Systems and methods for electrode seal assemblies - Patents.com
The electrode seal assembly addresses gas leaks and corrosion issues in vitrification processes by using a pressure gradient and high-pressure sealing, ensuring efficient operation and safety.
Patent Information
- Application Number
- JP2023149087
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2015-12-29
- Filing Date
- 2023-09-14
- Publication Date
- 2024-10-16
- Estimated Expiration
- 2036-12-22
AI Technical Summary
Vitrification processes face issues with gas leaks and electrode corrosion due to pressure fluctuations and exposure to hot gases, leading to heat loss and reduced efficiency, which can be harmful to the environment and equipment.
An electrode seal assembly that utilizes a pressure gradient and high-pressure sealing to maintain an effective seal, preventing gas leaks and protecting the electrodes from corrosion.
The solution effectively prevents gas leaks and maintains the integrity of the vitrification vessel atmosphere, enhancing efficiency and reducing environmental and equipment risks.
Smart Images

Figure 0007568807000001 
Figure 0007568807000002 
Figure 0007568807000003
Abstract
Description
Copyright Notice
[0001]
[0001] The material contained herein is subject to copyright protection. The copyright owner has no objection to the facsimile reproduction by anyone of the patent document or the patent disclosure, but reserves all rights to the copyright in the patent application or records with the U.S. Patent and Trademark Office. The following notice applies to the software, screen shots and data described below and shown in the drawings to this document, and all rights are reserved.
[0002] [Technical field]
[0003] This disclosure relates generally to electrode seals and electrode seal assemblies for high temperature vitrification containers.
[0004] background
[0005]
[0003] The vitrification process involves heating the waste material to be processed, a starter passage which may contain one or more conductive materials (e.g., glass frit, graphite flake, silica, cullet) in a vitrification chamber. Heating is effected by supplying electrical current to the vitrification vessel using an axially inserted electrode to raise the temperature of the starter passage to a point where the adjacent material to be processed begins to melt. Once heating begins, melting of the material begins and the molten material itself is electrically conductive and can continue to conduct electrical current and heat. Power can be applied to the electrode until the material contained within the vitrification chamber is completely melted. The electrode is typically consumed by the melt within the vitrification vessel.
[0006] Gas may leak from the vitrification vessel between the electrode and the lid and / or cold air may be drawn in if the vitrification vessel is operated at negative pressure. The environment inside the vitrification vessel cannot be maintained, resulting in loss of heat, reduced efficiency, and potential loss of gas in the vent chamber. The exterior surface of the electrode may be subject to corrosion through oxidation due to the hot gas inside the vitrification vessel and heating of the electrode which may reduce the current carrying capacity of the electrode. It is desirable to avoid gas leakage from the vitrification vessel as this can be harmful to the environment, workers, and equipment.
[0007] There is a need for an electrode seal assembly that can maintain the atmosphere within the vitrification containment vessel, allow axial movement of the electrode, and prevent outgassing in at least one effective seal under both positive and negative pressure conditions within the vitrification containment vessel. In some embodiments of the electrode seal assembly disclosed herein, the seal is effective using a gas pressure that results in a pressure gradient higher than the pressure within the vitrification containment vessel.
[0008]
[0006] To reduce the complexity and length of the detailed specification, applicant specifically incorporates by reference herein all of the following materials, as identified in the following paragraphs: Although the incorporated material is not necessarily "prior art," applicant specifically reserves the right to subscribe to the incorporated material.
[0009]
[0007] Application No. 62 / 239,660, filed October 9, 2015, entitled "Advanced Tritium System and Advanced Permeation System for Separation of Tritium from Radioactive Wastes and Reactor Water in Light Water Systems," is hereby incorporated by reference in its entirety.
[0010]
[0008] Application No. 62 / 272,604, filed December 29, 2015, entitled "GeoMelt Electrode Seal," is hereby incorporated by reference in its entirety.
[0011]
[0009] Application No. 15 / 012,101, entitled "Ion Specific Media Removal from Vessel for Vitrification," filed on February 1, 2016 and having a priority date of February 1, 2015, is hereby incorporated by reference in its entirety.
[0012]
[0010] Application No. 14 / 748,535, entitled "Mobile Processing System for Hazardous and Radioactive Isotope Removal," filed on June 24, 2015, and having a priority date of June 24, 2014, is hereby incorporated by reference in its entirety.
[0013]
[0011] Application No. 14 / 294,033, entitled "Balanced Closed Loop Continuous Extraction Process for Hydrogen Isotopes," filed on June 2, 2014, and having a priority date of May 31, 2013, is hereby incorporated by reference in its entirety.
[0014]
[0012] Patent No. 7,211,038, entitled "Methods for Melting of Materials to be Treated," filed on March 25, 2001, and having a priority date of September 25, 2001, is incorporated herein by reference in its entirety.
[0015]
[0013] Patent No. 7,429,239, entitled "Methods for Melting of Materials to be Treated," filed on April 27, 2007, and having a priority date of September 25, 2001, is incorporated herein by reference in its entirety.
[0016]
[0014] Patent No. 5,678,237, entitled "In-Situ Vitrification of Waste Materials," filed on June 24, 1996, and having a priority date of June 24, 1996, is hereby incorporated by reference in its entirety.
[0017]
[0015] Patent No. 6,283,908, entitled "Vitrification of Waste with Continuous Filling and Sequential Melting," filed on May 4, 2000, and having a priority date of May 4, 2000, is incorporated herein by reference in its entirety.
[0018]
[0016] Patent No. 6,558,308, entitled "AVS Melting Process," filed on April 25, 2002, and having a priority date of May 7, 2001, is incorporated herein by reference in its entirety.
[0019]
[0017] Patent No. 6,941,878, entitled "Advanced Vitrification System 2," filed on September 26, 2003, and having a priority date of September 27, 2002, is hereby incorporated by reference in its entirety.
[0020]
[0018] Applicant believes that the incorporated material is "non-essential" under 1 CFR 1.57 because it is referenced to provide background and illustrate the state of the art. However, if the examiner believes that the incorporated material constitutes "essential material" under 1 CFR 1.57(c)(1)-(3), Applicant will amend the specification to specify the essential material incorporated by reference as permitted by the applicable regulations.
[0021]
[0019] The following drawings and detailed description will explain the embodiments and applications presented herein. Unless otherwise specified, the terms and phrases in the specification and claims will have their plain, ordinary, and customary meaning conveyed to those of ordinary skill in the relevant art. The inventors are fully aware that they are their own lexicographers, if necessary. The inventors, as their own lexicographers, have clearly selected terms with their plain, ordinary, and customary meanings for use in the specification and claims, unless they expressly state and provide a definition of a "special" term and explain how it differs from the plain, ordinary meaning. It is the intention and desire of the inventors that the plain, plain, ordinary meaning of a term be applied in interpreting the specification and claims, unless there is an express statement of intent to apply a "special" definition.
[0022]
[0020] The inventors are also aware of the normal rules of English grammar, so that where a noun, term, or phrase is intended to be further characterized, specified, or narrowed in any way, in accordance with the normal rules of English grammar, such noun, term, or phrase will obviously include additional adjectives, descriptive terms, or other modifiers, and in the absence of the use of such adjectives, descriptive terms, or modifiers, such noun, term, or phrase is intended to convey its plain ordinary English meaning to one of ordinary skill in the art as described above.
[0023]
[0021] Furthermore, the inventors are fully aware of the criteria and application of the specific provisions of 35 USC § 112, 6. As such, the use of "functions," "means," and "steps" in the detailed description, drawing descriptions, and claims is not intended to indicate a desire to invoke 35 USC § 112, 6 to define the systems, methods, processes, and / or apparatus disclosed herein. In contrast, when the provisions of 35 USC § 112, 6 are sought to be invoked to define an embodiment, the claims will specifically and explicitly recite the precise phrase "means for," "step for," and in such phrase, the word "function" without reciting any structure, material, or act in support of that function. (i.e., it states "means for performing the function of ....") Thus, even when a claim recites "means for performing the function of ..." or "steps for performing the function of ...," it is the inventors' express intent not to invoke the provisions of 35 USC § 112, 6 when the claim similarly recites any structure, material, or acts supporting or performing the recited function. Moreover, when the provisions of 35 USC § 112, 6 are invoked to define claimed embodiments, those embodiments are not limited to only the particular structure, materials, or acts described in the preferred embodiment, but further are intended to include all structures, materials, or acts, now known or later developed, that perform the claimed function as described in alternative embodiments or configurations, and equivalent structures, materials, or acts that perform the claimed function. [Brief description of the drawings]
[0024] A more complete understanding of the systems, methods, processes, and / or apparatus disclosed herein can be obtained by reference to the detailed description when considered in conjunction with the following drawings, in which like reference characters refer to like elements, acts, and functions throughout the drawings, and in which:
[0023] [Figure 1] FIG. 1 is a block diagram showing the primary components in a typical vitrification system. [Diagram 2] FIG. 2 is an illustration of an electrode.
[0025] [Figure 3A] FIG. 3A is an isometric view of an electrode seal embodiment.
[0026] [Figure 3B] FIG. 3B is a top view of the electrode seal of FIG. 3A.
[0027] [Figure 3C] FIG. 3C is a front view of the electrode seal of FIG. 3A.
[0028] [Figure 4A] FIG. 4A is an isometric view of a seal assembly embodiment.
[0029] [Figure 4B] FIG. 4B is a top view of the embodiment of the electrode seal assembly of FIG. 4A.
[0030] [Figure 4C] FIG. 4C is a front view of the electrode seal assembly embodiment of FIG. 4A.
[0031] [Figure 4D] FIG. 4D is a bottom view of the electrode seal assembly embodiment of FIG. 4A.
[0032] [Figure 4E] 4E is an isometric view of a clamp shell style seal housing half of the electrode seal assembly embodiment of FIG. 4A.
[0033] [Figure 4F] FIG. 4F is a cross-section of the seal assembly showing details of the internal components of the electrode seal assembly embodiment of FIG. 4A.
[0034] [Figure 4G] FIG. 4G is a cross-section of the electrode seal assembly embodiment of FIG. 4A without the graphite rod or its electrode seal.
[0035] [Figure 5A] FIG. 5A is an isometric view of an embodiment of an electrode seal assembly.
[0036] [Figure 5B] FIG. 5B depicts an exploded isometric view of the embodiment of the electrode seal assembly of FIG. 5A.
[0037] [Figure 5C] FIG. 5C depicts a cross-section of the electrode seal assembly embodiment of FIG. 5A.
[0038] [Figure 5D] FIG. 5D depicts an isometric view of the clamp shell-style seal housing of the electrode seal assembly embodiment of FIG. 5A.
[0039] [Figure 5E] FIG. 5E depicts a bottom view of the electrode seal assembly embodiment of FIG. 5A.
[0040] [Figure 6A] FIG. 6A is an isometric view of an embodiment of an electrode seal assembly.
[0041] [Figure 6B] FIG. 6B is a cross-section of the electrode seal assembly embodiment of FIG. 6A.
[0042] [Figure 7A] FIG. 7A is an isometric view of an embodiment of an electrode seal assembly.
[0043] [Figure 7B] FIG. 7B is an exploded view of the electrode seal assembly of FIG. 7A.
[0044] [Figure 7C] FIG. 7C is a front opposed cross-section of the electrode seal assembly embodiment of FIG. 7A.
[0045] [Figure 7D] FIG. 7D is an isometric cross-section of the electrode seal assembly of FIG. 7A.
[0046] [Figure 8A] FIG. 8A depicts an embodiment of a vitrification zone in the vitrification and off-gas treatment process embodiment of FIG. [Figure 8B] FIG. 8B depicts an embodiment of an off-gas pretreatment zone in the vitrification and off-gas treatment process embodiment of FIG. [Figure 8C] FIG. 8C depicts an embodiment of a cooling zone in the vitrification and off-gas treatment process embodiment of FIG. [Figure 8D] FIG. 8D depicts an embodiment of an off-gas wet scrubbing zone in the vitrification and off-gas treatment process embodiment of FIG. [Figure 8E] FIG. 8E depicts an embodiment of an off-gas final conditioning zone in the vitrification and off-gas treatment process embodiment of FIG. [Figure 8F] Figure 8F illustrates an embodiment of an off-gas exhaust zone in the vitrification and off-gas treatment process embodiment of Figure 1. The elements and acts in the figure are shown for simplicity and are not necessarily depicted according to any particular step or embodiment.
[0025] Detailed Description
[0026]
[0054] In the following description, for purposes of explanation, many specific details, process durations, and / or numerical values of specific formulas are set out to provide a detailed understanding of various aspects of the exemplary embodiments. However, it will be understood by those skilled in the art that the apparatus, system, and method may be practiced without having these specific details, process durations, and / or numerical values of specific formulas herein. It will be understood that other embodiments may be utilized, and structural and functional changes may be made without departing from the scope of the apparatus, system, and method herein. In other instances, known structures and devices are shown and discussed more generally to avoid obscuring the exemplary embodiments. In many cases, the description of the operations is sufficient to realize various forms, especially when the operations are to be implemented in software. It should be noted that there are many different alternative configurations, devices, and techniques to which the disclosed embodiments may be applied. The full scope of the embodiments is not limited to the examples described below.
[0027]
[0055] In the following examples of illustrated embodiments, reference is made to the accompanying drawings, which form a part hereof, and which illustrate various embodiments in which the systems, methods, processes, and / or apparatus disclosed herein may be practiced. It is to be understood that other embodiments may be utilized, and that structural and functional changes may be made without departing from the scope thereof.
[0028] Process Overview
[0029]
[0056] FIG. 1 depicts different stages in an embodiment of a vitrification process, including vitrification 100 (Zone 1), off-gas pretreatment 120 (Zone 2), cooling (optional when needed) 130 (Zone 3), off-gas wet scrubbing 140 (Zone 4), off-gas final conditioning 150 (Zone 5), and off-gas exhaust 160 (Zone 6). Other embodiments may utilize different zones and processes. Vitrification is used to destroy or immobilize hazardous waste by exposure to high temperatures, leading to the rejection or entrainment of contaminants within the glass matrix. The process reduces or eliminates pretreatment requirements, increases waste load capacity, and reduces maintenance costs compared to other hazardous waste treatment and storage methods. While some hazardous waste treatment and storage methods are only suitable for a single waste type or classification, vitrification can be applied to a wide range of hazardous materials. Vitrified glass has a high waste load capacity and is considered stable.
[0030]
[0057] In some embodiments, the vitrification process used is In-Container Vitrification (ICV™). In-Container Vitrification (ICV™) processing is similar to conventional vitrification. The difference is that the entire vitrification process and subsequent storage of the vitrification process product occurs within the same container, thus reducing the equipment and steps required for final processing. The container used in the vitrification process may be a sealed arc furnace, a joule heated melter, or other type of sealed furnace or melter. In this document, a system in which a vitrification containment vessel is used is referred to as a Vitrification Containment System (VCS). The VCS comprises a vitrification containment vessel, at least one electrode, and a lid for sealing the top of the vitrification containment vessel. The lid or vent chamber comprises one or more outlets (hereinafter referred to as "electrode seal assemblies") through which one or more electrodes are routed into the vitrification containment vessel. The electrode seal assembly may provide one of thermal and electrical insulation for the electrodes in some embodiments. The electrode seal assembly, in some embodiments, may provide pressure and gas / air flow isolation for the electrode from the surrounding hood. The electrode seal assembly, in some embodiments, may provide an atmospheric seal under different pressure conditions.
[0031]
[0058] Continuing with the embodiment of FIG. 1, off-gas from the vitrification process may be pre-treated in off-gas pre-treatment process 120 (zone 2). Cooling process 130 (zone 3) is an optional step and can be used if there is a need to reduce the temperature of the off-gas. The off-gas may contain substances that are considered harmful to the environment. Off-gas wet scrubbing 140 (zone 4) may utilize wet scrubbers to decontaminate the off-gas, combustion gases, and other gases including various pollutants. After off-gas wet scrubbing process 140, the off-gas may proceed to further conditioning in off-gas final conditioning process 150 (zone 5) based on output requirements including meeting ambient discharge requirements. This may include further processing such as moisture removal, residual impurities or particles. Once processing is complete, the off-gas can be released via off-gas exhaust 160 (zone 6). When the off-gas satisfies regulations, it may be released to the environment, reused as waste heat in the process or a separate process, or exhausted for further processing.
[0032] technology
[0033]
[0059] Vitrification container - Vitrification container refers to the container in which the electrodes are inserted and vitrification takes place. In some embodiments, the electrode seal assembly is coupled to the lid of the vitrification container to facilitate the insertion of the electrode.
[0034]
[0060] Electrode - Electrode refers to an electrical conductor used to contact non-metallic parts of the circuit. The electrode transfers energy to the interior of the vitrification vessel to facilitate vitrification of the material therein. An embodiment of an electrode is depicted in Figure 2. Electrode is generally a generic term for various embodiments of electrode seal assembly designs.
[0035]
[0061] Electrode Seal Assembly (also referred to as Seal Assembly or Lead-Out) - Electrode seal assembly refers to the complete assembly including the electrode seal housing, sealing ring, other fasteners and gaskets that form each embodiment. The electrode seal assembly for a high temperature vitrification containment vessel has a primary purpose of preventing gases from escaping the process containment vessel and a secondary purpose of providing a guide for inserting the electrode into the molten environment. One or more components that form any embodiment of the electrode seal assembly may have one or more chamfered edges to facilitate electrode insertion and minimize the possibility of shavings shearing off the electrode.
[0036]
[0062] Seal Housing - The term seal housing refers to one or more of the main structural components of the electrode seal assembly. The seal housing contains the sealing ring and serves as insulation between the electrode and other conductive components and is bonded to the vitrification vessel lid.
[0037]
[0063] Electrode seals, also referred to as graphite seals, sealing rings, seals - this term refers to individual sealing rings and not the entire electrode seal assembly. Embodiments of sealing rings are depicted in Figures 3A-3C. The depicted sealing rings are used throughout the depicted electrode seal assembly embodiments, although other sealing ring embodiments are also available. In some embodiments, the sealing rings may include at least 95% carbon content.
[0038]
[0064] Sealing Section - A sealing section refers to a separate area within the seal housing where one or more sealing rings are located. Each sealing section may include one or more sealing rings. Each seal housing may include one or more sealing sections. The need for sealing section embodiments is discussed further below in this disclosure.
[0039] Electrodes and Seals
[0040]
[0065] FIG. 2 depicts an embodiment of an electrode 250. The length of the electrode 250 is generally greater than its diameter. In some embodiments, one end of the electrode 250 is tapered 251. The tapered end 251 facilitates alignment of the electrode 250 during insertion into the electrode seal assembly and vitrification containment vessel. One or more electrodes 250 may be inserted into the electrode seal assembly and fed into the vitrification containment vessel as the melt deepens, keeping the end of the electrode 251 at or near the bottom of the melt region. This requires that a portion of the electrode 250 extend above the vitrification containment vessel early in the melting process.
[0041]
[0066] Since longer electrodes 250 are more likely to break due to the increased moment arm, in some embodiments the electrodes 250 may be threaded to allow shorter sections to be added incrementally. Typically the smaller electrodes 250 are male / female and the larger electrodes 250 are female / male and may be attached using a dual threaded male nipple. The male end of the electrode 250 is typically fully threaded, while the female end may only be threaded to a minimum shell thickness. At the junction of the smaller diameter male / female electrode 250 section there is a gap created by the threads.
[0042]
[0067] Graphite electrodes are commonly used in arc furnaces due to their excellent electrical and thermal conductivity, high temperature strength, and low thermal expansion. Graphite is the preferred electrode material, but other materials are considered, including both consumable and non-consumable electrode materials. Although graphite electrodes are commonly used for vitrification, there are several aspects that can be problematic. A common problem with graphite electrodes 250 is that they produce small shavings that sometimes cut off the electrode 250 at the top of the vitrification chamber and electrode seal assembly. These shavings can create electrical arc potentials, solutions of which embodiments are discussed later in this disclosure. The electrodes 250 may be conductive, heat resistant, and corrosion resistant.
[0043]
[0068] 3A-3C depict different views of an embodiment of an electrode seal 200 (also referred to as a "seal," "sealing ring," or "graphite seal"). These terms refer to individual sealing rings and not to the entire electrode seal assembly. Each electrode seal assembly may include one or more sealing rings. Sealing ring is generally a generic term for various embodiments of electrode seal assemblies. In some embodiments, one or more sealing rings 200 may be made from graphite. Graphite sealing rings 200 are preferred because graphite is heat resistant, oxidation resistant, wear resistant, and has a low coefficient of friction, although other materials may be used. In embodiments utilizing more than one sealing ring 200, each sealing ring 200 may be made from a different material or may be made from the same material.
[0044]
[0069] In some embodiments, the sealing ring 200 may be covered with a material that forms a thick, stable passivating oxide layer when exposed to heat and pressure, which protects the surface of the sealing ring 200 from degradation. In some embodiments, the sealing ring 200 is covered with an austenitic nickel-chromium based material. In some embodiments, one or more of the sealing rings 200 may be covered with Inconel. In some embodiments, the Inconel is wrapped around the outer circumference of the sealing ring 200 in a spiral fashion. The Inconel enhances corrosion resistance and rigidity at high temperatures. The sealing ring 200 may be made from a material (e.g., graphite) that is suitable for handling extreme environments, including extreme heat and pressure, in some embodiments utilizing more than one sealing ring 200.
[0045]
[0070] In some embodiments, the aforementioned gaps present in the rod sections may be passed through the seal assembly without losing the seal on the electrode, in other words, at least one sealing ring 200 or sealing section is fully engaged around the electrode at any given time.
[0046] For example, if there are two sealed sections, the electrode gap can pass through one sealed section while the other remains fully engaged. The more sealed sections there are, the higher the safety factor.
[0047]
[0071] Since the same force is applied over a smaller inner surface 208 area and higher pressure results in enhanced sealing effectiveness, the sealing ring 200 in some embodiments is manufactured with chamfered inner edges 201 as shown in FIG. 3A. In some embodiments, the sealing ring 200 has dragged cuts, or splits, or edges that allow them to shrink and tighten around the electrode under induced pressure on the outer surface 207. One or more of the sealing rings 200 may have one or both inner ring sides chamfered to facilitate movement of the rod down the seal housing and reduce the incidence of chips shearing off the electrode. In some embodiments, only the inner surface of the top or bottom edge of the sealing ring 200 is chamfered.
[0048] Electrode Seal Assembly Embodiments
[0049]
[0072] The following section discusses several seal assembly embodiments. No order of description implies priority. It will be apparent that, although each embodiment is considered as a separate whole from the other embodiments, one or more of the embodiments may be combined to form other embodiments not expressly disclosed herein.
[0050]
[0073] In some embodiments, the seal may be reinforced by a positive gas pressure curtain barrier and / or multiple mechanical seals. In some embodiments utilizing a pressure seal, the air or inert gas used to create the pressure seal may be heated or cooled depending on the material being vitrified and other system variables. In some embodiments utilizing a pressure seal, one or more sensors, regulators, and / or valves may be used to monitor and control the flow within the seal assembly. In some embodiments, gas escaping past the seal may be siphoned off for recycling to the vitrification containment vessel.
[0051]
[0074] In an exemplary embodiment, the sealing system includes two or more electrodes and a vitrification container. A lid is attached to the vitrification container to form a sealed vitrification container. The two or more electrodes are operatively positioned through the lid and extend down into the vitrification container. In this exemplary embodiment, the two or more electrode seal assemblies are attached to the lid. The two or more electrode seal assemblies may, in some embodiments, provide at least one of thermal and electrical insulation for the two or more electrodes. The two or more electrode seal assemblies may provide a method for the vitrification system to isolate the external environment from conditions inside the lid or the off-gas vent chamber while simultaneously allowing penetration of the electrodes into and out of the vitrification zone. The two or more electrode seal assemblies each include a housing, where the housing includes two halves and a ring groove recessed within the housing. A sealing ring with a split portion may be disposed in the groove, such that an outer surface of the sealing ring is recessed into the ring groove. The system also includes gas passages, which may be cast or machined into the housing such that they are adjacent to two or more ring grooves. The gas passages distribute gas evenly from the inner surface of the ring groove to the outer surface of the sealing ring. The distributed gas creates a pressure change that causes the sealing ring to compress over the electrode to form a seal.
[0052]
[0075] 4A-4G depict an embodiment of an electrode seal assembly 300.
[0053]
[0076] FIG. 4A depicts an isometric view of an embodiment of an electrode seal assembly 300. The electrode seal assembly 300 includes a seal housing 310, a housing gasket 350, two split gaskets 355, and one or more hose fittings 325, 320 (FIG. 4B). In some embodiments, such as the embodiment depicted in FIGS. 4A-4G, the seal housing 310 is split into halves in a "clamshell" design. In some embodiments, the seal housing 310 is split into more sections. In some embodiments, the sections of the seal housing 310 are identical. The clamshell design of the seal housing 310 allows for easy maintenance and replacement. The sections of the seal housing 310 may be fastened together using fasteners. A split gasket (not shown) may be disposed between each of the sections of the seal housing 310. In some embodiments, the split gasket may be made of graphite, or other thermally and / or electrically insulating materials, or a combination thereof. In some embodiments, the split gasket may be constructed from rope sealant, heat resistant fabric, or other materials capable of withstanding high heat (greater than about 500° C. in some embodiments) and providing a seal to prevent leakage. In some embodiments, one or more gaskets may be formed from graphite with a stainless steel core.
[0054]
[0077] 4B depicts the top of the electrode seal assembly 300. The depicted bolt holes 364 may be used to secure the electrode seal assembly 300 to the top of a vitrification vessel. In the depicted embodiment, there are four bolt holes 364, but the number of bolt holes can vary depending on many factors such as the size of the electrode seal assembly 300, the type and size of fasteners, to name a few. Hose fittings 325, 320 may be used to supply and release pressure around the seal using air or other inert gas.
[0055]
[0078] FIG. 4C depicts a front view of the electrode seal assembly 300. In the depicted embodiment, the electrode seal assembly 300 is comprised of two identical seal housings 310. The two seal housings 310 are fastened together using a number of fasteners that can vary between embodiments. The electrode seal assembly 300 includes a flange 362 that rests on top of a vitrification containment vessel. The flange 362 includes a hole 364 (FIG. 4D) through which the electrode seal assembly 300 may be attached to the vitrification containment vessel. A housing gasket 350 may be located between the flange 362 and the vitrification containment vessel. The flange 362 of the seal housing 310 is fastened to the top cover of the vitrification containment vessel. In some embodiments, the seal housing 310 may be comprised of ceramic, graphite, Macol™, CS-85, other thermally and / or electrically insulating materials, or combinations thereof. Other seal housing materials may be used. Housing gasket 350, in some embodiments, may be constructed from graphite with a stainless steel core.
[0056]
[0079] 4D depicts a bottom view of the electrode seal assembly 300. In the depicted embodiment, gas passages 330 are drilled through the base of the electrode seal assembly 300. The depicted embodiment includes eighteen evenly distributed vertical gas passages 330, although other quantities and configurations are possible. The gas passages 330 are shown and described in more detail in FIGs. 4H and 4I.
[0057]
[0080] FIG. 4E depicts an isometric view of one half of the seal housing 310. The ring grooves 375 inside the seal housing 310 are designed to hold and secure the sealing ring 200 (FIGS. 4G, 4H) in place. In the depicted embodiment, there are four ring grooves 375, but other embodiments may include other quantities. In some embodiments, one or more of the ring grooves 375 may be sized to accommodate two or more sealing rings 200. In some embodiments, the ring grooves 375 include a pressure groove 376 that can create a pressure seal for gas flow around the sealing ring 200 (FIGS. 4F, 4G).
[0058]
[0081] The depicted embodiment 300 uses pressurization to reinforce and tighten the sealing ring 200 around the electrode 250. Each sealing ring 200 is seated within a ring groove 375 to secure it in place. In some embodiments, such as the embodiment depicted in FIGS. 4F-4G, one or more of the ring grooves 375 include an additional pressurization groove 376 through which pressurized air and / or inert gas may act on the sealing ring 200. The pressurization may be achieved by introducing air and / or inert gas into the seal housing 310. Pressure is supplied to the seal housing 310 via a hose fitting 325, which passes through gas passages or cavities in each of the seal housing sections 310 to the sealing ring 200.
[0059]
[0082] 4A-4G, the cavity, or gas passage, 330 in the electrode seal assembly 300 may be machined or cast. The gas passage 330 is adjacent to the ring groove 375 and allows air or inert gas to be evenly distributed around the seal housing 310 and sealing ring 200. The pressurized air or inert gas pressurizes the exterior surfaces 208 (FIG. 3A) of the sealing ring 200, compressing them around the electrode 250.
[0060]
[0083] FIG. 4G depicts a cross-sectional view of the seal housing 310. Each ring groove 375 has a hole inlet 340 through which pressurized air and / or inert gas may be added to the sealing ring. These hole inlets 340 allow pressure to be evenly distributed along the exterior surface of each sealing ring 200. The ability to control the pressure within the electrode seal assembly 300 allows for precise electrode feed rates, tighter sealing rings 200, high system reliability, and the ability to gradually move the electrode 250 up and down. High pressure allows the sealing ring 200 to seal and lock the electrode 250 in place as needed. High pressure sealing reduces off-gassing. In some embodiments, the operating range of air pressure is 5-10 psi, but may be increased to 20-30 psi. The pressure change may be maintained with the addition of more air or inert gas such that the resulting compression pressure increases the pressure within the vitrification containment system during operation.
[0061]
[0084] Figures 5A-5E depict an embodiment of an electrode seal assembly 400. Figures 5A-5E utilize a pressure seal similar to the pressure seal depicted and described in Figures 4A-4G.
[0062]
[0085] 5A depicts an isometric view of electrode seal assembly 400. In the depicted embodiment, seal housing 410 is split in half in a clamshell design. In some embodiments, seal housing 410 may comprise three or more parts. In the depicted embodiment, the two halves of seal housing 410 are fastened together with fasteners via holes 405. The two halves of seal housing 410 clamp around electrode 250 and sealing ring 200 (FIG. 5B).
[0063]
[0086] FIG. 5B depicts an exploded isometric view of the electrode seal assembly 400. The depicted embodiment includes a housing seal 410 split into two pieces, four sealing rings 200, and fasteners (not depicted). The electrode seal assembly 400 allows for a longer overall length of the seal housing 410 which extends into the vitrification containment vessel lid and allows for a longer distance between the sealing rings 200. The extended length of the seal housing 410 seals a larger surface area of the electrode 250 and provides additional electrical insulation between the electrode 250 and the vitrification vessel. Additionally, the longer distance between the sealing rings 200 maintains at least one engaged sealing ring 200 at all times while allowing gaps (if any) between the electrode 250 segments to pass through the sealing ring 200. Some embodiments may use more or less sealing rings 200. In some embodiments, one or more of the sealing rings 200 may be identical.
[0064]
[0087] FIG. 5C illustrates a cross-sectional view of the electrode seal assembly 400. The illustrated embodiment of the electrode seal assembly 400 uses high pressure sealing to reinforce and clamp the sealing ring 200 around the electrode 250. Each sealing ring 200 is seated in a ring groove 475 (FIG. 5D) to secure it in place. In some embodiments, one or more ring grooves 475 (FIG. 5D) may be sized to accommodate one or more sealing rings 200. The high pressure sealing may be achieved by introducing air and / or an inert gas into the seal housing 410. Pressure is supplied to the seal housing 410 through a hose fitting and passes through gas passages 430 or cavities in each seal housing section 410 to the sealing rings 200. The cavities, or gas passages, 430 in the electrode seal assembly 400 may be machined or cast. Vertical gas passages 430 are connected to the ring grooves via holes 420 (FIG. 5D) and allow air or inert gas to flow around the seal housing 410 and sealing ring 200. The pressurized air or inert gas pressurizes the outer surfaces of the seals around the electrode 250, compressing them around the electrode 250.
[0065]
[0088] FIG. 5D illustrates how air pressure is provided through holes 420 in the ring grooves 475 in the seal housing 410. Each ring groove 475 has holes 440 through which pressurized air or inert gas can enter and exit the electrode seal assembly 400. The ability to control the pressure in the electrode seal assembly 400 allows for more precise electrode feed rates, tighter sealing rings 200, and higher system reliability. If necessary, higher pressure allows the sealing rings 200 to tightly lock the electrodes in place. High pressure sealing reduces off-gassing. The operating range for air pressure is 5-10 psi, but may be increased to 20-30 psi. The pressure change may be maintained with additional air or inert gas so that the resulting compression pressure is greater than the pressure in the vitrification vessel during operation.
[0066]
[0089] 5E depicts a bottom view of the electrode seal assembly 400 and shows the vertical gas passages 430. In the depicted embodiment, there are 22 vertical gas passages. Other embodiments may include a different amount of vertical gas passages. In some embodiments, such as the depicted embodiment, the vertical gas passages 430 are evenly distributed.
[0067]
[0090] 6A and 6B depict an embodiment of an electrode seal assembly 500.
[0068]
[0091] FIG. 6A depicts an electrode seal assembly 500 that includes an upper seal housing 520, an electrode collar 510, and one or more sealing rings 200. The electrode collar 510 fits over the electrode 250 (FIG. 6B) and is partially inserted into the top of the vitrification container. The electrode collar 510 includes a flange 511 that rests on the top of the vitrification container. A graphite sealing ring 200 then fits over the electrode 250 and rests on top of the electrode collar 510. The upper seal housing 520 then fits over the sealing ring 200 to complete the electrode seal assembly 500. The electrode seal assembly 500 may be fastened together and / or to the top of the vitrification container.
[0069]
[0092] 6B depicts a cross-sectional view of the electrode seal assembly 500. One or more fastener holes 505 may be used to fasten the upper seal housing 520 to the electrode collar 510 and may be used to fasten the electrode seal assembly 500 to the top of the vitrification vessel. The depicted embodiment includes four seal rings 200. In some embodiments, such as the depicted embodiment, the inner seal ring 200 may be a flat graphite seal ring and the outer seal ring 205 may be an Inconel wrapped graphite seal ring 200. In some embodiments, the Inconel is spiral wrapped. This embodiment has been tested and found to maintain good vacuum.
[0070]
[0093] 7A-7D depict an embodiment of an electrode seal assembly 600. FIG.
[0071]
[0094] 7A-7D, starting from the base, the housing seal 650 may be placed between the vitrification container lid and the bottom of the electrode seal assembly 600. The bottom seal housing 620 may be flanged, with the flange resting on top of the housing seal 650, and the remainder of the bottom seal housing 620 inserted into the top of the vitrification container. A bolt hub 610 may be connected to the bottom of the bottom seal housing 620 with a bolt hub gasket 625 in some embodiments, fastening the electrode seal assembly 600 together. The first seal ring 200 is held in place against the bottom of the bottom seal housing by the bolt hub 610. The second seal ring 200 fits into a groove in the top of the bottom seal housing 620. Ring 630 fits between the second seal ring 200 and the third seal ring 200. An upper seal housing 605 fits over the second and third sealing rings 200 and ring 630 .
[0072]
[0095] One or more housing gaskets 655 may be disposed between the top of the bottom seal housing 620 and the top seal housing 605. The depicted embodiment includes three housing gaskets. The outer two gaskets 653 may be made from graphite. The center housing gasket 655 may be made from a metal such as stainless steel sandwiched between layers of graphite in some embodiments. The number and composition of the housing gaskets 655 may vary in different embodiments. The fourth sealing ring 200 fits on top of the top seal housing 605 and is held in place by the bolt hub 610. The bolt hub gasket 625 may be disposed between the bolt hub 610 and the top seal housing 605. Fasteners such as bolts may extend through the electrode seal assembly 600 to fasten the components together. In some embodiments, one or more of the top seal housing 605, bottom seal housing 620, bolt hub 610, and ring 630 may be constructed from ceramic or other materials.
[0073] Processing and Control
[0074]
[0096] 8A-8F depict embodiments of vitrification (FIG. 8A) and off-gassing (FIG. 8B-8F) control systems. In these figures, the long thick dotted line (FIG. 8A) represents the frit feed, the double lines (FIGS. 8A and 8B) represent air, the thick lines (FIGS. 8A-8B, 8D-8F) represent off-gassing, the middle lines with small arrows (FIGS. 8B-8D) represent water (FIGS. 8A-8B) including scrub water (FIGS. 8A-8B), the short dotted line (FIG. 8C) represents glycol, the dotted line (FIG. 8D) represents pH adjustment chemicals, and the thick dotted lines (FIGS. 8A-8E) represent electrical or control signals.
[0075]
[0097] FIG. 8A illustrates an embodiment of a vitrification system (Zone 1). The vitrification vessel may comprise one or more layers of insulating material. The illustrated embodiment comprises cast refractory and silica sand. Frit, which may comprise a glass former in some embodiments, may be fed to the top of the vitrification vessel via one or more pressure control valves. In the illustrated embodiment, two pressure control valves PCV-102, PCV-103 have a feed while melting (FWM) airlock control. The FWM airlock control allows additional material to be fed to the vitrification vessel when the amount of previously loaded material decreases during the vitrification process. The airlock provides an air seal in the plenum area so that there is no open path for plenum air to leak to the surroundings. The feed point is connected to a heat shield and a heat shield level control. The electrode may be fed to the vitrification vessel via an electrode level control and an electrode seal assembly.
[0076]
[0098] The depicted process embodiment is powered by a three-phase utility input to a power transformer (a Scott T power transformer in the depicted embodiment). The power transformer may allow for minimal operator interface to accomplish the goal of initiating and providing a heating mechanism for the vitrification process. The output from the power transformer may be initially controlled by an operator input program to gradually increase power to the vitrification zone within the vitrification vessel.
[0077]
[0099] Currently, the vitrification process is manually controlled. The ability to control the process with little or no manual input can improve process efficiency, eliminate required processing time and the potential for human error. Programmed inputs may be utilized to initially control the power ramp-up to initiate the melting process. A software program may be linked to the existing process control system to gradually increase the transformer power output to a nominal operating level on a predefined schedule (timeline). Continuous operation of the system beyond that point may then use logic based on inputs from temperature, pressure, visual (e.g., infrared) and / or other sensory inputs to adjust the power input to a desired level that will operate the process safely and efficiently. Power control may run in parallel with other system control logic that manages off-gas flow, vent vacuum, differential pressure, and other variables throughout the system. Such control systems may be utilized for both Surfaced Plane™ (in situ approach) and In-vessel Vitrification, ICV™, techniques, and other vitrification systems and methods.
[0078]
[0100] In zone 1, plenum sweep air is introduced via line 2 through pressure control valve PCV-101 and through a filter (HEPA in the depicted embodiment). The plenum sweep air is used to remove water vapor and gases generated during vitrification from the off-gas vent chamber and divert them to the off-gas treatment system for treatment before releasing the treated off-gas to the environment. In some embodiments, the removed contaminants may be treated and stored separately.
[0079]
[0101] Referring to FIG. 8B, off-gas enters zone 2 via line 4. It may be joined by balance air, which is introduced via pressure control valve PCV-201 and further through a filter (HEPA in the depicted embodiment). The off-gas (mixed with the balance air in some embodiments) may then proceed through at least one filter. In some embodiments, two or more filters are in parallel. In some embodiments with parallel filters, the flow moves through more than one filter at a time. In some embodiments with parallel filters, the flow only moves through more than one filter at a time and is controlled by a valve.
[0080]
[0102] In the depicted embodiment, the flow may travel through valve HV-201, enter a sintered metal filter (SMF), and exit via valve HV-202. Alternatively, the flow may be directed to a HEPA filter via valve HV-203 and exit via valve HV-204. From one of valves HV-202 and / or HV-204, the flow travels to Zone 4. A water (or other cleaning fluid) rinse may be provided via valve HV-207 to periodically clean captured contaminants from the SMF filter.
[0081]
[0103] Air or fluid may be introduced into the backpulse air reservoir via valve HV-205 and into the SMF via valve HV-206. Backpulse air may flow out of the SMF to the backpulse recycle via valve HV-208. Backpulse air is used to clean the SMF. Backpulse air is blown quickly back into the SMF to knock particulates off the filters and into the bottom of the filter housing where they are collected and sent back to the vitrification vessel for processing. In some embodiments, the filter housing may contain two or more filters, each backpulsed at a different time with small individual pulses to avoid pressurizing the offgas system with a single large backpulse.
[0082]
[0104] Some embodiments may include optional zone 3 depicted in FIG. 8C to cool the water in zone 4 (FIG. 8D). In other embodiments, zone 3 is a requirement rather than an option. Glycol travels in a loop, through a glycol cooler to the first heat exchanger (HX-1), from the bottom of HX-1, through a pump, to the base of the second heat exchanger (HX-2), and back to the glycol cooler. Water flows through heat exchangers HX-1 and HX-2 and back to zone 4 (FIG. 8D).
[0083]
[0105] In the depicted embodiment, the off-gas travels from zone 2 to a tandem venturi scrubber, through a mist eliminator, and to zone 5 as shown in FIG. 8E. Other embodiments may utilize different scrubbing systems including dry scrubbers, electrostatic precipitators, and the like. The tandem venturi scrubber is in the vicinity of a scrub tank. Fresh water may be sent to the scrub tank via valve HV-410. The water leaves the scrub tank and goes to a scrub pump via valve HV-403. Optionally, the water may be exhausted through valve HV-412. The scrub pump may funnel water to a particulate scrub filter via valves HV-404, HV-405. Alternatively, the flow may bypass the particulate scrub filter via valve HV-409. Water may be drawn from the particulate scrub filter via valve HV-406. The off-gas may be exhausted from the particulate scrub filter via valve HV-408. Water leaving the particulate scrub filter via valve HV-407 travels through valves HV-401 and HV-402 to a tandem venturi scrubber. In some embodiments, the water may travel to a scrub tank via valve HV-411. In some embodiments, the pH of the water in the scrub tank is adjusted with pH adjustment chemicals delivered via a chemical pump from a chemical (pH) buffer tank via valve HV-413.
[0084]
[0106] The scrubbed and filtered off-gas from zone 4 (FIG. 8D) may travel through a heater and through one or more series filters. In the depicted embodiment, the heated off-gas travels through valve HV-501 to the first filter, through valves HV-502, HV-504, through other filters and valve HV-505 to zone 6 (FIG. 8F). Alternatively, one or more filters may be bypassed by passing the off-gas through valves HV-503 and / or HV-506. In some embodiments, one or more filters may be in parallel and may be used in combination with the primary filter, but may also be used as a replacement for the primary filter.
[0085]
[0107] Off-gas from zone 5 passes through valve HV-601, through the primary blower and out the stack outlet, or it may pass through valve HV-602 to the secondary blower and further through valve HV-603 for discharge via the stack outlet.
[0086] Other Process Embodiments
[0087]
[0108] A variety of filter types are contemplated, including but not limited to HEPA, SMF, HEGA. A variety of valve types are contemplated. Valves can be varied from the illustrated process diagram for different flow rates and volumes and other design considerations. Additional valves, such as check valves, may be located throughout the system to prevent fluid from moving in the wrong direction. Other valves, including automatic motorized valves or redundant valves, may be included at various points within the process to increase safety factors.
[0088] Sensors
[0089]
[0109] One or more sensors and instruments may be used to monitor and control system characteristics throughout the process. In the embodiment of Figures 8A-8F, several instruments and / or sensors may be included in each zone. Other embodiments may include more or less sensors and / or instruments at other locations throughout the system. The location and type of sensors and / or instruments will depend on the scale of the process, the chemistry of the off-gas, among other design considerations. The type of sensor may include one or more of contact sensors, non-contact sensors, capacitive sensors, inductive sensors, 3D imagers, cameras, thermal imagers, thermometers, pressure sensors, radiation detectors, LIDAR, microphones, among others.
[0090]
[0110] Some embodiments may include one or more imaging sensors. The one or more image sensors may comprise one or more 3D imaging, 2D range sensors, cameras, thermal imagers, radiation detectors, among others. The one or more imaging sensors may be used to test and monitor the performance of the remote operator. Signals from the one or more imaging sensors may be displayed in real time, recorded for later review, and / or recorded for operational documentation. The one or more cameras may be of a fixed or pan-tilt-zoom type. The operator selects and manages the desired camera view for operation, while controlling the cameras with associated control functions such as left-right movement, up-down movement, zoom (PTZ), focus, and light. In some embodiments, an adequate visual operating range may be enabled by the camera system through sufficient camera coverage determined by the quantity and location of the cameras.
[0091]
[0111] In some embodiments, sensors are added solely to track material properties throughout the system. In some embodiments, the sensor data is used to control the operation of the system. Some embodiments may utilize sensor fusion algorithms to analyze data readings from one or more sensors of one or more different types. In some embodiments, the sensor data is automatically analyzed to automatically effect changes in the control system for processes requiring little or no input from a human operator. In some embodiments, the sensor data and analysis is displayed to a human operator to perform manual adjustments.
[0092]
[0112] In the depicted embodiment, Zone 1 (FIG. 8A) includes 19 gauges. In the depicted embodiment, 15 temperature indicators are used to monitor the temperature of the vitrification containment vessel. TI-101 through TI-106 monitor incremental depths of material within the vitrification containment vessel, TI-107 monitors the sand in the northeast (NE) corner, TI-109 monitors the sand in the southwest (SW) corner, TI-110 monitors the sand in the northwest (NW) corner, TI-111 monitors the inner sand, TI-112 monitors the middle sand, TI-113 monitors the outer sand, TI-114 monitors the outer skin, and TI-115 monitors the bottom skin. Additional temperature indicators may be used to monitor temperatures at various other locations. In the depicted embodiment, additional temperature indicating transmitters TI-116, TI-117, TI-118 are used to monitor the temperature of the electrode seal, an infrared (IR) video camera, and the top of the vitrification vessel. A pressure indicating transmitter may be used to monitor the pressure inside the vitrification vessel.
[0093]
[0113] In the depicted embodiment, Zone 2 (FIG. 8B) includes five instruments. A pressure differential indicator transmitter, PDIT-201, is used to measure and transmit the pressure differential across the SMF and / or HEPA filters. A flow indicator transmitter FIT-201 and temperature indicator TI-201 are used to monitor the balance air input. The off-gas temperature is monitored by temperature indicator TI-202 just before the filters and after balance air has been added.
[0094]
[0114] In the depicted embodiment, Zone 4 (FIG. 8D) includes 14 instruments. Flow indicating transmitter FIT-401 and temperature indicating transmitter TI-401 are used to monitor the characteristics of the off-gas entering Zone 4. Pressure differential indicating transmitters PDIT-401 and PDIT-402 are used to monitor the off-gas differential pressure just before and just after the tandem venturi scrubbers and just before and just after the mist eliminator, respectively. Pressure indicating transmitters PIT-401 and 402 monitor the water pressure just before the first tandem venturi scrubber and the second tandem venturi scrubber. Temperature indicating transmitter TI-402, level indicating transmitter LIT-401, and pressure indicating transmitter PIT-403 are used to monitor the scrub tank. The TI-403 Temperature Indicator, PIT-404 Pressure Indicator Transmitter, and FIT-402 Flow Indicator Transmitter are used to monitor the water downstream of the scrub pump. The PDIT-403 Differential Pressure Indicator Transmitter monitors the differential pressure of the water across the particulate scrub filter. The AIT-401 Analyzer Indicator Transmitter is used to connect to the Variable Frequency Drive (VFD) on the scrub tank and chemical pump to monitor the pH and feed pumps that add caustic to the scrub tank.
[0095]
[0115] In the depicted embodiment, Zone 5 (FIG. 8E) includes five instruments. Differential pressure indicator transmitters PDIT-501, PDIT-502 are used to monitor the differential pressure across the first and second filters. Temperature indicators TI-501, TI-502, TI-503 monitor the temperature of the off-gas entering between the heater and the first filter, as well as the temperature of the off-gas after the filters.
[0096]
[0116] In the depicted embodiment, Zone 6 (FIG. 8F) includes four instruments. Temperature indicators TI-601 and TI-602 monitor the temperature of the off-gas entering Zone 6 and the temperature of the exhaust, respectively. Pressure indicator transmitter PIT-601 monitors the pressure of the off-gas before it enters the blower. Flow control transmitter FCT-601 monitors and controls the flow generated by the primary blower using a variable frequency drive. FCT-601 is connected to Zone 1 off-gas vent chamber pressure indicator transmitter PIT-101. As the vacuum in the vent chamber drops, the blower increases speed to increase flow and vacuum.
[0097]
[0117] For convenience, the operations are described as various interconnected functional blocks or separate software modules. Although not necessarily, these functional blocks or modules may be equivalently aggregated into a single logical device, program, or operation with indistinct boundaries. In any case, the functional blocks or software modules or described features may be performed by themselves or in combination with other operations, either in hardware or software.
[0098]
[0118] Having herein described and illustrated the principles of the disclosed systems, methods, processes, and / or apparatus in their preferred embodiments, it will be apparent that the systems, methods, processes, and / or apparatus can be modified in arrangement and detail without departing from such principles, and it is intended that the following claims be construed to cover all such variations and modifications that fall within the spirit and scope of the claims.
Claims
1. An electrode seal assembly for mounting an electrode to a vitrification vessel, comprising: a housing that extends around the electrode when the electrode is inserted through the housing; a first housing section and a second housing section coupled to the first housing section; at least one fastener fastening the first housing section and the second housing section together; two or more annular ring grooves recessed into the housing, the first housing section and the second housing section cooperating to define two or more of the annular ring grooves; a sealing ring received within each of the two or more annular ring grooves; Equipped with an outer surface of each sealing ring recessed into a respective one of the annular ring grooves, and an inner surface of each sealing ring positioned to engage and seal against the electrode when the electrode is inserted through the housing.
2. The electrode seal assembly of claim 1 , wherein the first housing section and the second housing section define a portion of the housing that cooperate to surround the electrode when the electrode is inserted into the housing.
3. The electrode seal assembly of claim 1 , further comprising a seal between the first and second housing sections.
4. The electrode seal assembly of claim 1 , further comprising a seal positioned on an exterior surface of the second housing section to seal the housing to the vitrification container.
5. The electrode seal assembly of claim 1 , wherein the sealing ring is movable to clamp the sealing ring around the electrode when the electrode is inserted through the housing.
6. The electrode seal assembly of claim 1 , further comprising a bore defined in the housing through which the annular ring groove is pressurized.
7. The electrode seal assembly of claim 1 , wherein the first housing section has an annular flange by which the first housing section is fastened to the second housing section.
8. The electrode seal assembly of claim 1 , wherein the first and second housing sections each have an annular flange by which the first and second housing sections are fastened to one another.
9. The electrode seal assembly of claim 8 , wherein the annular flange extends outwardly for support on the vitrification vessel.
10. 1. A method of sealing an electrode to a vitrification vessel, comprising: inserting a first sealing ring into a first annular ring groove defined in an inner surface of the housing; inserting a second sealing ring into a second annular ring groove defined in the inner surface of the housing, the first annular ring groove being defined in both a first section and a second section of the housing; fastening a first section of the housing to a second section of the housing to define a passageway through the housing; receiving the electrode in the passage; engaging the first sealing ring against the electrode at a first location along the electrode; engaging the second sealing ring against the electrode at a second location along the electrode; sealing the first sealing ring to the electrode at the first location; sealing the second sealing ring to the electrode at the second location; A method for sealing an electrode comprising:
11. fastening the housing to the vitrification vessel; sealing the housing to a surface of the vitrification container; The method of claim 10 further comprising:
12. The method of claim 10 further comprising the step of sealing the first section of the housing to the second section of the housing.
13. The method of claim 10 further comprising the step of clamping the sealing ring against an outer surface of the electrode.
Citation Information
Patent Citations
Electricity-supply pole sealing device of preform vitrification stove
CN203672150U
Sealing device for sealing around an electrode for steelmaking furnace -
JP1984108185U
Method and apparatus for dissolving treated substance
JP2007530262A
Waste vitrification melter
US5643350A
Sealing device
WO2011015712A1