side and the second surface after the reflector is tilted and arranged. Therefore, the space occupied when the reflector applied to the periscope lens module can be reduced, and further, the risk of cracking or edge damage of the side edge of the silicon-based substrate caused by collision or friction force during assembly of the reflector can be effectively reduced. In addition, since the Young's modulus of the silicon-based substrate is relatively high, the coating of the surface of the silicon-based substrate with the reflective film does not cause a relatively large deformation of the silicon-based substrate, which can ensure the flatness of the adjusted reflector.
[0080] An embodiment of the present application further provides a method for manufacturing a reflector, which can be used to manufacture the reflector provided in the above-mentioned embodiments. See Figure 12. The method may include the following steps.
[0081] Step 401: Form a first reflective material film layer on a first surface of a silicon wafer.
[0082] In this embodiment of the present application, a silicon wafer made of single crystal silicon can be used as a starting material for forming a silicon-based substrate. The silicon wafer can be made of single crystal silicon, for example, single crystal silicon (111). In addition, the resistivity of single crystal silicon is not limited in this embodiment of the present application.
[0083] Optionally, the first reflective material film layer may be an insulating film. Thus, the first reflective material film layer may be formed by using a chemical vapor deposition (CVD) or plasma enhanced chemical vapor deposition (PECVD) process.
[0084] Alternatively, the first reflective material film layer may be a metal film.The first reflective material film layer may therefore be formed by a magnetron sputtering process or an e-beam evaporation process.
[0085] Since the silicon wafer has a relatively high Young's modulus, a relatively high stress resistance and a relatively small deformation amount generated after coating, the surface of the silicon wafer can be directly coated without grinding and polishing the concave surface on the surface of the silicon wafer in advance, to offset the stress generated by the coating process.Therefore, this effectively reduces the complexity of the reflector manufacturing process, reduces the reflector manufacturing cost, and improves the reflector adjustment efficiency.
[0086] Step 402: Processing a silicon wafer and a first reflective material film layer to obtain at least one reflector.
[0087] In this embodiment of the present application, the silicon wafer and the first reflective material film layer can be cut to obtain at least one reflector. Alternatively, the silicon wafer and the first reflective material film layer can be etched and cut to obtain at least one reflector.
[0088] As shown in FIG. 1, each of the tuned reflectors includes a silicon-based substrate 101 obtained by processing a silicon wafer, and a first reflective film 102 obtained by processing a first reflective material film layer. The silicon-based substrate 101 has a first surface 1a and a second surface 1b, a first side surface 1c and a second side surface 1d facing each other. The first side surface 1c is connected to both the first surface 1a and the second side surface 1d, and the second side surface 1d is connected to the second surface 1b. The first reflective film 102 is located on the first surface 1a, and the included angle α between the first side surface 1c and the first surface 1a is greater than a first angle threshold. The included angle β between the second side surface 1d and the first side surface 1c is greater than a second angle threshold. The included angle γ between the second side surface 1d and the second surface 1b is an obtuse angle.
[0089] In the manufacturing method provided in this embodiment of the present application, a silicon wafer and a first reflective material film layer can be processed to obtain a plurality of reflectors. In this way, mass production of reflectors can be realized, which effectively improves reflector adjustment efficiency and reduces reflector adjustment costs. In addition, the performance consistency of the plurality of adjusted reflectors can be guaranteed.
[0090] In an optional implementation, as shown in FIG. 13, a method for manufacturing a reflector provided in one embodiment of the present application may include the following steps.
[0091] Step 501: Form a first reflective material film layer on a first surface of a silicon wafer.
[0092] See steps S11 and S12 in Figure 14. A silicon wafer 01 may be obtained first, and then a first reflective material film layer 02 is formed on a first surface of the silicon wafer 01. For the mounting process of step 501, see step 401 above. Details will not be described again here.
[0093] Step 502: Attach a dicing membrane to the side of the first reflective material membrane layer facing away from the silicon wafer.
[0094] See step S13 in Fig. 14. The silicon wafer 01 provided with the first reflective material film layer 02 may be turned over, and then the side of the first reflective material film layer 02 facing away from the silicon wafer 01 is attached to a dicing film 03. Optionally, the dicing film may be a viscous ultraviolet (UV) film.
[0095] Step 503: Cut the second surface of the silicon wafer by using a first cutting blade to form a second side of the reflector.
[0096] See step S14 in Figure 14. A first cutting blade (also referred to as a V-shaped blade or a V-shaped hub cutting blade) D1 can be used to cut the second side of the silicon wafer 01. The second side and the first side are two opposite sides of the silicon wafer 01, for example, the second side is parallel to the first side. The cutting depth h1 of the first cutting blade D1 is smaller than the thickness of the silicon wafer 01.
[0097] FIG. 15 is a schematic diagram of a first cutting blade according to an embodiment of the present application. Please refer to the side view in FIG. 15. The first cutting blade D1 may be of a ring shape. FIG. 15 further shows three optional cross-sectional views of the first cutting blade. As shown in the left and right cross-sectional views in FIG. 15, the cross-section of the cutting edge D11 of the first cutting blade D1 may be trapezoidal. Alternatively, as shown in the middle cross-sectional view in FIG. 15, the cross-section of the cutting edge D11 may be hexagonal, including a rectangle and a trapezoid. In addition, as shown in the left and middle cross-sectional views in FIG. 15, respectively, the maximum thickness of the cutting edge D11 may be equal to the thickness of the center of the first cutting blade D1. Alternatively, as shown in the right cross-sectional view in FIG. 15, the maximum thickness of the cutting edge D11 may be smaller than the thickness of the center of the first cutting blade D1.
[0098] After the second side of the silicon wafer 01 is cut by using the first cutting blade D1, a bevel groove may be formed on the second side of the silicon wafer 01, and the sidewall of the bevel groove may become the second side 1d of the silicon base substrate in the reflector. During manufacturing, different shapes of the first cutting blade D1 may be flexibly selected to cut the silicon wafer 01 based on different inclination angles of the second side 1d (which is the included angle between the second side 1d and the second surface) required by the design. Cutting the silicon wafer 01 by using the first cutting blade D1 can realize precise control and adjustment of the inclination angle of the second side 1d formed through cutting, which helps to meet the design requirements of different reflectors.
[0099] Step 504: Continue cutting the silicon wafer by using a second cutting blade to cut through the first reflective material film layer to form a first side of the reflector and a first reflective film of the reflector.
[0100] See step S15 in Fig. 14. The second cutting blade (which may also be referred to as a straight cutting blade or a vertical hub cutting blade) D2 may be used to continue cutting the silicon wafer 01 starting from the bottom surface of the bevel groove of the silicon wafer 01 and cut the first reflective material film layer 02. In this way, the first side of the reflector and the first reflective film of the reflector may be formed. The cutting direction of the second cutting blade D2 may be perpendicular to the first surface of the silicon wafer 01, and accordingly, the first side formed through cutting is perpendicular to the first surface of the silicon base substrate.
[0101] For a side view of the second cutting blade D2, please refer to the side view shown in FIG. 15. That is, the second cutting blade D2 may also be ring-shaped. FIG. 16 is a cross-sectional view of the second cutting blade according to an embodiment of the present application. As shown in FIG. 16, the cross section of the cutting edge D21 of the second cutting blade D2 may be a hexagon, including a rectangle and a trapezoid. The maximum thickness of the cutting edge D21 is smaller than the thickness of the center of the second cutting blade D2.
[0102] In this embodiment of the present application, the cutting depth h3 when the second cutting blade D2 is used for cutting may be greater than or equal to the sum of the remaining thickness of the silicon wafer 01 obtained after cutting by using the first cutting blade D1 and the thickness of the first reflective material film layer 02. That is, the second cutting blade D2 may completely cut the silicon wafer 01 provided with the first reflective material film layer 02 to obtain a plurality of separated reflectors.
[0103] As shown in FIG. 14, a dicing film 03 is attached to the side of the first reflective material film layer 02 facing away from the silicon wafer 01, so that after the multiple reflectors are separated by using the second cutting blade D2, the multiple reflectors can be fixed on the dicing film 03 to prevent them from scattering (also called flying pieces) and causing damage.
[0104] In this embodiment of the present application, if mass production of multiple reflectors is required, the aforementioned step 503 may be performed multiple times, i.e., the second surface of the silicon wafer may be cut multiple times by using a first cutting blade to obtain multiple bevel grooves. Correspondingly, the aforementioned step 504 may also be performed multiple times, i.e., the silicon wafer and the first reflective material film layer may be cut multiple times by using a second cutting blade to obtain multiple separated reflectors. Then, the multiple separated reflectors may be peeled off from the dicing film and packaged into a periscope lens module respectively. If the dicing film is a UV film, a UV irradiation device may be used to irradiate the UV film to reduce the viscosity of the UV film to peel off the reflectors.
[0105] The above-mentioned method of mechanically cutting the silicon wafer and the reflective material film layer by using two different kinds of cutting blades is relatively simple and has relatively high efficiency.
[0106] In another optional implementation, as shown in FIG. 17, a method for manufacturing a reflector provided in an embodiment of the present application may include the following steps.
[0107] Step 601: Form alignment marks on a second side of a silicon wafer.
[0108] In this embodiment of the present application, as shown in step S21 in Figure 18, a plurality of alignment marks 011 may be formed on the second side of the silicon wafer 01. The plurality of alignment marks 011 may be located at the edge of the silicon wafer 01.
[0109] Optionally, a number of grooves may be formed as alignment marks 011 on the second side of the silicon wafer 01 through etching or cutting. For example, the alignment marks 011 may be formed on the second side of the silicon wafer 01 by using a deep reactive ion etching (DRIE) technique. Alternatively, the alignment marks may be attached or coated directly on the second side of the silicon wafer 01.
[0110] Step 602: Form a first reflective material film layer on a first surface of a silicon wafer.
[0111] See step S22 in Figure 18. The first reflective material film layer 02 can be formed on the first surface of the silicon wafer 01 (i.e., the surface on which the alignment mark 011 is not formed). The first surface and the second surface are two opposite surfaces of the silicon wafer 01. For the mounting process of step 602, see step 401 above. Details will not be described again here.
[0112] Step 603: To form a first side of the reflector and a first reflective film of the reflector, the first reflective material film layer and the silicon wafer are processed starting from the side of the first reflective material film layer facing away from the silicon wafer using the alignment marks as references.
[0113] In this embodiment of the present application, as shown in step S23 in Figure 18, the alignment mark can be used as a reference for processing the first reflective material film layer and the silicon wafer to form a rectangular groove in the first reflective material film layer and the silicon wafer. The sidewall of the rectangular groove can be formed as a first side of the reflector. In addition, since the rectangular groove penetrates the first reflective material film layer 02, the first reflective film of the reflector can be further formed.
[0114] In an optional implementation, the first reflective material film layer 02 and the silicon wafer 01 can be etched starting from the side of the first reflective material film layer 02 facing away from the silicon wafer 01 to form the first side 1c of the reflector and the first reflective film of the reflector. For example, the first reflective material film layer 02 and the silicon wafer 01 can be etched by using a DRIE technique. The etching depth of the first reflective material film layer 02 can be equal to the thickness of the first reflective material film layer 02, i.e., the first reflective material film layer 02 needs to be etched completely. The etching depth h2 of the silicon wafer 01 can be smaller than the thickness of the silicon wafer 01.
[0115] Since the thickness of the first reflective material film layer 02 is relatively thin, processing the first reflective material film layer 02 through etching can effectively reduce the probability of cracks occurring in the first reflective material film layer 02. In other words, the reliability of the etching is high, and the yield of the tuned reflector can be guaranteed.
[0116] In another optional implementation, the first reflective material film layer 02 and the silicon wafer 01 can be cut by using a second cutting blade starting from the side of the first reflective material film layer 02 facing away from the silicon wafer 01 to form the first side 1c of the reflector and the first reflective film of the reflector. The depth of the first reflective material film layer 02 cut by using the second cutting blade can be equal to the thickness of the first reflective material film layer 02, i.e., the first reflective material film layer 02 needs to be etched completely. The cutting depth h2 of the silicon wafer 01 can be smaller than the thickness of the silicon wafer 01. In addition, the cutting direction of the second cutting blade can be perpendicular to the first surface of the silicon wafer 01.
[0117] Step 604: Attach a dicing membrane to the side of the first reflective material membrane layer facing away from the silicon wafer.
[0118] See step S24 in Figure 18. The first reflective material film layer 02 and the silicon wafer 01 may be turned over, and then the side of the first reflective material film layer 02 facing away from the silicon wafer 01 is attached to the dicing film 03. For the mounting process of step 604, see step 502 above. Details will not be described again here.
[0119] Step 605: Cut the second surface of the silicon wafer by using a first cutting blade using the alignment marks as references to form a first side of a reflector and a second side of a reflector.
[0120] See step S25 in Figure 18. A first cutting blade D1 can be used to cut the second side of the silicon wafer 01 to form a bevel groove on the second side of the silicon wafer 01. To ensure that the bevel groove is connected to the rectangular groove formed in the above step 603, that is, to ensure that the silicon wafer 01 is cut completely, the alignment mark needs to be used as a reference for cutting. After the second side of the silicon wafer 01 is cut by using the first cutting blade D1, the second side of the reflector can be formed.
[0121] In this embodiment of the present application, if mass production of multiple reflectors is required, multiple rectangular grooves may be formed in the first reflective material film layer and the silicon wafer in the aforementioned step 603. Accordingly, the aforementioned step 605 may be performed multiple times, that is, the silicon wafer may be cut multiple times by using the first cutting blade to obtain multiple separated reflectors. Then, the multiple separated reflectors may be peeled off from the dicing film and packaged into periscope lens modules respectively.
[0122] 19 is a flow chart of yet another method for manufacturing a reflector according to an embodiment of the present application. This method can be used to manufacture a reflector including a second reflective film. As shown in FIG. 19, the method can include the following steps:
[0123] Step 701: Form a first reflective material film layer on a first surface of a silicon wafer.
[0124] For the implementation process of step 701, please refer to the above step 401, and the details will not be described again here.
[0125] Step 702: Form a second reflective material film layer on a second side of the silicon wafer.
[0126] In this embodiment of the present application, the same material as that of the first reflective material film layer can be used to form the second reflective material film layer on the second side of the silicon wafer. For the mounting process of step 702, please also refer to the above step 401. Here, the details are not described again.
[0127] A reflective material film layer made of the same material is formed on the first side and the second side of the silicon wafer, so that two kinds of stresses generated by the thin film coating process can cancel each other out, thereby further reducing the deformation of the silicon wafer generated during the thin film coating, thereby ensuring the flatness of the adjusted reflector.
[0128] Step 703: Process a second reflective material film layer to obtain a second reflective film in the reflector.
[0129] It can be seen with reference to FIG. 8 that the second reflective film 103 is located on the second surface 1b of the silicon base substrate 101 in the finally formed reflector. In this embodiment of the present application, the second reflective material film layer can be cut by using a cutting blade to obtain the second reflective film in the reflector. For example, the second reflective material film layer and the second surface of the silicon wafer can be cut by using a first cutting blade to obtain the second reflective film in the reflector and form the second side of the silicon base substrate in the reflector. For the implementation process of step 703, please refer to the above step 503 or the above step 605. Details will not be described again here.
[0130] Step 704: Processing the silicon wafer and the first reflective material film layer to obtain at least one reflector.
[0131] For the implementation process of step 704, please refer to the aforementioned step 504 or the aforementioned step 603. Details will not be described again here.
[0132] Optionally, the order of steps of the method for manufacturing a reflector provided in the embodiment of the present application may be appropriately adjusted, and these steps may be increased or decreased accordingly as required. For example, step 602 may be performed before step 601, and step 702 may be performed before step 701. Any method variations that a person skilled in the art can easily conceive within the technical scope disclosed in the present application shall be included in the protection scope of the present application. Therefore, details will not be described again here.
[0133] In summary, the embodiment of the present application provides a method for manufacturing a reflector. In this method, a silicon wafer is used as a base for manufacturing the reflector, so as to effectively reduce the volume and mass of the reflector. In addition, in the reflector manufactured by using this method, the included angle between the second side and the second surface of the silicon base substrate is an obtuse angle, so as to ensure that no outwardly protruding right angle is formed between the second side and the second surface after the reflector is placed at an angle. Therefore, the space occupied when the reflector applied to the periscope lens module can be reduced, and further, the risk of side edge cracks or edge breakage of the silicon base substrate caused due to collision or friction force during the assembly of the reflector can be effectively reduced. In addition, since the Young's modulus of the silicon wafer is relatively high, the coating of the surface of the silicon wafer with a reflective material film layer does not cause a relatively large deformation of the silicon wafer, which can ensure a relatively high quality of the adjusted reflector.
[0134] An embodiment of the present application further provides a lens module. The lens module may be a periscope lens module. As shown in Fig. 20, the lens module includes the reflector 10, the lens set 20, and the photosensitive element 30 provided in the above embodiment.
[0135] The lens set 20 is located between the reflector 10 and the photosensitive element 30, and a first reflective film 102 in the reflector 10 is closer to the lens set 20 than the silicon-based substrate 101, and the first reflective film 102 is configured to reflect incident light to the lens set 20. For example, the first reflective film 102 may change the optical path direction of the incident light by 90°, so that the incident light is transmitted to the lens set 20. The lens set 20 may then converge the light reflected by the first reflective film 102 and transmit the light to the photosensitive element 30.
[0136] The lens set 20 may include multiple lenses. The photosensitive element 30 may be a complementary metal oxide semiconductor (CMOS) device.
[0137] Optionally, as shown in Fig. 20, the reflector 10 in the lens module is arranged to be inclined, and the included angle between the first reflective film 102 and the optical axis of the lens set 20 is θ, and the included angle θ is an acute angle. To enable the second side 1d of the silicon-based substrate 101 to be parallel to the optical axis of the lens set 20, the included angle δ between the second side 1d of the silicon-based substrate 101 and the first surface 1a can be designed to be the same as the included angle θ. In other words, the included angle γ between the second side 1d of the silicon-based substrate 101 and the second surface 1b can be designed as an angle complementary to the included angle θ.
[0138] Optionally, the included angle between the optical axis of the lens set 20 in the lens module and the incident light may be a right angle. Thus, the included angle between the first reflective film 102 and the optical axis of the lens set 20 may be 45°, the included angle δ between the second side 1d and the first surface 1a of the silicon-based substrate 101 may be 45°, and the included angle γ between the second side 1d and the second surface 1b of the silicon-based substrate 101 may be 135°. Thus, it can be ensured that the light reflected by the first reflective film 102 can be transmitted to the lens set 20 in a direction parallel or approximately parallel to the optical axis of the lens set 20. The incident light enters the silicon-based flat reflector through the optical window, is reflected by the reflector to undergo a 90° optical path change, is then focused by the lens set, and finally illuminates the CMOS photosensitive element.
[0139] The included angle γ between the second side 1d and the second surface 1b of the silicon-based substrate 101 is designed as a complementary angle to the included angle θ, so that in the lens module, the second side 1d of the silicon-based substrate 101 is parallel to the optical axis of the lens set 20, thereby ensuring that no outwardly protruding right angle is formed between the second side 1d and the second surface 1b. Therefore, the space occupied by the reflector 10 in the lens module can be reduced, and the risk of side edge cracks or edge breakage of the silicon-based substrate 101 caused by collision or friction force during assembly of the reflector 10 can be effectively reduced.
[0140] In summary, one embodiment of the present application provides a lens module. In order to ensure that the volume and mass of the lens module are also relatively small, the reflector in the lens module has a relatively small volume and a relatively small mass. In addition, the included angle between the second side and the second surface of the silicon base substrate in the reflector is an obtuse angle. Therefore, the space occupied when the reflector applied to the periscope lens module can be reduced, and further, the risk of cracking or edge damage of the side edge of the silicon base substrate caused by collision or friction force during the assembly of the reflector can be effectively reduced.
[0141] An embodiment of the present application further provides an electronic device. As shown in Fig. 21, the electronic device may include a housing 000 and a lens module 001 disposed in the housing 000, as provided in the above-mentioned embodiment.
[0142] Optionally, as shown in Fig. 21, the electronic device further includes an optical window 002. The housing 000 is provided with a slot 00a, and the optical window 002 may be disposed in the slot 00a for light transmission. Specifically, the optical window 002 may transmit incident light to the first reflective film 102 of the reflector 10. The included angle between the optical window 002 and the first reflective film 102 may be 45°. The optical window 002 may be made of a transparent material, such as a transparent optical glass.
[0143] Further, see Fig. 21. The electronic device further includes a reflector fixing structure 003, which is located on the bottom surface of the reflector 10, i.e., on the surface of the reflector 10 facing the first reflective film 102. The reflector fixing structure 003 is configured to support the reflector 10, so that the reflector 10 is fixed within the housing 000. The reflector fixing structure 003 can be fixedly connected to the reflector 10 in a manner such as bonding using an adhesive.
[0144] Optionally, the electronic device provided in this embodiment of the present application may be a mobile phone, as shown in Figure 21. Alternatively, the electronic device may be a device with a camera function, such as a tablet computer or a wearable device.
[0145] In summary, an embodiment of the present application provides an electronic device. The reflector used by the lens module in the electronic device has a relatively small volume and a relatively small mass. Therefore, the volume and mass of the lens module are relatively small, so that the volume and mass of the electronic device can be reduced. In addition, in order to realize the anti-shake function, the electronic device can further be provided with a motor for driving the reflector to deflect or transform. Since the mass of the reflector used in the electronic device is relatively small, the power consumption of the motor can be reduced, thereby reducing the power consumption of the electronic device, and further, the deflection frequency of the reflector can be improved, thereby improving the anti-shake performance of the electronic device.
[0146] Terms such as "first" and "second" in this application are used to distinguish between the same or similar items having substantially the same effect and function. It should be understood that elements described by terms such as "first" and "second" do not have a logical or chronological dependency, and are not limited in either number or execution order. It should be further understood that terms such as "first" and "second" are used to describe elements in the above description, but these elements should not be limited by these terms. These terms are only intended to distinguish one element from the other. For example, the first aspect may be referred to as the second aspect, and similarly, the second aspect may be referred to as the first aspect, without departing from the scope of the described examples. Both the first aspect and the second aspect may be aspects, and in some cases, may be separate and distinct aspects.
[0147] The term "at least one" as used herein means one or more, and "multiple" as used herein means two or more. For example, a plurality of reflectors refers to two or more reflectors.
[0148] The above description is merely an optional embodiment of the present application, and is not intended to limit the protection scope of the present application. Any modifications or replacements that a person skilled in the art can easily think of within the technical scope disclosed in the present application shall be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the protection scope of the claims.
Claims
1. 1. A method of manufacturing a reflector, comprising the steps of: forming a first reflective material film layer on a first surface of a silicon wafer, the material of the silicon wafer being single crystal silicon; attaching a dicing film to the first reflective material film layer on a side facing away from the silicon wafer; cutting a second surface of the silicon wafer by using a first cutting blade to form a bevel groove on the second surface of the silicon wafer, a sidewall of the bevel groove being a second side surface of the silicon wafer, the second surface of the silicon wafer facing the first surface, a cutting depth of the first cutting blade being less than a thickness of the silicon wafer, and an included angle between the sidewall of the bevel groove and the second surface being an obtuse angle; continuing cutting the silicon wafer starting from a bottom surface of the bevel groove by using a second cutting blade to cut the first reflective material film layer to form a first side of the silicon wafer, wherein an included angle between the first side and the first surface is greater than a first angle threshold, and an included angle between a sidewall of the bevel groove and the first side is greater than a second angle threshold; peeling off the dicing film; A method comprising:
2. 1. A method of manufacturing a reflector, comprising the steps of: forming a first reflective material film layer on a first surface of a silicon wafer, the material of the silicon wafer being single crystal silicon; processing the first reflective material layer and the silicon wafer starting from a side of the first reflective material layer facing away from the silicon wafer to form a rectangular groove in the first reflective material layer and the silicon wafer, a sidewall of the rectangular groove being formed as a first side of the silicon wafer, and an included angle between the first side and the first surface being greater than a first angle threshold; attaching a dicing film to the first reflective material film layer on a side facing away from the silicon wafer; cutting a second surface of the silicon wafer by using a first cutting blade to form a bevel groove on the second surface of the silicon wafer, a sidewall of the bevel groove being a second side of the silicon wafer, the second surface of the silicon wafer facing the first surface, the bevel groove being connected to the rectangular groove, an included angle between the second side and the first side being greater than a second angle threshold, and an included angle between the sidewall of the bevel groove and the second surface being an obtuse angle; peeling off the dicing film; A method comprising:
3. The step of forming a rectangular groove in the first reflective material film layer and the silicon wafer comprises: Etching the first reflective material layer and the silicon wafer starting from the side of the first reflective material layer facing away from the silicon wafer; or cutting the first reflective material film layer and the silicon wafer starting from the side of the first reflective material film layer facing away from the silicon wafer by using a second cutting blade. Including, The method of claim 2.
4. Prior to the step of processing the first reflective material film layer and the silicon wafer starting from a side of the first reflective material film layer facing away from the silicon wafer, the method further comprises: forming an alignment mark on the second surface of the silicon wafer; Further equipped with The step of forming a rectangular groove in the first reflective material film layer and the silicon wafer comprises: processing the first reflective material film layer and the silicon wafer starting from the side of the first reflective material film layer facing away from the silicon wafer by using the alignment marks as a reference. Including, The step of forming a bevel groove on the second surface of the silicon wafer comprises: cutting the second side of the silicon wafer by using the alignment marks as references and the first cutting blade. Including, The method according to claim 2 or 3.
5. forming a second reflective material layer on a second side of the silicon wafer using the same material as that of the first reflective material layer; and processing the second reflective material film layer to obtain a second reflective film in the reflector, the second reflective film being located on the second surface. The method of claim 1 , further comprising:
6. The method of claim 1 , wherein the included angles between each of the first sides and the first surface are equal to one another.
7. The method of claim 1 , wherein the included angles between each of the second sides and the second surface are equal to one another.
Citation Information
Patent Citations
Method for producing a component assembly for a package, method for producing a package having a component assembly, component assembly, and package
CN114008876A
Image collating device
JP1997179969A
Manufacture of micromirror
JP1997218304A
Shutter unit and imaging apparatus
JP2006030511A
Method of forming and mounting an angled reflector
US20070086095A1