Layered container
The laminated container design with an easily tearable label layer and container layer allows for easy separation and recycling, addressing the challenges of existing laminated containers by reducing environmental burden and facilitating recycling.
Patent Information
- Application Number
- JP2021078151
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-04-30
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2041-04-30
AI Technical Summary
Existing laminated containers with shrink labels face challenges in recycling due to the need for additional components and environmental burden when attempting to make them thinner, as well as difficulties in separating the ink used for decoration.
A laminated container design featuring a container layer and a label layer with a rupture layer that can be easily peeled off, including an easily tearable portion and a difficult layer, formed through extrusion blow molding, allowing for easy separation and recycling.
The design enables easy recycling of containers while reducing environmental impact by facilitating the separation of the label from the container body, even when decorated, thus enhancing recyclability.
Smart Images

Figure 0007570785000001 
Figure 0007570785000002 
Figure 0007570785000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to laminated containers. [Background technology]
[0002] Currently, due to social demands such as reducing the burden on the environment, there is a demand for recycling resin containers. On the other hand, containers are widely used that have been decorated by printing, transferring, vapor deposition, painting, or other means on the body of the container to create a beautiful appearance or display a trademark, product name, manufacturer name, or description of the contents (for example, Patent Document 1). When trying to recycle these containers, it is difficult to completely remove the ink, etc. used for printing, making it difficult to separate and recycle the containers.
[0003] To address these problems, for example, Patent Document 2 proposes a container that is made easier to recycle by wrapping a shrink label displaying the product name and a description of the contents around the body and cap of the container and removing the shrink label from the container body when recycling. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2010-149910 A [Patent Document 2] JP 2012-176760 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, with the shrink-labeled container described in Patent Document 2, it is necessary to prepare a shrink label separately from the container body, and if attempts are made to thin the container body in consideration of the burden on the environment, it can become difficult to attach the shrink label, so there is room for improvement in these respects.
[0006] The present disclosure is directed to solving such problems, and has an object to propose a laminated container that can be easily recycled while reducing the burden on the environment. [Means for solving the problem]
[0007] The laminated container of the present disclosure comprises: a container layer having a body portion for accommodating contents, a mouth portion connected to an upper end portion of the body portion, and a bottom portion closing a lower end portion of the body portion; a label layer that covers the container layer from the outside at least in the body portion; Equipped with The label layer has an easy-to-break breakable layer that contacts the outermost surface of the container layer, and a difficult-to-break layer that is provided outside the breakable layer. A laminated structure that provides Has The outermost surface of the container layer and the tear layer of the label layer are formed of materials that are peelable from each other, The label layer in the part of the body portion has In the laminate structure The present invention is characterized in that an easy-tear portion that does not have the difficult-to-fault layer is provided.
[0008] In addition, in the above-mentioned configuration of the laminated container of the present disclosure, it is preferable that the laminated container is formed by extrusion blow molding, and that the lower part of the easy-tear portion is formed so as to be connected to a pinch-off portion provided at the bottom.
[0009] In addition, in the above-described configuration of the laminated container of the present disclosure, it is preferable that the pinch-off portion is provided with a gripping portion hanging down from the bottom portion, and the lower portion of the easy-tear portion is formed so as to overlap the gripping portion.
[0010] In the laminated container of the present disclosure, in the above configuration, it is preferable that the easy-tear portion extends in a substantially vertical direction, and an upper end of the easy-tear portion extends to the mouth portion.
[0011] In addition, in the laminated container of the present disclosure, in the above configuration, it is preferable that the fracture layer has a smaller fracture elongation than the fracture-resistant layer.
[0012] In the laminated container of the present disclosure, in the above configuration, it is preferable that the fracture layer has a fracture strength of 50 MPa or less, and the difference in fracture elongation between the fracture layer and the less-fracturable layer is 50% or more. Effect of the Invention
[0013] According to the present disclosure, it is possible to propose a laminated container that can be easily recycled while reducing the burden on the environment. [Brief description of the drawings]
[0014] [Figure 1] FIG. 2 is a front partial cross-sectional view of a laminated container according to an embodiment of the present disclosure. [Diagram 2] FIG. 2 is a side view of a stacked container according to one embodiment of the present disclosure. [Diagram 3] FIG. 2 is a bottom view of a laminated container according to one embodiment of the present disclosure. [Figure 4A] FIG. 2 is a detailed view of part A in FIG. [Figure 4B] 1 is a cross-sectional view of an easy-tear portion in a laminated container according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] The present disclosure will now be described more specifically with reference to the drawings.
[0016] FIG. 1 is a front view showing a configuration of a stacked container 100 according to an embodiment of the present disclosure. The stacked container 100 includes a body 20 having a substantially elliptical shape in a plan view (see FIG. 3) that forms a storage space S for contents, a mouth 10 that is connected to the upper end of the body 20 via a shoulder 30 and forms an opening 10a on the inside for supplying and discharging the contents, and a bottom 40 that closes the lower end of the body 20. As shown in FIG. 1, the outer peripheral surface of the mouth 10 is provided with a male thread 10b that allows a cap, a pump, or the like to be attached by threaded engagement. A bottle layer 22 (container layer) shown in a partial cross section in FIG. 1 forms the entire area of the mouth 10, the shoulder 30, the body 20, and the bottom 40 in FIG. 1.
[0017] In this specification, claims, and drawings, the side where the mouth 10 is located is referred to as the upper side (upper side in FIG. 1), and the side where the bottom 40 is located is referred to as the lower side (lower side in FIG. 1). In addition, in describing the layer structure of the stacked container 100, the storage space S side is referred to as the inner side, and the side of the stacked container 100 with the difficult-to-fault layer 24c is referred to as the outer side. In addition, the radially outer side refers to the direction away from the central axis O along a straight line passing through the central axis O of the stacked container 100 in FIG. 1 and perpendicular to the central axis O, and the radially inner side refers to the direction toward the central axis O along that straight line.
[0018] As shown in Fig. 4A, the body 20 includes the above-mentioned bottle layer 22 that forms the storage space S for the contents, and a label layer 24 that covers the bottle layer 22 from the outside. In this embodiment, the label layer 24 covers the outside of not only the body 20 but the entire area of the bottle layer 22. However, this is not limited to the above, and it is sufficient that the bottle layer 22 is covered by the label layer 24 in at least a part of the body 20. In this embodiment, as described later, the thickness of the bottle layer 22 is configured to be thicker than the thickness of the label layer 24 in the entire area where the label layer 24 is formed.
[0019] The bottle layer 22 forming the skeleton of the laminated container 100 can be formed of a resin mainly made of a polyolefin resin such as polyethylene (PE) or polypropylene (PP), or a polyester resin such as polyethylene terephthalate (PET), polycyclohexylene dimethylene terephthalate (PCT), or polyethylene naphthalate (PEN). For example, when polyethylene is used for the bottle layer 22, low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), or high-density polyethylene resin (HDPE) can be used, and when HDPE or PP is used, high rigidity can be imparted to the laminated container 100. When a single PET resin is used, it may be possible to collect and recycle it as a PET bottle. The bottle layer 22 may be a resin layer formed of a resin other than a polyolefin resin and a polyester resin. In addition, the bottle layer 22 may be a resin layer formed of a virgin material such as a polyolefin resin or a polyester resin, or a virgin material mixed with a recycled material. Also, a layer of a virgin material and a layer containing a recycled material may be laminated. The bottle layer 22 may also be made of only recycled materials.
[0020] The bottle layer 22 is preferably a single resin layer made of virgin material such as the above-mentioned polyolefin resin, a mixture of virgin material and recycled material, or only recycled material. By making the bottle layer 22 a single resin layer, the separation of the laminated container 100 can be completed by only peeling off the label layer 24. In addition, by recycling the bottle layer 22 from which the label layer 24 has been separated, it can be used as a single material recycled material, so that the recyclability can be improved. However, this is not limited to the embodiment, and the bottle layer 22 may be made by laminating multiple resin layers that can be separated together. An example of including multiple resin layers includes, for example, a case where the bottle layer 22 is made of multiple resin layers including a mixture of virgin polypropylene material and recycled material, and virgin polypropylene material. In this embodiment, virgin polypropylene material is used as the bottle layer 22.
[0021] In addition, it is preferable that the bottle layer 22 does not contain a coloring material. Since the bottle layer 22 does not contain a coloring material, the laminated container 100 can be recycled as a recycled material that does not contain a coloring material. However, the present invention is not limited to this embodiment, and the bottle layer 22 may contain a coloring material.
[0022] In this embodiment, the thickness of the bottle layer 22 is 170 μm. The thickness of the bottle layer 22 is desirably 150 μm or more and 200 μm or less. By forming the bottle layer 22 to be thin in this way, the amount of resin used can be reduced, and therefore the burden on the environment can be reduced.
[0023] In this embodiment, the label layer 24 is laminated in the order of the fracture layer 24a, the adhesive layer 24b, and the hard-to-fracture layer 24c from the inside as shown in Fig. 4A. In this embodiment, the fracture layer 24a has a fracture strength and a fracture elongation that can be easily broken by a sorter, as described later. In addition, the hard-to-fracture layer 24c has a fracture elongation that cannot be easily broken by a sorter.
[0024] As shown in FIG. 1, the body 20 is provided with two easy-to-tear portions 26 extending in a substantially vertical direction. In this embodiment, the easy-to-tear portion 26 extends in a substantially vertical direction from the gripping portion 41 of the bottom to the opening 10a of the mouth portion 10. As shown in FIG. 4B, the easy-to-tear portion 26 is a portion of the label layer 24 where the adhesive layer 24b and the hard-to-fracture layer 24c are not provided, and the fracture layer 24a is exposed on the surface of the body 20. As will be described later, a sorter can peel the label layer 24 upward from the gripping portion 41 of the bottom 40 along the easy-to-tear portion 26 while easily breaking the fracture layer 24a. In this embodiment, as shown in FIGS. 1 to 3, the easy-to-tear portion 26 is provided laterally from the center position on the front side, but is not limited to this embodiment and may be provided at any circumferential position.
[0025] The bottom 40 is provided with a recess 43 that is raised higher than the peripheral edge, and as shown in Figures 1 and 3, a knob 41 extending in the left-right direction of the figure is formed in the recess 43. The knob 41 is provided along a pinch-off portion 45 that extends in the left-right direction of the figure on the bottom 40 as shown in Figure 3.
[0026] The laminated structure of the bottle layer 22 and the label layer 24 according to this embodiment is formed by forming a laminated parison in which the bottle layer 22 and the label layer 24 are laminated by extrusion molding, and then performing blow molding on the laminated parison. The pinch-off portion 45 is formed by cutting off the label layer 24 with a split die for blow molding, but since the label layer 24 is formed thinner than the bottle layer 22, the label layer 24 at the pinch-off portion 45 is not fused. In addition, a recess that defines the outer shape of the gripping portion 41 is formed at the lower end of the split die for blow molding, and the gripping portion 41 is formed by cutting off the laminated parison with the recess. The label layer 24 is not fused even at the lower end of the gripping portion 41.
[0027] As shown in Fig. 3, the lower end of the easy-tear portion 26 extending in a substantially vertical direction is connected to the region of the pinch-off portion 45 of the bottom portion 40 and is provided so as to overlap the gripping portion 41. That is, the region of the label layer 24 where the rupture layer 24a and the adhesive layer 24b are not provided extends to the lower end via the side of the gripping portion 41. With this configuration, the sorter can easily rupture the rupture layer 24a along the easy-tear portion 26 by peeling the unfused label layer 24 (the region including the hard-to-fracture layer 24c, the adhesive layer 24b, and the rupture layer 24a) between the easy-tear portions 26 at the lower end of the gripping portion 41 from the bottle layer 22 upward from the lower end.
[0028] Even if the gripping portion 41 is not provided, by configuring the lower end of the easy-tear portion 26 to be connected to the pinch-off portion 45, the sorter can easily tear the rupture layer 24a along the easy-tear portion 26 by peeling the unfused label layer 24 (the area including the hard-to-fracture layer 24c, the adhesive layer 24b and the rupture layer 24a) between the easy-tear portions 26 at the pinch-off portion 45 from the bottle layer 22 upward starting from the pinch-off portion 45.
[0029] The rupture layer 24a forms the innermost surface of the label layer 24 and is in contact with the outermost surface of the bottle layer 22. The rupture layer 24a is formed of a material that is incompatible with the outermost surface of the bottle layer 22 and can be peeled off from the bottle layer 22. When a resin mainly made of a polyolefin resin is used for the bottle layer 22, the rupture layer 24a can be made of, for example, ethylene-vinyl alcohol copolymer resin (EVOH), polyamide (nylon), polyester resin (polyethylene terephthalate (PET), polycyclohexylene dimethylene terephthalate (PCT), polyethylene naphthalate (PEN), etc.), polycarbonate (PC), ionomer (product name: Himilan (registered trademark)), or cyclic olefin copolymer. When a material mainly made of a polyester resin is used for the bottle layer 22, the rupture layer 24a can be made of, for example, EVOH, polyamide, polyolefin resin, PC, ionomer, or cyclic olefin copolymer. In this embodiment, EVOH is used for the rupture layer 24a. The EVOH used for the rupture layer 24a has a breaking strength of 34 MPa and a breaking elongation of 15% or less. In consideration of the ease of breaking of the rupture layer 24a, it is preferable that the breaking strength of the rupture layer 24a is 50 MPa or less and the breaking elongation is 10% or more and 25% or less.
[0030] In this embodiment, the hard-to-fault layer 24c in the label layer 24 is laminated on the fracture layer 24a via the adhesive layer 24b, as shown in Fig. 4A. The hard-to-fault layer 24c is decorated by means of printing, transfer, vapor deposition, painting, or adding a coloring material. The coloring material is, for example, a master batch to which a pigment is added. The decoration may be, for example, a design that evokes an aesthetic feeling in the user, a trademark, a product name, a manufacturer name, or a description of the contents.
[0031] It should be noted that decoration may be applied to at least one of the resin layers constituting the label layer 24, and the resin layer to be decorated is not limited to the hard-to-fault layer 24c.
[0032] Moreover, the hard-to-fault layer 24c may be made of glossy PP or matte PP to impart a glossy or matte finish to the outer surface of the laminated container 100.
[0033] The material of the difficult-to-fault layer 24c may be, for example, a polyolefin resin such as polyethylene (PE) such as LDPE, LLDPE, or HDPE, or polypropylene (PP), or a resin mainly made of a polyester resin such as polyethylene terephthalate (PET), polycyclohexylene dimethylene terephthalate (PCT), or polyethylene naphthalate (PEN). In this embodiment, LDPE is used as the difficult-to-fault layer 24c. The LDPE used in the difficult-to-fault layer 24c has a tensile yield stress of 13 MPa and an elongation at break of 100%. The elongation at break of the difficult-to-fault layer 24c is preferably 100% or more.
[0034] In addition, the difference in elongation at break between the break layer 24a and the difficult-to-fracture layer 24c is preferably 50% or more. Conventionally, even if an attempt was made to tear the label layer 24 during sorting, the LDPE or the like formed in the label layer 24 was stretched, and it was sometimes difficult to break it. In this embodiment, by providing an easy-to-tear portion 26 that does not have a difficult-to-fracture layer 24c in a part of the circumferential direction and providing a significant difference in elongation between the break layer 24a and the difficult-to-fracture layer 24c, it is possible to selectively break only the easy-to-tear portion 26 starting from the grip portion 41 while peeling the region between at least two easy-to-tear portions 26 in the label layer 24 upward from the bottle layer 22. Then, the remaining label layer 24 can be easily peeled from the bottle layer 22 starting from the broken easy-to-tear portion 26.
[0035] The label layer 24 is configured such that a peelable rupture layer 24a that is incompatible with the outermost surface of the bottle layer 22 is disposed in the innermost layer, and a difficult-to-fault layer 24c is disposed via an adhesive layer 24b. For example, even if it is desired to use EVOH for the rupture layer 24a to ensure gas barrier properties but decoration of the EVOH would deteriorate due to moisture in the environment, by providing the difficult-to-fault layer 24c made of polyethylene or polypropylene on the outside of the EVOH, it is possible to apply a decoration with excellent environmental resistance to the difficult-to-fault layer 24c.
[0036] In the present embodiment, the label layer 24 is configured such that the difficult-to-fault layer 24c is laminated on the outer side of the fracture layer 24a via the adhesive layer 24b, but is not limited to this form. An adhesive resin may be mixed into at least one of the fracture layer 24a and the difficult-to-fault layer 24c, and the difficult-to-fault layer 24c may be adhered to the fracture layer 24a and laminated without using the adhesive layer 24b. Also, another resin layer may be provided on the outer side of the difficult-to-fault layer 24c.
[0037] In this embodiment, for example, when inkjet printing is used, which is easy to print on thin-walled containers, the label layer 24 can be peeled off and removed from the bottle layer 22 during sorting. Therefore, it is possible to achieve both a reduction in environmental impact by thinning the containers and easy sorting of the containers. Also, when silk screen printing is used for decoration, the printing can sometimes be removed by washing, but in this embodiment, washing is not necessary.
[0038] The thickness of the label layer 24 is preferably 5 μm or more and 200 μm or less. In this embodiment, the thickness of the label layer 24 is 50 μm. If the thickness of the label layer 24 is less than 5 μm, it is difficult to form the label layer 24, and if the thickness of the label layer 24 exceeds 200 μm, it is difficult to peel and remove the label layer 24.
[0039] Furthermore, the thickness of the label layer 24 is more preferably 30 μm or more and 100 μm or less. If the thickness of the label layer 24 is less than 30 μm, it is difficult to form a laminated structure, but by making the thickness of the label layer 24 100 μm or less, it can be made thinner than the thickness of the above-mentioned bottle layer 22, making it easier to peel off and remove the label layer 24 during sorting.
[0040] Furthermore, the thickness of the label layer 24 is more preferably 40 μm or more and 80 μm or less. If the thickness is 40 μm or more, it can be made to be the same thickness as a shrink label, and can be easily formed and decorated by printing, etc. Furthermore, by making the thickness 80 μm or less, the label layer 24 can be more easily peeled off and removed during sorting.
[0041] In this embodiment, the entire area of the label layer 24 is configured to be peelable from the bottle layer 22. With this configuration, when sorting the laminated containers 100, the entire decorated label layer 24 can be peeled off from the bottle layer 22 and easily sorted.
[0042] The entire area of the label layer 24 does not necessarily have to be peelable from the bottle layer 22. For example, the label layer 24 may be provided on the entire area from the mouth 10 to the bottom 40 of the laminated container 100, and the label layer 24 and the bottle layer 22 may be partially fixed together by complex irregularities such as the male screw portion 10b of the mouth 10. The label layer 24 and the bottle layer 22 may also be bonded together in a peelable manner using an adhesive or the like.
[0043] Also, through holes may be formed in the outer surfaces of the mouth 10, bottom 40, etc. of the laminated container 100 so that the label layer 24 can be easily peeled off from the bottle layer 22 by blowing air through the through holes.
[0044] The laminated structure of the bottle layer 22 and the label layer 24 has been described based on an example in which a laminated parison in which the bottle layer 22 and the label layer 24 are laminated by extrusion molding is formed, and then the laminated parison is blow molded to manufacture the laminated container 100, but the laminated container 100 may be manufactured by stretch blow molding a laminated preform in which the bottle layer 22 and the label layer 24 are laminated.
[0045] As described above, the laminated container 100 according to this embodiment includes a container layer (bottle layer 22) having a body 20 for accommodating contents, a mouth 10 connected to the upper end of the body 20, and a bottom 40 closing the lower end of the body 20, and a label layer 24 covering the container layer from the outside at least in the body 20, the label layer 24 having an easy-to-break breakable layer 24a abutting the outermost surface of the container layer and a hard-to-break layer 24c provided outside the breakable layer 24a and difficult to break, the outermost surface of the container layer and the breakable layer 24a of the label layer 24 are formed of materials that can be peeled off from each other, and the label layer 24 in a part of the body 20 is configured to have an easy-to-tear portion 26 that does not have the hard-to-fracture layer 24c. By adopting such a configuration, separation is completed by peeling off the thin label layer 24 that has been decorated from the bottle layer 22 after use, making it easier to recycle while suppressing the burden on the environment. In particular, in this embodiment, the hard-to-fracture layer 24c is made harder to break than the break layer 24a, so that only the easy-to-tear portion 26 can be selectively broken. Then, the remaining label layer 24 can be easily peeled off from the bottle layer 22 starting from the broken easy-to-tear portion 26.
[0046] In this embodiment, the laminated container 100 is formed by extrusion blow molding, and the lower part of the easy-tear portion 26 is configured to be connected to the pinch-off portion 45 provided on the bottom portion 40. By adopting such a configuration, a sorter can easily tear the rupture layer 24a along the easy-tear portion 26 by peeling the unfused label layer 24 (the region including the hard-to-fracture layer 24c, the adhesive layer 24b, and the rupture layer 24a) between the easy-tear portions 26 at the pinch-off portion 45 from the bottle layer 22 upward starting from the pinch-off portion 45.
[0047] In this embodiment, the pinch-off portion 45 is provided with a gripping portion 41 that hangs down from the bottom portion 40, and the lower portion of the easy-tear portion 26 is configured to overlap the gripping portion 41. By adopting such a configuration, the sorter can easily break the break layer 24a along the easy-tear portion 26 by peeling the unfused label layer 24 (the region including the hard-to-fracture layer 24c, the adhesive layer 24b, and the break layer 24a) between the easy-tear portions 26 at the lower end of the gripping portion 41 from the bottle layer 22 from the bottom upward.
[0048] In this embodiment, the easy-tear portion 26 extends in a substantially vertical direction, and the upper end of the easy-tear portion 26 is configured to extend to the mouth portion 10. By adopting such a configuration, it is possible to make it easier to peel off the label layer 24 over the entire container.
[0049] In this embodiment, the fracture elongation of the fracture layer 24a is smaller than the fracture elongation of the fracture-resistant layer 24c. By adopting such a configuration, a difference in fracture elongation is provided between the fracture layer 24a and the fracture-resistant layer 24c, making it possible to easily fracture the fracture layer 24a.
[0050] In this embodiment, the fracture strength of the fracture layer 24a is 50 MPa or less, and the difference in fracture elongation between the fracture layer 24a and the fracture-resistant layer 24c is 50% or more. By adopting such a configuration, the fracture strength of the fracture layer 24a is reduced, and a significant difference in fracture elongation between the fracture layer 24a and the fracture-resistant layer 24c is provided, so that the fracture layer 24a can be broken even more easily.
[0051] Although the present disclosure has been described based on the drawings and embodiments, it should be noted that those skilled in the art can easily make various modifications and corrections based on the present disclosure. Therefore, it should be noted that these modifications and corrections are included in the scope of the present invention. For example, the functions included in each component can be rearranged so as not to cause logical inconsistency, and multiple components can be combined into one or divided. It should be understood that these are also included in the scope of the present invention.
[0052] For example, in this embodiment, the outer peripheral surface of the mouth portion 10 is provided with the male thread portion 10b, and an attachment cap, pump, etc. can be attached by threaded engagement, but the present invention is not limited to this embodiment. The mouth portion 10 may be provided with an annular protrusion for attaching an attachment cap, pump, etc. by plugging engagement, instead of or in addition to the male thread portion 10b. Also, the mouth portion 10 may be configured without an engagement portion.
[0053] In the present embodiment, the laminated container 100 is formed by blow molding a laminated parison formed by extrusion molding, or by stretch blow molding a laminated preform, but the present invention is not limited to these forms. The laminated container 100 may be formed, for example, by two-color molding, or by setting a plurality of preforms in a mold and performing stretch blow molding. The laminated structure of the bottle layer 22 (container layer) and the label layer 24 can also be formed by a method other than extrusion molding.
[0054] The present disclosure is not limited to the laminated container 100 in which the body 20 has a substantially elliptical shape in plan view as shown in Figures 1 to 3, but may simply have a flat shape having a major axis and a minor axis. It can also be widely applied to rectangular containers, pouch containers, cup containers, and the like.
[0055] In addition, in this embodiment, the easy tear portion 26 is configured to be provided at two locations in the circumferential direction, but is not limited to this embodiment. The easy tear portion 26 may be provided at one location in the circumferential direction or at three or more locations. Even if the easy tear portion 26 is provided at only one location in the circumferential direction, the boundary portion between the easy tear portion 26 and the rest (the area covered with the hard-to-fault layer 24c) can be easily torn, and the label layer 24 can be easily peeled off. [Industrial Applicability]
[0056] According to the present disclosure, it is possible to propose a laminated container 100 that can be easily recycled while suppressing the burden on the environment. [Explanation of symbols]
[0057] 10 Mouth 10a opening 10b Male thread 20 Torso 22 Bottle layer (container layer) 24 Label Layer 24a Fracture layer 24b Adhesive layer 24c difficult fault 26 Easily tearable part 30 Shoulder 40 bottom 41 Knob 43 Recess 45 Pinch-off section 100 Laminated container O center axis S Storage space
Claims
1. a container layer having a body portion for accommodating contents, a mouth portion connected to an upper end portion of the body portion, and a bottom portion closing a lower end portion of the body portion; a label layer that covers the container layer from the outside at least in the body portion; Equipped with The label layer has a laminated structure including an easy-to-break breakable layer abutting the outermost surface of the container layer and a hard-to-break layer provided outside the breakable layer, The outermost surface of the container layer and the tear layer of the label layer are formed of materials that are peelable from each other, A laminated container characterized in that the label layer in a part of the body portion has an easy-tear portion that does not have the difficult-to-fracture layer in the laminated structure.
2. 2. The laminated container according to claim 1, wherein the laminated container is formed by extrusion blow molding, and a lower portion of the easy-tear portion is formed so as to be connected to a pinch-off portion provided in the bottom portion.
3. 3. The laminated container according to claim 2, wherein the pinch-off portion is provided with a tab portion that hangs down from the bottom portion, and a lower portion of the easy-tear portion is formed so as to overlap the tab portion.
4. 4. The laminated container according to claim 2, wherein the easy tear portion extends in a substantially vertical direction, and an upper end of the easy tear portion extends to the mouth portion.
5. The laminated container according to claim 1 , wherein the fracture layer has a fracture elongation smaller than the fracture-resistant layer.
6. The laminated container according to claim 5, wherein the fracture layer has a fracture strength of 50 MPa or less, and a difference in fracture elongation between the fracture layer and the fracture-resistant layer is 50% or more.
Citation Information
Patent Citations
Multipleelayer stretched hollow container* and producing method thereof
JP1978023774A
An outer container for preventing illegal
JP1985062070U
Polypropylene resin composition for container, method for producing container and container
JP2002212358A
Multi-layer divided vessel and its molding machine
JP2004123174A
Plastic container
JP2008081169A
Cited By
Stacked bottles
JP2026143256A