Reactor, converter, and power conversion device

The reactor design addresses the challenge of resin filling in the gap between core pieces by optimizing core shapes and surface configurations, achieving high inductance, heat dissipation, and low loss, suitable for vehicle power conversion systems.

JP7569502B2Active Publication Date: 2024-10-18AUTONETWORKS TECH LTD +2
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021156094
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-09-24
Publication Date
2024-10-18
Estimated Expiration
2041-09-24

AI Technical Summary

Technical Problem

The reactor in Patent Document 1 faces challenges in filling the gap between flat-surfaced inner core pieces with molded resin, leading to difficulties in maintaining desired inductance and resin quantity, as widening the gap to accommodate more resin may compromise inductance.

Method used

A reactor design with a cylindrical winding portion, a magnetic core comprising a first core part with an E-shape and a second core part with a T-shape or E-shape, where the gap is positioned between these core parts, and the end surfaces are configured to facilitate effective resin filling, with specific area ratios and dimensions to enhance inductance and resin spread.

Benefits of technology

The design achieves high resin filling properties, resulting in high inductance, excellent heat dissipation, and reduced eddy current loss, while maintaining a compact size suitable for applications in vehicles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569502000003
    Figure 0007569502000003
  • Figure 0007569502000004
    Figure 0007569502000004
  • Figure 0007569502000005
    Figure 0007569502000005
Patent Text Reader

Abstract

To provide a reactor which improves filling property of a mold resin into a gap part in a resin core and improves inductance.SOLUTION: The present invention relates to a reactor comprising: a coil including a winding part; a magnetic core including an E-shaped first core part, a T-shaped or E-shaped second core part and a gap part; and a mold resin part. The first core part is a molded body of a composite material including a first middle core part. The second core part is a power-compressed molded body including a second middle core part. The gap part is disposed between an end face of the first middle core part and an end face of the second middle core part inside of the winding part. The end face of the first middle core part includes an annular outer end face, a peripheral surface and an inner end face. The end face of the second middle core part, the outer end face and the inner end face are flat surfaces. A ratio of an area of the inner end face with respect to an area of the outer end face is 0.30 or more and 1.35 or less. The mold resin part includes a portion provided between the outer end face and the end face of the second middle core part.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a reactor, a converter, and a power conversion device. [Background technology]

[0002] The reactor of Patent Document 1 includes a coil, a magnetic core, and a molded resin portion. The coil has a winding portion. The winding portion is formed by winding a wire in a spiral shape. The magnetic core has an inner core portion and an outer core portion. The inner core portion is disposed inside the winding portion. The inner core portion has a plurality of inner core pieces and a gap portion provided between adjacent inner core pieces. The outer core portion is disposed outside the winding portion. The molded resin portion covers at least a portion of the combination of the coil and the magnetic core. The molded resin portion has a portion that fills the gap portion. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-139310 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the reactor of Patent Document 1, the end face of each inner core piece is configured as a flat face. That is, a gap portion is provided between the two end faces configured as flat faces. If the interval between the two end faces is narrow, it is difficult to fill the molded resin portion between the two end faces. If the amount of the molded resin portion filled between the two end faces is small, it is difficult to maintain the above-mentioned interval. If the above-mentioned interval is widened so that the amount of the molded resin portion filled between the two end faces increases, the desired inductance may not be obtained.

[0005] An object of the present disclosure is to provide a reactor having a high inductance and a molded resin portion that is highly fillable in a gap portion of a magnetic core. Another object of the present disclosure is to provide a converter including the reactor. Still another object of the present disclosure is to provide a power conversion device including the converter. [Means for solving the problem]

[0006] The reactor of the present disclosure includes: A coil having a cylindrical winding portion; a magnetic core including a first core portion and a second core portion combined in an axial direction of the winding portion, and a gap portion provided between the first core portion and the second core portion; a molded resin portion covering at least a portion of the magnetic core, The number of the windings is one, The first core portion has an E-shape, The second core portion has a T-shape or an E-shape, the first core portion is a composite material molded body having a first middle core portion disposed inside the winding portion, the second core portion is a powder compact having a second middle core portion disposed inside the winding portion, the gap portion is disposed inside the winding portion between an end surface of the first middle core portion and an end surface of the second middle core portion, The end surface of the first middle core portion is an annular outer end surface connected to an outer peripheral surface of the first middle core portion; a circumferential surface extending from the outer end surface toward an end surface of the second middle core portion; an inner end surface connected to a tip of the peripheral surface; The end surface of the second middle core portion is a flat surface, the outer end surface and the inner end surface are flat surfaces, The ratio of the area of ​​the inner end face to the area of ​​the outer end face is 0.30 or more and 1.35 or less. below and The molded resin portion has a portion provided between the outer end surface and an end surface of the second middle core portion. Effect of the Invention

[0007] The reactor of the present disclosure has a high filling efficiency of the molded resin portion in the gap portion of the magnetic core, and has a high inductance. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a schematic perspective view showing the entire reactor of the first embodiment. [Diagram 2] FIG. 2 is a schematic side view showing the entire reactor of the first embodiment. [Diagram 3] FIG. 3 is a schematic perspective view showing a state in which the reactor of the first embodiment is disassembled. [Figure 4] FIG. 4 is a schematic plan view of an end face of a first core portion included in the reactor of the first embodiment, viewed from a first direction. [Diagram 5] FIG. 5 is a schematic top view showing the entire reactor of the first embodiment. [Figure 6] FIG. 6 is a schematic enlarged view showing an area A in FIG. [Figure 7] FIG. 7 is a schematic top view showing the entire reactor of the second embodiment. [Figure 8] FIG. 8 is a schematic diagram showing the power supply system of a hybrid vehicle. [Figure 9] FIG. 9 is a circuit diagram showing an example of a power conversion device including a converter. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Description of the embodiments of the present disclosure First, the embodiments of the present disclosure will be listed and described.

[0010] (1) A reactor according to an embodiment of the present disclosure includes: A coil having a cylindrical winding portion; a magnetic core including a first core portion and a second core portion combined in an axial direction of the winding portion, and a gap portion provided between the first core portion and the second core portion; a molded resin portion covering at least a portion of the magnetic core, The number of the windings is one, The first core portion has an E-shape, The second core portion has a T-shape or an E-shape, the first core portion is a composite material molded body having a first middle core portion disposed inside the winding portion, the second core portion is a powder compact having a second middle core portion disposed inside the winding portion, the gap portion is disposed inside the winding portion between an end surface of the first middle core portion and an end surface of the second middle core portion, The end surface of the first middle core portion is an annular outer end surface connected to an outer peripheral surface of the first middle core portion; a circumferential surface extending from the outer end surface toward an end surface of the second middle core portion; an inner end surface connected to a tip of the peripheral surface; The end surface of the second middle core portion is a flat surface, the outer end surface and the inner end surface are flat surfaces, The ratio of the area of ​​the inner end face to the area of ​​the outer end face is 0.30 or more and 1.35 or less. below and The molded resin portion has a portion provided between the outer end surface and an end surface of the second middle core portion.

[0011] Hereinafter, the gap portion provided between the outer end face and the end face of the second middle core portion will be referred to as the outer gap portion, and the gap portion provided between the inner end face and the end face of the second middle core portion will be referred to as the inner gap portion.

[0012] The reactor has a high filling property of the molded resin portion in the gap portion. The reason is as follows. In the process of forming the molded resin portion, a part of the constituent material of the molded resin portion is filled inside the winding portion. The outer end face, the inner end face, and the end face of the second middle core portion are flat surfaces. Therefore, the thickness of the outer gap portion is larger than the thickness of the inner gap portion. The outer end face is provided in an annular shape. Therefore, the outer gap portion is provided in an annular shape. The ratio of the area of ​​the inner end face to the area of ​​the outer end face is 1.35 or less, so that the proportion of the outer gap portion is appropriately secured. Therefore, the constituent material of the molded resin portion filled inside the winding portion easily spreads between the end face of the first middle core portion and the end face of the second middle core portion.

[0013] The reactor has a high inductance for the following reasons: the length between the inner end face and the end face of the second middle core portion is shorter than the length between the outer end face and the end face of the second middle core portion, and the ratio of the area of ​​the inner end face to the area of ​​the outer end face is 0.30 or more, so that the proportion of the inner gap portion is appropriately secured.

[0014] The reactor has excellent heat dissipation properties because the molded resin portion has a portion provided between the outer end face and the end face of the second middle core portion, which tends to increase thermal conduction between the first core portion and the second core portion.

[0015] The reactor has low loss. Since the gap portion is disposed inside the winding portion, leakage magnetic flux is unlikely to enter the winding portion. Therefore, eddy current loss occurring in the winding portion can be easily reduced.

[0016] (2) As one embodiment of the above reactor, It is preferable that the ratio of the length between the outer end face and the end face of the second middle core portion to the length between the inner end face and the end face of the second middle core portion is 3.00 or greater and 15.00 or less.

[0017] In the above configuration in which the ratio is 3.00 or more, the molded resin portion fills the gap portion well. This is because the constituent material of the molded resin portion filled inside the winding portion easily spreads between the end faces of the first middle core portion and the second middle core portion. In the above configuration in which the ratio is 15.00 or less, the inductance is high. This is because the thickness of the outer gap portion is not too large. In addition, the above configuration has low loss.

[0018] (3) As one embodiment of the above reactor, a length of the winding portion in the second middle core portion along the axial direction is shorter than a length of the winding portion in the first middle core portion along the axial direction; The length from the end face of the winding portion facing the second core portion to the gap portion may be 0.2 to 0.49 times the length of the winding portion.

[0019] The above embodiment has low loss. In the above embodiment, the length of the second middle core portion is shorter than the length of the first middle core portion, so that the ratio of the green compact having a larger loss than the green compact of the composite material is likely to be reduced. In addition, in the above embodiment, the gap portion is disposed inside the winding portion, and the length from the end face of the winding portion to the gap portion is 0.2 times or more the length of the winding portion, so that leakage flux is unlikely to enter the winding portion. Therefore, it is easy to reduce eddy current loss generated in the winding portion. Furthermore, the length from the end face to the gap portion is 0.49 times or less the length of the winding portion, so that the ratio of the green compact of the composite material having a lower loss than the green compact can be increased inside the winding portion.

[0020] The above embodiment can suppress problems such as the effect of leakage flux on peripheral devices, because the gap portion is disposed inside the winding portion and the length from the end face to the gap portion is 0.2 times or more the length of the winding portion, which makes it easy to suppress leakage of magnetic flux to the outside of the winding portion.

[0021] The above embodiment has a high filling property of the molded resin portion in the gap portion, because the length from the end face to the gap portion is 0.49 times or less the length of the winding portion, which makes it easy to spread the constituent material of the molded resin portion between the outer end face and the end face of the second middle core portion.

[0022] (4) As one embodiment of the reactor, It is preferable that the ratio of the thickness of the gap portion to the sum of the axial length of the winding portion in the first middle core portion, the axial length of the winding portion in the second middle core portion, and the thickness of the gap portion is 0.02 or more and 0.05 or less.

[0023] The thickness of the gap portion here refers to the length along the axial direction of the winding portion between the outer end face and the end face of the second middle core portion, i.e., the thickness of the gap portion is the thickness of the outer gap portion.

[0024] In the above embodiment, the ratio is 0.02 or more, so that the filling of the molded resin into the gap is high. In the above embodiment, the ratio is 0.05 or less, so that the inductance is high. Furthermore, in the above embodiment, leakage flux is small, and the effect of reducing eddy current loss is likely to be high.

[0025] (5) As one embodiment of the above reactor, The thickness of the gap portion is preferably 1.0 mm or more and 2 mm or less.

[0026] In the above embodiment, the thickness is 1.0 mm or more, so that the mold resin fills the gap well. In the above embodiment, the thickness is 2 mm or less, so that the inductance is high. In addition, the leakage flux is small, so that the effect of reducing eddy current loss is likely to be high.

[0027] (6) As one embodiment of the reactor, The powder compact is a compact of a raw material powder containing a soft magnetic powder, The content of the soft magnetic powder in the powder compact may be 85% by volume or more and 99% by volume or less.

[0028] The magnetic properties of the above-mentioned powder compact can be improved more easily than those of a composite material compact.

[0029] (7) As one embodiment of the reactor, The composite material compact is a compact in which soft magnetic powder is dispersed in a resin, The content of the soft magnetic powder in the composite material compact may be 20% by volume or more and 80% by volume or less.

[0030] The magnetic properties of the composite material compact can be adjusted more easily than with a powder compact, and it is also easier to form the composite material into a complex shape.

[0031] (8) A converter according to an embodiment of the present disclosure includes: The reactor includes the reactor according to any one of (1) to (7) above.

[0032] The converter has excellent performance since it includes the reactor.

[0033] (9) A power conversion device according to an embodiment of the present disclosure includes: Equipped with the converter (8) above.

[0034] The power conversion device has excellent performance since it includes the converter.

[0035] Details of the embodiments of the present disclosure DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The details of the embodiments of the present disclosure will be described below with reference to the drawings. In the drawings, the same reference numerals indicate the same objects.

[0036] First Embodiment [Reactor] A reactor 1 according to a first embodiment will be described with reference to Figs. 1 to 6. As shown in Fig. 1, the reactor 1 includes a coil 2, a magnetic core 3, and a molded resin portion 4. The coil 2 has a cylindrical winding portion 21. The number of the winding portion 21 is one. The magnetic core 3 has a first core portion 3f, a second core portion 3s, and a gap portion 3g. The first core portion 3f and the second core portion 3s are combined in the axial direction of the winding portion 21. The gap portion 3g is provided between the first core portion 3f and the second core portion 3s. The molded resin portion 4 covers at least a portion of the magnetic core 3. One of the features of the reactor 1 according to this embodiment is that it satisfies the following requirements (a) to (e).

[0037] (a) The first core portion 3f and the second core portion 3s have specific shapes. (b) The first core portion 3f and the second core portion 3s are formed of a specific molded body. (c) The gap portion 3g is located at a specific location. (d) As shown in FIG. 3, an end face 312 of the first middle core portion 31f included in the first core portion 3f, and as shown in FIG. 6, an end face 318 of the second middle core portion 31s included in the second core portion 3s have a specific shape. (e) As shown in FIG. 6, the mold resin portion 4 has a portion provided in a specific region of the gap portion 3g.

[0038] Each component will be described in detail below. For convenience of explanation, the coil 2 is indicated by a two-dot chain line in Fig. 5. In the following explanation, a first direction D1, a second direction D2, and a third direction D3 defined as follows may be used. The first direction D1 is a direction along the axial direction of the winding portion 21. The second direction D2 is a direction along the parallel arrangement direction of a first middle core portion 31f, a first side core portion 321, and a second side core portion 322, which will be described later. The third direction D3 is a direction perpendicular to both the first direction D1 and the second direction D2.

[0039] [coil] 1 and 3, the winding portion 21 of the coil 2 is formed by winding a single wire without joints in a spiral shape. Since there is only one winding portion 21, the length along the second direction D2 can be made shorter than when multiple winding portions are arranged in parallel in the second direction D2.

[0040] The shape of the winding part 21 in this embodiment is a rectangular cylinder. The rectangle includes a rectangle and a square. The end face shape of the winding part 21 in this embodiment is a rectangular frame shape. Since the shape of the winding part 21 is a rectangular cylinder, it is easy to increase the contact area between the winding part 21 and the installation target 100 compared to when the winding part 21 is a circular cylinder with the same cross-sectional area. Therefore, the reactor 1 is easy to dissipate heat to the installation target 100 shown in FIG. 2 through the winding part 21. In addition, the winding part 21 is easy to stably install on the installation target 100. An example of the installation target 100 is a cooling base or the inner bottom surface of a case described later. The corners of the winding part 21 are rounded. Unlike this embodiment, the shape of the winding part 21 may be a circular cylinder. The circle includes a perfect circle and an ellipse.

[0041] The winding may be a known winding. The winding in this embodiment uses a coated rectangular wire. The conductor wire of the coated rectangular wire is made of a rectangular copper wire. The insulating coating of the coated rectangular wire is made of enamel. The winding portion 21 is made of an edgewise coil in which the coated rectangular wire is wound edgewise.

[0042] In this embodiment, the first end 21a and the second end 21b of the winding portion 21 are extended toward the outer periphery of the winding portion 21 at the first end side and the second end side in the axial direction of the winding portion 21, respectively. Although not shown in the figure, the insulating coating of the first end 21a and the second end 21b is stripped to expose the conductor wire. As shown in FIG. 2, the exposed conductor wire is drawn to the outside of the molded resin portion 4. A terminal member is connected to the exposed conductor wire. The terminal member is not shown in the figure. An external device is connected to the coil 2 via this terminal member. The external device is not shown in the figure. An example of the external device is a power source that supplies power to the coil 2.

[0043] The outer peripheral surface 25 of the winding portion 21 has a portion that contacts the installation target 100 of the reactor 1. Therefore, the reactor 1 is easy to improve the heat dissipation. The outer peripheral surface 25 has a portion that protrudes in the third direction D3 beyond the magnetic core 3. That is, the length of the winding portion 21 along the third direction D3 is longer than the length of the magnetic core 3 along the third direction D3. In this embodiment, since the shape of the winding portion 21 is a rectangular tube, the outer peripheral surface 25 of the winding portion 21 has four flat surfaces. In this embodiment, one of the four flat surfaces is a portion that contacts the installation target 100. Therefore, the winding portion 21 can secure a sufficient contact area with the installation target 100. Therefore, the reactor 1 is easy to further improve the heat dissipation. In this embodiment, the contact portion of the winding portion 21 is exposed from the molded resin portion 4 described later. Therefore, the heat of the coil 2 is easy to be released through the installation target 100.

[0044] [Magnetic core] As shown in FIG. 1, the magnetic core 3 is an assembly in which the first core portion 3f and the second core portion 3s are combined in the first direction D1. Since the magnetic core 3 can be constructed by combining the first core portion 3f and the second core portion 3s in the first direction D1, the reactor 1 has excellent manufacturing workability. A gap portion 3g, which will be described later, is provided between the first core portion 3f and the second core portion 3s. In this embodiment, the combination of the first core portion 3f and the second core portion 3s is an ET type. Unlike this embodiment, the combination may be an EE type. These combinations make it easier to adjust the inductance and heat dissipation. The first core portion 3f is made of a molded body of a composite material, which will be described later. The second core portion 3s is made of a powder compact, which will be described later.

[0045] The total volume Va of the first core portion 3f, the second core portion 3s, and the gap portion 3g is 50 cm 3 More than 500cm 3 The total volume V is 50 cm 3 More than 500cm 3The reactor 1 having the above-mentioned volume Va is suitable for a converter of an electric vehicle, a hybrid vehicle, or a fuel cell vehicle. Since the winding portion 21 has a portion that contacts the installation target 100 and the second core portion 3s is made of a powder compact, the total volume Va is 50 cm 3 Even if the total volume Va is more than 500 cm, the heat of the magnetic core 3 is easily dissipated. 3 By keeping the total volume Va at 60 cm or less, the reactor 1 is unlikely to become excessively large. 3 More than 400cm 3 Less than 70cm, especially 3 More than 300cm 3 The volume of the gap portion 3g is the volume of a space surrounded by the end face 312 of the first middle core portion 31f, the end face 318 of the second middle core portion 31s, and a virtual outer circumferential surface. The virtual outer circumferential surface is an outer circumferential surface obtained by extending the outer circumferential surface 311 of the first middle core portion 31f in the first direction D1.

[0046] (First core part) The planar shape of the first core portion 3f is E-shaped as shown in FIG. 5. The planar shape of the first core portion 3f refers to the shape of the first core portion 3f when viewed from the third direction D3. The concept of the planar shape is the same for the second core portion 3s described later. The first core portion 3f has a first end core portion 33f, a first middle core portion 31f, a first side core portion 321, and a second side core portion 322. The first end core portion 33f and a first end face of the winding portion 21 face each other. The first middle core portion 31f has a portion that is disposed inside the winding portion 21. The first side core portion 321 and the second side core portion 322 are disposed facing each other so as to sandwich the first middle core portion 31f. The first side core portion 321 and the second side core portion 322 are disposed on the outer periphery of the winding portion 21.

[0047] As shown in Fig. 3, the first core portion 3f is an integrally molded body of a first end core portion 33f, a first middle core portion 31f, a first side core portion 321, and a second side core portion 322. The first end core portion 33f connects the first middle core portion 31f, the first side core portion 321, and the second side core portion 322. The first side core portion 321 and the second side core portion 322 are provided at both ends of the first end core portion 33f. The first middle core portion 31f is provided in the center of the first end core portion 33f.

[0048] In this embodiment, the shape of the first end core portion 33f is a thin prismatic column. The shapes of the first side core portion 321 and the second side core portion 322 are the same. In this embodiment, the shapes of the first side core portion 321 and the second side core portion 322 are a thin prismatic column.

[0049] The shape of the first middle core portion 31f corresponds to the inner circumferential shape of the winding portion 21. In this embodiment, the shape of the first middle core portion 31f is a quadrangular prism.

[0050] As shown in Fig. 3, first middle core portion 31f has an outer peripheral surface 311 and an end surface 312. Outer peripheral surface 311 is a surface that faces an inner peripheral surface of winding portion 21. The corners of outer peripheral surface 311 are shown as angular in Fig. 3, but are rounded to fit the corners of the inner peripheral surface of winding portion 21 as shown in Fig. 4.

[0051] As shown in Figs. 3 and 6, the end surface 312 has an outer end surface 313, a circumferential surface 314, and an inner end surface 315. The outer end surface 313 is connected to the outer circumferential surface 311. The outer end surface 313 is an annular flat surface. As shown in Fig. 4, the outer end surface 313 of this embodiment is a rectangular annular flat surface. The circumferential surface 314 is connected to the outer end surface 313 and the inner end surface 315 as shown in Figs. 3 and 6. The circumferential surface 314 is a cylindrical surface extending from the outer end surface 313 toward the end surface 318. The circumferential surface 314 of this embodiment is a rectangular cylindrical surface. The circumferential surface 314 may be a cylindrical surface extending linearly along the first direction D1, or may be a cylindrical surface tapering from the outer end surface 313 toward the inner end surface 315. The inner end surface 315 is a flat surface. The planar shape of the inner end face 315 of this embodiment is similar to the contour shape of the outer peripheral surface 311 as shown in FIG. 4. That is, the planar shape of the inner end face 315 of this embodiment is a square. Unlike this embodiment, the planar shape of the inner end face 315 may be different from the contour shape of the outer peripheral surface 311. For example, the planar shape of the inner end face 315 of this embodiment may be a circle. Since the outer end face 313, the inner end face 315, and the end face 318 are flat surfaces, as shown in FIG. 6, the length Lge between the outer end face 313 and the end face 318 in the first direction D1 is longer than the length Lgi between the inner end face 315 and the end face 318 in the first direction D1. In other words, the length Lgi is shorter than the length Lge.

[0052] The ratio of the area Si of the inner end face 315 to the area Se of the outer end face 313, that is, the area Si / area Se, is 0.30 or more and 1.35 or less (see FIG. 4). The reactor 1 with the area Si / area Se of 0.30 or more has a high inductance. This is because the ratio of the inner gap portion 3gi, which will be described later with reference to FIG. 6, is appropriately ensured by the area Si / area Se of 0.30 or more. The reactor 1 with the area Si / area Se of 1.35 or less has a high filling property of the molded resin portion 4 into the gap portion 3g. The reason is as follows. In the process of molding the molded resin portion 4, a part of the constituent material of the molded resin portion 4 is filled into the inside of the winding portion 21. The outer gap portion 3ge, which will be described later with reference to FIG. 6, is provided in an annular shape. The ratio of the outer gap portion 3ge, which will be described later with reference to FIG. 6, is appropriately ensured by the area Si / area Se of 1.35 or less. Therefore, the constituent material of molded resin portion 4 filled inside winding portion 21 easily spreads between end face 312 and end face 318. Area Si / area Se may be 0.31 or more and 1.25 or less, or 0.32 or more and 1.15 or less. Area Si / area Se may be 0.32 or more and 1.00 or less, or 0.32 or more and 0.85 or less.

[0053] An example of the length of the circumferential surface 314 shown in Figures 3 and 6, i.e., an example of the length between the outer end surface 313 and the inner end surface 315, is a length in which the length Lge / length Lgi described below satisfies the range described below.

[0054] In this embodiment, the sum of the cross-sectional area of ​​the first side core portion 321 and the cross-sectional area of ​​the second side core portion 322 is the same as the cross-sectional area of ​​the first middle core portion 31f and the cross-sectional area of ​​the second middle core portion 31s. The cross-sectional area here refers to the cross-sectional area of ​​a cross section perpendicular to the first direction D1.

[0055] As shown in FIG. 5, the length L1f of the first middle core portion 31f along the first direction D1 is shorter than the length of the wound portion 21 along the first direction D1. The length L1f is the length along the first direction D1 between the part of the first middle core portion 31f connected to the first end core portion 33f and the inner end face 315. The length of the wound portion 21 along the first direction D1 is the length along the first direction D1 between the first end face and the second end face of the wound portion 21. When there is a gap between the turns of the wound portion 21, the length of the wound portion 21 along the first direction D1 includes the length of the gap between the turns. The length of the first middle core portion 31f along the second direction D2 is longer than each of the length of the first side core portion 321 along the second direction D2 and the length of the second side core portion 322 along the second direction D2. As shown in FIG. 1, the length of the first middle core portion 31f along the third direction D3 is the same as the length of the first side core portion 321 along the third direction D3 and the length of the second side core portion 322 along the third direction D3.

[0056] As shown in Fig. 5, a length L21 of the first side core portion 321 along the first direction D1 and a length L22 of the second side core portion 322 along the first direction D1 are the same. The lengths L21 and L22 are longer than the length L1f and longer than the length of the winding portion 21 along the first direction D1. The length of the first side core portion 321 along the second direction D2 and the length of the second side core portion 322 along the second direction D2 are the same. As shown in Fig. 1, the length of the first side core portion 321 along the third direction D3 and the length of the second side core portion 322 along the third direction D3 are the same.

[0057] (Second core part) As shown in FIG. 5, the planar shape of the second core portion 3s is T-shaped in this embodiment. Unlike this embodiment, the planar shape of the second core portion 3s may be E-shaped. As described above, the second core portion 3s is composed of a powder compact. A powder compact having a T-shaped planar shape is easier to manufacture than a powder compact having an E-shaped planar shape. Therefore, a powder compact having a T-shaped planar shape is easier to manufacture with high accuracy than a powder compact having an E-shaped planar shape. Therefore, when the second core portion 3s having a T-shaped planar shape is combined with the first core portion 3f, an unnecessary gap is less likely to be formed than when the planar shape is E-shaped.

[0058] The second core portion 3s in this embodiment has a second end core portion 33s and a second middle core portion 31s. The second end core portion 33s and a second end face of the wound portion 21 face each other. The second middle core portion 31s has a portion disposed inside the wound portion 21. As shown in FIG. 3, the second core portion 3s is a molded body in which the second end core portion 33s and the second middle core portion 31s are integrally formed. The second middle core portion 31s is provided in the center of the second end core portion 33s.

[0059] The shape of the second end core portion 33s is the same as the shape of the first end core portion 33f. That is, the second end core portion 33s is a thin rectangular column. The shape of the second middle core portion 31s is a quadrangular column. The corners of the second middle core portion 31s are rounded to fit the inner circumferential surface of the corners of the winding portion 21. The end face 318 of the second middle core portion 31s is a flat surface.

[0060] As shown in Fig. 5, in this embodiment, the length L1s of the second middle core portion 31s along the first direction D1 is shorter than the length L1f. The sum of the length L1s and the length L1f is shorter than each of the lengths L21 and L22. The length of the second middle core portion 31s along the second direction D2 is the same as the length of the first middle core portion 31f along the second direction D2. As shown in Fig. 1, the length of the second middle core portion 31s along the third direction D3 is the same as the length of the first middle core portion 31f along the third direction D3.

[0061] As shown in FIG. 5, the length L3s of the second end core portion 33s along the first direction D1 is the same as the length L3f of the first end core portion 33f along the first direction D1. The length of the second end core portion 33s along the second direction D2 is the same as the length of the first end core portion 33f along the second direction D2. The length of the second end core portion 33s along the second direction D2 is longer than the length of the wound portion 21 along the second direction D2. As shown in FIG. 1, the length of the second end core portion 33s along the third direction D3 is the same as the length of the first end core portion 33f along the third direction D3. As shown in FIG. 2, the length of the second end core portion 33s along the third direction D3 is shorter than the length of the wound portion 21 along the third direction D3. As shown in FIG. 1, the length of the second end core portion 33s along the third direction D3 is the same as the length of the second middle core portion 31s along the third direction D3.

[0062] An example of the volume ratio Vps calculated by (volume Vs / total volume Va)×100 is 25% or more and 40% or less. The volume Vs is the volume of the second core portion 3s. As described above, the total volume Va is the total volume of the first core portion 3f, the second core portion 3s, and the gap portion 3g. If the volume ratio Vps is 25% or more, the heat dissipation of the reactor 1 is likely to be improved. If the volume ratio Vps is 40% or less, the loss of the reactor 1 is likely to be reduced. The volume ratio Vps may be 27% or more and 38% or less, or may be 29% or more and 36% or less.

[0063] An example of the volume ratio Vpm calculated by (volume Vms / total volume Vma)×100 is 15% or more and 49% or less. The volume Vms is the volume of the second middle core portion 31s. The total volume Vma is the total volume of the first middle core portion 31f, the second middle core portion 31s, and the gap portion 3g. If the ratio Vpm is 15% or more, the heat dissipation of the reactor 1 is likely to be improved. If the ratio Vpm is 49% or less, the loss of the reactor 1 is likely to be reduced. The ratio Vpm may be 20% or more and 40% or less, or 25% or more and 35% or less.

[0064] The first core portion 3f and the second core portion 3s are combined so that the end faces of the first side core portion 321 and the second side core portion 322 are in contact with the end face of the second end core portion 33s. A gap is provided between the end face 312 of the first middle core portion 31f and the end face 318 of the second middle core portion 31s. A gap portion 3g, which will be described later, is provided between the end face 312 and the end face 318.

[0065] The composite material molded body constituting the first core portion 3f is a molded body in which soft magnetic powder is dispersed in resin. The composite material molded body is obtained by filling a mold with a fluid material in which soft magnetic powder is dispersed in unsolidified resin, and solidifying the resin. The composite material molded body allows easy adjustment of the content of soft magnetic powder in the resin. Therefore, the magnetic properties of the composite material molded body are easy to adjust. Furthermore, the composite material molded body is easy to form even complex shapes compared to pressed powder molded bodies. An example of the content of soft magnetic powder in the composite material molded body is 20 volume % or more and 80 volume % or less. An example of the content of resin in the composite material molded body is 20 volume % or more and 80 volume % or less. These contents are values ​​when the composite material molded body is 100 volume %.

[0066] The powder compact constituting the second core portion 3s is a compact obtained by compressing and molding soft magnetic powder. Compared to a composite material compact, the powder compact can have a higher ratio of soft magnetic powder in the core portion. Therefore, the powder compact is easy to improve magnetic properties. Examples of magnetic properties include relative permeability and saturation magnetic flux density. Also, compared to a composite material compact, the powder compact has a smaller amount of resin and a larger amount of soft magnetic powder, and therefore has excellent heat dissipation properties. An example of the content of magnetic powder in the powder compact is 85 volume % or more and 99 volume % or less. This content is the value when the powder compact is 100 volume %.

[0067] Examples of the particles constituting the soft magnetic powder include soft magnetic metal particles, coated particles, and soft magnetic nonmetal particles. The coated particles include a soft magnetic metal particle and an insulating coating provided on the outer periphery of the soft magnetic metal particle. The soft magnetic metal includes pure iron or an iron-based alloy. An example of the iron-based alloy is an Fe-Si alloy or an Fe-Ni alloy. An example of the insulating coating is a phosphate. An example of the soft magnetic nonmetal is a ferrite.

[0068] An example of the resin of the composite material molded body is a thermosetting resin or a thermoplastic resin. An example of the thermosetting resin is an epoxy resin, a phenolic resin, a silicone resin, a urethane resin, etc. An example of the thermoplastic resin is a polyphenylene sulfide resin, a polyamide resin, a liquid crystal polymer, a polyimide resin, a fluororesin, etc. An example of the polyamide resin is Nylon 6, Nylon 66, Nylon 9T, etc.

[0069] The composite material compact may contain a ceramic filler. Examples of the ceramic filler include alumina and silica. The ceramic filler contributes to improving heat dissipation and electrical insulation.

[0070] The content of soft magnetic powder in the composite material compact and the content of soft magnetic powder in the powder compact are considered to be equivalent to the area ratio of the soft magnetic powder in the cross section of the compact. The content of soft magnetic powder in the compact is determined as follows. The cross section of the compact is observed with a SEM (scanning electron microscope) to obtain an observation image. The cross section of the compact is any cross section. The magnification of the SEM is 200 times or more and 500 times or less. At least 10 observation images are obtained. The total cross section is 0.1 cm2. 2 That is all. One observation image may be acquired per cross section, or multiple observation images may be acquired per cross section. Each acquired observation image is subjected to image processing to extract particle contours. Image processing includes, for example, binarization processing. The area ratio of soft magnetic particles in each observation image is calculated, and the average value of the area ratios is obtained. The average value is regarded as the content of soft magnetic powder.

[0071] The first core portion 3f is made of a composite material molded body and the second core portion 3s is made of a powder compact, which makes it easy to adjust the inductance without using the long gap portion 3g and also makes it easy to adjust the heat dissipation. In addition, the reactor 1 has the second core portion 3s made of a powder compact with a relatively high thermal conductivity, which makes it easy to improve the heat dissipation.

[0072] (Gap part) The gap portion 3g is disposed inside the winding portion 21. The gap portion 3g is disposed between the end face 312 of the first middle core portion 31f and the end face 318 of the second middle core portion 31s. Because the gap portion 3g is provided inside the winding portion 21, leakage magnetic flux is less likely to enter the winding portion 21 than when the gap portion 3g is provided outside the winding portion 21. Therefore, eddy current loss generated in the winding portion 21 can be easily reduced.

[0073] 6, the gap 3g has an outer gap 3ge and an inner gap 3gi. The outer gap 3ge is provided between the outer end face 313 and the end face 318. The inner gap 3gi is provided between the inner end face 315 and the end face 318.

[0074] The gap portion 3g is made of a material having a smaller relative magnetic permeability than the first core portion 3f and the second core portion 3s. At least a part of the gap portion 3g is made of a part of the molded resin portion 4 described later. The gap portion 3g may be made of only the molded resin portion 4, or may be made of the molded resin portion 4 and an air gap. In this embodiment, as shown in FIG. 6, the outer gap portion 3ge is made of the molded resin portion 4, and the inner gap portion 3gi is substantially made of an air gap.

[0075] An example of the ratio of the thickness of the outer gap portion 3ge to the thickness of the inner gap portion 3gi is 3.00 or more and 15.00 or less. The thickness of the inner gap portion 3gi is a length Lgi. The thickness of the outer gap portion 3ge is a length Lge. That is, the ratio of the thickness of the outer gap portion 3ge to the thickness of the inner gap portion 3gi is length Lge / length Lgi.

[0076] The reactor 1 in which the length Lge / length Lgi is 3.00 or more has a high filling property of the molded resin portion 4 in the gap portion 3g. The reactor 1 in which the length Lge / length Lgi is 15.00 or less has a high inductance. And the reactor 1 in which the length Lge / length Lgi is 3.00 or more and 15.00 or less has a low loss. The length Lge / length Lgi may be 3.25 or more and 12.50 or less, or 3.50 or more and 10.00 or less. The length Lge / length Lgi may be 3.50 or more and 7.00 or less.

[0077] An example of the ratio of the thickness of the gap portion 3g to the total length of the length L1f, the length L1s, and the thickness of the gap portion 3g is 0.02 or more and 0.05 or less. The thickness of the gap portion 3g is the length Lge. If the ratio is 0.02 or more, the filling property of the molded resin portion 4 into the gap portion 3g is high. If the ratio is 0.05 or less, it is easy to ensure a predetermined inductance. In addition, leakage flux is small, and the effect of reducing eddy current loss is likely to be high. The ratio may be 0.02 or more and 0.04 or less, or 0.02 or more and 0.035 or less.

[0078] An example of the length Lge is 1.0 mm or more and 2 mm or less. If the length Lge is 1.0 mm or more, the molded resin portion 4 is highly filled into the gap portion 3g. If the length Lge is 2 mm or less, a predetermined inductance is easily ensured. In addition, leakage flux is small, and the effect of reducing eddy current loss is easily increased. The length Lge may be more than 1.0 mm and 2 mm or less, may be 1.2 mm or more and 1.75 mm or less, or may be 1.25 mm or more and 1.5 mm or less.

[0079] An example of the length Le from the second end face of the winding portion 21 to the gap portion 3g along the first direction D1 is 0.2 to 0.49 times the length of the winding portion 21 along the first direction D1. The length Le is the length along the first direction D1 between the position closest to the second end face in the gap portion 3g and the second end face. In other words, the length Le is the length along the first direction D1 between the end face 318 shown in FIG. 6 and the second end face.

[0080] If the length Le is 0.2 times or more the length of the winding portion 21 in the first direction D1, leakage flux is less likely to enter the winding portion 21. This makes it easier to reduce eddy current loss generated in the winding portion 21. The closer the length Le is to 0.5 times the length of the winding portion 21 in the first direction D1, that is, the closer the position of the gap portion 3g is to the center of the winding portion 21 in the first direction D1, the greater the effect of reducing eddy current loss.

[0081] If the length Le is 0.49 times or less the length of the winding portion 21 along the first direction D1, the volume of the first middle core portion 31f is likely to be larger than the volume of the second middle core portion 31s inside the winding portion 21. Therefore, the volume of the first core portion 3f is likely to be larger than the volume of the second core portion 3s, and the proportion of the composite material molded body, which has lower loss than the powder compact, is likely to be higher. Therefore, the reactor 1 has low loss. Furthermore, if the length Le is 0.49 times or less the length of the winding portion 21 along the first direction D1, at least a part of the gap portion 3g is likely to be formed by a part of the molded resin portion 4. By having the length Le be 0.49 times or less the length of the winding portion 21 along the first direction D1, the total volume Va is 50 cm 3 Even in this case, the constituent material of the molded resin portion 4 can easily spread between the end face 312 and the end face 318. The shorter the length Le, the easier it is for the constituent material of the molded resin portion 4 to spread between the end face 312 and the end face 318.

[0082] The length Le may be 0.2 to 0.4 times the length of the wound portion 21 along the first direction D1, or 0.25 to 0.375 times the length of the wound portion 21 along the first direction D1.

[0083] [Space between the coil and the first middle core part and the second middle core part] The ratio of the length Lt to the length Lc (length Lt / length Lc) is 0.05 or more and 0.5 or less, and further 0.1 or more and 0.35 or less. The length Lc is the inner dimension of the winding portion 21 along the third direction D3. The length Lt is the sum of the length Lu and the length Ld. The length Lu is the length along the third direction D3 between the upper surfaces of the first middle core portion 31f and the second middle core portion 31s and the inner peripheral surface of the winding portion 21. The length Ld is the length along the third direction D3 between the lower surfaces of the first middle core portion 31f and the second middle core portion 31s and the inner peripheral surface of the winding portion 21. The upper surface is the surface of the first middle core portion 31f and the second middle core portion 31s opposite to the installation target 100. The lower surface is the surface of the first middle core portion 31f and the second middle core portion 31s on the installation target 100 side.

[0084] It is preferable that the interval between the inner peripheral surface of the winding portion 21 and the outer peripheral surfaces of the first middle core portion 31f and the second middle core portion 31s is substantially uniform in the circumferential direction. An example of the interval between the inner peripheral surface of the winding portion 21 and the outer peripheral surfaces of the first middle core portion 31f and the second middle core portion 31s is 1.0 mm or more and 5.0 mm or less, and further 1.5 mm or more and 4.0 mm or less. This interval is the minimum interval.

[0085] [Molded resin part] The molded resin part 4 covers at least a part of the magnetic core 3 as shown in Fig. 1, and also constitutes at least a part of the gap part 3g as shown in Fig. 6. The molded resin part 4 may cover the outer periphery of the magnetic core 3 but not the outer periphery of the coil 2, or may cover both the outer periphery of the magnetic core 3 and the outer periphery of the coil 2. For convenience of explanation, Fig. 5 omits the molded resin part 4, which will be described later.

[0086] As shown in FIG. 2, the molded resin part 4 in this embodiment covers the outer periphery of the assembly of a part of the coil 2 and the magnetic core 3. Therefore, the assembly is substantially protected from the external environment. In this embodiment, the flat surface of the outer periphery 25 on the side of the installation target is exposed from the molded resin part 4. The outer periphery 25 except for the flat surface on the side of the installation target is covered by the molded resin part 4. The entire outer periphery of the magnetic core 3 is covered by the molded resin part 4. The molded resin part 4 is provided between the winding part 21 and the first middle core part 31f, and between the winding part 21 and the second middle core part 31s. Furthermore, the molded resin part 4 is provided at least in a part between the end face 312 and the end face 318. In this embodiment, the molded resin part 4 is provided between the outer end face 313 and the end face 318 as shown in FIG. 6. Since the molded resin portion 4 has a portion provided between the outer end face 313 and the end face 318, thermal conduction between the first core portion 3f and the second core portion 3s is likely to be high, and therefore the reactor 1 has excellent heat dissipation properties. The molded resin portion 4 is not substantially provided between the inner end face 315 and the end face 318. The molded resin portion 4 integrates the coil 2 and the magnetic core 3.

[0087] An example of the resin of the molded resin portion 4 is the same as the resin of the above-mentioned compact of the composite material. The resin of the molded resin portion 4 may contain a ceramic filler, like the compact of the composite material.

[0088] [others] Although not shown, the reactor 1 may include at least one of a case, an adhesive layer, and a holding member. The case houses the assembly of the coil 2 and the magnetic core 3 inside. The assembly in the case may be embedded with a sealing resin portion. The case is placed on a cooling base or the like. The adhesive layer fixes the assembly to the cooling base or the inner bottom surface of the case, or fixes the case to the cooling base or the like. The holding member is provided between the coil 2 and the magnetic core 3, and ensures insulation between the coil 2 and the magnetic core 3.

[0089] [Effects of the First Embodiment] Reactor 1 has a high filling property of molded resin portion 4 in gap portion 3g. This is because area Si / area Se is 1.35 or less and length Lge / length Lgi is 3.00 or more, so that the constituent material of molded resin portion 4 filled inside winding portion 21 easily spreads between end face 312 and end face 318.

[0090] The reactor 1 has a high inductance because the ratio of the area Si / area Se is 0.30 or more, so that the ratio of the inner gap portion 3gi is appropriately secured, and because the length Lge / length Lgi is 15.00 or less, so that the length Lge is not too large.

[0091] The reactor 1 has excellent heat dissipation properties. This is because, as shown in Fig. 2, the winding portion 21 includes a portion that contacts the installation target 100, and thus the heat of the coil 2 can be effectively dissipated through the installation target 100. In addition, as shown in Fig. 6, the molded resin portion 4 has a portion provided between the outer end face 313 and the end face 318, and thus the thermal conduction between the first core portion 3f and the second core portion 3s is likely to be high.

[0092] The reactor 1 has low loss. This is because the length L1s is shorter than the length L1f, and therefore the proportion of powder compacts, which have higher loss than the compacts of the composite material, is low. In addition, the gap portion 3g is disposed inside the winding portion 21, and the length Le is 0.2 times or more the length of the winding portion 21, and therefore leakage flux is unlikely to enter the winding portion 21. This makes it easy to reduce eddy current loss occurring in the winding portion 21. Furthermore, the length Le is 0.49 times or less the length of the winding portion 21, and therefore it is possible to increase the proportion of the compacts of the composite material, which have lower loss than the powder compacts, inside the winding portion 21.

[0093] Second Embodiment A reactor 1 according to a second embodiment will be described with reference to Fig. 7. The reactor 1 according to this embodiment differs from the reactor 1 according to the first embodiment in that the combination of the first core portion 3f and the second core portion 3s is an EE type. That is, the planar shape of the first core portion 3f and the planar shape of the second core portion 3s in this embodiment are E-shaped. The following description will focus on the differences from the first embodiment. Description of the same configuration as the first embodiment will be omitted.

[0094] (First core part) The first core portion 3f of this embodiment has a first end core portion 33f, a first middle core portion 31f, a first side core portion 321f, and a second side core portion 322f. The first core portion 3f of this embodiment differs from the first embodiment in that the length L21f of the first side core portion 321f and the length L22f of the second side core portion 322f are shorter than the length L21 of the first side core portion 321 and the length L22 of the second side core portion 322 of the first embodiment.

[0095] (Second core part) The second core portion 3s of this embodiment has a second end core portion 33s, a second middle core portion 31s, a first side core portion 321s, and a second side core portion 322s. The second core portion 3s is an integrally molded body of the second end core portion 33s, the second middle core portion 31s, the first side core portion 321s, and the second side core portion 322s. The second end core portion 33s connects the second middle core portion 31s, the first side core portion 321s, and the second side core portion 322s. The first side core portion 321s and the second side core portion 322s are provided at both ends of the second end core portion 33s. The second middle core portion 31s is provided in the center of the second end core portion 33s. The first side core portion 321s and the second side core portion 322s are shaped like thin rectangular columns.

[0096] In this embodiment, the first core portion 3f and the second core portion 3s are different in size. fThe length L21s of the first side core portion 321s along the first direction D1 and the length L22s of the second side core portion 322s along the first direction D1 are the same. The lengths L21f and L22f are longer than the length L1f. The length L21s of the first side core portion 321s along the first direction D1 and the length L22s of the second side core portion 322s along the first direction D1 are the same. The lengths L21s and L22s are longer than the length L1s. The length L1f is longer than the length L1s. The length L21f is longer than the length L21s and the length L22f is longer than the length L22s. The lengths L3f and L3s are the same.

[0097] The first middle core portion 31f and the second middle core portion 31s have the same length along the second direction D2. The first side core portion 321f, the first side core portion 321s, the second side core portion 322f, and the second side core portion 322s have the same length along the second direction D2. The first end core portion 33f and the second end core portion 33s have the same length along the second direction D2. The lengths of the core portions along the third direction D3 are the same. The length of each core portion along the third direction D3 is shorter than the length of the winding portion 21 along the third direction D3.

[0098] The first core portion 3f and the second core portion 3s are assembled so that the end faces of the first side core portion 321f and the second side core portion 322f are in contact with the end faces of the first side core portion 321s and the second side core portion 322s, respectively. Middle Core 3 1 A gap 3g is provided between the end face of the substrate s.

[0099] [Effects of the second embodiment] In the reactor 1 of this embodiment, similarly to the reactor 1 of the first embodiment, the molded resin portion 4 is highly filled into the gap portion 3g. The reactor 1 also has a high inductance. Furthermore, the reactor 1 has an excellent heat dissipation property. And the reactor 1 has a low loss.

[0100] Third Embodiment [Converter / Power Conversion Device] The reactor 1 of the first and second embodiments can be used for applications that satisfy the following energization conditions. For example, the energization conditions include a maximum DC current of about 100 A to 1000 A, an average voltage of about 100 V to 1000 V, and a usage frequency of about 5 kHz to 100 kHz. The reactor 1 of the first and second embodiments can be used as a component of a converter mounted on a vehicle 1200, typically an electric vehicle, a hybrid vehicle, or a fuel cell vehicle, or as a component of a power conversion device including the converter.

[0101] As shown in Fig. 8, the vehicle 1200 includes a main battery 1210, a power conversion device 1100 connected to the main battery 1210, and a motor 1220 that is driven by power supplied from the main battery 1210 and used for traveling. The motor 1220 is typically a three-phase AC motor that drives wheels 1250 during traveling and functions as a generator during regeneration. In the case of a hybrid vehicle, the vehicle 1200 includes an engine 1300 in addition to the motor 1220. Although Fig. 8 shows an inlet as a charging point for the vehicle 1200, a form including a plug may also be used.

[0102] The power conversion device 1100 includes a converter 1110 connected to a main battery 1210, and an inverter 1120 connected to the converter 1110 and performing mutual conversion between direct current and alternating current. The converter 1110 shown in this example boosts the input voltage of the main battery 1210, which is about 200V to 300V, to about 400V to 700V when the vehicle 1200 is running, and supplies power to the inverter 1120. During regeneration, the converter 1110 lowers the input voltage output from the motor 1220 via the inverter 1120 to a direct current voltage suitable for the main battery 1210, and charges the main battery 1210. The input voltage is a direct current voltage. When the vehicle 1200 is running, the inverter 1120 converts the DC boosted by the converter 1110 into a predetermined AC and supplies it to the motor 1220. During regeneration, the inverter 1120 converts the AC output from the motor 1220 into DC and outputs it to the converter 1110.

[0103] As shown in FIG. 9, the converter 1110 includes a plurality of switching elements 1111, a drive circuit 1112 that controls the operation of the switching elements 1111, and a reactor 1115, and converts the input voltage by repeatedly switching on and off. The conversion of the input voltage means stepping up and down the voltage here. The switching elements 1111 are power devices such as field effect transistors and insulated gate bipolar transistors. The reactor 1115 has a function of smoothing the change when the current increases or decreases due to the switching operation by utilizing the property of a coil that prevents a change in the current flowing through the circuit. The reactor 1 of the first embodiment is included as the reactor 1115. By including the reactor 1, the power conversion device 1100 and the converter 1110 have excellent performance.

[0104] In addition to the converter 1110, the vehicle 1200 includes a converter 1150 for a power supply device connected to the main battery 1210, and a converter 1160 for an auxiliary power supply connected to a sub-battery 1230 serving as a power source for the auxiliary devices 1240 and the main battery 1210 to convert the high voltage of the main battery 1210 to a low voltage. The converter 1110 typically performs DC-DC conversion, while the converter 1150 for a power supply device and the converter 1160 for an auxiliary power supply perform AC-DC conversion. Some of the converters 1150 for a power supply device perform DC-DC conversion. The reactors of the converter 1150 for a power supply device and the converter 1160 for an auxiliary power supply may have the same configuration as the reactor 1 of the first embodiment, and may be reactors whose size, shape, and the like are appropriately changed. The reactor 1 of the first embodiment may also be used as a converter that converts input power and that performs only step-up or step-down.

[0105] Test Example The above-mentioned area Si / area S eThe difference in inductance and loss of the reactor due to the difference in area Si / length Lge or the difference in length Lge / length Lgi was investigated. In this test example, the reactor that was actually manufactured was not evaluated, but the reactor was constructed on the simulation software and the area Si / length Lgi was calculated. area S e An analytical model was evaluated in which length Lge / length Lgi was set.

[0106] [Sample No. 1 to Sample No. 16] As the analytical models of samples No. 1 to No. 16, an assembly of a coil 2 and a magnetic core 3 as shown in Fig. 1 was constructed. In other words, the analytical models of each sample did not include a molded resin portion 4 as shown in Fig. 1.

[0107] The end face of the first middle core portion 31f in each sample was the same as the end face 312 having the outer end face 313, the circumferential surface 314, and the inner end face 315 described with reference to FIG. 3. The shape of the inner end face in each sample was as shown in Table 1 or Table 2. true The shape was a circle or a square. The four corners of the inner end face and the four corners of the outer end face of Sample No. 2 to Sample No. 16 were rounded. The area Si, area Se, and area Si / area Se of each sample are shown in Table 1 or Table 2. Area Si is the area of ​​the inner end face, and area Se is the area of ​​the outer end face. Area Si was adjusted to adjust area Si / area Se. Area Si / area Se in each table is rounded to two decimal places.

[0108] The end face of the second middle core portion 31s in each sample was a flat surface. The length Lge, length Lgi, and length Lge / length Lgi in each sample are shown in Table 1 or Table 2. Length Lge is the thickness of the outer gap portion, and length Lgi is the thickness of the inner gap portion. Length Lge / length Lgi was adjusted by adjusting the length of the peripheral surface. Length Lge / length Lgi in each table is rounded to two decimal places.

[0109] The length Le in each sample was 0.2 to 0.49 times the length of the wound portion 21 along the first direction D1. The ratio of the length Lge to the total length of the lengths L1f, L1s, and Lge in each sample was 0.02 to 0.05. The ratio (Lt / Lc) of the length Lt to the length Lc in each sample was about 0.14. In each sample, the distance between the inner peripheral surface of the wound portion 21 and the outer peripheral surfaces of the first middle core portion 31f and the second middle core portion 31s was about 2.5 mm.

[0110] [Sample No. 100] Sample No. 100 was similar to Sample No. 1, etc., except that the end face of the first middle core portion 31f was flat and the thickness of the gap portion was 1.0 mm.

[0111] 〔analysis〕 For the analysis, one of two members obtained by cutting each sample along a plane passing through the center of the coil 2 and parallel to the first direction D1 and the third direction D3 was used. The analysis software used was the electromagnetic field analysis software JMAG-Designer Ver.20.1 made by JSOL Corporation. The analysis method used was magnetic field transient response analysis (solution method: A-φ method 2).

[0112] [Inductance] Currents ranging from 1 A to 400 A were applied to the coil, and the inductance was calculated from the amount of magnetic flux linkage in the coil at each current value obtained by analysis. The maximum value of the calculated inductance is shown in Table 1 or Table 2. The inductance shown in each table is a percentage when the maximum inductance value of sample No. 100 is set to 100.

[0113] [loss] A voltage of a specific frequency was applied to the coil, and the joule loss of the coil and the iron loss of the magnetic core were calculated based on the magnetic flux density distribution and the current density distribution. The calculated coil loss and total loss are shown in Table 1 or Table 2. The total loss was calculated based on the coil loss and the magnetic core loss. The coil loss and total loss shown in each table are each a percentage (%) when the coil loss and total loss of sample No. 100 are each set to 100.

[0114] [Table 1]

[0115] [Table 2]

[0116] As shown in Table 1, the maximum inductance values ​​of Samples No. 4 to No. 7 were equal to or greater than the maximum inductance value of Sample No. 100, and were greater than the maximum inductance values ​​of Samples No. 1 to No. 3. In addition, the coil loss of Samples No. 4 to No. 7 was equal to or less than the coil loss of Sample No. 100, and was smaller than the coil loss of Samples No. 1 to No. 3. The total loss of Samples No. 4 to No. 7 was equal to the total loss of Sample No. 100, and was smaller than the total loss of Samples No. 1 to No. 3.

[0117] As shown in Table 2, the maximum inductance values ​​of Samples No. 9 to No. 11 were equal to or greater than the maximum inductance value of Sample No. 100, and were greater than the maximum inductance values ​​of Samples No. 12 to No. 16. The coil loss of Samples No. 9 to No. 11 was equal to or less than the coil loss of Sample No. 100, and was smaller than the coil loss of Samples No. 12 to No. 16. The total loss of Samples No. 9 to No. 11 was equal to the total loss of Samples No. 12 to No. 16 and Sample No. 100.

[0118] The filling of the molded resin portion into the gap was investigated using resin flow analysis software Moldex 3D studio 2020 manufactured by JSOL Corporation. The molded resin portion was polyphenylene sulfide resin containing glass fiber fibers. The constituent material of the molded resin portion was filled from the outside of the above-mentioned assembly toward the inside of the winding portion 21. The filling of the resin between the end face of the first middle core portion 31f and the end face of the second middle core portion 31s was visually confirmed together with the contour diagram. As a result, the larger the area Se, the greater the amount of the molded resin portion filled into the outer gap portion. In particular, the amount of the molded resin portion filled into the outer gap portion was greater in Samples No. 1 to No. 7 and Samples No. 9 to No. 16 compared to Sample No. 8. In addition, in Samples No. 1 to No. 16, the molded resin portion was not substantially filled into the inner gap portion. In Sample No. 100, the molded resin portion was not substantially filled into the gap portion.

[0119] From the above results, it was found that Samples No. 4 to No. 7 and Samples No. 9 to No. 11 had high filling properties of the mold resin in the gap and high inductance.

[0120] The present invention is not limited to these examples, but is defined by the claims, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0121] 1 Reactor 2 Coil 21 winding portion, 21a first end portion, 21b second end portion 25 Outer surface 3 magnetic core, 3f first core part, 3s second core part 31F First Middle Core Section 311 Outer surface 312 End face 313 Outer end face, 314 Peripheral face, 315 Inner end face 31s Second Middle Core Section 318 End face 321, 321f, 321s First side core part 322, 322f, 322s Second side core part 33f first end core part, 33s second end core part 3g Gap section 3ge outer gap, 3gi inner gap 4 Molded resin part L1f, L1s length L21, L21f, L21s length, L22, L22f, L22s length L3f, L3s length Le Length D1 first direction, D2 second direction, D3 third direction Area A 100 Installation targets 1100 Power Converter, 1110 Converter 1111 switching element, 1112 drive circuit, 1115 reactor 1120 Inverter 1150 Converter for power supply device, 1160 Converter for auxiliary power supply 1200 vehicles 1210 Main battery, 1220 Motor, 1230 Sub battery 1240 Auxiliary equipment, 1250 Wheels 1300 Engine

Claims

1. A coil having a cylindrical winding portion; a magnetic core including a first core portion and a second core portion combined in an axial direction of the winding portion, and a gap portion provided between the first core portion and the second core portion; a molded resin portion covering at least a portion of the magnetic core, The number of the windings is one, The first core portion has an E-shape, The second core portion has a T-shape or an E-shape, the first core portion is a composite material molded body having a first middle core portion disposed inside the winding portion, the second core portion is a powder compact having a second middle core portion disposed inside the winding portion, the gap portion is disposed inside the winding portion between an end surface of the first middle core portion and an end surface of the second middle core portion, The end surface of the first middle core portion is an annular outer end surface connected to an outer peripheral surface of the first middle core portion; a circumferential surface extending from the outer end surface toward an end surface of the second middle core portion; an inner end surface connected to a tip of the peripheral surface; The end surface of the second middle core portion is a flat surface, the outer end surface and the inner end surface are flat surfaces, a ratio of an area of ​​the inner end face to an area of ​​the outer end face is 0.30 or more and 1.35 or less; the molded resin portion has a portion provided between the outer end surface and an end surface of the second middle core portion. Reactor.

2. 2. The reactor according to claim 1, wherein a ratio of a length between the outer end face and the end face of the second middle core portion to a length between the inner end face and the end face of the second middle core portion is 3.00 or more and 15.00 or less.

3. a length of the winding portion in the second middle core portion along the axial direction is shorter than a length of the winding portion in the first middle core portion along the axial direction; 3. The reactor according to claim 1, wherein a length from an end face of the winding portion facing the second core portion to the gap portion is 0.2 to 0.49 times the length of the winding portion.

4. 4. The reactor according to claim 1, wherein a ratio of a thickness of the gap portion to a total length of a length of the winding portion in the axial direction of the first middle core portion, a length of the winding portion in the axial direction of the second middle core portion, and a thickness of the gap portion is 0.02 or more and 0.05 or less.

5. The reactor according to claim 1 , wherein a thickness of the gap portion is equal to or greater than 1.0 mm and equal to or less than 2 mm.

6. The powder compact is a compact of a raw material powder containing a soft magnetic powder, The reactor according to claim 1 , wherein a content of the soft magnetic powder in the powder compact is 85 vol % or more and 99 vol % or less.

7. The composite material molded body is a molded body in which soft magnetic powder is dispersed in a resin, The reactor according to claim 1 , wherein a content of the soft magnetic powder in the compact of the composite material is 20% by volume or more and 80% by volume or less.

8. A reactor according to any one of claims 1 to 7, converter.

9. A converter comprising: Power conversion equipment.

Citation Information

Patent Citations

  • Reactor

    JP2015008236A

  • Reactor

    JP2017139310A

  • Inductor and manufacturing method therefor

    WO2013001592A1

  • Inductor and manufacturing method therefor

    WO2013001593A1