Three-dimensional modeling device

The three-dimensional printing device addresses the issue of powder scattering by using controlled laser beam irradiation and a specific energy density to stabilize model thickness, improving precision and uniformity.

JP7567372B2Active Publication Date: 2024-10-16SEIKO EPSON CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2020182320
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-30
Publication Date
2024-10-16
Estimated Expiration
2040-10-30

AI Technical Summary

Technical Problem

When a material containing metal powder and an adhesion promoter is irradiated with laser light, the adhesion promoter with a low boiling point vaporizes first, causing the metal powder to scatter, leading to variations in the thickness of the three-dimensional model and reducing precision.

Method used

A three-dimensional printing device with a material supply means for inorganic powder and binder, controlled by a unit that applies a specific energy density of 140 J/mm² laser beam irradiation, along with a laser beam of a square top hat shape, to stabilize the thickness and suppress powder scattering.

Benefits of technology

The device achieves increased residual film ratio, suppresses powder scattering, and maintains uniform thickness, enhancing the precision of the three-dimensional model.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007567372000001
    Figure 0007567372000001
  • Figure 0007567372000002
    Figure 0007567372000002
  • Figure 0007567372000003
    Figure 0007567372000003
Patent Text Reader

Abstract

To provide a three-dimensional molding apparatus which can suppress scattering of inorganic powder.SOLUTION: A three-dimensional molding apparatus includes a stage, material supply means for supplying a material containing inorganic powder and a binder, a laser, and a control part, in which the control part performs processing of controlling the material supply means and supplying the material onto the stage, and processing of controlling the laser, and irradiating the material on the stage with a laser beam with energy density of 140 J / mm3 or more.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a three-dimensional modeling apparatus. [Background technology]

[0002] 2. Description of the Related Art Three-dimensional printing apparatuses for printing three-dimensional objects are known.

[0003] For example, Patent Document 1 describes a method for producing a three-dimensional object by supplying a material containing a metal powder, a solvent, and an adhesion promoter to a modeling plate and irradiating the plate with laser light. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2008-184622 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, when a material containing a metal powder and an adhesion promoter is irradiated with a laser beam as described above, the adhesion promoter, which has a low boiling point, may vaporize before the metal powder is melted or sintered by the laser beam, causing the metal powder to scatter. If the metal powder scatters, the thickness of the three-dimensional object may vary, resulting in a decrease in the modeling accuracy. [Means for solving the problem]

[0006] One aspect of the three-dimensional printing apparatus according to the present invention is to Stage and A material supplying means for supplying a material including an inorganic powder and a binder; Means of transportation; Lasers and A control unit; Including, The control unit is A process of controlling the material supplying means to supply the material onto the stage; The laser is controlled to apply an energy density of 140 J / mm to the material on the stage. 3 The above-mentioned laser light irradiation process is carried out. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a cross-sectional view illustrating a three-dimensional modeling apparatus according to an embodiment of the present invention. [Diagram 2] 5 is a flowchart for explaining a process of a control unit of the three-dimensional printing apparatus according to the embodiment. [Diagram 3] 1A to 1C are cross-sectional views each showing a schematic diagram of a manufacturing process of a three-dimensional object manufactured by the three-dimensional printing apparatus according to the embodiment. [Figure 4] 1A to 1C are cross-sectional views each showing a schematic diagram of a manufacturing process of a three-dimensional object manufactured by the three-dimensional printing apparatus according to the embodiment. [Diagram 5] A table showing the relationship between the energy density of the laser light and the residual film rate and surface roughness Sz of the modeling layer. [Figure 6] 13 is a graph showing the relationship between the energy density of the laser light and the remaining film rate of the modeling layer. [Figure 7] Graph showing the relationship between the energy density of the laser light and the surface roughness Sz of the modeling layer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Preferred embodiments of the present invention will be described in detail below with reference to the drawings. Note that the embodiments described below do not unduly limit the contents of the present invention described in the claims. In addition, not all of the configurations described below are necessarily essential components of the present invention.

[0009] 1. Three-dimensional printing equipment 1.1. Overall structure First, a three-dimensional modeling apparatus according to this embodiment will be described with reference to the drawings. Fig. 1 is a cross-sectional view that shows a three-dimensional modeling apparatus 100 according to this embodiment. In Fig. 1, an X-axis, a Y-axis, and a Z-axis are shown as three mutually orthogonal axes. The X-axis direction and the Y-axis direction are, for example, horizontal directions. The Z-axis direction is, for example, vertical directions.

[0010] As shown in FIG. 1, the three-dimensional modeling apparatus 100 includes, for example, a modeling unit 10, a stage 20, a moving means 30, and a control unit 40.

[0011] The modeling unit 10 includes, for example, a support member 110, a material supplying means 120, and a laser 130.

[0012] The support member 110 is, for example, a plate-shaped member and supports the material supply means 120 and the laser 130.

[0013] The material supplying means 120 supplies a material onto the stage 20. The supplied material will be described later. The material supplying means 120 has, for example, a material introduction part 121, a motor 122, a flat screw 123, a barrel 124, a heater 125, and a nozzle 126.

[0014] The material introduction section 121 of the material supply means 120 introduces the material into a groove 123a provided on the surface of the flat screw 123 on the barrel 124 side. The material introduced into the groove 123a is, for example, in powder form. The flat screw 123 is rotated by a motor 122. A heater 125 is provided in the barrel 124. The material is plasticized in the groove 123a by the heat of the heater 125. The plasticized material passes through a communication hole 124a provided in the barrel 124 and is discharged from a nozzle 126 toward the stage 20. The discharged material loses its fluidity on the stage 20.

[0015] The laser 130 irradiates laser light onto the material on the stage 20. The laser may be, for example, a YAG (Yttrium Aluminum Garnet) laser, a fiber laser, or a UV (ultraviolet) laser.

[0016] The laser light has an angular top hat shape. Laser light having an angular top hat shape has a highly uniform flat top and steeper boundary characteristics than laser light having a Gaussian shape.

[0017] The stage 20 is provided below the modeling unit 10. A material is supplied onto the stage 20, and a three-dimensional model is formed.

[0018] The moving means 30 changes the relative position of the modeling unit 10 and the stage 20. For example, the moving means 30 simultaneously changes the relative position of the stage 20 and the material supplying means 120 and the relative position of the stage 20 and the laser 130. In the illustrated example, the stage 20 is fixed, and the moving means 30 moves the modeling unit 10 with respect to the stage 20. In this way, it is possible to change the relative positions of the stage 20, the material supplying means 120, and the laser 130. In the illustrated example, the moving means 30 is connected to a support member 110, and the modeling unit 10 is moved by moving the support member 110.

[0019] The moving means 30 is configured, for example, by a three-axis positioner that moves the modeling unit 10 in the X-axis direction, the Y-axis direction, and the Z-axis direction by the driving forces of three motors (not shown). The motors of the moving means 30 are controlled by the control unit 40.

[0020] The moving means 30 may be configured to move the stage 20 without moving the modeling unit 10. In this case, the moving means 30 is connected to the stage 20. Alternatively, the moving means 30 may be configured to move both the modeling unit 10 and the stage 20. In this case, the moving means 30 is connected to both the modeling unit 10 and the stage 20.

[0021] The control unit 40 is configured, for example, by a computer having a processor, a main storage device, and an input / output interface that inputs and outputs signals from and to the outside. The control unit 40 performs various functions, for example, by the processor executing a program loaded into the main storage device. The control unit 40 controls the modeling unit 10 and the moving means 30. Specific processing of the control unit 40 will be described later. Note that the control unit 40 may be configured by a combination of multiple circuits instead of a computer.

[0022] 1.2. Materials The material supplied onto the stage 20 by the material supplying means 120 includes an inorganic powder and a binder. The inorganic powder is made of, for example, a metal or a ceramic. The material supplied by the material supplying means 120 may include both a metal powder and a ceramic powder.

[0023] Examples of metals include single metals such as magnesium (Mg), iron (Fe), cobalt (Co), chromium (Cr), aluminum (Al), titanium (Ti), copper (Cu), and nickel (Ni), or alloys containing one or more of these metals, as well as maraging steel, stainless steel (SUS), cobalt-chromium-molybdenum, titanium alloys, nickel alloys, aluminum alloys, cobalt alloys, and cobalt-chromium alloys.

[0024] Examples of ceramics include oxide ceramics such as silicon dioxide, titanium dioxide, aluminum oxide, and zirconium oxide, and non-oxide ceramics such as aluminum nitride.

[0025] Examples of the binder include synthetic resins such as acrylic resin, epoxy resin, silicone resin, and PVA (polyvinyl alcohol). The binder binds the inorganic powder together before the laser irradiation. The binder is vaporized by the irradiation of the laser light, for example.

[0026] The binder content in the material discharged from the nozzle 126 is, for example, 6% by mass or more and 9% by mass or less, and preferably 7.5% by mass or more and 8.5% by mass or less. If the binder content is 6% by mass or more, the lubricity of the material can be increased, and the material can be discharged from the nozzle 126. If the binder content is 9% by mass or less, the cost can be reduced. Note that the material discharged from the nozzle 126 is the material before it is irradiated with the laser light.

[0027] 1.3. Processing of the control section The control unit 40 controls the moving means 30, the material supplying means 120, and the laser 130. Fig. 2 is a flowchart for explaining the processing of the control unit 40. Figs. 3 and 4 are cross-sectional views that typically show the manufacturing process of a three-dimensional object manufactured by the three-dimensional printing apparatus 100.

[0028] For example, a user operates an operation unit (not shown) to send a processing start signal to the control unit 40. The operation unit is realized by, for example, a mouse, a keyboard, a touch panel, etc. When the control unit 40 receives the processing start signal, it starts processing as shown in FIG.

[0029] First, the control unit 40 performs a process of acquiring the modeling data (step S1). The modeling data is used to create a three-dimensional object. The modeling data includes information on the shape, size, material, and so on of the three-dimensional object to be created. The process of the control unit 40 described below is performed based on the modeling data. The modeling data is generated, for example, by slicer software installed on a computer connected to the three-dimensional modeling device 100. The control unit 40 acquires the modeling data from a computer connected to the three-dimensional modeling device 100 or a recording medium such as a Universal Serial Bus (USB) memory.

[0030] Next, the control unit 40 controls the moving means 30 to move the modeling unit 10 relative to the stage 20, while controlling the material supplying means 120 to supply the material 50 onto the stage 20, as shown in FIG. 3 (step S2).

[0031] In step S2, the control unit 40 supplies the material 50 to the first region 22 of the stage 20, but does not supply the material 50 to the second region 24 of the stage 20. That is, the control unit 40 supplies the material 50 only to the first region 22. The second region 24 is a region different from the first region 22. The second region 24 surrounds the first region 22 when viewed from the Z-axis direction, for example.

[0032] Next, the control unit 40 controls the moving means 30 to move the modeling unit 10 relative to the stage 20, while controlling the laser 130 to irradiate the material 50 on the stage 20 with laser light, as shown in Fig. 4 (step S3). By irradiating the material 50 with laser light, the material 50 is sintered or melted, and a modeling layer 52 with high flatness can be formed.

[0033] In step S3, the control unit 40 applies an energy density of 140 J / mm to the material 50 on the stage 20. 3 The laser beam is irradiated with a laser energy density of 140 J / mm. 3If the energy density is 140 J / mm or more, the remaining film ratio can be increased and the scattering of inorganic powder can be suppressed, as described in the experimental example described later. 3 The above laser beam is irradiated to form a three-dimensional object. The energy density of the laser beam is preferably 145 J / mm 3 That's all.

[0034] In step S3, the laser beam is irradiated with an energy density that does not exceed the boiling point of the inorganic powder contained in the material 50. If the laser beam is irradiated with an energy density that exceeds the boiling point of the inorganic powder, the inorganic powder will be vaporized and the amount of the inorganic powder will be reduced. The energy density of the laser beam is, for example, 500 J / mm 3 or less, preferably 400 J / mm 3 or less, more preferably 350 J / mm 3 The energy density of the laser light is, for example, 500 J / mm 3 If it is below this, energy savings can be achieved.

[0035] In step S3, the control unit 40 performs control according to the relational expression shown in Equation (1). For example, when the coating thickness d is set to 100 μm, the output power Pw of the laser light is set to 500 W, and the beam width Db of the laser light is set to 200 μm, the control unit 40 sets the scanning speed S of the laser light to approximately 18 0 mm / sec or less, energy density Eg 140 J / mm 3 Control is performed so that the above is satisfied.

[0036] Eg=Pw / (Db×S×d) (1)

[0037] Next, the control unit 40 performs a process of determining whether the number of stacked modeling layers 52 has reached a predetermined number based on the acquired modeling data (step S4). If it is determined that the number of stacked modeling layers 52 has not reached the predetermined number ("NO" in step S4), the control unit 40 returns to step S2 and repeats steps S2 and S3 until the number of stacked modeling layers 52 reaches the predetermined number. If it is determined that the number of stacked modeling layers 52 has reached the predetermined number ("YES" in step S4), the control unit 40 ends the process.

[0038] 1.4. Effects In the three-dimensional modeling apparatus 100, the control unit 40 controls the material supplying means 120 to supply the material 50 onto the stage 20, and controls the laser 130 to apply a laser beam having an energy density of 140 J / mm 3 The above-mentioned laser light irradiation process is performed. Therefore, in the three-dimensional modeling apparatus 100, as in the experimental example described later, it is possible to increase the remaining film rate of the modeling layer 52 and suppress scattering of inorganic powder. This makes it possible to stabilize the thickness of the three-dimensional model.

[0039] In the three-dimensional modeling apparatus 100, the material supplying means 120 has a nozzle 126 that discharges the material 50, and the binder content in the material 50 before being irradiated with the laser light is 6% by mass or more and 9% by mass or less. Therefore, in the three-dimensional modeling apparatus 100, the material 50 can be discharged from the nozzle 126 while achieving low costs.

[0040] In the three-dimensional modeling apparatus 100, the laser beam has a square top hat shape. Therefore, in the three-dimensional modeling apparatus 100, as in an experimental example described later, the surface roughness (maximum height) Sz of the modeling layer 52 can be made smaller than when the laser beam has a Gaussian shape.

[0041] In the three-dimensional modeling apparatus 100, the control unit 40 supplies the material 50 to the first region 22 of the stage 20 in the process of supplying the material 50, and does not supply the material 50 to the second region 24 different from the first region 22 of the stage 20. For example, in a powder bed fusion (PBF) method in which a hopper is used as a material supplying means and the material is supplied to the entire surface of the stage, even if inorganic powder is scattered and the thickness of the first modeling layer varies, the thickness can be made uniform in the material supply of the second modeling layer formed on the first modeling layer. On the other hand, in an FDM (fused deposition modeling) or PIJ (paste inkjet) method in which the material supplying means has a nozzle, the material is selectively supplied onto the stage, so that if the thickness varies in the first modeling layer, it is difficult to restore the thickness variation in the material supply of the second modeling layer. Therefore, the three-dimensional modeling apparatus 100 can be highly effective in the case where the material 50 is supplied to the first region 22 of the stage 20 and the material 50 is not supplied to the second region 24.

[0042] In the above example, the relative positions of the stage 20, the material supplying means 120, and the laser 130 can be changed simultaneously, but the material supplying means 120 and the laser 130 may be moved separately. Alternatively, the laser 130 may be fixed, and the laser light may be moved using a galvanometer mirror. In this case, the galvanometer mirror is controlled by the control unit 40.

[0043] In the above example, the flat screw 123 is used, but instead of the flat screw 123, an in-line screw or an FDM type head may be used.

[0044] 2. Experimental Example A material containing SUS630 powder as an inorganic powder and PVA as a binder was prepared. The PVA content in the material was set to 8 mass%. This material was supplied onto the stage from a nozzle and irradiated with laser light. Two types of laser light were used: a square top hat shape and a Gaussian shape. The irradiation energy density was varied by adjusting the beam width, output, and scan speed of the laser light.

[0045] Fig. 5 is a table showing the relationship between the energy density of the laser light and the remaining film rate and surface roughness Sz of the modeling layer. Fig. 6 is a graph showing the relationship between the energy density of the laser light and the remaining film rate of the modeling layer. Fig. 7 is a graph showing the relationship between the energy density of the laser light and the surface roughness Sz of the modeling layer. Figs. 6 and 7 are plots of the values ​​shown in Fig. 5. The surface roughness Sz was measured using a one-shot 3D shape measuring instrument VR3200 manufactured by KEYENCE.

[0046] In Fig. 5, the remaining film ratio is the ratio of the thickness of the bulk body to the thickness of the green body. The green body is the material supplied to the stage before it is irradiated with the laser light. The bulk body is the material supplied to the stage after it is irradiated with the laser light.

[0047] As shown in Figures 5 and 6, the energy density of the laser light is 140 J / mm 3 If the residual film ratio was greater than this, the residual film ratio was about 40%. Here, the content of SUS powder in the green body was 38.4% by volume. Therefore, if the residual film ratio was about 40%, it can be said that the SUS powder did not scatter due to the irradiation of the laser light. In Figure 6, the residual film ratio of 38.4% is indicated by a dashed line. Note that the residual film ratio exceeding 38.4% by volume is an error. If the energy density of the laser light is small, the SUS powder will scatter due to the volume expansion when the PVA vaporizes, resulting in a small residual film ratio.

[0048] As shown in Figures 5 and 6, when the laser beam has an angular top hat shape, the remaining film rate was about 40% even though the energy density was smaller than when the laser beam had a Gaussian shape. Also, as shown in Figures 5 and 7, when the laser beam has an angular top hat shape, the surface roughness Sz was smaller than when the laser beam had a Gaussian shape. When the laser beam has a Gaussian shape, the temperature becomes higher locally than when the laser beam has an angular top hat shape. Therefore, the SUS powder is more likely to scatter, and the surface roughness Sz increases.

[0049] The present invention includes configurations that are substantially the same as the configurations described in the embodiments, for example, configurations with the same functions, methods, and results, or configurations with the same purpose and effects. The present invention also includes configurations in which non-essential parts of the configurations described in the embodiments are replaced. The present invention also includes configurations that achieve the same effects as the configurations described in the embodiments, or configurations that can achieve the same purpose. The present invention also includes configurations in which publicly known technology is added to the configurations described in the embodiments.

[0050] The following can be derived from the above-described embodiment.

[0051] One aspect of the three-dimensional printing apparatus includes: Stage and A material supplying means for supplying a material including an inorganic powder and a binder; Lasers and A control unit; Including, The control unit is A process of controlling the material supplying means to supply the material onto the stage; The laser is controlled to apply an energy density of 140 J / mm to the material on the stage. 3 The above-mentioned laser light irradiation process is carried out.

[0052] According to this three-dimensional modeling apparatus, scattering of inorganic powder can be suppressed.

[0053] In one embodiment of the three-dimensional printing apparatus, the material supplying means has a nozzle for discharging the material, The content of the binder in the material before being irradiated with the laser light may be 6% by mass or more and 9% by mass or less.

[0054] This three-dimensional modeling apparatus can eject material from the nozzle while reducing costs.

[0055] In one embodiment of the three-dimensional printing apparatus, The laser beam may have a squared top hat shape.

[0056] According to this three-dimensional modeling apparatus, the surface roughness Sz of the modeling layer can be made smaller than when the laser light has a Gaussian shape.

[0057] In one embodiment of the three-dimensional printing apparatus, In the process of supplying the material, the control unit may supply the material to a first area of ​​the stage, and may not supply the material to a second area of ​​the stage that is different from the first area. [Explanation of symbols]

[0058] 10...modeling unit, 20...stage, 22...first area, 24...second area, 30...moving means, 40...control unit, 50...material, 52...modeling layer, 100...three-dimensional modeling device, 110...support member, 120...material supply means, 121...material introduction unit, 122...motor, 123...flat screw, 123a...groove, 124...barrel, 124a...communicating hole, 125...heater, 126...nozzle, 130...laser

Claims

1. Stage and A material supplying means for supplying a material including an inorganic powder and a binder; Lasers and A control unit; Including, The control unit is A process of controlling the material supplying means to supply the material onto the stage; The laser is controlled to apply an energy density of 140 J / mm to the material on the stage. 3 A process of irradiating the substrate with laser light having an intensity of 500 J / mm or more and 500 J / mm or less is performed. the material supplying means has a nozzle for discharging the material, a content of the binder in the material before the laser light is irradiated is 6% by mass or more and 9% by mass or less.

2. In claim 1, The laser beam has a square top hat shape.

3. In claim 1 or 2, The control unit, in the process of supplying the material, supplies the material to a first region of the stage, and does not supply the material to a second region of the stage different from the first region.

Citation Information

Patent Citations

  • Method for producing three-dimensional molding

    JP2008184622A

  • Three-dimensional formation apparatus and three-dimensional formation method

    JP2017002387A

  • Three-dimensional forming apparatus, three-dimensional forming method and three-dimensional formed object

    JP2017043805A

  • Method for manufacturing molded article, and molded article

    WO2018230421A1