Electrode lead bending and welding device and electrode lead welding method using the same
The electrode lead bending and welding device addresses the issue of welding defects by incorporating a sensing part and vision camera to verify the bending state, ensuring a wide contact surface and preventing defects.
Patent Information
- Application Number
- JP2022560125
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-07-15
- Filing Date
- 2021-07-08
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2041-07-08
AI Technical Summary
Existing electrode lead bending devices fail to ensure a proper bending state before welding, leading to gaps and reduced adhesive force between electrode leads and bus bars, resulting in welding defects.
An electrode lead bending and welding device with a sensing part that checks the bending state of the electrode lead before welding, ensuring a proper angle and contact with the bus bar, and includes a vision camera for advanced inspection.
Prevents welding defects by ensuring a wide contact surface and detecting potential issues before welding, improving production quality and reducing costs.
Smart Images

Figure 0007570754000001 
Figure 0007570754000002 
Figure 0007570754000003
Abstract
Description
[Technical field]
[0001] This application claims the benefit of priority based on Korean Patent Application No. 2020-0087736 filed on July 15, 2020, and all contents disclosed in the documents of that Korean patent application are incorporated herein by reference.
[0002] The present invention relates to an electrode lead bending and welding device, and more particularly, to an electrode lead bending and welding device having a structure capable of evaluating a bending state of an electrode lead and then performing welding for electrical connection between an electrode lead and a bus bar. [Background technology]
[0003] As rechargeable and dischargeable lithium secondary batteries have been rapidly improved in terms of safety and capacity, the types of devices to which the lithium secondary batteries are applied are gradually increasing.
[0004] For example, they are used not only as energy sources for wireless mobile devices and wearable devices, which are small, multi-functional products, but also as energy sources for electric vehicles and hybrid electric vehicles, which are presented as alternatives to gasoline and diesel vehicles that cause air pollution.
[0005] The lithium secondary batteries used in electric vehicles and the like require high output and high capacity characteristics, so a battery module and a battery pack are formed by connecting a plurality of battery cells in series and / or parallel.
[0006] In this manner, in order to electrically connect a plurality of battery cells, a method of coupling electrode leads of the plurality of battery cells to a bus bar can be used.
[0007] For example, the electrode lead passes through a slit in the bus bar, is bent so as to make surface contact with the bus bar, and is then moved to a welding jig in this state and welded. However, during the process of transferring the bus bar and the battery cells to the welding jig and the process of mounting the bus bar and the battery cells on the welding jig, gaps are likely to occur in the welded portion where the bus bar and the electrode lead are welded.
[0008] In this regard, FIG. 1 is a front view showing an electrode lead in which a welding defect occurs when a conventional bending device is used.
[0009] Referring to FIG. 1, a plurality of pouch-type battery cells 110 are arranged in close contact with each other, and electrode leads 111 pass through slits 131 in a bus bar 130 and protrude upward.
[0010] The electrode lead bending device 120 is disposed on one side of the electrode lead 111 so as to contact the bus bar 130 and bends the electrode lead 111 while moving leftward.
[0011] However, in this process, the electrode lead 111 on the left side in Fig. 1 may be bent at an angle greater than 90 degrees, as in the electrode lead 112 on the right side in Fig. 1. Alternatively, in the process of transferring the bent electrode lead together with the bus bar to a welding jig (not shown), the bent portion of the electrode lead may break or be bent more, resulting in a problem of a reduction in the welding surface between the bus bar and the electrode lead.
[0012] In this way, when a gap occurs in the welded portion, the adhesive strength between the electrode lead and the bus bar decreases, which may result in defective welding.
[0013] In this regard, Patent Document 1 discloses a method for producing a battery module, in which a plurality of bus bars are disposed near electrode leads provided on a plurality of battery cells, respectively, a welding jig presses the electrode leads so that the electrode leads contact the respective bus bars, and the electrode leads and the bus bars are welded through openings formed in the welding jig.
[0014] In the invention of Patent Document 1, the electrode lead is bent using a welding jig and welding is performed through an opening formed in the welding jig, but since the welding is performed without being able to check whether the electrode lead is bent properly, there is a limit to checking for welding defects after welding. Therefore, it is difficult to prevent welding defects from occurring in advance.
[0015] Patent Document 2 discloses a secondary battery cell lead tab bending device that bends a protruding lead tab of a secondary battery by pressing it to one side.
[0016] Although the bending device of Patent Document 2 can bend a plurality of lead tabs quickly and accurately, it cannot solve the problem of the bent lead tabs becoming misaligned while being transferred to the welding jig.
[0017] Patent Document 3 discloses a welding jig assembly including a tilting portion and an elastic member so that a tight contact state can be maintained between a cell lead, which is a base material for welding, and a contact member even if the flatness of the cell lead is changed.
[0018] Patent Document 3 uses a structure in which a welding jig is tilted in case the flatness of the bent cell lead is changed, but fails to recognize the technology for bending the cell lead.
[0019] As described above, there is a strong need for a technology that can not only quickly bend the electrode leads to electrically connect the electrode leads to the bus bar, but also ensure a wide welding surface between the electrode leads and the bus bar and reduce welding defects by inspecting for the possibility of welding defects before welding. [Prior art documents] [Patent documents]
[0020] [Patent Document 1] Korean Patent Publication No. 2018-0129170 [Patent Document 2] Korean Patent No. 2015898 [Patent Document 3] Korean Patent Publication No. 2018-0082914 Summary of the Invention [Problem to be solved by the invention]
[0021] The present invention has been made to solve the above problems, and an object of the present invention is to provide an electrode lead bending and welding device having a structure capable of preventing welding defects in advance by checking the bending state of the electrode lead in advance before welding after bending the electrode lead, and a method of welding an electrode lead using the same. [Means for solving the problem]
[0022] To achieve the above object, the electrode lead bending and welding device according to the present invention includes a base portion movable in vertical and horizontal directions, a bending portion attached to the base portion and extending downward, and a sensing portion rotatably attached to the bending portion, and can perform welding between the electrode lead and a bus bar in a state where the bending portion bends the electrode lead.
[0023] In the electrode lead bending and welding device of the present invention, the sensing unit may have a structure that is attached to the bending portion in a state perpendicular to a lower surface of the bending portion before the bending portion bends the electrode lead, and rotates to become parallel to the lower surface of the bending portion when the electrode lead is bent.
[0024] Also, the angle between the sensing portion and the lower surface of the bent portion can be measured to determine whether the bent state of the electrode lead is good or bad.
[0025] Alternatively, the angle between the sensing portion and the bus bar can be measured to determine whether the electrode lead is bent properly.
[0026] In the electrode lead bending and welding device of the present invention, a size of a gap formed between the sensing portion and the bus bar may be formed to be the same as a thickness of the electrode lead.
[0027] In the electrode lead bending and welding device of the present invention, the sensing unit is connected to the bending unit via an elastic member, and after welding of the electrode lead is completed, the elastic force of the elastic member allows the sensing unit to return to a standby state.
[0028] The electrode lead bending and welding apparatus of the present invention may further include a vision camera for inspecting a welding state between the electrode lead and the bus bar.
[0029] In the electrode lead bending and welding device of the present invention, the bending portion has a rectangular prism shape with a hollow, and a welding rod can be inserted through the hollow to perform welding.
[0030] In the electrode lead bending and welding device of the present invention, a welding rod may be provided on the lower surface of the bending portion.
[0031] In the electrode lead bending and welding device of the present invention, one bending part coupled with one sensing part is attached to the base part to form a unit, and a structure in which a plurality of units can be assembled may be provided.
[0032] The present invention also provides a method for welding an electrode lead using the electrode lead bending and welding device, which includes the steps of: (a) preparing a battery cell and arranging the electrode lead so that it passes through a slit in a bus bar; (b) arranging a bending portion of the electrode lead bending and welding device on a first surface of the electrode lead; (c) bending the electrode lead; and (d) welding the bent electrode lead to the bus bar.
[0033] The method for welding an electrode lead according to the present invention may further include, before step (d), a step of determining whether the bent state of the electrode lead is good or bad.
[0034] In the electrode lead welding method according to the present invention, in step (b), the electrode lead bending and welding device may be moved downward, a sensing portion of the electrode lead bending and welding device may be positioned to pass through the slit of the bus bar parallel to a direction in which the electrode lead protrudes, and a lower surface of the bending portion of the electrode lead bending and welding device may be disposed adjacent to the bus bar.
[0035] In the electrode lead welding method according to the present invention, step (c) may include a step of disposing the bent portion on a first surface of the electrode lead, and horizontally moving the bent portion so that a second surface opposite to the first surface faces the bus bar in parallel.
[0036] In the electrode lead welding method according to the present invention, a sensing unit of the electrode lead bending and welding device may be rotated 90 degrees in a first direction by horizontal movement of the bending unit and positioned on an outer surface of the bus bar.
[0037] In the electrode lead welding method according to the present invention, after step (d), the sensing unit may move away from the bus bar and rotate 90 degrees in a second direction opposite to the first direction to return to a standby state. Effect of the Invention
[0038] As described above, the present invention has a structure in which the electrode lead is welded to the bus bar in a bent state by eliminating the processes of transporting the electrode lead and the bus bar to the welding jig and mounting the electrode lead on the welding jig, thereby preventing a problem of misalignment of the welded portion during the transport and mounting processes.
[0039] In addition, since the welding device includes a sensing unit capable of sensing a bending state of the electrode lead, it is possible to determine whether a welding defect will occur from the appearance of the sensing unit before welding the electrode lead.
[0040] In this way, since it is possible to detect in advance any gaps formed between the bus bar and the electrode lead that cause welding defects, it is possible to improve production quality and reduce costs due to the occurrence of defects.
[0041] In addition, the sensing unit can also detect in advance the maintenance and repair cycles of the electrode lead bending and welding device. [Brief description of the drawings]
[0042] [Figure 1] FIG. 11 is a front view showing an electrode lead in which poor welding occurred when a conventional bending device was used. [Diagram 2] 4 is a front view showing a process of using the electrode lead bending and welding device according to the present invention; FIG. [Diagram 3] 1 is a perspective view showing a state in which an electrode lead bending and welding device is disposed above a battery cell in which an electrode lead penetrates a bus bar. FIG. [Figure 4] FIG. 4 is a perspective view of the electrode lead bending and welding device of FIG. 3. [Diagram 5] FIG. 2 is a perspective view of an electrode lead bending and welding device according to one embodiment. [Figure 6] 13 is a perspective view of an electrode lead bending and welding device according to another embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0043] Hereinafter, the present invention will be described in detail with reference to the accompanying drawings, which are provided to enable a person having ordinary skill in the art to which the present invention pertains to easily carry out the present invention. However, in describing the operation principle of the preferred embodiment of the present invention in detail, detailed description of related well-known functions or configurations will be omitted if it is determined that such detailed description may unnecessarily obscure the gist of the present invention.
[0044] In addition, the same reference numerals are used throughout the drawings for parts having similar functions and actions. Throughout the specification, when a part is said to be connected to another part, this includes not only the case where the part is directly connected to another part, but also the case where the part is indirectly connected via another element between the two parts. In addition, when a part includes a certain component, it does not mean that the other component is excluded, but that the part may further include the other component, unless otherwise specified.
[0045] Furthermore, descriptions that limit or add specific elements are applicable to all inventions and are not limited to a particular invention unless otherwise specified.
[0046] Furthermore, throughout the present specification, the singular includes the plural unless otherwise specified.
[0047] In addition, throughout the specification of the present invention, unless otherwise specified, "or" includes "and." Therefore, "including A or B" means three cases: including A, including B, or including both A and B.
[0048] Furthermore, all numerical ranges include the endpoints and all intermediate values therebetween unless expressly stated to the contrary.
[0049] The invention will now be explained with reference to the drawings and in conjunction with detailed embodiments.
[0050] FIG. 2 is a front view showing a process of using the electrode lead bending and welding device according to the present invention.
[0051] Referring to FIG. 2, the electrode lead bending and welding device 220 according to the present invention includes a base part 221 movable in a vertical direction (y-axis direction) and a horizontal direction (x-axis direction), a bending part 222 attached to the base part 221 and extending downward, and a sensing part 223 rotatably attached to the bending part 222, and welding is performed between the electrode lead 211 and the bus bar 230 when the bending part 222 bends the electrode lead 211.
[0052] A method for welding an electrode lead according to one embodiment includes the steps of: (a) preparing a battery cell and arranging the electrode lead so that it passes through a slit in a bus bar; (b) arranging a bending portion of an electrode lead bending and welding device on a first surface of the electrode lead; and (c) bending the electrode lead; and welding the bent electrode lead to the bus bar.
[0053] Also, referring to FIG. 2 , the pouch-type battery cells 210 are arranged in close contact with each other so that the electrode leads 211 of the pouch-type battery cells 210 protrude upward, and the bus bar 230 is disposed on the upper part of the battery cells 210 so that the electrode leads 211 pass through the slits 231 of the bus bar 230.
[0054] The electrode lead welding and bending device 220 moves downward so that the bending portion 222 is disposed on a first surface, which is one of both sides of the electrode lead. Here, the sensing portion 223 of the electrode lead bending and welding device 220 is parallel to the protruding direction of the electrode lead and is positioned passing through the slit 231 of the bus bar 230 while extending downward toward the battery cell 210. The lower surface 222a of the bending portion is disposed adjacent to the bus bar 230.
[0055] When base portion 221 moves in the -x direction so that bent portion 222 moves horizontally, electrode lead 211 is bent into an "L" shape so that a second surface, which is the surface opposite to the first surface, faces parallel to the upper surface of bus bar 230. The portion where the electrode lead bent in this manner makes surface contact with the bus bar becomes a welded portion. Here, in order to ensure the bonding strength between the bus bar and the electrode lead, it is necessary to ensure that the welded portion is as wide as possible.
[0056] Before the bending portion 222 bends the electrode lead 211, the sensing portion 223 is attached to the bending portion 222 in a state perpendicular to the lower surface 222a of the bending portion, and as the bending portion 222 moves horizontally, the sensing portion 223 rotates 90 degrees in the first direction and is positioned on the upper surface of the bus bar 230. That is, when the electrode lead 211 is bent, the sensing portion 223 has a structure that rotates to become parallel to the lower surface 222a of the bending portion.
[0057] Since the sensing part 223 is connected to the bending part 222 via an elastic member, when the electrode lead bending and welding device moves away from the bus bar after welding of the electrode lead 211 is completed, the elastic force of the elastic member causes the sensing part 223 to rotate 90 degrees in a second direction, which is the opposite direction to the first direction, and return to a standby state.
[0058] The standby state refers to a state before the sensing unit is rotated 90 degrees in the first direction.
[0059] The elastic member may include, for example, a spring and a rubber band.
[0060] When electrode lead 211 is bent 90 degrees in the first direction, the distance of the space formed between bus bar 230 and bent portion 222 becomes the same as the thickness of electrode lead 211 .
[0061] Since the present invention includes a vision camera for inspecting the welding condition between the electrode lead 211 and the bus bar 230, it is possible to check in advance whether the bending condition of the electrode lead is normal before welding the bent electrode lead to the bus bar.
[0062] Specifically, the vision camera can determine whether the electrode lead is bent properly by measuring the distance between the bent portion of the electrode lead and the bus bar, by measuring the angle between the sensing portion and the underside of the bent portion, or by measuring the angle between the sensing portion and the bus bar.
[0063] Therefore, when the thickness of the sensing portion is smaller than the thickness of the electrode lead or the sensing portion is joined at a position that does not affect the distance between the bus bar and the bent portion, and when the distance between the bus bar 230 and the bent portion 222 is the same as the thickness of the electrode lead, the electrode lead 211 is in close contact with the bus bar, so that the welding surface is maximized, thereby significantly reducing the possibility of poor welding.
[0064] For example, if the distance between busbar 230 and underside 222a of the bent portion is measured to be 0.4 mm and 0.2 mm when a positive electrode lead made of aluminum and 0.4 mm thick is used, and when a negative electrode lead made of copper and 0.2 mm thick is used, it can be seen that the electrode lead is bent 90 degrees and positioned on the upper surface of the busbar.
[0065] In addition, when the angle between the sensing portion 223 and the underside 222a of the bent portion, and the angle between the sensing portion 223 and the bus bar 230 are 0 degrees, the bent state of the electrode lead is normal, and when the angles are not 0 degrees, the bent state of the electrode lead is poor.
[0066] In this way, if the electrode lead is not properly bent, the electrode lead can be bent again to maximize the contact area between the electrode lead and the bus bar.
[0067] FIG. 3 is a perspective view showing a state in which an electrode lead bending and welding device is disposed above a battery cell in which an electrode lead penetrates a bus bar, and FIG. 4 is a perspective view of the electrode lead bending and welding device of FIG.
[0068] Referring to FIG. 3, the electrode lead bending and welding device 220 is the same as that shown in FIG. 2 and includes a plurality of bent portions 222 extending downward from a base portion 221, and shows that when placed on the bus bar 230, the bent portions 222 are positioned on the first surface 211a of the electrode lead 211.
[0069] The bent portion 222 has a rectangular prism shape with a hollow 224 formed therein, and the hollow 224 is formed so as to penetrate the bent portion 222 from the base portion 221. Thus, a welding rod can be inserted through the hollow 224 to perform welding, and welding can be performed between the electrode lead 211 and the bus bar 230 in a state where the bent portion presses the electrode lead.
[0070] Referring to FIG. 4, the sensing portion 223 is attached to the slit of the busbar while extending downward so as to be perpendicular to the underside 222a of the bent portion, and when the bent portion 222 moves to bend the electrode lead, the sensing portion 223 rotates 90 degrees to become parallel to the underside 222a of the bent portion.
[0071] That is, as shown in FIG. 4, when the sensing part 223 is attached to the lower surface 222a of the bent part, the electrode lead can be bent with the sensing part 223 in close contact with the electrode lead.
[0072] Therefore, the sensing portion 223 rotates at the same angle as the bending angle of the electrode lead 211. Therefore, if the angle of the sensing portion 223 with respect to the lower surface 222a of the bending portion is not 0 degrees, the bending state of the electrode lead can be determined to be defective.
[0073] In this manner, when the sensing portion 223 is attached to the underside 222a of the bent portion, the electrode lead and the sensing portion 223 are bent in a state of close contact with each other, so that it is possible to check whether the electrode lead is bent properly even if the width of the bus bar is smaller than the width w of the bent portion 222.
[0074] FIG. 5 is a perspective view of an electrode lead bending and welding device according to one embodiment.
[0075] Referring to FIG. 5, the electrode lead bending and welding device 320 has a bending portion 322 attached to extend downward from a base portion 321, and a sensing portion 323 having a rotatable shape is attached to the lower portion of a side 322b of the bending portion.
[0076] It is preferable that the sensing portion 323 be in the same plane as the lower surface 322a of the bent portion so that the angle formed between the sensing portion 323 and the lower surface 322a of the bent portion becomes 0 degrees when the sensing portion 323 is rotated.
[0077] In this manner, when the sensing portion 323 is provided on the side 322b of the bent portion, the electrode lead can be bent 90 degrees even if the thickness of the electrode lead is greater than the thickness of the sensing portion, so that it is possible to check whether the electrode lead is bent properly.
[0078] Unlike the bent portion 222 having the hollow 224 in Fig. 4, a welding rod 325 can be provided on the lower surface 322a of the bent portion 322. The lower end of the welding rod 325 can protrude beyond the lower surface 322a of the bent portion or can be disposed on the same plane as the lower surface 322a of the bent portion.
[0079] Therefore, the welding process can be quickly performed after the electrode lead is bent and pressed.
[0080] The number of welding rods may be three for each bent portion as shown in FIG. 4, but is not limited thereto.
[0081] FIG. 6 is a perspective view of an electrode lead bending and welding device according to another embodiment.
[0082] Referring to FIG. 6, the electrode lead bending and welding device unit 420, 420' is formed by attaching one bending portion 422 to which one sensing portion 423 is coupled to a base portion 421, and the respective units may be coupled to each other to assemble a plurality of units.
[0083] A recess 427 is formed in the base part 421 of the unit body 420, and a protrusion 428 of a corresponding shape is formed in the unit body 420' so as to be coupled in a sliding manner to the recess 427 of the unit body 420. Also, the unit body 420' is formed with a recess 427 so as to be coupled to another unit body.
[0084] Although not shown in FIG. 6, the unit body may be welded by inserting a welding rod into a hollow formed to pass from the base portion through the bent portion as in the form shown in FIG. 3 and FIG. 4, or may have a form in which a welding rod protrudes from the underside of the bent portion as in the form shown in FIG. 5.
[0085] The present invention relates to a device for bending and welding electrode leads of a plurality of battery cells in a state where the battery cells are closely arranged. When a structure capable of combining a plurality of units is provided, it is advantageous in that the combination and separation of the units can be selectively performed depending on the number of pouch-type battery cells.
[0086] In this manner, when using the electrode lead bending and welding device according to the present invention, the quality of the bent state of the electrode lead can be inspected in advance before the welding operation, thereby preventing the occurrence of welding defects in advance.
[0087] Those skilled in the art will appreciate that the present invention can be applied and modified in various ways within the scope of the present invention based on the above content. [Industrial Applicability]
[0088] As described above, the present invention has a structure in which the electrode lead is welded to the bus bar in a bent state by eliminating the processes of transporting the electrode lead and the bus bar to the welding jig and mounting the electrode lead on the welding jig, thereby preventing a problem of misalignment of the welded portion during the transport and mounting processes.
[0089] In addition, since the welding device includes a sensing unit capable of sensing a bending state of the electrode lead, it is possible to determine whether a welding defect will occur from the appearance of the sensing unit before welding the electrode lead.
[0090] In this manner, since it is possible to detect in advance any gaps formed between the bus bar and the electrode lead that may cause welding defects, it is possible to improve production quality and reduce costs due to the occurrence of defects.
[0091] In addition, the sensing unit can also detect in advance the maintenance and repair cycles of the electrode lead bending and welding device. [Explanation of symbols]
[0092] 110, 210 battery cells 111, 112, 211 Electrode leads 120 Electrode lead bending device 130, 230 busbar 131, 231 Slit 211a 1st page 220, 320 Electrode lead bending and welding device 221, 321, 421 Base 222, 322, 422 Bend section 222a, 322a Underside of bent portion 223, 323, 423 Sensing section 224 Hollow 322b Side of bent part 325 Welding Rod 420, 420´ Unit 427 Recess 428 Protrusion w Bending width
Claims
1. A base portion that is movable in vertical and horizontal directions; a bent portion attached to the base portion and extending downward; a sensing unit rotatably attached to the bent portion; Including, The bending unit performs welding between the electrode lead and a bus bar in a state where the electrode lead is bent, the sensing unit is attached to the bending portion in a state perpendicular to a lower surface of the bending portion before the bending portion bends the electrode lead, and has a structure that rotates to be parallel to the lower surface of the bending portion when the electrode lead is bent, measuring an angle between the sensing portion and a lower surface of the bent portion to determine whether the bent state of the electrode lead is good or bad; or The electrode lead bending and welding device measures an angle between the sensing portion and a bus bar to determine whether the electrode lead is bent properly.
2. 2. The electrode lead bending and welding device according to claim 1, wherein a size of a gap between the bent portion and the bus bar is equal to a thickness of the electrode lead.
3. 3. The electrode lead bending and welding device according to claim 1, wherein the sensing part is coupled to the bending part via an elastic member, and after welding of the electrode lead is completed, the elastic force of the elastic member causes the sensing part to return to a standby state.
4. The electrode lead bending and welding device according to claim 1 , further comprising a vision camera for inspecting a welding condition between the electrode lead and the bus bar.
5. 5. The electrode lead bending and welding device of claim 1, wherein the bending portion has a rectangular prism shape with a hollow, and a welding rod is inserted through the hollow to perform welding.
6. The electrode lead bending and welding device according to claim 1 , wherein a welding rod is provided on the underside of the bent portion.
7. 7. The electrode lead bending and welding device according to claim 1, wherein one bending portion coupled to one sensing portion is attached to the base portion to form a unit, and a plurality of units are assembled.
8. A method for welding an electrode lead using the electrode lead bending and welding device according to any one of claims 1 to 7, comprising: (a) preparing a battery cell and arranging the battery cell so that an electrode lead passes through a slit in a bus bar; (b) disposing a bend portion of an electrode lead bending and welding device on a first surface of the electrode lead; (c) bending the electrode lead; (d) welding the bent electrode lead to the bus bar; before step (d), determining whether the bent state of the electrode lead is good or bad; A method for welding an electrode lead, comprising:
9. In the step (b), The electrode lead bending and welding device moves downward, a sensing unit of the electrode lead bending and welding device is disposed to pass through the slit of the bus bar in parallel with a direction in which the electrode lead protrudes, The electrode lead welding method according to claim 8 , wherein a lower surface of a bending portion of the electrode lead bending and welding apparatus is disposed adjacent to the bus bar.
10. 10. The method of claim 8, wherein step (c) includes the step of disposing the bent portion on a first surface of the electrode lead, and horizontally moving the bent portion such that a second surface opposite to the first surface faces the bus bar in parallel.
11. 11. The electrode lead welding method according to claim 8, wherein a sensing unit of the electrode lead bending and welding apparatus is rotated 90 degrees in a first direction by the horizontal movement of the bending unit and positioned on an outer surface of the bus bar.
12. The method of claim 11 , wherein, after step (d), the sensing unit moves away from the bus bar, rotates 90 degrees in a second direction opposite to the first direction, and returns to a standby state.
Citation Information
Patent Citations
Inspection method of joined state between electrode tab and bus bar
JP2018006217A
Manufacturing method of power storage device, power storage element, and power storage device
JP2018116926A
Manufacturing apparatus for battery pack and manufacturing method for battery pack
JP2018181678A
Terminal welding device
JP2020087751A
Folding Device for electrode lead Part of Battery Cell
KR102015898B1