Fireproof covering structure and construction method thereof

A fireproof coating structure integrating inorganic and combustible organic layers enhances fire resistance and insulation by suppressing temperature rise and preventing condensation, addressing the limitations of existing organic-only coatings.

JP7563936B2Active Publication Date: 2024-10-08SHIMIZU CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020171497
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-09
Publication Date
2024-10-08
Estimated Expiration
2040-10-09

AI Technical Summary

Technical Problem

Existing fireproof coating structures for steel structures rely solely on organic materials, which can compromise insulation performance due to exothermic reactions, and lack integration with inorganic materials for enhanced fire resistance, especially in humid environments where condensation can cause damage.

Method used

A fireproof coating structure that combines an inorganic fireproof coating with a combustible organic moisture-proof layer, utilizing materials like rubber asphalt or urethane foam, to enhance fire resistance and prevent condensation.

Benefits of technology

The structure improves fire resistance by suppressing temperature rise through endothermic effects of the organic layer and provides moisture-proofing, ensuring effective insulation and protection against condensation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007563936000001
    Figure 0007563936000001
  • Figure 0007563936000002
    Figure 0007563936000002
  • Figure 0007563936000003
    Figure 0007563936000003
Patent Text Reader

Abstract

To provide a fireproof coating structure with improved fireproof performance and a construction method of the same.SOLUTION: A fireproof structure 10 with which a steel material 12 is coated in a fireproof mode comprises an inorganic fireproof coating material 14 provided on a surface of the steel material 12 and a moisture-proof layer 18 comprising an inflammable inorganic material 16 provided outside of the inorganic fireproof coating material 14. The organic material 16 may include at least one of a rubber asphalt waterproof material, an urethane rubber waterproof material, a nitrile rubber waterproof material, an acrylic rubber waterproof material or a spray rigid urethane foam as a principal material.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a fire-resistant covering structure in which the surface of a steel material is covered with a fire-resistant covering material, and a construction method thereof. [Background technology]

[0002] Conventionally, when a structure made of steel, such as a steel building, is exposed to a fire, the strength and rigidity of the steel material decreases due to the increase in temperature, which may cause the structure to collapse. Therefore, fire-resistant coating is applied to the beams and columns of steel-framed structures to suppress the increase in temperature caused by fire.

[0003] Fireproof coating materials include inorganic sprayed rock wool and organic fireproof paint. The former is a light-density material that forms a relatively thick insulating layer to ensure thermal insulation, while the latter is a thin coating of fireproof paint that forms a foam layer through a combustion reaction caused by fire heating, ensuring thermal insulation. In recent years, wood materials that burn in the event of a fire have also been used as fireproof coating materials.

[0004] As described above, organic fire-resistant coating materials involving a combustion reaction have been developed and are in practical use. However, because organic materials involve an exothermic reaction called combustion, they are thought to have a detrimental effect on the insulating performance of inorganic fire-resistant coating materials, and as a result, fire-resistant coating materials that combine inorganic and organic materials are not currently in practical use.

[0005] Meanwhile, a conventional fire-resistant coating structure is known in which an intumescent fire-resistant paint layer and an anti-condensation paint layer are laminated on the surface of a structure (see, for example, Patent Document 1). However, the fire-resistant coating structure of Patent Document 1 is composed of an organic fire-resistant paint layer and an organic anti-condensation paint layer, and no inorganic fire-resistant coating material is used. In addition, the anti-condensation paint layer is provided to protect the water-soluble foaming agent and carbonization material that constitute the intumescent fire-resistant paint from condensation water and water vapor, and does not contribute to fire resistance.

[0006] Also known is a fire-resistant coating structure that includes a fire-resistant coating sheet layer that covers a steel column, and a heat insulating layer that is mainly made of a phenolic resin foam and is provided between the steel column and the fire-resistant coating sheet layer (see, for example, Patent Document 2). However, the fire-resistant coating structure of Patent Document 2, like the fire-resistant coating structure of Patent Document 1, is made of an organic fire-resistant coating sheet layer and an organic phenolic resin foam, and does not use an inorganic fire-resistant coating material. Furthermore, Patent Document 2 states, "The inventors of the present application have confirmed through experiments, etc. that in the event of a fire, the insulating layer made of the phenolic resin foam has the effect of inhibiting heat transfer even at high temperatures of 300°C or more caused by hot air until it is carbonized due to overheating, thereby slowing down (delaying) the temperature rise on the surface of the steel column, thereby making it possible to ensure a fire resistance time. Furthermore, it has been confirmed that the insulating layer is flammable but non-ignitable, and that even if it is carbonized, it simply carbonizes but does not burst into flames or melt, and furthermore, that no gas that could cause fire or temperature rise is generated." Phenolic resin foam is said to be a material that does not generate flammable gases or cause flaming combustion.

[0007] Also, a structure is known in which a moisture-proof layer made of moisture-proof synthetic resin is formed on the indoor surface of a building to which a fire-resistant covering material is attached (see, for example, Patent Document 3). However, Patent Document 3 relates to a moisture-proofing construction method and not to a fire-resistant covering structure. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2001-200597 A [Patent Document 2] JP 2010-043445 A [Patent Document 3] Japanese Patent Application Publication No. 6-185128 Summary of the Invention [Problem to be solved by the invention]

[0009] In steel-framed buildings, the mainstream approach is to install the outer perimeter columns and beams close to the exterior walls from the standpoint of design and ensuring effective area, and a composite-covered fire-resistant structure in which the exterior walls form part of the fire-resistant covering for the steel members is often adopted.

[0010] On the other hand, in a building with an exterior wall 1 separating indoor A from outdoor B, insulation material 2 for preventing condensation, a floor 3, and a synthetic coated fire-resistant structure 6 made of steel frame members 4 covered with sprayed rock wool 5 as shown in Fig. 5(1), flammable foamed plastic insulation material cannot be applied to the exterior wall surface 7 inside the synthetic coated fire-resistant structure 6 due to fire-resistance certification, so in buildings that humidify the interior in winter or in cold regions, there have been occasional cases where a large amount of condensation C is generated by the water vapor W inside the building, causing actual damage. As a countermeasure, it would be best to separate the outer periphery steel frame members 4 from the exterior wall 1 and provide a single coating as shown in Fig. 5(2), but this is often difficult.

[0011] Therefore, instead of separating the steel frame members 4 from the exterior wall 1, the inventor devised a measure to reduce condensation by applying a moisture-proof layer made of a moisture-proof material with high moisture permeability resistance to the surface of the inorganic sprayed rock wool 5, resulting in the present invention described below.

[0012] The present invention has been made in view of the above, and an object of the present invention is to provide a fire-resistant covering structure having improved fire resistance performance and a construction method thereof. [Means for solving the problem]

[0013] In order to solve the above-mentioned problems and achieve the object, the fire-resistant coating structure of the present invention is a fire-resistant coating structure in which a steel material is fire-resistant coated, and is characterized in that it comprises an inorganic fire-resistant coating material provided on the surface of the steel material, and a moisture-proof layer made of a flammable organic material provided on the outside of this inorganic fire-resistant coating material.

[0014] Furthermore, another fire-resistant covering structure according to the present invention is characterized in that, in the above-mentioned invention, the organic material contains at least one of a rubber asphalt-based waterproofing material, a urethane rubber-based waterproofing material, a nitrile rubber-based waterproofing material, an acrylic rubber-based waterproofing material, or a sprayed rigid urethane foam as a main material.

[0015] In addition, the method of constructing a fire-resistant coating structure according to the present invention is a method of constructing the above-mentioned fire-resistant coating structure, which is characterized in that after an inorganic fire-resistant coating material is applied to the surface of a steel material, a moisture-proof layer made of a flammable organic material is applied to the outside of this inorganic fire-resistant coating material. Effect of the Invention

[0016] The fire-resistant covering structure according to the present invention is a fire-resistant covering structure in which a steel material is fire-resistantly covered, and includes an inorganic fire-resistant covering material provided on the surface of the steel material, and a moisture-proof layer made of a combustible organic material provided on the outside of the inorganic fire-resistant covering material, so that the fire-resistant performance can be improved compared to a structure in which the steel material is covered only with an inorganic fire-resistant covering material, and also has the effect of imparting moisture-proof performance.

[0017] Furthermore, according to another fire-resistant covering structure of the present invention, the organic material contains at least one of a rubber asphalt-based waterproofing material, a urethane rubber-based waterproofing material, a nitrile rubber-based waterproofing material, an acrylic rubber-based waterproofing material, or a sprayed rigid urethane foam as a main material, and therefore it is possible to achieve the effect of improving fire resistance and imparting moisture-proofing performance by using this organic material.

[0018] Furthermore, according to the method for constructing a fire-resistant covering structure of the present invention, which is a method for constructing the above-mentioned fire-resistant covering structure, an inorganic fire-resistant covering material is applied to the surface of a steel material, and then a moisture-proof layer made of a combustible organic material is applied to the outside of the inorganic fire-resistant covering material, so that the fire resistance can be improved compared to a structure in which a steel material is covered only with an inorganic fire-resistant covering material, and also an effect of imparting moisture-proofing performance can be achieved. [Brief description of the drawings]

[0019] [Figure 1] FIG. 1 is a cross-sectional view showing an embodiment of a fire-resistant covering structure and a construction method thereof according to the present invention. [Diagram 2] FIG. 2 is a cross-sectional view showing the shape and dimensions of the test specimen and the temperature measurement positions. [Diagram 3] FIG. 3 shows the results of measuring the steel temperature of the test specimens, where (1) is test specimen N, (2) is test specimen A, and (3) is test specimen U. [Figure 4] FIG. 4 shows the measurement results at the center of the span, where (1) is the deflection amount and (2) is the deflection velocity. [Diagram 5] Figure 5 is an explanatory diagram of the condensation problem in a conventional fire-resistant coating structure and its countermeasures. (1) shows the condensation on the exterior wall surface, and (2) shows the countermeasure against condensation by moving the beam position. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, preferred embodiments of a fire-resistant covering structure and a method for constructing the same according to the present invention will be described in detail with reference to the accompanying drawings. However, the present invention is not limited to these preferred embodiments.

[0021] As shown in Fig. 1, a fire-resistant covered structure 10 according to an embodiment of the present invention is applied to a steel beam provided adjacent to an exterior wall 1 that separates an interior space A from an exterior space B. This fire-resistant covered structure 10 includes an inorganic fire-resistant covering material 14 provided on the surface of a steel member 12 (steel material) made of H-shaped steel, and a moisture-proof layer 18 made of a flammable organic material 16 provided on the outer surface of the fire-resistant covering material 14.

[0022] The fireproof coating material 14 can be made of an inorganic fireproof coating material such as sprayed rock wool. The organic material 16 can be made of a flammable moisture-proof material such as a rubber asphalt waterproof material, a urethane rubber waterproof material, a nitrile rubber waterproof material, an acrylic rubber waterproof material, or a sprayed hard urethane foam. The organic material 16 may be made of at least one of a rubber asphalt waterproof material, a urethane rubber waterproof material, a nitrile rubber waterproof material, an acrylic rubber waterproof material, or a sprayed hard urethane foam as a main material. By providing a moisture-proof layer 18 of the organic material 16 on the outer surface of the fireproof coating material 14, it is possible to prevent the water vapor W in the room from condensing on the outer wall surface.

[0023] In addition, examples of organic materials mentioned above include rubber asphalt waterproofing materials, urethane rubber waterproofing materials, nitrile rubber waterproofing materials, acrylic rubber waterproofing materials, sprayed hard urethane foam, etc., but the present invention is not limited to these materials, and any organic material that has moisture-proofing properties and the following thermal properties will do.

[0024] [Thermal properties] The differential heat characteristic values ​​in TG-DTA analysis (temperature conditions: room temperature to 1000°C (20°C / min), sample amount: approximately 5 mg) must satisfy the following conditions. - 10μV or less in helium gas atmosphere and 0.36mV or less in air

[0025] When constructing this fire-resistant covered structure 10, first, an inorganic fire-resistant covering material 14 is applied to the surface of the steel frame member 12. Then, a flammable organic material 16 is sprayed onto the outside of this fire-resistant covering material 14 to form a moisture barrier layer 18. In this manner, the fire-resistant covered structure 10 can be constructed.

[0026] The operation and function of the above configuration will now be described. When the combustible moisture barrier layer 18 made of the organic material 16 applied to the surface of the inorganic fire-resistant coating material 14 burns in the event of a fire, the heat energy from the self-combustion is consumed by the thermal decomposition (phase change) of the unburned parts of the moisture barrier layer 18, resulting in an endothermic effect. Therefore, while the combustible moisture barrier layer 18 remains on the surface of the inorganic fire-resistant coating material 14, the heat energy from the self-combustion does not directly heat the inorganic fire-resistant coating material 14, suppressing the temperature rise of the inorganic fire-resistant coating material 14. Furthermore, even if a part of the heat energy generated not only by the self-combustion of the combustible moisture barrier layer 18 but also by the combustion of combustible materials other than the moisture barrier layer 18 in the fire room flows into the moisture barrier layer 18 of the fire-resistant coating, it is consumed by the thermal decomposition of the unburned parts of the moisture barrier layer 18, suppressing the temperature rise of the inorganic fire-resistant coating material 14.

[0027] Therefore, according to this embodiment, by applying the organic material 16 to the surface of the inorganic fire-resistant covering material 14, it is possible to improve the fire resistance performance more than when the steel frame member 12 is covered only with the inorganic fire-resistant covering material 14. In addition, since the moisture-proof layer 18 is provided, it is possible to impart moisture-proof performance to the fire-resistant covering structure under normal conditions.

[0028] (Verification of the Effects of the Invention) Next, an example of a test carried out to verify the effects of the present invention and the results thereof will be described.

[0029] This test was conducted to examine the fire resistance (1-hour fire resistance) of the fire-resistant coating structure according to the present invention. Figure 2 shows the shape and dimensions of the test specimen and the temperature measurement positions. The numbers (C1 to C7) in the figure indicate the temperature measurement positions. As shown in this figure, the test specimen was composed of a steel beam (H-shaped steel) coated with a fire-resistant coating material and a moisture-proof coating. The H-shaped steel used was H-400 x 200 x 8 x 13 mm, SN490B. ALC panels with a thickness of 100 mm were used for the floor above the beam, and ALC panels with a thickness of 125 mm were used for the wall that constitutes part of the fire-resistant coating. The total length of the steel beam was 5800 mm, and the width of the floor and the height of the wall were 1100 mm.

[0030] The fire-resistant coating material used was sprayed rock wool (1-hour fire resistance specification, thickness 25 mm, bulk specific gravity 0.28 or more (bone dry), moisture content 2.3-2.7 wt%). The sprayed rock wool was applied prior to the application of the moisture-proof coat. Two types of materials were used for the moisture-proof coat: Moisture-proof coat A "environmentally friendly modified asphalt-based waterproofing material (compliant with JIS A 6021)" and Moisture-proof coat U "sprayed rigid urethane foam", both of which were applied using the spraying method. The target thickness for Moisture-proof coat A was set at 3 mm, and for Moisture-proof coat U the target thickness was set at 25-30 mm.

[0031] Test specimen A with moisture-proof coating A, test specimen U with moisture-proof coating U (Example), and test specimen N without moisture-proof coating (Comparative Example) were placed in a furnace and subjected to a loaded heating experiment. The load on the test specimen was a three-point two-line load, and heating was performed with a long-term allowable bending moment acting on the center of the span of the test specimen. The applied load was a load obtained by subtracting the weight of the test specimen and the weight of the loading jig placed directly on the test specimen from the required applied load, and was applied with an oil jack. The total load of the two-line load was 274 kN. The heating time was 60 minutes, and the test specimen was gradually cooled while still placed in the furnace until it was confirmed that the steel temperature reached the maximum temperature and the deflection rate was stable. The heating temperature was such that the temperature measured over time by a thermocouple followed the standard heating temperature curve of ISO834.

[0032] The moisture-proof coating was completely burned away by this heating. Although there were some differences in the coloring of the cross section of the sprayed rock wool, there was no difference in the adhesion state.

[0033] Figures 4 (1) to (3) show the measurement results of the furnace temperature and the steel temperature (center of span). Compared to specimen N, there is no significant difference in the steel temperature of specimen A and specimen U. The maximum steel temperature at each steel temperature measurement cross section was higher for specimen N at each cross section. One possible reason for this is the endothermic effect of the thermal decomposition of the unburned parts of the moisture-proof coating.

[0034] The measurement results of the deflection amount are shown in Figure 5 (1). The measurement results of the deflection speed are shown in Figure 5 (2). Each measurement result was below the maximum value stipulated in the Fire Resistance Testing and Performance Evaluation Procedures Manual (General Incorporated Foundation, Japan Construction Materials Testing Center), and it was determined that the material had one-hour fire resistance.

[0035] In this way, a one-hour loaded heating experiment was conducted on a steel beam coated with a sprayed rock wool synthetic coating and an organic moisture-proof coating. The results confirmed that the moisture-proof coating did not reduce the fire resistance performance and satisfied the one-hour fire resistance requirement.

[0036] In this test, sprayed rock wool was used as the inorganic fire-resistant coating material, but similar results were observed in tests using wrapped fire-resistant coating material made of heat-resistant rock wool felt.

[0037] As described above, the fire-resistant covering structure according to the present invention is a fire-resistant covering structure in which a steel material is fire-resistantly covered, and includes an inorganic fire-resistant covering material provided on the surface of the steel material, and a moisture-proof layer made of a combustible organic material provided on the outside of the inorganic fire-resistant covering material, so that the fire-resistant performance can be improved compared to a structure in which the steel material is covered only with an inorganic fire-resistant covering material, and moisture-proof performance can also be imparted.

[0038] Furthermore, according to another fire-resistant covering structure of the present invention, the organic material contains at least one of a rubber asphalt-based waterproofing material, a urethane rubber-based waterproofing material, a nitrile rubber-based waterproofing material, an acrylic rubber-based waterproofing material, or a sprayed rigid urethane foam as a main material, and therefore the use of this organic material can improve fire resistance and impart moisture-proofing performance.

[0039] Furthermore, according to the method for constructing a fire-resistant covering structure of the present invention, which is a method for constructing the above-mentioned fire-resistant covering structure, an inorganic fire-resistant covering material is applied to the surface of a steel material, and then a moisture-proof layer made of a combustible organic material is applied to the outside of the inorganic fire-resistant covering material, so that the fire resistance can be improved compared to a structure in which the steel material is covered only with an inorganic fire-resistant covering material, and moisture-proof performance can also be imparted. [Industrial Applicability]

[0040] INDUSTRIAL APPLICABILITY As described above, the fire-resistant coating structure and its construction method of the present invention are useful for fire-resistant coating structures in which the surface of steel material is coated with a fire-resistant coating material, and are particularly suitable for improving fire resistance and imparting moisture-proofing performance. [Explanation of symbols]

[0041] 1. Exterior wall 3 Beds 10 Fire-resistant coating structure 12 Steel members (steel materials) 14 Fireproof cladding 16 Organic materials 18 Moisture barrier A Indoor B Outdoors

Claims

1. A fire-resistant coating structure in which a steel material provided opposite an exterior wall is fire-resistant coated, the structure comprising the exterior wall, a deck installed on top of the steel material, and an inorganic fire-resistant coating material provided on the surface of the steel material, the fire-resistant covering material is provided on a side of the steel material opposite to a side facing the exterior wall and an opposite side to a side facing the deck so as to seal a gap between the exterior wall and the steel material, and is provided with a moisture-proof layer made of a flammable organic material on a surface thereof; A fire-resistant covering structure, characterized in that no insulation material is provided inside the space surrounded by the exterior wall, the deck, and the fire-resistant covering material.

2. A method for applying the fire-resistant coating structure of claim 1, comprising the steps of: A method for constructing a fire-resistant covering structure, comprising the steps of: applying the fire-resistant covering material to a surface of the steel material; and then applying the moisture-proof layer to the outside of the fire-resistant covering material.

Citation Information

Patent Citations

  • Moisture preventive construction method with site spraying

    JP1994185128A

  • Fire-resistant covering laminate structure of steel for external use

    JP1996093076A

  • Fire-resistant coating material

    JP1998152913A

  • Fireproof covering structure with condensation prevention function and fireproof covering method

    JP2001200597A

  • Fire-resistant coating structure of steel column

    JP2010043445A