Thin film capacitor and its manufacturing method
The thin film capacitor design addresses crack issues during singulation by positioning insulating resin layers and terminal electrodes to disperse stress, ensuring structural reliability and minimizing damage during the singulation process.
Patent Information
- Application Number
- JP2021067252
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-04-12
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2041-04-12
AI Technical Summary
Thin film capacitors face issues with cracks during singulation due to stress concentration at the edges of the capacitor layer, insulating resin layer, and terminal electrode, leading to structural weaknesses.
The thin film capacitor design includes a supporting material with a capacitor layer, insulating resin layers positioned to cover the capacitor layer edges, and terminal electrodes located outside the resin layer edges, dispersing stress concentration points and reducing the likelihood of cracks during singulation.
The design effectively minimizes cracks during singulation, maintaining structural integrity and ensuring reliable performance by dispersing stress concentrations, thus protecting the internal elements from damage.
Smart Images

Figure 0007569258000001 
Figure 0007569258000002 
Figure 0007569258000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a thin film capacitor and a method for manufacturing the same, and more particularly to a thin film capacitor having a rewiring layer that connects a capacitor layer and a terminal electrode, and a method for manufacturing the same. [Background technology]
[0002] Circuit boards on which ICs are mounted normally have decoupling capacitors to stabilize the potential of the power supply supplied to the IC. Multilayer ceramic chip capacitors are generally used as decoupling capacitors, and the necessary decoupling capacitance is ensured by mounting a large number of multilayer ceramic chip capacitors on the surface of a circuit board.
[0003] However, in recent years, there has been a shortage of space on a circuit board for mounting a large number of multilayer ceramic chip capacitors, and as a result, thin film capacitors that can be embedded in a circuit board are sometimes used instead of multilayer ceramic chip capacitors (see Patent Document 1).
[0004] The thin film capacitor described in Patent Document 1 has a rewiring layer that connects a capacitor layer and a terminal electrode. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2018-137310 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, depending on the positional relationship between the outer edge of the capacitor layer, the outer edge of the insulating resin layer on which the redistribution layer is formed, and the outer edge of the terminal electrode, internal cracks may occur due to stress applied during individualization.
[0007] SUMMARY OF THE PRESENT EMBODIMENTS Accordingly, an object of the present invention is to provide a thin film capacitor having a structure in which cracks are unlikely to occur during singulation, and a method for manufacturing the same. [Means for solving the problem]
[0008] The thin film capacitor according to the present invention comprises a support material, a capacitor layer provided on the support material and consisting of a plurality of electrode layers and a plurality of dielectric layers alternately stacked, a first redistribution layer provided on a first insulating resin layer covering the capacitor layer, a second redistribution layer provided on a second insulating resin layer covering the first redistribution layer, and a terminal electrode connected to the second redistribution layer, wherein the peripheral edge of the first insulating resin layer is located outside the peripheral edge of the capacitor layer, and the peripheral edge of the terminal electrode is located outside the peripheral edge of the first insulating resin layer.
[0009] According to the present invention, when the support material is pushed through and separated into individual pieces using a blade, the fulcrum positions at which stress is concentrated are dispersed, making it difficult for cracks to occur during separation.
[0010] The thin-film capacitor according to the present invention may further include a passivation layer made of an inorganic insulating material provided between the capacitor layer and the first insulating resin layer, which makes it difficult for cracks to occur in the passivation layer during singulation.
[0011] In the present invention, the terminal electrodes may be inclined near the outer peripheral edge so that the distance between the terminal electrodes and the substrate becomes shorter as the terminal electrodes approach the outer peripheral edge. In this way, stress is concentrated at the outer peripheral edge of the terminal electrodes during singulation. As a result, cracks are likely to occur in the second insulating resin layer at this position, and the inside of the element located away from the outer peripheral edge of the terminal electrodes is protected.
[0012] In the present invention, the distance from the outer peripheral edge of the first insulating resin layer to the outer peripheral edge of the terminal electrode may be 10 μm or more, which disperses the fulcrum positions at which stress is concentrated, making it more difficult for cracks to occur during singulation.
[0013] In the present invention, the outer peripheral edge of the first insulating resin layer may be covered with a dummy pattern of the first rewiring layer, so that the characteristics do not change even if stress is applied to the dummy pattern. Effect of the Invention
[0014] As described above, according to the present invention, it is possible to provide a thin film capacitor having a structure in which cracks are unlikely to occur during singulation, and a method for manufacturing the same. [Brief description of the drawings]
[0015] [Figure 1] FIG. 1 is a schematic plan view of a thin film capacitor 1 according to an embodiment of the present invention. [Diagram 2] 2(a) is a schematic cross-sectional view taken along line AA shown in FIG. 1, and FIG. 2(b) is a schematic cross-sectional view taken along line BB shown in FIG. [Diagram 3] FIG. 3 is a schematic cross-sectional view taken along line CC shown in FIG. [Figure 4] FIG. 4 is a schematic cross-sectional view for illustrating a method for dividing the thin film capacitor 1 into individual pieces. [Diagram 5] FIG. 5 is a schematic plan view of a thin film capacitor 1A according to a first modified example. [Figure 6] FIG. 6 is a schematic plan view of a thin film capacitor 1B according to a second modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings.
[0017] Fig. 1 is a schematic plan view of a thin-film capacitor 1 according to an embodiment of the present invention. Also, Fig. 2(a) is a schematic cross-sectional view taken along line AA shown in Fig. 1, Fig. 2(b) is a schematic cross-sectional view taken along line BB shown in Fig. 1, and Fig. 3 is a schematic cross-sectional view taken along line CC shown in Fig. 1.
[0018] As shown in Figures 1 to 3, the thin film capacitor 1 according to this embodiment comprises a support material 10, a capacitor layer 20 provided on the surface of the support material 10, a passivation layer 30 covering the capacitor layer 20, insulating resin layers 31, 32 covering the passivation layer 30, redistribution layers 41, 42 provided on the surfaces of the insulating resin layers 31, 32, respectively, and terminal electrodes 51, 52 connected to the redistribution layer 42.
[0019] The support material 10 is made of a high melting point metal such as nickel (Ni) and functions as a support for ensuring the mechanical strength of the thin film capacitor 1 according to this embodiment, and also functions as a part of the electrode layer of the capacitor. However, it is not essential for the present invention that the support material 10 is a part of the electrode layer. It is also not essential that the support material 10 is made of a conductive material, and it may be, for example, a film made of an insulating material.
[0020] The capacitor layer 20 has a structure in which electrode layers 21, 22 made of nickel (Ni) or the like are alternately stacked with dielectric layers 23 interposed therebetween. In the example shown in Fig. 2, the capacitor layer 20 is composed of three electrode layers 21, three electrode layers 22, and six dielectric layers 23, but the number of layers of these electrode layers 21, 22 and dielectric layers 23 is not particularly limited.
[0021] The dielectric layer 23 is made of, for example, a perovskite-based dielectric material. Examples of perovskite-based dielectric materials include BaTiO3 (barium titanate), (Ba 1-X Sr X )TiO3 (barium strontium titanate), (Ba 1-X Ca X )TiO3, PbTiO3, Pb(Zr X Ti 1-X)O3 and other (ferro)electric materials with perovskite structure, such as Pb(Mg 1 / 3 Nb 2 / 3 )O3 and other composite perovskite relaxor-type ferroelectric materials, and Bi4Ti3O 12 , Bismuth layer compounds such as SrBi2Ta2O9, (Sr 1-X Ba X )Nb2O6, PbNb2O6, and tungsten bronze type ferroelectric materials are examples. Here, in the perovskite structure, perovskite relaxor type ferroelectric materials, bismuth layered compounds, and tungsten bronze type ferroelectric materials, the A site to B site ratio is usually an integer ratio, but may be intentionally deviated from the integer ratio in order to improve characteristics. Note that, in order to control the characteristics of the dielectric layer 23, the dielectric layer 23 may contain additive substances as subcomponents as appropriate. The dielectric layer 23 is sintered, and its relative dielectric constant (ε r ) is, for example, 100 or more. The higher the relative dielectric constant of the dielectric layers 23, the more preferable it is, and there is no particular upper limit. The thickness of each dielectric layer 23 is, for example, about 10 nm to 1000 nm.
[0022] The passivation layer 30 is made of an inorganic insulating material such as silicon oxide (SiO2), and covers the entire surface of the capacitor layer 20 except for the connection portion to the rewiring layer 41. The passivation layer 30 is relatively brittle, and is therefore prone to cracks due to stress.
[0023] The insulating resin layer 31 is made of an organic insulating material and covers the capacitor layer 20 via the passivation layer 30. As shown in FIG. 1 and FIG. 3, the outer peripheral edge of the insulating resin layer 31 is located outside the outer peripheral edge of the capacitor layer 20 (the edge side of the chip constituting the thin film capacitor). As a result, the insulating resin layer 31 has a portion that overlaps with the capacitor layer 20 in a planar view and a portion that does not overlap with the capacitor layer 20. Here, the outer peripheral edge of the capacitor layer 20 refers to the outer peripheral edge of the portion that functions as a capacitor. In other words, when some layers of the electrode layers 21, 22 close to the support material 10 are not connected to the terminal electrodes 51, 52 and do not function as a capacitor, the portion consisting of these electrode layers 21, 22 and the dielectric layer 23 located between them does not constitute the capacitor layer 20, and the portion consisting of the electrode layers 21, 22 connected to the terminal electrodes 51, 52 and the dielectric layer 23 located between them constitutes the capacitor layer 20. The reason why the electrode layers 21, 22 located in the lower layers are not connected to the terminal electrodes 51, 52 is because the film quality of the dielectric layer 23 located in the lower layer is unstable. Therefore, a capacitor layer 20 is formed by the electrode layers 21 and 22 located in the upper layers and the dielectric layer 23 located therebetween.
[0024] A rewiring layer 41 made of a metal such as Cu is provided on the surface of the insulating resin layer 31. The rewiring layer 41 has a portion connected to the electrode layer 21 through a via hole provided in the capacitor layer 20, and a portion connected to the electrode layer 22 through a via hole provided in the capacitor layer 20. FIG. 2(a) shows the rewiring layer 41 connected to the electrode layer 22, and FIG. 2(b) shows the rewiring layer 41 connected to the electrode layer 21. As shown in FIG. 3, the peripheral portion of the rewiring layer 41 forms a dummy pattern 41D, and is separated in-plane from the portion connected to the electrode layers 21 and 22. As a result, the peripheral edge of the insulating resin layer 31 is covered by the dummy pattern 41D of the rewiring layer 41.
[0025] The rewiring layer 41 is covered with an insulating resin layer 32. The insulating resin layer 32 is made of the same organic insulating material as the insulating resin layer 31. In this embodiment, the outer peripheral edge of the insulating resin layer 32 coincides with the side surface 12 of the support material 10 in plan view.
[0026] A redistribution layer 42 made of a metal such as Cu is provided on the surface of the insulating resin layer 32. The redistribution layer 42 has a portion connected to the electrode layer 21 via the redistribution layer 41, and a portion connected to the electrode layer 22 via the redistribution layer 41. Fig. 2(a) shows the redistribution layer 42 connected to the electrode layer 22, and Fig. 2(b) shows the redistribution layer 42 connected to the electrode layer 21.
[0027] The rewiring layer 42 is covered with terminal electrodes 51, 52 made of a metal such as Cu. The terminal electrode 51 is connected to the electrode layer 21 via the rewiring layers 42, 41, and the terminal electrode 52 is connected to the electrode layer 22 via the rewiring layers 42, 41. When the dummy pattern 41D is in contact with the support material 10 made of a conductive material and the support material 10 functions as a part of the electrode layer, the dummy pattern 41D and the terminal electrode 51 or 52 are electrically connected to each other. As shown in FIG. 1 and FIG. 3, the outer peripheral edges of the terminal electrodes 51, 52 are located outside the outer peripheral edge of the insulating resin layer 31. As a result, the terminal electrodes 51, 52 have a portion that overlaps with the insulating resin layer 31 and a portion that does not overlap with the insulating resin layer 31 in a plan view.
[0028] The above is the structure of the thin film capacitor 1 according to this embodiment. Next, a method for manufacturing the thin film capacitor 1 according to this embodiment will be described.
[0029] First, an assembly substrate made of nickel (Ni) or the like is prepared. The assembly substrate is a substrate for obtaining a large number of thin film capacitors 1, and corresponds to the support material 10 before cutting. Next, the dielectric layer 23 and the electrode layers 21, 22 are alternately laminated on the surface of the assembly substrate by using a method such as sputtering, and then via holes for connection are formed, and the electrode layers 21, 22 and the dielectric layer 23 in the peripheral region are removed to form the capacitor layer 20. Next, the dielectric layer 23 is sintered by firing.
[0030] Next, a passivation layer 30 is formed on the entire surface of the capacitor layer 20 by sputtering or the like. Next, the passivation layer 30 in the portion corresponding to the via hole is removed by patterning, and then an insulating resin layer 31 is formed on the entire surface. Next, a via hole is provided in the insulating resin layer 31, and the insulating resin layer 31 in the peripheral region is removed. At this time, patterning is performed so that the peripheral edge of the insulating resin layer 31 is positioned outside the peripheral edge of the capacitor layer 20.
[0031] Next, a rewiring layer 41 is formed on the surface of the insulating resin layer 31. As a result, a part of the rewiring layer 41 is connected to the electrode layer 21 through the via hole, and the remaining part of the rewiring layer 41 is connected to the electrode layer 22 through the via hole. Next, an insulating resin layer 32 is formed to cover the rewiring layer 41, and then a via hole that exposes the rewiring layer 41 is formed in the insulating resin layer 32. Next, a rewiring layer 42 is formed on the surface of the insulating resin layer 32. As a result, a part of the rewiring layer 42 is connected to the electrode layer 21 through the rewiring layer 41, and the remaining part of the rewiring layer 42 is connected to the electrode layer 22 through the rewiring layer 41.
[0032] Next, the terminal electrodes 51, 52 are formed on the surface of the rewiring layer 42 by electrolytic plating or the like. At this time, the position of the plating resist is adjusted so that the outer peripheral edges of the terminal electrodes 51, 52 are positioned outside the outer peripheral edge of the insulating resin layer 31. Then, as shown in FIG. 4, the assembly substrate 10a and the insulating resin layer 32 are pressed through with a blade 60 to separate into a plurality of thin-film capacitors 1. At this time, stress is applied to each part of the thin-film capacitor 1 by the pressure of the blade 60. The stress applied at this time is particularly concentrated at position P1 of the outer peripheral edge of the capacitor layer 20, position P2 of the outer peripheral edge of the insulating resin layer 31, and position P3 of the outer peripheral edges of the terminal electrodes 51, 52. This is because the positions P1 to P3 serve as fulcrums when the thin-film capacitor 1 tries to deform due to the pressure of the blade 60. In particular, since the terminal electrodes 51, 52 have a relatively high rigidity, the most stress is concentrated at position P3.
[0033] However, in this embodiment, the positions P1 to P3 are distributed, and the position P3 where the stress is most concentrated is far away from the capacitor layer 20, so that the capacitor layer 20 itself is not subjected to strong stress. Moreover, as shown in FIG. 4, the terminal electrode 51 (52) is inclined near the outer peripheral edge, and the height position becomes lower as it approaches the outer peripheral edge, so that stress is concentrated on the terminal electrode edge at the position P3 during singulation. As a result, cracks are likely to occur in the insulating resin layer 32 at the position P3, so that the inside of the element disposed at a position away from the outer peripheral edge of the terminal electrode 51 (52) is protected. Therefore, cracks are unlikely to occur in the passivation layer 30 during singulation, and even if cracks occur, they occur outside the capacitor layer 20, so that various characteristics such as insulation resistance are not affected.
[0034] In order to fully obtain such effects, it is desirable that the distance between positions P1 and P2 and the distance between positions P2 and P3 are greater, and in particular, reliability is significantly improved by ensuring that the distance between positions P2 and P3 is 10 μm or more. On the other hand, if these distances are large, the effective area of capacitor layer 20 relative to the chip size decreases, so it is preferable that the distance between positions P1 and P2 is in the range of 5 to 30 μm, and the distance between positions P2 and P3 is in the range of 5 to 50 μm.
[0035] Fig. 5 is a schematic plan view of a thin film capacitor 1A according to a first modified example. As shown in Fig. 5, the thin film capacitor 1A according to the first modified example differs from the thin film capacitor 1 according to the above embodiment in that the thin film capacitor 1A includes four terminal electrodes 51 to 54. Thus, in the present invention, the number of terminal electrodes is not particularly limited.
[0036] Fig. 6 is a schematic plan view of a thin film capacitor 1B according to the second modified example. As shown in Fig. 6, the thin film capacitor 1B according to the second modified example differs from the thin film capacitor 1 according to the above embodiment in that the terminal electrodes 51, 52 are arranged in the short side direction. By arranging the terminal electrodes 51, 52 in this way in the short side direction, it is possible to reduce the ESL.
[0037] Although a preferred embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and various modifications are possible without departing from the spirit of the present invention, and it goes without saying that these modifications are also included within the scope of the present invention. [Explanation of symbols]
[0038] 1,1A,1B Thin Film Capacitor 10 Support material 10a Collective board 12 Side of support 20 Capacitor Layer 21,22 Electrode layer 23 Dielectric layer 30 Passivation Layer 31, 32 Insulating resin layer 41,42 Redistribution layer 41D Dummy Pattern 51~54 Terminal electrode 60 Blades P1~P3 Position of outer edge
Claims
1. A support material; a capacitor layer provided on the support material and including a plurality of electrode layers and a plurality of dielectric layers alternately stacked; a first rewiring layer provided on a first insulating resin layer covering the capacitor layer; a second rewiring layer provided on a second insulating resin layer covering the first rewiring layer; a terminal electrode connected to the second redistribution layer; an outer peripheral edge of the first insulating resin layer is located outside an outer peripheral edge of the capacitor layer; an outer peripheral edge of the terminal electrode is located outside an outer peripheral edge of the first insulating resin layer; a thin-film capacitor characterized in that the height position of the terminal electrode based on the support material is inclined near the outer peripheral edge so that the height at a portion overlapping with the capacitor layer, outside the outer peripheral edge of the capacitor layer, and the height at a portion overlapping with the first insulating resin layer, outside the outer peripheral edge of the first insulating resin layer, is lower than the height at a portion overlapping with the capacitor layer, outside the outer peripheral edge of the capacitor layer, and the height at a portion overlapping with the second insulating resin layer, outside the outer peripheral edge of the first insulating resin layer, is lower than the height at a portion overlapping with the first insulating resin layer, outside the outer peripheral edge of the capacitor layer.
2. 2. The thin film capacitor according to claim 1, further comprising a passivation layer made of an inorganic insulating material provided between the capacitor layer and the first insulating resin layer.
3. 3. The thin film capacitor according to claim 1, wherein the distance from an outer peripheral edge of the first insulating resin layer to an outer peripheral edge of the terminal electrode is 10 [mu]m or more.
4. 4. The thin film capacitor according to claim 1, wherein an outer peripheral edge of the first insulating resin layer is covered with a dummy pattern of a first rewiring layer.
5. 5. A method for producing a thin film capacitor according to claim 1, wherein the supporting material is cut with a blade to separate the thin film capacitor.
Citation Information
Patent Citations
Electronic part
JP2007300002A
Thin film capacitor
JP2018137310A
Capacitor and method of manufacturing the same
JP2019179804A