How to operate a crystallization facility

By controlling the pressure within the crystallization vessel to suppress carryover, the method effectively reduces component loss and maintains product quality in crystallization processes, addressing inefficiencies and cost issues in existing technologies.

JP7567190B2Active Publication Date: 2024-10-16SUMITOMO METAL MINING CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020057297
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-03-27
Publication Date
2024-10-16
Estimated Expiration
2040-03-27

AI Technical Summary

Technical Problem

Existing methods to prevent carryover of solute components in crystallization processes incur high equipment and material costs, and existing solutions are inefficient in reducing component loss and maintaining product quality.

Method used

Adjusting the pressure inside the crystallization vessel to a range narrower than the crystallization temperature range, maintaining a higher pressure than the saturated vapor pressure of the stock solution, effectively suppresses carryover without additional equipment or material costs.

Benefits of technology

Significantly reduces component loss due to carryover, maintains product quality by stabilizing the crystallization process, and enhances production efficiency by minimizing equipment degradation and operational costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007567190000002
    Figure 0007567190000002
  • Figure 0007567190000003
    Figure 0007567190000003
  • Figure 0007567190000001
    Figure 0007567190000001
Patent Text Reader

Abstract

To provide an operating method for crystallization equipment, which inhibits the production of carry-over including a solute component, without the need for a special equipment cost and a material cost.SOLUTION: In an operating method for crystallization equipment, a solvent of an undiluted solution introduced into a crystallizer kept in a decompressed atmosphere is evaporated at a prescribe temperature and under prescribed pressure so as to crystallize a crystallization object component included in the undiluted solution. The pressure within the crystallizer is controlled so that prescribed pressure can be higher than saturation vapor pressure of the undiluted solution at the prescribe temperature.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for operating a crystallization facility, and more particularly to a method for operating a crystallization facility capable of reducing loss of a component to be crystallized by suppressing carryover from the upper part of a crystallizer. [Background technology]

[0002] In various fields such as inorganic chemical industry, pharmaceutical industry, and sugar refining industry that handle crystalline substances, a crystallization operation is performed in which a specific component dissolved in a liquid phase is crystallized and separated as a solid. In this crystallization operation, a stock solution containing the component to be crystallized is generally introduced into a crystallizer, and the stock solution is heated to evaporate the solvent, making the solution in the crystallizer supersaturated, thereby crystallizing a part of the solute and extracting the crystals in the form of a concentrated slurry from the bottom of the crystallizer. This concentrated slurry can be further subjected to solid-liquid separation, drying, sieving, etc. in subsequent processes to produce crystals as a product.

[0003] In the crystallization operation using the above-mentioned crystallizer, the vapor of the solvent evaporated by the heating is generated from the liquid surface inside the crystallizer, and the vapor is withdrawn from the withdrawal line at the top of the crystallizer connected to a vacuum pump. The vapor withdrawn from the top of the crystallizer is introduced into a heat exchanger (cooler) that exchanges heat with cooling water, where it is condensed and then removed as condensed water.

[0004] In the above-mentioned crystallizer, a phenomenon (also called carryover) may occur in which the solution in the crystallizer containing the solute components is carried away from the top of the crystallizer to the outside along with the vapor of the solvent generated from the liquid surface. This phenomenon occurs when a mist of the solution containing the solute components is generated when the solvent evaporates, and this mist is caught in the vapor moved by the vacuum pump. This mist is usually removed together with the condensed water extracted from the outlet side of the heat exchanger (cooler). When carryover occurs in this way, the solute components that should have been crystallized as crystals are lost, resulting in a problem of reduced productivity. In addition, if the carried-over solute contains heavy metals, there is a risk that additional processing costs such as detoxification treatment will be incurred as environmental measures.

[0005] The above carryover is believed to be caused by the entrainment of droplets, which occurs when steam bubbles burst near the liquid surface due to the intense boiling of the solution in the crystallizer, causing the mist generated by this to be blown up by the steam rising from the liquid surface and scattered together with the liquid. Therefore, a possible countermeasure is to reduce the amount of steam supplied to the heat exchanger (heater) that heats the solution in the crystallizer, thereby suppressing excessive evaporation of the solution.

[0006] However, this method causes another problem of lowering productivity because the concentration rate of the raw liquid is reduced. Therefore, as a method for suppressing the problems caused by carryover without reducing the amount of steam supplied to the heater, it is possible to slow down the rising speed of the steam generated from the liquid phase by increasing the height of the gas phase space in the upper part of the crystallizer or by increasing the inner diameter of the gas phase space in the upper part of the crystallizer.

[0007] Furthermore, as disclosed in Patent Document 1, it is possible to collect mist by installing a droplet collector (demister, cyclone, mist catcher, etc.) at the steam outlet at the top of the crystallizer. Also, Patent Document 2 discloses a technology for collecting mist generated in a regenerative burner system, which is a device for supplying combustion air into a furnace, by using a porous adsorbent, and it is possible to apply this technology to the crystallizer. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] Special Publication No. 2009-529911 [Patent Document 2] JP 2000-055351 A Summary of the Invention [Problem to be solved by the invention]

[0009] As described above, the measures of increasing the size of the gas phase space at the top of the crystallizer or installing a splash collector are thought to be able to prevent the problem of mist being discharged outside the crystallizer, but they require increasing the size of the equipment or new equipment for splash collection, which increases the equipment cost. In addition, the technology using a porous adsorbent described in Patent Document 2 adsorbs and collects mist containing crystal precipitation type mist (calcium phosphate) and the like using a porous adsorbent provided in the path, so it is necessary to replace the adsorbent after mist adsorption. Therefore, a new adsorbent is required each time it is replaced, which increases the material cost for operation.

[0010] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a method for operating a crystallization facility that suppresses the occurrence of carry-over containing solute components without requiring special equipment or material costs. [Means for solving the problem]

[0011] As a result of intensive research conducted by the present inventors in order to achieve the above object, it was found that the occurrence of carryover containing solute components in the crystallizer can be effectively suppressed by appropriately adjusting the pressure in the crystallizer, and thus the present invention was completed. Using a vacuum pump The solvent in the stock solution introduced into the crystallizer, which is maintained under a reduced pressure, is evaporated at a specified temperature and pressure. and discharging steam from the top of the crystallizer.The method for operating a crystallization facility causes a component to be crystallized contained in the raw solution to crystallize by controlling the pressure in the crystallizer so that the predetermined pressure is higher than the saturated vapor pressure of the raw solution at the predetermined temperature, which is set within a narrower range than the crystallization temperature range for crystallizing a desired crystal form. Effect of the Invention

[0012] According to the present invention, it is possible to suppress the occurrence of carry-over in a crystallizer without requiring special equipment costs or material costs. [Brief description of the drawings]

[0013] [Figure 1] FIG. 1 is a schematic front view of a crystallization facility to which a method for operating a crystallization facility according to an embodiment of the present invention is preferably applied. [Diagram 2] 1 is a graph showing the crystallization temperature ranges of each crystal form of nickel sulfate, and the saturated vapor pressure curve of an aqueous nickel sulfate solution used as a stock solution in a method for operating a crystallization system according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] Hereinafter, the method for operating the crystallization equipment according to the embodiment of the present invention will be described with reference to the drawings. The method for operating the crystallization equipment according to the embodiment of the present invention is a method for efficiently crystallizing a component to be crystallized as a product contained in the raw solution while suppressing carryover by evaporating a solvent of the raw solution introduced into a crystallizer maintained in a reduced pressure atmosphere under a predetermined temperature and pressure condition.

[0015] The stock solution containing the component to be crystallized may be an aqueous solution or an organic solvent solution. Examples of the component to be crystallized include nickel sulfate, ammonium sulfate, sodium carbonate, caprolactam, and trehalose. Hereinafter, the method of operating the crystallization equipment according to the embodiment of the present invention will be described using an example in which the component to be crystallized is nickel sulfate.

[0016] A crystallization facility to which the operating method of the embodiment of the present invention is suitably applied is composed of at least a crystallizer that crystallizes nickel sulfate, a component to be crystallized, by evaporating and concentrating an aqueous nickel sulfate solution introduced as a raw solution under predetermined temperature and pressure conditions, a heat exchanger (heater) for maintaining a slurry consisting of the crystals and solution produced in the crystallizer at a predetermined temperature, a vacuum pump for maintaining a predetermined reduced pressure atmosphere inside the crystallizer, and a heat exchanger (cooler) for condensing steam discharged by the vacuum pump from the top of the crystallizer.

[0017] Specifically, a DTB (Draft Tube Baffle) type continuous crystallizer as shown in Fig. 1 is preferably used as the crystallizer. A draft tube 11 is provided inside this crystallizer 10, and a slurry phase consisting of an aqueous nickel sulfate solution and nickel sulfate crystals is circulated as shown by the arrows by an agitator blade 12 provided inside the draft tube 11. Since evaporation of water occurs mainly near the upper surface of the slurry phase, the aqueous solution near the upper surface of the slurry phase is concentrated and the degree of supersaturation increases.

[0018] The aqueous solution with a high degree of supersaturation is circulated in the crystallizer 10 by the stirring blades 12 while decreasing in concentration due to the formation and growth of crystals, and returns to the upper surface of the slurry phase again. In this way, crystallization proceeds almost uniformly in the crystallizer. When the crystals circulate with the aqueous solution circulating in the crystallizer 10 in the above-mentioned manner grow to a certain size, they leave the circulating flow and settle to the bottom of the crystallizer 10, and are extracted in the form of a concentrated slurry from the classifier 13 installed at the bottom. The crystals in the form of a concentrated slurry are turned into a crystal product through a solid-liquid separator, a dryer, a sieve, etc.

[0019] The slurry phase in the crystallizer 10 loses heat due to the heat of vaporization when the water evaporates, so that the temperature of the slurry does not drop due to this, the slurry phase is supplied to the heat exchanger (heater) 15 via the settling section 14 in the crystallizer 10. This keeps the temperature of the slurry in the crystallizer at, for example, 32 to 53°C. In the settling section 14, an aqueous solution containing fine crystals is separated, and the fine crystals are dissolved by introducing this separated aqueous solution into the heater. This allows the production of crystals with a uniform particle size. There is no particular limitation on the type of the heat exchanger (heater) 15, and for example, a shell-and-tube type heat exchanger can be suitably used, and for example, steam can be used as the heat medium.

[0020] The inside of the crystallizer 10 is controlled to a reduced pressure atmosphere of, for example, about 8 kPaA by a vacuum pump 16 and a control valve 17 provided on the suction side thereof. The pressure control of the crystallizer 10 is not limited to that by the control valve 17, and may be controlled, for example, by the rotation speed of the drive motor of the vacuum pump 16. Since the solvent vapor generated in the crystallizer 10 is extracted by the vacuum pump 16, a heat exchanger (cooler) 18 for condensing the vapor is provided on the suction side of the vacuum pump 16. The condensed water generated by the condensation by the cooler 18 is extracted from the outlet side of the cooler 18. There is no particular limitation on the type of the heat exchanger (cooler) 18, and for example, a shell-and-tube type heat exchanger can be suitably used, and cooling water can be used as the refrigerant.

[0021] Incidentally, the aqueous nickel sulfate solution (crystallization mother liquor) introduced as a stock solution into the crystallizer 10 has a saturated vapor pressure curve as shown by the group of dots in Fig. 2. The solid line in Fig. 2 indicates the saturated vapor pressure curve of water, and the saturated vapor pressure curve (group of dots) of the stock solution in which nickel sulfate as a solute is dissolved in water as a solvent is plotted at a position shifted in parallel by about 3°C ​​to the right from the saturated vapor pressure curve of water due to an increase in the molar boiling point.

[0022] The graph in Fig. 2 further shows that the crystal form produced differs depending on the crystallization temperature. That is, when the crystallization temperature is in the range of 31.2°C or less, nickel sulfate heptahydrate crystallizes out, when the crystallization temperature is in the range of 31.2 to 53.3°C, α-type nickel sulfate hexahydrate crystallizes out, and when the crystallization temperature is 53.3°C or more, β-type nickel sulfate hexahydrate crystallizes out. This shows that, as described above, by maintaining the slurry temperature in the crystallizer 10 at 32 to 53°C, it is possible to stably crystallize α-type nickel sulfate hexahydrate, which is the desired crystal form.

[0023] The saturated vapor pressures of the above-mentioned raw solution at the lower limit temperature (i.e., 31.2°C) and the upper limit temperature (i.e., 53.3°C) for stable crystallization of the above-mentioned α-type nickel sulfate hexahydrate are respectively defined as the lower limit pressure P A and upper limit pressure P B In the case of the stock solution shown in Figure 2, P A =3.8kPaA, P B However, if the pressure inside the crystallizer 10 is controlled to 3.8 to 12.5 kPaA while maintaining the slurry temperature inside the crystallizer 10 at 32 to 53° C., the pressure may exceed the above upper or lower limits due to factors such as disturbances, which may cause bumping or crystallization of a crystal form other than α-nickel sulfate hexahydrate.

[0024] Therefore, the internal pressure of the crystallizer 10 is set to the lower limit pressure P A and upper limit pressure P B Approximate median (i.e. arithmetic mean) of P C The set value is controlled to 8kPaA, and the median value P CBy setting the upper limit of the slurry temperature at about 48°C, which is the temperature of the raw solution when 8 kPaA, which is the saturated vapor pressure, it is possible to suppress the crystallization of crystal forms other than α-type nickel sulfate hexahydrate even if the temperature and pressure inside the crystallizer 10 fluctuate slightly, while making it difficult for bumping of the slurry inside the crystallizer 10 to occur. Note that when increasing production, the evaporation rate of the raw solution introduced into the crystallizer 10 can be increased, and the amount of steam supplied to the heat exchanger (heater) 15 (unit: t / h) can be increased so that the above-mentioned slurry temperature approaches the above-mentioned upper limit of 48°C.

[0025] However, even if the amount of steam supplied to the heater 15 is adjusted so that the slurry temperature in the crystallizer 10 falls within the upper limit as described above, in reality, the amount of steam supplied to the heater 15 may fluctuate due to disturbances in the control system, or the concentration of the slurry circulating in the crystallizer 10 may vary, causing the molar boiling point rise of the aqueous solution in the crystallizer 10 to fluctuate, and the dots in FIG. 2 may swing left and right. As a result, unexpected boiling occurs in the slurry in the crystallizer 10, and a mist of the solution is generated on the upper surface of the slurry phase and discharged to the outside of the crystallizer 10 together with the steam, which may cause a problem of loss of nickel sulfate, which is a component to be crystallized, contained in the mist. Furthermore, since the mist discharged as a carryover to the outside of the crystallizer 10 as described above is made of a supersaturated aqueous solution, it is easily crystallized in the heat exchanger (cooler) 18, and as a result, it may adhere to the heat transfer surface of the heat exchanger 18 as scale, which may cause a problem of a decrease in the heat transfer performance of the heat exchanger (cooler) 18.

[0026] Therefore, in the operating method according to the embodiment of the present invention, the set pressure inside the crystallizer 10 is changed from 8 kPaA to the upper limit pressure P B Specifically, the median value P C and upper limit pressure P B The pressure obtained by the following formula 1, which is the median value of D It is preferable to set the above. [Formula 1] Set pressure P D =(P C +P B ) / 2={(P A +P B) / 2+P B} / 2

[0027] In the above formula 1, the above-mentioned P A =3.8kPaA, P B = 12.5kPaA, the set pressure P D That is, in the crystallizer 10, the lower limit pressure P A and upper limit pressure P B Median of P C Set the pressure P to about 10 kPaA, which is 2 kPa higher than 8 kPaA. D As a result, in the case of the undiluted solution shown in FIG. 2, the temperature range of the corresponding saturated vapor pressure curve is expanded from the above-mentioned 31.2 to 48°C to 31.2 to 50°C.

[0028] As a result, even if steam is supplied to heater 15 to heat the slurry in the vessel to about 48°C in an attempt to increase the above-mentioned production volume, there is a 2°C margin to the boiling point, so the frequency of boiling or bumping due to disturbances such as fluctuations in the composition of the raw liquid or fluctuations in the control system is significantly reduced. This makes it possible to effectively suppress the generation of mist, and significantly reduces the loss of the components to be crystallized due to carryover. Furthermore, even if there is a request for further production increase in the future and steam is supplied to heater 15 to raise the slurry temperature to, for example, 49°C, this can be accommodated because there is a 1°C margin to the boiling point of the aqueous solution in the vessel.

[0029] If the set pressure of the crystallizer 10 exceeds 10 kPaA, the temperature of the saturated vapor curve of the corresponding raw solution exceeds 50° C., which makes it easier for crystal forms other than α-nickel sulfate hexahydrate to be crystallized, and the amount of crystals precipitated becomes too large, promoting scaling on the inner wall of the crystallizer 10 and the heat transfer surface of the cooler 18, which is not preferable. Furthermore, the temperature of the steam discharged from the upper part of the crystallizer 10 increases, which is also not preferable in that the consumption of cooling water for condensation increases.

[0030] As described above, the method of operating the crystallization equipment according to the embodiment of the present invention can suppress carryover from the top of the crystallizer without requiring any particular equipment or material costs. As a result, the solute, which is the component to be crystallized, can be suppressed from being carried away with the condensed water derived from the steam extracted from the top of the crystallizer, so that the loss of the component to be crystallized as the crystal product can be reduced and productivity can be increased. In addition, the rate at which β-type nickel sulfate hexahydrate and nickel sulfate heptahydrate are crystallized can be reduced, so that high-quality crystals consisting essentially of a single crystal form of α-type nickel sulfate hexahydrate can be produced as the product, so that the value of the product can be increased. Thus, the present invention has extremely high industrial value. EXAMPLES

[0031] A nickel sulfate aqueous solution having a saturated vapor pressure curve shown by the dots in Figure 2 was introduced as a stock solution into the crystallization equipment shown in Figure 1, and crystallization was carried out while controlling the pressure inside the vessel at various levels. The results are shown in Table 1 below.

[0032] [Table 1]

[0033] As can be seen from Table 1 above, in Runs 1 to 4 of the embodiment in which the crystallizer was operated with the pressure set in the vessel at 0.9 kPa or more higher than 8.15 kPaA, which is the median of the lower limit pressure of 3.8 kPa and the upper limit pressure of 12.5 kPaA, which are the saturated vapor pressures of the raw solution corresponding to the lower limit temperature of 31.2°C and the upper limit temperature of 53.3°C, respectively, at which α-type nickel sulfate hexahydrate crystallizes, the concentration of nickel sulfate in the condensed water was 0.03 g / L or less.

[0034] In contrast, in Runs 5 to 7 of the comparative examples in which the crystallizer was operated with the pressure set in the crystallizer near 8.15 kPaA, which is the above-mentioned median value, the concentration of nickel sulfate in the condensed water was 0.06 to 0.09 g / L, and the nickel sulfate loss was about 2 to 3 times that of the above-mentioned Examples. In Runs 1 to 3 and 5 to 7, when the inside of the cooler was visually inspected after the operation was stopped, no particular scale was formed on the heat transfer surface, but in Run 4, scale was formed on the heat transfer surface of the cooler. This is thought to be because in Run 4, the set pressure in the cooler was operated at more than 10 kPaA, so the amount of steam supplied to the heater increased by about 15 to 20% compared to Runs 1 to 3, and the concentration of the aqueous solution in the cooler became excessively high. [Explanation of symbols]

[0035] 10 Crystallizer 11 Draft Tube 12 Mixing blade 13 Classified leg 14 Set ring section 15 Heat exchanger (heater) 16 Vacuum Pump 17 Control valve 18 Heat exchanger (cooler)

Claims

1. A method for operating a crystallization system, which crystallizes a component to be crystallized contained in an original liquid by evaporating the solvent of the original liquid introduced into a crystallizer maintained at a reduced pressure using a vacuum pump at a predetermined temperature and pressure and discharging the vapor from the top of the crystallizer, characterized in that the pressure inside the crystallizer is controlled so that the predetermined pressure is higher than the saturated vapor pressure of the original liquid at the predetermined temperature, which is set within a narrower range than the crystallization temperature range for crystallizing a desired crystal form.

2. 2. The method for operating a crystallization system according to claim 1, characterized in that the system comprises a crystallizer for evaporating the solvent of the raw solution to crystallize a solute, a heater for maintaining the solution in the crystallizer at the predetermined temperature, a vacuum pump for maintaining the interior of the crystallizer at the predetermined pressure, and a cooler for condensing vapor consisting of the evaporated solvent discharged by the vacuum pump.

3. The saturated vapor pressure of the raw solution at the lower and upper limit temperatures for stably crystallizing the crystal of the desired crystal form is P A and P B Then, these P A and P B 3. The method for operating a crystallization facility according to claim 1 or 2, wherein the temperature of the raw solution when the median value of the above-mentioned is the saturated vapor pressure is set as the upper limit of the predetermined temperature, and the lower limit temperature is set as the lower limit of the predetermined temperature.

4. The P A and P B The median of P C When the predetermined pressure is P C and P B The method for operating a crystallization facility according to claim 3, wherein the median value of

5. The method for operating a crystallization facility according to any one of claims 1 to 4, wherein the component to be crystallized is nickel sulfate.

6. 6. The method for operating a crystallization facility according to claim 5, wherein the desired crystal form is α-nickel sulfate hexahydrate.

7. 7. The method for operating a crystallization facility according to claim 6, wherein the predetermined pressure is 2 kPa higher than the saturated vapor pressure of the raw solution.

8. 8. The method for operating a crystallization facility according to claim 6 or 7, wherein the upper limit of the predetermined pressure is 10 kPaA.

9. A method for operating a crystallization facility as described in claim 8, characterized in that the lower limit of the specified pressure is 9.05 kPaA.

10. A method for operating a crystallization facility as described in claim 9, characterized in that the specified temperature is 31.2°C or higher and 48°C or lower.

Citation Information

Patent Citations

  • Apparatus for pulling out slurry

    JP1998287889A

  • Thermal storage type burner system

    JP2000055351A

  • Improved vertical continuous vacuum pot

    JP2009529911A

  • Crystallization equipment and crystallization method

    JP2019156654A

  • Method for producing vanadium dioxide-containing particles, vanadium dioxide-containing particles and optical film