Method for manufacturing printed material and printed material
By adjusting the surface energy of metal cans to 30-50 mN/m using receptive layers and surface modifications, inkjet printing achieves improved image quality by preventing ink coalescence and ensuring uniform film thickness.
Patent Information
- Application Number
- JP2021550414
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-03-02
- Filing Date
- 2020-08-19
- Publication Date
- 2024-10-16
- Estimated Expiration
- 2040-08-19
Smart Images

Figure 0007567800000002 
Figure 0007567800000003 
Figure 0007567800000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a printed substrate and a printed substrate. More specifically, the present invention provides a method for manufacturing a printed substrate and a printed substrate that can improve the quality of a printed image in inkjet printing on the printed substrate regardless of the resolution of the inkjet image. [Background technology]
[0002] In the manufacturing process of printed cans, patterns and letters are printed on the metal plate that forms the can body, or on the can body after the can body and the bottom are integrally formed. Printing on the metal plate or the can body can be done by plate printing or inkjet printing. Inkjet printing has the advantage that it is cost-effective because it does not require plate making, and that the printing design can be changed in a short period of time.
[0003] As an example of a printing technique for printing onto printed cans using inkjet printing, FIG. 5 of Patent Document 1 discloses a technique in which droplets of each ink (white (W), yellow (Y), magenta (M), cyan (C), and black (K)) are sprayed in sequence from inkjet heads corresponding to each ink, forming a printed image on a seamless can attached to a mandrel.
[0004] On the other hand, when using a recording medium with high liquid repellency, the droplets coalesce, making it impossible to form a solid image with a uniform film thickness. To solve this problem, a technology has been disclosed in which a specific relationship is established between the surface energy of the receiving medium and the surface energy of the droplets, and a specific relationship is also established between the diameter of the landing dots and the maximum distance of the resolution pitch (see Patent Document 2). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2012-86870 A [Patent Document 2] Patent No. 4903024 Summary of the Invention [Problem to be solved by the invention]
[0006] Matters to be considered when printing include forming an image with a uniform thickness as in Patent Document 2, as well as suppressing deterioration in image quality caused by the wetting and spreading of the ink forming the printed image, ink repellency, etc. An object of the present invention is to improve the quality of printed images in inkjet image printing on a substrate selected from cans and container films. [Means for solving the problem]
[0007] Through research, the inventors have discovered that in order to improve the quality of printed images in inkjet printing on substrates selected from cans and container films, it is important to adjust the free energy of the printed area on the surface of the substrate within a certain range, regardless of the resolution of the inkjet image, and have thus completed the present invention.
[0008] The present invention provides a method for producing a printing substrate having a printing area on a surface thereof, comprising the steps of: The substrate is selected from cans and container films; The method for producing a printed material includes a surface adjustment step of adjusting the printing area so that the surface energy E (mN / m) of the printing area is 30 or more and 50 or less.
[0009] The surface conditioning step is preferably carried out in such a manner that a receiving layer is formed on at least a part of the printing area, and specific examples of the receiving layer are preferably a porous receiving layer or a swelling type receiving layer. Furthermore, the receiving layer preferably contains a base resin selected from the group consisting of acrylic resins, polyester resins, epoxy resins, and blends thereof, and is preferably in a semi-cured state. It is preferable that the receiving layer contains titanium oxide. In addition, the surface conditioning step preferably includes treating at least a part of the printing area with a surface modifying means. The method may also include a printing step of forming an inkjet image in a printing area of a substrate manufactured by the above-mentioned manufacturing method, and it is preferable that the printing step includes an image forming step of forming an inkjet image on an image conveying means, and a transfer step of transferring the inkjet image formed on the image conveying means to the printing area.
[0010] Another aspect of the present invention is a substrate, which is a film for cans or containers, including a printed area on its surface, wherein the surface energy E (mN / m) of the printed area is 30 or more and 50 or less. The printing area preferably has a receptive layer on its surface, the receptive layer preferably containing titanium oxide. Effect of the Invention
[0011] The present invention allows for improved quality of printed images in inkjet printing on a substrate, regardless of the resolution of the inkjet image. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a schematic diagram illustrating an example of a configuration of a printing system. [Diagram 2] FIG. 13 is a schematic diagram showing another example of the configuration of a printing system. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] One embodiment of the present invention is a method for manufacturing a printed substrate having a printed area on its surface, which includes a surface adjustment step of adjusting the printed area so that the surface energy E (mN / m) of the printed area is 30 or more and 50 or less. The substrate is selected from cans and container films, which are prone to ink wetting and spreading or ink repellency. The container film is not limited as long as it is used for containers, and may be a film for pouches or labels.
[0014] In this embodiment, when printing an inkjet image on a substrate such as a can, the surface energy E (mN / m) of the printed area of the substrate is adjusted to the above range in order to improve the quality of the printed image. In inkjet image printing, it is possible to vary the diameter of the inkjet ink droplets that land on the printed area from the inkjet nozzle depending on the resolution of the inkjet image to be printed, but according to the study of the present inventors, it was found that the surface energy of the printed area is important for improving the quality of the printed image, regardless of the diameter of the inkjet ink droplets that land, i.e., regardless of the resolution of the inkjet image.
[0015] If the surface energy E is less than 30 mN / m, the surface of the printed area becomes less wet and repels the ink droplets excessively, resulting in poor image quality. On the other hand, if the surface energy exceeds 50 mN / m, the surface of the printed area becomes more wet, leading to ink droplets bleeding, blurring the image contour, clouding the colors, and poor image quality. It is preferable that the surface energy E is 35 mN / m or more and 50 mN / m or less.
[0016] In this embodiment, the quality of the printed image can be improved regardless of the diameter of the landing inkjet ink droplets, i.e., the resolution of the inkjet printed image, which is usually 300 dpi or more, but is not limited to this. The printing area to be adjusted in the surface adjustment step may be the entire surface of the can or a part of the can surface. When adjusting a part of the can surface, it is preferable to adjust the printing area to be inkjet printed.
[0017] In this embodiment, in order to set the surface free energy E of the printed area in the surface adjustment step to the above-mentioned suitable range, for example, a method of providing a receptive layer on at least a part of the printed area, a method of modifying at least a part of the printed area using a surface modification means, etc., can be used, but are not limited to these.
[0018] The receiving layer is a layer that enables inkjet printing on materials on which inkjet printing is not possible or is difficult, and typically there are swelling-type receiving layers with a transparent surface and porous-type receiving layers with a whitish surface.
[0019] The swelling type receiving layer is made of a resin that easily absorbs ink, and the absorbed ink swells the resin layer and remains in the receiving layer, making printing possible. The base resin contained in the swelling type receiving layer is not limited as long as it is a resin that easily absorbs ink, but examples thereof include acrylic resins, polyester resins, epoxy resins, vinyl resins, urethane resins, and blends thereof, and among these, it is preferable to contain one or more selected from acrylic resins, polyester resins, epoxy resins, urethane resins, and blends thereof. Note that when making a blend resin, the ratio of each resin is not particularly limited, and it may be a blend of two types or a blend of three or more types. The swelling type receptor layer may contain resins other than those mentioned above as long as the function of the layer is not impaired.
[0020] The base resin contained in the swelling type receiving layer is preferably in a semi-cured state, since the resin may lose its ability to absorb ink and swell when in a cured state.
[0021] The porous receiving layer contains inorganic fine particles to form voids, and ink penetrates the voids and remains in the receiving layer, making printing possible. The inorganic fine particles contained in the porous receiving layer are not limited as long as they can form voids, but examples include silica, alumina, titania (titanium oxide), boron nitride, and the like, and are preferably selected from silica and alumina. The particle size of the inorganic fine particles is not particularly limited, but the average primary particle size is usually 10 nm or more, and may be 50 nm or more, and may be usually 50 μm or less. The average primary particle size can be determined from the results of measuring the particle size distribution using a laser diffraction / scattering type particle size distribution measuring device or the like, but for commercially available products, the catalog value may be used. The thickness of the receiving layer is not particularly limited and can be appropriately determined by a person skilled in the art.
[0022] The receiving layer may contain a white pigment, such as titanium oxide, zinc sulfide, zinc oxide (zinc oxide), lithopone (zinc sulfide + barium sulfate), etc., with titanium oxide being particularly preferred. By containing a white pigment in the receiving layer, the pattern layer, such as a design, formed on the receiving layer can be more clearly recognized.
[0023] The method of modifying the surface by the surface modification means is not particularly limited as long as it can modify the printing area and set the surface free energy E within the above range, and for example, the surface can be modified by spraying a combustion flame containing a silicon compound. By spraying a combustion flame containing a silicon compound, a silicon oxide film can be formed on the printing area, and the surface free energy E can be set to satisfy the above range.
[0024] The silicon compound is not particularly limited, and typically includes, but is not limited to, silane compounds such as alkylsilanes and alkoxysilanes. These silane compounds may have nitrogen, halogens such as chlorine, vinyl groups, amino groups, etc. As a surface modification means, a corona treatment, a plasma treatment, a glow discharge treatment, an arc discharge treatment, etc. may be used. Furthermore, by adjusting the printing area, the ink adhesion to the printing substrate can be improved.
[0025] In this embodiment, after the printed object is manufactured, if the printed object is a can, a printing step may be included in which an inkjet image is printed on the can. Also, if the printed object is a container film, a printing step may be included in which an inkjet image is printed on the container film. The printing step is not particularly limited, and inkjet printing may be performed directly from the inkjet nozzle onto the printed area on the surface of the can or container film, or offset printing may be performed in which an inkjet image is printed once from the inkjet nozzle onto a blanket or the like, and then the inkjet image is transferred to the printed area. An example of an inkjet printing system to which the embodiment of the present invention can be applied will be described below.
[0026] FIG. 1 is a schematic diagram showing the configuration of an inkjet printing system 1 for forming an inkjet image on a printing area on a can surface. When printing is performed on at least the outer surface of the body of a seamless can, a printing system in which a seamless can is rotatably fixed to a mandrel formed on a mandrel wheel and inkjet printing is performed by printing stations installed along the mandrel wheel has excellent productivity. In the inkjet printing system 1, a plurality of mandrels 3 are evenly arranged on a mandrel wheel 2, and the mandrel wheel 2 revolves intermittently clockwise, and the mandrels 3 rotate clockwise at each station. As a can 4 placed on the mandrel 3 is transported along the arrow, an image is printed by a plurality of nozzle heads 5 that eject ink of each color, white (W), yellow (Y), magenta (M), cyan (C), and black (K). The order of the colors is not particularly limited, and the colors of the ink are not limited to these. Therefore, clear ink may be used. In addition, two inkjet heads may be installed in each printing station, and by adopting such a configuration, the printing speed is high, and the resolution can be increased by increasing the halftone dot density, and the ink thickness can be increased by precisely overlapping the halftone dots, making it possible to obtain a printed image with a high sense of density. In addition, the type of ink is not particularly limited, and may be a water-based ink or a UV-curable ink.
[0027] The can 4 with the printed image is pre-baked in a pre-baking section 6, and then a varnish is applied to the surface of the can by a varnish application device 7, producing a printed can. In addition, a receptive layer forming means (including a coating means and a receptive layer drying means) for forming a receptive layer on the can surface may be provided in the printing system 1, and a surface modifying means for modifying the surface of the can may be provided. For example, the receptive layer forming means and the surface modifying means may be provided upstream of the nozzle head 5. Furthermore, a receiving layer forming means or a surface modifying means may be provided in a process prior to entering the printing system 1.
[0028] FIG. 2 is a schematic diagram showing the configuration of the inkjet printing system 100. As shown in FIG. The inkjet printing system 100 includes a printing station 10 as an image forming means, a conveyor belt 20 as an image conveying means, a transfer station 30 as a transfer means, a mandrel wheel 40 and a mandrel 42 as a can conveying means, a cleaning station 50 as a cleaning means, and an overcoat station 60 as a coating means. The inkjet printing system 100 may include other components.
[0029] The printing station 10 includes a printing unit 11, and an inkjet image 14 (not shown) is formed on a blanket 23 of the transport belt 20 by an inkjet printer head included in the printing unit 11. The printing station 10 may include only one printing unit 11, or may include multiple printing units 11. By including multiple printing units 11, it is possible to support high-speed printing and also to support a printing method with a large number of passes, thereby improving the quality of the printed image and allowing a high-resolution inkjet image 14 to be formed on the blanket 23.
[0030] The inkjet printer head of the printing unit 11 typically includes a plurality of nozzle heads 12 that eject ink of each color, white (W), black (K), yellow (Y), magenta (M), and cyan (C). The order of the colors is not particularly limited, and the ink colors are not limited to these. Therefore, clear ink may be used.
[0031] The printing unit 11 may be equipped with a nozzle bed that ejects a primer layer (Pr), in which case it may be positioned downstream of the inkjet printer head so that the formed inkjet image 14 can be covered with the primer layer. Printing unit 11 may further include a UV irradiation unit 13 as a curing means. When the ink ejected from the inkjet printer head is a UV-curable ink, the ink can be semi-cured by UV irradiation to reduce ink residue that may occur when inkjet image 14 is transferred to can 41 at the transfer station. Moreover, a drying means may be provided as a curing means instead of the UV irradiation unit 13. The drying means can semi-cure the inkjet image 14 by, for example, blowing hot air onto the inkjet image.
[0032] The conveyor belt 20 is circularly shaped via a first roller 21 and a second roller 22, and conveys an inkjet image printed on a blanket 23 of the conveyor belt 20 to a transfer station 30 by rotating in the direction of the arrow in the figure. The number of blankets 23 of the conveyor belt 20 can be appropriately determined according to the circumferential length of the circular conveyor belt and the operating speed of the printing system.
[0033] The conveyor belt 20 may be flexible, but if the material is too flexible, the tension of the belt may be insufficient, which may cause misalignment during printing or transfer. The material of the conveyor belt 20 is not particularly limited. In order to guide the conveyor belt, in addition to the first roller 21 and the second roller 22, one or more auxiliary rollers may be provided.
[0034] The blanket 23 on which the inkjet image 14 has been formed is transported to the transfer station 30 along the outer periphery of the first roller 21. Meanwhile, a plurality of cans 41 are transported to the transfer station 30 by the mandrel wheel 40. When the leading end of the blanket 23 comes into contact with the transported can 41, or just before the leading end comes into contact with the can 41, the can 41 starts to rotate, and after the contact, the inkjet image 14 formed on the blanket 23 is transferred in the circumferential direction of the can 41, forming an inkjet image on the surface of the can 41. The blanket 23 and the can 41 may be appropriately aligned, and the alignment may be performed by a known method. Also, when the leading end of the blanket 23 comes into contact with the transported can 41, the rotation of the mandrel wheel 40 itself may be stopped, and the can 41 on the mandrel 42 may be rotated while the mandrel wheel 40 is stopped, so that the inkjet image 14 formed on the blanket 23 may be transferred to the can 41. This embodiment may also be applied to such intermittent printing.
[0035] After the inkjet image 14 is transferred from the blanket 23 to the surface of the can 41 at the transfer station 30, the surface of the blanket 23 may be cleaned at the cleaning station 50. In this embodiment, since there may be cases where not all of the ink is transferred to the blanket 23, the cleaning station 50 may be provided to clean the ink on the blanket 23.
[0036] The cleaning station 50 typically includes a cleaning agent supplying section 51 that ejects a cleaning agent onto the blanket 23, and a scraper 52 that wipes off the ink on the blanket 23. The blanket 23, the surface of which has been cleaned in the cleaning station 50, is guided by the second roller 22 and transported again to the printing station 10, where an inkjet image 14 is formed thereon.
[0037] The can 41 onto which the inkjet image 14 has been transferred is transported by the mandrel wheel 40 to the overcoat station 60. At the overcoat station 60, the inkjet image 14 transferred onto the surface of the can 41 is coated. Typically, a varnish is used for the coating, but other coatings may be used as long as they can protect the inkjet image and improve its durability, and it is not necessary to apply varnish over the inkjet image 14.
[0038] A receptive layer forming means (including a coating means and a receptive layer drying means) for forming a receptive layer on the can surface may be provided in the printing system 100, and a surface modifying means for modifying the surface of the can surface may be provided. For example, the receptive layer forming means and the surface modifying means may be provided upstream of the transfer station of the can conveying means. It will be appreciated that the printing system 100 may also be used to pre-print cans. EXAMPLES
[0039] The following is a detailed investigation of the relationship between the surface energy E (mN / m) of a can when printing an image on it with an inkjet and the quality of the printed image. First, an aluminum can body and a bottom were integrally formed to prepare a can as a printing substrate. The prepared cans were subjected to the treatments shown in Table 1 below, and the surface energy E of the cans was measured. The surface energy E was measured using a contact angle meter (DropMaster DM500, manufactured by Kyowa Interface Science Co., Ltd.).
[0040] <Method of measuring surface energy> Using two liquids (water and diiodomethane) with known surface energies, the contact angle of each of the target substrate surfaces was measured using a contact angle meter. The surface energy of the target substrate surface was obtained using the Kaelble-Uy theoretical formula. The results are shown in Table 1.
[0041] An inkjet image was printed on the treated can using the printing system 1 shown in Fig. 1. The printing results (visually observed) are shown in Table 1. The evaluation was performed according to the following evaluation criteria. <Evaluation criteria> A: The printed image was very clear. B: The image was slightly blurred around the edges, but was still clearly visible. C: The image was unclear.
[0042] [Table 1]
[0043] These results show that, regardless of the resolution, when the surface energy E of the can is in a specific range, the printed inkjet image is clear and good quality inkjet image printing can be provided on the surface of the can.
[0044] Although the present invention will be described in detail with reference to specific embodiments, it will be apparent to those skilled in the art that various changes and modifications can be made without departing from the spirit and scope of the present invention. [Explanation of symbols]
[0045] 1. Inkjet Printing System 2 Mandrel Wheel 3 Mandrel 4 cans 5 Nozzle Head 6 Temporary curing section 7 Varnish application device 100 Inkjet Printing System 10 Printing Station 11 Printing unit 12 Nozzle head 13 UV irradiation section 14 Inkjet Images 20 Conveyor belt 21 First Roller 22 Second Roller 23 Blanket 30 Transfer Station 40 Mandrel Wheel 41 Cans 42 Mandrel 50 Washing Station 51 Cleaning agent supply section 52 Scraper 60 Overcoat Station
Claims
1. A method for manufacturing a printing substrate having a printing area on a surface thereof, comprising the steps of: The substrate is selected from cans and container films; A surface adjustment step of adjusting the surface of the printing area so that the surface energy E (mN / m) of the printing area is 30 or more and 50 or less, The surface conditioning step is a step of forming a receiving layer on at least a part of the printing area, the receiving layer is a swelling type receiving layer, The method for producing a printed material, wherein the swelling type receiving layer is in a semi-cured state.
2. The method for producing a printed material according to claim 1 , wherein the swelling type receiving layer contains a base resin selected from the group consisting of an acrylic resin, a polyester resin, an epoxy resin, a urethane resin, and blends thereof.
3. The method for producing a printing substrate according to claim 1 or 2, wherein the receptive layer contains titanium oxide.
4. A method for producing a printed matter, comprising a printing step of forming an inkjet image in a printing area of a printed matter produced by the method according to any one of claims 1 to 3.
5. The printing step includes: forming the inkjet image on an image conveying means; The method for producing a printed matter according to claim 4, further comprising a transfer step of transferring the inkjet image formed on the image transport means to the region to be printed.
Citation Information
Patent Citations
JP1974003024A
Ink jet recorder for medical use
JP2003154641A
Aqueous coating composition for can
JP2007269889A
Resin coated metal sheet for container