Design methods, manufacturing methods, welding methods, and waterproofing methods for precoated components
The method strategically positions fire-resistant materials on pre-coated steel members to prevent foaming during welding and maintain fire resistance, ensuring performance in fires and reducing on-site coating needs.
Patent Information
- Application Number
- JP2021017387
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-02-05
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2041-02-05
AI Technical Summary
Welding pre-coated steel members coated with fire-resistant paint can adversely affect the paint film, causing it to foam and lose its fire-resistant performance before exposure to actual fire, as the welding heat reaches the foaming temperature of the paint.
A method to design, manufacture, and weld pre-coated members by determining the placement position of fire-resistant materials to avoid foaming due to welding heat, involving a relational expression to set the distance from the welding position based on steel plate thickness and temperature rise, and applying fire-resistant materials strategically to maintain performance.
Ensures the fire-resistant materials maintain their performance during welding and in a fire by preventing foaming and protecting against rainwater, thereby ensuring the required fire resistance and minimizing site-specific coating work.
Smart Images

Figure 0007564004000001 
Figure 0007564004000002 
Figure 0007564004000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for designing, manufacturing, welding, and waterproofing a precoated member in which a fire-resistant paint or the like is applied to a steel frame member in advance at a factory or the like, and then the precoated member is transported to a construction site and welded to other members. [Background technology]
[0002] Conventionally, when a structure using steel materials, such as a steel-frame building, is exposed to a fire, the strength and rigidity of the steel materials decrease due to the rise in temperature, and there is a risk that the structure may collapse. Therefore, fire-resistant coating is applied to the beams and columns of steel-framed structures to suppress the rise in temperature due to fire heating (for example, see Patent Document 1).
[0003] One type of fire-resistant coating material is a fire-resistant paint whose main component is ammonium polyphosphate. When exposed to heat during a fire, fire-resistant paint begins to foam at around 200-300℃, expanding 20-30 times in size to form an insulating layer and suppress the temperature rise of steel materials.
[0004] When steel components are pre-painted with fire-resistant paint at a factory or the like and then transported to a construction site for erection (hereinafter, components pre-painted with fire-resistant paint or the like at a factory or the like may be referred to as pre-coated components), it is common to use welding and / or bolting to join them to other steel components (see, for example, Patent Document 2). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 11-222958 [Patent Document 2] Special Publication No. 6-69614 Summary of the Invention [Problem to be solved by the invention]
[0006] However, when welding is performed on the precoated member, there is a concern that the coating of the fire-resistant paint may be adversely affected by the heat generated during welding. When welding the end of the precoated member to another member, if the temperature of the steel material of the precoated member reaches 200 to 300°C, which is the foaming temperature of the fire-resistant paint described above, the fire-resistant paint may foam even though it is not exposed to fire, and the required performance may not be exhibited in the event of a fire. For this reason, when welding is performed on the end of the member to join the precoated member, which has been pre-painted with fire-resistant paint in a factory, to another member, there has been a demand for a technology that allows the fire-resistant paint to exhibit the required performance in the event of a fire without the welding heat adversely affecting the coating of the fire-resistant paint and the undercoat paint (e.g., anti-rust paint) that serves as the base for the fire-resistant paint.
[0007] The present invention has been made in consideration of the above, and aims to provide a design method, a manufacturing method, a welding method, and a waterproofing method for a precoat member that can exhibit the required fire resistance performance in the event of a fire. [Means for solving the problem]
[0008] In order to solve the above problems and achieve the object, a design method for a precoat member according to the present invention is a method for designing a position of a fire-resistant material in a precoat member comprising a steel member and a foamable fire-resistant material that is provided on the surface of the steel member and foams in a predetermined temperature range when heated, such that the fire-resistant material does not foam due to welding heat for the precoat member and can exhibit predetermined fire resistance in the event of a fire, the method comprising the steps of: determining, for each steel thickness, the relationship between the amount of steel temperature rise of the steel member when welding the ends of the steel members and the distance from the welding position; determining the relationship between the coefficient of a relational equation expressing the relationship and the steel thickness; setting the steel thickness and the amount of steel temperature rise, determining the coefficient of the relational equation based on the set steel thickness, and applying the set amount of steel temperature rise to the relational equation to determine the distance from the welding position; and designing the position of the fire-resistant material based on the determined distance.
[0009] In addition, the manufacturing method of the precoat member of the present invention is characterized by having a step of designing the placement position of the fire-resistant material based on the above-mentioned design method of the precoat member, and a step of applying the fire-resistant material to the surface of the steel member in the designed placement position to produce the precoat member.
[0010] In addition, the welding method for precoated members according to the present invention is characterized by having a step of manufacturing a precoated member based on the above-mentioned manufacturing method for a precoated member, and a step of welding another steel member to a welding position set on the manufactured precoated member.
[0011] Furthermore, the waterproofing method for precoated members of the present invention is based on the above-mentioned manufacturing method for precoated members, and is characterized in that, when a precoated member is produced by successively applying an undercoat material, a main material which is a fire-resistant material, an intermediate coat material and / or a top coat material to the surface of a steel frame member, the application range of the main material is set farther from the welding position than the undercoat material applied to the surface closer to the end of the precoated member which is the welding position, and the end of the main material which forms the boundary with the undercoat material is protected by the intermediate coat material and / or top coat material. Effect of the Invention
[0012] According to the method for designing a precoat member of the present invention, in a precoat member comprising a steel member and a foamable fireproof material that is provided on the surface of the steel member and foams in a predetermined temperature range when heated, the method for designing the position of the fireproof material allows the fireproof material to exhibit a predetermined fire resistance in the event of a fire, and the method includes the steps of: determining, for each steel thickness, the relationship between the amount of steel temperature rise of the steel member when welding the ends of the steel members and the distance from the welding position; determining the relationship between the coefficient of a relational equation expressing the relationship and the steel plate thickness; setting the steel plate thickness and the amount of steel temperature rise, determining the coefficient of the relational equation based on the set steel plate thickness, and applying the set amount of steel temperature rise to the relational equation to determine the distance from the welding position; and designing the position of the fireproof material based on the determined distance, thereby achieving the effect of designing a precoat member in which the fireproof material is able to exhibit a required fire resistance in the event of a fire.
[0013] Furthermore, according to the method for manufacturing a precoat member of the present invention, it has a step of designing the position of the fire-resistant material based on the above-mentioned design method for a precoat member, and a step of applying the fire-resistant material to the surface of the steel member in the designed position to produce a precoat member, thereby achieving the effect of manufacturing a precoat member in which the fire-resistant material can exhibit the required fire resistance performance in the event of a fire.
[0014] Furthermore, the welding method for precoated members according to the present invention includes a step of manufacturing a precoated member based on the above-mentioned manufacturing method for a precoated member, and a step of welding other steel members to welding positions set on the manufactured precoated member, thereby achieving the effect of being able to exhibit the required fire resistance performance in the event of a fire.
[0015] According to the waterproofing method for precoated members of the present invention, when a precoated member is produced by successively applying an undercoat, a fire-resistant main material, an intermediate coat and / or a top coat to the surface of a steel frame member based on the above-mentioned manufacturing method for precoated members, the application range of the main material is set farther from the welding position than the undercoat applied to the surface closer to the end of the precoated member, which is the welding position, and the end of the main material forming the boundary with the undercoat is protected by the intermediate coat and / or top coat, so that it is possible to prevent the main material from getting wet with rainwater or the like and dissolving at construction sites, etc. This has the effect of providing the required fire resistance in the event of a fire. [Brief description of the drawings]
[0016] [Figure 1] FIG. 1 is a diagram showing the relationship between the temperature rise of steel material during welding (the amount of temperature rise from the initial temperature) and the distance from the welding position. [Diagram 2] FIG. 2 shows the relationship between the coefficients in the regression equation for the relationship between steel temperature rise and plate thickness and the plate thickness, where (1) shows the relationship between coefficient a and plate thickness, and (2) shows the relationship between coefficient b and plate thickness. [Diagram 3] FIG. 3 is a table showing the coefficients a·b in the regression equation for the relationship between steel temperature rise and plate thickness. [Figure 4] FIG. 4 is a table showing an example of calculation of the separation distance from the welding position in the case where the interpass control temperature is 350° C., the allowable steel temperature is 200° C., and the initial steel temperature is 200° C. [Diagram 5] FIG. 5 is a table showing an example of calculation of the separation distance from the welding position in the case where the interpass control temperature is 250° C., the allowable steel temperature is 200° C., and the initial steel temperature is 200° C. [Figure 6] FIG. 6 is a diagram showing an embodiment of a method for designing, manufacturing, welding, and waterproofing a precoated member according to the present invention, where (1) is a side view of the main part, and (2) is an enlarged cross-sectional view of part P. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] The present invention relates to a technique for ensuring that fire-resistant paint exerts the required performance in the event of a fire without adversely affecting the coating of the fire-resistant paint and the undercoat paint (e.g., anti-rust paint) that serves as the base for the fire-resistant paint when welding is performed on the end of a precoated member that has been pre-coated with a fire-resistant paint (fire-resistant material) in a factory to join the precoated member to another member. Hereinafter, embodiments of the design method, manufacturing method, welding method, and waterproofing method for the precoated member according to the present invention will be described in detail with reference to the drawings. Note that the present invention is not limited to these embodiments.
[0018] First, the background of the investigation that led to the present invention and the basic configuration of the present invention will be described. Regarding the welding heat that affects the coating of the precoated member, the present inventors considered the following three properties. (1) Although the number of welds (passes) per unit weld length increases as the plate element of the steel material to be welded becomes thicker, the thicker the plate element of the steel material is, the greater the heat capacity, so the amount of heat energy per unit weld length due to welding can be considered to be roughly the same regardless of the thickness of the plate element of the steel material. However, even if the plate element is thicker, the heat dissipation area per unit weld length is almost the same depending on the thickness of the plate element of the steel material. Therefore, the thicker the plate element is, the slower the cooling due to heat dissipation becomes, so there is a possibility that the steel temperature will be slightly higher with a thicker plate element. (2) If the control temperature between passes during welding is lowered, the difference in steel temperature rise due to plate thickness mentioned above will be smaller. (3) Due to the consumption of thermal energy through thermal conduction and the release of thermal energy from the steel surface to the surrounding air, etc. through convection and radiation, the temperature of the steel decreases with increasing distance from the weld position in the direction of the material axis of the component.
[0019] In order to verify these three properties (1) to (3), the inventors carried out welding experiments on steel members. For the steel members, steel beams of H-shaped steel (SN490B) with fixed outside dimensions were used. The cross section of this H-shaped steel was 700 x 250 x 12 x t. Three flange thicknesses t were used: t = 19, 22, and 25 mm. The ends of steel members with the same flange thickness were butted together, and the web parts were bolted together via gusset plates. The flanges were then welded together using full penetration butt welding, and the temperature range affected was confirmed by measuring the steel temperature at that time.
[0020] Figure 1 shows the relationship between steel temperature rise during welding (temperature rise from the initial temperature) and the distance from the welding position. Figures 1 (1) and (2) show the case where the interpass temperature control is T = 350°C, and Figures 1 (3) and (4) show the case where T = 250°C. Figures 1 (1) and (3) show the top flange, and Figures 1 (2) and (4) show the bottom flange. Each figure also shows the results of a regression analysis (regression equation) of the relationship between steel temperature rise (y) and distance from the welding position (x). The three properties mentioned above were largely confirmed from these figures.
[0021] To prevent the steel temperature of the welded plate element of the welded component from reaching 200-300°C, which is the foaming temperature of the fire-resistant paint, it is necessary to provide a separation distance between the welding position and the pre-coated painted area. The separation distance can be found by calculating the coefficients of the regression equation shown in Figure 1 according to the plate thickness. Figure 2 shows the relationship between the coefficients of the regression equation in Figure 1 and the plate thickness. The coefficients a and b of the regression equation are given by the following formula (1), which is based on the regression equation shown in Figure 1.
[0022] y = a × exp(bx) Equation (1) Here, y is the steel temperature rise (℃), x is the distance from the welding position (mm), and a and b are the coefficients of the regression equation.
[0023] In addition, the results of a regression analysis (regression equation) of the relationship between the coefficients a and b (y) and the plate thickness (x) are also shown in Figure 2. This regression equation can be summarized as shown in Figure 3.
[0024] The above formula (1) is the relationship between the steel temperature rise and plate thickness. In reality, steel has an initial temperature, so the target steel temperature rise value must be the target steel temperature minus the initial steel temperature. This can be expressed as formulas (2) and (2A).
[0025] (T M -T i )=a×exp(bx) ··· Equation (2) That is, T M =a×exp(bx)+T i ··· Formula (2A)
[0026] Here, T M : Target steel temperature (℃), T i : Initial temperature of steel (℃). Formula (2) is used to calculate the distance x from the welding position. M When this is transformed into an equation expressed as above, it becomes equation (3).
[0027] x = (1 / b) × log e {(T M -T i ) / a} ··· Formula (3)
[0028] Here, a and b are from Figure 3. For this formula (3), a and b obtained from plate thickness t, and allowable steel temperature T M , initial temperature of steel T i The necessary clearance distance x can be calculated by applying these three conditions. However, the coefficients a and b in Figure 3 were obtained from plate thicknesses t = 19 mm, 22 mm, and 25 mm, and since the coefficients are extrapolated when the plate thickness is significantly different from these, it is advisable to confirm the results by conducting welding tests, etc., as necessary.
[0029] For example, when the interpass control temperatures are 350°C and 250°C, the allowable steel temperature T M =150℃, steel initial temperature T i The calculation results of the separation distance when the temperature is set to 20°C are shown in Figures 4 and 5, respectively.
[0030] The above method allows the distance from the welding position (steel end) to the precoat range to be determined based on the interpass control temperature, steel allowable temperature, initial steel temperature, and plate thickness. Therefore, when designing a precoated member, the interpass control temperature, steel allowable temperature, initial steel temperature, and plate thickness are set, and the coefficients a and b are determined based on the set plate thickness. Then, the set steel allowable temperature and initial steel temperature are applied to formula (3) to determine the distance, and the precoat range (position) of the fire-resistant paint can be designed based on this distance. Then, by precoating the fire-resistant paint on the steel member while avoiding the part at the distance, a precoated member can be manufactured in which the steel temperature during welding does not reach 200 to 300°C, which is the foaming temperature of the fire-resistant paint.
[0031] (Example) Next, an embodiment of the present invention will be described. FIG. 6 shows an example of the side of the end of a precoated member produced using the above method. As shown in this figure, the precoated member 1 is made of an H-shaped steel having a web 2, an upper flange 3, and a lower flange 4. The surface of the end 5 side of the precoated member 1 is divided into an unpainted part 6 that is not precoated and a painted part 7 that is precoated. The unpainted part 6 is set within a range of a distance L from the end 5 of the precoated member 1 to the painted part 7. The painted part 7 is set inside a position that is separated by the distance L from the end 5 of the precoated member 1. The repainting specification of the painted part 7 is divided into a part A with only a primer 8 (rust-preventive paint), a part B with the primer 8, a main material 9 (fireproof paint), a middle coat 10, and a top coat 11 painted in this order, and a part C at the boundary between them.
[0032] In the example shown in this figure, the precoated member is assumed to be made of H-shaped steel (SN490B) with cross-sectional dimensions of 700 x 250 x 12 x t. The flange thicknesses t are assumed to be 19, 22, and 25 mm, and the flanges are assumed to be butted against the end 5 of the precoated member 1 and welded to each other by full penetration butt welding. In this case, the separation distance L in the precoated member 1 can be set to about 200 mm, the section length LA of part A to about 100 mm, and the section length LC of part C to about 10 mm. If such a precoated member is transported to a construction site, erected, and welded to other steel members, the welding heat will not adversely affect the coating of the main material 9 (fire-resistant paint) and the undercoat material 8, and the fire-resistant paint can perform as required in the event of a fire.
[0033] In addition, after the precoated member is joined to another member, a fireproof coating must be applied around the joint, but according to this embodiment, the precoated area of the fireproof paint can be expanded to the maximum extent possible, minimizing the area of the fireproof coating at the construction site, thereby reducing the labor required for fireproof coating work at the construction site.
[0034] In the above precoated member 1, the area affected by the heat of welding becomes the uncoated portion 6, which is not precoated, so it is necessary to take measures to prevent rust (e.g., rust fluid due to rainfall, etc.) generated in the uncoated portion 6 from contaminating the precoated area of the coated portion 7. Therefore, as a rust prevention measure before the welding work, the end portion 5 of the precoated member 1 may be wrapped with a wrapping material in advance, and the wrapping material may be peeled off at the time of welding. Alternatively, the boundary between the uncoated portion 6 and the undercoat material 8 may be covered with a masking tape of about 50 mm in width, and the masking tape may be peeled off at the time of on-site painting without being peeled off at the time of welding. Alternatively, the boundary between the undercoat material 8 and the main material 9 may be protected by the intermediate coat material 10 and the top coat material 11, and the protective layer of the intermediate coat material 10 and the top coat material 11 may be roughened with sandpaper or the like at the time of on-site painting.
[0035] In addition, after welding of the precoated member to other members is completed, the precoated member may be exposed to rainwater, etc. until a floor, roof, etc. are constructed on top of it. When water-soluble ammonium polyphosphate, the main component of the fire-resistant paint, gets wet with rainwater, etc., it dissolves and the specified fire resistance performance cannot be achieved. Therefore, as shown in Figure 6 (2), it is desirable to protect the boundary (part C) between the undercoat material 8 and the main material 9 with an intermediate coat material 10 and a top coat material 11. This type of protection method has the effect of preventing the water-soluble ammonium polyphosphate, the main component of the fire-resistant paint, from getting wet with rainwater and dissolving, and is an important method for ensuring the specified fire resistance performance.
[0036] In addition, measures to prevent scattering of spatter may be taken to protect the pre-coated painted portion 7 during welding. In this case, for example, a metal fitting for attaching lighting to the unpainted portion 6 on the inner surface of the flange may be used as a member for preventing scattering of spatter.
[0037] As described above, according to the design method of a precoat member of the present invention, in a precoat member including a steel member and a foamable fireproof material that is provided on the surface of the steel member and foams in a predetermined temperature range when heated, the method is a method for designing a position of the fireproof material such that the fireproof material does not foam due to welding heat for the precoat member and the fireproof material can exhibit a predetermined fire resistance in the event of a fire, the method includes the steps of: determining, for each steel plate thickness, the relationship between the amount of steel temperature rise of the steel member when welding the ends of the steel members and the distance from the welding position; determining the relationship between the coefficient of a relational equation expressing the relationship and the steel plate thickness; setting the steel plate thickness and the amount of steel temperature rise, determining the coefficient of the relational equation based on the set steel plate thickness, and applying the set amount of steel temperature rise to the relational equation to determine the distance from the welding position; and designing the position of the fireproof material based on the determined distance, so that a precoat member can be designed in which the fireproof material can exhibit a required fire resistance in the event of a fire.
[0038] Furthermore, the method for manufacturing a precoat member of the present invention includes a step of designing the position of the fire-resistant material based on the above-mentioned precoat member design method, and a step of applying the fire-resistant material to the surface of the steel member in the designed position to produce a precoat member, so that a precoat member can be manufactured in which the fire-resistant material can exhibit the required fire resistance performance in the event of a fire.
[0039] Furthermore, the welding method for precoated members according to the present invention includes a step of producing a precoated member based on the above-mentioned manufacturing method for a precoated member, and a step of welding other steel members to welding positions set on the produced precoated member, so that the required fire resistance performance can be exhibited in the event of a fire.
[0040] According to the waterproofing method for precoated members of the present invention, when a precoated member is produced by successively applying an undercoat, a fire-resistant main material, an intermediate coat and / or a top coat to the surface of a steel frame member based on the above-mentioned manufacturing method for precoated members, the application range of the main material is set farther from the welding position than the undercoat applied to the surface closer to the end of the precoated member, which is the welding position, and the end of the main material forming the boundary with the undercoat is protected by the intermediate coat and / or top coat, so that it is possible to prevent the main material from getting wet with rainwater or the like and dissolving at construction sites, etc. This makes it possible to exhibit the required fire resistance in the event of a fire. [Industrial Applicability]
[0041] As described above, the design method, manufacturing method, welding method, and waterproofing method for a precoated member of the present invention are useful for precoated members in which fire-resistant paint, etc. is applied to steel components in advance at a factory or the like, and then the precoated members are transported to a construction site and welded to other components, and are particularly suitable for enabling the fire-resistant paint, etc. of the precoated member to exhibit the required fire resistance performance in the event of a fire. [Explanation of symbols]
[0042] 1 Precoated material 2. Web 3 Top flange 4 Bottom flange 5 End 6 Unpainted area 7. Painting Department 8. Undercoat 9 Main materials (fire-resistant paint, fire-resistant materials) 10 Undercoat material 11 Topcoat
Claims
1. A method for designing a position of a precoated member including a steel frame member and a foamable fireproof material that is provided on the surface of the steel frame member and foams at a predetermined temperature range when heated, so that the fireproof material does not foam due to welding heat to the precoated member and can exhibit a predetermined fire resistance in the event of a fire, comprising: A step of determining a relationship between a temperature rise of a steel material of a steel member and a distance from a welding position when welding ends of the steel member together for each steel plate thickness; A step of determining a relationship between a coefficient of a relational equation representing the relationship and a plate thickness of a steel material; A step of setting a thickness of a steel material and an amount of temperature rise of the steel material, determining a coefficient of the relational expression based on the set thickness of the steel material, and applying the set amount of temperature rise of the steel material to the relational expression to obtain a distance from a welding position; and designing a placement position of the refractory material based on the determined distance.
2. A step of designing an arrangement position of a fire-resistant material based on the design method of a precoat member according to claim 1; and applying a fire-resistant material to the surface of the steel member in the designed position to produce a precoated member.
3. A step of manufacturing a precoat member based on the method for manufacturing a precoat member according to claim 2; and welding another steel member to the welding position set on the manufactured precoated member.
4. In the case of producing a precoated member by sequentially coating a base coat material, a main material which is a fire-resistant material, a middle coat material and / or a top coat material on the surface of a steel frame member based on the manufacturing method of the precoated member according to claim 2, A waterproofing method for a precoated member, characterized in that the application range of the main material is set farther from the welding position than the undercoat material applied to the surface closer to the end of the precoated member, which is the welding position, and the end of the main material forming the boundary with the undercoat material is protected with a middle coat material and / or a top coat material.
Citation Information
Patent Citations
Data indicating manufacturing date of printed wiring board
JP1994069614A
Construction method of steel frame fire resistive covering
JP1995268985A
Hybrid fire resistive cover structure body and fire resistive covering method
JP1999222958A
Steel material having refractory capacity
JP2002079606A
Fireproof construction method for structure
JP2014105566A