Thermal Switch

A thermal switch using a flexible elastomer with a high thermal expansion coefficient and conductive filler addresses the instability and responsiveness issues of ceramic-based switches, ensuring stable and efficient heat management in battery packs.

JP7569710B2Active Publication Date: 2024-10-18SUMITOMO RIKO CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2021034883
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-05
Publication Date
2024-10-18
Estimated Expiration
2041-03-05

AI Technical Summary

Technical Problem

Existing thermal switches using ceramics for thermal expansion members have low thermal conductivity and poor responsiveness to temperature changes, leading to instability in connection states and inadequate insulation or heat dissipation.

Method used

A thermal switch utilizing a flexible elastomer with a high average linear thermal expansion coefficient and thermally conductive filler, allowing for reversible volume changes with temperature, providing stable connection states and efficient heat dissipation.

Benefits of technology

The thermal switch achieves high responsiveness to temperature changes, ensuring stable connection states and effective heat dissipation or retention, preventing damage to battery cells and optimizing battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569710000003
    Figure 0007569710000003
  • Figure 0007569710000004
    Figure 0007569710000004
  • Figure 0007569710000005
    Figure 0007569710000005
Patent Text Reader

Abstract

To provide a thermal switch superior in switching between the heat dissipation property and the heat retaining property by improving a material of an elastic thermal expansion member of which the volume reversibly changes accompanying the change in temperature.SOLUTION: A thermal switch comprises: a first base material; a second base material; and an elastic thermal expansion member interposed between the first and second base materials, connecting the first and second base materials as the expansion under a given temperature condition, and forming a heat transfer path from the first base material to the second base material. The elastic thermal expansion member is a crosslinked material of a composition containing (A) a crosslinkable elastomer, (B) a heat-conducting filler, and (C) a crosslinking agent. The elastic thermal expansion member has an average linear thermal expansion coefficient of 1×10-4 / K to 10×10-4 / K in a range of 0-100°C.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a thermal switch whose thermal conductivity changes with temperature. [Background technology]

[0002] Hybrid and electric vehicles are equipped with battery packs that contain multiple battery cells. In battery packs, the internal resistance increases as the temperature decreases, so insulation is required to promote the rise of heat at low temperatures. In addition, if the temperature becomes too high, there is a concern that the battery may be damaged, so heat dissipation is required at high temperatures.

[0003] As such a technique, a thermal switch is disclosed in which the thermal conductivity differs between a connected state in which the first protective layer, the second protective layer, and the thermal expansion member are in contact with each other and a non-connected state in which they are not in contact with each other (Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] International Publication No. 2014 / 156991 Summary of the Invention [Problem to be solved by the invention]

[0005] However, in Patent Document 1, ceramics is used for the thermal expansion member, and although the thermal conductivity is high and the heat dissipation is good in the connected state, the average linear thermal expansion coefficient is low, so the gap precision is required, and the expansion change due to temperature change is small, so the response as a thermal switch to temperature change is not good. In addition, if the gap is 0.1 to 100 μm, the expansion and contraction of the cell itself may not be absorbed, or sufficient insulation may not be achieved in the unconnected state. Furthermore, since the thermal expansion member and the protective layer are hard, there are problems such as an unstable connection state and the thermal expansion member may destroy the cell during thermal expansion.

[0006] The present invention has been made in view of the above circumstances, and aims to provide a thermal switch that is excellent in switching between heat dissipation and heat retention by improving the material of a thermal expansion member whose volume reversibly changes with temperature change, and also aims to provide a battery pack having the thermal switch. [Means for solving the problem]

[0007] In order to solve the above problems, the thermal switch of the present invention has a thermal expansion member made of a flexible elastomer having a large average linear thermal expansion coefficient and a thermally conductive filler, thereby solving the above problems.

[0008] A thermal switch comprising: a first substrate; a second substrate; and an elastic thermal expansion member interposed between the first substrate and the second substrate, the elastic thermal expansion member expanding under a predetermined temperature condition to connect the first substrate and the second substrate and to form a heat transfer path between the first substrate and the second substrate, The elastic thermal expansion member includes a thermosetting elastomer and a thermally conductive filler dispersed in the thermosetting elastomer; The elastic thermal expansion member has an average linear thermal expansion coefficient of 1×10 -4 / K~10×10 -4 / K. Effect of the Invention

[0009] The thermal switch of the present invention has a heat-retaining effect because the elastic thermal expansion member is in a disconnected state at room temperature or low temperatures, and at high temperatures the elastic thermal expansion member is in a connected state due to thermal expansion, so that heat is transferred from the elastic thermal expansion member and the switch functions as a heat dissipation switch.

[0010] In this way, by using a thermosetting elastomer with a large average linear thermal expansion coefficient and a thermally conductive filler for the elastic thermal expansion member, the thermal switch of the present invention has a large expansion change in response to a temperature change, and therefore has high responsiveness as a thermal switch to a temperature change. In addition, since the elastic thermal expansion member is flexible, the connection state with the mating material is stable and the mating material is not destroyed during thermal expansion. [Brief description of the drawings]

[0011] [Figure 1] FIG. 1 is a schematic cross-sectional view showing a first embodiment of a thermal switch of the present invention. [Diagram 2] FIG. 2 is a schematic cross-sectional view showing a second embodiment of the thermal switch of the present invention. [Diagram 3] FIG. 4 is a schematic cross-sectional view showing a third embodiment of the thermal switch of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, the embodiment of the thermal switch of the present invention will be described. Note that the thermal switch of the present invention is not limited to the following embodiment, and can be embodied in various forms by applying modifications and improvements that can be made by those skilled in the art within the scope of the gist of the present invention.

[0013] First Embodiment First, the configuration of the thermal switch 1 of this embodiment will be described. The left side of FIG. 1 shows the thermal switch 1 in a disconnected state of the elastic thermal expansion member 10 made of a thermosetting elastomer, and the right side of FIG. 1 shows the thermal switch 1 in a connected state of the elastic thermal expansion member 10 made of a thermosetting elastomer. As shown in FIG. 1, below a predetermined temperature, the elastic thermal expansion member 10 and the second base material 12 are not in contact with each other and have a gap (disconnected state). On the other hand, when the ambient temperature is raised to a predetermined temperature or higher by a heat source, the elastic thermal expansion member 10 and the second base material 12 are connected to each other and form a heat transfer path (connected state). Since the elastic thermal expansion member 10 is formed of a material whose volume reversibly changes with temperature change, when the ambient temperature falls below a predetermined temperature, the elastic thermal expansion member 10 contracts, causing the elastic thermal expansion member 10 and the second base material 12 to become disconnected, and a gap is generated again. Furthermore, the heat source that increases the ambient temperature may be on the first substrate side, may be on the second substrate side, or may be on both the first substrate side and the second substrate side.

[0014] The size of the gap is determined in accordance with the relationship between the material properties of the elastic thermal expansion member 10 and the usage environment so that the elastic thermal expansion member 10, the first base material 11, and the second base material 12 are connected by the thermal expansion of the elastic thermal expansion member 10, enabling thermal conduction. The size of the gap is not particularly limited as long as it satisfies the above requirements. Specifically, when the predetermined temperature is 100°C and the linear thermal expansion coefficient of the elastic thermal expansion member 10 is 4×10 -4 In the case where the elastic thermal expansion member 10 has a thickness of 10 mm and the shortest distance between the elastic thermal expansion member 10 and the second substrate 12 is 0.3 mm or less at room temperature (23° C.), the elastic thermal expansion member 10 and the second substrate 12 come into contact with each other at 100° C., and a heat dissipation effect is achieved. In addition, the elastic thermal expansion member 10 expands not only in the direction along the first substrate 11 and the second substrate 12, but also in the direction perpendicular to the direction along the first substrate 11 and the second substrate 12 when the ambient temperature rises. Therefore, it is preferable to provide a restricting member (not shown) having a small linear thermal expansion coefficient that restricts thermal expansion on four surfaces of the elastic thermal expansion member 10 other than the surfaces in contact with the first substrate 11 and the second substrate 12, because the thermal expansion of the elastic thermal expansion member 10 in the direction along the first substrate 11 and the second substrate 12 is larger than that in the case where the restricting member is not provided.

[0015] Second Embodiment FIG. 2 is a schematic cross-sectional view showing a second embodiment of the thermal switch 1 of the present invention. The difference from the thermal switch 1 of the first embodiment is that the elastic thermal expansion member 10 is fixed to the connecting member 13, the elastic thermal expansion member 10 does not contact the first base material 11 and the second base material 12 below a predetermined temperature, and a heat insulating member 14 is provided on a part or all of the connecting member 13. In this case, the elastic thermal expansion member 10 contacts the first base material 11 and the second base material at a predetermined temperature. In addition, by providing the heat insulating member 14, the first base material 11 and the second base material 12 are reliably insulated from each other below a predetermined temperature. Here, an example is given in which the elastic thermal expansion member 10 does not contact the first base material 11 and the second base material below a predetermined temperature, but the elastic thermal expansion member 10 may contact the first base material 11 and not contact the second base material 12 below a predetermined temperature, or the elastic thermal expansion member 10 may contact the second base material 12 and not contact the first base material 11.

[0016] <Third embodiment> 3 is a schematic cross-sectional view showing a third embodiment of the thermal switch 1 of the present invention. The difference from the thermal switch 1 of the first embodiment is that the elastic thermal expansion member 10 of the first embodiment is interposed between the first substrate 11 and the second substrate 12, but in this embodiment, the elastic thermal expansion member 10 is arranged so as to contact the side surfaces of the first substrate 11 and the second substrate 12. Even if the elastic thermal expansion member 10 is arranged in a space other than the space where the first substrate 11 and the second substrate 12 face each other, the elastic thermal expansion member 10 forms a heat transfer path between the first substrate 11 and the second substrate 12 in the connected state, and such an embodiment is also included in the expression that the elastic thermal expansion member is interposed between the first substrate and the second substrate.

[0017] The elastic thermal expansion member is preferably made of a material whose volume changes reversibly with temperature change, and whose dimensions increase by 1% or more when the temperature rises by 100° C. If the dimensions increase by less than 1%, the elastic thermal expansion member may not function as a switch in actual use, and its responsiveness to temperature changes will be poor. The average linear thermal expansion coefficient of an elastic thermal expansion material when the temperature changes from 0°C to 100°C is 1×10 -4 / K~10×10 -4 / K. The average linear thermal expansion coefficient when the temperature is changed from 0°C to 100°C is more preferably in the range of 1×10 -4 If the average linear thermal expansion coefficient is less than 10×10 / K, the dimensional change of the elastic thermal expansion member is too small, and the gap between the elastic thermal expansion member and the first and second substrates must be precisely set, and the responsiveness to temperature changes may be poor. -4 If the gap is larger than 1 / K, the elastic thermal expansion member will expand too much, and if a gap is created to allow for this expansion, the effect of the thermally conductive filler will be reduced, which may result in a decrease in thermal conductivity and poor heat dissipation, which is not desirable.

[0018] The elastic thermal expansion member has a thermosetting elastomer and a thermally conductive filler dispersed in the thermosetting elastomer. Here, the thermosetting elastomer is an elastomer vulcanized or crosslinked by a vulcanizing agent or a crosslinking agent. Examples of the thermosetting elastomer include silicone rubber, urethane rubber, fluororubber, acrylic rubber, natural rubber, butadiene rubber, chlorinated polyethylene, epichlorohydrin rubber, and chlorosulfonated polyethylene. The thermosetting elastomer may be a solid or a foam.

[0019] The thermal conductivity of the elastic thermal expansion member is 0.25 W / m·K or more. A suitable thermal conductivity is 0.4 W / m·K or more, and more preferably 0.5 W / m·K or more. From the viewpoint of increasing the thermal conductivity of the elastic thermal expansion member, it is desirable that the elastic thermal expansion member has a thermally conductive filler with a relatively high thermal conductivity. A suitable thermal conductivity of the thermally conductive filler used to increase the thermal conductivity of the elastic thermal expansion member is 20 W / m·K or more. Examples of thermally conductive fillers with a relatively high thermal conductivity include magnesium oxide, aluminum oxide, aluminum nitride, boron nitride, silicon carbide, metal powder, graphite, graphene oxide, ferrite, etc. In particular, when used in batteries, etc., a thermally conductive filler with insulating properties is preferable in consideration of the possibility of leakage current. Examples of thermally conductive fillers with insulating properties include magnesium oxide, aluminum oxide, aluminum nitride, boron nitride, silicon carbide, etc.

[0020] The content of the thermally conductive filler in the elastic thermal expansion member is 20 to 350 parts by mass, preferably 50 to 300 parts by mass, and more preferably 100 to 250 parts by mass, per 100 parts by mass of the elastomer. If the thermally conductive filler is 20 parts by mass or less, the thermal conductivity of the elastic thermal expansion member becomes less than 0.25 W / m·K, and the heat dissipation may deteriorate. If the thermally conductive filler is 350 parts by mass or more, the thermal linear expansion coefficient of the thermal conductive filler decreases, and the responsiveness as a thermal switch may deteriorate. The thermally conductive filler may be oriented to increase the thermal linear expansion coefficient while maintaining the thermal conductivity of the elastic thermal expansion member. As a method for orienting the thermally conductive filler, a thermally conductive filler with a large aspect ratio and an elastomer may be extrusion molded, or magnetic particles may be added to the thermally conductive anisotropic particles and the elastomer, and orientation may be performed by a magnetic field.

[0021] [Orientation by magnetic field] As an example of reducing the thermally conductive filler in the elastic thermal expansion member, orientation by a magnetic field will be described. As the thermally conductive filler oriented by a magnetic field, composite particles consisting of thermally conductive anisotropic particles, magnetic particles, and a binder are used. The thermally conductive anisotropic particles are particles having anisotropy in thermal conduction, that is, particles whose thermal conductivity varies depending on the direction, and have a large thermal conductivity in the direction of the crystal plane. The thermal conductivity of the thermally conductive anisotropic particles in the direction of the crystal plane is preferably 150 W / m·K or more. The shape of the thermally conductive anisotropic particles is preferably flaky. The thermally conductive anisotropic particles may be non-magnetic particles. Examples of the thermally conductive anisotropic particles include boron nitride particles and graphite particles.

[0022] The magnetic particles may be any particles having excellent magnetic properties, and may be, for example, ferromagnetic materials such as iron, nickel, cobalt, gadolinium, stainless steel, magnetite, maghemite, manganese zinc ferrite, barium ferrite, and strontium ferrite, MnO, Cr 2 O 3 , FeCl 2 In view of the fact that they are easily available as fine particles and have high saturation magnetization, powders of iron, nickel, cobalt, and ferritic alloys thereof are preferably used.

[0023] The magnetic particles are attached to the surfaces of the thermally conductive anisotropic particles and serve to orient the thermally conductive anisotropic particles. The magnetic particles may be attached to only a portion of the surfaces of the thermally conductive anisotropic particles, or may be attached so as to cover the entire surfaces.

[0024] The binder for bonding the thermally conductive anisotropic particles and the magnetic particles is preferably a water-soluble binder, since it has little effect on moldability and is environmentally friendly. Examples of such binders include methyl cellulose, carboxymethyl cellulose, hydroxypropyl methyl cellulose, and polyvinyl alcohol.

[0025] Since boron nitride particles are electrically insulating, the use of boron nitride particles as thermally conductive anisotropic particles is advantageous for applications requiring insulation. however , Attach to or coat a surface When conductive particles are used as magnetic particles, the insulating properties of the elastic thermal expansion member are reduced. Therefore, when insulating properties are required for the elastic thermal expansion member, such as for heat dissipation applications in batteries and electronic components, magnetic particles are used. Even in It is preferable to use insulating particles. As electrically insulating particles, iron oxide particles, manganese ferrite particles, etc., which are themselves insulating, are suitable.

[0026] The content of the thermally conductive anisotropic particles in the elastic thermal expansion member may be appropriately determined according to the type of the thermally conductive anisotropic particles. If the content of the thermally conductive anisotropic particles is too small, the heat transfer path is not sufficiently formed. Therefore, in order to obtain the effect of improving the thermal conductivity, the content of the thermally conductive anisotropic particles is preferably 20 parts by mass or more when the mass of the thermosetting elastomer is 100 parts by mass. On the other hand, from the viewpoint of reducing the influence of moldability and physical properties and preventing high costs, the content of the thermally conductive anisotropic particles is preferably 300 parts by mass or less when the mass of the thermosetting elastomer is 100 parts by mass.

[0027] The manufacturing method of the present invention for orienting thermally conductive anisotropic particles in an elastomer by a magnetic field includes a composite particle manufacturing step, a raw material mixing preparation step, and a molding step.

[0028] First, the composite particles are produced by mixing the respective powders using a mixing granulator.

[0029] The elastomer raw material contains, in addition to the elastomer component, as necessary, a retarder, a plasticizer, a catalyst, a foaming agent, a foam stabilizer, a flame retardant, an antistatic agent, a viscosity reducer, a stabilizer, a filler, a colorant, etc. The mixed raw material may be prepared by stirring and mixing the thermally conductive particles and the elastomer raw material using an intermixer, a stirring blade, etc.

[0030] In the molding process, the mixed raw material prepared in the previous process is placed in a mold and molded in a magnetic field.

[0031] The molding die may be either closed or open. The magnetic field may be formed in the direction in which the thermally conductive anisotropic particles are oriented. For example, when aligning the thermally conductive anisotropic particles in a linear manner, it is desirable to apply magnetic field lines from one end of the mixed raw material to the other end. To form such a magnetic field, magnets may be arranged to sandwich the mixed raw material. The magnets may be permanent magnets or electromagnets. When an electromagnet is used, the magnetic field can be instantly switched on and off, making it easy to control the strength of the magnetic field.

[0032] In this process, it is desirable to apply a magnetic field with a substantially uniform magnetic flux density to the mixed raw material. Specifically, the difference in magnetic flux density in the mixed raw material should be within ±10%, and more preferably within ±5%, and even more preferably within ±3%. By applying a uniform magnetic field to the mixed raw material, uneven distribution of the thermally conductive anisotropic particles can be suppressed, and a desired orientation state can be obtained. Furthermore, molding should be performed at a magnetic flux density of 150 mT or more and 1200 mT or less. In this way, the thermally conductive anisotropic particles in the mixed raw material can be reliably oriented. After molding is completed in this process, the material is demolded and cross-linked to obtain the elastic thermal expansion member of the present invention.

[0033] In the thermal switch of the present invention, the elastic thermal expansion member may be fixed to the connecting member, the first base material, and the second base material by caulking with a metal member or the like, or by using an adhesive.

[0034] [Materials other than elastic thermal expansion materials] The first and second substrates are not particularly limited as long as they have thermal conductivity, but it is preferable that the thermal conductivity of the material is high. Specifically, it is preferable that the first and second substrates are formed of a material having a thermal conductivity of 1 to 500 W / mK. The higher the thermal conductivity of the material, the greater the difference in apparent thermal conductivity between the connected and unconnected states of the thermal switch, so that insulation and heat dissipation work efficiently. The material forming the first and second substrates is preferably a metal or an alloy.

[0035] The material of the connecting member is not particularly limited as long as it has heat insulating properties. The material of the connecting member is preferably one that has relatively little thermal expansion in response to thermal changes, and may be one that has low thermal conductivity, such as resin or elastomer. In addition, a heat insulating material may be provided in part of the connecting member to improve heat retention.

[0036] The heat insulating material should insulate against heat, and its thermal conductivity should preferably be 0.2 W / m K or less. In addition, it is preferable that the average linear thermal expansion coefficient is not large, and the average linear thermal expansion coefficient when the temperature changes from 0°C to 100°C should be less than 1×10 -6 / K~5×10 -4 It is preferable that the range is 1 / K.

[0037] The heat insulating member is not particularly limited, but is preferably a resin or an elastomer from the viewpoint of heat insulating properties. The resin and elastomer are preferably any one selected from the group consisting of acrylic, urethane, silicone, polystyrene, latex, synthetic rubber, polyester, polyvinyl alcohol, polypropylene, polyethylene, polyfluorocarbon, polycarbonate, polyamide, polyphenylene ether, polyacetal, polybutylene terephthalate, polyether ether ketone, epoxy resin, phenol resin, polyphenylene sulfide, and polyimide.

[0038] To further improve thermal insulation, ceramic particles such as titania, alumina, and zirconia, silica, silica aerogel, glass fiber, aramid fiber, and other engineering plastics and super engineering plastic fibers may be mixed into resin and elastomer foams, and resin and elastomers. From the viewpoint of high thermal insulation in a small space, silica aerogel (thermal conductivity: 0.025 W / m K) and ALC panels (thermal conductivity: 0.17 W / m K) are particularly preferable.

[0039] In the thermal switch of the present invention, the method of providing a gap of a predetermined size is not particularly limited as long as the structure maintains heat retention in the unconnected state. As shown in Figure 2, the thermal switch may be fixed using a connecting member having thermal insulation properties.

[0040] Next, the temperature adjustment function of the thermal switch of the present invention provided around the battery pack will be described. By changing the heat dissipation state at a predetermined temperature, the battery pack effectively utilizes the heat generated by discharge while adjusting the temperature, thereby improving the function of the battery. Specifically, when the vehicle is started, the temperature is low, the battery resistance is high, and it is desirable not to dissipate heat inside the battery pack as much as possible. On the other hand, after the vehicle is warmed up, the temperature inside the battery pack increases and there is a risk of fire due to electrolyte decomposition, so it is preferable to actively dissipate the temperature inside the battery pack. Since the thermal switch of the present invention provided in the battery pack is in a non-connected state when the vehicle is started, it is difficult to dissipate heat inside the battery pack, and the heat can be effectively used to keep the battery warm and raise the temperature to a temperature with good discharge efficiency. On the other hand, after the vehicle is warmed up, the temperature inside the battery pack rises, the thermal switch is in a connected state, and the heat transfer efficiency increases rapidly, so that the heat inside the battery pack can be actively released to the outside. EXAMPLES

[0041] Next, the present invention will be specifically described with reference to examples.

[0042] [Example 1] 100 parts by mass of natural rubber, 200 parts by mass of magnesium oxide powder as a thermally conductive filler (Ube Material Industries, Ltd. "RF-50SC", thermal conductivity 45 W / m K), 5 parts by mass of zinc oxide (Sakai Chemical Industry Co., Ltd. zinc oxide type 2), 1 part by mass of zinc stearate (Kao Corporation Lunac S30), 1.5 parts by mass of antioxidant A (Seiko Chemical Co., Ltd. Ozonone 6C), 1 part by mass of antioxidant B (Seiko Chemical Co., Ltd. Nonflex RD), vulcanization aid (zinc monomethacrylate, Sartomer Corporation PRO115 42)3 parts by mass, wax (Sunoc manufactured by Ouchi Shinko Chemical Co., Ltd.) 2 parts by mass, oil (naphthene oil, Diana Process NM-280 manufactured by Idemitsu Kosan Co., Ltd.) 5 parts by mass, vulcanization accelerator A (N-cyclohexyl-2-benzothiazolyl sulfenamide, Noccela CZ manufactured by Ouchi Shinko Chemical Co., Ltd.) 2 parts by mass, vulcanization accelerator B (tetramethylthiuram disulfide, Sunceler TT manufactured by Sanshin Chemical Industry Co., Ltd.) 1 part by mass, and vulcanizing agent (sulfur manufactured by Karuizawa Seirensho Co., Ltd.) 0.5 parts by mass were mixed and adjusted. In addition, the above-mentioned mixing was carried out by first mixing the materials other than the vulcanizing agent and the vulcanization accelerator at 140°C for 5 minutes using a Banbury mixer, and then mixing the vulcanizing agent and the vulcanization accelerator, and kneading the mixture at 60°C for 5 minutes using an open roll. Then, the mixture was press molded (vulcanized) at 160°C for 20 minutes to produce a natural rubber sheet having a length of 100 mm, a width of 100 mm, and a thickness of 10 mm, thereby obtaining an elastic thermal expansion member.

[0043] The first and second substrates were made of aluminum plates measuring 100 mm × 100 mm × 1 mm (thermal conductivity: 237 W / m·K).

[0044] The elastic thermal expansion member, the first substrate, and the second substrate were attached to the connecting member with an adhesive, and a gap of 0.1 mm was left between the elastic thermal expansion member and the first substrate and between the elastic thermal expansion member and the second substrate, respectively, to produce the thermal switch of Example 1.

[0045] [Example 2] A thermal switch of Example 2 was produced in the same manner as in Example 1, except that the blending amount of magnesium oxide powder in the elastic thermal expansion member was changed to 300 parts by mass.

[0046] [Example 3] A thermal switch of Example 3 was produced in the same manner as in Example 1, except that the blending amount of magnesium oxide powder in the elastic thermal expansion member was changed to 50 parts by mass.

[0047] [Comparative Example 1] A thermal switch of Comparative Example 1 was produced in the same manner as in Example 1, except that the blending amount of magnesium oxide powder in the elastic thermal expansion member was changed to 0 parts by mass.

[0048] [Comparative Example 2] A thermal switch of Comparative Example 2 was produced in the same manner as in Example 1, except that the blending amount of magnesium oxide powder in the elastic thermal expansion member was changed to 400 parts by mass.

[0049] [Example 4] <Production of Composite Particle A> The thermally conductive filler was produced by the stirring granulation method. First, scaly boron particles (3M Japan "Flakes 70 / 500", average particle size (D 50 The magnetic particles were prepared as follows: magnetic particles made of insulating stainless steel powder (insulated Fe-3.5%Si-4.5%Cr manufactured by Epson Atmix Corporation, spherical, average particle diameter 3 μm); and a binder made of hydroxypropyl methylcellulose (HPMC, manufactured by Shin-Etsu Chemical Co., Ltd., TC-5).

[0050] Next, 300 g of the scaly boron particles, 150 g of insulating stainless steel powder, and 13.5 g of HPMC were placed in a container of an FM mixer (manufactured by Nippon Coke & Engineering Co., Ltd.) and mixed for 1 minute. Then, 125 g of water was added and mixed for an additional 6 minutes to produce composite particle A.

[0051] <Manufacturing of Elastic Thermal Expansion Members> An elastic thermal expansion member was manufactured using the composite particle A. First, 100 parts by mass of liquid silicone rubber ("EG-3100" manufactured by Toray Dow Corning Co., Ltd.), 0.2 parts by mass of hydrogen dimethicone ("KF9901" manufactured by Shin-Etsu Chemical Co., Ltd.) as a crosslinking agent, and 0.05 parts by mass of acetylene glycol ("Surfynol (registered trademark) 61" manufactured by Nissin Chemical Industry Co., Ltd.) as a retarder were mixed to manufacture a silicone compound.

[0052] Next, 104 parts by mass of composite particles A were added to adjust the mixed raw material. The mixed raw material was then poured into an aluminum mold (cavity is a rectangular parallelepiped of length 100 mm x width 100 mm x thickness 10 mm) that had been preheated to 130°C in an oven, and sealed. The mold was then placed in a magnetic induction molding device, and the magnetic flux density in the cavity was set to about 1000 mT, and the molding was performed at 130°C for 10 minutes while applying a magnetic field. After molding was completed, the mold was removed to obtain an elastic thermal expansion member. Then, a thermal switch was produced in the same manner as in Example 1, and the thermal switch of Example 4 was obtained.

[0053] [Table 1]

[0054] [Table 2]

[0055] <Type A durometer hardness measurement> Using a hardness tester ("ASKER P1-A" manufactured by Kobunshi Keiki Co., Ltd.) conforming to JIS K6253-3:2012, three elastic thermal expansion members with a thickness of 1 mm were stacked together and the Type A durometer hardness was measured. The Type A durometer hardness was measured as the instantaneous value immediately after the indenter came into contact with the elastic thermal expansion member.

[0056] <Measurement of thermal conductivity> The thermal conductivity of the elastic thermal expansion member was measured using a heat flux meter "HC-074" manufactured by Eiko Seiki Co., Ltd., in accordance with the heat flow meter method of JIS A1412-2:1999.

[0057] <Average coefficient of linear thermal expansion> The average linear thermal expansion coefficient of the elastic thermal expansion member was measured based on JIS K7197-1991 and used as the average linear thermal expansion coefficient.

[0058] <Evaluation of thermal switches> The heat transfer from the first substrate to the second substrate was evaluated using a heat flux meter. Specifically, the temperature of the first substrate was adjusted, and the amount of heat was measured using a heat flux meter attached to the second substrate when the temperature of the first substrate was set to 23°C and 150°C. As a result, in Example 3, the thermal conductivity of the elastic thermal expansion member was low, resulting in slightly poorer heat dissipation, but it functioned as a thermal switch. In Comparative Example 1, the thermal conductivity of the elastic thermal expansion member was low, resulting in poorer heat dissipation. In Comparative Example 2, the average linear thermal expansion coefficient of the elastic thermal expansion member was low, and the elastic thermal expansion member did not come into contact with the second substrate, and did not function as a thermal switch. [Industrial Applicability]

[0059] The thermal switch of the present invention can be used as a switch whose heat transfer performance changes depending on the temperature. For example, in a battery pack, exhaust gas filter, etc., even if the catalytic activity is low at a low temperature at the start, it is expected that the temperature can be raised to the active temperature in a relatively short time by insulation, and conversely, if the temperature becomes too high, it is expected that the heat dissipation property can be exhibited and the thermal deterioration of the catalyst and the base material body can be suppressed. When the thermal switch of the present invention is used in a battery pack, exhaust gas filter, etc., the heat dissipation and heat retention can be controlled to maintain an optimal temperature and optimize the discharge effect of the battery. [Explanation of symbols]

[0060] 1. Thermal Switch 10 Elastic thermal expansion member 11 First base material 12 Second base material 13 Connecting members 14 Thermal insulation materials 15 Support member

Claims

1. A thermal switch comprising: a first substrate; a second substrate; and an elastic thermal expansion member interposed between the first substrate and the second substrate, the elastic thermal expansion member expanding under a predetermined temperature condition to connect the first substrate and the second substrate and to form a heat transfer path between the first substrate and the second substrate, The elastic thermal expansion member includes a thermosetting elastomer and a thermally conductive filler dispersed in the thermosetting elastomer; The elastic thermal expansion member has an average linear thermal expansion coefficient of 1×10 -4 / K~10x10 -4 / K, The thermal switch is characterized in that the thermally conductive filler is oriented in the elastic thermal expansion member to form the heat transfer path from the first substrate along the second substrate.

2. 2. The thermal switch according to claim 1, wherein the thermosetting elastomer is selected from among cross-linkable elastomers such as silicone rubber, urethane rubber, fluororubber, acrylic rubber, natural rubber, butadiene rubber, chlorinated polyethylene, epichlorohydrin rubber, and chlorosulfonated polyethylene.

3. 3. The thermal switch according to claim 1, wherein the thermal conductive filler has a thermal conductivity of 20 W / m·K or more.

4. The thermal switch according to any one of claims 1 to 3, wherein the thermally conductive filler is 20 to 350 parts by mass with respect to 100 parts by mass of the thermosetting elastomer.

5. 5. The thermal switch according to claim 1, wherein the thermally conductive filler is a composite particle comprising a thermally conductive anisotropic particle, a magnetic particle, and a binder.

Citation Information

Patent Citations

  • Heat transfer sheet, and heat dissipation structure

    JP2008258199A

  • Thermal switch, temperature regulating structure and battery pack

    WO2014156991A1

  • Resin member, heat switch, composition for heat switch, and temperature adjustment structure

    WO2017163316A1