Method and system for producing particles

By adjusting the foaming ratio during crystallization to between 100% and 112%, the method and system improve filtration properties of particles, addressing the limitations of conventional defoaming methods and ensuring better product quality.

JP7565815B2Active Publication Date: 2024-10-11SUMITOMO CHEM CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021017673
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-02-05
Publication Date
2024-10-11
Estimated Expiration
2041-02-05

AI Technical Summary

Technical Problem

Conventional defoaming methods in particle crystallization processes are not universally applicable due to equipment requirements and may compromise product quality, and there is a need for particles with good filtration properties.

Method used

A manufacturing method and system that adjusts the foaming ratio of the foam layer during crystallization to be between 100% and 112% by controlling the addition rate of the second solution, stirring power, temperature, and solvent amount, using a foaming ratio adjusting device to enhance dispersion and prevent localized concentration.

Benefits of technology

This approach produces particles with improved filtration properties, reducing filtration resistance and drying time, thereby enhancing overall product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007565815000002
    Figure 0007565815000002
  • Figure 0007565815000003
    Figure 0007565815000003
  • Figure 0007565815000004
    Figure 0007565815000004
Patent Text Reader

Abstract

To manufacture grains with good filtration properties.SOLUTION: A manufacturing method for manufacturing grains by crystallization comprises a supply step, an agitation step, and an expansion ratio adjustment step for adjusting the expansion ratio of a foam layer to be greater than 100% and less than or equal to 112%, where the expansion ratio is defined by formula (1): expansion ratio [%]=(VS+VF) / VS where VS [m3] refers to the volume of the mixed solution and VF [m3] refers to the volume of the foam layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method and system for producing particles by crystallization. [Background technology]

[0002] In a process for producing particles by crystallization, foaming may occur due to the by-production of gas. Excessive foaming may cause a decrease in the yield of the product. Therefore, when foaming occurs, a means is used to defoam the foam. As a means for defoaming, chemical defoaming by adding a defoaming agent or adjusting the pH, thermal defoaming by adjusting the temperature, mechanical defoaming, etc. are known as prior art.

[0003] For example, Patent Document 1 discloses, as an example of mechanical foam destruction, a method in which generated foam is mechanically destroyed by a foam destruction impeller rotating above the liquid surface. Patent Document 2 discloses a configuration in which foam that is generated in a stirring tank and flows into a steam exhaust pipe is destroyed in a foam destruction tower. In Patent Document 2, foam that flows in from the bottom of the foam destruction tower is destroyed by dissolving in the liquid flowing down in the foam destruction tower. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2003-146937 A [Patent Document 2] JP 2003-146938 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, the above-mentioned conventional techniques may not be applicable to some systems due to the need to ensure product quality, the need for post-processing, the need to invest in additional equipment, and the like.

[0006] Furthermore, if there is a filtration step after crystallization, it is desirable to produce particles with good filterability.

[0007] One aspect of the present invention aims to produce particles with good filtration properties. [Means for solving the problem]

[0008] In order to solve the above problems, a production method according to one embodiment of the present invention is a production method for producing particles by crystallization in which a solid is precipitated by adding a second solution to a first solution, and includes a supplying step of dropping the second solution into a stirring tank in which the first solution is stored, a stirring step of stirring the mixed solution in the stirring tank, and an expansion ratio adjusting step of adjusting the expansion ratio of a foam layer formed on the liquid surface of the mixed solution to be greater than 100% and less than or equal to 112%.

[0009] Here, the expansion ratio is calculated by dividing the volume of the mixed solution by V S [m 3 ], the volume of the foam layer is V F [m 3 ], it is defined by the following equation (1).

[0010] Foaming ratio [%] = (V S +V F ) / V S (1) Further, a manufacturing system according to one aspect of the present invention is a manufacturing system for manufacturing particles by crystallization in which a solid is precipitated by adding a second solution to a first solution, the manufacturing system comprising an agitation tank and an expansion ratio adjustment device, the expansion ratio adjustment device being a device for adjusting the expansion ratio of a foam layer formed on a liquid surface of the mixed solution in the agitation tank during the crystallization in the agitation tank to be greater than 100% and less than or equal to 112%. Here, the expansion ratio is calculated by dividing the volume of the mixed solution by V S [m 3 ], the volume of the foam layer is V F [m 3 ], it is defined by the following equation (1).

[0011] Foaming ratio [%] = (V S +V F ) / V S (1) Effect of the Invention

[0012] According to one aspect of the present invention, particles having good filtration properties can be produced. [Brief description of the drawings]

[0013] [Figure 1] FIG. 1 is a system diagram illustrating a configuration of a system according to a first embodiment of the present invention. [Diagram 2] 1 is a block diagram showing a configuration of a system according to a first embodiment of the present invention. [Diagram 3] 1 is an example of a flow diagram showing an outline of a method for producing particles using the system according to the first embodiment. [Figure 4] FIG. 2 is an enlarged schematic view of the surface of a mixed solution in a reaction tank. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] [Embodiment 1] Hereinafter, a particle manufacturing method according to one embodiment of the present invention will be described in detail with reference to the drawings, together with a system used therein. The attached drawings are used to explain the present invention, and may differ from the actual dimensions. In this specification, "A to B" indicates A or more and B or less.

[0015] <Particle Manufacturing System (System 100)> The following describes a system 100 (manufacturing system) that manufactures particles of a substance containing carboxylic acid by adding a solution containing sulfuric acid (second solution A2) to an aqueous solution (first solution A1) of a substance containing an inorganic carboxylate.

[0016] Fig. 1 is a system diagram showing a schematic configuration of a system 100 according to the embodiment 1. Fig. 2 is a block diagram showing the configuration of the system 100 according to the embodiment 1.

[0017] As shown in FIG. 1 and FIG. 2, the system 100 of this embodiment includes a particle production device 1 and an expansion ratio adjustment device 10. The particle production device 1 is generally configured to include a stirring tank 20, a second solution supply device 11, a solvent supply device 12, a temperature control system 14, a foaming height measurement device 15, and each path. The expansion ratio adjustment device 10 includes a second solution supply management unit 102, a solvent supply management unit 103, a temperature management unit 104, a stirring power management unit 105, and an expansion ratio calculation unit 106. The expansion ratio adjustment device 10 is a device for adjusting the expansion ratio in the stirring tank 20. The expansion ratio will be described in detail later.

[0018] Fig. 3 is an example of a flow diagram showing an outline of a method for producing particles using the system 100 according to embodiment 1. As shown in Fig. 3, first, a solution A1 is stored in a stirring tank 20 (charging step: S1).

[0019] In the subsequent crystallization step S2, while stirring the mixed solution S in the stirring tank 20 (stirring step S21), the solution A2 is dropped into the stored solution A1 (supply step S22) to precipitate a substance containing carboxylic acid. The mixed solution S means a solution present in the stirring tank 20 in the crystallization step S2, and is a solution mainly containing the first solution A1. In addition, in the crystallization step S2, carbon dioxide gas may be generated as a side reaction along with the generation of carboxylic acid due to salt elimination of the carboxylic acid inorganic salt during crystallization. In the manufacturing method of the present embodiment, in the crystallization step S2, the expansion ratio of the foam layer F formed on the liquid surface by the gas generated by the reaction of the mixed solution S is adjusted to more than 100% to 112% or less (expansion ratio adjustment step S23). The expansion ratio and the expansion ratio adjustment step will be described later.

[0020] Thereafter, the slurry containing the solid (substance containing carboxylic acid) produced in the crystallization step S2 is filtered (filtration step: S3), and the wet cake (W / C) after filtration is dried (drying step: S4) to obtain crystals of the substance containing carboxylic acid as the product.

[0021] 1 and 2, the configuration for performing the filtering step S3 and the drying step S4 is omitted. The filtering step S3 and the drying step S4 may be performed using a known filtering device and a known drying device.

[0022] (Adjustment of foaming ratio) In the method for producing particles, when the filtration step S3 and the drying step S4 after the particles are generated by crystallization are taken into consideration, it is preferable to obtain crystal particles with good filtration characteristics. The filtration characteristics can be evaluated, for example, by the filtration resistivity or the liquid content. If the filtration resistivity increases, the cycle time of the filtration step S3 becomes longer. Also, if the liquid content increases, the time required for the drying step S4 becomes longer. Therefore, as the filtration characteristics, for example, the filtration resistivity is 5×10 9 m / kg or less. Also, the liquid content is preferably 26 wt% or less.

[0023] As a result of intensive research, the inventors have found that the filtration characteristics can be improved by adjusting the expansion ratio in the crystallization step S2. In the production method of the present invention, particles with good filtration characteristics can be obtained by adjusting the expansion ratio to more than 100% and not more than 112% (expansion ratio adjustment step).

[0024] The expansion ratio is the volume of the mixed solution S divided by V S [m 3 ], the volume of the foam layer F is V F [m 3 ], it is defined by the following equation (1).

[0025] Foaming ratio [%] = (V S +V F ) / V S (1) In order to obtain particles with good filtration properties, it is important that the second solution A2 is well dispersed in the first solution A1 when the second solution A2 is dropped in the crystallization step S2. If the second solution A2 is not dispersed in the first solution A1 and the concentration of the second solution A2 becomes locally high, fine particles may be generated as particles of the substance containing carboxylic acid. The fine particles are a factor that deteriorates the filtration properties.

[0026] The foam layer F is appropriately present on the liquid surface of the mixed solution S, and thus the interface area between the liquid phase and the gas phase is increased. This improves the dispersion efficiency of the second solution A2 when the second solution A2 is dropped. Therefore, it is preferable that the foaming ratio is greater than 100% (for example, 101%).

[0027] On the other hand, if the foam layer F is present in excess, the foam layer F prevents the second solution A2 from penetrating into the liquid phase (mixed solution S), which causes the concentration of the second solution A2 to be locally high. Therefore, the foaming ratio is preferably 112% or less.

[0028] In the crystallization step S2, when the supply rate of the second solution A2 is increased, the expansion ratio increases, and when the supply rate is decreased, the expansion ratio decreases. In addition, when the amount or addition rate of water (solvent for the first solution or the second solution) is increased, the expansion ratio decreases, and when the amount or addition rate is decreased, the expansion ratio increases. In addition, when the temperature of the mixed solution S is increased, the expansion ratio decreases, and when the temperature is decreased, the expansion ratio increases. In addition, when the stirring power in the stirring step S21 is increased, the expansion ratio increases, and when the stirring power is decreased, the expansion ratio decreases.

[0029] The expansion ratio calculation unit 106 of the expansion ratio adjusting device 10 acquires data on the height from a foam height measuring device 15 described later to the top end of the foam layer F, and calculates the expansion ratio. Based on the calculated expansion ratio, the expansion ratio adjusting device 10 can adjust the expansion ratio to be greater than 100% and less than or equal to 112% by adjusting one or more of the amount of water (solvent) added, the stirring power, the second solution supply speed, or the temperature of the mixed solution.

[0030] (Each component of the particle production system) Each component of the system 100 will be described in detail below.

[0031] The second solution supplying device 11 is a device that supplies the second solution A2 to the stirring tank 20. More specifically, the second solution supplying device 11 is connected to the stirring tank 20 and can supply the second solution A2 to the stirring tank 20 via a path L1 formed by a pipe extending into the stirring tank 20. The second solution A2 is dripped into the first solution A1 stored in the stirring tank 20, whereby a substance containing a carboxylic acid is precipitated.

[0032] The second solution supplying device 11 can be connected to the expansion ratio adjusting device 10. The second solution supply management unit 102 of the expansion ratio adjusting device 10 can control the second solution supplying device 11 and control the supply amount of the second solution A2.

[0033] The solvent supplying device 12 is a device that supplies the solvent W to the stirring tank 20. In this embodiment, the solvent W is water. More specifically, the solvent supplying device 12 is connected to the stirring tank 20 and can supply the solvent to the stirring tank 20 through a path L2 formed by a pipe extending into the stirring tank 20. The solvent supplying device 12 can be connected to the expansion ratio adjusting device 10. The solvent supply management unit 103 of the expansion ratio adjusting device 10 can control the solvent supplying device 12 and control the supply amount or supply speed of the solvent W.

[0034] The stirring tank 20 is a container for storing the first solution A1 and performing crystallization within the tank. That is, the stirring tank 20 may be any container having a stirrer. The second solution A2 is dripped into the stirring tank 20 through a path L1. An exhaust port is provided at the top of the stirring tank 20 for discharging gas generated within the stirring tank 20. The exhaust port is connected to a path L3 formed by piping. The gas is discharged to the outside of the system 1 through the path L3.

[0035] The stirring tank 20 is provided with an agitator 31 including an electric motor 13, an agitator blade 311, and an agitator shaft 310. The agitator blade 311 is rotated by rotating the agitator shaft 310 with the electric motor 13, and the mixed solution S in the stirring tank 20 can be agitated. The electric motor 13 can be connected to the expansion ratio adjusting device 10. The agitation power management unit 105 of the expansion ratio adjusting device 10 can control the electric motor 13 and control the agitation power of the agitator 31.

[0036] The temperature control system 14 is a system that controls the temperature of the mixed solution S in the stirring tank 20. The temperature control system 14 includes a thermometer 61 and a temperature adjustment system 62, and can be connected to the expansion ratio adjusting device 10. The temperature management unit 104 of the expansion ratio adjusting device 10 can control the temperature of the mixed solution S by receiving temperature data from the thermometer 61 and controlling the temperature adjustment system 62.

[0037] The thermometer 61 measures the temperature of the mixed solution S. The temperature control system 62 may be composed of a plurality of devices described later, and may be, for example, a device that keeps the temperature inside the stirring tank 20 constant. Alternatively, it may be a device that can supply heat to the stirring tank 20, or a device that cools the stirring tank 20.

[0038] The temperature adjustment system 62 may be configured to include, for example, a jacket 141 that covers at least a part of the outer surface of the stirring tank 20 and allows liquid to pass through, and a heat medium tank 140, as shown in FIG. 1. The jacket 141 is connected to the heat medium tank 140 by a path L4 and a path L5 formed by piping. The heat medium (e.g., hot water) in the heat medium tank 140 is supplied to the jacket 141 via the path L4 by a pump (not shown), circulates in the jacket 141, and returns to the heat medium tank 140 via the path L5. The temperature management unit 104 receives data on the temperature of the mixed solution S from the thermometer 61, and controls, for example, the flow rate of the pump so as to maintain the temperature of the mixed solution S at 28±3°C. The temperature adjustment system 62 is not limited to the above example. When cooling of the stirring tank 20 is required, the temperature adjustment system 62 may include a refrigerant tank (e.g., a cold water tank) instead of the heat medium tank 140. The temperature adjustment system 62 may also include a heat exchange plate or the like installed in the stirring tank 20.

[0039] The foam height measuring device 15 is a device for measuring the foam height in the mixing tank 20. For example, a sonic liquid level gauge or a monitoring camera installed on a sight glass attached to the mixing tank 20 can be used as the foam height measuring device 15. The foam height measuring device 15 measures the height (H F +H S 4) can be measured. The foaming height measuring device 15 can be connected to the foaming ratio adjusting device 10. The foaming ratio calculating section 106 of the foaming ratio adjusting device 10 can obtain data on the height from the foaming height measuring device 15 to the upper end of the foamed layer F and calculate the foaming ratio.

[0040] As described above, the expansion ratio is defined by the following formula (1).

[0041] Foaming ratio [%] = (V S +V F ) / V S (1) In the formula, V S [m 3 ] is the volume of the mixed solution S, and V F [m3 ] is the volume of the foam layer F.

[0042] FIG. 4 is an enlarged schematic diagram of the surface of the mixed solution S in the stirring tank 20. F [m] is the height of the foam layer F, and the height H S indicates the liquid height of the mixed solution S.

[0043] The height from the bottom surface of the mixing tank 20 to the top end of the foam layer F (H F +H S ) can be measured by the foaming height measuring device 15. Alternatively, it may be measured visually using a sight glass and a liquid level scale provided in the stirring tank 20. The upper end of the foamed layer F is the highest point of the foamed layer F. When measured visually, data on the height to the upper end of the foamed layer F may be input from an input unit (not shown) of the foaming ratio adjusting device 10. The foaming ratio calculating unit 106 can obtain data on the height to the upper end of the foamed layer F input from the foaming height measuring device 15 or the input unit of the foaming ratio adjusting device 10 and calculate the foaming ratio. Specifically, the foaming ratio calculating unit 106 calculates the foaming ratio as follows.

[0044] (i) Height from the bottom to the top of the foam layer F (H F +H S ) based on V S +V F [m 3 (ii) Calculate the V in the denominator of the above formula (1). S The theoretical amount of the first solution A1 charged in the stirring tank 20 [m 3 ] to calculate the expansion ratio. F and V S +V F is calculated based on the height to the top of the foam layer F, so V F and V S +V F At least a portion of the space may be free of foam.

[0045] When the stirring tank 20 has a cylindrical shape with the same inner diameter from the top to the bottom, the expansion ratio calculation unit 106 may calculate the expansion ratio as follows.

[0046] (i) The amount of the first solution A1 charged in the stirring tank 20 and the bottom area [m 2 ], height H S (ii) Calculate the height to the top of the foam layer F (H F +H S ) and calculate the liquid height H S By subtracting F (iii) Calculate the foam height H F , liquid height H S and the bottom area of ​​the mixing vessel 20, the volume V of the mixed solution S S and the volume V of the foam layer F F (iv) Using the above formula (1) and the calculated volume V of the mixed solution S S and the volume V of the foam layer F F The expansion ratio is calculated from the above.

[0047] (Demonstration test) The following describes the results of a demonstration test conducted to examine the relationship between the expansion ratio and the filtration characteristics.

[0048] Table 1 shows a summary of the experimental conditions and results of Examples 1 and 2 and Comparative Examples 1 to 4.

[0049] [Table 1] First, Example 1 will be described. In Example 1, a glass separable flask with a capacity of 1 L and an inner diameter of the tank of 114 mm was used. 0.74 kg (0.66 L) of an aqueous solution of a substance containing an inorganic carboxylate was charged into the separable flask. The aqueous solution contained 0.032 kg of an inorganic carboxylate and 0.67 kg of water, and the weight ratio of water to the inorganic carboxylate was 21 WR. 0.13 kg of water was added to the aqueous solution, and the weight ratio was set to 25 WR. In other words, the water weight ratio was adjusted by adjusting the amount of water added. Crystallization was performed by supplying 40 wt% sulfuric acid at a constant rate until the pH reached a range of 4.0 ± 0.3 while stirring the liquid phase by rotating the three-blade swept-back impeller. Cooling water was fed into the jacket of the separable flask, and the internal temperature of the flask was adjusted to 28 ± 3 ° C. This experiment was performed under normal pressure. The stirring power during crystallization was 0.5 kW / m 3 and the gas superficial velocity was 4.2 cm / h.

[0050] (Measurement of foaming ratio) The height from the bottom of the flask to the top of the foam layer, which was generated by carbon dioxide during the supply of sulfuric acid, was measured visually when the foam layer reached its highest point. Based on the measured height, the expansion ratio was calculated as described above. The calculation results are shown in Table 1.

[0051] (Measurement of filtration resistance and liquid content) Crystallization was stopped when the pH reached 4.0±0.3, and the resulting mixture (slurry) of reaction crystallization material and water was placed upstream of a 30 mm inner diameter pressure filter equipped with quantitative filter paper (ADVANTEC, No. 5C). The upstream pressure was adjusted to 100 kPaG with nitrogen, and pressure was continued until the nitrogen was confirmed to blow through the quantitative filter paper. The weight of the filtrate that passed through the quantitative filter paper was measured over time, and the wet cake (W / C) remaining on the quantitative filter paper after the nitrogen had blown through was collected and weighed. The filtration resistance calculated based on the Ruth formula is shown in Table 1.

[0052] The collected W / C was dried at 50°C for 24 hours using a vacuum dryer, and the weight after drying was measured. The weight loss due to drying was divided by the weight of the W / C measured after filtration to calculate the W / C liquid content. The results are shown in Table 1.

[0053] (Other examples) For Example 2 and Comparative Example 1, the same experiment as in Example 1 was carried out except that the water weight ratio, stirring power, and gas superficial velocity were set as shown in Table 1.

[0054] In Comparative Example 2 and Comparative Example 3, the inner diameter of the tank was 2500 mm and the capacity was 15 m 3 A glass-lined reactor of the above-mentioned was used. 9270 kg (8250 L) of an aqueous solution of a substance containing an inorganic carboxylate was charged into the glass-lined reactor. The experiment was conducted in the same manner as in Example 1, except that the water weight ratio, stirring power, and gas superficial velocity were set to the conditions shown in Table 1.

[0055] For Comparative Example 4, a glass separable flask stirring vessel with a volume of 2 L and an inner diameter of 143 mm was used. 1.47 kg (1.31 L) of an aqueous solution of a substance containing an inorganic carboxylate was charged into the separable flask stirring vessel. The experiment was conducted in the same manner as in Example 1, except that the water weight ratio, stirring power, and gas superficial velocity were set to the conditions shown in Table 1.

[0056] In Table 1, comparing Example 1, Example 2 and Comparative Example 4, it can be seen that the higher the stirring power, the higher the expansion ratio. Also, comparing Example 1 and Comparative Example 1, it can be seen that the lower the water weight ratio (the smaller the amount of water added), the higher the expansion ratio. Furthermore, comparing Comparative Example 1 and Comparative Example 2, it can be seen that the higher the gas superficial velocity, the higher the expansion ratio. Note that since the gas superficial velocity is proportional to the supply rate of sulfuric acid, it can also be said that the higher the supply rate of sulfuric acid, the higher the expansion ratio.

[0057] As a result of the above-mentioned experiments, the expansion ratios of Examples 1 and 2 were greater than 100% and equal to or less than 112%, which were within the range of the present invention, whereas Comparative Examples 1 to 4 were outside the range of the present invention.

[0058] Filtration resistivity is 5 x 10 9 m / kg or less is good (〇) 5×10 9 When the W / C liquid content was greater than 26wt%, it was evaluated as good (◯), and when it was greater than 26wt%, it was evaluated as bad (×).

[0059] In Examples 1 and 2, good results were obtained for the filtration resistivity and W / C liquid content. On the other hand, the evaluations for the filtration resistivity and W / C liquid content were all poor for Comparative Examples 1 to 4. In other words, it was demonstrated that particles with good filtration properties can be obtained by adjusting the expansion ratio within the range of the present invention.

[0060] In the first embodiment, a system for producing particles of a substance containing carboxylic acid by crystallization between an aqueous solution of a substance containing an inorganic carboxylate and a solution containing sulfuric acid has been described. However, the method and system for producing particles of the present invention can also be applied to other examples of producing particles by crystallization accompanied by foaming. Depending on the reaction system, it is also possible to control the foaming ratio by controlling the reaction temperature.

[0061] The present invention is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present invention. [Explanation of symbols]

[0062] 100 System (Manufacturing System) 1 Particle production equipment 10. Foaming ratio adjustment device 20 Stirring tank

Claims

1. 1. A method for producing particles by crystallization in which a solid is precipitated by adding a second solution to a first solution, comprising the steps of: A supplying step of dropping the second solution into a stirring tank storing the first solution; A stirring step of stirring the mixed solution in the stirring tank; and A method for producing the foamed layer formed on the liquid surface of the mixed solution, comprising: adjusting the foaming ratio of the foamed layer to be greater than 100% and less than 112%; Here, the expansion ratio is calculated by dividing the volume of the mixed solution by V S [m 3 ], the volume of the foam layer is V F [m 3 ], it is defined by the following formula (1). Foaming ratio [%] = (V S +V F ) / V S ...(1)

2. The manufacturing method according to claim 1 , wherein the first solution is a solution containing a substance having an acidic dissociable group, and the second solution is a solution containing an acid.

3. The method according to claim 1 or 2, wherein the first solution is an aqueous solution of a substance containing an inorganic carboxylate.

4. The filtration resistance of the particles precipitated by the crystallization is 5×10 9 The method according to any one of claims 1 to 3, wherein the viscosity is 100 MPa or less.

5. 5. The method according to claim 1, wherein the expansion ratio is adjusted by adjusting one or more of the amount of the solvent added in the supply step, the stirring power in the stirring step, the second solution supply rate in the supply step, or the temperature of the mixed solution in the stirring tank.

6. A production system for producing particles by crystallization in which a solid is precipitated by adding a second solution to a first solution, comprising: The apparatus is provided with a mixing tank and a foaming ratio adjusting device, The expansion ratio adjusting device is a device for adjusting the expansion ratio of a foam layer formed on the liquid surface of the mixed solution in the stirring tank during the crystallization in the stirring tank to be greater than 100% and less than 112%. Here, the expansion ratio is calculated by dividing the volume of the mixed solution by V S [m 3 ], the volume of the foam layer is V F [m 3 ], it is defined by the following formula (1). Foaming ratio [%] = (V S +V F ) / V S ...(1)

Citation Information

Patent Citations

  • JP1971019610B1

  • JP1974020119A

  • Crystallization reaction apparatus

    JP1976136572A

  • Treatment of ammonium adipate waste solution

    JP1999077065A

  • Method for crystallizing terephthalic acid

    JP2003146937A